{"id":10289,"date":"2024-09-11T10:20:00","date_gmt":"2024-09-11T02:20:00","guid":{"rendered":"https:\/\/app11147.cloudwayssites.com\/?p=10289"},"modified":"2025-02-17T19:04:45","modified_gmt":"2025-02-17T11:04:45","slug":"grade-18-10","status":"publish","type":"post","link":"https:\/\/steelprogroup.com\/ar\/stainless-steel\/grades\/grade-18-10\/","title":{"rendered":"\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10: \u0627\u0644\u062a\u0631\u0643\u064a\u0628 \u0648\u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0648\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a"},"content":{"rendered":"<p class=\"wp-block-paragraph\">\u0639\u0646\u062f \u0627\u062e\u062a\u064a\u0627\u0631 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0644\u0623\u0648\u0627\u0646\u064a \u0627\u0644\u0637\u0647\u064a \u0623\u0648 \u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0627\u0626\u062f\u0629 \u0623\u0648 \u062d\u062a\u0649 \u0627\u0644\u0623\u062c\u0647\u0632\u0629 \u0627\u0644\u0637\u0628\u064a\u0629\u060c \u0631\u0628\u0645\u0627 \u0635\u0627\u062f\u0641\u062a \u0645\u0635\u0637\u0644\u062d &quot;\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10&quot;. \u064a\u064f\u0639\u0631\u0641 \u0647\u0630\u0627 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0628\u062c\u0648\u062f\u062a\u0647 \u0627\u0644\u0639\u0627\u0644\u064a\u0629 \u0648\u0642\u062f\u0631\u062a\u0647 \u0639\u0644\u0649 \u0627\u0644\u062a\u062d\u0645\u0644. \u0648\u0644\u0643\u0646 \u0645\u0627\u0630\u0627 \u064a\u0639\u0646\u064a &quot;18\/10&quot; \u0628\u0627\u0644\u0636\u0628\u0637\u060c \u0648\u0644\u0645\u0627\u0630\u0627 \u064a\u062d\u0638\u0649 \u0628\u062a\u0642\u062f\u064a\u0631 \u0643\u0628\u064a\u0631\u061f \u0641\u064a \u0647\u0630\u0647 \u0627\u0644\u0645\u062f\u0648\u0646\u0629\u060c \u0633\u0646\u0633\u062a\u0643\u0634\u0641 \u062a\u0631\u0643\u064a\u0628 \u0648\u062e\u0635\u0627\u0626\u0635 \u0648\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10 \u0648\u0645\u0627 \u0625\u0644\u0649 \u0630\u0644\u0643.&nbsp;<\/p><h2 class=\"wp-block-heading\">\u0645\u0627 \u0647\u0648 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10\u061f<\/h2><p class=\"wp-block-paragraph\">\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10\u060c \u0648\u0627\u0644\u0645\u0639\u0631\u0648\u0641 \u0623\u064a\u0636\u064b\u0627 \u0628\u0627\u0633\u0645 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 304\u060c \u0647\u0648 \u0633\u0628\u064a\u0643\u0629 \u0645\u0643\u0648\u0646\u0629 \u0645\u0646 \u0627\u0644\u062d\u062f\u064a\u062f 72% \u0648\u0627\u0644\u0643\u0631\u0648\u0645 18% \u0648\u0627\u0644\u0646\u064a\u0643\u0644 10%\u060c \u0648\u0627\u0644\u0645\u0639\u0631\u0648\u0641 \u0628\u0634\u0643\u0644\u0647 \u0627\u0644\u0635\u0644\u0628 \u0648\u0645\u0638\u0647\u0631\u0647 \u0627\u0644\u0644\u0627\u0645\u0639 \u0627\u0644\u0645\u0635\u0642\u0648\u0644. \u064a\u0645\u0646\u062d \u0627\u0644\u0643\u0631\u0648\u0645 \u0645\u0642\u0627\u0648\u0645\u0629 \u0644\u0644\u062a\u0622\u0643\u0644\u060c \u0628\u064a\u0646\u0645\u0627 \u064a\u0632\u064a\u062f \u0627\u0644\u0646\u064a\u0643\u0644 \u0645\u0646 \u0627\u0644\u0642\u0648\u0629 \u0648\u0627\u0644\u0635\u0644\u0627\u0628\u0629. \u064a\u062a\u0645 \u0625\u0646\u062a\u0627\u062c \u0647\u0630\u0627 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0639\u0627\u0644\u064a \u0627\u0644\u062c\u0648\u062f\u0629 \u0645\u0646 \u062e\u0644\u0627\u0644 \u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0633\u0627\u062e\u0646\u0629\u060c \u0648\u0647\u0648 \u0645\u062a\u064a\u0646 \u0648\u063a\u064a\u0631 \u062a\u0641\u0627\u0639\u0644\u064a \u0648\u0633\u0647\u0644 \u0627\u0644\u062a\u0646\u0638\u064a\u0641. \u064a\u062a\u0645 \u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0647 \u0641\u064a \u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0637\u0628\u062e \u0648\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0627\u0626\u062f\u0629 \u0648\u0627\u0644\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0637\u0628\u064a\u0629 \u0648\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0635\u0646\u0627\u0639\u064a\u0629 \u0648\u0627\u0644\u0628\u0646\u0627\u0621 \u0648\u0627\u0644\u0645\u062c\u0648\u0647\u0631\u0627\u062a.&nbsp;<\/p><h2 class=\"wp-block-heading\">\u0645\u0627\u0630\u0627 \u064a\u0639\u0646\u064a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10\u061f&nbsp;<\/h2><p class=\"wp-block-paragraph\">\u064a\u0634\u064a\u0631 \u0645\u0635\u0637\u0644\u062d &quot;18\/10&quot; \u0641\u064a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0625\u0644\u0649 \u062a\u0631\u0643\u064a\u0628\u062a\u0647 \u0645\u0646 \u0627\u0644\u0643\u0631\u0648\u0645 18% \u0648\u0627\u0644\u0646\u064a\u0643\u0644 10%. \u064a\u0648\u0641\u0631 \u0627\u0644\u0643\u0631\u0648\u0645 \u0645\u0642\u0627\u0648\u0645\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0648\u064a\u0645\u0646\u0639 \u0627\u0644\u0635\u062f\u0623 \u0648\u0627\u0644\u0628\u0642\u0639 \u0645\u0646 \u062e\u0644\u0627\u0644 \u062a\u0643\u0648\u064a\u0646 \u0637\u0628\u0642\u0629 \u0633\u0637\u062d\u064a\u0629 \u0648\u0627\u0642\u064a\u0629\u060c \u0628\u064a\u0646\u0645\u0627 \u064a\u0639\u0632\u0632 \u0627\u0644\u0646\u064a\u0643\u0644 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644 \u0647\u0630\u0647 \u0648\u064a\u0636\u064a\u0641 \u0627\u0644\u0642\u0648\u0629. \u0647\u0630\u0627 \u0627\u0644\u0645\u0632\u064a\u062c \u064a\u062c\u0639\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10 \u0645\u0642\u0627\u0648\u0645\u064b\u0627 \u0644\u0644\u0635\u062f\u0623 \u0648\u0642\u0648\u064a\u064b\u0627 \u0648\u0645\u062a\u064a\u0646\u064b\u0627 \u0648\u062c\u0630\u0627\u0628\u064b\u0627 \u0628\u0635\u0631\u064a\u064b\u0627\u060c \u0645\u062b\u0627\u0644\u064a\u064b\u0627 \u0644\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0637\u0628\u062e \u0639\u0627\u0644\u064a\u0629 \u0627\u0644\u062c\u0648\u062f\u0629 \u0648\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0627\u0626\u062f\u0629 \u0648\u0627\u0644\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0637\u0628\u064a\u0629\u060c \u0645\u0645\u0627 \u064a\u0636\u0645\u0646 \u0623\u062f\u0627\u0621\u064b \u064a\u062f\u0648\u0645 \u0637\u0648\u064a\u0644\u0627\u064b \u0648\u0645\u0638\u0647\u0631\u064b\u0627 \u0623\u0646\u064a\u0642\u064b\u0627.<\/p><h2 class=\"wp-block-heading\">\u0645\u0627 \u0647\u0648 \u0627\u0644\u062a\u0631\u0643\u064a\u0628 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10\u061f<\/h2><p class=\"wp-block-paragraph\">\u064a\u062a\u0643\u0648\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10 \u0628\u0634\u0643\u0644 \u0623\u0633\u0627\u0633\u064a \u0645\u0646 \u0627\u0644\u0643\u0631\u0648\u0645 18% \u0648\u0627\u0644\u0646\u064a\u0643\u0644 10%\u060c \u0645\u0639 \u0628\u0642\u064a\u0629 \u0627\u0644\u062d\u062f\u064a\u062f \u0648\u0643\u0645\u064a\u0627\u062a \u0635\u063a\u064a\u0631\u0629 \u0645\u0646 \u0627\u0644\u0639\u0646\u0627\u0635\u0631 \u0627\u0644\u0623\u062e\u0631\u0649. \u062a\u0645\u0646\u062d \u0647\u0630\u0647 \u0627\u0644\u062a\u0631\u0643\u064a\u0628\u0629 \u062e\u0635\u0627\u0626\u0635 \u0645\u0645\u064a\u0632\u0629\u060c \u0628\u0645\u0627 \u0641\u064a \u0630\u0644\u0643 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644 \u0627\u0644\u0641\u0627\u0626\u0642\u0629 \u0648\u0627\u0644\u0642\u0648\u0629 \u0648\u0627\u0644\u0645\u062a\u0627\u0646\u0629.<\/p><figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td><strong>\u0639\u0646\u0635\u0631<\/strong><\/td><td><strong>\u0627\u0644\u062a\u0631\u0643\u064a\u0628 (\u0627\u0644\u0648\u0632\u0646 %)<\/strong><\/td><\/tr><tr><td>\u0627\u0644\u0643\u0631\u0648\u0645 (Cr)<\/td><td>18.0-20.0%<\/td><\/tr><tr><td>\u0627\u0644\u0646\u064a\u0643\u0644 (Ni)<\/td><td>8.0-10.5%<\/td><\/tr><tr><td>\u0627\u0644\u0643\u0631\u0628\u0648\u0646 (C)<\/td><td>\u2264 0.08%<\/td><\/tr><tr><td>\u0627\u0644\u0645\u0646\u063a\u0646\u064a\u0632 (Mn)<\/td><td>\u2264 2.00%<\/td><\/tr><tr><td>\u0627\u0644\u0633\u064a\u0644\u064a\u0643\u0648\u0646 (Si)<\/td><td>\u2264 1%<\/td><\/tr><tr><td>\u0627\u0644\u0641\u0648\u0633\u0641\u0648\u0631 (P)<\/td><td>\u2264 0.045%<\/td><\/tr><tr><td>\u0627\u0644\u0643\u0628\u0631\u064a\u062a (S)<\/td><td>\u2264 0.030%<\/td><\/tr><tr><td>\u0627\u0644\u0646\u064a\u062a\u0631\u0648\u062c\u064a\u0646 (\u0646)<\/td><td>\u2264 0.10%<\/td><\/tr><tr><td>\u0627\u0644\u062d\u062f\u064a\u062f (Fe)<\/td><td>\u062a\u0648\u0627\u0632\u0646<\/td><\/tr><\/tbody><\/table><\/figure><h3 class=\"wp-block-heading\">\u0627\u0644\u0643\u0631\u0648\u0645<\/h3><p class=\"wp-block-paragraph\">\u0627\u0644\u0643\u0631\u0648\u0645 \u0636\u0631\u0648\u0631\u064a \u0644\u062c\u0639\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0645\u0642\u0627\u0648\u0645\u064b\u0627 \u0644\u0644\u062a\u0622\u0643\u0644 \u0648\u0627\u0644\u0635\u062f\u0623. \u0641\u064a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10\u060c \u064a\u0634\u0643\u0644 \u0627\u0644\u0643\u0631\u0648\u0645 18% \u0637\u0628\u0642\u0629 \u0631\u0642\u064a\u0642\u0629 \u0645\u0646 \u0623\u0643\u0633\u064a\u062f \u0627\u0644\u0643\u0631\u0648\u0645 \u0639\u0644\u0649 \u0627\u0644\u0633\u0637\u062d \u062a\u0645\u0646\u0639 \u0627\u0644\u0635\u062f\u0623. \u0641\u064a \u062d\u0627\u0644\u0629 \u0627\u0644\u062e\u062f\u0634 \u0623\u0648 \u0627\u0644\u062a\u0644\u0641\u060c \u062a\u0635\u0644\u062d \u0627\u0644\u0637\u0628\u0642\u0629 \u0646\u0641\u0633\u0647\u0627 \u0645\u0646 \u062e\u0644\u0627\u0644 \u062a\u0643\u0648\u064a\u0646 \u0637\u0628\u0642\u0629 \u0648\u0627\u0642\u064a\u0629 \u062c\u062f\u064a\u062f\u0629 \u0645\u0646 \u062e\u0644\u0627\u0644 \u062a\u0641\u0627\u0639\u0644 \u0627\u0644\u0643\u0631\u0648\u0645 \u0645\u0639 \u0627\u0644\u0623\u0643\u0633\u062c\u064a\u0646.