{"id":10689,"date":"2024-09-24T11:56:00","date_gmt":"2024-09-24T03:56:00","guid":{"rendered":"https:\/\/app11147.cloudwayssites.com\/?p=10689"},"modified":"2024-11-20T17:27:57","modified_gmt":"2024-11-20T09:27:57","slug":"mill","status":"publish","type":"post","link":"https:\/\/steelprogroup.com\/ar\/stainless-steel\/finish\/mill\/","title":{"rendered":"\u0634\u0631\u062d \u062a\u0634\u0637\u064a\u0628 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623"},"content":{"rendered":"<p class=\"wp-block-paragraph\">\u0625\u0646 \u0641\u0647\u0645 \u0627\u0644\u0645\u0641\u0627\u0647\u064a\u0645 \u0627\u0644\u0623\u0633\u0627\u0633\u064a\u0629 \u0644\u0644\u0637\u062d\u0646 \u0648\u0639\u0645\u0644\u064a\u0629 \u0627\u0644\u062a\u0635\u0646\u064a\u0639 \u0648\u0645\u0642\u0627\u0631\u0646\u062a\u0647\u0627 \u0628\u0645\u0639\u0627\u0644\u062c\u0627\u062a \u0627\u0644\u0623\u0633\u0637\u062d \u0627\u0644\u0623\u062e\u0631\u0649 \u0623\u0645\u0631 \u0636\u0631\u0648\u0631\u064a \u0644\u0627\u062e\u062a\u064a\u0627\u0631 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0645\u0646\u0627\u0633\u0628 \u0644\u062a\u0637\u0628\u064a\u0642\u0643. \u0641\u064a \u0647\u0630\u0647 \u0627\u0644\u0645\u0642\u0627\u0644\u0629\u060c \u0633\u0646\u062a\u0639\u0645\u0642 \u0641\u064a \u062a\u0641\u0627\u0635\u064a\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0645\u062f\u0644\u0641\u0646 \u0639\u0644\u0649 \u0627\u0644\u0633\u0637\u062d\u060c \u0648\u0639\u0645\u0644\u064a\u062a\u0647 \u0627\u0644\u0639\u0627\u0645\u0629\u060c \u0648\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0645\u062f\u0644\u0641\u0646\u060c \u0648\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a\u060c \u0648\u0627\u0644\u0635\u064a\u0627\u0646\u0629. \u0633\u0646\u0642\u0627\u0631\u0646 \u0623\u064a\u0636\u064b\u0627 \u0627\u0644\u0623\u0633\u0637\u062d \u0627\u0644\u0645\u062f\u0644\u0641\u0646\u0629 \u0628\u0627\u0644\u0623\u0633\u0637\u062d \u0627\u0644\u0645\u0635\u0642\u0648\u0644\u0629 \u0648\u0627\u0644\u0645\u0641\u0631\u0648\u0634\u0629.<\/p><h2 class=\"wp-block-heading\">\u0645\u0627 \u0647\u0648 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0645\u0637\u0644\u064a\u061f<\/h2><p class=\"wp-block-paragraph\">\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0645\u0637\u0644\u064a \u0647\u0648 \u0627\u0644\u062a\u0634\u0637\u064a\u0628 \u0627\u0644\u0623\u0635\u0644\u064a \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0628\u0639\u062f \u062a\u0635\u0646\u064a\u0639\u0647 \u0641\u064a \u0627\u0644\u0645\u0635\u0646\u0639 \u0648\u0647\u0648 \u0627\u0644\u0634\u0643\u0644 \u0627\u0644\u0623\u0633\u0627\u0633\u064a \u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0633\u0637\u062d. \u0644\u0645 \u064a\u062e\u0636\u0639 \u0644\u062a\u0644\u0645\u064a\u0639 \u0623\u0648 \u0645\u0639\u0627\u0644\u062c\u0629 \u0625\u0636\u0627\u0641\u064a\u0629 \u0648\u0644\u0647 \u0645\u0638\u0647\u0631 \u0628\u0627\u0647\u062a \u0648\u063a\u064a\u0631 \u0644\u0627\u0645\u0639 \u0645\u0639 \u0627\u062e\u062a\u0644\u0627\u0641\u0627\u062a \u0637\u0641\u064a\u0641\u0629 \u0641\u064a \u0627\u0644\u0645\u0644\u0645\u0633 \u0646\u0627\u062a\u062c\u0629 \u0639\u0646 \u0639\u0645\u0644\u064a\u0629 \u0627\u0644\u062f\u0631\u0641\u0644\u0629. \u0647\u0630\u0627 \u0627\u0644\u062a\u0634\u0637\u064a\u0628 \u0645\u0641\u0636\u0644 \u0644\u062c\u0645\u0627\u0644\u0647 \u0627\u0644\u0635\u0646\u0627\u0639\u064a \u0648\u0645\u062a\u0627\u0646\u062a\u0647 \u0648\u0641\u0639\u0627\u0644\u064a\u062a\u0647 \u0645\u0646 \u062d\u064a\u062b \u0627\u0644\u062a\u0643\u0644\u0641\u0629.<\/p><h2 class=\"wp-block-heading\">\u0627\u0644\u0639\u0645\u0644\u064a\u0629 \u0627\u0644\u0639\u0627\u0645\u0629 \u0644\u0644\u0637\u062d\u0646<\/h2><p class=\"wp-block-paragraph\">\u064a\u0645\u0643\u0646 \u062a\u0642\u0633\u064a\u0645 \u0639\u0645\u0644\u064a\u0629 \u0627\u0644\u0637\u062d\u0646 \u0625\u0644\u0649 \u0639\u062f\u0629 \u0645\u0631\u0627\u062d\u0644 \u0631\u0626\u064a\u0633\u064a\u0629\u060c \u0648\u0644\u0643\u0644 \u0645\u0646\u0647\u0627 \u062a\u0623\u062b\u064a\u0631 \u0645\u0647\u0645 \u0639\u0644\u0649 \u0627\u0644\u062a\u0623\u062b\u064a\u0631 \u0627\u0644\u0633\u0637\u062d\u064a \u0627\u0644\u0646\u0647\u0627\u0626\u064a:<\/p><p class=\"wp-block-paragraph\">\u0625\u0639\u062f\u0627\u062f \u0627\u0644\u0645\u0648\u0627\u062f \u0627\u0644\u062e\u0627\u0645: \u062a\u0628\u062f\u0623 \u0639\u0645\u0644\u064a\u0629 \u0627\u0644\u0637\u062d\u0646 \u0628\u0627\u062e\u062a\u064a\u0627\u0631 \u0627\u0644\u0645\u0648\u0627\u062f \u0627\u0644\u062e\u0627\u0645. \u0648\u0639\u0627\u062f\u0629 \u0645\u0627 \u064a\u062a\u0645 \u0627\u062e\u062a\u064a\u0627\u0631 \u0635\u0641\u0627\u0626\u062d \u0623\u0648 \u0634\u0631\u0627\u0626\u062d \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0639\u0627\u0644\u064a\u0629 \u0627\u0644\u062c\u0648\u062f\u0629 \u0643\u0645\u0648\u0627\u062f \u0623\u0633\u0627\u0633\u064a\u0629 \u0644\u0636\u0645\u0627\u0646 \u0623\u062f\u0627\u0621 \u0627\u0644\u0645\u0646\u062a\u062c \u0627\u0644\u0646\u0647\u0627\u0626\u064a.<\/p><p class=\"wp-block-paragraph\">\u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629 \u0627\u0644\u0623\u0648\u0644\u064a\u0629: \u062a\u062a\u0636\u0645\u0646 \u0645\u0631\u062d\u0644\u0629 \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629 \u0627\u0644\u0623\u0648\u0644\u064a\u0629 \u0639\u0645\u0644\u064a\u0629 \u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0633\u0627\u062e\u0646\u0629\u060c \u0648\u0627\u0644\u062a\u064a \u062a\u062a\u0645 \u0639\u0627\u062f\u0629 \u0641\u064a \u0638\u0644 \u0638\u0631\u0648\u0641 \u062f\u0631\u062c\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u0639\u0627\u0644\u064a\u0629 \u0648\u062a\u0647\u062f\u0641 \u0625\u0644\u0649 \u062a\u0642\u0644\u064a\u0644 \u0633\u0645\u0643 \u0627\u0644\u0645\u0627\u062f\u0629 \u0627\u0644\u0645\u0639\u062f\u0646\u064a\u0629 \u0645\u0646 \u062e\u0644\u0627\u0644 \u0627\u0644\u062a\u0633\u062e\u064a\u0646 \u0648\u0627\u0644\u062f\u0631\u0641\u0644\u0629\u060c \u0648\u0627\u0644\u0642\u0636\u0627\u0621 \u0628\u0634\u0643\u0644 \u0641\u0639\u0627\u0644 \u0639\u0644\u0649 \u0627\u0644\u0625\u062c\u0647\u0627\u062f \u0627\u0644\u0645\u062a\u0631\u0627\u0643\u0645 \u062f\u0627\u062e\u0644\u0647\u0627.<\/p><p class=\"wp-block-paragraph\">\u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0628\u0627\u0631\u062f\u0629: \u064a\u062a\u0645 \u0625\u062c\u0631\u0627\u0621 \u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0628\u0627\u0631\u062f\u0629 \u0639\u0644\u0649 \u0623\u0633\u0627\u0633 \u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0633\u0627\u062e\u0646\u0629 \u0644\u062a\u0642\u0644\u064a\u0644 \u0633\u0645\u0643 \u0627\u0644\u0645\u0627\u062f\u0629 \u0628\u0634\u0643\u0644 \u0623\u0643\u0628\u0631 \u0648\u062a\u062d\u0633\u064a\u0646 \u062a\u0634\u0637\u064a\u0628 \u0633\u0637\u062d\u0647\u0627. \u0639\u0627\u062f\u0629 \u0645\u0627 \u064a\u0643\u0648\u0646 \u0627\u0644\u0633\u0637\u062d \u0628\u0639\u062f \u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0628\u0627\u0631\u062f\u0629 \u0623\u0643\u062b\u0631 \u0633\u0644\u0627\u0633\u0629\u060c \u0644\u0643\u0646\u0647 \u0644\u0627 \u064a\u0632\u0627\u0644 \u064a\u062d\u062a\u0641\u0638 \u0628\u0627\u0644\u0645\u0644\u0645\u0633 \u0648\u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0623\u0635\u0644\u064a\u0629.<\/p><p class=\"wp-block-paragraph\">\u0627\u0644\u062a\u062e\u0644\u064a\u0644 \u0648\u0627\u0644\u062a\u0644\u062f\u064a\u0646: \u064a\u0633\u062a\u062e\u062f\u0645 \u0627\u0644\u062a\u062e\u0644\u064a\u0644 \u0644\u0625\u0632\u0627\u0644\u0629 \u0623\u0643\u0627\u0633\u064a\u062f \u0627\u0644\u0633\u0637\u062d \u0648\u0627\u0644\u0634\u0648\u0627\u0626\u0628\u060c \u0628\u064a\u0646\u0645\u0627 \u064a\u0633\u0627\u0639\u062f \u0627\u0644\u062a\u0644\u062f\u064a\u0646 \u0639\u0644\u0649 \u062a\u062d\u0633\u064a\u0646 \u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0645\u064a\u0643\u0627\u0646\u064a\u0643\u064a\u0629 \u0644\u0644\u0645\u0639\u062f\u0646. \u064a\u0645\u0643\u0646 \u0623\u0646 \u062a\u0636\u0645\u0646 \u0647\u0627\u062a\u0627\u0646 \u0627\u0644\u062e\u0637\u0648\u062a\u0627\u0646 \u0623\u0646 \u0627\u0644\u0633\u0637\u062d \u0627\u0644\u0645\u0637\u062d\u0648\u0646 \u064a\u062a\u0645\u062a\u0639 \u0628\u0645\u0642\u0627\u0648\u0645\u0629 \u062c\u064a\u062f\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0648\u0627\u0644\u0627\u0633\u062a\u0642\u0631\u0627\u0631 \u0623\u062b\u0646\u0627\u0621 \u0627\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645.<\/p><p class=\"wp-block-paragraph\">\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0633\u0637\u062d: \u064a\u062c\u0628 \u062a\u0635\u062d\u064a\u062d \u062a\u0633\u0637\u062d \u0627\u0644\u0633\u0637\u062d \u0628\u0639\u062f \u0627\u0644\u0637\u062d\u0646 \u0644\u0636\u0645\u0627\u0646 \u062c\u0648\u062f\u0629 \u0627\u0644\u0645\u0646\u062a\u062c.