{"id":10946,"date":"2024-09-30T05:14:00","date_gmt":"2024-09-29T21:14:00","guid":{"rendered":"https:\/\/app11147.cloudwayssites.com\/?p=10946"},"modified":"2024-09-30T13:10:06","modified_gmt":"2024-09-30T05:10:06","slug":"production","status":"publish","type":"post","link":"https:\/\/steelprogroup.com\/ar\/stainless-steel\/production\/","title":{"rendered":"\u0625\u0646\u062a\u0627\u062c \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623"},"content":{"rendered":"<p class=\"wp-block-paragraph\">\u064a\u062a\u0645\u062a\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0628\u0645\u0642\u0627\u0648\u0645\u0629 \u0639\u0627\u0644\u064a\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0648\u0645\u062a\u0627\u0646\u0629 \u0637\u0648\u064a\u0644\u0629 \u0627\u0644\u0623\u0645\u062f \u0648\u0627\u062d\u062a\u064a\u0627\u062c\u0627\u062a \u0635\u064a\u0627\u0646\u0629 \u0628\u0633\u064a\u0637\u0629 \u0641\u064a \u0638\u0631\u0648\u0641 \u0645\u062a\u0646\u0648\u0639\u0629. \u064a\u0633\u0627\u0639\u062f\u0646\u0627 \u0641\u0647\u0645 \u0643\u064a\u0641\u064a\u0629 \u062a\u0635\u0646\u064a\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0641\u064a \u062a\u0642\u062f\u064a\u0631 \u0642\u064a\u0645\u062a\u0647 \u0648\u062a\u0646\u0648\u0639\u0647 \u0641\u064a \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u064a\u0648\u0645\u064a\u0629. \u062f\u0639\u0646\u0627 \u0646\u0633\u062a\u0643\u0634\u0641 \u0643\u064a\u0641\u064a\u0629 \u062a\u0635\u0646\u064a\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u062e\u0637\u0648\u0629 \u0628\u062e\u0637\u0648\u0629.<\/p><h2 class=\"wp-block-heading\">\u0645\u0646 \u0645\u0627\u0630\u0627 \u064a\u062a\u0643\u0648\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623\u061f<\/h2><p class=\"wp-block-paragraph\">\u064a\u062a\u0645 \u062a\u0635\u0646\u064a\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0645\u0646 \u0645\u0632\u064a\u062c \u0645\u0646 \u0627\u0644\u0645\u0648\u0627\u062f \u0627\u0644\u062e\u0627\u0645\u060c \u0648\u064a\u062e\u062a\u0644\u0641 \u0627\u0644\u062a\u0631\u0643\u064a\u0628 \u0627\u0644\u062f\u0642\u064a\u0642 \u0627\u0639\u062a\u0645\u0627\u062f\u064b\u0627 \u0639\u0644\u0649 \u0639\u0627\u0626\u0644\u0629 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623.&nbsp;<\/p><p class=\"wp-block-paragraph\">\u0641\u064a\u0645\u0627 \u064a\u0644\u064a \u062c\u062f\u0648\u0644 \u064a\u0648\u0636\u062d \u0627\u0644\u0645\u0643\u0648\u0646\u0627\u062a \u0627\u0644\u0623\u0633\u0627\u0633\u064a\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623:<\/p><figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td><strong>\u0627\u0644\u0645\u0648\u0627\u062f \u0627\u0644\u062e\u0627\u0645<\/strong><\/td><td><strong>\u062e\u0635\u0627\u0626\u0635 \u0630\u0627\u062a \u0635\u0644\u0629<\/strong><\/td><\/tr><tr><td>\u062e\u0627\u0645 \u0627\u0644\u062d\u062f\u064a\u062f<\/td><td>\u0627\u0644\u0642\u0648\u0629 \u0648\u0627\u0644\u0628\u0646\u064a\u0629 \u0627\u0644\u0623\u0633\u0627\u0633\u064a\u0629<\/td><\/tr><tr><td>\u0627\u0644\u0643\u0631\u0648\u0645<\/td><td>\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644<\/td><\/tr><tr><td>\u0627\u0644\u0646\u064a\u0643\u0644<\/td><td>\u0627\u0644\u0642\u0648\u0629 \u0648\u0627\u0644\u0645\u0631\u0648\u0646\u0629 \u0648\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644<\/td><\/tr><tr><td>\u0627\u0644\u0645\u0648\u0644\u064a\u0628\u062f\u064a\u0646\u0648\u0645<\/td><td>\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644 \u0648\u0627\u0644\u062a\u0622\u0643\u0644 \u0627\u0644\u0646\u0627\u062a\u062c \u0639\u0646 \u0627\u0644\u0634\u0642\u0648\u0642\u061b \u0627\u0644\u0642\u0648\u0629<\/td><\/tr><tr><td>\u0627\u0644\u0643\u0631\u0628\u0648\u0646<\/td><td>\u0627\u0646\u062e\u0641\u0627\u0636 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644<\/td><\/tr><tr><td>\u0627\u0644\u0645\u0646\u063a\u0646\u064a\u0632<\/td><td>\u0627\u0644\u0642\u0648\u0629 \u0648\u0627\u0644\u0635\u0644\u0627\u0628\u0629<\/td><\/tr><tr><td>\u0627\u0644\u0633\u064a\u0644\u064a\u0643\u0648\u0646<\/td><td>\u0627\u0644\u0642\u0648\u0629 \u0648\u0627\u0644\u0645\u0631\u0648\u0646\u0629<\/td><\/tr><\/tbody><\/table><\/figure><ul class=\"wp-block-list\"><li>\u064a\u0645\u0643\u0646 \u0625\u0636\u0627\u0641\u0629 \u0627\u0644\u0646\u064a\u062a\u0631\u0648\u062c\u064a\u0646 \u0648\u0627\u0644\u062a\u064a\u062a\u0627\u0646\u064a\u0648\u0645 \u0648\u0627\u0644\u0646\u062d\u0627\u0633 \u0648\u0639\u0646\u0627\u0635\u0631 \u0623\u062e\u0631\u0649 \u0644\u062a\u062d\u0642\u064a\u0642 \u062e\u0635\u0627\u0626\u0635 \u0645\u062d\u062f\u062f\u0629 \u0645\u062b\u0644 \u0632\u064a\u0627\u062f\u0629 \u0627\u0644\u0642\u0648\u0629 \u0623\u0648 \u062a\u062d\u0633\u064a\u0646 \u0642\u0627\u0628\u0644\u064a\u0629 \u0627\u0644\u0644\u062d\u0627\u0645.<\/li><\/ul><h2 class=\"wp-block-heading\">\u0643\u064a\u0641 \u064a\u062a\u0645 \u062a\u0635\u0646\u064a\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623\u061f<\/h2><p class=\"wp-block-paragraph\">\u062a\u062a\u0636\u0645\u0646 \u0639\u0645\u0644\u064a\u0629 \u0625\u0646\u062a\u0627\u062c \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0639\u062f\u0629 \u062e\u0637\u0648\u0627\u062a \u0645\u062a\u0633\u0644\u0633\u0644\u0629. \u0648\u062a\u0639\u062a\u0628\u0631 \u0643\u0644 \u0645\u0631\u062d\u0644\u0629 \u062d\u0627\u0633\u0645\u0629 \u0644\u062a\u062d\u0642\u064a\u0642 \u0627\u0644\u062c\u0648\u062f\u0629 \u0648\u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0645\u0637\u0644\u0648\u0628\u0629 \u0644\u0644\u0645\u0646\u062a\u062c \u0627\u0644\u0646\u0647\u0627\u0626\u064a.<\/p><h3 class=\"wp-block-heading\">\u062a\u0635\u0646\u064a\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623<\/h3><ol class=\"wp-block-list\"><li>\u0627\u0644\u0635\u0647\u0631 \u0648\u0627\u0644\u0635\u0628<\/li><\/ol><p class=\"wp-block-paragraph\">\u064a\u062a\u0645 \u062a\u062d\u0645\u064a\u0644 \u0627\u0644\u0645\u0648\u0627\u062f \u0627\u0644\u062e\u0627\u0645 \u0645\u062b\u0644 \u062e\u0627\u0645 \u0627\u0644\u062d\u062f\u064a\u062f \u0648\u0627\u0644\u0643\u0631\u0648\u0645 \u0648\u0627\u0644\u0646\u064a\u0643\u0644 \u0648\u0639\u0646\u0627\u0635\u0631 \u0623\u062e\u0631\u0649 \u0641\u064a \u0641\u0631\u0646 \u0627\u0644\u0642\u0648\u0633 \u0627\u0644\u0643\u0647\u0631\u0628\u0627\u0626\u064a. \u064a\u0642\u0648\u0645 \u0627\u0644\u0641\u0631\u0646 \u0628\u062a\u0633\u062e\u064a\u0646 \u0627\u0644\u062e\u0644\u064a\u0637 \u0625\u0644\u0649 \u062d\u0648\u0627\u0644\u064a 1600 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629. \u0628\u0645\u062c\u0631\u062f \u0630\u0648\u0628\u0627\u0646\u0647\u0627\u060c \u062a\u062a\u062d\u062f \u0647\u0630\u0647 \u0627\u0644\u0645\u0648\u0627\u062f \u0644\u062a\u0643\u0648\u064a\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0645\u0646\u0635\u0647\u0631.<\/p><ol start=\"2\" class=\"wp-block-list\"><li>\u0625\u0632\u0627\u0644\u0629 \u0627\u0644\u0643\u0631\u0628\u0646\u0629<\/li><\/ol><ul class=\"wp-block-list\"><li>\u0625\u0632\u0627\u0644\u0629 \u0627\u0644\u0643\u0631\u0628\u0646\u0629 \u0645\u0646 \u0627\u0644\u0623\u0631\u062c\u0648\u0646 \u0648\u0627\u0644\u0623\u0643\u0633\u062c\u064a\u0646 (AOD)<\/li><\/ul><p class=\"wp-block-paragraph\">\u0627\u0646\u0642\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0646\u0635\u0647\u0631 \u0625\u0644\u0649 \u0648\u0639\u0627\u0621 AOD. \u064a\u062a\u0645 \u062d\u0642\u0646 \u063a\u0627\u0632\u064a \u0627\u0644\u0623\u0643\u0633\u062c\u064a\u0646 \u0648\u0627\u0644\u0623\u0631\u062c\u0648\u0646. \u064a\u0632\u064a\u0644 \u0627\u0644\u0623\u0643\u0633\u062c\u064a\u0646 \u0627\u0644\u0643\u0631\u0628\u0648\u0646 \u0627\u0644\u0632\u0627\u0626\u062f \u0639\u0646 \u0637\u0631\u064a\u0642 \u062a\u0643\u0648\u064a\u0646 \u063a\u0627\u0632 \u0623\u0648\u0644 \u0623\u0643\u0633\u064a\u062f \u0627\u0644\u0643\u0631\u0628\u0648\u0646. \u064a\u062e\u0641\u0641 \u0627\u0644\u0623\u0631\u062c\u0648\u0646 \u062e\u0644\u064a\u0637 \u0627\u0644\u063a\u0627\u0632 \u0644\u0644\u062a\u062d\u0643\u0645 \u0641\u064a \u0645\u0639\u062f\u0644 \u0627\u0644\u062a\u0641\u0627\u0639\u0644.