{"id":10290,"date":"2024-09-11T11:45:00","date_gmt":"2024-09-11T03:45:00","guid":{"rendered":"https:\/\/app11147.cloudwayssites.com\/?p=10290"},"modified":"2025-02-17T19:03:27","modified_gmt":"2025-02-17T11:03:27","slug":"grade-409","status":"publish","type":"post","link":"https:\/\/steelprogroup.com\/ar\/stainless-steel\/grades\/grade-409\/","title":{"rendered":"\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409: \u0627\u0644\u062a\u0639\u0631\u064a\u0641 \u0648\u0627\u0644\u062a\u0631\u0643\u064a\u0628 \u0648\u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0648\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0648\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0648\u0627\u0644\u0645\u0632\u064a\u062f"},"content":{"rendered":"<h2 class=\"wp-block-heading\">\u0645\u0627 \u0647\u0648 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409\u061f<\/h2><p class=\"wp-block-paragraph\">409\u060c \u0648\u0627\u0644\u0645\u0639\u0631\u0648\u0641\u0629 \u0623\u064a\u0636\u064b\u0627 \u0628\u0627\u0633\u0645 UNS S40900\u060c \u0647\u064a \u0633\u0644\u0633\u0644\u0629 400 <a href=\"https:\/\/steelprogroup.com\/ar\/stainless-steel\/type\/ferritic\/\">\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0641\u0631\u064a\u062a\u064a<\/a> \u064a\u062a\u0643\u0648\u0646 \u0628\u0634\u0643\u0644 \u0623\u0633\u0627\u0633\u064a \u0645\u0646 \u0627\u0644\u0643\u0631\u0648\u0645 (10.5-11.75%) \u0645\u0639 \u0643\u0645\u064a\u0629 \u0635\u063a\u064a\u0631\u0629 \u0645\u0646 \u0627\u0644\u0643\u0631\u0628\u0648\u0646 (\u22640.08%) \u0648\u0627\u0644\u062a\u064a\u062a\u0627\u0646\u064a\u0648\u0645 \u0627\u0644\u0645\u0636\u0627\u0641 (\u22640.75%). \u064a\u062a\u0648\u0627\u0641\u0642 409 \u0645\u0639 \u0645\u0639\u0627\u064a\u064a\u0631 \u0645\u062b\u0644 ASTM A240 \u0644\u0644\u0635\u0641\u0627\u0626\u062d \u0648\u0627\u0644\u0623\u0644\u0648\u0627\u062d \u0648\u0627\u0644\u0623\u0634\u0631\u0637\u0629 \u0648\u064a\u0639\u0627\u062f\u0644 1.4512 (EN). \u064a\u062a\u0645\u064a\u0632 \u0628\u0645\u0642\u0627\u0648\u0645\u062a\u0647 \u0627\u0644\u0645\u0645\u062a\u0627\u0632\u0629 \u0644\u0644\u0623\u0643\u0633\u062f\u0629 \u0648\u0627\u0644\u062a\u0622\u0643\u0644 \u0641\u064a \u062f\u0631\u062c\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u0639\u0627\u0644\u064a\u0629\u060c \u0648\u062e\u0627\u0635\u0629 \u0641\u064a \u0646\u0637\u0627\u0642 400-600 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629. \u062a\u0634\u0645\u0644 \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0634\u0627\u0626\u0639\u0629 \u0623\u0646\u0638\u0645\u0629 \u0639\u0627\u062f\u0645 \u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a \u0648\u0627\u0644\u0645\u0628\u0627\u062f\u0644\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629 \u0648\u0627\u0644\u0623\u062c\u0647\u0632\u0629. \u064a\u062a\u0645\u062a\u0639 409 \u0628\u0645\u0642\u0627\u0648\u0645\u0629 \u0623\u0642\u0644 \u0644\u0644\u062a\u0622\u0643\u0644 \u0645\u0642\u0627\u0631\u0646\u0629 \u0628\u0627\u0644\u062f\u0631\u062c\u0627\u062a \u0627\u0644\u0623\u0648\u0633\u062a\u0646\u064a\u062a\u064a\u0629 \u0645\u062b\u0644 304 \u0623\u0648 316. \u0648\u0639\u0627\u062f\u0629 \u0645\u0627 \u062a\u062a\u0645 \u0645\u0639\u0627\u0644\u062c\u062a\u0647 \u0645\u0646 \u062e\u0644\u0627\u0644 \u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0628\u0627\u0631\u062f\u0629 \u0648\u0627\u0644\u0644\u062d\u0627\u0645 \u0648\u0627\u0644\u062a\u0634\u0643\u064a\u0644 \u0648\u0645\u0627 \u0625\u0644\u0649 \u0630\u0644\u0643\u060c \u0644\u062a\u062d\u0642\u064a\u0642 \u0627\u0644\u0634\u0643\u0644 \u0648\u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0645\u064a\u0643\u0627\u0646\u064a\u0643\u064a\u0629 \u0627\u0644\u0645\u0637\u0644\u0648\u0628\u0629.&nbsp;<\/p><h2 class=\"wp-block-heading\">\u0627\u0644\u062a\u0631\u0643\u064a\u0628 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409<\/h2><p class=\"wp-block-paragraph\">\u064a\u062a\u0645 \u0625\u062f\u0631\u0627\u062c \u0627\u0644\u062a\u0631\u0643\u064a\u0628 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409 \u0639\u0644\u0649 \u0627\u0644\u0646\u062d\u0648 \u0627\u0644\u062a\u0627\u0644\u064a:<\/p><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u0639\u0646\u0635\u0631<\/strong><\/td><td><strong>\u0627\u0644\u0643\u0631\u0628\u0648\u0646\u060c \u062c<\/strong><\/td><td><strong>\u0627\u0644\u0643\u0631\u0648\u0645\u060c \u0627\u0644\u0643\u0631\u0648\u0645<\/strong><\/td><td><strong>\u0627\u0644\u0645\u0646\u063a\u0646\u064a\u0632\u060c \u0627\u0644\u0645\u0646\u063a\u0646\u064a\u0632<\/strong><\/td><td><strong>\u0627\u0644\u0641\u0648\u0633\u0641\u0648\u0631\u060c \u0641<\/strong><\/td><td><strong>\u0627\u0644\u0633\u064a\u0644\u064a\u0643\u0648\u0646<\/strong><\/td><td><strong>\u0627\u0644\u0643\u0628\u0631\u064a\u062a\u060c \u0633<\/strong><\/td><td><strong>\u0627\u0644\u062a\u064a\u062a\u0627\u0646\u064a\u0648\u0645\u060c \u062a\u064a<\/strong><\/td><td><strong>\u0627\u0644\u062d\u062f\u064a\u062f\u060c Fe<\/strong><\/td><\/tr><tr><td>\u0627\u0644\u0645\u062d\u062a\u0648\u0649 (%)<\/td><td>\u2264 0.080<\/td><td>11.13<\/td><td>\u2264 1.0<\/td><td>\u2264 0.045<\/td><td>\u2264 1.0<\/td><td>\u2264 0.045<\/td><td>0.75<\/td><td>\u062a\u0648\u0627\u0632\u0646<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409<\/h2><p class=\"wp-block-paragraph\">\u0641\u064a\u0645\u0627 \u064a\u0644\u064a \u062b\u0644\u0627\u062b\u0629 \u0623\u0633\u0628\u0627\u0628 \u0631\u0626\u064a\u0633\u064a\u0629 \u062a\u062c\u0639\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409 \u0641\u0631\u064a\u062f\u064b\u0627 \u0645\u0646 \u0646\u0648\u0639\u0647:<\/p><ol class=\"wp-block-list\"><li>\u0645\u0642\u0627\u0648\u0645\u0629 \u0645\u0645\u062a\u0627\u0632\u0629 \u0644\u0644\u062a\u0622\u0643\u0644\u060c \u0648\u062e\u0627\u0635\u0629 \u0641\u064a \u0623\u0646\u0638\u0645\u0629 \u0627\u0644\u0639\u0627\u062f\u0645.<\/li>\n\n<li>\u0633\u0647\u0644\u0629 \u0627\u0644\u0644\u062d\u0627\u0645 \u0648\u0627\u0644\u062a\u0634\u0643\u064a\u0644 \u0625\u0644\u0649 \u0623\u0634\u0643\u0627\u0644 \u0645\u062e\u062a\u0644\u0641\u0629.<\/li>\n\n<li>\u0641\u0639\u0627\u0644\u0629 \u0645\u0646 \u062d\u064a\u062b \u0627\u0644\u062a\u0643\u0644\u0641\u0629 \u0645\u0642\u0627\u0631\u0646\u0629 \u0628\u0623\u0646\u0648\u0627\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0623\u062e\u0631\u0649.