<\/p><p class=\"wp-block-paragraph\">\u0641\u062d\u0635 \u0627\u0644\u062c\u0648\u062f\u0629: \u064a\u062c\u0628 \u0641\u062d\u0635 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0645\u0637\u062d\u0648\u0646 \u0644\u0644\u062a\u062d\u0642\u0642 \u0645\u0646 \u0627\u0644\u062a\u0634\u0637\u064a\u0628 \u0648\u0627\u0644\u062f\u0642\u0629 \u0648\u0627\u0644\u0645\u0638\u0647\u0631 \u0644\u0636\u0645\u0627\u0646 \u0627\u0644\u0627\u0645\u062a\u062b\u0627\u0644 \u0644\u0644\u0645\u0639\u0627\u064a\u064a\u0631.<\/p><h2 class=\"wp-block-heading\">\u0623\u0646\u0648\u0627\u0639 \u062a\u0634\u0637\u064a\u0628\u0627\u062a \u0627\u0644\u0637\u0627\u062d\u0648\u0646\u0629<\/h2><p class=\"wp-block-paragraph\">\u0628\u0633\u0628\u0628 \u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0639\u0645\u0644\u064a\u0629 \u0648\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u060c \u064a\u0645\u0643\u0646 \u062a\u0642\u0633\u064a\u0645 \u0623\u0646\u0648\u0627\u0639 \u0627\u0644\u0637\u062d\u0646 \u0625\u0644\u0649 \u0627\u0644\u0623\u0646\u0648\u0627\u0639 \u0627\u0644\u062a\u0627\u0644\u064a\u0629.<\/p><h3 class=\"wp-block-heading\">\u0631\u0642\u0645 1 \u0627\u0644\u0646\u0647\u0627\u064a\u0629<\/h3><p class=\"wp-block-paragraph\">\u064a\u062a\u0645 \u062a\u0635\u0646\u064a\u0639 \u0627\u0644\u0637\u0644\u0627\u0621 \u0631\u0642\u0645 1 \u0639\u0646 \u0637\u0631\u064a\u0642 \u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0633\u0627\u062e\u0646\u0629 \u0648\u0627\u0644\u062a\u0644\u062f\u064a\u0646 \u0648\u0627\u0644\u062a\u062e\u0644\u064a\u0644. \u0648\u0647\u0648 \u0627\u0644\u0637\u0644\u0627\u0621 \u0627\u0644\u0623\u0643\u062b\u0631 \u062e\u0634\u0648\u0646\u0629 \u0648\u0627\u0644\u0623\u0642\u0644 \u0627\u0646\u0639\u0643\u0627\u0633\u064b\u0627\u060c \u0648\u064a\u062a\u0645\u064a\u0632 \u0628\u0645\u0638\u0647\u0631 \u062f\u0627\u0643\u0646 \u0648\u063a\u064a\u0631 \u0645\u0648\u062d\u062f. \u064a\u0633\u062a\u062e\u062f\u0645 \u0647\u0630\u0627 \u0627\u0644\u0637\u0644\u0627\u0621 \u0628\u0634\u0643\u0644 \u0623\u0633\u0627\u0633\u064a \u0641\u064a \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u062a\u064a \u0644\u0627 \u064a\u0643\u0648\u0646 \u0641\u064a\u0647\u0627 \u0627\u0644\u0645\u0638\u0647\u0631 \u0627\u0644\u062c\u0645\u0627\u0644\u064a \u0623\u0648\u0644\u0648\u064a\u0629\u060c \u0645\u062b\u0644 \u0623\u062c\u0632\u0627\u0621 \u0627\u0644\u0623\u0641\u0631\u0627\u0646 \u0648\u0627\u0644\u062a\u0648\u0631\u0628\u064a\u0646\u0627\u062a \u0627\u0644\u063a\u0627\u0632\u064a\u0629 \u0648\u0627\u0644\u063a\u0644\u0627\u064a\u0627\u062a \u0627\u0644\u0635\u0646\u0627\u0639\u064a\u0629.<\/p><h3 class=\"wp-block-heading\">\u0631\u0642\u0645 2D \u0627\u0644\u0646\u0647\u0627\u064a\u0629<\/h3><p class=\"wp-block-paragraph\">\u064a\u062a\u0645 \u062a\u0635\u0646\u064a\u0639 \u0627\u0644\u0637\u0644\u0627\u0621 \u062b\u0646\u0627\u0626\u064a \u0627\u0644\u0623\u0628\u0639\u0627\u062f \u0639\u0646 \u0637\u0631\u064a\u0642 \u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0628\u0627\u0631\u062f\u0629 \u0648\u0627\u0644\u062a\u0644\u062f\u064a\u0646 \u0648\u0627\u0644\u062a\u062e\u0644\u064a\u0644. \u0648\u064a\u0646\u062a\u062c \u0639\u0646 \u0630\u0644\u0643 \u0633\u0637\u062d \u063a\u064a\u0631 \u0644\u0627\u0645\u0639 \u0623\u0645\u0644\u0633 \u0648\u063a\u064a\u0631 \u0639\u0627\u0643\u0633. \u0647\u0630\u0627 \u0627\u0644\u0637\u0644\u0627\u0621 \u0645\u0646\u0627\u0633\u0628 \u0644\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u062a\u064a \u062a\u062a\u0637\u0644\u0628 \u0633\u0637\u062d\u064b\u0627 \u0646\u0638\u064a\u0641\u064b\u0627 \u0648\u063a\u064a\u0631 \u0639\u0627\u0643\u0633\u060c \u0645\u062b\u0644 \u0623\u0646\u0638\u0645\u0629 \u0639\u0627\u062f\u0645 \u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a \u0648\u0627\u0644\u0645\u0639\u062f\u0627\u062a \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629 \u0648\u0645\u0644\u062d\u0642\u0627\u062a \u0627\u0644\u062a\u0633\u0642\u064a\u0641.<\/p><h3 class=\"wp-block-heading\">\u0631\u0642\u0645 2\u0628 \u0627\u0644\u0646\u0647\u0627\u064a\u0629<\/h3><p class=\"wp-block-paragraph\">\u0625\u0646 \u0627\u0644\u0637\u0644\u0627\u0621 \u0631\u0642\u0645 2B \u064a\u0634\u0628\u0647 \u0627\u0644\u0637\u0644\u0627\u0621 \u0631\u0642\u0645 2D \u0648\u0644\u0643\u0646\u0647 \u064a\u062a\u0636\u0645\u0646 \u0645\u0631\u0648\u0631\u064b\u0627 \u062e\u0641\u064a\u0641\u064b\u0627 \u0625\u0636\u0627\u0641\u064a\u064b\u0627 \u0639\u0628\u0631 \u0628\u0643\u0631\u0627\u062a \u0645\u0635\u0642\u0648\u0644\u0629\u060c \u0645\u0645\u0627 \u064a\u0645\u0646\u062d\u0647 \u0633\u0637\u062d\u064b\u0627 \u0623\u0645\u0644\u0633\u064b\u0627 \u0648\u0639\u0627\u0643\u0633\u064b\u0627 \u0625\u0644\u0649 \u062d\u062f \u0645\u0627. \u0648\u0647\u0648 \u0627\u0644\u0637\u0644\u0627\u0621 \u0627\u0644\u0623\u0643\u062b\u0631 \u0627\u0633\u062a\u062e\u062f\u0627\u0645\u064b\u0627 \u0641\u064a \u0627\u0644\u0645\u0637\u0627\u062d\u0646 \u0646\u0638\u0631\u064b\u0627 \u0644\u062a\u0639\u062f\u062f \u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0627\u062a\u0647\u060c \u0648\u064a\u0648\u062c\u062f \u0639\u0627\u062f\u0629\u064b \u0641\u064a \u0645\u0639\u062f\u0627\u062a \u0627\u0644\u0645\u0637\u0628\u062e\u060c \u0648\u0627\u0644\u0645\u0639\u062f\u0627\u062a \u0627\u0644\u0635\u064a\u062f\u0644\u0627\u0646\u064a\u0629\u060c \u0648\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0645\u0639\u0645\u0627\u0631\u064a\u0629.<\/p><h3 class=\"wp-block-heading\">\u062a\u0634\u0637\u064a\u0628 \u0644\u0627\u0645\u0639 \u0645\u0635\u0642\u0648\u0644 (BA)<\/h3><p class=\"wp-block-paragraph\">\u062a\u062a\u0645\u062b\u0644 \u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u062a\u0644\u062f\u064a\u0646 \u0627\u0644\u0644\u0627\u0645\u0639 (BA) \u0641\u064a \u062a\u0644\u062f\u064a\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0641\u064a \u062c\u0648 \u0645\u0639\u064a\u0646 \u0644\u062a\u062c\u0646\u0628 \u0627\u0644\u0623\u0643\u0633\u062f\u0629 \u0648\u0625\u0646\u062a\u0627\u062c \u0633\u0637\u062d \u0644\u0627\u0645\u0639 \u0648\u0646\u0627\u0639\u0645 \u0643\u0627\u0644\u0645\u0631\u0622\u0629 \u0645\u0628\u0627\u0634\u0631\u0629 \u062f\u0648\u0646 \u062a\u0644\u0645\u064a\u0639 \u0625\u0636\u0627\u0641\u064a. \u063a\u0627\u0644\u0628\u064b\u0627 \u0645\u0627 \u062a\u0633\u062a\u062e\u062f\u0645 \u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0633\u0637\u062d \u0647\u0630\u0647 \u0641\u064a \u0627\u0644\u062f\u064a\u0643\u0648\u0631 \u0648\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0637\u0628\u062e \u0648\u0627\u0644\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u062c\u0631\u0627\u062d\u064a\u0629 \u0627\u0644\u0637\u0628\u064a\u0629.<\/p><h3 class=\"wp-block-heading\">\u0631\u0642\u0645 0 \u0627\u0644\u0646\u0647\u0627\u064a\u0629<\/h3><p class=\"wp-block-paragraph\">\u0631\u0642\u0645 0 Finish \u0647\u0648 \u0633\u0637\u062d \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u062a\u0645 \u0645\u0639\u0627\u0644\u062c\u062a\u0647 \u0628\u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0633\u0627\u062e\u0646\u0629 \u0648\u0627\u0644\u062a\u0644\u062f\u064a\u0646. \u064a\u062a\u0645\u064a\u0632 \u0631\u0642\u0645 0 Finish \u0628\u0633\u0637\u062d \u062e\u0634\u0646\u060c \u0648\u0639\u0627\u062f\u0629\u064b \u0645\u0627 \u064a\u0643\u0648\u0646 \u0628\u0647 \u0642\u0634\u0648\u0631\u060c \u0648\u064a\u064f\u0633\u062a\u062e\u062f\u0645 \u0628\u0634\u0643\u0644 \u0623\u0633\u0627\u0633\u064a \u0641\u064a \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0635\u0646\u0627\u0639\u064a\u0629 \u062d\u064a\u062b \u0644\u0627 \u062a\u0643\u0648\u0646 \u0647\u0646\u0627\u0643 \u062d\u0627\u062c\u0629 \u0625\u0644\u0649 \u062a\u0634\u0637\u064a\u0628 \u0627\u0644\u0633\u0637\u062d\u060c \u0645\u062b\u0644 \u0627\u0644\u0623\u062c\u0632\u0627\u0621 \u0627\u0644\u0647\u064a\u0643\u0644\u064a\u0629 \u0648\u0627\u0644\u0623\u062c\u0632\u0627\u0621 \u0627\u0644\u0645\u0648\u062c\u0648\u062f\u0629 \u0641\u064a \u0628\u064a\u0626\u0627\u062a \u0630\u0627\u062a \u062f\u0631\u062c\u0627\u062a \u062d\u0631\u0627\u0631\u0629 \u0639\u0627\u0644\u064a\u0629.<\/p><h3 class=\"wp-block-heading\">2H \u0627\u0644\u0646\u0647\u0627\u064a\u0629<\/h3><p class=\"wp-block-paragraph\">\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0633\u0637\u062d 2H \u0647\u064a \u0633\u0637\u062d \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u064a\u062a\u0645 \u0627\u0644\u062d\u0635\u0648\u0644 \u0639\u0644\u064a\u0647 \u0628\u0639\u062f \u0627\u0644\u062a\u0635\u0644\u0628 \u0628\u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0628\u0627\u0631\u062f\u0629. \u0625\u0646\u0647 \u0623\u0645\u0644\u0633 \u0648\u0639\u0627\u0643\u0633\u060c \u0648\u0647\u0648 \u0645\u062b\u0627\u0644\u064a \u0644\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u062a\u064a \u062a\u062a\u0637\u0644\u0628 \u0642\u0648\u0629 \u0648\u0635\u0644\u0627\u0628\u0629 \u0639\u0627\u0644\u064a\u0629\u060c \u0645\u062b\u0644 \u0627\u0644\u0646\u0648\u0627\u0628\u0636 \u0648\u0627\u0644\u0623\u062c\u0632\u0627\u0621 \u0639\u0627\u0644\u064a\u0629 \u0627\u0644\u0642\u0648\u0629.