&nbsp;<\/p><p class=\"wp-block-paragraph\">\u064a\u062a\u0645 \u0627\u0633\u062a\u062e\u062f\u0627\u0645 AOD \u0641\u064a \u0645\u0639\u0638\u0645 \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a.<\/p><ul class=\"wp-block-list\"><li>\u0625\u0632\u0627\u0644\u0629 \u0627\u0644\u0643\u0631\u0628\u0646\u0629 \u0628\u0627\u0644\u0623\u0643\u0633\u062c\u064a\u0646 \u062a\u062d\u062a \u0627\u0644\u062a\u0641\u0631\u064a\u063a (VOD)<\/li><\/ul><p class=\"wp-block-paragraph\">\u0627\u0646\u0642\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0646\u0635\u0647\u0631 \u0625\u0644\u0649 \u062d\u062c\u0631\u0629 \u0645\u0641\u0631\u063a\u0629 \u0645\u0646 \u0627\u0644\u0647\u0648\u0627\u0621. \u064a\u062a\u0645 \u062d\u0642\u0646 \u0627\u0644\u0623\u0643\u0633\u062c\u064a\u0646 \u0644\u0644\u062a\u0641\u0627\u0639\u0644 \u0645\u0639 \u0627\u0644\u0643\u0631\u0628\u0648\u0646\u060c \u0645\u0643\u0648\u0646\u064b\u0627 \u063a\u0627\u0632 \u0623\u0648\u0644 \u0623\u0643\u0633\u064a\u062f \u0627\u0644\u0643\u0631\u0628\u0648\u0646\u060c \u0648\u0627\u0644\u0630\u064a \u064a\u062a\u0645 \u0625\u0632\u0627\u0644\u062a\u0647 \u062a\u062d\u062a \u0636\u063a\u0637 \u0645\u0646\u062e\u0641\u0636.&nbsp;<\/p><p class=\"wp-block-paragraph\">\u064a\u062a\u0645 \u0627\u0633\u062a\u062e\u062f\u0627\u0645 VOD \u0639\u0646\u062f\u0645\u0627 \u062a\u0643\u0648\u0646 \u0647\u0646\u0627\u0643 \u062d\u0627\u062c\u0629 \u0625\u0644\u0649 \u0645\u062d\u062a\u0648\u0649 \u0645\u0646\u062e\u0641\u0636 \u0644\u0644\u063a\u0627\u064a\u0629 \u0645\u0646 \u0627\u0644\u0643\u0631\u0628\u0648\u0646 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0639\u0627\u0644\u064a \u0627\u0644\u062c\u0648\u062f\u0629 \u0645\u062b\u0644 304L.<\/p><ul class=\"wp-block-list\"><li>\u0645\u0646 \u062e\u0644\u0627\u0644 \u062e\u0641\u0636 \u0645\u062d\u062a\u0648\u0649 \u0627\u0644\u0643\u0631\u0628\u0648\u0646\u060c \u064a\u0642\u0648\u0645 \u0627\u0644\u0645\u0635\u0646\u0639\u0648\u0646 \u0628\u0625\u0646\u0634\u0627\u0621 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0645\u0646\u062e\u0641\u0636 \u0627\u0644\u0643\u0631\u0628\u0648\u0646 \u0645\u062b\u0644 304L \u0648316L. \u0648\u0642\u062f \u062a\u062d\u0633\u0646\u062a \u0642\u0627\u0628\u0644\u064a\u0629 \u0627\u0644\u0644\u062d\u0627\u0645 \u0644\u0647\u0630\u0647 \u0627\u0644\u0641\u0648\u0644\u0627\u0630\u0627\u062a \u0648\u0642\u0644\u0644\u062a \u0645\u0646 \u062e\u0637\u0631 \u0627\u0644\u062a\u0622\u0643\u0644.<\/li><\/ul><ol start=\"3\" class=\"wp-block-list\"><li>\u0636\u0628\u0637 \u0627\u0644\u062a\u0643\u0648\u064a\u0646<\/li><\/ol><p class=\"wp-block-paragraph\">\u064a\u062a\u0645 \u0625\u0636\u0627\u0641\u0629 \u0639\u0646\u0627\u0635\u0631 \u0625\u0636\u0627\u0641\u064a\u0629 \u0645\u062b\u0644 \u0627\u0644\u0646\u064a\u0643\u0644 \u0648\u0627\u0644\u0645\u0648\u0644\u064a\u0628\u062f\u064a\u0646\u0648\u0645 \u0648\u0627\u0644\u0646\u064a\u062a\u0631\u0648\u062c\u064a\u0646 \u0644\u062a\u0639\u0632\u064a\u0632 \u0627\u0644\u0642\u0648\u0629 \u0648\u0627\u0644\u0645\u0631\u0648\u0646\u0629 \u0648\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644\u060c \u0627\u0639\u062a\u0645\u0627\u062f\u064b\u0627 \u0639\u0644\u0649 \u062f\u0631\u062c\u0629 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0637\u0644\u0648\u0628\u0629. \u062a\u0630\u0648\u0628 \u0647\u0630\u0647 \u0627\u0644\u0639\u0646\u0627\u0635\u0631 \u0641\u064a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0646\u0635\u0647\u0631\u060c \u0645\u0645\u0627 \u064a\u063a\u064a\u0631 \u062e\u0635\u0627\u0626\u0635\u0647.