<\/li><\/ol><h3 class=\"wp-block-heading\">\u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0641\u064a\u0632\u064a\u0627\u0626\u064a\u0629<\/h3><p class=\"wp-block-paragraph\">\u0642\u0645 \u0628\u0641\u062d\u0635 \u0627\u0644\u062c\u062f\u0648\u0644 \u0623\u062f\u0646\u0627\u0647 \u0644\u0645\u0639\u0631\u0641\u0629 \u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0641\u064a\u0632\u064a\u0627\u0626\u064a\u0629 \u0627\u0644\u0623\u0633\u0627\u0633\u064a\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409:<\/p><figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td><strong>\u0645\u0644\u0643\u064a\u0629<\/strong><\/td><td><strong>\u0627\u0644\u0642\u064a\u0645\u0629 (\u0645\u062a\u0631\u064a\u0629)<\/strong><\/td><td><strong>\u0627\u0644\u0642\u064a\u0645\u0629 (\u0627\u0644\u0625\u0645\u0628\u0631\u0627\u0637\u0648\u0631\u064a\u0629)<\/strong><\/td><\/tr><tr><td>\u0643\u062b\u0627\u0641\u0629<\/td><td>7.80 \u062c\u0631\u0627\u0645\/\u0633\u0645 \u0645\u0643\u0639\u0628<\/td><td>0.282 \u0631\u0637\u0644\/\u0628\u0648\u0635\u0629 \u0645\u0643\u0639\u0628\u0629<\/td><\/tr><tr><td>\u0646\u0642\u0637\u0629 \u0627\u0644\u0627\u0646\u0635\u0647\u0627\u0631<\/td><td>1425 \u2013 1510 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629<\/td><td>2597 \u2013 2750 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a<\/td><\/tr><tr><td>CTE\u060c \u062e\u0637\u064a (20.0 \u2013 100 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \/ 68.0 \u2013 212 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/td><td>11.7 \u0645\u064a\u0643\u0631\u0648\u0645\u062a\u0631\/\u0645\u062a\u0631-\u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629<\/td><td>6.50 \u0645\u064a\u0643\u0631\u0648\u0646\/\u0628\u0648\u0635\u0629-\u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a<\/td><\/tr><tr><td>CTE\u060c \u062e\u0637\u064a (20.0 \u2013 260 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \/ 68.0 \u2013 500 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/td><td>11.9 \u0645\u064a\u0643\u0631\u0648\u0645\u062a\u0631\/\u0645\u062a\u0631-\u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629<\/td><td>6.61 \u0645\u064a\u0643\u0631\u0648\u0646\/\u0628\u0648\u0635\u0629-\u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a<\/td><\/tr><tr><td>CTE\u060c \u062e\u0637\u064a (20.0 \u2013 480 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \/ 68.0 \u2013 896 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/td><td>12.4 \u0645\u064a\u0643\u0631\u0648\u0645\u062a\u0631\/\u0645\u062a\u0631-\u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629<\/td><td>6.89 \u0645\u064a\u0643\u0631\u0648\u0646\/\u0628\u0648\u0635\u0629-\u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a<\/td><\/tr><tr><td>CTE\u060c \u062e\u0637\u064a (20.0 \u2013 650 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \/ 68.0 \u2013 1200 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/td><td>12.9 \u0645\u064a\u0643\u0631\u0648\u0645\u062a\u0631\/\u0645\u062a\u0631-\u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629<\/td><td>7.17 \u0645\u064a\u0643\u0631\u0648\u0646\/\u0628\u0648\u0635\u0629-\u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a<\/td><\/tr><tr><td>CTE\u060c \u062e\u0637\u064a (20.0 \u2013 815 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \/ 68.0 \u2013 1500 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/td><td>13.5 \u0645\u064a\u0643\u0631\u0648\u0645\u062a\u0631\/\u0645\u062a\u0631-\u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629<\/td><td>7.50 \u0645\u064a\u0643\u0631\u0648\u0646\/\u0628\u0648\u0635\u0629-\u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a<\/td><\/tr><tr><td>\u0627\u0644\u0633\u0639\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629 \u0627\u0644\u0646\u0648\u0639\u064a\u0629 (0.0 \u2013 100 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \/ 32.0 \u2013 212 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/td><td>0.460 \u062c\u0648\u0644\/\u062c\u0645-\u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629<\/td><td>0.110 \u0648\u062d\u062f\u0629 \u062d\u0631\u0627\u0631\u064a\u0629 \u0628\u0631\u064a\u0637\u0627\u0646\u064a\u0629\/\u0631\u0637\u0644-\u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a<\/td><\/tr><tr><td>\u0627\u0644\u0645\u0648\u0635\u0644\u064a\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629 (95.0 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \/ 203 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/td><td>24.9 \u0648\u0627\u0637\/\u0645\u062a\u0631 \u0643\u0644\u0641\u0646<\/td><td>173 \u0648\u062d\u062f\u0629 \u062d\u0631\u0627\u0631\u064a\u0629 \u0628\u0631\u064a\u0637\u0627\u0646\u064a\u0629\/\u0633\u0627\u0639\u0629\/\u0642\u062f\u0645 \u0645\u0631\u0628\u0639-\u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a<\/td><\/tr><tr><td>\u0627\u0644\u0645\u0648\u0635\u0644\u064a\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629 (540 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \/ 1000 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/td><td>28.6 \u0648\u0627\u0637\/\u0645\u062a\u0631 \u0643\u0644\u0641\u0646<\/td><td>198 \u0648\u062d\u062f\u0629 \u062d\u0631\u0627\u0631\u064a\u0629 \u0628\u0631\u064a\u0637\u0627\u0646\u064a\u0629\/\u0633\u0627\u0639\u0629\/\u0642\u062f\u0645 \u0645\u0631\u0628\u0639-\u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a<\/td><\/tr><tr><td>\u0627\u0644\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u0643\u0647\u0631\u0628\u0627\u0626\u064a\u0629 (20.0 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \/ 68.0 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/td><td>0.0000600 \u0623\u0648\u0645-\u0633\u0645<\/td><td>0.0000600 \u0623\u0648\u0645-\u0633\u0645<\/td><\/tr><tr><td>\u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0645\u063a\u0646\u0627\u0637\u064a\u0633\u064a\u0629<\/td><td>\u0645\u063a\u0646\u0627\u0637\u064a\u0633\u064a\u0629 \u0628\u0633\u0628\u0628 \u0627\u0644\u0628\u0646\u064a\u0629 \u0627\u0644\u0641\u0631\u064a\u062a\u064a\u0629<\/td><td>\/<\/td><\/tr><\/tbody><\/table><\/figure><h3 class=\"wp-block-heading\">\u0627\u0644\u062e\u0648\u0627\u0635 \u0627\u0644\u0645\u064a\u0643\u0627\u0646\u064a\u0643\u064a\u0629<\/h3><p class=\"wp-block-paragraph\">\u0642\u0645 \u0628\u0641\u062d\u0635 \u0627\u0644\u062c\u062f\u0648\u0644 \u0623\u062f\u0646\u0627\u0647 \u0644\u0645\u0639\u0631\u0641\u0629 \u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0645\u064a\u0643\u0627\u0646\u064a\u0643\u064a\u0629 \u0627\u0644\u0623\u0633\u0627\u0633\u064a\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409:<\/p><figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td><strong>\u0645\u0644\u0643\u064a\u0629<\/strong><\/td><td><strong>\u0642\u064a\u0645\u0629<\/strong><\/td><td><strong>\u0623\u062f\u0627\u0621<\/strong><\/td><\/tr><tr><td>\u0642\u0648\u0629 \u0627\u0644\u0634\u062f<\/td><td>448 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644 (65 \u0643\u064a\u0644\u0648\u0628\u0627\u0633\u0643\u0627\u0644)<\/td><td>\u0645\u062a\u0648\u0633\u0637\u061b \u0623\u0642\u0644 \u0645\u0646 304 \u0648316 \u062f\u0631\u062c\u0629<\/td><\/tr><tr><td>\u0642\u0648\u0629 \u0627\u0644\u062e\u0636\u0648\u0639 (\u0633\u0644\u0627\u0644\u0629 0.2%)<\/td><td>238 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644 (34.5 \u0643\u064a\u0644\u0648\u0628\u0627\u0633\u0643\u0627\u0644)<\/td><td>\u0645\u0646\u0627\u0633\u0628 \u0644\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u0647\u064a\u0643\u0644\u064a \u0627\u0644\u0639\u0627\u0645<\/td><\/tr><tr><td>\u0635\u0644\u0627\u0628\u0629 \u0628\u0631\u064a\u0646\u064a\u0644 (HB)<\/td><td>143<\/td><td rowspan=\"3\">\u0635\u0644\u0627\u0628\u0629 \u0645\u0639\u062a\u062f\u0644\u0629\u061b \u0623\u0643\u062b\u0631 \u0644\u064a\u0648\u0646\u0629 \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0639\u0627\u0644\u064a \u0627\u0644\u0642\u0648\u0629 \u0645\u062b\u0644 316\u060c \u0642\u0627\u0628\u0644\u064a\u0629 \u062a\u0634\u0643\u064a\u0644 \u0623\u0641\u0636\u0644<\/td><\/tr><tr><td>\u0635\u0644\u0627\u0628\u0629 \u0631\u0648\u0643\u0648\u064a\u0644 (HRB)<\/td><td>72<\/td><\/tr><tr><td>\u0635\u0644\u0627\u0628\u0629 \u0641\u064a\u0643\u0631\u0632 (HV)<\/td><td>155<\/td><\/tr><tr><td>\u0627\u0644\u0627\u0633\u062a\u0637\u0627\u0644\u0629 \u0639\u0646\u062f \u0627\u0644\u0643\u0633\u0631 (50 \u0645\u0645)<\/td><td>32.50%<\/td><td>\u0644\u064a\u0648\u0646\u0629 \u062c\u064a\u062f\u0629\u060c \u0633\u0647\u0644\u0629 \u0627\u0644\u062a\u0634\u0643\u064a\u0644<\/td><\/tr><tr><td>\u0645\u0639\u0627\u0645\u0644 \u064a\u0648\u0646\u063a<\/td><td>200 \u062c\u064a\u062c\u0627\u0628\u0627\u0633\u0643\u0627\u0644 (29 \u0645\u0644\u0644\u064a \u062b\u0627\u0646\u064a\u0629)<\/td><td>\u0646\u0645\u0648\u0630\u062c\u064a \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623\u060c \u0635\u0644\u0628<\/td><\/tr><\/tbody><\/table><\/figure><h3 class=\"wp-block-heading\">\u0627\u0644\u062e\u0648\u0627\u0635 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629<\/h3><p class=\"wp-block-paragraph\">\u0642\u0645 \u0628\u0641\u062d\u0635 \u0627\u0644\u062c\u062f\u0648\u0644 \u0623\u062f\u0646\u0627\u0647 \u0644\u0645\u0639\u0631\u0641\u0629 \u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629 \u0627\u0644\u0623\u0633\u0627\u0633\u064a\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409:<\/p><figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td><strong>\u0627\u0644\u062e\u0627\u0635\u064a\u0629 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629<\/strong><\/td><td><strong>\u0648\u0635\u0641<\/strong><\/td><td><strong>\u0623\u062f\u0627\u0621<\/strong><\/td><\/tr><tr><td>\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644<\/td><td>\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u062f\u0647\u0648\u0631 \u0627\u0644\u0628\u064a\u0626\u064a.<\/td><td>\u0645\u0639\u062a\u062f\u0644\u060c \u0623\u0642\u0644 \u0645\u0646 304 \u0648\u0644\u0643\u0646\u0647 \u0645\u0646\u0627\u0633\u0628 \u0644\u0644\u0628\u064a\u0626\u0627\u062a \u0648\u0627\u0644\u0639\u0648\u0627\u062f\u0645 \u0627\u0644\u0645\u0639\u062a\u062f\u0644\u0629.<\/td><\/tr><tr><td>\u062d\u0633\u0627\u0633\u064a\u0629 \u0627\u0644\u0631\u0642\u0645 \u0627\u0644\u0647\u064a\u062f\u0631\u0648\u062c\u064a\u0646\u064a<\/td><td>\u0627\u0644\u062a\u0641\u0627\u0639\u0644 \u0645\u0639 \u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u062d\u0645\u0636\u064a\u0629 \u0623\u0648 \u0627\u0644\u0642\u0627\u0639\u062f\u064a\u0629.<\/td><td>\u0645\u0633\u062a\u0642\u0631 \u0641\u064a \u0627\u0644\u0628\u064a\u0626\u0629 \u0627\u0644\u0645\u062d\u0627\u064a\u062f\u0629\/\u0627\u0644\u062d\u0645\u0636\u064a\u0629 \u0642\u0644\u064a\u0644\u0627\u064b\u061b \u0623\u0642\u0644 \u0645\u0642\u0627\u0648\u0645\u0629 \u0644\u0644\u0623\u062d\u0645\u0627\u0636 \u0627\u0644\u0642\u0648\u064a\u0629.<\/td><\/tr><tr><td>\u0627\u0644\u062a\u0641\u0627\u0639\u0644\u064a\u0629<\/td><td>\u0627\u0644\u0645\u064a\u0644 \u0644\u0644\u062a\u0641\u0627\u0639\u0644 \u0645\u0639 \u0627\u0644\u0645\u0648\u0627\u062f \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629 \u0623\u0648 \u0627\u0644\u063a\u0627\u0632\u0627\u062a.<\/td><td>\u062a\u0641\u0627\u0639\u0644\u064a\u0629 \u0645\u0646\u062e\u0641\u0636\u0629\u060c \u0645\u062b\u0627\u0644\u064a\u0629 \u0644\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0641\u064a \u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a.<\/td><\/tr><tr><td>\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u0623\u0643\u0633\u062f\u0629<\/td><td>\u0645\u0642\u0627\u0648\u0645\u0629 \u0644\u0644\u0623\u0643\u0633\u062f\u0629 \u0641\u064a \u062f\u0631\u062c\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u0639\u0627\u0644\u064a\u0629.<\/td><td>\u062c\u064a\u062f \u062d\u062a\u0649 675 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \u0628\u0634\u0643\u0644 \u0645\u0633\u062a\u0645\u0631\u060c \u0648815 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \u0628\u0634\u0643\u0644 \u0645\u062a\u0642\u0637\u0639.<\/td><\/tr><tr><td>\u0627\u0644\u062a\u062e\u0645\u064a\u0644<\/td><td>\u0627\u0644\u0642\u062f\u0631\u0629 \u0639\u0644\u0649 \u062a\u0643\u0648\u064a\u0646 \u0637\u0628\u0642\u0629 \u0623\u0643\u0633\u064a\u062f \u0648\u0627\u0642\u064a\u0629.<\/td><td>\u064a\u062a\u0634\u0643\u0644 \u0628\u0634\u0643\u0644 \u0637\u0628\u064a\u0639\u064a \u0648\u0644\u0643\u0646\u0647 \u0623\u0642\u0644 \u0641\u0639\u0627\u0644\u064a\u0629 \u0645\u0646 \u0627\u0644\u062f\u0631\u062c\u0627\u062a 304\/316.<\/td><\/tr><tr><td>\u0642\u0627\u0628\u0644\u064a\u0629 \u0627\u0644\u0627\u0634\u062a\u0639\u0627\u0644<\/td><td>\u0627\u0644\u0642\u062f\u0631\u0629 \u0639\u0644\u0649 \u0625\u0634\u0639\u0627\u0644 \u0627\u0644\u0646\u0627\u0631.<\/td><td>\u063a\u064a\u0631 \u0642\u0627\u0628\u0644\u0629 \u0644\u0644\u0627\u0634\u062a\u0639\u0627\u0644 \u0648\u0622\u0645\u0646\u0629 \u0644\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u0635\u0646\u0627\u0639\u064a.<\/td><\/tr><tr><td>\u0642\u0627\u0628\u0644\u064a\u0629 \u0627\u0644\u0627\u0634\u062a\u0639\u0627\u0644<\/td><td>\u0627\u0644\u0645\u064a\u0644 \u0625\u0644\u0649 \u0627\u0644\u0627\u0634\u062a\u0639\u0627\u0644 \u0641\u064a \u0627\u0644\u0646\u064a\u0631\u0627\u0646.<\/td><td>\u063a\u064a\u0631 \u0642\u0627\u0628\u0644\u0629 \u0644\u0644\u0627\u0634\u062a\u0639\u0627\u0644\u060c \u062a\u0636\u0645\u0646 \u0627\u0644\u0633\u0644\u0627\u0645\u0629 \u0645\u0646 \u0627\u0644\u062d\u0631\u0627\u0626\u0642.