<\/p><h3 class=\"wp-block-heading\">2Q \u0627\u0644\u0646\u0647\u0627\u064a\u0629<\/h3><p class=\"wp-block-paragraph\">2Q Finish \u0647\u064a \u0637\u0631\u064a\u0642\u0629 \u0645\u0639\u0627\u0644\u062c\u0629 \u0633\u0637\u062d \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u062a\u064a \u064a\u062a\u0645 \u062f\u062d\u0631\u062c\u062a\u0647\u0627 \u0639\u0644\u0649 \u0627\u0644\u0628\u0627\u0631\u062f \u0648\u062a\u0628\u0631\u064a\u062f\u0647\u0627 \u0648\u062a\u0644\u0637\u064a\u0641\u0647\u0627. \u064a\u062a\u0645\u064a\u0632 2Q Finish \u0628\u0633\u0637\u062d \u0623\u0645\u0644\u0633 \u0648\u0642\u0648\u0629 \u0639\u0627\u0644\u064a\u0629 \u0648\u0627\u0646\u0639\u0643\u0627\u0633\u064a\u0629 \u062c\u064a\u062f\u0629\u060c \u0648\u0647\u0648 \u0645\u0646\u0627\u0633\u0628 \u0644\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u062a\u064a \u062a\u062a\u0637\u0644\u0628 \u0642\u0648\u0629 \u0639\u0627\u0644\u064a\u0629 \u0648\u0645\u0642\u0627\u0648\u0645\u0629 \u0639\u0627\u0644\u064a\u0629 \u0644\u0644\u062a\u0622\u0643\u0644\u060c \u0645\u062b\u0644 \u0627\u0644\u0633\u0643\u0627\u0643\u064a\u0646 \u0648\u0627\u0644\u0623\u062c\u0632\u0627\u0621 \u0627\u0644\u0645\u0642\u0627\u0648\u0645\u0629 \u0644\u0644\u062a\u0622\u0643\u0644.<\/p><h3 class=\"wp-block-heading\">2M \u0627\u0644\u0646\u0647\u0627\u064a\u0629<\/h3><p class=\"wp-block-paragraph\">2M Finish \u0639\u0628\u0627\u0631\u0629 \u0639\u0646 \u0633\u0637\u062d \u0632\u062e\u0631\u0641\u064a \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u064a\u062a\u0645 \u0627\u0644\u062d\u0635\u0648\u0644 \u0639\u0644\u064a\u0647 \u0639\u0646 \u0637\u0631\u064a\u0642 \u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0628\u0627\u0631\u062f\u0629 \u0648\u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0646\u0645\u0637\u064a\u0629. \u064a\u062a\u0645\u062a\u0639 \u0633\u0637\u062d 2M Finish \u0628\u062a\u0623\u062b\u064a\u0631 \u0628\u0635\u0631\u064a \u0641\u0631\u064a\u062f \u0648\u063a\u0627\u0644\u0628\u064b\u0627 \u0645\u0627 \u064a\u0633\u062a\u062e\u062f\u0645 \u0641\u064a \u0627\u0644\u062f\u064a\u0643\u0648\u0631 \u0627\u0644\u0645\u0639\u0645\u0627\u0631\u064a \u0648\u0627\u0644\u062f\u064a\u0643\u0648\u0631 \u0627\u0644\u062f\u0627\u062e\u0644\u064a \u0648\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0623\u062e\u0631\u0649 \u0627\u0644\u062a\u064a \u062a\u062a\u0637\u0644\u0628 \u0645\u0638\u0647\u0631\u064b\u0627 \u062c\u0645\u064a\u0644\u064b\u0627.<\/p><h3 class=\"wp-block-heading\">2B Finish \u0645\u0642\u0627\u0628\u0644 No.4 Finish<\/h3><figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td>\u064a\u0635\u0641<\/td><td>2\u0628 \u0627\u0644\u0646\u0647\u0627\u064a\u0629<\/td><td>\u0631\u0642\u0645 4 \u0627\u0644\u0646\u0647\u0627\u064a\u0629<\/td><\/tr><tr><td>\u062e\u0627\u0631\u062c\u064a\u0627<\/td><td>\u0646\u0627\u0639\u0645\u060c \u0639\u0627\u0643\u0633 \u0642\u0644\u064a\u0644\u0627\u064b<\/td><td>\u0645\u0635\u0642\u0648\u0644\u0629\u060c \u0645\u0639 \u062e\u0637\u0648\u0637 \u0645\u062a\u0648\u0627\u0632\u064a\u0629 \u0645\u0631\u0626\u064a\u0629<\/td><\/tr><tr><td>\u0637\u0644\u0628<\/td><td>\u0637\u0628\u0627\u062e\u0627\u062a \u0648\u062e\u0632\u0627\u0646\u0627\u062a \u062a\u062e\u0632\u064a\u0646 \u0635\u063a\u064a\u0631\u0629 \u0648\u0645\u0639\u062f\u0627\u062a \u0635\u064a\u062f\u0644\u0627\u0646\u064a\u0629<\/td><td>\u0623\u062c\u0647\u0632\u0629 \u0627\u0644\u0645\u0637\u0628\u062e\u060c \u0645\u0639\u062f\u0627\u062a \u0627\u0644\u0645\u0633\u062a\u0634\u0641\u064a\u0627\u062a\u060c \u0645\u0639\u062f\u0627\u062a \u062a\u062c\u0647\u064a\u0632 \u0627\u0644\u0623\u063a\u0630\u064a\u0629<\/td><\/tr><tr><td>\u064a\u0643\u0644\u0641<\/td><td>\u0639\u0645\u0648\u0645\u0627 \u0623\u0642\u0644 \u0645\u0646 \u0627\u0644\u0646\u0647\u0627\u064a\u0629 \u0631\u0642\u0645 4<\/td><td>\u0623\u0639\u0644\u0649 \u0628\u0633\u0628\u0628 \u0639\u0645\u0644\u064a\u0629 \u0627\u0644\u062a\u0646\u0638\u064a\u0641 \u0627\u0644\u0625\u0636\u0627\u0641\u064a\u0629<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u0623\u0646\u0648\u0627\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0645\u0646\u0627\u0633\u0628\u0629 \u0644\u0644\u0637\u062d\u0646<\/h2><p class=\"wp-block-paragraph\">\u064a\u0639\u062a\u0628\u0631 \u062a\u0634\u0637\u064a\u0628 \u0627\u0644\u0637\u0627\u062d\u0648\u0646\u0629 \u0645\u0646\u0627\u0633\u0628\u064b\u0627 \u0644\u062f\u0631\u062c\u0627\u062a \u0645\u062e\u062a\u0644\u0641\u0629 \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623\u060c \u0628\u0645\u0627 \u0641\u064a \u0630\u0644\u0643:<\/p><p class=\"wp-block-paragraph\"><strong>\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 304\/304L:<\/strong> \u064a\u062a\u0645 \u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0647 \u0639\u0644\u0649 \u0646\u0637\u0627\u0642 \u0648\u0627\u0633\u0639 \u0628\u0633\u0628\u0628 \u062a\u0648\u0627\u0632\u0646 \u0627\u0644\u0642\u0648\u0629 \u0648\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644 \u0648\u0627\u0644\u0642\u062f\u0631\u0629 \u0639\u0644\u0649 \u062a\u062d\u0645\u0644 \u0627\u0644\u062a\u0643\u0627\u0644\u064a\u0641.\u00a0<\/p><p class=\"wp-block-paragraph\"><strong>\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 316\/316L:<\/strong> \u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u062a\u0622\u0643\u0644 \u0628\u0627\u0644\u0643\u0644\u0648\u0631\u064a\u062f\u0627\u062a \u0648\u0627\u0644\u0645\u0630\u064a\u0628\u0627\u062a \u0627\u0644\u0635\u0646\u0627\u0639\u064a\u0629. \u0648\u064a\u0641\u0636\u0644 \u0627\u0633\u062a\u062e\u062f\u0627\u0645 316 \u0641\u064a \u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u0628\u062d\u0631\u064a\u0629 \u0648\u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629 \u0627\u0644\u0642\u0627\u0633\u064a\u0629.<\/p><p class=\"wp-block-paragraph\"><strong><a href=\"https:\/\/steelprogroup.com\/ar\/stainless-steel\/grades\/grade-430\/\" data-type=\"link\" data-id=\"https:\/\/steelprogroup.com\/stainless-steel\/grades\/grade-430\/\">430 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623<\/a>:<\/strong> \u0627\u0642\u062a\u0635\u0627\u062f\u064a \u0648\u064a\u064f\u0633\u062a\u062e\u062f\u0645 \u0641\u064a \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u062a\u064a \u062a\u0643\u0648\u0646 \u0641\u064a\u0647\u0627 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644 \u0627\u0644\u0645\u0639\u062a\u062f\u0644\u0629 \u0643\u0627\u0641\u064a\u0629\u060c \u0645\u062b\u0644 \u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u062f\u0627\u062e\u0644\u064a\u0629 \u0648\u0627\u0644\u0638\u0631\u0648\u0641 \u0627\u0644\u0635\u0646\u0627\u0639\u064a\u0629 \u0627\u0644\u0645\u0639\u062a\u062f\u0644\u0629.<\/p><h2 class=\"wp-block-heading\">\u0642\u0648\u0627\u0644\u0628 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0630\u0627\u062a \u0627\u0644\u0644\u0645\u0633\u0629 \u0627\u0644\u0646\u0647\u0627\u0626\u064a\u0629 \u0644\u0644\u0645\u0637\u062d\u0646\u0629<\/h2><p class=\"wp-block-paragraph\">\u0641\u064a\u0645\u0627 \u064a\u0644\u064a \u0627\u0644\u0623\u0634\u0643\u0627\u0644 \u0627\u0644\u0634\u0627\u0626\u0639\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0645\u0637\u0644\u064a \u0628\u0627\u0644\u0645\u0637\u062d\u0646\u0629:<\/p><p class=\"wp-block-paragraph\"><strong>\u0644\u0648\u062d\u0629 \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0630\u0627\u062a \u0644\u0645\u0633\u0629 \u0646\u0647\u0627\u0626\u064a\u0629 \u0644\u0644\u0645\u0637\u062d\u0646\u0629:<\/strong> \u0642\u0637\u0639 \u0633\u0645\u064a\u0643\u0629 \u0648\u0645\u0633\u0637\u062d\u0629 \u062a\u0633\u062a\u062e\u062f\u0645 \u0641\u064a \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0647\u064a\u0643\u0644\u064a\u0629 \u0648\u0627\u0644\u0622\u0644\u0627\u062a \u0627\u0644\u062b\u0642\u064a\u0644\u0629.<\/p><p class=\"wp-block-paragraph\"><strong>\u0635\u0641\u0627\u0626\u062d \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0630\u0627\u062a \u0627\u0644\u0646\u0647\u0627\u064a\u0629 \u0627\u0644\u0645\u0637\u062d\u0648\u0646\u0629:<\/strong> \u0623\u0631\u0642 \u0645\u0646 \u0627\u0644\u0623\u0644\u0648\u0627\u062d\u060c \u0648\u064a\u0633\u062a\u062e\u062f\u0645 \u0641\u064a \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0623\u062e\u0641 \u0648\u0632\u0646\u0627\u064b\u060c \u0628\u0645\u0627 \u0641\u064a \u0630\u0644\u0643 \u062a\u0635\u0646\u064a\u0639 \u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a \u0648\u0627\u0644\u0623\u062c\u0647\u0632\u0629.