&nbsp;<\/p><h3 class=\"wp-block-heading\">\u0627\u0644\u0646\u064a\u0643\u0644<\/h3><p class=\"wp-block-paragraph\">\u064a\u062a\u0645 \u0625\u0636\u0627\u0641\u0629 \u0627\u0644\u0646\u064a\u0643\u0644 \u0644\u062a\u0639\u0632\u064a\u0632 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644 \u0627\u0644\u062a\u064a \u064a\u0648\u0641\u0631\u0647\u0627 \u0627\u0644\u0643\u0631\u0648\u0645. \u0643\u0645\u0627 \u064a\u0639\u0645\u0644 \u0627\u0644\u0646\u064a\u0643\u0644 10% \u0641\u064a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10 \u0639\u0644\u0649 \u062a\u062d\u0633\u064a\u0646 \u0642\u0648\u062a\u0647 \u0648\u0635\u0644\u0627\u0628\u062a\u0647 \u0628\u0634\u0643\u0644 \u0639\u0627\u0645\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647 \u0623\u0643\u062b\u0631 \u0645\u062a\u0627\u0646\u0629 \u0648\u0645\u0642\u0627\u0648\u0645\u0629 \u0644\u0644\u062a\u0644\u0641. \u064a\u0645\u0646\u062d \u0627\u0644\u0646\u064a\u0643\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0645\u0638\u0647\u0631\u064b\u0627 \u0644\u0627\u0645\u0639\u064b\u0627 \u0648\u062c\u0630\u0627\u0628\u064b\u0627\u060c \u0648\u0644\u0647\u0630\u0627 \u0627\u0644\u0633\u0628\u0628 \u063a\u0627\u0644\u0628\u064b\u0627 \u0645\u0627 \u064a\u0633\u062a\u062e\u062f\u0645 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10 \u0641\u064a \u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0637\u0628\u062e \u0648\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0627\u0626\u062f\u0629. \u0627\u0646\u062e\u0641\u0627\u0636 \u0627\u0644\u062a\u0648\u0635\u064a\u0644 \u0627\u0644\u0643\u0647\u0631\u0628\u0627\u0626\u064a \u0648\u0627\u0644\u062d\u0631\u0627\u0631\u064a \u0628\u0633\u0628\u0628 \u0645\u062d\u062a\u0648\u0649 \u0627\u0644\u0643\u0631\u0648\u0645 \u0648\u0627\u0644\u0646\u064a\u0643\u0644 \u0627\u0644\u0623\u0639\u0644\u0649.<\/p><h3 class=\"wp-block-heading\">\u0627\u0644\u062d\u062f\u064a\u062f \u0648\u0627\u0644\u0639\u0646\u0627\u0635\u0631 \u0627\u0644\u0623\u062e\u0631\u0649<\/h3><p class=\"wp-block-paragraph\">\u064a\u062a\u0643\u0648\u0646 \u0628\u0627\u0642\u064a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10 \u0628\u0634\u0643\u0644 \u0623\u0633\u0627\u0633\u064a \u0645\u0646 \u0627\u0644\u062d\u062f\u064a\u062f\u060c \u0625\u0644\u0649 \u062c\u0627\u0646\u0628 \u0643\u0645\u064a\u0627\u062a \u0635\u063a\u064a\u0631\u0629 \u0645\u0646 \u0639\u0646\u0627\u0635\u0631 \u0623\u062e\u0631\u0649 \u0645\u062b\u0644 \u0627\u0644\u0645\u0646\u063a\u0646\u064a\u0632 \u0648\u0627\u0644\u0633\u064a\u0644\u064a\u0643\u0648\u0646 \u0648\u0627\u0644\u0643\u0631\u0628\u0648\u0646. \u062a\u0639\u0645\u0644 \u0647\u0630\u0647 \u0627\u0644\u0639\u0646\u0627\u0635\u0631 \u0627\u0644\u0645\u0636\u0627\u0641\u0629 \u0639\u0644\u0649 \u062a\u062d\u0633\u064a\u0646 \u0639\u0645\u0644\u064a\u0629 \u0627\u0644\u062a\u0635\u0646\u064a\u0639 \u0648\u062a\u0639\u0632\u064a\u0632 \u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u062d\u062f\u062f\u0629. \u0639\u0644\u0649 \u0633\u0628\u064a\u0644 \u0627\u0644\u0645\u062b\u0627\u0644\u060c \u064a\u0639\u0645\u0644 \u0627\u0644\u0645\u0646\u063a\u0646\u064a\u0632 \u0639\u0644\u0649 \u062a\u062d\u0633\u064a\u0646 \u0635\u0644\u0627\u0628\u0629 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0648\u0642\u0648\u062a\u0647\u060c \u0628\u064a\u0646\u0645\u0627 \u064a\u0633\u0627\u0639\u062f \u0627\u0644\u0633\u064a\u0644\u064a\u0643\u0648\u0646 \u0641\u064a \u0625\u0632\u0627\u0644\u0629 \u0627\u0644\u0623\u0643\u0633\u062f\u0629 \u0623\u062b\u0646\u0627\u0621 \u0627\u0644\u0625\u0646\u062a\u0627\u062c.<\/p><h2 class=\"wp-block-heading\">\u0645\u0627 \u0647\u064a \u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10\u061f<\/h2><p class=\"wp-block-paragraph\">\u064a\u062a\u0645\u064a\u0632 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10 \u0628\u0645\u062c\u0645\u0648\u0639\u0629 \u0645\u0646 \u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0645\u062b\u064a\u0631\u0629 \u0644\u0644\u0625\u0639\u062c\u0627\u0628\u060c \u0628\u0645\u0627 \u0641\u064a \u0630\u0644\u0643 \u0627\u0644\u0643\u062b\u0627\u0641\u0629 \u0627\u0644\u0639\u0627\u0644\u064a\u0629\u060c \u0648\u0627\u0644\u062a\u0648\u0635\u064a\u0644 \u0627\u0644\u062d\u0631\u0627\u0631\u064a \u0627\u0644\u0645\u0639\u062a\u062f\u0644\u060c \u0648\u0646\u0642\u0637\u0629 \u0627\u0646\u0635\u0647\u0627\u0631 \u0639\u0627\u0644\u064a\u0629\u060c \u0648\u0627\u0644\u062a\u0645\u062f\u062f \u0627\u0644\u062d\u0631\u0627\u0631\u064a \u0627\u0644\u0645\u0639\u062a\u062f\u0644\u060c \u0648\u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0645\u063a\u0646\u0627\u0637\u064a\u0633\u064a\u0629 \u0627\u0644\u0645\u062a\u063a\u064a\u0631\u0629\u060c \u0648\u0627\u0644\u0645\u062a\u0627\u0646\u0629 \u0648\u0627\u0644\u0642\u0648\u0629 \u0627\u0644\u0645\u062a\u0645\u064a\u0632\u0629\u060c \u0648\u0627\u0644\u062c\u0627\u0630\u0628\u064a\u0629 \u0627\u0644\u062c\u0645\u0627\u0644\u064a\u0629 \u0627\u0644\u0639\u0627\u0644\u064a\u0629\u060c \u0648\u0627\u0644\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u0645\u0645\u062a\u0627\u0632\u0629 \u0644\u062f\u0631\u062c\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u0639\u0627\u0644\u064a\u0629\u060c \u0648\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0633\u062a\u062b\u0646\u0627\u0626\u064a\u0629 \u0644\u0644\u062a\u0622\u0643\u0644\u060c \u0648\u0627\u0644\u0633\u0637\u062d \u063a\u064a\u0631 \u0627\u0644\u062a\u0641\u0627\u0639\u0644\u064a \u0644\u0644\u063a\u0627\u064a\u0629\u060c \u0648\u0633\u0647\u0648\u0644\u0629 \u0627\u0644\u062a\u0646\u0638\u064a\u0641 \u0648\u0627\u0644\u0635\u064a\u0627\u0646\u0629.<\/p><h3 class=\"wp-block-heading\">\u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0641\u064a\u0632\u064a\u0627\u0626\u064a\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10<\/h3><figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td><strong>\u0645\u0644\u0643\u064a\u0629<\/strong><\/td><td><strong>\u0648\u062d\u062f\u0629 \u0627\u0644\u0642\u064a\u0627\u0633 \u0627\u0644\u0645\u062a\u0631\u064a\u0629<\/strong><\/td><td><strong>\u0627\u0644\u0648\u062d\u062f\u0629 \u0627\u0644\u0625\u0645\u0628\u0631\u0627\u0637\u0648\u0631\u064a\u0629<\/strong><\/td><\/tr><tr><td>\u0643\u062b\u0627\u0641\u0629<\/td><td>7.9 \u062c\u0631\u0627\u0645\/\u0633\u06453<\/td><td>0.285 \u0631\u0637\u0644\/\u0628\u0648\u0635\u0629 \u0645\u0643\u0639\u0628\u0629<\/td><\/tr><tr><td>\u0646\u0642\u0637\u0629 \u0627\u0644\u0627\u0646\u0635\u0647\u0627\u0631<\/td><td>1400-1450 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629<\/td><td>2552-2642 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a<\/td><\/tr><tr><td>\u0627\u0644\u0645\u0648\u0635\u0644\u064a\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629<\/td><td>16.2 \u0648\u0627\u0637\/\u0645\u062a\u0631\u00b7\u0643\u0644\u0641\u0646 \u0639\u0646\u062f 100 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629<\/td><td>9.36 \u0648\u062d\u062f\u0629 \u062d\u0631\u0627\u0631\u064a\u0629 \u0628\u0631\u064a\u0637\u0627\u0646\u064a\u0629\/\u0633\u0627\u0639\u0629 \u0642\u062f\u0645 \u0645\u0643\u0639\u0628 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a<\/td><\/tr><tr><td>\u0627\u0644\u062a\u0645\u062f\u062f \u0627\u0644\u062d\u0631\u0627\u0631\u064a<\/td><td>16.5 \u0645\u064a\u0643\u0631\u0648\u0645\u062a\u0631\/\u0645\u062a\u0631\u00b7\u0643<\/td><td>9.17 \u0645\u064a\u0643\u0631\u0648\u0646\/\u0628\u0648\u0635\u0629\u00b7\u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a<\/td><\/tr><tr><td>\u0645\u0639\u0627\u0645\u0644 \u0627\u0644\u0645\u0631\u0648\u0646\u0629<\/td><td>193 \u062c\u064a\u062c\u0627\u0628\u0627\u0633\u0643\u0627\u0644<\/td><td>28 \u00d7 10\u00b3 \u0643\u064a\u0644\u0648 \u0628\u0648\u0635\u0629 \u0645\u0631\u0628\u0639\u0629<\/td><\/tr><\/tbody><\/table><\/figure><h4 class=\"wp-block-heading\">\u0643\u062b\u0627\u0641\u0629 \u0639\u0627\u0644\u064a\u0629<\/h4><p class=\"wp-block-paragraph\">\u062a\u0628\u0644\u063a \u0643\u062b\u0627\u0641\u0629 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10 \u062d\u0648\u0627\u0644\u064a 7.9 \u062c\u0645\/\u0633\u0645\u00b3. \u062a\u0648\u0641\u0631 \u0647\u0630\u0647 \u0627\u0644\u0643\u062b\u0627\u0641\u0629 \u0627\u0644\u0639\u0627\u0644\u064a\u0629 \u0625\u062d\u0633\u0627\u0633\u064b\u0627 \u0642\u0648\u064a\u064b\u0627 \u0648\u062a\u0634\u064a\u0631 \u0625\u0644\u0649 \u0645\u062a\u0627\u0646\u062a\u0647 \u0648\u062c\u0648\u062f\u062a\u0647\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647 \u0645\u0627\u062f\u0629 \u0645\u0641\u0636\u0644\u0629 \u0644\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0637\u0628\u062e \u0648\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0627\u0626\u062f\u0629 \u0627\u0644\u0631\u0627\u0642\u064a\u0629.<\/p><h4 class=\"wp-block-heading\">\u0627\u0644\u0645\u0648\u0635\u0644\u064a\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629 \u0627\u0644\u0645\u0639\u062a\u062f\u0644\u0629<\/h4><p class=\"wp-block-paragraph\">\u064a\u062a\u0645\u062a\u0639 \u0647\u0630\u0627 \u0627\u0644\u0646\u0648\u0639 \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0628\u0645\u0648\u0635\u0644\u064a\u0629 \u062d\u0631\u0627\u0631\u064a\u0629 \u062a\u0628\u0644\u063a \u062d\u0648\u0627\u0644\u064a 16 \u0648\u0627\u0637\/\u0645\u062a\u0631\u00b7\u0643\u0644\u0641\u0646. \u062a\u0633\u0645\u062d \u0647\u0630\u0647 \u0627\u0644\u0645\u0648\u0635\u0644\u064a\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629 \u0627\u0644\u0645\u0639\u062a\u062f\u0644\u0629 \u0644\u0647 \u0628\u062a\u0648\u0635\u064a\u0644 \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0628\u0643\u0641\u0627\u0621\u0629 \u062f\u0648\u0646 \u0627\u0631\u062a\u0641\u0627\u0639 \u062f\u0631\u062c\u0629 \u062d\u0631\u0627\u0631\u062a\u0647\u060c \u0648\u0647\u0648 \u0623\u0645\u0631 \u0628\u0627\u0644\u063a \u0627\u0644\u0623\u0647\u0645\u064a\u0629 \u0644\u0623\u0648\u0627\u0646\u064a \u0627\u0644\u0637\u0647\u064a \u0627\u0644\u062a\u064a \u062a\u062d\u062a\u0627\u062c \u0625\u0644\u0649 \u0627\u0644\u062d\u0641\u0627\u0638 \u0639\u0644\u0649 \u062f\u0631\u062c\u0627\u062a \u062d\u0631\u0627\u0631\u0629 \u0637\u0647\u064a \u062b\u0627\u0628\u062a\u0629.<\/p><h4 class=\"wp-block-heading\">\u0646\u0642\u0637\u0629 \u0627\u0646\u0635\u0647\u0627\u0631 \u0639\u0627\u0644\u064a\u0629<\/h4><p class=\"wp-block-paragraph\">\u064a\u062a\u0645\u062a\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10 \u0628\u0646\u0642\u0637\u0629 \u0627\u0646\u0635\u0647\u0627\u0631 \u0639\u0627\u0644\u064a\u0629 \u062a\u0628\u0644\u063a \u062d\u0648\u0627\u0644\u064a 1400-1450 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629. \u0647\u0630\u0647 \u0627\u0644\u062e\u0627\u0635\u064a\u0629 \u062a\u062c\u0639\u0644\u0647 \u0645\u062b\u0627\u0644\u064a\u064b\u0627 \u0644\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0630\u0627\u062a \u062f\u0631\u062c\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u0639\u0627\u0644\u064a\u0629 \u0645\u062b\u0644 \u0627\u0644\u0623\u0641\u0631\u0627\u0646 \u0648\u0627\u0644\u0634\u0648\u0627\u064a\u0627\u062a.