<\/p><ol start=\"4\" class=\"wp-block-list\"><li>\u0635\u0628<\/li><\/ol><p class=\"wp-block-paragraph\">\u0627\u0646\u0642\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0646\u0635\u0647\u0631 \u0625\u0644\u0649 \u0642\u0627\u0644\u0628 \u062d\u064a\u062b \u0633\u064a\u062a\u0635\u0644\u0628. \u064a\u0628\u0631\u062f \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0648\u0644\u0643\u0646\u0647 \u064a\u0638\u0644 \u0639\u0646\u062f \u062f\u0631\u062c\u0629 \u062d\u0631\u0627\u0631\u0629 \u0623\u0639\u0644\u0649 \u0645\u0646 1200 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \u0623\u062b\u0646\u0627\u0621 \u0627\u0644\u0635\u0628. \u064a\u062d\u062f\u062f \u0627\u0644\u0634\u0643\u0644 \u0627\u0644\u0646\u0627\u062a\u062c \u0623\u062b\u0646\u0627\u0621 \u0627\u0644\u0635\u0628 \u0634\u0643\u0644 \u0627\u0644\u0645\u0646\u062a\u062c \u0627\u0644\u0646\u0647\u0627\u0626\u064a\u060c \u0645\u062b\u0644 \u0627\u0644\u0623\u0644\u0648\u0627\u062d \u0623\u0648 \u0627\u0644\u0642\u0636\u0628\u0627\u0646.<\/p><ul class=\"wp-block-list\"><li>\u0627\u0644\u0623\u0644\u0648\u0627\u062d: \u062a\u0633\u062a\u062e\u062f\u0645 \u0644\u0635\u0646\u0639 \u0627\u0644\u0635\u0641\u0627\u0626\u062d \u0648\u0627\u0644\u0623\u0644\u0648\u0627\u062d.<\/li>\n\n<li>\u0627\u0644\u0643\u062a\u0644: \u062a\u0633\u062a\u062e\u062f\u0645 \u0644\u0625\u0646\u062a\u0627\u062c \u0627\u0644\u0642\u0636\u0628\u0627\u0646 \u0648\u0627\u0644\u0623\u0633\u0644\u0627\u0643.<\/li>\n\n<li>\u0627\u0644\u0623\u0632\u0647\u0627\u0631: \u062a\u0633\u062a\u062e\u062f\u0645 \u0644\u0644\u0623\u0634\u0643\u0627\u0644 \u0627\u0644\u0647\u064a\u0643\u0644\u064a\u0629.<\/li><\/ul><h3 class=\"wp-block-heading\">\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623<\/h3><ol class=\"wp-block-list\"><li>\u062a\u0634\u0643\u064a\u0644<\/li><\/ol><ul class=\"wp-block-list\"><li>\u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0633\u0627\u062e\u0646\u0629<\/li><\/ul><p class=\"wp-block-paragraph\">\u064a\u062a\u0645 \u0625\u0639\u0627\u062f\u0629 \u062a\u0633\u062e\u064a\u0646 \u0623\u0634\u0643\u0627\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0634\u0628\u0647 \u0627\u0644\u0646\u0647\u0627\u0626\u064a\u0629 \u0625\u0644\u0649 \u062d\u0648\u0627\u0644\u064a 1200 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \u0648\u062a\u0645\u0631\u064a\u0631\u0647\u0627 \u0639\u0628\u0631 \u0628\u0643\u0631\u0627\u062a. \u064a\u062a\u0645 \u062a\u0642\u0644\u064a\u0644 \u0627\u0644\u0633\u064f\u0645\u0643 \u0648\u062a\u0634\u0643\u064a\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0625\u0644\u0649 \u0623\u0644\u0648\u0627\u062d \u0623\u0648 \u0635\u0641\u0627\u0626\u062d \u0623\u0648 \u0644\u0641\u0627\u0626\u0641 \u0623\u0648 \u0642\u0636\u0628\u0627\u0646 \u0623\u0648 \u0623\u0633\u0644\u0627\u0643.<\/p><ul class=\"wp-block-list\"><li>\u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0628\u0627\u0631\u062f\u0629<\/li><\/ul><p class=\"wp-block-paragraph\">\u0642\u0645 \u0628\u062a\u062f\u0648\u064a\u0631 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0641\u064a \u062f\u0631\u062c\u0629 \u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u063a\u0631\u0641\u0629. \u064a\u0645\u0643\u0646 \u062a\u062d\u0642\u064a\u0642 \u0623\u0628\u0639\u0627\u062f \u062f\u0642\u064a\u0642\u0629 \u0648\u062a\u062d\u0633\u064a\u0646 \u062a\u0634\u0637\u064a\u0628 \u0627\u0644\u0633\u0637\u062d. \u064a\u0632\u064a\u062f \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0645\u0646 \u0642\u0648\u062a\u0647 \u0645\u0646 \u062e\u0644\u0627\u0644 \u0627\u0644\u062a\u0635\u0644\u0628 \u0628\u0627\u0644\u0625\u062c\u0647\u0627\u062f.<\/p><ul class=\"wp-block-list\"><li>\u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0633\u0627\u062e\u0646\u0629 \u0645\u0646\u0627\u0633\u0628\u0629 \u0623\u0643\u062b\u0631 \u0644\u0644\u0635\u0644\u0628 \u0627\u0644\u0623\u0648\u0633\u062a\u064a\u0646\u064a\u062a\u064a \u0648\u0627\u0644\u0641\u0631\u064a\u062a\u064a \u0648\u0627\u0644\u0635\u0644\u0628 \u0627\u0644\u0645\u0632\u062f\u0648\u062c. \u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0628\u0627\u0631\u062f\u0629 \u0645\u062b\u0627\u0644\u064a\u0629 \u0644\u0644\u0635\u0644\u0628 \u0627\u0644\u0623\u0648\u0633\u062a\u064a\u0646\u064a\u062a\u064a \u0648\u0627\u0644\u0635\u0644\u0628 \u0627\u0644\u0645\u0627\u0631\u062a\u0646\u0633\u064a\u062a\u064a\u060c \u062e\u0627\u0635\u0629 \u0639\u0646\u062f\u0645\u0627 \u064a\u0643\u0648\u0646 \u0627\u0644\u062a\u0634\u0637\u064a\u0628 \u0627\u0644\u0633\u0637\u062d\u064a \u0648\u0627\u0644\u0623\u0628\u0639\u0627\u062f \u0627\u0644\u062f\u0642\u064a\u0642\u0629 \u0623\u0645\u0631\u064b\u0627 \u0645\u0647\u0645\u064b\u0627.