<\/p><p class=\"wp-block-paragraph\"><strong>\u0634\u0631\u064a\u0637 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0630\u0648 \u0627\u0644\u0646\u0647\u0627\u064a\u0629 \u0627\u0644\u0645\u0637\u062d\u0648\u0646\u0629:<\/strong> \u0645\u062a\u0648\u0641\u0631 \u0628\u0623\u0634\u0643\u0627\u0644 \u0645\u062e\u062a\u0644\u0641\u0629 (\u062f\u0627\u0626\u0631\u064a\u060c \u0645\u0631\u0628\u0639\u060c \u0633\u062f\u0627\u0633\u064a)\u061b \u064a\u0633\u062a\u062e\u062f\u0645 \u0641\u064a \u0627\u0644\u0628\u0646\u0627\u0621 \u0648\u0627\u0644\u062a\u0634\u063a\u064a\u0644 \u0648\u0627\u0644\u062a\u0635\u0646\u064a\u0639.<\/p><p class=\"wp-block-paragraph\"><strong>\u0623\u0646\u0628\u0648\u0628 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0630\u0648 \u0627\u0644\u0646\u0647\u0627\u064a\u0629 \u0627\u0644\u0646\u0647\u0627\u0626\u064a\u0629 \u0644\u0644\u0645\u0637\u062d\u0646\u0629:<\/strong> \u0623\u0634\u0643\u0627\u0644 \u0623\u0633\u0637\u0648\u0627\u0646\u064a\u0629 \u0645\u062c\u0648\u0641\u0629 \u062a\u0633\u062a\u062e\u062f\u0645 \u0641\u064a \u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0645\u062e\u062a\u0644\u0641\u0629\u060c \u0628\u0645\u0627 \u0641\u064a \u0630\u0644\u0643 \u0627\u0644\u0628\u0646\u0627\u0621 \u0648\u0627\u0644\u0633\u0628\u0627\u0643\u0629 \u0648\u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a.<\/p><p class=\"wp-block-paragraph\"><strong>\u0623\u0646\u0628\u0648\u0628 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0630\u0648 \u0627\u0644\u0646\u0647\u0627\u064a\u0629 \u0627\u0644\u0646\u0647\u0627\u0626\u064a\u0629 \u0644\u0644\u0645\u0637\u062d\u0646\u0629: <\/strong>\u0645\u064f\u0635\u0645\u0645 \u062e\u0635\u064a\u0635\u064b\u0627 \u0644\u0646\u0642\u0644 \u0627\u0644\u0633\u0648\u0627\u0626\u0644 \u0648\u0627\u0644\u063a\u0627\u0632\u0627\u062a\u061b \u0648\u064a\u064f\u0633\u062a\u062e\u062f\u0645 \u063a\u0627\u0644\u0628\u064b\u0627 \u0641\u064a \u0627\u0644\u0633\u0628\u0627\u0643\u0629 \u0648\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0635\u0646\u0627\u0639\u064a\u0629.<\/p><h2 class=\"wp-block-heading\">\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0645\u0637\u062d\u0648\u0646<\/h2><p class=\"wp-block-paragraph\">\u0628\u0627\u0644\u0645\u0642\u0627\u0631\u0646\u0629 \u0645\u0639 \u0637\u0631\u0642 \u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0633\u0637\u062d \u0627\u0644\u0623\u062e\u0631\u0649 \u0645\u062b\u0644 \u0627\u0644\u062a\u0644\u0645\u064a\u0639 \u0648\u0627\u0644\u0641\u0631\u0634\u0627\u0629\u060c \u0641\u0625\u0646 \u0627\u0644\u062a\u0623\u062b\u064a\u0631 \u0627\u0644\u0633\u0637\u062d\u064a \u0644\u0644\u0637\u062d\u0646 \u0623\u0633\u0627\u0633\u064a \u0646\u0633\u0628\u064a\u064b\u0627\u060c \u0648\u0644\u0643\u0646 \u0627\u0642\u062a\u0635\u0627\u062f\u064a\u062a\u0647 \u0648\u0639\u0645\u0644\u064a\u062a\u0647 \u062a\u062c\u0639\u0644\u0647 \u0627\u0644\u062e\u064a\u0627\u0631 \u0627\u0644\u0623\u0648\u0644 \u0641\u064a \u0627\u0644\u0639\u062f\u064a\u062f \u0645\u0646 \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a.<\/p><h3 class=\"wp-block-heading\">\u0627\u0642\u062a\u0635\u0627\u062f\u064a<\/h3><p class=\"wp-block-paragraph\">\u0627\u0644\u0637\u062d\u0646 \u0647\u0648 \u0637\u0631\u064a\u0642\u0629 \u0645\u0639\u0627\u0644\u062c\u0629 \u0633\u0637\u062d\u064a\u0629 \u0623\u0633\u0627\u0633\u064a\u0629 \u0628\u062a\u0643\u0644\u0641\u0629 \u0623\u0642\u0644 \u0645\u0646 \u0627\u0644\u062a\u0644\u0645\u064a\u0639 \u0623\u0648 \u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0645\u0631\u0622\u0629. \u0645\u0646\u0627\u0633\u0628 \u0644\u0644\u0645\u0634\u0627\u0631\u064a\u0639 \u0627\u0644\u062a\u064a \u062a\u062a\u0637\u0644\u0628 \u0625\u0646\u062a\u0627\u062c\u064b\u0627 \u0648\u0627\u0633\u0639 \u0627\u0644\u0646\u0637\u0627\u0642 \u0648\u0645\u064a\u0632\u0627\u0646\u064a\u0627\u062a \u0645\u062d\u062f\u0648\u062f\u0629. \u0646\u0638\u0631\u064b\u0627 \u0644\u0639\u0645\u0644\u064a\u0629 \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0628\u0633\u064a\u0637\u0629\u060c \u064a\u0645\u0643\u0646 \u0644\u0644\u0637\u062d\u0646 \u0627\u0644\u062a\u062d\u0643\u0645 \u0628\u0641\u0639\u0627\u0644\u064a\u0629 \u0641\u064a \u062a\u0643\u0627\u0644\u064a\u0641 \u0627\u0644\u0625\u0646\u062a\u0627\u062c.<\/p><h3 class=\"wp-block-heading\">\u0627\u0644\u0645\u0638\u0647\u0631 \u0627\u0644\u0623\u0635\u0644\u064a<\/h3><p class=\"wp-block-paragraph\">\u0639\u0627\u062f\u0629\u064b \u0645\u0627 \u064a\u062d\u0627\u0641\u0638 \u0627\u0644\u0633\u0637\u062d \u0627\u0644\u0645\u0637\u062d\u0648\u0646 \u0639\u0644\u0649 \u0627\u0644\u0645\u0644\u0645\u0633 \u0627\u0644\u0637\u0628\u064a\u0639\u064a \u0644\u0644\u0645\u0639\u062f\u0646 \u062f\u0648\u0646 \u0645\u0639\u0627\u0644\u062c\u0629 \u062a\u0644\u0645\u064a\u0639 \u0625\u0636\u0627\u0641\u064a\u0629. \u0648\u0631\u063a\u0645 \u0623\u0646 \u0647\u0630\u0647 \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0644\u0627 \u062a\u0648\u0641\u0631 \u062f\u0631\u062c\u0629 \u0639\u0627\u0644\u064a\u0629 \u0645\u0646 \u0627\u0644\u062a\u0634\u0637\u064a\u0628\u060c \u0625\u0644\u0627 \u0623\u0646\u0647\u0627 \u062a\u0648\u0641\u0631 \u0623\u0633\u0627\u0633\u064b\u0627 \u0644\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0623\u0648 \u0627\u0644\u0632\u062e\u0631\u0641\u0629 \u0627\u0644\u0644\u0627\u062d\u0642\u0629.<\/p><h3 class=\"wp-block-heading\">\u0623\u062f\u0627\u0621 \u0645\u0633\u062a\u0642\u0631<\/h3><p class=\"wp-block-paragraph\">\u0627\u0644\u0633\u0637\u062d \u0627\u0644\u0645\u0635\u0642\u0648\u0644 \u0645\u062a\u064a\u0646 \u0648\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u062a\u0622\u0643\u0644 \u0641\u064a \u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u0642\u0627\u0633\u064a\u0629. \u0625\u0646 \u0639\u062f\u0645 \u0648\u062c\u0648\u062f \u0633\u0637\u062d \u0645\u0635\u0642\u0648\u0644 \u0644\u0644\u063a\u0627\u064a\u0629 \u064a\u0639\u0646\u064a \u0623\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0645\u0635\u0642\u0648\u0644 \u064a\u062a\u0637\u0644\u0628 \u0627\u0644\u062d\u062f \u0627\u0644\u0623\u062f\u0646\u0649 \u0645\u0646 \u0627\u0644\u0635\u064a\u0627\u0646\u0629 \u0648\u0627\u0644\u062a\u0646\u0638\u064a\u0641.<\/p><h3 class=\"wp-block-heading\">\u0645\u062c\u0645\u0648\u0639\u0629 \u0648\u0627\u0633\u0639\u0629 \u0645\u0646 \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a<\/h3><p class=\"wp-block-paragraph\">\u062a\u0639\u062a\u0628\u0631 \u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0637\u062d\u0646 \u0645\u0646\u0627\u0633\u0628\u0629 \u0644\u0623\u0646\u0648\u0627\u0639 \u0645\u062e\u062a\u0644\u0641\u0629 \u0645\u0646 \u0645\u0648\u0627\u062f \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0648\u0647\u064a \u0637\u0631\u064a\u0642\u0629 \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0623\u0633\u0627\u0633\u064a\u0629 \u0644\u0644\u0639\u062f\u064a\u062f \u0645\u0646 \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0635\u0646\u0627\u0639\u064a\u0629. \u064a\u062a\u0645 \u062a\u0637\u0628\u064a\u0642\u0647\u0627 \u0639\u0644\u0649 \u0646\u0637\u0627\u0642 \u0648\u0627\u0633\u0639 \u0641\u064a \u0645\u062c\u0627\u0644\u0627\u062a \u0645\u062e\u062a\u0644\u0641\u0629 \u0645\u062b\u0644 \u0627\u0644\u0628\u0646\u0627\u0621 \u0648\u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a \u0648\u0627\u0644\u0645\u0648\u0627\u062f \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629 \u0648\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0623\u063a\u0630\u064a\u0629.<\/p><h2 class=\"wp-block-heading\">\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0645\u0637\u0644\u064a \u0628\u0627\u0644\u0637\u062d\u0646<\/h2><p class=\"wp-block-paragraph\"><strong>\u0647\u0646\u062f\u0633\u0629 \u0627\u0644\u0628\u0646\u0627\u0621:<\/strong> \u062a\u064f\u0633\u062a\u062e\u062f\u0645 \u0627\u0644\u0623\u0633\u0637\u062d \u0627\u0644\u0645\u0637\u062d\u0648\u0646\u0629 \u063a\u0627\u0644\u0628\u064b\u0627 \u0641\u064a \u0627\u0644\u0645\u0643\u0648\u0646\u0627\u062a \u0627\u0644\u0647\u064a\u0643\u0644\u064a\u0629 \u0648\u0627\u0644\u0645\u0648\u0627\u062f \u0627\u0644\u0632\u062e\u0631\u0641\u064a\u0629 \u0646\u0638\u0631\u064b\u0627 \u0644\u0645\u0642\u0627\u0648\u0645\u062a\u0647\u0627 \u0644\u0644\u062a\u0622\u0643\u0644 \u0648\u0642\u0648\u062a\u0647\u0627\u060c \u0645\u0645\u0627 \u0642\u062f \u064a\u0644\u0628\u064a \u0645\u062a\u0637\u0644\u0628\u0627\u062a \u0645\u062a\u0627\u0646\u0629 \u0627\u0644\u0647\u064a\u0627\u0643\u0644 \u0627\u0644\u0645\u0628\u0646\u064a\u0629. \u062a\u0634\u0645\u0644 \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0634\u0627\u0626\u0639\u0629 \u0625\u0637\u0627\u0631\u0627\u062a \u062f\u0639\u0645 \u0627\u0644\u0645\u0628\u0627\u0646\u064a \u0648\u0623\u0644\u0648\u0627\u062d \u0627\u0644\u062c\u062f\u0631\u0627\u0646 \u0627\u0644\u062e\u0627\u0631\u062c\u064a\u0629 \u0648\u0627\u0644\u0634\u0631\u0627\u0626\u0637 \u0627\u0644\u0632\u062e\u0631\u0641\u064a\u0629.