<\/p><h4 class=\"wp-block-heading\">\u0627\u0644\u062a\u0645\u062f\u062f \u0627\u0644\u062d\u0631\u0627\u0631\u064a \u0627\u0644\u0645\u0639\u062a\u062f\u0644<\/h4><p class=\"wp-block-paragraph\">\u0645\u0639 \u0645\u0639\u0627\u0645\u0644 \u062a\u0645\u062f\u062f \u062d\u0631\u0627\u0631\u064a \u064a\u0628\u0644\u063a \u062d\u0648\u0627\u0644\u064a 16.5 \u0645\u064a\u0643\u0631\u0648\u0645\u062a\u0631\/\u0645\u062a\u0631\u00b7\u0643\u060c \u064a\u062a\u0645\u062f\u062f \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10 \u0628\u0634\u0643\u0644 \u0645\u0639\u062a\u062f\u0644 \u0639\u0646\u062f \u062a\u0633\u062e\u064a\u0646\u0647. \u0648\u064a\u0628\u0644\u063a \u0645\u0639\u062f\u0644 \u062a\u0645\u062f\u062f\u0647 \u0627\u0644\u062d\u0631\u0627\u0631\u064a 16.5 \u00d7 10^-6 \u0645\u0645\/\u0645\u062a\u0631\/\u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \u0639\u0646\u062f 20 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629. \u0648\u0647\u0630\u0627 \u0645\u0647\u0645 \u0644\u0623\u0648\u0627\u0646\u064a \u0627\u0644\u0637\u0647\u064a \u0648\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0623\u062e\u0631\u0649 \u0627\u0644\u062a\u064a \u062a\u062d\u062a\u0627\u062c \u0625\u0644\u0649 \u0627\u0644\u062d\u0641\u0627\u0638 \u0639\u0644\u0649 \u0634\u0643\u0644\u0647\u0627 \u0648\u0633\u0644\u0627\u0645\u062a\u0647\u0627 \u0627\u0644\u0628\u0646\u064a\u0648\u064a\u0629 \u062a\u062d\u062a \u062f\u0631\u062c\u0627\u062a \u062d\u0631\u0627\u0631\u0629 \u0645\u062a\u0641\u0627\u0648\u062a\u0629.<\/p><h4 class=\"wp-block-heading\">\u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0645\u063a\u0646\u0627\u0637\u064a\u0633\u064a\u0629 \u0627\u0644\u0645\u062a\u063a\u064a\u0631\u0629<\/h4><p class=\"wp-block-paragraph\">\u0639\u0644\u0649 \u0627\u0644\u0631\u063a\u0645 \u0645\u0646 \u0623\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10 \u063a\u064a\u0631 \u0645\u063a\u0646\u0627\u0637\u064a\u0633\u064a \u0628\u0634\u0643\u0644 \u0639\u0627\u0645\u060c \u0625\u0644\u0627 \u0623\u0646\u0647 \u064a\u0645\u0643\u0646 \u0623\u0646 \u064a\u0638\u0647\u0631 \u0628\u0639\u0636 \u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0645\u063a\u0646\u0627\u0637\u064a\u0633\u064a\u0629 \u0628\u0639\u062f \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0628\u0627\u0631\u062f\u0629. \u0648\u0647\u0630\u0627 \u064a\u062c\u0639\u0644\u0647 \u0645\u062a\u0639\u062f\u062f \u0627\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0627\u062a \u0644\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u062a\u064a \u0642\u062f \u062a\u062a\u0637\u0644\u0628 \u062e\u0635\u0627\u0626\u0635 \u063a\u064a\u0631 \u0645\u063a\u0646\u0627\u0637\u064a\u0633\u064a\u0629 \u0648\u062e\u0635\u0627\u0626\u0635 \u0645\u063a\u0646\u0627\u0637\u064a\u0633\u064a\u0629 \u0637\u0641\u064a\u0641\u0629.<\/p><h3 class=\"wp-block-heading\">\u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0645\u064a\u0643\u0627\u0646\u064a\u0643\u064a\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10<\/h3><figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td><strong>\u0645\u0644\u0643\u064a\u0627\u062a<\/strong><\/td><td><strong>\u0645\u062a\u0631\u064a<\/strong><\/td><td><strong>\u0625\u0645\u0628\u0631\u0627\u0637\u0648\u0631\u064a<\/strong><\/td><\/tr><tr><td>\u0642\u0648\u0629 \u0627\u0644\u0634\u062f<\/td><td>515-750 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644<\/td><td>74.7-108.8 \u0643\u064a\u0644\u0648 \u0628\u0648\u0635\u0629 \u0645\u0631\u0628\u0639\u0629<\/td><\/tr><tr><td>\u0642\u0648\u0629 \u0627\u0644\u062e\u0636\u0648\u0639<\/td><td>215 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644<\/td><td>31.2 \u0643\u064a\u0644\u0648 \u0628\u0627\u064a\u062a \u0641\u064a \u0627\u0644\u0628\u0648\u0635\u0629 \u0627\u0644\u0645\u0631\u0628\u0639\u0629<\/td><\/tr><tr><td>\u0635\u0644\u0627\u0628\u0629 \u0641\u064a\u0643\u0631\u0632<\/td><td>129 \u0641\u0648\u0644\u062a \u0639\u0627\u0644\u064a<\/td><td>129 \u0641\u0648\u0644\u062a \u0639\u0627\u0644\u064a<\/td><\/tr><tr><td>\u0635\u0644\u0627\u0628\u0629 \u0628\u0631\u064a\u0646\u064a\u0644<\/td><td>123 \u0647\u0640 \u0628<\/td><td>123 \u0647\u0640 \u0628<\/td><\/tr><tr><td>\u0635\u0644\u0627\u0628\u0629 \u0631\u0648\u0643\u0648\u064a\u0644<\/td><td>\u062870-\u062890<\/td><td>\u062870-\u062890<\/td><\/tr><tr><td>\u0627\u0633\u062a\u0637\u0627\u0644\u0629<\/td><td>40%<\/td><td>40%<\/td><\/tr><tr><td>\u0645\u0639\u0627\u0645\u0644 \u0627\u0644\u0645\u0631\u0648\u0646\u0629<\/td><td>193 \u062c\u064a\u062c\u0627\u0628\u0627\u0633\u0643\u0627\u0644<\/td><td>28 \u00d7 10\u00b3 \u0643\u064a\u0644\u0648 \u0628\u0648\u0635\u0629 \u0645\u0631\u0628\u0639\u0629<\/td><\/tr><\/tbody><\/table><\/figure><h3 class=\"wp-block-heading\">\u0645\u062a\u0627\u0646\u0629 \u0648\u0642\u0648\u0629 \u0645\u062a\u0645\u064a\u0632\u0629<\/h3><p class=\"wp-block-paragraph\">\u062a\u0639\u0645\u0644 \u0625\u0636\u0627\u0641\u0629 \u0627\u0644\u0646\u064a\u0643\u0644 10% \u0639\u0644\u0649 \u062a\u0639\u0632\u064a\u0632 \u0627\u0644\u0642\u0648\u0629 \u0648\u0627\u0644\u0645\u062a\u0627\u0646\u0629 \u0627\u0644\u0634\u0627\u0645\u0644\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10. \u062a\u0642\u0644 \u0627\u062d\u062a\u0645\u0627\u0644\u064a\u0629 \u062a\u0634\u0642\u0642 \u0647\u0630\u0647 \u0627\u0644\u0645\u0627\u062f\u0629 \u0623\u0648 \u0643\u0633\u0631\u0647\u0627 \u062a\u062d\u062a \u0627\u0644\u0636\u063a\u0637\u060c \u0645\u0645\u0627 \u064a\u0636\u0645\u0646 \u0623\u0646 \u0627\u0644\u0645\u0646\u062a\u062c\u0627\u062a \u0627\u0644\u0645\u0635\u0646\u0648\u0639\u0629 \u0645\u0646\u0647\u0627 \u062a\u062a\u0645\u062a\u0639 \u0628\u0639\u0645\u0631 \u0627\u0641\u062a\u0631\u0627\u0636\u064a \u0637\u0648\u064a\u0644 \u0648\u064a\u0645\u0643\u0646\u0647\u0627 \u062a\u062d\u0645\u0644 \u0627\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u064a\u0648\u0645\u064a.<\/p><h4 class=\"wp-block-heading\">\u0645\u0642\u0627\u0648\u0645\u0629 \u0645\u0645\u062a\u0627\u0632\u0629 \u0644\u062f\u0631\u062c\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u0639\u0627\u0644\u064a\u0629<\/h4><p class=\"wp-block-paragraph\">\u064a\u0645\u0643\u0646 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10 \u0623\u0646 \u064a\u062a\u062d\u0645\u0644 \u062f\u0631\u062c\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u0639\u0627\u0644\u064a\u0629 \u062f\u0648\u0646 \u0623\u0646 \u064a\u0641\u0642\u062f \u0642\u0648\u062a\u0647 \u0623\u0648 \u0633\u0644\u0627\u0645\u062a\u0647. \u0648\u0647\u0630\u0627 \u064a\u062c\u0639\u0644\u0647 \u0645\u0646\u0627\u0633\u0628\u064b\u0627 \u0644\u0623\u0648\u0627\u0646\u064a \u0627\u0644\u0637\u0647\u064a \u0648\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0623\u062e\u0631\u0649 \u062d\u064a\u062b \u064a\u0643\u0648\u0646 \u0627\u0644\u062a\u0639\u0631\u0636 \u0644\u0644\u062d\u0631\u0627\u0631\u0629 \u0623\u0645\u0631\u064b\u0627 \u0634\u0627\u0626\u0639\u064b\u0627. \u064a\u062d\u062a\u0641\u0638 \u0628\u0634\u0643\u0644\u0647 \u0648\u062e\u0635\u0627\u0626\u0635\u0647 \u062d\u062a\u0649 \u062a\u062d\u062a \u0627\u0644\u062a\u0633\u062e\u064a\u0646 \u0644\u0641\u062a\u0631\u0627\u062a \u0637\u0648\u064a\u0644\u0629\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647 \u0645\u0627\u062f\u0629 \u0645\u0648\u062b\u0648\u0642\u0629 \u0644\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629 \u0627\u0644\u0645\u062e\u062a\u0644\u0641\u0629.<\/p><h3 class=\"wp-block-heading\">\u062e\u0635\u0627\u0626\u0635 \u0623\u062e\u0631\u0649<\/h3><h4 class=\"wp-block-heading\">\u062c\u0627\u0630\u0628\u064a\u0629 \u062c\u0645\u0627\u0644\u064a\u0629 \u0639\u0627\u0644\u064a\u0629<\/h4><p class=\"wp-block-paragraph\">\u064a\u062a\u0645\u064a\u0632 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10 \u0628\u0645\u0638\u0647\u0631\u0647 \u0627\u0644\u0644\u0627\u0645\u0639 \u0627\u0644\u0645\u0635\u0642\u0648\u0644. \u0643\u0645\u0627 \u064a\u0648\u0641\u0631 \u0645\u062d\u062a\u0648\u0627\u0647 \u0627\u0644\u0639\u0627\u0644\u064a \u0645\u0646 \u0627\u0644\u0646\u064a\u0643\u0644 \u0644\u0645\u0633\u0629 \u0646\u0647\u0627\u0626\u064a\u0629 \u0646\u0627\u0639\u0645\u0629 \u0648\u062c\u0630\u0627\u0628\u0629\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647 \u0645\u062b\u0627\u0644\u064a\u064b\u0627 \u0644\u0644\u0623\u062c\u0647\u0632\u0629 \u0627\u0644\u0645\u0637\u0628\u062e\u064a\u0629 \u0627\u0644\u0631\u0627\u0642\u064a\u0629 \u0648\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0627\u0626\u062f\u0629 \u0648\u0627\u0644\u0639\u0646\u0627\u0635\u0631 \u0627\u0644\u0632\u062e\u0631\u0641\u064a\u0629. \u0643\u0645\u0627 \u064a\u0636\u0641\u064a \u0645\u0638\u0647\u0631\u0647 \u0627\u0644\u0623\u0646\u064a\u0642 \u0644\u0645\u0633\u0629 \u0645\u0646 \u0627\u0644\u0623\u0646\u0627\u0642\u0629 \u0639\u0644\u0649 \u0623\u064a \u0645\u0643\u0627\u0646.<\/p><h4 class=\"wp-block-heading\">\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0633\u062a\u062b\u0646\u0627\u0626\u064a\u0629 \u0644\u0644\u062a\u0622\u0643\u0644<\/h4><p class=\"wp-block-paragraph\">\u064a\u062a\u0645\u064a\u0632 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10 \u0628\u0645\u0642\u0627\u0648\u0645\u0629 \u0639\u0627\u0644\u064a\u0629 \u0644\u0644\u0635\u062f\u0623 \u0648\u0627\u0644\u062a\u0622\u0643\u0644 \u0628\u0633\u0628\u0628 \u0646\u0633\u0628\u0629 \u0627\u0644\u0643\u0631\u0648\u0645 \u0627\u0644\u0639\u0627\u0644\u064a\u0629 \u0641\u064a\u0647. \u064a\u0634\u0643\u0644 \u0627\u0644\u0643\u0631\u0648\u0645 18% \u0637\u0628\u0642\u0629 \u0623\u0643\u0633\u064a\u062f \u0648\u0627\u0642\u064a\u0629 \u0639\u0644\u0649 \u0627\u0644\u0633\u0637\u062d\u060c \u0645\u0645\u0627 \u064a\u0645\u0646\u0639 \u0627\u0644\u0635\u062f\u0623 \u0648\u064a\u062d\u0627\u0641\u0638 \u0639\u0644\u0649 \u0633\u0644\u0627\u0645\u0629 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u062d\u062a\u0649 \u0641\u064a \u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u0631\u0637\u0628\u0629 \u0648\u0627\u0644\u0642\u0627\u0633\u064a\u0629. \u0648\u0647\u0630\u0627 \u064a\u062c\u0639\u0644\u0647 \u0645\u062b\u0627\u0644\u064a\u064b\u0627 \u0644\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0637\u0628\u062e \u0648\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0627\u0626\u062f\u0629 \u0648\u0627\u0644\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0637\u0628\u064a\u0629 \u0627\u0644\u062a\u064a \u062a\u062a\u0639\u0631\u0636 \u0644\u0644\u0631\u0637\u0648\u0628\u0629 \u0628\u0634\u0643\u0644 \u0645\u062a\u0643\u0631\u0631.