<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0648\u0627\u0644\u062a\u0622\u0643\u0644 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409<\/h2><h3 class=\"wp-block-heading\">\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u0629<\/h3><p class=\"wp-block-paragraph\">\u064a\u062a\u0645\u062a\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409 \u0628\u0645\u0642\u0627\u0648\u0645\u0629 \u062c\u064a\u062f\u0629 \u0644\u0644\u062d\u0631\u0627\u0631\u0629. \u0648\u064a\u0645\u0643\u0646\u0647 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0643\u0644\u0633 \u0641\u064a \u0627\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u0645\u0633\u062a\u0645\u0631 \u062d\u062a\u0649 675 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \u0648\u062d\u062a\u0649 815 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \u0641\u064a \u0627\u0644\u062e\u062f\u0645\u0629 \u0627\u0644\u0645\u062a\u0642\u0637\u0639\u0629.<\/p><h3 class=\"wp-block-heading\">\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644<\/h3><p class=\"wp-block-paragraph\">\u064a\u0648\u0641\u0631 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409 \u0645\u0642\u0627\u0648\u0645\u0629 \u062c\u064a\u062f\u0629 \u0644\u0644\u062a\u0622\u0643\u0644\u060c \u0648\u062e\u0627\u0635\u0629 \u0641\u064a \u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u062c\u0648\u064a\u0629 \u0648\u063a\u0627\u0632\u0627\u062a \u0627\u0644\u0639\u0627\u062f\u0645. \u0642\u062f \u062a\u062a\u0643\u0648\u0646 \u0637\u0628\u0642\u0629 \u062e\u0641\u064a\u0641\u0629 \u0645\u0646 \u0627\u0644\u0635\u062f\u0623\u060c \u0645\u0645\u0627 \u064a\u0633\u0627\u0639\u062f \u0639\u0644\u0649 \u0625\u0628\u0637\u0627\u0621 \u0627\u0644\u0645\u0632\u064a\u062f \u0645\u0646 \u0627\u0644\u062a\u0622\u0643\u0644 \u0648\u0644\u0643\u0646\u0647 \u064a\u0624\u062b\u0631 \u0639\u0644\u0649 \u0645\u0638\u0647\u0631 \u0627\u0644\u0633\u0637\u062d.&nbsp;<\/p><p class=\"wp-block-paragraph\">\u064a\u062a\u0645\u064a\u0632 \u0628\u0645\u0642\u0627\u0648\u0645\u0629 \u0623\u0641\u0636\u0644 \u0644\u0644\u062a\u0622\u0643\u0644 \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 410 \u0648\u0644\u0643\u0646\u0647 \u0644\u064a\u0633 \u0642\u0648\u064a\u0627\u064b \u0645\u062b\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 430 \u0630\u0648 \u0627\u0644\u0645\u062d\u062a\u0648\u0649 \u0627\u0644\u0639\u0627\u0644\u064a \u0645\u0646 \u0627\u0644\u0643\u0631\u0648\u0645. 409 \u0645\u0646\u0627\u0633\u0628 \u0644\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u063a\u064a\u0631 \u0627\u0644\u0632\u062e\u0631\u0641\u064a\u0629 \u062d\u064a\u062b \u062a\u0643\u0648\u0646 \u0647\u0646\u0627\u0643 \u062d\u0627\u062c\u0629 \u0625\u0644\u0649 \u062d\u0645\u0627\u064a\u0629 \u0645\u0639\u062a\u062f\u0644\u0629 \u0645\u0646 \u0627\u0644\u062a\u0622\u0643\u0644.<\/p><h2 class=\"wp-block-heading\">\u062e\u0635\u0627\u0626\u0635 \u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409<\/h2><h3 class=\"wp-block-heading\">\u0642\u0627\u0628\u0644\u064a\u0629 \u0627\u0644\u062a\u0634\u0643\u064a\u0644<\/h3><p class=\"wp-block-paragraph\">\u064a\u062a\u0645\u062a\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409 \u0628\u0642\u0627\u0628\u0644\u064a\u0629 \u062c\u064a\u062f\u0629 \u0644\u0644\u062a\u0634\u0643\u064a\u0644 \u0648\u0644\u0643\u0646\u0647 \u0623\u0642\u0644 \u0645\u0631\u0648\u0646\u0629 \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0623\u0648\u0633\u062a\u0646\u064a\u062a\u064a. \u064a\u062c\u0628 \u0625\u062c\u0631\u0627\u0621 \u0639\u0645\u0644\u064a\u0627\u062a \u0645\u062b\u0644 \u0627\u0644\u0633\u062d\u0628 \u0623\u0648 \u0627\u0644\u062a\u0645\u062f\u062f \u0641\u064a \u062f\u0631\u062c\u0629 \u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u063a\u0631\u0641\u0629 \u0644\u062a\u062d\u0642\u064a\u0642 \u0646\u062a\u0627\u0626\u062c \u0623\u0641\u0636\u0644. \u0642\u062f \u064a\u062d\u062a\u0627\u062c \u0625\u0644\u0649 \u0627\u0644\u0645\u0632\u064a\u062f \u0645\u0646 \u0627\u0644\u0642\u0648\u0629 \u0623\u0648 \u0623\u062f\u0648\u0627\u062a \u0645\u062a\u062e\u0635\u0635\u0629 \u0644\u0644\u062a\u0634\u0643\u064a\u0644. \u064a\u0645\u0643\u0646 \u0623\u0646 \u064a\u0633\u0627\u0639\u062f \u0627\u0644\u062a\u0644\u062f\u064a\u0646 \u0628\u0639\u062f \u0627\u0644\u062a\u0634\u0643\u064a\u0644 \u0641\u064a \u0627\u0633\u062a\u0639\u0627\u062f\u0629 \u062e\u0635\u0627\u0626\u0635\u0647 \u0628\u0633\u0628\u0628 \u0627\u0644\u062a\u0635\u0644\u0628 \u0627\u0644\u0646\u0627\u062a\u062c \u0639\u0646 \u0627\u0644\u0639\u0645\u0644.<\/p><h3 class=\"wp-block-heading\">\u0642\u0627\u0628\u0644\u064a\u0629 \u0627\u0644\u0644\u062d\u0627\u0645<\/h3><p class=\"wp-block-paragraph\">\u064a\u0648\u0641\u0631 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409 \u0642\u0627\u0628\u0644\u064a\u0629 \u0644\u062d\u0627\u0645 \u062c\u064a\u062f\u0629\u060c \u0648\u0644\u0643\u0646 \u0647\u0646\u0627\u0643 \u0628\u0639\u0636 \u0627\u0644\u0627\u062d\u062a\u064a\u0627\u0637\u0627\u062a \u0627\u0644\u0644\u0627\u0632\u0645\u0629.<\/p><ul class=\"wp-block-list\"><li>\u064a\u0624\u062f\u064a \u0627\u0644\u062a\u0633\u062e\u064a\u0646 \u0627\u0644\u0645\u0633\u0628\u0642 \u0625\u0644\u0649 \u062f\u0631\u062c\u0629 \u062d\u0631\u0627\u0631\u0629 \u062a\u062a\u0631\u0627\u0648\u062d \u0628\u064a\u0646 150 \u0648260 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \u0625\u0644\u0649 \u062a\u0642\u0644\u064a\u0644 \u0645\u062e\u0627\u0637\u0631 \u0627\u0644\u062a\u0634\u0642\u0642.&nbsp;<\/li>\n\n<li>\u064a\u062d\u0627\u0641\u0638 \u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0645\u0648\u0627\u062f \u0627\u0644\u062d\u0634\u0648 \u0627\u0644\u0645\u0646\u0627\u0633\u0628\u0629 \u0645\u062b\u0644 409 Cb\u060c \u0623\u0648 409 Ti\u060c \u0623\u0648 430L \u0639\u0644\u0649 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644 \u0648\u0627\u0644\u0642\u0648\u0629.<\/li>\n\n<li>\u064a\u0645\u0643\u0646 \u0623\u0646 \u064a\u0624\u062f\u064a \u0627\u0644\u062a\u0644\u062f\u064a\u0646 \u0628\u0639\u062f \u0627\u0644\u0644\u062d\u0627\u0645 \u0639\u0646\u062f \u062f\u0631\u062c\u0629 \u062d\u0631\u0627\u0631\u0629 760 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \u0625\u0644\u0649 \u062a\u062e\u0641\u064a\u0641 \u0627\u0644\u0636\u063a\u0637 \u0648\u062a\u062d\u0633\u064a\u0646 \u0627\u0644\u0644\u062f\u0648\u0646\u0629. <em>*\u0644\u0627 \u064a\u0644\u0632\u0645 \u0644\u0644\u0623\u062c\u0632\u0627\u0621 \u0627\u0644\u0645\u0644\u062d\u0648\u0645\u0629 \u0627\u0644\u0631\u0642\u064a\u0642\u0629.