<\/p><p class=\"wp-block-paragraph\"><strong>\u0635\u0646\u0627\u0639\u0629 \u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a:<\/strong> \u0641\u064a \u062a\u0635\u0646\u064a\u0639 \u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a\u060c \u064a\u062a\u0645 \u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0645\u0637\u062d\u0648\u0646 \u0643\u0645\u0648\u0627\u062f \u0623\u0633\u0627\u0633\u064a\u0629 \u0644\u0625\u0646\u062a\u0627\u062c \u0623\u062c\u0632\u0627\u0621 \u0645\u062e\u062a\u0644\u0641\u0629 \u0644\u0644\u0633\u064a\u0627\u0631\u0627\u062a. \u062a\u0634\u0645\u0644 \u0647\u0630\u0647 \u0627\u0644\u0623\u062c\u0632\u0627\u0621 \u0623\u0646\u0638\u0645\u0629 \u0627\u0644\u0639\u0627\u062f\u0645 \u0648\u0625\u0637\u0627\u0631\u0627\u062a \u0627\u0644\u0647\u064a\u0643\u0644 \u0648\u0627\u0644\u0623\u062c\u0632\u0627\u0621 \u0627\u0644\u0647\u064a\u0643\u0644\u064a\u0629 \u0627\u0644\u062f\u0627\u062e\u0644\u064a\u0629. \u064a\u0645\u0643\u0646 \u0644\u0644\u0633\u0637\u062d \u0627\u0644\u0645\u0637\u062d\u0648\u0646 \u0623\u0646 \u064a\u062a\u062d\u0645\u0644 \u062f\u0631\u062c\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u0639\u0627\u0644\u064a\u0629 \u0648\u0627\u0644\u062a\u0622\u0643\u0644 \u0627\u0644\u0645\u064a\u0643\u0627\u0646\u064a\u0643\u064a\u060c \u0648\u0647\u0648 \u0645\u0627\u062f\u0629 \u0634\u0627\u0626\u0639\u0629 \u0641\u064a \u0635\u0646\u0627\u0639\u0629 \u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a.<\/p><p class=\"wp-block-paragraph\"><strong>\u0627\u0644\u0635\u0646\u0627\u0639\u0629 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629: <\/strong>\u063a\u0627\u0644\u0628\u064b\u0627 \u0645\u0627 \u064a\u062a\u0645 \u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0645\u0637\u062d\u0648\u0646 \u0641\u064a \u0627\u0644\u0645\u0641\u0627\u0639\u0644\u0627\u062a \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629 \u0648\u062e\u0637\u0648\u0637 \u0627\u0644\u0623\u0646\u0627\u0628\u064a\u0628 \u0648\u062e\u0632\u0627\u0646\u0627\u062a \u0627\u0644\u062a\u062e\u0632\u064a\u0646 \u0648\u063a\u064a\u0631\u0647\u0627 \u0645\u0646 \u0627\u0644\u0645\u0639\u062f\u0627\u062a \u0644\u0623\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0645\u0637\u062d\u0648\u0646 \u064a\u062a\u0645\u062a\u0639 \u0628\u0645\u0642\u0627\u0648\u0645\u0629 \u0645\u0645\u062a\u0627\u0632\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u060c \u0645\u0645\u0627 \u064a\u0636\u0645\u0646 \u0627\u0644\u062a\u0634\u063a\u064a\u0644 \u0627\u0644\u0645\u0633\u062a\u0642\u0631 \u0648\u0637\u0648\u064a\u0644 \u0627\u0644\u0623\u0645\u062f \u0644\u0644\u0645\u0639\u062f\u0627\u062a.<\/p><p class=\"wp-block-paragraph\"><strong>\u0627\u0644\u0623\u062c\u0647\u0632\u0629 \u0627\u0644\u0645\u0646\u0632\u0644\u064a\u0629: <\/strong>\u0641\u064a \u0635\u0646\u0627\u0639\u0629 \u0627\u0644\u0623\u062c\u0647\u0632\u0629 \u0627\u0644\u0645\u0646\u0632\u0644\u064a\u0629\u060c \u064a\u062a\u0645 \u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0645\u0637\u062d\u0648\u0646 \u0644\u062a\u0635\u0646\u064a\u0639 \u0623\u062c\u0632\u0627\u0621 \u0645\u062b\u0644 \u0623\u063a\u0644\u0641\u0629 \u0627\u0644\u062b\u0644\u0627\u062c\u0629 \u0648\u0627\u0644\u0637\u0628\u0648\u0644 \u0627\u0644\u062f\u0627\u062e\u0644\u064a\u0629 \u0644\u0644\u063a\u0633\u0627\u0644\u0629. \u0646\u0638\u0631\u064b\u0627 \u0644\u0645\u062a\u0627\u0646\u0629 \u0627\u0644\u0633\u0637\u062d \u0627\u0644\u0645\u0637\u062d\u0648\u0646 \u0648\u0645\u0642\u0627\u0648\u0645\u062a\u0647 \u0627\u0644\u0623\u0633\u0627\u0633\u064a\u0629 \u0644\u0644\u062a\u0622\u0643\u0644\u060c \u0641\u0625\u0646\u0647 \u064a\u0645\u0643\u0646 \u0623\u0646 \u064a\u0644\u0628\u064a \u0627\u0644\u0645\u062a\u0637\u0644\u0628\u0627\u062a \u0627\u0644\u0623\u0633\u0627\u0633\u064a\u0629 \u0644\u0644\u0623\u062c\u0647\u0632\u0629 \u0627\u0644\u0645\u0646\u0632\u0644\u064a\u0629 \u0644\u0644\u0645\u0648\u0627\u062f.<\/p><p class=\"wp-block-paragraph\"><strong>\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0623\u063a\u0630\u064a\u0629:<\/strong> \u0641\u064a \u0645\u0639\u062f\u0627\u062a \u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0623\u063a\u0630\u064a\u0629\u060c \u064a\u062a\u0645 \u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0645\u0637\u062d\u0648\u0646 \u0644\u0635\u0646\u0639 \u0645\u062e\u062a\u0644\u0641 \u0622\u0644\u0627\u062a \u0648\u062d\u0627\u0648\u064a\u0627\u062a \u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0623\u063a\u0630\u064a\u0629. \u0625\u0646 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644 \u0648\u0646\u0638\u0627\u0641\u0629 \u0627\u0644\u0633\u0637\u062d \u0627\u0644\u0645\u0637\u062d\u0648\u0646 \u062a\u062c\u0639\u0644\u0647 \u062e\u064a\u0627\u0631\u064b\u0627 \u0645\u062b\u0627\u0644\u064a\u064b\u0627 \u0644\u0635\u0646\u0627\u0639\u0629 \u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0623\u063a\u0630\u064a\u0629.<\/p><h2 class=\"wp-block-heading\">\u0643\u064a\u0641\u064a\u0629 \u0627\u0644\u062d\u0641\u0627\u0638 \u0639\u0644\u0649 \u062a\u0634\u0637\u064a\u0628 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623\u061f<\/h2><p class=\"wp-block-paragraph\">\u0625\u0646 \u0635\u064a\u0627\u0646\u0629 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0645\u0637\u062d\u0648\u0646 \u064a\u0645\u0643\u0646 \u0623\u0646 \u064a\u0624\u062f\u064a \u0625\u0644\u0649 \u0625\u0637\u0627\u0644\u0629 \u0639\u0645\u0631\u0647 \u0627\u0644\u0627\u0641\u062a\u0631\u0627\u0636\u064a \u0648\u0627\u0644\u062d\u0641\u0627\u0638 \u0639\u0644\u0649 \u0645\u0638\u0647\u0631\u0647 \u0627\u0644\u062c\u064a\u062f\u060c \u0628\u0645\u0627 \u0641\u064a \u0630\u0644\u0643 \u0627\u0644\u0646\u0642\u0627\u0637 \u0627\u0644\u062a\u0627\u0644\u064a\u0629 \u0628\u0634\u0643\u0644 \u0623\u0633\u0627\u0633\u064a.<\/p><ul class=\"wp-block-list\"><li>\u0627\u0644\u062a\u0646\u0638\u064a\u0641 \u0627\u0644\u0645\u0646\u062a\u0638\u0645: \u0627\u0633\u062a\u062e\u062f\u0645 \u0645\u0646\u0638\u0641\u064b\u0627 \u062e\u0641\u064a\u0641\u064b\u0627 \u0648\u0642\u0637\u0639\u0629 \u0642\u0645\u0627\u0634 \u0646\u0627\u0639\u0645\u0629 \u0644\u062a\u0646\u0638\u064a\u0641 \u0627\u0644\u0633\u0637\u062d \u0627\u0644\u0645\u0637\u062d\u0648\u0646 \u0628\u0627\u0646\u062a\u0638\u0627\u0645 \u0644\u0625\u0632\u0627\u0644\u0629 \u0627\u0644\u0623\u0648\u0633\u0627\u062e \u0648\u0627\u0644\u0628\u0642\u0639. \u062a\u062c\u0646\u0628 \u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u0645\u0646\u0638\u0641\u0627\u062a \u0627\u0644\u062d\u0645\u0636\u064a\u0629 \u0623\u0648 \u0627\u0644\u0642\u0644\u0648\u064a\u0629 \u0627\u0644\u0642\u0648\u064a\u0629 \u0644\u0645\u0646\u0639 \u062a\u0644\u0641 \u0627\u0644\u0633\u0637\u062d.&nbsp;<\/li><\/ul><ul class=\"wp-block-list\"><li>\u0645\u0646\u0639 \u0627\u0644\u062a\u0622\u0643\u0644: \u062a\u062c\u0646\u0628 \u0645\u0644\u0627\u0645\u0633\u0629 \u0627\u0644\u0623\u062d\u0645\u0627\u0636 \u0627\u0644\u0642\u0648\u064a\u0629 \u0623\u0648 \u0627\u0644\u0642\u0644\u0648\u064a\u0627\u062a \u0627\u0644\u0642\u0648\u064a\u0629 \u0644\u0645\u0646\u0639 \u0627\u0644\u062a\u0622\u0643\u0644. \u0639\u0644\u0649 \u0627\u0644\u0631\u063a\u0645 \u0645\u0646 \u0623\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0645\u0637\u062d\u0648\u0646 \u064a\u062a\u0645\u062a\u0639 \u0628\u0645\u0642\u0627\u0648\u0645\u0629 \u062c\u064a\u062f\u0629 \u0644\u0644\u062a\u0622\u0643\u0644\u060c \u0625\u0644\u0627 \u0623\u0646\u0647 \u0642\u062f \u064a\u062a\u0622\u0643\u0644 \u0625\u0630\u0627 \u062a\u0639\u0631\u0636 \u0644\u0628\u064a\u0626\u0627\u062a \u062a\u0622\u0643\u0644\u064a\u0629 \u0644\u0641\u062a\u0631\u0629 \u0637\u0648\u064a\u0644\u0629. \u0625\u0646 \u0625\u0628\u0639\u0627\u062f \u0633\u0637\u062d \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0639\u0646 \u0627\u0644\u0645\u0648\u0627\u062f \u0627\u0644\u0645\u0633\u0628\u0628\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u064a\u0645\u0643\u0646 \u0623\u0646 \u064a\u0637\u064a\u0644 \u0645\u0646 \u0639\u0645\u0631\u0647 \u0627\u0644\u0627\u0641\u062a\u0631\u0627\u0636\u064a.<\/li><\/ul><ul class=\"wp-block-list\"><li>\u062a\u062c\u0646\u0628 \u0627\u0644\u062e\u062f\u0648\u0634: \u062a\u062c\u0646\u0628 \u062e\u062f\u0634 \u0627\u0644\u0633\u0637\u062d \u0628\u0623\u0634\u064a\u0627\u0621 \u0635\u0644\u0628\u0629 \u0644\u0645\u0646\u0639 \u0627\u0644\u062e\u062f\u0648\u0634 \u0648\u0627\u0644\u062a\u0622\u0643\u0644. \u0627\u0644\u0623\u0633\u0637\u062d \u0627\u0644\u0645\u0637\u062d\u0648\u0646\u0629 \u062e\u0634\u0646\u0629 \u0646\u0633\u0628\u064a\u064b\u0627 \u0648\u064a\u0645\u0643\u0646 \u062e\u062f\u0634\u0647\u0627 \u0628\u0633\u0647\u0648\u0644\u0629 \u0628\u0648\u0627\u0633\u0637\u0629 \u0623\u0634\u064a\u0627\u0621 \u0635\u0644\u0628\u0629\u060c \u0645\u0645\u0627 \u064a\u0624\u062f\u064a \u0625\u0644\u0649 \u062a\u0644\u0641 \u0627\u0644\u0633\u0637\u062d. \u0627\u0633\u062a\u062e\u062f\u0645 \u0642\u0637\u0639\u0629 \u0642\u0645\u0627\u0634 \u0646\u0627\u0639\u0645\u0629 \u0648\u0623\u062f\u0648\u0627\u062a \u062a\u0646\u0638\u064a\u0641 \u063a\u064a\u0631 \u0643\u0627\u0634\u0637\u0629 \u0644\u062a\u062c\u0646\u0628 \u0627\u0644\u062e\u062f\u0648\u0634 \u0628\u0634\u0643\u0644 \u0641\u0639\u0627\u0644.