<\/p><p class=\"wp-block-paragraph\">\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 304 \u0639\u0631\u0636\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0648\u0627\u0644\u062a\u0622\u0643\u0644 \u0627\u0644\u0646\u0627\u062a\u062c \u0639\u0646 \u0627\u0644\u0625\u062c\u0647\u0627\u062f \u0641\u064a \u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u0643\u0644\u0648\u0631\u064a\u062f\u064a\u0629. \u0648\u0641\u064a \u0627\u0644\u0638\u0631\u0648\u0641 \u0627\u0644\u0623\u0643\u062b\u0631 \u0642\u0633\u0648\u0629 \u062d\u064a\u062b \u064a\u0643\u0648\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 304 \u0639\u0631\u0636\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0648\u0627\u0644\u062a\u0622\u0643\u0644 \u0627\u0644\u0646\u0627\u062a\u062c \u0639\u0646 \u0627\u0644\u0634\u0642\u0648\u0642 \u0628\u0633\u0628\u0628 \u0627\u0644\u0643\u0644\u0648\u0631\u064a\u062f\u0627\u062a \u0623\u0648 \u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u062d\u0645\u0636\u064a\u0629\u060c \u063a\u0627\u0644\u0628\u064b\u0627 \u0645\u0627 \u064a\u062a\u0645 \u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 316 \u0628\u062f\u0644\u0627\u064b \u0645\u0646\u0647.<\/p><h4 class=\"wp-block-heading\">\u0633\u0637\u062d \u063a\u064a\u0631 \u062a\u0641\u0627\u0639\u0644\u064a \u0628\u062f\u0631\u062c\u0629 \u0643\u0628\u064a\u0631\u0629<\/h4><p class=\"wp-block-paragraph\">\u0645\u0646 \u0623\u0647\u0645 \u0645\u0645\u064a\u0632\u0627\u062a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10 \u0647\u0648 \u0633\u0637\u062d\u0647 \u063a\u064a\u0631 \u0627\u0644\u0645\u062a\u0641\u0627\u0639\u0644. \u0641\u0639\u0644\u0649 \u0639\u0643\u0633 \u0627\u0644\u0645\u0639\u0627\u062f\u0646 \u0627\u0644\u0623\u062e\u0631\u0649\u060c \u0644\u0627 \u064a\u062a\u0641\u0627\u0639\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10 \u0645\u0639 \u0627\u0644\u0623\u0637\u0639\u0645\u0629 \u0627\u0644\u062d\u0645\u0636\u064a\u0629 \u0623\u0648 \u0627\u0644\u0642\u0644\u0648\u064a\u0629\u060c \u0645\u0645\u0627 \u064a\u0636\u0645\u0646 \u0639\u062f\u0645 \u062a\u0623\u062b\u0631 \u0637\u0639\u0645 \u0648\u062c\u0648\u062f\u0629 \u0627\u0644\u0637\u0639\u0627\u0645. \u0648\u0647\u0630\u0647 \u0627\u0644\u062e\u0627\u0635\u064a\u0629 \u0645\u0647\u0645\u0629 \u062c\u062f\u064b\u0627 \u0644\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0637\u0628\u062e \u0648\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0627\u0626\u062f\u0629 \u0627\u0644\u062a\u064a \u062a\u0644\u0627\u0645\u0633 \u0627\u0644\u0637\u0639\u0627\u0645 \u0628\u0634\u0643\u0644 \u0645\u0628\u0627\u0634\u0631.<\/p><h4 class=\"wp-block-heading\">\u0633\u0647\u0644\u0629 \u0627\u0644\u062a\u0646\u0638\u064a\u0641 \u0648\u0627\u0644\u0635\u064a\u0627\u0646\u0629<\/h4><p class=\"wp-block-paragraph\">\u0645\u0646 \u0627\u0644\u0633\u0647\u0644 \u062a\u0646\u0638\u064a\u0641\u0647 \u0648\u0635\u064a\u0627\u0646\u062a\u0647\u060c \u0643\u0645\u0627 \u0623\u0646\u0647 \u0622\u0645\u0646 \u0644\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0641\u064a \u063a\u0633\u0627\u0644\u0629 \u0627\u0644\u0623\u0637\u0628\u0627\u0642 \u0648\u064a\u0645\u0643\u0646 \u063a\u0633\u0644\u0647 \u0628\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u0645\u0646\u0638\u0641\u0627\u062a \u0627\u0644\u0645\u0646\u0632\u0644\u064a\u0629 \u0627\u0644\u0639\u0627\u062f\u064a\u0629 \u062f\u0648\u0646 \u0627\u0644\u0625\u0636\u0631\u0627\u0631 \u0628\u0633\u0637\u062d\u0647. \u0643\u0645\u0627 \u062a\u0636\u0645\u0646 \u0642\u062f\u0631\u062a\u0647 \u0639\u0644\u0649 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u0628\u0642\u0639 \u0648\u0628\u0635\u0645\u0627\u062a \u0627\u0644\u0623\u0635\u0627\u0628\u0639 \u0628\u0642\u0627\u0621\u0647 \u0628\u0645\u0638\u0647\u0631 \u062c\u062f\u064a\u062f \u0628\u0623\u0642\u0644 \u062c\u0647\u062f.<\/p><h2 class=\"wp-block-heading\">\u0645\u0627 \u0647\u064a \u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10\u061f<\/h2><p class=\"wp-block-paragraph\">\u064a\u064f\u0633\u062a\u062e\u062f\u0645 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10 \u0639\u0644\u0649 \u0646\u0637\u0627\u0642 \u0648\u0627\u0633\u0639 \u0646\u0638\u0631\u064b\u0627 \u0644\u062e\u0635\u0627\u0626\u0635\u0647 \u0627\u0644\u0627\u0633\u062a\u062b\u0646\u0627\u0626\u064a\u0629. \u0648\u062a\u062a\u0631\u0627\u0648\u062d \u062a\u0637\u0628\u064a\u0642\u0627\u062a\u0647 \u0645\u0646 \u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0637\u0628\u062e \u0648\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0627\u0626\u062f\u0629 \u0625\u0644\u0649 \u0627\u0644\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0637\u0628\u064a\u0629 \u0648\u0627\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0627\u062a \u0627\u0644\u0635\u0646\u0627\u0639\u064a\u0629 \u0648\u0627\u0644\u0628\u0646\u0627\u0621 \u0648\u062d\u062a\u0649 \u0627\u0644\u0645\u062c\u0648\u0647\u0631\u0627\u062a \u0648\u0627\u0644\u0623\u0632\u064a\u0627\u0621.<\/p><h3 class=\"wp-block-heading\">\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0637\u0628\u062e \u0648\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0627\u0626\u062f\u0629<\/h3><p class=\"wp-block-paragraph\">\u064a\u064f\u0639\u062f \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10 \u062e\u064a\u0627\u0631\u064b\u0627 \u0645\u0641\u0636\u0644\u064b\u0627 \u0644\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0637\u0628\u062e \u0648\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0627\u0626\u062f\u0629 \u0639\u0627\u0644\u064a\u0629 \u0627\u0644\u062c\u0648\u062f\u0629. \u062a\u0636\u0645\u0646 \u0645\u0642\u0627\u0648\u0645\u062a\u0647 \u0627\u0644\u0645\u0645\u062a\u0627\u0632\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0628\u0642\u0627\u0621 \u0627\u0644\u0623\u0648\u0627\u0646\u064a \u062e\u0627\u0644\u064a\u0629 \u0645\u0646 \u0627\u0644\u0635\u062f\u0623\u060c \u062d\u062a\u0649 \u0645\u0639 \u0627\u0644\u063a\u0633\u064a\u0644 \u0627\u0644\u0645\u062a\u0643\u0631\u0631. \u062a\u062c\u0639\u0644\u0647 \u0645\u062a\u0627\u0646\u0629 \u0627\u0644\u0645\u0627\u062f\u0629 \u0648\u0642\u0648\u062a\u0647\u0627 \u0645\u062b\u0627\u0644\u064a\u064b\u0627 \u0644\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u064a\u0648\u0645\u064a\u060c \u0628\u064a\u0646\u0645\u0627 \u064a\u0636\u0645\u0646 \u0633\u0637\u062d\u0647 \u063a\u064a\u0631 \u0627\u0644\u062a\u0641\u0627\u0639\u0644\u064a \u0639\u062f\u0645 \u062a\u063a\u064a\u064a\u0631 \u0646\u0643\u0647\u0627\u062a \u0627\u0644\u0637\u0639\u0627\u0645. \u064a\u0636\u064a\u0641 \u0645\u0638\u0647\u0631\u0647 \u0627\u0644\u0645\u0635\u0642\u0648\u0644 \u0627\u0644\u0644\u0627\u0645\u0639 \u0644\u0645\u0633\u0629 \u0645\u0646 \u0627\u0644\u0623\u0646\u0627\u0642\u0629 \u0625\u0644\u0649 \u0623\u064a \u0645\u0637\u0628\u062e.<\/p><h3 class=\"wp-block-heading\">\u0627\u0644\u0623\u062c\u0647\u0632\u0629 \u0648\u0627\u0644\u0645\u0639\u062f\u0627\u062a \u0627\u0644\u0637\u0628\u064a\u0629<\/h3><p class=\"wp-block-paragraph\">\u0625\u0646 \u0627\u0644\u0635\u0641\u0627\u062a \u0627\u0644\u0635\u062d\u064a\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10 \u062a\u062c\u0639\u0644\u0647 \u0645\u062b\u0627\u0644\u064a\u064b\u0627 \u0644\u0644\u0623\u062f\u0648\u0627\u062a \u0648\u0627\u0644\u0645\u0639\u062f\u0627\u062a \u0627\u0644\u0637\u0628\u064a\u0629. \u0641\u0633\u0637\u062d\u0647 \u0627\u0644\u0623\u0645\u0644\u0633 \u063a\u064a\u0631 \u0627\u0644\u0645\u0633\u0627\u0645\u064a \u0644\u0627 \u064a\u0624\u0648\u064a \u0627\u0644\u0628\u0643\u062a\u064a\u0631\u064a\u0627\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644 \u062a\u0639\u0642\u064a\u0645\u0647 \u0648\u0635\u064a\u0627\u0646\u062a\u0647 \u0623\u0645\u0631\u064b\u0627 \u0633\u0647\u0644\u0627\u064b. \u063a\u0627\u0644\u0628\u064b\u0627 \u0645\u0627 \u062a\u0633\u062a\u062e\u062f\u0645 \u0627\u0644\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u062c\u0631\u0627\u062d\u064a\u0629 \u0648\u0623\u062f\u0648\u0627\u062a \u0637\u0628 \u0627\u0644\u0623\u0633\u0646\u0627\u0646 \u0648\u0645\u0639\u062f\u0627\u062a \u0627\u0644\u0645\u0633\u062a\u0634\u0641\u064a\u0627\u062a \u0647\u0630\u0627 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0646\u0638\u0631\u064b\u0627 \u0644\u0642\u0648\u062a\u0647 \u0648\u0645\u062a\u0627\u0646\u062a\u0647 \u0648\u0645\u0642\u0627\u0648\u0645\u062a\u0647 \u0644\u0644\u062a\u0622\u0643\u0644\u060c \u0645\u0645\u0627 \u064a\u0636\u0645\u0646 \u0623\u062f\u0627\u0621\u064b \u0637\u0648\u064a\u0644 \u0627\u0644\u0623\u0645\u062f \u0641\u064a \u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u0635\u0639\u0628\u0629.<\/p><h3 class=\"wp-block-heading\">\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0635\u0646\u0627\u0639\u064a\u0629<\/h3><p class=\"wp-block-paragraph\">\u0641\u064a \u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u0635\u0646\u0627\u0639\u064a\u0629\u060c \u064a\u0641\u0636\u0644 \u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10 \u0644\u0642\u0648\u062a\u0647 \u0648\u0645\u062a\u0627\u0646\u062a\u0647 \u0648\u0645\u0642\u0627\u0648\u0645\u062a\u0647 \u0644\u0644\u062a\u0622\u0643\u0644. \u0648\u064a\u064f\u0633\u062a\u062e\u062f\u0645 \u0641\u064a \u062a\u0635\u0646\u064a\u0639 \u0623\u062c\u0632\u0627\u0621 \u0627\u0644\u0622\u0644\u0627\u062a \u0648\u0627\u0644\u0623\u062f\u0648\u0627\u062a \u0648\u0627\u0644\u0645\u0639\u062f\u0627\u062a \u0627\u0644\u062a\u064a \u064a\u062c\u0628 \u0623\u0646 \u062a\u062a\u062d\u0645\u0644 \u0627\u0644\u0638\u0631\u0648\u0641 \u0627\u0644\u0642\u0627\u0633\u064a\u0629 \u0648\u0627\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u0645\u0643\u062b\u0641. \u0643\u0645\u0627 \u0623\u0646 \u0645\u0642\u0627\u0648\u0645\u062a\u0647 \u0644\u0644\u062a\u0641\u0627\u0639\u0644\u0627\u062a \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629 \u0648\u0627\u0633\u062a\u0642\u0631\u0627\u0631\u0647 \u0641\u064a \u062f\u0631\u062c\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u0639\u0627\u0644\u064a\u0629 \u064a\u062c\u0639\u0644\u0647 \u0645\u062b\u0627\u0644\u064a\u064b\u0627 \u0644\u0635\u0646\u0627\u0639\u0627\u062a \u0645\u062a\u0646\u0648\u0639\u0629\u060c \u0645\u062b\u0644 \u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0623\u063a\u0630\u064a\u0629 \u0648\u0627\u0644\u062a\u0635\u0646\u064a\u0639 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a \u0648\u0627\u0644\u0628\u062a\u0631\u0648\u0643\u064a\u0645\u0627\u0648\u064a\u0627\u062a.