<\/em><\/li>\n\n<li>\u062d\u0627\u0641\u0638 \u0639\u0644\u0649 \u062f\u0631\u062c\u0629 \u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u062a\u062f\u0627\u062e\u0644 \u0623\u0642\u0644 \u0645\u0646 150 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \u0644\u0645\u0646\u0639 \u0627\u0644\u0647\u0634\u0627\u0634\u0629.<\/li>\n\n<li>\u0628\u0633\u0628\u0628 \u0627\u0631\u062a\u0641\u0627\u0639 \u0646\u0633\u0628\u0629 \u0627\u0644\u0643\u0631\u0648\u0645\u060c \u0647\u0646\u0627\u0643 \u062d\u0627\u062c\u0629 \u0625\u0644\u0649 \u063a\u0627\u0632\u0627\u062a \u0627\u0644\u062d\u0645\u0627\u064a\u0629 \u0645\u062b\u0644 \u0627\u0644\u0623\u0631\u062c\u0648\u0646 \u0644\u0645\u0646\u0639 \u0627\u0644\u0623\u0643\u0633\u062f\u0629.<\/li>\n\n<li>\u0639\u0627\u062f\u0629 \u0645\u0627 \u064a\u062a\u0645 \u0644\u062d\u0627\u0645 \u0623\u0646\u0627\u0628\u064a\u0628 \u0639\u0627\u062f\u0645 \u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a \u062f\u0648\u0646 \u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0645\u0639\u062f\u0646 \u062d\u0634\u0648.<\/li><\/ul><h3 class=\"wp-block-heading\">\u0642\u0627\u0628\u0644\u064a\u0629 \u0627\u0644\u062a\u0635\u0644\u0628<\/h3><p class=\"wp-block-paragraph\">\u064a\u062a\u0645\u064a\u0632 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409 \u0628\u0635\u0644\u0627\u0628\u0629 \u0645\u0646\u062e\u0641\u0636\u0629 \u0648\u0644\u0627 \u064a\u0645\u0643\u0646 \u062a\u0642\u0633\u064a\u062a\u0647 \u0628\u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629. \u064a\u0638\u0644 \u0637\u0631\u064a\u064b\u0627 \u062d\u062a\u0649 \u0628\u0639\u062f \u0627\u0644\u062a\u0633\u062e\u064a\u0646.<\/p><p class=\"wp-block-paragraph\">\u064a\u062a\u0645 \u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409 \u0639\u0627\u062f\u0629 \u0641\u064a \u062f\u0631\u062c\u0627\u062a \u062d\u0631\u0627\u0631\u0629 \u062a\u062a\u0631\u0627\u0648\u062d \u0628\u064a\u0646 790 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 - 900 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (1450 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a - 1650 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)\u060c \u0648\u0639\u0627\u062f\u0629 \u0645\u0627 \u064a\u062a\u0628\u0639 \u0630\u0644\u0643 \u0627\u0644\u062a\u0628\u0631\u064a\u062f \u0628\u0627\u0644\u0647\u0648\u0627\u0621.<\/p><h2 class=\"wp-block-heading\">\u0645\u0645\u064a\u0632\u0627\u062a \u0648\u0639\u064a\u0648\u0628 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409<\/h2><p class=\"wp-block-paragraph\">\u0641\u064a\u0645\u0627 \u064a\u0644\u064a \u0645\u0645\u064a\u0632\u0627\u062a \u0648\u0641\u0648\u0627\u0626\u062f \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409:<\/p><ol class=\"wp-block-list\"><li>\u0645\u0642\u0627\u0648\u0645\u0629 \u0645\u0645\u062a\u0627\u0632\u0629 \u0644\u0644\u062d\u0631\u0627\u0631\u0629\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647\u0627 \u0645\u062b\u0627\u0644\u064a\u0629 \u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u062f\u0631\u062c\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u0639\u0627\u0644\u064a\u0629.<\/li>\n\n<li>\u0645\u0642\u0627\u0648\u0645\u0629 \u062c\u064a\u062f\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0641\u064a \u0623\u0646\u0638\u0645\u0629 \u0627\u0644\u0639\u0627\u062f\u0645 \u0648\u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a.<\/li>\n\n<li>\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0623\u0643\u0633\u062f\u0629\u060c \u0648\u064a\u0639\u0645\u0644 \u0628\u0634\u0643\u0644 \u062c\u064a\u062f \u0641\u064a \u0627\u0644\u0638\u0631\u0648\u0641 \u0627\u0644\u0628\u064a\u0626\u064a\u0629 \u0627\u0644\u0645\u0639\u062a\u062f\u0644\u0629.<\/li>\n\n<li>\u062a\u0639\u062a\u0628\u0631 \u0628\u0623\u0633\u0639\u0627\u0631 \u0645\u0639\u0642\u0648\u0644\u0629 \u0645\u0642\u0627\u0631\u0646\u0629 \u0628\u0623\u0646\u0648\u0627\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0623\u062e\u0631\u0649\u060c \u0648\u062e\u0627\u0635\u0629 \u0641\u064a \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0643\u0628\u064a\u0631\u0629.<\/li>\n\n<li>\u0633\u0647\u0644\u0629 \u0627\u0644\u062a\u0635\u0646\u064a\u0639 \u0648\u0627\u0644\u0644\u062d\u0627\u0645\u060c \u0648\u0645\u0646\u0627\u0633\u0628\u0629 \u0644\u0644\u0639\u062f\u064a\u062f \u0645\u0646 \u0627\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0627\u062a \u0627\u0644\u0635\u0646\u0627\u0639\u064a\u0629.<\/li><\/ol><p class=\"wp-block-paragraph\">\u0641\u064a\u0645\u0627 \u064a\u0644\u064a \u0639\u064a\u0648\u0628 \u0648\u0642\u064a\u0648\u062f \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409:<\/p><ol class=\"wp-block-list\"><li>\u0645\u0642\u0627\u0648\u0645\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0623\u0642\u0644 \u0645\u0646 \u0627\u0644\u062f\u0631\u062c\u0627\u062a \u0645\u062b\u0644 304 \u0623\u0648 316.<\/li>\n\n<li>\u0642\u0648\u0629 \u0645\u0646\u062e\u0641\u0636\u0629 \u0641\u064a \u062f\u0631\u062c\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u0645\u0631\u062a\u0641\u0639\u0629 \u0645\u0642\u0627\u0631\u0646\u0629 \u0628\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0622\u062e\u0631.<\/li>\n\n<li>\u063a\u064a\u0631 \u0645\u0646\u0627\u0633\u0628 \u0644\u0644\u0628\u064a\u0626\u0627\u062a \u0634\u062f\u064a\u062f\u0629 \u0627\u0644\u062a\u0622\u0643\u0644\u060c \u0645\u062b\u0644 \u0627\u0644\u0635\u0646\u0627\u0639\u0627\u062a \u0627\u0644\u0628\u062d\u0631\u064a\u0629 \u0623\u0648 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629.<\/li>\n\n<li>\u0623\u0642\u0644 \u0645\u062a\u0627\u0646\u0629 \u0641\u064a \u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u0642\u0627\u0633\u064a\u0629\u060c \u0648\u062e\u0627\u0635\u0629 \u0639\u0646\u062f \u0627\u0644\u062a\u0639\u0631\u0636 \u0644\u0644\u0645\u0644\u062d.<\/li>\n\n<li>\u0642\u062f \u064a\u062a\u0637\u0644\u0628 \u0637\u0644\u0627\u0621\u064b \u0623\u0648 \u0645\u0639\u0627\u0644\u062c\u0629 \u0633\u0637\u062d\u064a\u0629 \u0644\u062a\u062d\u0633\u064a\u0646 \u0627\u0644\u0645\u0638\u0647\u0631 \u0648\u0637\u0648\u0644 \u0627\u0644\u0639\u0645\u0631.