<\/li><\/ul><ul class=\"wp-block-list\"><li>\u0627\u0644\u062a\u0641\u062a\u064a\u0634 \u0627\u0644\u062f\u0648\u0631\u064a: \u0627\u0644\u062a\u062d\u0642\u0642 \u0645\u0646 \u062d\u0627\u0644\u0629 \u0627\u0644\u0633\u0637\u062d \u0628\u0627\u0646\u062a\u0638\u0627\u0645 \u0648\u0627\u0644\u062a\u0639\u0627\u0645\u0644 \u0645\u0639 \u0645\u0634\u0627\u0643\u0644 \u0627\u0644\u062a\u0622\u0643\u0644 \u0623\u0648 \u0627\u0644\u062a\u0644\u0641 \u0627\u0644\u0645\u062d\u062a\u0645\u0644\u0629 \u0641\u064a \u0627\u0644\u0648\u0642\u062a \u0627\u0644\u0645\u0646\u0627\u0633\u0628 \u0644\u0636\u0645\u0627\u0646 \u0627\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0637\u0648\u064a\u0644 \u0627\u0644\u0623\u0645\u062f \u0644\u0645\u0648\u0627\u062f \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623.<\/li><\/ul><h2 class=\"wp-block-heading\">\u062a\u0634\u0637\u064a\u0628 \u0627\u0644\u0637\u0627\u062d\u0648\u0646\u0629 \u0645\u0642\u0627\u0628\u0644 \u0627\u0644\u062a\u0634\u0637\u064a\u0628\u0627\u062a \u0627\u0644\u0645\u0635\u0642\u0648\u0644\u0629 \u0648\u0627\u0644\u0645\u0635\u0642\u0648\u0644\u0629<\/h2><p class=\"wp-block-paragraph\">\u062a\u062e\u062a\u0644\u0641 \u062a\u0634\u0637\u064a\u0628\u0627\u062a \u0627\u0644\u0637\u062d\u0646 \u0648\u0627\u0644\u062a\u0634\u0637\u064a\u0628\u0627\u062a \u0627\u0644\u0645\u0635\u0642\u0648\u0644\u0629 \u0648\u0627\u0644\u062a\u0634\u0637\u064a\u0628\u0627\u062a \u0627\u0644\u0645\u0635\u0642\u0648\u0644\u0629 \u0628\u0634\u0643\u0644 \u0648\u0627\u0636\u062d \u0641\u064a \u0627\u0644\u0645\u0638\u0647\u0631 \u0648\u0627\u0644\u0635\u064a\u0627\u0646\u0629 \u0648\u0627\u0644\u062a\u0643\u0644\u0641\u0629 \u0648\u0627\u0644\u0645\u062a\u0627\u0646\u0629 \u0648\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a.<\/p><p class=\"wp-block-paragraph\">\u064a\u062a\u0645\u064a\u0632 \u0637\u0644\u0627\u0621 \u0627\u0644\u0637\u0627\u062d\u0648\u0646\u0629 \u0628\u0645\u0638\u0647\u0631 \u0628\u0627\u0647\u062a \u0648\u063a\u064a\u0631 \u0644\u0627\u0645\u0639 \u0645\u0639 \u0627\u062e\u062a\u0644\u0627\u0641\u0627\u062a \u0637\u0641\u064a\u0641\u0629 \u0641\u064a \u0627\u0644\u0645\u0644\u0645\u0633 \u0648\u064a\u062a\u0637\u0644\u0628 \u0627\u0644\u062d\u062f \u0627\u0644\u0623\u062f\u0646\u0649 \u0645\u0646 \u0627\u0644\u0635\u064a\u0627\u0646\u0629. \u0648\u0647\u0648 \u0623\u0643\u062b\u0631 \u0641\u0639\u0627\u0644\u064a\u0629 \u0645\u0646 \u062d\u064a\u062b \u0627\u0644\u062a\u0643\u0644\u0641\u0629 \u0628\u0633\u0628\u0628 \u062e\u0637\u0648\u0627\u062a \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0623\u0642\u0644 \u0648\u064a\u0648\u0641\u0631 \u0645\u062a\u0627\u0646\u0629 \u0639\u0627\u0644\u064a\u0629. \u063a\u0627\u0644\u0628\u064b\u0627 \u0645\u0627 \u064a\u0643\u0648\u0646 \u0647\u0630\u0627 \u0627\u0644\u0646\u0648\u0639 \u0645\u0646 \u0627\u0644\u0637\u0644\u0627\u0621 \u0645\u0646\u0627\u0633\u0628\u064b\u0627 \u0644\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0635\u0646\u0627\u0639\u064a\u0629 \u0648\u0627\u0644\u0628\u0646\u0627\u0621 \u0648\u0627\u0644\u0628\u062d\u0631\u064a\u0629.<\/p><p class=\"wp-block-paragraph\">\u0645\u0646 \u0646\u0627\u062d\u064a\u0629 \u0623\u062e\u0631\u0649\u060c \u064a\u0648\u0641\u0631 \u0627\u0644\u062a\u0634\u0637\u064a\u0628 \u0627\u0644\u0645\u0635\u0642\u0648\u0644 \u0633\u0637\u062d\u064b\u0627 \u0623\u0645\u0644\u0633\u064b\u0627 \u0628\u062e\u0637\u0648\u0637 \u0641\u0631\u0634\u0627\u0629 \u0645\u0631\u0626\u064a\u0629 \u0648\u0628\u0631\u064a\u0642\u064b\u0627 \u064a\u0634\u0628\u0647 \u0627\u0644\u0633\u0627\u062a\u0627\u0646. \u0648\u064a\u062a\u0637\u0644\u0628 \u0627\u0644\u062a\u0646\u0638\u064a\u0641 \u0627\u0644\u0645\u0646\u062a\u0638\u0645 \u0644\u0644\u062d\u0641\u0627\u0638 \u0639\u0644\u0649 \u0645\u0638\u0647\u0631\u0647\u060c \u0648\u062a\u0643\u0648\u0646 \u0627\u0644\u062a\u0643\u0644\u0641\u0629 \u0623\u0639\u0644\u0649 \u0628\u0633\u0628\u0628 \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0625\u0636\u0627\u0641\u064a\u0629. \u0648\u0645\u062a\u0627\u0646\u0629 \u0627\u0644\u062a\u0634\u0637\u064a\u0628 \u0627\u0644\u0645\u0635\u0642\u0648\u0644 \u0645\u0639\u062a\u062f\u0644\u0629\u060c \u0648\u064a\u064f\u0633\u062a\u062e\u062f\u0645 \u0639\u0627\u062f\u0629\u064b \u0641\u064a \u0627\u0644\u0623\u062c\u0647\u0632\u0629 \u0627\u0644\u0645\u0637\u0628\u062e\u064a\u0629 \u0648\u0627\u0644\u0639\u0646\u0627\u0635\u0631 \u0627\u0644\u0645\u0639\u0645\u0627\u0631\u064a\u0629 \u0648\u0632\u062e\u0627\u0631\u0641 \u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a.<\/p><p class=\"wp-block-paragraph\">\u062a\u062a\u0645\u064a\u0632 \u0627\u0644\u062a\u0634\u0637\u064a\u0628\u0627\u062a \u0627\u0644\u0645\u0635\u0642\u0648\u0644\u0629 \u0628\u0644\u0645\u0639\u0627\u0646\u0647\u0627 \u0627\u0644\u0644\u0627\u0645\u0639 \u0627\u0644\u0630\u064a \u064a\u0634\u0628\u0647 \u0627\u0644\u0645\u0631\u0622\u0629 \u0648\u062a\u062a\u0637\u0644\u0628 \u0627\u0644\u062a\u0646\u0638\u064a\u0641 \u0648\u0627\u0644\u0639\u0646\u0627\u064a\u0629 \u0627\u0644\u0645\u062a\u0643\u0631\u0631\u0629 \u0644\u0644\u062d\u0641\u0627\u0638 \u0639\u0644\u0649 \u0645\u0638\u0647\u0631\u0647\u0627. \u0648\u0647\u064a \u0627\u0644\u062e\u064a\u0627\u0631 \u0627\u0644\u0623\u0643\u062b\u0631 \u062a\u0643\u0644\u0641\u0629 \u0628\u0633\u0628\u0628 \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0645\u0643\u062b\u0641\u0629. \u0648\u0641\u064a \u062d\u064a\u0646 \u0623\u0646 \u0627\u0644\u062a\u0634\u0637\u064a\u0628\u0627\u062a \u0627\u0644\u0645\u0635\u0642\u0648\u0644\u0629 \u0645\u0639\u0631\u0636\u0629 \u0644\u0644\u062e\u062f\u0648\u0634 \u0648\u0627\u0644\u0628\u0642\u0639\u060c \u0625\u0644\u0627 \u0623\u0646\u0647\u0627 \u062a\u064f\u0633\u062a\u062e\u062f\u0645 \u063a\u0627\u0644\u0628\u064b\u0627 \u0641\u064a \u0627\u0644\u0639\u0646\u0627\u0635\u0631 \u0627\u0644\u0632\u062e\u0631\u0641\u064a\u0629 \u0648\u0627\u0644\u0623\u062c\u0647\u0632\u0629 \u0627\u0644\u0631\u0627\u0642\u064a\u0629 \u0648\u0627\u0644\u0645\u064a\u0632\u0627\u062a \u0627\u0644\u0645\u0639\u0645\u0627\u0631\u064a\u0629.<\/p><p class=\"wp-block-paragraph\"><strong>\u0642\u0631\u0627\u0621\u0629 \u0630\u0627\u062a \u0635\u0644\u0629<\/strong><br><a href=\"https:\/\/steelprogroup.com\/ar\/stainless-steel\/maintenance\/clean\/\">\u0643\u064a\u0641\u064a\u0629 \u062a\u0646\u0638\u064a\u0641 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623\u061f<\/a><\/p><h2 class=\"wp-block-heading\">\u0645\u0627 \u0647\u064a \u062e\u0634\u0648\u0646\u0629 \u0627\u0644\u0633\u0637\u062d\u061f<\/h2><p class=\"wp-block-paragraph\">\u062e\u0634\u0648\u0646\u0629 \u0627\u0644\u0633\u0637\u062d \u0647\u064a \u0645\u0642\u064a\u0627\u0633 \u0644\u0645\u0644\u0645\u0633 \u0627\u0644\u0633\u0637\u062d\u060c \u0648\u0639\u0627\u062f\u0629 \u0645\u0627 \u064a\u062a\u0645 \u0642\u064a\u0627\u0633\u0647\u0627 \u0628\u0627\u0644\u0645\u064a\u0643\u0631\u0648\u0646 (\u00b5m). \u062a\u0624\u062b\u0631 \u062e\u0634\u0648\u0646\u0629 \u0627\u0644\u0633\u0637\u062d \u0639\u0644\u0649 \u0645\u062f\u0649 \u0633\u0647\u0648\u0644\u0629 \u062a\u0646\u0638\u064a\u0641 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0648\u062e\u0635\u0627\u0626\u0635\u0647 \u0627\u0644\u0627\u062d\u062a\u0643\u0627\u0643\u064a\u0629 \u0648\u0642\u062f\u0631\u062a\u0647 \u0639\u0644\u0649 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644. \u062a\u0634\u0645\u0644 \u0627\u0644\u0645\u0639\u0644\u0645\u0627\u062a \u0627\u0644\u0645\u0633\u062a\u062e\u062f\u0645\u0629 \u0628\u0634\u0643\u0644 \u0634\u0627\u0626\u0639 \u0645\u0627 \u064a\u0644\u064a:<\/p><p class=\"wp-block-paragraph\">RA (\u0645\u062a\u0648\u0633\u0637 \u0627\u0644\u062e\u0634\u0648\u0646\u0629): \u064a\u0634\u064a\u0631 \u0625\u0644\u0649 \u0645\u062a\u0648\u0633\u0637 \u062e\u0634\u0648\u0646\u0629 \u0627\u0644\u0633\u0637\u062d\u060c \u0648\u0647\u0648 \u0623\u062d\u062f \u0627\u0644\u0645\u0639\u0627\u064a\u064a\u0631 \u0627\u0644\u0645\u0633\u062a\u062e\u062f\u0645\u0629 \u0628\u0634\u0643\u0644 \u0634\u0627\u0626\u0639 \u0641\u064a \u0623\u0645\u0631\u064a\u0643\u0627 \u0627\u0644\u0634\u0645\u0627\u0644\u064a\u0629. \u0648\u0647\u0648 \u064a\u0635\u0641 \u0646\u0639\u0648\u0645\u0629 \u0627\u0644\u0633\u0637\u062d \u0645\u0646 \u062e\u0644\u0627\u0644 \u062d\u0633\u0627\u0628 \u0627\u0644\u0642\u064a\u0645\u0629 \u0627\u0644\u0645\u062a\u0648\u0633\u0637\u0629 \u0644\u0646\u0642\u0627\u0637 \u0627\u0644\u0633\u0637\u062d \u0627\u0644\u0645\u0631\u062a\u0641\u0639\u0629 \u0648\u0627\u0644\u0645\u0646\u062e\u0641\u0636\u0629. \u0648\u0643\u0644\u0645\u0627 \u0643\u0627\u0646\u062a \u0642\u064a\u0645\u0629 RA \u0623\u0635\u063a\u0631\u060c \u0643\u0627\u0646 \u0627\u0644\u0633\u0637\u062d \u0623\u0643\u062b\u0631 \u0646\u0639\u0648\u0645\u0629.