<\/p><h3 class=\"wp-block-heading\">\u0627\u0644\u0628\u0646\u0627\u0621 \u0648\u0627\u0644\u0639\u0645\u0627\u0631\u0629<\/h3><p class=\"wp-block-paragraph\">\u0643\u0645\u0627 \u0623\u0646\u0647\u0627 \u062a\u0633\u062a\u062e\u062f\u0645 \u0639\u0644\u0649 \u0646\u0637\u0627\u0642 \u0648\u0627\u0633\u0639 \u0641\u064a \u0627\u0644\u0628\u0646\u0627\u0621 \u0648\u0627\u0644\u0647\u0646\u062f\u0633\u0629 \u0627\u0644\u0645\u0639\u0645\u0627\u0631\u064a\u0629. \u0625\u0646 \u062c\u0627\u0630\u0628\u064a\u062a\u0647\u0627 \u0627\u0644\u0628\u0635\u0631\u064a\u0629\u060c \u0625\u0644\u0649 \u062c\u0627\u0646\u0628 \u0645\u062a\u0627\u0646\u062a\u0647\u0627 \u0648\u0645\u0642\u0627\u0648\u0645\u062a\u0647\u0627 \u0644\u0644\u0635\u062f\u0623\u060c \u062a\u062c\u0639\u0644\u0647\u0627 \u062e\u064a\u0627\u0631\u064b\u0627 \u0645\u062b\u0627\u0644\u064a\u064b\u0627 \u0644\u0644\u0645\u0643\u0648\u0646\u0627\u062a \u0627\u0644\u0647\u064a\u0643\u0644\u064a\u0629 \u0648\u0627\u0644\u0643\u0633\u0648\u0629 \u0648\u0627\u0644\u062f\u0631\u0627\u0628\u0632\u064a\u0646 \u0648\u0627\u0644\u0639\u0646\u0627\u0635\u0631 \u0627\u0644\u0632\u062e\u0631\u0641\u064a\u0629. \u0641\u0647\u064a \u062a\u0648\u0641\u0631 \u0643\u0644\u064b\u0627 \u0645\u0646 \u0627\u0644\u0648\u0638\u064a\u0641\u0629 \u0648\u0627\u0644\u062c\u0627\u0630\u0628\u064a\u0629 \u0627\u0644\u0628\u0635\u0631\u064a\u0629\u060c \u0645\u0645\u0627 \u064a\u0633\u0627\u0647\u0645 \u0641\u064a \u0637\u0648\u0644 \u0639\u0645\u0631 \u0627\u0644\u0645\u0628\u0627\u0646\u064a \u0648\u0627\u0644\u0647\u064a\u0627\u0643\u0644 \u0648\u062c\u0645\u0627\u0644\u0647\u0627.<\/p><h3 class=\"wp-block-heading\">\u0627\u0644\u0645\u062c\u0648\u0647\u0631\u0627\u062a \u0648\u0627\u0644\u0623\u0632\u064a\u0627\u0621<\/h3><p class=\"wp-block-paragraph\">\u0625\u0646 \u0627\u0644\u0644\u0645\u0633\u0629 \u0627\u0644\u0646\u0647\u0627\u0626\u064a\u0629 \u0627\u0644\u062c\u0630\u0627\u0628\u0629 \u0648\u0627\u0644\u0644\u0627\u0645\u0639\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10\u060c \u0625\u0644\u0649 \u062c\u0627\u0646\u0628 \u0645\u062a\u0627\u0646\u062a\u0647\u060c \u062a\u062c\u0639\u0644\u0647 \u0645\u0627\u062f\u0629 \u0634\u0627\u0626\u0639\u0629 \u0641\u064a \u0635\u0646\u0627\u0639\u0629 \u0627\u0644\u0645\u062c\u0648\u0647\u0631\u0627\u062a \u0648\u0625\u0643\u0633\u0633\u0648\u0627\u0631\u0627\u062a \u0627\u0644\u0645\u0648\u0636\u0629. \u0641\u0647\u0648 \u0644\u0627 \u064a\u0628\u0647\u062a \u0623\u0648 \u064a\u062a\u0622\u0643\u0644\u060c \u0645\u0645\u0627 \u064a\u0636\u0645\u0646 \u0628\u0642\u0627\u0621 \u0627\u0644\u0642\u0637\u0639 \u062c\u0645\u064a\u0644\u0629 \u0628\u0645\u0631\u0648\u0631 \u0627\u0644\u0648\u0642\u062a. \u0643\u0645\u0627 \u0623\u0646 \u062e\u0635\u0627\u0626\u0635\u0647 \u0627\u0644\u0645\u0636\u0627\u062f\u0629 \u0644\u0644\u062d\u0633\u0627\u0633\u064a\u0629 \u062a\u062c\u0639\u0644\u0647 \u0645\u0646\u0627\u0633\u0628\u064b\u0627 \u0644\u0644\u0628\u0634\u0631\u0629 \u0627\u0644\u062d\u0633\u0627\u0633\u0629. \u0645\u0646 \u0627\u0644\u0633\u0627\u0639\u0627\u062a \u0648\u0627\u0644\u0623\u0633\u0627\u0648\u0631 \u0625\u0644\u0649 \u0627\u0644\u062e\u0648\u0627\u062a\u0645 \u0648\u0627\u0644\u0623\u0642\u0631\u0627\u0637\u060c \u064a\u0639\u062f \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10 \u062e\u064a\u0627\u0631\u064b\u0627 \u0645\u0641\u0636\u0644\u064b\u0627 \u0644\u0644\u0642\u0637\u0639 \u0627\u0644\u0623\u0646\u064a\u0642\u0629 \u0648\u0627\u0644\u0645\u062a\u064a\u0646\u0629 \u0641\u064a \u0639\u0627\u0644\u0645 \u0627\u0644\u0645\u0648\u0636\u0629.<\/p><h2 class=\"wp-block-heading\">\u0645\u0627 \u0647\u064a \u0645\u0639\u0627\u064a\u064a\u0631 \u0627\u0644\u0635\u0646\u0627\u0639\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 304\u061f<\/h2><p class=\"wp-block-paragraph\">\u064a\u062a\u0648\u0627\u0641\u0642 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 304 \u0645\u0639 \u0645\u0639\u0627\u064a\u064a\u0631 SAE (\u062c\u0645\u0639\u064a\u0629 \u0645\u0647\u0646\u062f\u0633\u064a \u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a)\u060c \u0641\u064a \u062d\u064a\u0646 \u062a\u062d\u062f\u062f ASTM A240\/A240M (\u0627\u0644\u062c\u0645\u0639\u064a\u0629 \u0627\u0644\u0623\u0645\u0631\u064a\u0643\u064a\u0629 \u0644\u0627\u062e\u062a\u0628\u0627\u0631 \u0648\u0645\u0639\u0627\u064a\u064a\u0631 \u0627\u0644\u0645\u0648\u0627\u062f)\u060c \u0627\u0644\u062a\u0631\u0643\u064a\u0628 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a \u0648\u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0641\u064a\u0632\u064a\u0627\u0626\u064a\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 304.<\/p><h2 class=\"wp-block-heading\">\u0645\u0627 \u0647\u064a \u0627\u0644\u0623\u0633\u0645\u0627\u0621 \u0627\u0644\u0645\u0643\u0627\u0641\u0626\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10\u061f<\/h2><p class=\"wp-block-paragraph\">\u064a\u064f\u0639\u0631\u0641 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10 \u0628\u0623\u0633\u0645\u0627\u0621 \u0648\u062a\u0633\u0645\u064a\u0627\u062a \u0645\u0643\u0627\u0641\u0626\u0629 \u0645\u062e\u062a\u0644\u0641\u0629 \u0641\u064a \u0645\u062e\u062a\u0644\u0641 \u0627\u0644\u0628\u0644\u062f\u0627\u0646 \u0648\u0627\u0644\u0645\u0639\u0627\u064a\u064a\u0631. \u0641\u064a\u0645\u0627 \u064a\u0644\u064a \u062c\u062f\u0648\u0644 \u064a\u0644\u062e\u0635 \u0647\u0630\u0647 \u0627\u0644\u0645\u0643\u0627\u0641\u0626\u0627\u062a:<\/p><figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td><strong>\u062f\u0648\u0644\u0629<\/strong><\/td><td><strong>\u0627\u0644\u0627\u0633\u0645 \u0627\u0644\u0645\u0639\u0627\u062f\u0644<\/strong><\/td><\/tr><tr><td>\u0627\u0644\u0627\u062a\u062d\u0627\u062f \u0627\u0644\u0623\u0648\u0631\u0648\u0628\u064a<\/td><td>\u0627\u0643\u06335\u0643\u0631\u0648\u0645 \u0646\u064a\u0643\u0644 18-10<\/td><\/tr><tr><td>\u0646\u062d\u0646<\/td><td>304<\/td><\/tr><tr><td>\u0623\u0644\u0645\u0627\u0646\u064a\u0627<\/td><td>X5CrNi18-9<\/td><\/tr><tr><td>\u0627\u0644\u064a\u0627\u0628\u0627\u0646<\/td><td>\u0625\u0633 \u064a\u0648 \u0625\u0633 304<\/td><\/tr><tr><td>\u0641\u0631\u0646\u0633\u0627<\/td><td>\u0627\u0643\u06335\u0643\u0631\u0648\u0645 \u0646\u064a\u0643\u0644 18-10<\/td><\/tr><tr><td>\u0627\u0646\u062c\u0644\u062a\u0631\u0627<\/td><td>\u0627\u0643\u06335\u0643\u0631\u0648\u0645 \u0646\u064a\u0643\u0644 18-10<\/td><\/tr><tr><td>\u0625\u064a\u0637\u0627\u0644\u064a\u0627<\/td><td>\u0627\u0643\u06335\u0643\u0631\u0648\u0645 \u0646\u064a\u0643\u0644 18-10<\/td><\/tr><tr><td>\u0631\u0648\u0633\u064a\u0627<\/td><td>08KH18N10<\/td><\/tr><tr><td>\u0627\u0644\u0635\u064a\u0646<\/td><td>0Cr18Ni9<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u0643\u064a\u0641 \u064a\u062a\u0645 \u062a\u0635\u0646\u064a\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10\u061f<\/h2><p class=\"wp-block-paragraph\">\u064a\u062a\u0645 \u0625\u0646\u062a\u0627\u062c \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10 \u0645\u0646 \u062e\u0644\u0627\u0644 \u0633\u0644\u0633\u0644\u0629 \u0645\u0646 \u0627\u0644\u0639\u0645\u0644\u064a\u0627\u062a \u0627\u0644\u062a\u064a \u064a\u062a\u0645 \u0627\u0644\u062a\u062d\u0643\u0645 \u0641\u064a\u0647\u0627 \u0628\u0639\u0646\u0627\u064a\u0629 \u0648\u0627\u0644\u062a\u064a \u062a\u0636\u0645\u0646 \u062c\u0648\u062f\u062a\u0647 \u0627\u0644\u0639\u0627\u0644\u064a\u0629 \u0648\u0645\u062a\u0627\u0646\u062a\u0647. \u062a\u062a\u0636\u0645\u0646 \u0639\u0645\u0644\u064a\u0629 \u0627\u0644\u0625\u0646\u062a\u0627\u062c \u0627\u0644\u0635\u0647\u0631 \u0648\u0627\u0644\u062a\u0643\u0631\u064a\u0631 \u0648\u0627\u0644\u0635\u0628 \u0648\u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0644\u0644\u062d\u0635\u0648\u0644 \u0639\u0644\u0649 \u0627\u0644\u062a\u0631\u0643\u064a\u0628\u0629 \u0648\u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0645\u062b\u0627\u0644\u064a\u0629.&nbsp;<\/p><h3 class=\"wp-block-heading\">\u0630\u0648\u0628\u0627\u0646<\/h3><p class=\"wp-block-paragraph\">\u064a\u062a\u0645 \u0635\u0647\u0631 \u0627\u0644\u0645\u0643\u0648\u0646\u0627\u062a \u0627\u0644\u0623\u0633\u0627\u0633\u064a\u0629 - \u0627\u0644\u062d\u062f\u064a\u062f \u0648\u0627\u0644\u0643\u0631\u0648\u0645 \u0648\u0627\u0644\u0646\u064a\u0643\u0644 - \u0641\u064a \u0627\u0644\u0628\u062f\u0627\u064a\u0629 \u0641\u064a \u0641\u0631\u0646 \u0627\u0644\u0642\u0648\u0633 \u0627\u0644\u0643\u0647\u0631\u0628\u0627\u0626\u064a. \u064a\u0635\u0644 \u0647\u0630\u0627 \u0627\u0644\u0641\u0631\u0646 \u0625\u0644\u0649 \u062f\u0631\u062c\u0627\u062a \u062d\u0631\u0627\u0631\u0629 \u0623\u0639\u0644\u0649 \u0645\u0646 1500 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (2732 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)\u060c \u0645\u0645\u0627 \u064a\u0636\u0645\u0646 \u062a\u0633\u064a\u064a\u0644 \u0627\u0644\u0645\u0639\u0627\u062f\u0646 \u0648\u062e\u0644\u0637\u0647\u0627 \u0628\u0627\u0644\u0643\u0627\u0645\u0644.<\/p><h3 class=\"wp-block-heading\">\u0627\u0644\u062a\u0643\u0631\u064a\u0631<\/h3><p class=\"wp-block-paragraph\">\u0628\u0645\u062c\u0631\u062f \u0630\u0648\u0628\u0627\u0646\u0647\u060c \u064a\u062e\u0636\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0646\u0635\u0647\u0631 \u0644\u0644\u062a\u0643\u0631\u064a\u0631 \u0644\u0625\u0632\u0627\u0644\u0629 \u0627\u0644\u0634\u0648\u0627\u0626\u0628. \u062a\u062a\u0636\u0645\u0646 \u0647\u0630\u0647 \u0627\u0644\u0639\u0645\u0644\u064a\u0629 \u0639\u0627\u062f\u0629\u064b \u0625\u0632\u0627\u0644\u0629 \u0627\u0644\u0643\u0631\u0628\u0646\u0629 \u0628\u0627\u0644\u0623\u0631\u062c\u0648\u0646 \u0648\u0627\u0644\u0623\u0643\u0633\u062c\u064a\u0646 (AOD) \u0623\u0648 \u0625\u0632\u0627\u0644\u0629 \u0627\u0644\u0643\u0631\u0628\u0646\u0629 \u0628\u0627\u0644\u0623\u0643\u0633\u062c\u064a\u0646 \u0628\u0627\u0644\u062a\u0641\u0631\u064a\u063a (VOD). \u062a\u0633\u0627\u0639\u062f \u0647\u0630\u0647 \u0627\u0644\u0637\u0631\u0642 \u0641\u064a \u062a\u062d\u0642\u064a\u0642 \u0627\u0644\u062a\u0631\u0643\u064a\u0628\u0629 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629 \u0627\u0644\u062f\u0642\u064a\u0642\u0629 \u0627\u0644\u0645\u0637\u0644\u0648\u0628\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10.