<\/li><\/ol><h2 class=\"wp-block-heading\">\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0634\u0627\u0626\u0639\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409<\/h2><p class=\"wp-block-paragraph\">\u0642\u0645 \u0628\u0645\u0631\u0627\u062c\u0639\u0629 \u0627\u0644\u062c\u062f\u0648\u0644 \u0623\u062f\u0646\u0627\u0647 \u0644\u0644\u062d\u0635\u0648\u0644 \u0639\u0644\u0649 \u0646\u0638\u0631\u0629 \u0633\u0631\u064a\u0639\u0629 \u0639\u0644\u0649 \u062a\u0637\u0628\u064a\u0642\u0627\u062a\u0647 \u0627\u0644\u0634\u0627\u0626\u0639\u0629:<\/p><figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td><strong>\u0635\u0646\u0627\u0639\u0629<\/strong><\/td><td><strong>\u0637\u0644\u0628<\/strong><\/td><td><strong>\u0644\u0645\u0627\u0630\u0627 \u064a\u0646\u0627\u0633\u0628\u0643<\/strong><\/td><\/tr><tr><td>\u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a<\/td><td>\u0623\u0646\u0638\u0645\u0629 \u0627\u0644\u0639\u0627\u062f\u0645\u060c \u0643\u0627\u062a\u0645\u0627\u062a \u0627\u0644\u0635\u0648\u062a\u060c \u0627\u0644\u0645\u062d\u0648\u0644\u0627\u062a \u0627\u0644\u062d\u0641\u0627\u0632\u0629\u060c \u0648\u0627\u0642\u064a\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629<\/td><td>\u0645\u0642\u0627\u0648\u0645\u0629 \u0639\u0627\u0644\u064a\u0629 \u0644\u0644\u062d\u0631\u0627\u0631\u0629\u060c \u0648\u0645\u0642\u0627\u0648\u0645\u0629 \u0644\u0644\u062a\u0622\u0643\u0644\u060c \u0648\u0641\u0639\u0627\u0644\u0629 \u0645\u0646 \u062d\u064a\u062b \u0627\u0644\u062a\u0643\u0644\u0641\u0629<\/td><\/tr><tr><td>\u0628\u0646\u0627\u0621<\/td><td>\u0627\u0644\u0623\u0633\u0642\u0641\u060c \u0643\u0633\u0648\u0629 \u0627\u0644\u062c\u062f\u0631\u0627\u0646\u060c \u0623\u0646\u0638\u0645\u0629 \u0627\u0644\u062a\u062f\u0641\u0626\u0629 \u0648\u0627\u0644\u062a\u0647\u0648\u064a\u0629 \u0648\u062a\u0643\u064a\u064a\u0641 \u0627\u0644\u0647\u0648\u0627\u0621\u060c \u0642\u0646\u0648\u0627\u062a \u0627\u0644\u062a\u0647\u0648\u064a\u0629<\/td><td>\u0645\u0642\u0627\u0648\u0645\u0629 \u062c\u064a\u062f\u0629 \u0644\u0644\u062a\u0622\u0643\u0644\u060c \u0648\u0627\u0644\u0645\u062a\u0627\u0646\u0629\u060c \u0648\u0633\u0647\u0648\u0644\u0629 \u0627\u0644\u062a\u0635\u0646\u064a\u0639<\/td><\/tr><tr><td>\u0632\u0631\u0627\u0639\u0629<\/td><td>\u0627\u0644\u0635\u0648\u0627\u0645\u0639\u060c \u0623\u062d\u0648\u0627\u0636 \u0627\u0644\u0623\u0639\u0644\u0627\u0641\u060c \u062e\u0632\u0627\u0646\u0627\u062a \u0627\u0644\u0645\u064a\u0627\u0647\u060c \u0627\u0644\u0645\u0639\u062f\u0627\u062a \u0627\u0644\u0632\u0631\u0627\u0639\u064a\u0629<\/td><td>\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644\u060c \u0627\u0644\u0642\u062f\u0631\u0629 \u0639\u0644\u0649 \u062a\u062d\u0645\u0644 \u0627\u0644\u062a\u0643\u0627\u0644\u064a\u0641\u060c \u0633\u0647\u0648\u0644\u0629 \u0627\u0644\u0644\u062d\u0627\u0645<\/td><\/tr><tr><td>\u062a\u0648\u0644\u064a\u062f \u0627\u0644\u0637\u0627\u0642\u0629<\/td><td>\u0639\u0648\u0627\u062f\u0645 \u062a\u0648\u0631\u0628\u064a\u0646\u0627\u062a \u0627\u0644\u063a\u0627\u0632\u060c \u0623\u0646\u0638\u0645\u0629 \u0627\u0644\u063a\u0644\u0627\u064a\u0627\u062a\u060c \u0627\u0644\u0645\u0628\u0627\u062f\u0644\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629\u060c \u0642\u0646\u0648\u0627\u062a \u063a\u0627\u0632\u0627\u062a \u0627\u0644\u0645\u062f\u0627\u062e\u0646<\/td><td>\u0645\u0642\u0627\u0648\u0645\u0629 \u0644\u0644\u062d\u0631\u0627\u0631\u0629 \u0648\u0627\u0644\u062a\u0622\u0643\u0644\u060c \u0645\u0646\u0627\u0633\u0628\u0629 \u0644\u0644\u0628\u064a\u0626\u0627\u062a \u0630\u0627\u062a \u062f\u0631\u062c\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u0639\u0627\u0644\u064a\u0629<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u0627\u0644\u062f\u0631\u062c\u0627\u062a \u0627\u0644\u0645\u0643\u0627\u0641\u0626\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409 \u0641\u064a \u0628\u0644\u062f\u0627\u0646 \u0648\u0645\u0646\u0627\u0637\u0642 \u0645\u062e\u062a\u0644\u0641\u0629<\/h2><p class=\"wp-block-paragraph\">\u0641\u064a\u0645\u0627 \u064a\u0644\u064a \u0628\u0639\u0636 \u0627\u0644\u062f\u0631\u062c\u0627\u062a \u0627\u0644\u0645\u0643\u0627\u0641\u0626\u0629 \u0627\u0644\u0634\u0627\u0626\u0639\u0629 \u0644\u0640SS 409 \u0641\u064a \u0628\u0644\u062f\u0627\u0646 \u0648\u0645\u0646\u0627\u0637\u0642 \u0645\u062e\u062a\u0644\u0641\u0629:<\/p><figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td><strong>\u062f\u0648\u0644\u0629<\/strong><\/td><td><strong>\u0627\u0644\u0645\u0639\u064a\u0627\u0631\/\u0627\u0644\u0645\u0648\u0627\u0635\u0641\u0627\u062a<\/strong><\/td><td><strong>\u0627\u0644\u062f\u0631\u062c\u0629 \u0627\u0644\u0645\u0643\u0627\u0641\u0626\u0629<\/strong><\/td><\/tr><tr><td>\u0627\u0644\u0627\u062a\u062d\u0627\u062f \u0627\u0644\u0623\u0648\u0631\u0648\u0628\u064a<\/td><td>EN 10088-2<\/td><td>X2CrTi12 (1.4512)<\/td><\/tr><tr><td>\u0627\u0644\u0648\u0644\u0627\u064a\u0627\u062a \u0627\u0644\u0645\u062a\u062d\u062f\u0629 \u0627\u0644\u0623\u0645\u0631\u064a\u0643\u064a\u0629<\/td><td>\u0645\u0639\u0627\u064a\u064a\u0631 ASTM A240\/A240M<\/td><td>409 \/ \u063340900<\/td><\/tr><tr><td>\u0627\u0644\u064a\u0627\u0628\u0627\u0646<\/td><td>\u062c\u064a \u0627\u064a \u0627\u0633 \u062c\u064a 4304<\/td><td>\u0625\u0633 \u064a\u0648 \u0625\u0633 409 \u0625\u0644<\/td><\/tr><tr><td>\u0641\u0631\u0646\u0633\u0627<\/td><td>\u0646 \u0641 \u0623 35-573<\/td><td>Z3CT12<\/td><\/tr><tr><td>\u0627\u0646\u062c\u0644\u062a\u0631\u0627<\/td><td>BS 1449-2<\/td><td>409\u0633<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u0627\u0644\u0641\u0631\u0642 \u0628\u064a\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409 \u0648304 \u0648316<\/h2><p class=\"wp-block-paragraph\">\u0642\u0645 \u0628\u0645\u0631\u0627\u062c\u0639\u0629 \u0627\u0644\u062c\u062f\u0648\u0644 \u0623\u062f\u0646\u0627\u0647 \u0644\u0625\u062c\u0631\u0627\u0621 \u0645\u0642\u0627\u0631\u0646\u0629 \u0633\u0631\u064a\u0639\u0629 \u0628\u064a\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409 \u0648304 \u0648316:<\/p><figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td><strong>\u0645\u0644\u0643\u064a\u0629<\/strong><\/td><td><strong>409<\/strong><\/td><td><strong><a href=\"https:\/\/steelprogroup.com\/ar\/stainless-steel\/grades\/grade-304\/\">304<\/a><\/strong><\/td><td><strong><a href=\"https:\/\/steelprogroup.com\/ar\/stainless-steel\/grades\/grade-316\/\" target=\"_blank\" data-type=\"post\" data-id=\"10280\" rel=\"noreferrer noopener\">316<\/a><\/strong><\/td><\/tr><tr><td><strong>\u064a\u0643\u062a\u0628<\/strong><\/td><td>\u0627\u0644\u0641\u0631\u064a\u062a\u064a\u0629<\/td><td>\u0623\u0648\u0633\u062a\u064a\u0646\u064a\u062a\u064a<\/td><td>\u0623\u0648\u0633\u062a\u064a\u0646\u064a\u062a\u064a<\/td><\/tr><tr><td><strong>\u0627\u0644\u0628\u0646\u064a\u0629 \u0627\u0644\u0628\u0644\u0648\u0631\u064a\u0629<\/strong><\/td><td>\u0645\u0643\u0639\u0628 \u0645\u0631\u0643\u0632 \u0627\u0644\u062c\u0633\u0645 (BCC)<\/td><td>\u0645\u0643\u0639\u0628 \u0645\u0631\u0643\u0632 \u0627\u0644\u0648\u062c\u0647 (FCC)<\/td><td>\u0645\u0643\u0639\u0628 \u0645\u0631\u0643\u0632 \u0627\u0644\u0648\u062c\u0647 (FCC)<\/td><\/tr><tr><td><strong>\u0627\u0644\u062a\u0631\u0643\u064a\u0628 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a<\/strong><\/td><td>Cr: 11.13%\u060c Ti: 0.75%<\/td><td>\u0643\u0631: 18-20%\u060c \u0646\u064a: 8-10.5%<\/td><td>\u0627\u0644\u0643\u0631\u0648\u0645: .18%\u060c \u0645\u0648: .3%\u060c \u0646\u064a: .14%<\/td><\/tr><tr><td><strong>\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644<\/strong><\/td><td>\u0645\u0639\u062a\u062f\u0644\u061b \u0623\u0642\u0644 \u0645\u0646 304 \u0648316<\/td><td>\u0645\u0642\u0627\u0648\u0645\u0629 \u062c\u064a\u062f\u0629 \u0644\u0644\u062a\u0622\u0643\u0644\u061b \u0627\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u0639\u0627\u0645<\/td><td>\u0645\u0642\u0627\u0648\u0645\u0629 \u0645\u0645\u062a\u0627\u0632\u0629 \u0644\u0644\u062a\u0622\u0643\u0644\u060c \u0648\u062e\u0627\u0635\u0629 \u0641\u064a \u0628\u064a\u0626\u0627\u062a \u0627\u0644\u0643\u0644\u0648\u0631\u064a\u062f<\/td><\/tr><tr><td><strong>\u0642\u0648\u0629 \u0627\u0644\u0634\u062f<\/strong><\/td><td>448 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644 (65 \u0643\u064a\u0644\u0648\u0628\u0627\u0633\u0643\u0627\u0644)<\/td><td>505 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644 (73.2 \u0643\u064a\u0644\u0648\u0628\u0627\u0633\u0643\u0627\u0644)<\/td><td>580 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644 (84.1 \u0643\u064a\u0644\u0648\u0628\u0627\u0633\u0643\u0627\u0644)<\/td><\/tr><tr><td><strong>\u0642\u0648\u0629 \u0627\u0644\u062e\u0636\u0648\u0639<\/strong><\/td><td>238 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644 (34.5 \u0643\u064a\u0644\u0648\u0628\u0627\u0633\u0643\u0627\u0644)<\/td><td>215 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644 (31.2 \u0643\u064a\u0644\u0648\u0628\u0627\u0633\u0643\u0627\u0644)<\/td><td>290 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644 (42.1 \u0643\u064a\u0644\u0648\u0628\u0627\u0633\u0643\u0627\u0644)<\/td><\/tr><tr><td><strong>\u0635\u0644\u0627\u0628\u0629 \u0631\u0648\u0643\u0648\u064a\u0644 (HRB)<\/strong><\/td><td>75<\/td><td>70<\/td><td>79<\/td><\/tr><tr><td><strong>\u0642\u0627\u0628\u0644\u064a\u0629 \u0627\u0644\u0644\u062d\u0627\u0645<\/strong><\/td><td>\u062c\u064a\u062f\u060c \u0644\u0643\u0646\u0647 \u064a\u062a\u0637\u0644\u0628 \u0627\u0644\u062a\u0633\u062e\u064a\u0646 \u0627\u0644\u0645\u0633\u0628\u0642<\/td><td>\u0645\u0645\u062a\u0627\u0632 \u0648\u0633\u0647\u0644 \u0627\u0644\u0644\u062d\u0627\u0645<\/td><td>\u0645\u0645\u062a\u0627\u0632 \u0648\u0633\u0647\u0644 \u0627\u0644\u0644\u062d\u0627\u0645<\/td><\/tr><tr><td><strong>\u064a\u0643\u0644\u0641<\/strong><\/td><td>\u0642\u0644\u064a\u0644<\/td><td>\u0645\u0639\u062a\u062f\u0644<\/td><td>\u0639\u0627\u0644\u064a<\/td><\/tr><tr><td><strong>\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a<\/strong><\/td><td>\u0623\u0646\u0638\u0645\u0629 \u0639\u0627\u062f\u0645 \u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a \u0648\u0627\u0644\u0645\u0628\u0627\u062f\u0644\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629<\/td><td>\u0645\u0639\u062f\u0627\u062a \u0627\u0644\u0645\u0637\u0628\u062e\u060c \u062d\u0627\u0648\u064a\u0627\u062a \u0627\u0644\u0645\u0648\u0627\u062f \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629<\/td><td>\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0628\u062d\u0631\u064a\u0629\u060c \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629\u060c \u0627\u0644\u0645\u0639\u062f\u0627\u062a \u0627\u0644\u0635\u064a\u062f\u0644\u0627\u0646\u064a\u0629<\/td><\/tr><\/tbody><\/table><\/figure><p class=\"wp-block-paragraph\"><strong>\u0642\u0631\u0627\u0621\u0629 \u0625\u0636\u0627\u0641\u064a\u0629<\/strong><br><a href=\"https:\/\/steelprogroup.com\/ar\/stainless-steel\/grades\/comparisons\/304-vs-409\/\" target=\"_blank\" data-type=\"post\" data-id=\"10411\" rel=\"noreferrer noopener\">304 \u0645\u0642\u0627\u0628\u0644 409 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623<\/a><\/p><h2 class=\"wp-block-heading\">\u0645\u0627 \u0642\u062f \u064a\u062b\u064a\u0631 \u0642\u0644\u0642\u0643 \u0623\u064a\u0636\u064b\u0627<\/h2><h3 class=\"wp-block-heading\">\u0647\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409 \u0642\u0627\u0628\u0644 \u0644\u0644\u062d\u0627\u0645\u061f<\/h3><p class=\"wp-block-paragraph\">\u0646\u0639\u0645\u060c \u064a\u0645\u0643\u0646 \u0644\u062d\u0627\u0645 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409. \u0648\u064a\u064f\u0633\u062a\u062e\u062f\u0645 \u063a\u0627\u0644\u0628\u064b\u0627 \u0641\u064a \u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0645\u062b\u0644 \u0623\u0646\u0638\u0645\u0629 \u0627\u0644\u0639\u0627\u062f\u0645 \u062d\u064a\u062b \u064a\u0643\u0648\u0646 \u0627\u0644\u0644\u062d\u0627\u0645 \u0636\u0631\u0648\u0631\u064a\u064b\u0627.<\/p><h3 class=\"wp-block-heading\">\u0647\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409 \u0645\u063a\u0646\u0627\u0637\u064a\u0633\u064a\u061f<\/h3><p class=\"wp-block-paragraph\">\u0646\u0639\u0645\u060c \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409 \u0645\u063a\u0646\u0627\u0637\u064a\u0633\u064a\u060c \u0648\u0647\u0648 \u0639\u0628\u0627\u0631\u0629 \u0639\u0646 \u0641\u0648\u0644\u0627\u0630 \u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0645\u0646 \u0627\u0644\u0646\u0648\u0639 \u0627\u0644\u0641\u0631\u064a\u062a\u064a\u060c \u0648\u0627\u0644\u0630\u064a \u064a\u062d\u062a\u0641\u0638 \u0639\u0645\u0648\u0645\u064b\u0627 \u0628\u062e\u0635\u0627\u0626\u0635 \u0645\u063a\u0646\u0627\u0637\u064a\u0633\u064a\u0629.<\/p><p class=\"wp-block-paragraph\"><strong>\u0642\u0631\u0627\u0621\u0629 \u0630\u0627\u062a \u0635\u0644\u0629<\/strong><\/p><p class=\"wp-block-paragraph\"><a href=\"https:\/\/steelprogroup.com\/ar\/stainless-steel\/properties\/magnetic\/\">\u0647\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0645\u063a\u0646\u0627\u0637\u064a\u0633\u064a\u061f<\/a><\/p><h3 class=\"wp-block-heading\">\u0643\u064a\u0641\u064a\u0629 \u062d\u0645\u0627\u064a\u0629 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409 \u0645\u0646 \u0627\u0644\u0635\u062f\u0623\u061f<\/h3><p class=\"wp-block-paragraph\">\u0644\u0644\u062d\u0641\u0627\u0638 \u0639\u0644\u0649 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409 \u0645\u0646 \u0627\u0644\u0635\u062f\u0623\u060c \u0627\u062d\u0631\u0635 \u0639\u0644\u0649 \u062a\u0646\u0638\u064a\u0641\u0647 \u0648\u062c\u0641\u0627\u0641\u0647. \u0636\u0639 \u0637\u0628\u0642\u0627\u062a \u0648\u0627\u0642\u064a\u0629 \u0648\u062a\u062c\u0646\u0628 \u0627\u0644\u062a\u0639\u0631\u0636 \u0644\u0644\u0645\u0648\u0627\u062f \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629 \u0627\u0644\u0642\u0627\u0633\u064a\u0629 \u0623\u0648 \u0627\u0644\u0645\u064a\u0627\u0647 \u0627\u0644\u0645\u0627\u0644\u062d\u0629. \u062a\u0633\u0627\u0639\u062f \u0627\u0644\u0635\u064a\u0627\u0646\u0629 \u0627\u0644\u0645\u0646\u062a\u0638\u0645\u0629\u060c \u0645\u062b\u0644 \u0625\u0632\u0627\u0644\u0629 \u0627\u0644\u0645\u0644\u0648\u062b\u0627\u062a \u0627\u0644\u0633\u0637\u062d\u064a\u0629\u060c \u0641\u064a \u0645\u0646\u0639 \u0627\u0644\u062a\u0622\u0643\u0644.