<\/p><p class=\"wp-block-paragraph\">Rz (\u0645\u062a\u0648\u0633\u0637 \u0639\u0645\u0642 \u0627\u0644\u062e\u0634\u0648\u0646\u0629): \u064a\u0634\u064a\u0631 \u0625\u0644\u0649 \u0623\u0642\u0635\u0649 \u0639\u0645\u0642 \u0644\u0644\u0633\u0637\u062d \u0645\u0646 \u0627\u0644\u0642\u0645\u0629 \u0625\u0644\u0649 \u0627\u0644\u0648\u0627\u062f\u064a\u060c \u0648\u0647\u0648 \u0645\u0639\u0627\u0645\u0644 \u0645\u0633\u062a\u062e\u062f\u0645 \u0628\u0634\u0643\u0644 \u0634\u0627\u0626\u0639 \u0641\u064a \u0623\u0648\u0631\u0648\u0628\u0627. \u064a\u0635\u0641 \u062e\u0634\u0648\u0646\u0629 \u0627\u0644\u0633\u0637\u062d \u0639\u0646 \u0637\u0631\u064a\u0642 \u0642\u064a\u0627\u0633 \u0627\u0644\u0639\u0645\u0642 \u0628\u064a\u0646 \u0623\u0639\u0644\u0649 \u0648\u0623\u062f\u0646\u0649 \u0646\u0642\u0637\u0629 \u0639\u0644\u0649 \u0627\u0644\u0633\u0637\u062d. \u0643\u0644\u0645\u0627 \u0632\u0627\u062f\u062a \u0642\u064a\u0645\u0629 Rz\u060c \u0643\u0644\u0645\u0627 \u0643\u0627\u0646 \u0627\u0644\u0633\u0637\u062d \u0623\u0643\u062b\u0631 \u062e\u0634\u0648\u0646\u0629.<\/p><h2 class=\"wp-block-heading\">\u0645\u0627 \u0647\u0648 RA \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0641\u064a \u0646\u0647\u0627\u064a\u0629 \u0627\u0644\u0645\u0637\u0627\u0641\u061f<\/h2><p class=\"wp-block-paragraph\">\u064a\u062a\u0631\u0627\u0648\u062d \u0645\u062a\u0648\u0633\u0637 \u062e\u0634\u0648\u0646\u0629 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0645\u0637\u0644\u064a \u0628\u0627\u0644\u0645\u0637\u062d\u0646\u0629 \u0639\u0627\u062f\u0629\u064b \u0645\u0646 \u062d\u0648\u0627\u0644\u064a <strong>0.8 \u0625\u0644\u0649 3.2 \u0645\u064a\u0643\u0631\u0648\u0645\u062a\u0631<\/strong> (32 \u0625\u0644\u0649 125 \u0645\u064a\u0643\u0631\u0648\u0628\u0648\u0635\u0629). \u064a\u0645\u0643\u0646 \u0623\u0646 \u062a\u062e\u062a\u0644\u0641 \u0647\u0630\u0647 \u0627\u0644\u062e\u0634\u0648\u0646\u0629 \u0648\u0641\u0642\u064b\u0627 \u0644\u0637\u0631\u0642 \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0648\u0627\u0644\u062a\u0634\u0637\u064a\u0628 \u0627\u0644\u0645\u062d\u062f\u062f\u0629 \u0627\u0644\u0645\u0633\u062a\u062e\u062f\u0645\u0629.<\/p><h2 class=\"wp-block-heading\">\u0645\u062e\u0637\u0637 \u0644\u0645\u0633\u0627\u062a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623<\/h2><p class=\"wp-block-paragraph\">\u0628\u0627\u0644\u0625\u0636\u0627\u0641\u0629 \u0625\u0644\u0649 \u0627\u0644\u062a\u0634\u0637\u064a\u0628 \u0627\u0644\u0645\u0637\u062d\u0648\u0646 \u0648\u0627\u0644\u062a\u0634\u0637\u064a\u0628 \u0627\u0644\u0645\u0635\u0642\u0648\u0644 \u0648\u0627\u0644\u062a\u0634\u0637\u064a\u0628 \u0627\u0644\u0645\u0635\u0642\u0648\u0644\u060c \u0647\u0646\u0627\u0643 \u0627\u0644\u0639\u062f\u064a\u062f \u0645\u0646 \u0627\u0644\u0623\u0646\u0648\u0627\u0639 \u0627\u0644\u0623\u062e\u0631\u0649 \u0645\u0646 \u0627\u0644\u062a\u0634\u0637\u064a\u0628\u0627\u062a \u0627\u0644\u0633\u0637\u062d\u064a\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623\u060c \u0648\u0644\u0643\u0644 \u0645\u0646\u0647\u0627 \u062e\u0635\u0627\u0626\u0635 \u0641\u0631\u064a\u062f\u0629 \u0648\u0645\u062c\u0627\u0644\u0627\u062a \u062a\u0637\u0628\u064a\u0642 \u0641\u0631\u064a\u062f\u0629.<\/p><figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td>\u0646\u0648\u0639 \u0627\u0644\u062a\u0634\u0637\u064a\u0628<\/td><td>\u0648\u0635\u0641<\/td><td>\u0637\u0644\u0628<\/td><\/tr><tr><td>\u062a\u0634\u0637\u064a\u0628 \u0627\u0644\u0637\u0627\u062d\u0648\u0646\u0629<\/td><td>\u062a\u0634\u0637\u064a\u0628 \u0642\u064a\u0627\u0633\u064a \u0630\u0648 \u0633\u0637\u062d \u062e\u0634\u0646\u060c \u064a\u0633\u062a\u062e\u062f\u0645 \u0639\u0627\u062f\u0629 \u0643\u0646\u0642\u0637\u0629 \u0628\u062f\u0627\u064a\u0629 \u0644\u0644\u062a\u0634\u0637\u064a\u0628\u0627\u062a \u0627\u0644\u0623\u062e\u0631\u0649.<\/td><td>\u0627\u0644\u062a\u0635\u0646\u064a\u0639 \u0648\u0627\u0644\u0628\u0646\u0627\u0621 \u0627\u0644\u0639\u0627\u0645.<\/td><\/tr><tr><td>\u0644\u0645\u0633\u0629 \u0646\u0647\u0627\u0626\u064a\u0629 \u0645\u0635\u0642\u0648\u0644\u0629<\/td><td>\u0645\u0644\u0645\u0633 \u0646\u0627\u0639\u0645 \u0648\u062e\u0637\u064a \u062a\u0645 \u0625\u0646\u0634\u0627\u0624\u0647 \u0639\u0646 \u0637\u0631\u064a\u0642 \u0627\u0644\u062a\u0646\u0638\u064a\u0641 \u0628\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0645\u0646\u0635\u0627\u062a \u0643\u0627\u0634\u0637\u0629.<\/td><td>\u0627\u0644\u0623\u062c\u0647\u0632\u0629 \u0648\u0627\u0644\u062a\u062c\u0647\u064a\u0632\u0627\u062a \u0648\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0632\u062e\u0631\u0641\u064a\u0629.<\/td><\/tr><tr><td>\u0644\u0645\u0633\u0629 \u0646\u0647\u0627\u0626\u064a\u0629 \u0645\u0635\u0642\u0648\u0644\u0629<\/td><td>\u0633\u0637\u062d \u0639\u0627\u0643\u0633 \u0644\u0644\u063a\u0627\u064a\u0629 \u062a\u0645 \u062a\u062d\u0642\u064a\u0642\u0647 \u0645\u0646 \u062e\u0644\u0627\u0644 \u0627\u0644\u062a\u0644\u0645\u064a\u0639.<\/td><td>\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0631\u0627\u0642\u064a\u0629 \u0648\u0627\u0644\u0645\u062c\u0648\u0647\u0631\u0627\u062a \u0648\u0627\u0644\u0639\u0646\u0627\u0635\u0631 \u0627\u0644\u0632\u062e\u0631\u0641\u064a\u0629.<\/td><\/tr><tr><td>\u0644\u0645\u0633\u0629 \u0646\u0647\u0627\u0626\u064a\u0629 \u0645\u0646 \u0627\u0644\u0633\u0627\u062a\u0627\u0646<\/td><td>\u0633\u0637\u062d \u0623\u0645\u0644\u0633\u060c \u0630\u0648 \u0627\u0646\u0639\u0643\u0627\u0633 \u0645\u0646\u062e\u0641\u0636 \u0645\u0639 \u0627\u0644\u062d\u062f \u0627\u0644\u0623\u062f\u0646\u0649 \u0645\u0646 \u0627\u0644\u0645\u0644\u0645\u0633.<\/td><td>\u0627\u0644\u0639\u0646\u0627\u0635\u0631 \u0627\u0644\u0645\u0639\u0645\u0627\u0631\u064a\u0629 \u0648\u0645\u0639\u062f\u0627\u062a \u0627\u0644\u0645\u0637\u0628\u062e.<\/td><\/tr><tr><td>\u062e\u0631\u0632 \u0645\u062a\u0641\u062c\u0631<\/td><td>\u0645\u0644\u0645\u0633 \u063a\u064a\u0631 \u0644\u0627\u0645\u0639 \u063a\u064a\u0631 \u0627\u062a\u062c\u0627\u0647\u064a \u062a\u0645 \u0625\u0646\u0634\u0627\u0624\u0647 \u0639\u0646 \u0637\u0631\u064a\u0642 \u0627\u0644\u062a\u0641\u062c\u064a\u0631 \u0628\u0627\u0644\u062e\u0631\u0632.<\/td><td>\u0627\u0644\u062f\u064a\u0643\u0648\u0631\u0627\u062a \u0627\u0644\u0645\u0639\u0645\u0627\u0631\u064a\u0629 \u0648\u0627\u0644\u0645\u0646\u0634\u0622\u062a \u0627\u0644\u0641\u0646\u064a\u0629.<\/td><\/tr><tr><td>\u062a\u0634\u0637\u064a\u0628 \u0645\u0635\u0642\u0648\u0644 \u0643\u0647\u0631\u0628\u0627\u0626\u064a\u0627<\/td><td>\u0633\u0637\u062d \u0639\u0627\u0643\u0633 \u0644\u0644\u063a\u0627\u064a\u0629 \u0648\u0646\u0627\u0639\u0645 \u0645\u0646 \u0627\u0644\u062a\u0644\u0645\u064a\u0639 \u0627\u0644\u0643\u0647\u0631\u0648\u0643\u064a\u0645\u064a\u0627\u0626\u064a.<\/td><td>\u0627\u0644\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0637\u0628\u064a\u0629 \u0648\u0645\u0639\u062f\u0627\u062a \u062a\u062c\u0647\u064a\u0632 \u0627\u0644\u0623\u063a\u0630\u064a\u0629.<\/td><\/tr><tr><td>\u0644\u0645\u0633\u0629 \u0646\u0647\u0627\u0626\u064a\u0629 \u0645\u062d\u0641\u0648\u0631\u0629<\/td><td>\u0623\u0646\u0645\u0627\u0637 \u0632\u062e\u0631\u0641\u064a\u0629 \u0645\u062d\u0641\u0648\u0631\u0629 \u0639\u0644\u0649 \u0627\u0644\u0633\u0637\u062d.<\/td><td>\u0627\u0644\u0623\u0644\u0648\u0627\u062d \u0627\u0644\u0645\u0639\u0645\u0627\u0631\u064a\u0629 \u0648\u0627\u0644\u0632\u062e\u0627\u0631\u0641 \u0627\u0644\u0632\u062e\u0631\u0641\u064a\u0629.<\/td><\/tr><tr><td>\u0644\u0645\u0633\u0629 \u0646\u0647\u0627\u0626\u064a\u0629 \u0645\u0644\u0648\u0646\u0629<\/td><td>\u062a\u0645 \u062a\u0644\u0648\u064a\u0646 \u0627\u0644\u0633\u0637\u062d \u0645\u0646 \u062e\u0644\u0627\u0644 \u062a\u0642\u0646\u064a\u0629 PVD \u0648\u063a\u064a\u0631\u0647\u0627 \u0645\u0646 \u0627\u0644\u062a\u0642\u0646\u064a\u0627\u062a \u0644\u0644\u062d\u0635\u0648\u0644 \u0639\u0644\u0649 \u062a\u0623\u062b\u064a\u0631\u0627\u062a \u0628\u0635\u0631\u064a\u0629 \u063a\u0646\u064a\u0629.<\/td><td>\u0627\u0644\u062a\u0635\u0645\u064a\u0645 \u0627\u0644\u062f\u0627\u062e\u0644\u064a \u0648\u0627\u0644\u0645\u0646\u062a\u062c\u0627\u062a \u0627\u0644\u062f\u064a\u0643\u0648\u0631\u064a\u0629.<\/td><\/tr><tr><td>\u0644\u0645\u0633\u0629 \u0646\u0647\u0627\u0626\u064a\u0629 \u0645\u062d\u0628\u0628\u0629<\/td><td>\u0646\u0633\u064a\u062c \u0645\u0646\u0642\u0648\u0634 \u062a\u0645 \u0625\u0646\u0634\u0627\u0624\u0647 \u0639\u0646 \u0637\u0631\u064a\u0642 \u0627\u0644\u0644\u0641 \u0623\u0648 \u0627\u0644\u0636\u063a\u0637.