<\/li><\/ul><ol start=\"2\" class=\"wp-block-list\"><li>\u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629<\/li><\/ol><ul class=\"wp-block-list\"><li>\u0627\u0644\u062a\u0644\u062f\u064a\u0646<\/li><\/ul><p class=\"wp-block-paragraph\">\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0637\u0628\u0642: \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0623\u0648\u0633\u062a\u0646\u064a\u062a\u064a \u0648\u0627\u0644\u0641\u0631\u064a\u062a\u064a \u0648\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0645\u0632\u062f\u0648\u062c.<\/p><p class=\"wp-block-paragraph\">\u064a\u062a\u0645 \u062a\u0633\u062e\u064a\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0625\u0644\u0649 \u062f\u0631\u062c\u0629 \u062d\u0631\u0627\u0631\u0629 \u062a\u062a\u0631\u0627\u0648\u062d \u0628\u064a\u0646 1040 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \u06481120 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \u062b\u0645 \u064a\u062a\u0645 \u062a\u0628\u0631\u064a\u062f\u0647 \u0628\u0628\u0637\u0621 \u0644\u062a\u062e\u0641\u064a\u0641 \u0627\u0644\u0636\u063a\u0648\u0637 \u0648\u062a\u062d\u0633\u064a\u0646 \u0642\u0627\u0628\u0644\u064a\u0629 \u0627\u0644\u0634\u062f. \u062a\u0639\u0645\u0644 \u0647\u0630\u0647 \u0627\u0644\u0639\u0645\u0644\u064a\u0629 \u0639\u0644\u0649 \u062a\u0644\u064a\u064a\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0648\u0632\u064a\u0627\u062f\u0629 \u0642\u0627\u0628\u0644\u064a\u062a\u0647 \u0644\u0644\u062a\u0634\u0643\u064a\u0644 \u0648\u0645\u0642\u0627\u0648\u0645\u062a\u0647 \u0644\u0644\u062a\u0622\u0643\u0644.<\/p><ul class=\"wp-block-list\"><li>\u0625\u062e\u0645\u0627\u062f<\/li><\/ul><p class=\"wp-block-paragraph\">\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0637\u0628\u0642: \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0623\u0648\u0633\u062a\u0646\u064a\u062a\u064a \u0648\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0632\u062f\u0648\u062c.<\/p><p class=\"wp-block-paragraph\">\u064a\u062a\u0645 \u062a\u0633\u062e\u064a\u0646\u0647 \u0625\u0644\u0649 \u062f\u0631\u062c\u0627\u062a \u062d\u0631\u0627\u0631\u0629 \u0639\u0627\u0644\u064a\u0629\u060c \u062b\u0645 \u064a\u062a\u0645 \u062a\u0628\u0631\u064a\u062f\u0647 \u0628\u0633\u0631\u0639\u0629 (\u0625\u062e\u0645\u0627\u062f\u0647) \u0644\u0645\u0646\u0639 \u062a\u0643\u0648\u064a\u0646 \u0643\u0631\u0628\u064a\u062f\u0627\u062a \u0627\u0644\u0643\u0631\u0648\u0645. \u064a\u0639\u0645\u0644 \u0627\u0644\u0625\u062e\u0645\u0627\u062f \u0639\u0644\u0649 \u062a\u0639\u0632\u064a\u0632 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644 \u0648\u064a\u0645\u0646\u0639 \u0627\u0644\u062a\u0622\u0643\u0644 \u0628\u064a\u0646 \u0627\u0644\u062d\u0628\u064a\u0628\u0627\u062a.<\/p><ul class=\"wp-block-list\"><li>\u0627\u0644\u062a\u0644\u0637\u064a\u0641<\/li><\/ul><p class=\"wp-block-paragraph\">\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0646\u0627\u0633\u0628: \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0645\u0627\u0631\u062a\u0646\u0633\u064a\u062a\u064a \u0645\u062b\u0644 410 \u0648 420.<\/p><p class=\"wp-block-paragraph\">\u0623\u0639\u062f \u062a\u0633\u062e\u064a\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0625\u0644\u0649 \u062f\u0631\u062c\u0629 \u062d\u0631\u0627\u0631\u0629 \u062a\u062a\u0631\u0627\u0648\u062d \u0628\u064a\u0646 200 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \u0648600 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629. \u064a\u0645\u0643\u0646 \u0623\u0646 \u064a\u0624\u062f\u064a \u0647\u0630\u0627 \u0625\u0644\u0649 \u062a\u0642\u0644\u064a\u0644 \u0627\u0644\u0647\u0634\u0627\u0634\u0629 \u0648\u0627\u0644\u062d\u0641\u0627\u0638 \u0639\u0644\u0649 \u0627\u0644\u0635\u0644\u0627\u0628\u0629. \u062a\u064f\u0633\u062a\u062e\u062f\u0645 \u0647\u0630\u0647 \u0627\u0644\u0639\u0645\u0644\u064a\u0629 \u0644\u0645\u0648\u0627\u0632\u0646\u0629 \u0627\u0644\u0635\u0644\u0627\u0628\u0629 \u0648\u0627\u0644\u0645\u062a\u0627\u0646\u0629.