<\/p><h3 class=\"wp-block-heading\">\u0635\u0628<\/h3><p class=\"wp-block-paragraph\">\u064a\u062a\u0645 \u0628\u0639\u062f \u0630\u0644\u0643 \u062a\u0634\u0643\u064a\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0646\u0635\u0647\u0631 \u0627\u0644\u0645\u0646\u0642\u0649 \u0625\u0644\u0649 \u0645\u0646\u062a\u062c\u0627\u062a \u0634\u0628\u0647 \u0646\u0647\u0627\u0626\u064a\u0629 \u0645\u062b\u0644 \u0627\u0644\u0643\u062a\u0644 \u0623\u0648 \u0627\u0644\u0635\u0641\u0627\u0626\u062d \u0623\u0648 \u0627\u0644\u0623\u0644\u0648\u0627\u062d. \u062a\u0639\u0645\u0644 \u0647\u0630\u0647 \u0627\u0644\u0623\u0634\u0643\u0627\u0644 \u0643\u0645\u0648\u0627\u062f \u0623\u0648\u0644\u064a\u0629 \u0644\u0645\u0632\u064a\u062f \u0645\u0646 \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629. \u0627\u0644\u0635\u0628 \u0627\u0644\u0645\u0633\u062a\u0645\u0631 \u0647\u0648 \u0637\u0631\u064a\u0642\u0629 \u0634\u0627\u0626\u0639\u0629 \u0627\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645\u060c \u0645\u0645\u0627 \u064a\u0648\u0641\u0631 \u0645\u0646\u062a\u062c\u064b\u0627 \u0645\u062a\u0646\u0627\u0633\u0642\u064b\u0627 \u0648\u0639\u0627\u0644\u064a \u0627\u0644\u062c\u0648\u062f\u0629.<\/p><h3 class=\"wp-block-heading\">\u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0633\u0627\u062e\u0646\u0629<\/h3><p class=\"wp-block-paragraph\">\u064a\u062a\u0645 \u062a\u0633\u062e\u064a\u0646 \u0627\u0644\u0623\u0634\u0643\u0627\u0644 \u0634\u0628\u0647 \u0627\u0644\u0646\u0647\u0627\u0626\u064a\u0629 \u0648\u062f\u062d\u0631\u062c\u062a\u0647\u0627 \u0639\u0644\u0649 \u0627\u0644\u0633\u0627\u062e\u0646 \u0645\u0646 \u062e\u0644\u0627\u0644 \u0627\u0644\u0645\u0637\u0627\u062d\u0646. \u0648\u0647\u0630\u0627 \u064a\u0642\u0644\u0644 \u0645\u0646 \u0633\u0645\u0643 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0648\u064a\u0634\u0643\u0644\u0647 \u0639\u0644\u0649 \u0634\u0643\u0644 \u0635\u0641\u0627\u0626\u062d \u0623\u0648 \u0644\u0641\u0627\u0626\u0641. \u0648\u064a\u0645\u0643\u0646 \u062a\u062d\u0633\u064a\u0646 \u0627\u0644\u062e\u0648\u0627\u0635 \u0627\u0644\u0645\u064a\u0643\u0627\u0646\u064a\u0643\u064a\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0648\u0627\u0644\u0644\u0645\u0633\u0629 \u0627\u0644\u0646\u0647\u0627\u0626\u064a\u0629 \u0644\u0644\u0633\u0637\u062d \u0645\u0646 \u062e\u0644\u0627\u0644 \u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0639\u0644\u0649 \u0627\u0644\u0633\u0627\u062e\u0646.&nbsp;<\/p><h3 class=\"wp-block-heading\">\u0627\u0644\u062a\u0644\u062f\u064a\u0646<\/h3><p class=\"wp-block-paragraph\">\u0628\u0639\u062f \u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0633\u0627\u062e\u0646\u0629\u060c \u064a\u062a\u0645 \u062a\u0633\u062e\u064a\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0625\u0644\u0649 \u062f\u0631\u062c\u0629 \u062d\u0631\u0627\u0631\u0629 \u0645\u0639\u064a\u0646\u0629 \u062b\u0645 \u062a\u0628\u0631\u064a\u062f\u0647 \u0628\u0628\u0637\u0621. \u062a\u0639\u0645\u0644 \u0639\u0645\u0644\u064a\u0629 \u0627\u0644\u062a\u0644\u062f\u064a\u0646 \u0639\u0644\u0649 \u062a\u062e\u0641\u064a\u0641 \u0627\u0644\u0636\u063a\u0648\u0637 \u0627\u0644\u062f\u0627\u062e\u0644\u064a\u0629 \u0648\u062a\u062d\u0633\u064a\u0646 \u0627\u0644\u0644\u062f\u0648\u0646\u0629 \u0648\u062a\u0639\u0632\u064a\u0632 \u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0645\u064a\u0643\u0627\u0646\u064a\u0643\u064a\u0629 \u0627\u0644\u0639\u0627\u0645\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630.<\/p><h3 class=\"wp-block-heading\">\u062a\u062e\u0644\u064a\u0644<\/h3><p class=\"wp-block-paragraph\">\u062b\u0645 \u064a\u062a\u0645 \u0625\u062e\u0636\u0627\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u064f\u0644\u064e\u062f\u064e\u0651\u0646 \u0644\u0639\u0645\u0644\u064a\u0629 \u0627\u0644\u062a\u062e\u0644\u064a\u0644\u060c \u062d\u064a\u062b \u064a\u062a\u0645 \u0645\u0639\u0627\u0644\u062c\u062a\u0647 \u0628\u0645\u062d\u0644\u0648\u0644 \u062d\u0645\u0636\u064a \u0644\u0625\u0632\u0627\u0644\u0629 \u0623\u064a \u0637\u0628\u0642\u0629 \u0645\u0646 \u0627\u0644\u0642\u0634\u0648\u0631 \u0623\u0648 \u0627\u0644\u0623\u0643\u0633\u064a\u062f \u0627\u0644\u0645\u062a\u0643\u0648\u0646\u0629 \u0623\u062b\u0646\u0627\u0621 \u0639\u0645\u0644\u064a\u0627\u062a \u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0633\u0627\u062e\u0646\u0629 \u0648\u0627\u0644\u062a\u0644\u062f\u064a\u0646. \u062a\u0636\u0645\u0646 \u0647\u0630\u0647 \u0627\u0644\u062e\u0637\u0648\u0629 \u0633\u0637\u062d\u064b\u0627 \u0646\u0638\u064a\u0641\u064b\u0627 \u0648\u0646\u0627\u0639\u0645\u064b\u0627.<\/p><h3 class=\"wp-block-heading\">\u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0628\u0627\u0631\u062f\u0629 (\u0627\u062e\u062a\u064a\u0627\u0631\u064a)<\/h3><p class=\"wp-block-paragraph\">\u0628\u0627\u0644\u0646\u0633\u0628\u0629 \u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0645\u0639\u064a\u0646\u0629 \u062a\u062a\u0637\u0644\u0628 \u0623\u0628\u0639\u0627\u062f\u064b\u0627 \u062f\u0642\u064a\u0642\u0629 \u0648\u062a\u0634\u0637\u064a\u0628\u064b\u0627 \u0633\u0637\u062d\u064a\u064b\u0627 \u0641\u0627\u0626\u0642\u064b\u0627\u060c \u0642\u062f \u064a\u062e\u0636\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0644\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0628\u0627\u0631\u062f\u0629. \u062a\u0645\u0631 \u0647\u0630\u0647 \u0627\u0644\u0639\u0645\u0644\u064a\u0629 \u0628\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0639\u0628\u0631 \u0628\u0643\u0631\u0627\u062a \u0641\u064a \u062f\u0631\u062c\u0629 \u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u063a\u0631\u0641\u0629\u060c \u0645\u0645\u0627 \u064a\u0639\u0632\u0632 \u0642\u0648\u062a\u0647 \u0648\u0635\u0644\u0627\u0628\u062a\u0647 \u0645\u0646 \u062e\u0644\u0627\u0644 \u0627\u0644\u062a\u0635\u0644\u0628 \u0627\u0644\u0646\u0627\u062a\u062c \u0639\u0646 \u0627\u0644\u0639\u0645\u0644.<\/p><h3 class=\"wp-block-heading\">\u0627\u0644\u062a\u0634\u0637\u064a\u0628 \u0627\u0644\u0646\u0647\u0627\u0626\u064a<\/h3><p class=\"wp-block-paragraph\">\u0648\u062a\u0634\u0645\u0644 \u0627\u0644\u062e\u0637\u0648\u0627\u062a \u0627\u0644\u0646\u0647\u0627\u0626\u064a\u0629 \u0642\u0637\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0625\u0644\u0649 \u0627\u0644\u0623\u0634\u0643\u0627\u0644 \u0648\u0627\u0644\u0623\u062d\u062c\u0627\u0645 \u0627\u0644\u0645\u0637\u0644\u0648\u0628\u0629\u060c \u0648\u0625\u062c\u0631\u0627\u0621 \u0623\u064a \u0645\u0639\u0627\u0644\u062c\u0627\u062a \u0623\u0648 \u0637\u0644\u0627\u0621\u0627\u062a \u0633\u0637\u062d\u064a\u0629 \u0625\u0636\u0627\u0641\u064a\u0629 \u062d\u0633\u0628 \u0627\u0644\u062d\u0627\u062c\u0629\u060c \u0648\u0625\u062c\u0631\u0627\u0621 \u0639\u0645\u0644\u064a\u0627\u062a \u062a\u0641\u062a\u064a\u0634 \u0634\u0627\u0645\u0644\u0629 \u0644\u0644\u062c\u0648\u062f\u0629 \u0644\u0636\u0645\u0627\u0646 \u0623\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u064a\u0644\u0628\u064a \u062c\u0645\u064a\u0639 \u0627\u0644\u0645\u0639\u0627\u064a\u064a\u0631 \u0627\u0644\u0645\u0637\u0644\u0648\u0628\u0629.<\/p><h2 class=\"wp-block-heading\">\u0645\u0627 \u0647\u0648 \u0627\u0644\u0641\u0631\u0642 \u0628\u064a\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10 \u064818\/8 \u064818\/0\u061f&nbsp;<\/h2><p class=\"wp-block-paragraph\">\u062a\u0643\u0645\u0646 \u0627\u0644\u0627\u062e\u062a\u0644\u0627\u0641\u0627\u062a \u0627\u0644\u0623\u0633\u0627\u0633\u064a\u0629 \u0628\u064a\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10 \u064818\/8 \u064818\/0 \u0641\u064a \u062a\u0631\u0643\u064a\u0628\u0647\u0627\u060c \u0648\u062e\u0627\u0635\u0629 \u0645\u062d\u062a\u0648\u0649 \u0627\u0644\u0646\u064a\u0643\u0644\u060c \u0627\u0644\u0630\u064a \u064a\u0624\u062b\u0631 \u0639\u0644\u0649 \u062e\u0635\u0627\u0626\u0635\u0647\u0627 \u0648\u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0627\u062a\u0647\u0627. \u0641\u064a\u0645\u0627 \u064a\u0644\u064a \u0645\u0642\u0627\u0631\u0646\u0629 \u0645\u0641\u0635\u0644\u0629:<\/p><h3 class=\"wp-block-heading\">\u062a\u0639\u0628\u064a\u0631<\/h3><ul class=\"wp-block-list\"><li><strong>18\/10 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623<\/strong>:\u064a\u062a\u0643\u0648\u0646 \u0645\u0646 \u0627\u0644\u0643\u0631\u0648\u0645 18% \u0648\u0627\u0644\u0646\u064a\u0643\u0644 10%. \u064a\u0636\u0645\u0646 \u0645\u062d\u062a\u0648\u0649 \u0627\u0644\u0646\u064a\u0643\u0644 \u0627\u0644\u0639\u0627\u0644\u064a \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0633\u062a\u062b\u0646\u0627\u0626\u064a\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0648\u062a\u0639\u0632\u064a\u0632 \u0627\u0644\u0642\u0648\u0629 \u0648\u062e\u0635\u0627\u0626\u0635 \u0645\u0635\u0642\u0648\u0644\u0629 \u0627\u0644\u0645\u0638\u0647\u0631.<\/li><\/ul><ul class=\"wp-block-list\"><li><strong><a href=\"https:\/\/steelprogroup.com\/ar\/stainless-steel\/grades\/18-8\/\">18\/8 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623<\/a><\/strong>:\u064a\u062d\u062a\u0648\u064a \u0639\u0644\u0649 \u0627\u0644\u0643\u0631\u0648\u0645 18% \u0648\u0627\u0644\u0646\u064a\u0643\u0644 8%. \u064a\u0648\u0641\u0631 \u0645\u0642\u0627\u0648\u0645\u0629 \u062c\u064a\u062f\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0648\u0627\u0644\u0645\u062a\u0627\u0646\u0629 \u0648\u0644\u0643\u0646 \u0623\u0642\u0644 \u0642\u0644\u064a\u0644\u0627\u064b \u0645\u0646 18\/10 \u0628\u0633\u0628\u0628 \u0645\u062d\u062a\u0648\u0649 \u0627\u0644\u0646\u064a\u0643\u0644 \u0627\u0644\u0645\u0646\u062e\u0641\u0636.<\/li><\/ul><ul class=\"wp-block-list\"><li><strong><a href=\"https:\/\/steelprogroup.com\/ar\/stainless-steel\/grades\/18-0\/\">18\/0 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623<\/a><\/strong>:\u064a\u062d\u062a\u0648\u064a \u0639\u0644\u0649 \u0627\u0644\u0643\u0631\u0648\u0645 18% \u0648\u0644\u0627 \u064a\u062d\u062a\u0648\u064a \u0639\u0644\u0649 \u0627\u0644\u0646\u064a\u0643\u0644. \u064a\u0648\u0641\u0631 \u0645\u0642\u0627\u0648\u0645\u0629 \u0623\u0633\u0627\u0633\u064a\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0648\u0644\u0643\u0646\u0647 \u064a\u0641\u062a\u0642\u0631 \u0625\u0644\u0649 \u0627\u0644\u0641\u0648\u0627\u0626\u062f \u0627\u0644\u0625\u0636\u0627\u0641\u064a\u0629 \u0644\u0644\u0646\u064a\u0643\u0644\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647 \u0623\u0642\u0644 \u0645\u062a\u0627\u0646\u0629 \u0648\u0644\u0645\u0639\u0627\u0646\u064b\u0627 \u0645\u0642\u0627\u0631\u0646\u0629 \u0628\u0627\u0644\u062f\u0631\u062c\u0627\u062a \u0627\u0644\u0623\u062e\u0631\u0649.