<\/td><td>\u0648\u0627\u062c\u0647\u0627\u062a \u0627\u0644\u0645\u0635\u0627\u0639\u062f \u0648\u0627\u0644\u0645\u0628\u0627\u0646\u064a \u0627\u0644\u062f\u0627\u062e\u0644\u064a\u0629.<\/td><\/tr><tr><td>\u062a\u0634\u0637\u064a\u0628 \u062e\u0627\u0645\u0644<\/td><td>\u062a\u0645 \u062a\u062d\u0642\u064a\u0642 \u0645\u0642\u0627\u0648\u0645\u0629 \u0645\u0639\u0632\u0632\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0639\u0646 \u0637\u0631\u064a\u0642 \u0625\u0632\u0627\u0644\u0629 \u0627\u0644\u062d\u062f\u064a\u062f \u0627\u0644\u062d\u0631.<\/td><td>\u0627\u0644\u0645\u0639\u062f\u0627\u062a \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629 \u0648\u0627\u0644\u0623\u062c\u0647\u0632\u0629 \u0627\u0644\u0637\u0628\u064a\u0629.<\/td><\/tr><tr><td>\u0644\u0645\u0633\u0629 \u0646\u0647\u0627\u0626\u064a\u0629 \u063a\u064a\u0631 \u0644\u0627\u0645\u0639\u0629<\/td><td>\u0633\u0637\u062d \u063a\u064a\u0631 \u0639\u0627\u0643\u0633 \u062a\u0645 \u0625\u0646\u0634\u0627\u0624\u0647 \u0628\u0648\u0627\u0633\u0637\u0629 \u0627\u0644\u0637\u062d\u0646 \u0623\u0648 \u0627\u0644\u0646\u0641\u062e \u0627\u0644\u0631\u0645\u0644\u064a.<\/td><td>\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0635\u0646\u0627\u0639\u064a\u0629 \u0648\u0623\u062c\u0632\u0627\u0621 \u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a.<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u0645\u0627 \u0647\u0648 \u0623\u0641\u0636\u0644 \u0646\u0648\u0639 \u0645\u0639\u0627\u0644\u062c\u0629 \u0633\u0637\u062d\u064a\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623\u061f<\/h2><p class=\"wp-block-paragraph\">\u064a\u062a\u0637\u0644\u0628 \u0627\u062e\u062a\u064a\u0627\u0631 \u0623\u0641\u0636\u0644 \u0645\u0639\u0627\u0644\u062c\u0629 \u0644\u0633\u0637\u062d \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0645\u0631\u0627\u0639\u0627\u0629 \u0627\u0644\u0639\u062f\u064a\u062f \u0645\u0646 \u0627\u0644\u0639\u0648\u0627\u0645\u0644 \u0627\u0639\u062a\u0645\u0627\u062f\u064b\u0627 \u0639\u0644\u0649 \u0627\u0644\u062a\u0637\u0628\u064a\u0642 \u0648\u0627\u0644\u0645\u062a\u0637\u0644\u0628\u0627\u062a \u0627\u0644\u0645\u062d\u062f\u062f\u0629.<\/p><p class=\"wp-block-paragraph\">\u0645\u062a\u0637\u0644\u0628\u0627\u062a \u0627\u0644\u062a\u0637\u0628\u064a\u0642: \u062d\u062f\u062f \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0633\u0637\u062d\u064a\u0629 \u0627\u0644\u0645\u0646\u0627\u0633\u0628\u0629 \u0648\u0641\u0642\u064b\u0627 \u0644\u0645\u062a\u0637\u0644\u0628\u0627\u062a \u0627\u0644\u062a\u0637\u0628\u064a\u0642 \u0627\u0644\u0645\u062d\u062f\u062f\u0629. \u0639\u0644\u0649 \u0633\u0628\u064a\u0644 \u0627\u0644\u0645\u062b\u0627\u0644\u060c \u0642\u062f \u062a\u062a\u0637\u0644\u0628 \u0627\u0644\u0632\u062e\u0627\u0631\u0641 \u0627\u0644\u0645\u0639\u0645\u0627\u0631\u064a\u0629 \u0627\u0644\u062a\u0634\u0637\u064a\u0628 \u0628\u0627\u0644\u0641\u0631\u0634\u0627\u0629\u060c \u0628\u064a\u0646\u0645\u0627 \u0642\u062f \u062a\u0643\u0648\u0646 \u0645\u0639\u062f\u0627\u062a \u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0623\u063a\u0630\u064a\u0629 \u0623\u0643\u062b\u0631 \u0645\u0644\u0627\u0621\u0645\u0629 \u0644\u0644\u062a\u0634\u0637\u064a\u0628 2B.<\/p><p class=\"wp-block-paragraph\">\u0627\u0644\u0642\u064a\u0648\u062f \u0627\u0644\u0645\u0627\u0644\u064a\u0629: \u0627\u062e\u062a\u0631 \u0637\u0631\u064a\u0642\u0629 \u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0642\u062a\u0635\u0627\u062f\u064a\u0629 \u0628\u0646\u0627\u0621\u064b \u0639\u0644\u0649 \u0645\u064a\u0632\u0627\u0646\u064a\u0629 \u0627\u0644\u0645\u0634\u0631\u0648\u0639. \u0639\u0644\u0649 \u0633\u0628\u064a\u0644 \u0627\u0644\u0645\u062b\u0627\u0644\u060c \u064a\u0639\u062f Mill Finish \u062e\u064a\u0627\u0631\u064b\u0627 \u0645\u0646\u0627\u0633\u0628\u064b\u0627 \u0644\u0644\u0645\u0634\u0627\u0631\u064a\u0639 \u0630\u0627\u062a \u0627\u0644\u0645\u064a\u0632\u0627\u0646\u064a\u0627\u062a \u0627\u0644\u0645\u062d\u062f\u0648\u062f\u0629.<\/p><p class=\"wp-block-paragraph\">\u0645\u062a\u0637\u0644\u0628\u0627\u062a \u0627\u0644\u0645\u0638\u0647\u0631: \u0627\u062e\u062a\u0631 \u0637\u0631\u064a\u0642\u0629 \u0645\u0639\u0627\u0644\u062c\u0629 \u0644\u0627\u0645\u0639\u0629 \u0623\u0648 \u0646\u0627\u0639\u0645\u0629 \u0628\u0646\u0627\u0621\u064b \u0639\u0644\u0649 \u0645\u062a\u0637\u0644\u0628\u0627\u062a \u0627\u0644\u0645\u0638\u0647\u0631. \u0639\u0644\u0649 \u0633\u0628\u064a\u0644 \u0627\u0644\u0645\u062b\u0627\u0644\u060c \u064a\u0645\u0643\u0646 \u0644\u0644\u0623\u062c\u0632\u0627\u0621 \u0627\u0644\u0632\u062e\u0631\u0641\u064a\u0629 \u0627\u0644\u062a\u064a \u062a\u062a\u0637\u0644\u0628 \u062a\u0623\u062b\u064a\u0631\u064b\u0627 \u0628\u0635\u0631\u064a\u064b\u0627 \u0639\u0627\u0644\u064a\u064b\u0627 \u0627\u062e\u062a\u064a\u0627\u0631 \u0627\u0644\u062a\u0634\u0637\u064a\u0628 \u0627\u0644\u0645\u0635\u0642\u0648\u0644.<\/p><p class=\"wp-block-paragraph\">\u0645\u062a\u0637\u0644\u0628\u0627\u062a \u0627\u0644\u0645\u062a\u0627\u0646\u0629: \u0627\u062e\u062a\u064a\u0627\u0631 \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0627\u062a \u0627\u0644\u0645\u0646\u0627\u0633\u0628\u0629 \u0644\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644 \u0648\u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0645\u064a\u0643\u0627\u0646\u064a\u0643\u064a\u0629. \u0639\u0644\u0649 \u0633\u0628\u064a\u0644 \u0627\u0644\u0645\u062b\u0627\u0644\u060c \u0642\u062f \u062a\u062a\u0637\u0644\u0628 \u0627\u0644\u0645\u0639\u062f\u0627\u062a \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629 \u062a\u0634\u0637\u064a\u0628\u064b\u0627 \u0631\u0642\u0645 4 \u0644\u062a\u062d\u0633\u064a\u0646 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644.<\/p><h2 class=\"wp-block-heading\">\u0627\u062d\u0635\u0644 \u0639\u0644\u0649 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0645\u064f\u0631\u0636\u064a!<\/h2><p class=\"wp-block-paragraph\">\u0625\u0630\u0627 \u0643\u0646\u062a \u062a\u062a\u0633\u0627\u0621\u0644 \u0639\u0646 \u0645\u0646\u062a\u062c\u0627\u062a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0630\u0627\u062a \u0627\u0644\u0644\u0645\u0633\u0627\u062a \u0627\u0644\u0646\u0647\u0627\u0626\u064a\u0629 \u0627\u0644\u0645\u0637\u062d\u0648\u0646\u0629\u060c \u0623\u0648 \u062a\u062a\u0633\u0627\u0621\u0644 \u0639\u0645\u0627 \u0625\u0630\u0627 \u0643\u0627\u0646 \u0646\u0648\u0639 \u0645\u0639\u064a\u0646 \u0645\u0646 \u0627\u0644\u0644\u0645\u0633\u0627\u062a \u0627\u0644\u0646\u0647\u0627\u0626\u064a\u0629 \u0645\u0646\u0627\u0633\u0628\u064b\u0627 \u0644\u0643\u060c \u0641\u0625\u0646 \u0645\u062c\u0645\u0648\u0639\u0629 SteelPRO \u0647\u0646\u0627 \u0644\u0645\u0633\u0627\u0639\u062f\u062a\u0643. \u0627\u0646\u0642\u0631 \u0647\u0646\u0627 \u0644\u0645\u0639\u0631\u0641\u0629 \u0627\u0644\u0645\u0632\u064a\u062f \u0639\u0646 <a href=\"https:\/\/steelprogroup.com\/ar\/blog\/\">\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623<\/a>\u060c \u0623\u0648 <a href=\"https:\/\/steelprogroup.com\/ar\/contact-us\/\">\u0627\u062a\u0635\u0644 \u0628\u0646\u0627 <\/a>\u0627\u062a\u0635\u0644 \u0628\u0641\u0631\u064a\u0642 \u0627\u0644\u0645\u0628\u064a\u0639\u0627\u062a \u0627\u0644\u064a\u0648\u0645 \u0644\u0645\u0646\u0627\u0642\u0634\u0629 \u0645\u062a\u0637\u0644\u0628\u0627\u062a \u0645\u0634\u0631\u0648\u0639\u0643.<\/p>","protected":false},"excerpt":{"rendered":"<p>\u0625\u0646 \u0641\u0647\u0645 \u0627\u0644\u0645\u0641\u0627\u0647\u064a\u0645 \u0627\u0644\u0623\u0633\u0627\u0633\u064a\u0629 \u0644\u0644\u0637\u062d\u0646 \u0648\u0639\u0645\u0644\u064a\u0629 \u0627\u0644\u062a\u0635\u0646\u064a\u0639 \u0648\u0643\u064a\u0641\u064a\u0629 \u0645\u0642\u0627\u0631\u0646\u062a\u0647\u0627 \u0628\u0645\u0639\u0627\u0644\u062c\u0627\u062a \u0627\u0644\u0633\u0637\u062d \u0627\u0644\u0623\u062e\u0631\u0649 \u0623\u0645\u0631 \u0636\u0631\u0648\u0631\u064a [\u2026]<\/p>","protected":false},"author":1,"featured_media":10669,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"_eb_attr":"","rank_math_lock_modified_date":false,"site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"categories":[4196,112],"tags":[],"class_list":["post-10689","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-finish","category-stainless-steel"],"acf":[],"_links":{"self":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts\/10689","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/comments?post=10689"}],"version-history":[{"count":0,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts\/10689\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/media\/10669"}],"wp:attachment":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/media?parent=10689"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/categories?post=10689"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/tags?post=10689"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}