<\/p><ul class=\"wp-block-list\"><li>\u062a\u0635\u0644\u0628 \u0627\u0644\u062a\u0631\u0633\u064a\u0628<\/li><\/ul><p class=\"wp-block-paragraph\">\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0637\u0628\u0642: \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0645\u0642\u0633\u0649 \u0628\u0627\u0644\u062a\u0631\u0633\u064a\u0628 \u0645\u062b\u0644 17-4PH.<\/p><p class=\"wp-block-paragraph\">\u0628\u0639\u062f \u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0645\u062d\u0644\u0648\u0644\u060c \u064a\u062a\u0645 \u062a\u0639\u062a\u064a\u0642 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 (\u064a\u062a\u0645 \u062a\u0633\u062e\u064a\u0646\u0647 \u0625\u0644\u0649 \u062d\u0648\u0627\u0644\u064a 480 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \u0625\u0644\u0649 620 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629). \u062a\u0639\u0645\u0644 \u0647\u0630\u0647 \u0627\u0644\u0639\u0645\u0644\u064a\u0629 \u0639\u0644\u0649 \u062a\u0639\u0632\u064a\u0632 \u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0645\u064a\u0643\u0627\u0646\u064a\u0643\u064a\u0629 \u062f\u0648\u0646 \u0627\u0644\u0645\u0633\u0627\u0633 \u0628\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644.&nbsp;<\/p><ol start=\"3\" class=\"wp-block-list\"><li>\u0625\u0632\u0627\u0644\u0629 \u0627\u0644\u062a\u0631\u0633\u0628\u0627\u062a<\/li><\/ol><p class=\"wp-block-paragraph\">\u0628\u0639\u062f \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629\u060c \u063a\u0627\u0644\u0628\u064b\u0627 \u0645\u0627 \u064a\u064f\u063a\u0637\u0649 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0628\u0637\u0628\u0642\u0629 \u0645\u0646 \u0623\u0643\u0633\u064a\u062f \u0627\u0644\u062d\u062f\u064a\u062f. \u062a\u0639\u0645\u0644 \u0639\u0645\u0644\u064a\u0629 \u0625\u0632\u0627\u0644\u0629 \u0627\u0644\u062a\u0631\u0633\u0628\u0627\u062a \u0639\u0644\u0649 \u0625\u0632\u0627\u0644\u0629 \u0647\u0630\u0647 \u0627\u0644\u0637\u0628\u0642\u0629 \u0628\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u062a\u062e\u0644\u064a\u0644 \u0623\u0648 \u0627\u0644\u0637\u0631\u0642 \u0627\u0644\u0645\u064a\u0643\u0627\u0646\u064a\u0643\u064a\u0629 \u0645\u062b\u0644 \u0627\u0644\u062a\u0646\u0638\u064a\u0641 \u0628\u0627\u0644\u0631\u0645\u0644. \u062a\u0636\u0645\u0646 \u0647\u0630\u0647 \u0627\u0644\u0639\u0645\u0644\u064a\u0629 \u0633\u0637\u062d\u064b\u0627 \u0646\u0638\u064a\u0641\u064b\u0627 \u0644\u0645\u0632\u064a\u062f \u0645\u0646 \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0648\u0627\u0644\u062a\u0634\u0637\u064a\u0628.<\/p><h3 class=\"wp-block-heading\">\u062a\u0634\u0637\u064a\u0628 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623<\/h3><p class=\"wp-block-paragraph\">\u0641\u064a \u0635\u0646\u0627\u0639\u0629 \u0627\u0644\u0635\u0644\u0628\u060c \u062a\u0639\u062a\u0628\u0631 \u0639\u0645\u0644\u064a\u0627\u062a \u0627\u0644\u062a\u0634\u0637\u064a\u0628 \u0628\u0627\u0644\u063a\u0629 \u0627\u0644\u0623\u0647\u0645\u064a\u0629 \u0644\u062a\u062d\u0633\u064a\u0646 \u062c\u0648\u062f\u0629 \u0627\u0644\u0633\u0637\u062d \u0648\u0627\u0644\u0645\u0638\u0647\u0631 \u0648\u0627\u0644\u0623\u062f\u0627\u0621 \u0644\u0644\u0645\u0646\u062a\u062c \u0627\u0644\u0646\u0647\u0627\u0626\u064a. \u0648\u062a\u0636\u0645\u0646 \u0647\u0630\u0647 \u0627\u0644\u0623\u0633\u0627\u0644\u064a\u0628 \u0623\u0646 \u064a\u0641\u064a \u0627\u0644\u0635\u0644\u0628 \u0628\u0645\u0639\u0627\u064a\u064a\u0631 \u0645\u062d\u062f\u062f\u0629 \u0644\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u062a\u064a \u062a\u062a\u0637\u0644\u0628 \u0627\u0644\u062f\u0642\u0629 \u0648\u0627\u0644\u0645\u062a\u0627\u0646\u0629. \u0648\u062a\u0634\u0645\u0644 \u0637\u0631\u0642 \u0627\u0644\u062a\u0634\u0637\u064a\u0628 \u0627\u0644\u0634\u0627\u0626\u0639\u0629 \u0645\u0627 \u064a\u0644\u064a:<\/p><ul class=\"wp-block-list\"><li>\u0627\u0644\u0637\u062d\u0646 \u0648\u0627\u0644\u062a\u0644\u0645\u064a\u0639<\/li><\/ul><p class=\"wp-block-paragraph\">\u062a\u0639\u0645\u0644 \u0639\u0645\u0644\u064a\u0629 \u0627\u0644\u0637\u062d\u0646 \u0639\u0644\u0649 \u0625\u0632\u0627\u0644\u0629 \u0639\u064a\u0648\u0628 \u0627\u0644\u0633\u0637\u062d\u060c \u0645\u062b\u0644 \u0627\u0644\u062e\u062f\u0648\u0634 \u0623\u0648 \u0627\u0644\u062d\u0648\u0627\u0641 \u0627\u0644\u062e\u0634\u0646\u0629\u060c \u0648\u064a\u062a\u0645 \u0630\u0644\u0643 \u063a\u0627\u0644\u0628\u064b\u0627 \u0628\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0623\u062f\u0648\u0627\u062a \u0643\u0627\u0634\u0637\u0629 \u0623\u0648 \u0639\u062c\u0644\u0627\u062a \u0627\u0644\u0637\u062d\u0646.<\/p><p class=\"wp-block-paragraph\">\u064a\u0624\u062f\u064a \u0627\u0644\u062a\u0644\u0645\u064a\u0639 \u0625\u0644\u0649 \u0627\u0644\u062d\u0635\u0648\u0644 \u0639\u0644\u0649 \u0633\u0637\u062d \u0623\u0645\u0644\u0633 \u0648\u0639\u0627\u0643\u0633. \u0648\u064a\u0645\u0643\u0646 \u062a\u0646\u0641\u064a\u0630 \u0647\u0630\u0647 \u0627\u0644\u0639\u0645\u0644\u064a\u0629 \u0628\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u062f\u0631\u062c\u0627\u062a \u0645\u062e\u062a\u0644\u0641\u0629 \u0645\u0646 \u0627\u0644\u0645\u0648\u0627\u062f \u0627\u0644\u0643\u0627\u0634\u0637\u0629 \u0644\u0644\u062d\u0635\u0648\u0644 \u0639\u0644\u0649 \u0645\u0644\u0645\u0633 \u064a\u0634\u0628\u0647 \u0627\u0644\u0645\u0631\u0622\u0629.<\/p><ul class=\"wp-block-list\"><li>\u062a\u0646\u0638\u064a\u0641 \u0627\u0644\u0623\u0633\u0646\u0627\u0646 \u0628\u0627\u0644\u0641\u0631\u0634\u0627\u0629<\/li><\/ul><p class=\"wp-block-paragraph\">\u062a\u062e\u0644\u0642 \u0647\u0630\u0647 \u0627\u0644\u0637\u0631\u064a\u0642\u0629 \u0644\u0645\u0633\u0629 \u0646\u0647\u0627\u0626\u064a\u0629 \u0633\u0627\u062a\u0627\u0646\u064a\u0629 \u0623\u0648 \u063a\u064a\u0631 \u0644\u0627\u0645\u0639\u0629 \u0639\u0644\u0649 \u0633\u0637\u062d \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0628\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0641\u0631\u0634 \u0643\u0627\u0634\u0637\u0629. \u062a\u064f\u0633\u062a\u062e\u062f\u0645 \u0647\u0630\u0647 \u0627\u0644\u0637\u0631\u064a\u0642\u0629 \u0639\u0627\u062f\u0629\u064b \u0641\u064a \u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0645\u062b\u0644 \u0627\u0644\u0623\u062c\u0647\u0632\u0629\u060c \u062d\u064a\u062b \u064a\u064f\u0641\u0636\u0644 \u0627\u0644\u062d\u0635\u0648\u0644 \u0639\u0644\u0649 \u0644\u0645\u0633\u0629 \u0646\u0647\u0627\u0626\u064a\u0629 \u0646\u0627\u0639\u0645\u0629 \u0648\u0644\u0643\u0646 \u063a\u064a\u0631 \u0639\u0627\u0643\u0633\u0629.<\/p><ul class=\"wp-block-list\"><li>\u062a\u062e\u0644\u064a\u0644<\/li><\/ul><p class=\"wp-block-paragraph\">\u0627\u063a\u0645\u0631 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0641\u064a \u062d\u0645\u0627\u0645 \u062d\u0645\u0636\u064a\u060c \u0648\u0647\u0648 \u0639\u0627\u062f\u0629 \u0645\u0632\u064a\u062c \u0645\u0646 \u062d\u0645\u0636 \u0627\u0644\u0646\u064a\u062a\u0631\u064a\u0643 \u0648\u062d\u0645\u0636 \u0627\u0644\u0647\u064a\u062f\u0631\u0648\u0641\u0644\u0648\u0631\u064a\u0643\u060c \u0644\u0625\u0632\u0627\u0644\u0629 \u0637\u0628\u0642\u0629 \u0627\u0644\u0623\u0643\u0633\u064a\u062f \u0627\u0644\u0646\u0627\u062a\u062c\u0629 \u0639\u0646 \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629 \u0623\u0648 \u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0633\u0627\u062e\u0646\u0629. \u062a\u0639\u0645\u0644 \u0647\u0630\u0647 \u0627\u0644\u0639\u0645\u0644\u064a\u0629 \u0639\u0644\u0649 \u0627\u0633\u062a\u0639\u0627\u062f\u0629 \u0633\u0637\u062d \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0648\u062a\u0639\u0632\u064a\u0632 \u0645\u0642\u0627\u0648\u0645\u062a\u0647 \u0644\u0644\u062a\u0622\u0643\u0644.