<\/li><\/ul><h3 class=\"wp-block-heading\">\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644<\/h3><ul class=\"wp-block-list\"><li><strong>18\/10<\/strong>:\u0645\u0642\u0627\u0648\u0645\u0629 \u0645\u0645\u062a\u0627\u0632\u0629 \u0644\u0644\u062a\u0622\u0643\u0644\u060c \u0645\u0646\u0627\u0633\u0628\u0629 \u0644\u0623\u0648\u0627\u0646\u064a \u0627\u0644\u0645\u0637\u0628\u062e \u0648\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0627\u0626\u062f\u0629 \u0627\u0644\u0631\u0627\u0642\u064a\u0629 \u0627\u0644\u062a\u064a \u062a\u062a\u0644\u0627\u0645\u0633 \u0628\u0634\u0643\u0644 \u0645\u062a\u0643\u0631\u0631 \u0645\u0639 \u0627\u0644\u0637\u0639\u0627\u0645 \u0648\u0627\u0644\u0631\u0637\u0648\u0628\u0629.<\/li><\/ul><ul class=\"wp-block-list\"><li><strong>18\/8<\/strong>:\u0645\u0642\u0627\u0648\u0645\u0629 \u062c\u064a\u062f\u0629 \u062c\u062f\u064b\u0627 \u0644\u0644\u062a\u0622\u0643\u0644\u060c \u0645\u062b\u0627\u0644\u064a\u0629 \u0644\u0623\u0648\u0627\u0646\u064a \u0627\u0644\u0645\u0637\u0628\u062e \u0627\u0644\u0639\u0627\u0645\u0629 \u0648\u0627\u0644\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0646\u0632\u0644\u064a\u0629.<\/li><\/ul><ul class=\"wp-block-list\"><li><strong>18\/0<\/strong>:\u0645\u0642\u0627\u0648\u0645\u0629 \u0645\u0639\u062a\u062f\u0644\u0629 \u0644\u0644\u062a\u0622\u0643\u0644\u060c \u0648\u0647\u064a \u0627\u0644\u0623\u0641\u0636\u0644 \u0644\u0644\u0639\u0646\u0627\u0635\u0631 \u0627\u0644\u062a\u064a \u0644\u0627 \u062a\u062a\u0637\u0644\u0628 \u0627\u0633\u062a\u062e\u062f\u0627\u0645\u064b\u0627 \u0643\u062b\u064a\u0641\u064b\u0627 \u0623\u0648 \u0627\u0644\u062a\u0639\u0631\u0636 \u0644\u0628\u064a\u0626\u0627\u062a \u0642\u0627\u0633\u064a\u0629.<\/li><\/ul><h3 class=\"wp-block-heading\">\u0627\u0644\u0645\u062a\u0627\u0646\u0629 \u0648\u0627\u0644\u0642\u0648\u0629<\/h3><ul class=\"wp-block-list\"><li><strong>18\/10<\/strong>:\u0645\u062a\u0627\u0646\u0629 \u0648\u0642\u0648\u0629 \u0639\u0627\u0644\u064a\u0629\u060c \u0642\u0627\u062f\u0631\u0629 \u0639\u0644\u0649 \u062a\u062d\u0645\u0644 \u0627\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u0634\u0627\u0642 \u062f\u0648\u0646 \u0627\u0644\u0627\u0646\u062d\u0646\u0627\u0621 \u0623\u0648 \u0627\u0644\u0643\u0633\u0631.<\/li><\/ul><ul class=\"wp-block-list\"><li><strong>18\/8<\/strong>:\u0645\u062a\u0627\u0646\u0629 \u0648\u0642\u0648\u0629 \u062c\u064a\u062f\u0629\u060c \u0645\u0646\u0627\u0633\u0628\u0629 \u0644\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u064a\u0648\u0645\u064a.<\/li><\/ul><ul class=\"wp-block-list\"><li><strong>18\/0<\/strong>:\u0623\u0642\u0644 \u0645\u062a\u0627\u0646\u0629 \u0648\u0642\u0648\u0629\u060c \u0648\u0623\u0643\u062b\u0631 \u0639\u0631\u0636\u0629 \u0644\u0644\u0627\u0646\u062d\u0646\u0627\u0621 \u0648\u0627\u0644\u0643\u0633\u0631 \u062a\u062d\u062a \u0627\u0644\u0636\u063a\u0637.<\/li><\/ul><h3 class=\"wp-block-heading\">\u0627\u0644\u062c\u0627\u0630\u0628\u064a\u0629 \u0627\u0644\u062c\u0645\u0627\u0644\u064a\u0629<\/h3><ul class=\"wp-block-list\"><li><strong>18\/10<\/strong>:\u064a\u062a\u0645\u064a\u0632 \u0628\u062c\u0627\u0630\u0628\u064a\u0629 \u062c\u0645\u0627\u0644\u064a\u0629 \u0639\u0627\u0644\u064a\u0629 \u0645\u0639 \u0644\u0645\u0633\u0629 \u0646\u0647\u0627\u0626\u064a\u0629 \u0644\u0627\u0645\u0639\u0629 \u0648\u0645\u0635\u0642\u0648\u0644\u0629\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647 \u062e\u064a\u0627\u0631\u064b\u0627 \u0634\u0627\u0626\u0639\u064b\u0627 \u0644\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0637\u0628\u062e \u0648\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0627\u0626\u062f\u0629 \u0627\u0644\u0631\u0627\u0642\u064a\u0629.<\/li><\/ul><ul class=\"wp-block-list\"><li><strong>18\/8<\/strong>:\u064a\u062a\u0645\u064a\u0632 \u0623\u064a\u0636\u064b\u0627 \u0628\u0645\u0638\u0647\u0631 \u0645\u0635\u0642\u0648\u0644\u060c \u0639\u0644\u0649 \u0627\u0644\u0631\u063a\u0645 \u0645\u0646 \u0623\u0646\u0647 \u0623\u0642\u0644 \u0644\u0645\u0639\u0627\u0646\u064b\u0627 \u0642\u0644\u064a\u0644\u0627\u064b \u0645\u0646 18\/10.<\/li><\/ul><ul class=\"wp-block-list\"><li><strong>18\/0<\/strong>:\u0623\u0642\u0644 \u0644\u0645\u0639\u0627\u0646\u064b\u0627 \u0648\u0642\u062f \u064a\u0643\u0648\u0646 \u0644\u0647 \u0644\u0645\u0633\u0629 \u0646\u0647\u0627\u0626\u064a\u0629 \u063a\u064a\u0631 \u0644\u0627\u0645\u0639\u0629\u060c \u0648\u063a\u0627\u0644\u0628\u064b\u0627 \u0645\u0627 \u064a\u0633\u062a\u062e\u062f\u0645 \u0641\u064a \u0627\u0644\u0639\u0646\u0627\u0635\u0631 \u0630\u0627\u062a \u0627\u0644\u0645\u064a\u0632\u0627\u0646\u064a\u0629 \u0627\u0644\u0645\u062d\u062f\u0648\u062f\u0629.<\/li><\/ul><h3 class=\"wp-block-heading\">\u0633\u0637\u062d \u063a\u064a\u0631 \u062a\u0641\u0627\u0639\u0644\u064a<\/h3><ul class=\"wp-block-list\"><li><strong>18\/10<\/strong>:\u0644\u0627 \u064a\u062a\u0641\u0627\u0639\u0644 \u0645\u0639 \u0627\u0644\u0623\u0637\u0639\u0645\u0629 \u0627\u0644\u062d\u0645\u0636\u064a\u0629 \u0648\u0627\u0644\u0642\u0644\u0648\u064a\u0629\u060c \u0645\u0645\u0627 \u064a\u0636\u0645\u0646 \u0628\u0642\u0627\u0621 \u0637\u0639\u0645 \u0648\u062c\u0648\u062f\u0629 \u0627\u0644\u0637\u0639\u0627\u0645 \u062f\u0648\u0646 \u062a\u063a\u064a\u064a\u0631.<\/li><\/ul><ul class=\"wp-block-list\"><li><strong>18\/8<\/strong>:\u0643\u0645\u0627 \u0623\u0646\u0647\u0627 \u063a\u064a\u0631 \u062a\u0641\u0627\u0639\u0644\u064a\u0629\u060c \u0648\u0645\u0646\u0627\u0633\u0628\u0629 \u0644\u0645\u0639\u0638\u0645 \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0645\u0631\u062a\u0628\u0637\u0629 \u0628\u0627\u0644\u0623\u063a\u0630\u064a\u0629.<\/li><\/ul><ul class=\"wp-block-list\"><li><strong>18\/0<\/strong>:\u0642\u062f \u064a\u062a\u0641\u0627\u0639\u0644 \u0628\u0634\u0643\u0644 \u0637\u0641\u064a\u0641 \u0645\u0639 \u0628\u0639\u0636 \u0627\u0644\u0623\u0637\u0639\u0645\u0629\u060c \u0645\u0645\u0627 \u064a\u0624\u062b\u0631 \u0639\u0644\u0649 \u0627\u0644\u0637\u0639\u0645 \u0648\u0627\u0644\u062c\u0648\u062f\u0629 \u0645\u0639 \u0645\u0631\u0648\u0631 \u0627\u0644\u0648\u0642\u062a.<\/li><\/ul><h3 class=\"wp-block-heading\">\u064a\u0643\u0644\u0641<\/h3><ul class=\"wp-block-list\"><li><strong>18\/10<\/strong>:\u0639\u0627\u062f\u0629 \u0645\u0627 \u064a\u0643\u0648\u0646 \u0623\u063a\u0644\u0649 \u062b\u0645\u0646\u0627\u064b \u0628\u0633\u0628\u0628 \u0645\u062d\u062a\u0648\u0627\u0647 \u0627\u0644\u0639\u0627\u0644\u064a \u0645\u0646 \u0627\u0644\u0646\u064a\u0643\u0644 \u0648\u062e\u0635\u0627\u0626\u0635\u0647 \u0627\u0644\u0645\u062a\u0641\u0648\u0642\u0629.<\/li><\/ul><ul class=\"wp-block-list\"><li><strong>18\/8<\/strong>:\u0633\u0639\u0631 \u0645\u0639\u062a\u062f\u0644\u060c \u0648\u064a\u0648\u0641\u0631 \u062a\u0648\u0627\u0632\u0646\u064b\u0627 \u062c\u064a\u062f\u064b\u0627 \u0628\u064a\u0646 \u0627\u0644\u062a\u0643\u0644\u0641\u0629 \u0648\u0627\u0644\u0623\u062f\u0627\u0621.<\/li><\/ul><ul class=\"wp-block-list\"><li><strong>18\/0<\/strong>:\u0627\u0644\u062e\u064a\u0627\u0631 \u0627\u0644\u0623\u0643\u062b\u0631 \u0641\u0639\u0627\u0644\u064a\u0629 \u0645\u0646 \u062d\u064a\u062b \u0627\u0644\u062a\u0643\u0644\u0641\u0629\u060c \u0648\u0647\u0648 \u0645\u0646\u0627\u0633\u0628 \u0644\u0644\u0645\u0633\u062a\u0647\u0644\u0643\u064a\u0646 \u0627\u0644\u0645\u0647\u062a\u0645\u064a\u0646 \u0628\u0627\u0644\u0645\u064a\u0632\u0627\u0646\u064a\u0629.<\/li><\/ul><h3 class=\"wp-block-heading\">\u0627\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0627\u062a \u0627\u0644\u0634\u0627\u0626\u0639\u0629<\/h3><ul class=\"wp-block-list\"><li><strong>18\/10<\/strong>:\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0637\u0628\u062e \u0627\u0644\u0631\u0627\u0642\u064a\u0629\u060c \u0648\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0627\u0626\u062f\u0629\u060c \u0648\u0627\u0644\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0637\u0628\u064a\u0629\u060c \u0648\u0627\u0644\u0639\u0646\u0627\u0635\u0631 \u0627\u0644\u0632\u062e\u0631\u0641\u064a\u0629.<\/li><\/ul><ul class=\"wp-block-list\"><li><strong>18\/8<\/strong>:\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0637\u0628\u062e \u0627\u0644\u0639\u0627\u0645\u0629 \u0648\u0627\u0644\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0646\u0632\u0644\u064a\u0629 \u0648\u0628\u0639\u0636 \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0635\u0646\u0627\u0639\u064a\u0629.<\/li><\/ul><ul class=\"wp-block-list\"><li><strong>18\/0<\/strong>:\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0637\u0628\u062e \u0648\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0627\u0626\u062f\u0629 \u0648\u0627\u0644\u0623\u0634\u064a\u0627\u0621 \u0630\u0627\u062a \u0627\u0644\u0645\u064a\u0632\u0627\u0646\u064a\u0629 \u0627\u0644\u0645\u062d\u062f\u0648\u062f\u0629 \u0648\u0627\u0644\u062a\u064a \u062a\u062a\u0639\u0631\u0636 \u0628\u0634\u0643\u0644 \u0623\u0642\u0644 \u0644\u0644\u0638\u0631\u0648\u0641 \u0627\u0644\u0642\u0627\u0633\u064a\u0629.<\/li><\/ul><p class=\"wp-block-paragraph\">\u064a\u0645\u0643\u0646 \u0623\u0646 \u064a\u0633\u0627\u0639\u062f\u0643 \u0627\u0644\u062c\u062f\u0648\u0644 \u0627\u0644\u062a\u0627\u0644\u064a \u0639\u0644\u0649 \u0631\u0624\u064a\u0629 \u0627\u0644\u0627\u062e\u062a\u0644\u0627\u0641\u0627\u062a \u0628\u064a\u0646 \u0647\u0630\u0647 \u0627\u0644\u062f\u0631\u062c\u0627\u062a \u0627\u0644\u062b\u0644\u0627\u062b \u0628\u0634\u0643\u0644 \u0623\u0643\u062b\u0631 \u062d\u062f\u0633\u064b\u0627.