<\/p><p class=\"wp-block-paragraph\"><strong>\u0642\u0631\u0627\u0621\u0629 \u0630\u0627\u062a \u0635\u0644\u0629<\/strong><\/p><p class=\"wp-block-paragraph\"><a href=\"https:\/\/steelprogroup.com\/ar\/stainless-steel\/rust\/\">\u0647\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u064a\u0635\u062f\u0623 \u0648\u0643\u064a\u0641 \u064a\u0645\u0643\u0646\u0643 \u062d\u0644 \u0647\u0630\u0647 \u0627\u0644\u0645\u0634\u0643\u0644\u0629\u061f<\/a><\/p><h3 class=\"wp-block-heading\">\u0647\u0644 409 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0645\u0646\u0627\u0633\u0628 \u0644\u0644\u0637\u0639\u0627\u0645\u061f<\/h3><p class=\"wp-block-paragraph\">\u0644\u0627\u060c \u0644\u0627 \u064a\u0639\u062a\u0628\u0631 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409 \u0635\u0627\u0644\u062d\u064b\u0627 \u0644\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0641\u064a \u0627\u0644\u0623\u063a\u0630\u064a\u0629. \u0648\u064a\u064f\u0633\u062a\u062e\u062f\u0645 \u0641\u064a \u0627\u0644\u0645\u0642\u0627\u0645 \u0627\u0644\u0623\u0648\u0644 \u0641\u064a \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0635\u0646\u0627\u0639\u064a\u0629 \u0648\u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a. \u0648\u0628\u0627\u0644\u0646\u0633\u0628\u0629 \u0644\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0645\u062e\u0635\u0635\u0629 \u0644\u0644\u0623\u063a\u0630\u064a\u0629\u060c \u064a\u0641\u0636\u0644 \u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 304 \u0623\u0648 316 \u0646\u0638\u0631\u064b\u0627 \u0644\u0645\u0642\u0627\u0648\u0645\u062a\u0647 \u0627\u0644\u0641\u0627\u0626\u0642\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0648\u0627\u0645\u062a\u062b\u0627\u0644\u0647 \u0644\u0645\u0639\u0627\u064a\u064a\u0631 \u0633\u0644\u0627\u0645\u0629 \u0627\u0644\u0623\u063a\u0630\u064a\u0629.<\/p><h2 class=\"wp-block-heading\">\u0627\u0644\u0645\u0644\u062e\u0635 \u0648 \u0627\u0644\u0645\u0632\u064a\u062f<\/h2><p class=\"wp-block-paragraph\">\u062a\u0634\u0631\u062d \u0647\u0630\u0647 \u0627\u0644\u0645\u0642\u0627\u0644\u0629 \u0628\u0625\u064a\u062c\u0627\u0632 \u062a\u0639\u0631\u064a\u0641 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409 \u0648\u062a\u0631\u0643\u064a\u0628\u0647 \u0648\u062e\u0635\u0627\u0626\u0635\u0647 \u0648\u062e\u0635\u0627\u0626\u0635 \u0645\u0639\u0627\u0644\u062c\u062a\u0647 \u0648\u062a\u0637\u0628\u064a\u0642\u0627\u062a\u0647 \u0648\u063a\u064a\u0631 \u0630\u0644\u0643 \u0645\u0646 \u0627\u0644\u062c\u0648\u0627\u0646\u0628 \u0627\u0644\u0645\u0647\u0645\u0629. \u0644\u0645\u0639\u0631\u0641\u0629 \u0627\u0644\u0645\u0632\u064a\u062f \u0639\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0623\u0648 \u0623\u0646\u0648\u0627\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0623\u062e\u0631\u0649\u060c \u0631\u0627\u062c\u0639 <a href=\"https:\/\/steelprogroup.com\/ar\/blog\/\">\u0645\u062f\u0648\u0646\u062a\u0646\u0627<\/a> \u0623\u0648 <a href=\"https:\/\/steelprogroup.com\/ar\/contact-us\/\">\u0627\u062a\u0635\u0644 \u0628\u062e\u0628\u0631\u0627\u0626\u0646\u0627 \u0641\u064a \u0645\u062c\u0627\u0644 \u0627\u0644\u0645\u0639\u0627\u062f\u0646<\/a>.<\/p><p class=\"wp-block-paragraph\">\u0628\u0627\u0639\u062a\u0628\u0627\u0631\u0646\u0627 \u0634\u0631\u0643\u0629 \u0631\u0627\u0626\u062f\u0629 \u0641\u064a \u062a\u0635\u0646\u064a\u0639 \u0648\u062a\u0648\u0631\u064a\u062f \u062d\u0644\u0648\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u062a\u062e\u0635\u0635\u060c \u0641\u0625\u0646\u0646\u0627 \u0646\u0642\u062f\u0645 \u062d\u0644\u0648\u0644 \u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0645\u062a\u0639\u062f\u062f\u0629 \u0627\u0644\u0635\u0646\u0627\u0639\u0627\u062a \u0648\u062e\u062f\u0645\u0627\u062a \u0645\u062e\u0635\u0635\u0629 \u0645\u0639 \u0636\u0645\u0627\u0646 \u0627\u0644\u062c\u0648\u062f\u0629 100%\u060c \u0645\u0644\u062a\u0632\u0645\u0648\u0646 \u0628\u0627\u0644\u0646\u0645\u0648 \u0645\u0639 \u0639\u0645\u0644\u0627\u0626\u0646\u0627. \u0642\u0645 \u0628\u0632\u064a\u0627\u0631\u0629 <a href=\"https:\/\/steelprogroup.com\/ar\">\u0645\u0648\u0642\u0639\u0646\u0627<\/a> \u0644\u062a\u0639\u0644\u0645 \u0627\u0644\u0645\u0632\u064a\u062f\u060c \u0623\u0648 <a href=\"https:\/\/steelprogroup.com\/ar\/contact-us\/\">\u0623\u0631\u0633\u0644 \u0644\u0646\u0627 \u0639\u0631\u0636 \u0623\u0633\u0639\u0627\u0631<\/a>\u0648\u0633\u0648\u0641 \u0646\u062a\u0635\u0644 \u0628\u0643 \u0642\u0631\u064a\u0628\u0627!<\/p>","protected":false},"excerpt":{"rendered":"<p>\u0645\u0627 \u0647\u0648 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 409\u061f 409\u060c \u0627\u0644\u0645\u0639\u0631\u0648\u0641 \u0623\u064a\u0636\u064b\u0627 \u0628\u0627\u0633\u0645 UNS S40900\u060c \u0647\u0648 \u0641\u0648\u0644\u0627\u0630 \u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0645\u0646 \u0633\u0644\u0633\u0644\u0629 400 \u064a\u062a\u0643\u0648\u0646 \u0641\u064a \u0627\u0644\u0645\u0642\u0627\u0645 \u0627\u0644\u0623\u0648\u0644 \u0645\u0646 [\u2026]<\/p>","protected":false},"author":1,"featured_media":10287,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"_eb_attr":"","rank_math_lock_modified_date":false,"site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"categories":[4191,112],"tags":[],"class_list":["post-10290","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-grades","category-stainless-steel"],"acf":[],"_links":{"self":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts\/10290","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/comments?post=10290"}],"version-history":[{"count":0,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts\/10290\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/media\/10287"}],"wp:attachment":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/media?parent=10290"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/categories?post=10290"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/tags?post=10290"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}