<\/p><figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td><strong>\u0645\u0644\u0643\u064a\u0629<\/strong><\/td><td><strong>18\/10 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623<\/strong><\/td><td><strong>18\/8 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623<\/strong><\/td><td><strong>18\/0 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623<\/strong><\/td><\/tr><tr><td><strong>\u062a\u0639\u0628\u064a\u0631<\/strong><\/td><td>18% \u0643\u0631\u0648\u0645\u060c 10% \u0646\u064a\u0643\u0644<\/td><td>18% \u0643\u0631\u0648\u0645\u060c 8% \u0646\u064a\u0643\u0644<\/td><td>18% \u0643\u0631\u0648\u0645\u060c 0% \u0646\u064a\u0643\u0644<\/td><\/tr><tr><td><strong><a href=\"https:\/\/steelprogroup.com\/ar\/stainless-steel\/properties\/corrosion-resistant\/\">\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644<\/a><\/strong><\/td><td>\u0645\u0645\u062a\u0627\u0632<\/td><td>\u062c\u064a\u062f \u062c\u062f\u064b\u0627<\/td><td>\u0645\u0639\u062a\u062f\u0644<\/td><\/tr><tr><td><strong>\u0627\u0644\u0645\u062a\u0627\u0646\u0629 \u0648\u0627\u0644\u0642\u0648\u0629<\/strong><\/td><td>\u0639\u0627\u0644\u064a<\/td><td>\u062c\u064a\u062f<\/td><td>\u0623\u062f\u0646\u0649<\/td><\/tr><tr><td><strong>\u0627\u0644\u062c\u0627\u0630\u0628\u064a\u0629 \u0627\u0644\u062c\u0645\u0627\u0644\u064a\u0629<\/strong><\/td><td>\u0644\u0645\u0633\u0629 \u0646\u0647\u0627\u0626\u064a\u0629 \u0644\u0627\u0645\u0639\u0629 \u0648\u0645\u0635\u0642\u0648\u0644\u0629<\/td><td>\u0645\u0638\u0647\u0631 \u0645\u0635\u0642\u0648\u0644<\/td><td>\u0623\u0642\u0644 \u0644\u0645\u0639\u0627\u0646\u064b\u0627\u060c \u0648\u0623\u0643\u062b\u0631 \u0644\u0645\u0633\u0629 \u0646\u0647\u0627\u0626\u064a\u0629 \u063a\u064a\u0631 \u0644\u0627\u0645\u0639\u0629<\/td><\/tr><tr><td><strong>\u0633\u0637\u062d \u063a\u064a\u0631 \u062a\u0641\u0627\u0639\u0644\u064a<\/strong><\/td><td>\u063a\u064a\u0631 \u0645\u062a\u0641\u0627\u0639\u0644 \u0645\u0639 \u0627\u0644\u0623\u0637\u0639\u0645\u0629<\/td><td>\u0644\u0627 \u064a\u062a\u0641\u0627\u0639\u0644 \u0645\u0639 \u0645\u0639\u0638\u0645 \u0627\u0644\u0623\u0637\u0639\u0645\u0629<\/td><td>\u0642\u062f \u064a\u062a\u0641\u0627\u0639\u0644 \u0645\u0639 \u0628\u0639\u0636 \u0627\u0644\u0623\u0637\u0639\u0645\u0629<\/td><\/tr><tr><td><strong>\u064a\u0643\u0644\u0641<\/strong><\/td><td>\u0623\u063a\u0644\u0649<\/td><td>\u0623\u0633\u0639\u0627\u0631 \u0645\u0639\u062a\u062f\u0644\u0629<\/td><td>\u0627\u0644\u0623\u0643\u062b\u0631 \u0628\u0623\u0633\u0639\u0627\u0631 \u0645\u0639\u0642\u0648\u0644\u0629<\/td><\/tr><tr><td><strong>\u0627\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0627\u062a \u0627\u0644\u0634\u0627\u0626\u0639\u0629<\/strong><\/td><td>\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0637\u0628\u062e \u0627\u0644\u0631\u0627\u0642\u064a\u0629\u060c \u0648\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0627\u0626\u062f\u0629\u060c \u0648\u0627\u0644\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0637\u0628\u064a\u0629\u060c \u0648\u0627\u0644\u0639\u0646\u0627\u0635\u0631 \u0627\u0644\u0632\u062e\u0631\u0641\u064a\u0629<\/td><td>\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0637\u0628\u062e \u0627\u0644\u0639\u0627\u0645\u0629 \u0648\u0627\u0644\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0646\u0632\u0644\u064a\u0629<\/td><td>\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0637\u0628\u062e \u0648\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0627\u0626\u062f\u0629 \u0628\u0623\u0633\u0639\u0627\u0631 \u0645\u0639\u0642\u0648\u0644\u0629<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u0627\u0644\u0623\u0633\u0626\u0644\u0629 \u0627\u0644\u0634\u0627\u0626\u0639\u0629<\/h2><h2 class=\"wp-block-heading\">\u0644\u0645\u0627\u0630\u0627 \u064a\u062a\u0645 \u0627\u0633\u062a\u062e\u062f\u0627\u0645 18\/10 \u0644\u0623\u0648\u0627\u0646\u064a \u0627\u0644\u0637\u0628\u062e \u0627\u0644\u0645\u0635\u0646\u0648\u0639\u0629 \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623\u061f<\/h2><p class=\"wp-block-paragraph\">\u064a\u062a\u0645\u064a\u0632 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10 \u0628\u0645\u0642\u0627\u0648\u0645\u0629 \u0645\u0645\u062a\u0627\u0632\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0648\u0627\u0644\u0645\u062a\u0627\u0646\u0629 \u0648\u0627\u0644\u0645\u0638\u0647\u0631 \u0627\u0644\u0644\u0627\u0645\u0639\u060c \u0648\u064a\u0633\u062a\u062e\u062f\u0645 \u0641\u064a \u0623\u0648\u0627\u0646\u064a \u0627\u0644\u0637\u0647\u064a. \u064a\u0648\u0641\u0631 \u0627\u0644\u0643\u0631\u0648\u0645 18% \u0637\u0628\u0642\u0629 \u0648\u0627\u0642\u064a\u0629 \u0636\u062f \u0627\u0644\u0635\u062f\u0623\u060c \u0628\u064a\u0646\u0645\u0627 \u064a\u0636\u064a\u0641 \u0627\u0644\u0646\u064a\u0643\u0644 10% \u0627\u0644\u0642\u0648\u0629 \u0648\u0627\u0644\u0635\u0644\u0627\u0628\u0629\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647 \u0645\u062b\u0627\u0644\u064a\u064b\u0627 \u0644\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u064a\u0648\u0645\u064a \u0641\u064a \u0627\u0644\u0645\u0637\u0628\u062e.<\/p><h3 class=\"wp-block-heading\">\u0647\u0644 \u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0627\u0626\u062f\u0629 18\/10 \u062a\u0635\u062f\u0623\u061f<\/h3><p class=\"wp-block-paragraph\">\u062a\u062a\u0645\u064a\u0632 \u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0627\u0626\u062f\u0629 \u0627\u0644\u0645\u0635\u0646\u0648\u0639\u0629 \u0645\u0646 \u0645\u0627\u062f\u0629 18\/10 \u0628\u0645\u0642\u0627\u0648\u0645\u0629 \u0639\u0627\u0644\u064a\u0629 \u0644\u0644\u0635\u062f\u0623 \u0628\u0633\u0628\u0628 \u0645\u062d\u062a\u0648\u0627\u0647\u0627 \u0627\u0644\u0639\u0627\u0644\u064a \u0645\u0646 \u0627\u0644\u0643\u0631\u0648\u0645. \u0648\u0645\u0639 \u0630\u0644\u0643\u060c \u0625\u0630\u0627 \u062a\u0639\u0631\u0636\u062a \u0644\u0638\u0631\u0648\u0641 \u0642\u0627\u0633\u064a\u0629 \u0623\u0648 \u0644\u0645 \u064a\u062a\u0645 \u0627\u0644\u0639\u0646\u0627\u064a\u0629 \u0628\u0647\u0627 \u0628\u0634\u0643\u0644 \u0635\u062d\u064a\u062d\u060c \u0641\u0642\u062f \u062a\u062a\u0634\u0643\u0644 \u0639\u0644\u064a\u0647\u0627 \u0628\u0642\u0639 \u0635\u062f\u0623 \u0628\u0633\u064a\u0637\u0629 \u0628\u0645\u0631\u0648\u0631 \u0627\u0644\u0648\u0642\u062a. \u064a\u0645\u0643\u0646 \u0623\u0646 \u064a\u0633\u0627\u0639\u062f \u0627\u0644\u062a\u0646\u0638\u064a\u0641 \u0648\u0627\u0644\u062a\u062c\u0641\u064a\u0641 \u0627\u0644\u0645\u0646\u062a\u0638\u0645\u0627\u0646 \u0641\u064a \u0627\u0644\u062d\u0641\u0627\u0638 \u0639\u0644\u0649 \u062d\u0627\u0644\u062a\u0647\u0627 \u0627\u0644\u062e\u0627\u0644\u064a\u0629 \u0645\u0646 \u0627\u0644\u0635\u062f\u0623.<\/p><p class=\"wp-block-paragraph\"><strong>\u0642\u0631\u0627\u0621\u0629 \u0630\u0627\u062a \u0635\u0644\u0629<\/strong><br><a href=\"https:\/\/steelprogroup.com\/ar\/stainless-steel\/rust\/\">\u0647\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u064a\u0635\u062f\u0623 \u0648\u0643\u064a\u0641 \u064a\u0645\u0643\u0646\u0643 \u062d\u0644 \u0647\u0630\u0647 \u0627\u0644\u0645\u0634\u0643\u0644\u0629\u061f<\/a><br><a href=\"https:\/\/steelprogroup.com\/ar\/stainless-steel\/maintenance\/clean\/\">\u0643\u064a\u0641\u064a\u0629 \u062a\u0646\u0638\u064a\u0641 \u0648\u062a\u0644\u0645\u064a\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623\u061f<\/a><\/p><h3 class=\"wp-block-heading\">\u0647\u0644 \u064a\u062a\u0633\u0631\u0628 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10 \u0625\u0644\u0649 \u0627\u0644\u0637\u0639\u0627\u0645\u061f<\/h3><p class=\"wp-block-paragraph\">\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10 \u063a\u064a\u0631 \u0642\u0627\u0628\u0644 \u0644\u0644\u062a\u0641\u0627\u0639\u0644 \u0648\u0644\u0627 \u064a\u062a\u0633\u0631\u0628 \u0625\u0644\u0649 \u0627\u0644\u0637\u0639\u0627\u0645\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647 \u062e\u064a\u0627\u0631\u064b\u0627 \u0622\u0645\u0646\u064b\u0627 \u0644\u0644\u0637\u0647\u064a \u0648\u0627\u0644\u062a\u0642\u062f\u064a\u0645. \u062a\u0631\u0643\u064a\u0628\u062a\u0647 \u062a\u0645\u0646\u0639 \u0627\u0644\u062a\u0641\u0627\u0639\u0644\u0627\u062a \u0645\u0639 \u0627\u0644\u0623\u062d\u0645\u0627\u0636 \u0623\u0648 \u0627\u0644\u0642\u0644\u0648\u064a\u0627\u062a\u060c \u0645\u0645\u0627 \u064a\u062d\u0627\u0641\u0638 \u0639\u0644\u0649 \u0645\u0630\u0627\u0642 \u0648\u062c\u0648\u062f\u0629 \u0648\u062c\u0628\u0627\u062a\u0643.<\/p><h3 class=\"wp-block-heading\">\u0647\u0644 \u064a\u0645\u0643\u0646 \u0625\u0639\u0627\u062f\u0629 \u062a\u062f\u0648\u064a\u0631 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10\u061f<\/h3><p class=\"wp-block-paragraph\">\u0646\u0639\u0645\u060c \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 18\/10 \u0642\u0627\u0628\u0644 \u0644\u0625\u0639\u0627\u062f\u0629 \u0627\u0644\u062a\u062f\u0648\u064a\u0631 \u0628\u0627\u0644\u0643\u0627\u0645\u0644. \u062a\u0633\u0645\u062d \u062a\u0631\u0643\u064a\u0628\u062a\u0647 \u0628\u0635\u0647\u0631\u0647 \u0648\u0625\u0639\u0627\u062f\u0629 \u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0647 \u062f\u0648\u0646 \u0641\u0642\u062f\u0627\u0646 \u062e\u0635\u0627\u0626\u0635\u0647\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647 \u062e\u064a\u0627\u0631\u064b\u0627 \u0635\u062f\u064a\u0642\u064b\u0627 \u0644\u0644\u0628\u064a\u0626\u0629 \u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0627\u062a \u0645\u062e\u062a\u0644\u0641\u0629. \u064a\u0633\u0627\u0639\u062f \u0625\u0639\u0627\u062f\u0629 \u062a\u062f\u0648\u064a\u0631 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0641\u064a \u0627\u0644\u062d\u0641\u0627\u0638 \u0639\u0644\u0649 \u0627\u0644\u0645\u0648\u0627\u0631\u062f \u0648\u0627\u0644\u062d\u062f \u0645\u0646 \u0627\u0644\u062a\u0623\u062b\u064a\u0631 \u0627\u0644\u0628\u064a\u0626\u064a.<\/p>","protected":false},"excerpt":{"rendered":"<p>\u0639\u0646\u062f \u0627\u062e\u062a\u064a\u0627\u0631 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0644\u0623\u0648\u0627\u0646\u064a \u0627\u0644\u0637\u0647\u064a \u0623\u0648 \u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0627\u0626\u062f\u0629 \u0623\u0648 \u062d\u062a\u0649 \u0627\u0644\u0623\u062c\u0647\u0632\u0629 \u0627\u0644\u0637\u0628\u064a\u0629\u060c \u0631\u0628\u0645\u0627 \u062a\u0643\u0648\u0646 \u0642\u062f \u0635\u0627\u062f\u0641\u062a \u0627\u0644\u0645\u0635\u0637\u0644\u062d &quot;18\/10 [...]<\/p>","protected":false},"author":1,"featured_media":10285,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"_eb_attr":"","rank_math_lock_modified_date":false,"site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"categories":[4191,112],"tags":[],"class_list":["post-10289","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-grades","category-stainless-steel"],"acf":[],"_links":{"self":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts\/10289","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/comments?post=10289"}],"version-history":[{"count":0,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts\/10289\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/media\/10285"}],"wp:attachment":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/media?parent=10289"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/categories?post=10289"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/tags?post=10289"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}