<\/p><ul class=\"wp-block-list\"><li>\u0627\u0644\u062a\u0644\u0645\u064a\u0639 \u0627\u0644\u0643\u0647\u0631\u0628\u0627\u0626\u064a<\/li><\/ul><p class=\"wp-block-paragraph\">\u0627\u0633\u062a\u062e\u062f\u0645 \u062d\u0645\u0627\u0645\u064b\u0627 \u0643\u0647\u0631\u0648\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u064b\u0627 \u0644\u0625\u0632\u0627\u0644\u0629 \u0637\u0628\u0642\u0629 \u0631\u0642\u064a\u0642\u0629 \u0645\u0646 \u0633\u0637\u062d \u0627\u0644\u0645\u0627\u062f\u0629. \u062a\u0639\u0645\u0644 \u0647\u0630\u0647 \u0627\u0644\u0639\u0645\u0644\u064a\u0629 \u0639\u0644\u0649 \u062a\u062d\u0633\u064a\u0646 \u0645\u0638\u0647\u0631 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0648\u062a\u0642\u0644\u064a\u0644 \u0627\u0644\u062e\u0634\u0648\u0646\u0629 \u0627\u0644\u062f\u0642\u064a\u0642\u0629 \u0648\u062a\u062d\u0633\u064a\u0646 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644<\/p><ul class=\"wp-block-list\"><li>\u0627\u0644\u062a\u062e\u0645\u064a\u0644<\/li><\/ul><p class=\"wp-block-paragraph\">\u0627\u0633\u062a\u062e\u062f\u0645 \u0645\u062d\u0644\u0648\u0644\u064b\u0627 \u062d\u0627\u0645\u0636\u064a\u064b\u0627 \u0644\u062a\u0646\u0638\u064a\u0641 \u0633\u0637\u062d \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0639\u0646 \u0637\u0631\u064a\u0642 \u0625\u0632\u0627\u0644\u0629 \u0627\u0644\u062d\u062f\u064a\u062f \u0627\u0644\u062d\u0631 \u0648\u0627\u0644\u0634\u0648\u0627\u0626\u0628. \u062a\u0639\u0645\u0644 \u0647\u0630\u0647 \u0627\u0644\u0639\u0645\u0644\u064a\u0629 \u0639\u0644\u0649 \u062a\u0639\u0632\u064a\u0632 \u062a\u0643\u0648\u064a\u0646 \u0637\u0628\u0642\u0629 \u0623\u0643\u0633\u064a\u062f \u0627\u0644\u0643\u0631\u0648\u0645 \u0627\u0644\u0648\u0627\u0642\u064a\u0629\u060c \u0648\u062a\u062d\u0633\u064a\u0646 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644<\/p><ul class=\"wp-block-list\"><li>\u0637\u0644\u0627\u0621<\/li><\/ul><p class=\"wp-block-paragraph\">\u064a\u0645\u0643\u0646 \u0623\u0646 \u064a\u0639\u0632\u0632 \u0647\u0630\u0627 \u0645\u0646 \u0645\u062a\u0627\u0646\u0629 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0648\u0645\u0642\u0627\u0648\u0645\u062a\u0647 \u0644\u0644\u062a\u0622\u0643\u0644 \u0623\u0648 \u062c\u0627\u0630\u0628\u064a\u062a\u0647 \u0627\u0644\u062c\u0645\u0627\u0644\u064a\u0629. \u0627\u0644\u0637\u0644\u0627\u0621 \u0628\u0627\u0644\u0645\u0633\u062d\u0648\u0642 \u0648\u0627\u0644\u062c\u0644\u0641\u0646\u0629 \u0648\u0627\u0644\u0637\u0644\u0627\u0621 \u0628\u0627\u0644\u0637\u0644\u0627\u0621 \u0647\u064a \u0637\u0631\u0642 \u0634\u0627\u0626\u0639\u0629. \u062a\u0648\u0641\u0631 \u0627\u0644\u0637\u0644\u0627\u0621\u0627\u062a \u0627\u0644\u0645\u062e\u062a\u0644\u0641\u0629 \u0645\u0633\u062a\u0648\u064a\u0627\u062a \u0645\u062e\u062a\u0644\u0641\u0629 \u0645\u0646 \u0627\u0644\u062d\u0645\u0627\u064a\u0629 \u0623\u0648 \u0627\u0644\u062a\u0634\u0637\u064a\u0628 \u0627\u0644\u0632\u062e\u0631\u0641\u064a.<\/p><h3 class=\"wp-block-heading\">\u062a\u0635\u0646\u064a\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623<\/h3><ul start=\"8\" class=\"wp-block-list\"><li>\u0642\u0637\u0639<\/li><\/ul><p class=\"wp-block-paragraph\">\u064a\u062a\u0645 \u0642\u0637\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0625\u0644\u0649 \u0623\u062d\u062c\u0627\u0645 \u0648\u0623\u0634\u0643\u0627\u0644 \u0645\u062d\u062f\u062f\u0629 \u0628\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0637\u0631\u0642 \u0645\u062b\u0644 \u0627\u0644\u0642\u0635 \u0623\u0648 \u0627\u0644\u0646\u0634\u0631 \u0623\u0648 \u062a\u0642\u0646\u064a\u0627\u062a \u0627\u0644\u0642\u0637\u0639 \u0628\u0627\u0644\u0644\u064a\u0632\u0631. \u0627\u0644\u062f\u0642\u0629 \u0641\u064a \u0647\u0630\u0647 \u0627\u0644\u062e\u0637\u0648\u0629 \u0636\u0631\u0648\u0631\u064a\u0629 \u0644\u062a\u0644\u0628\u064a\u0629 \u0645\u0648\u0627\u0635\u0641\u0627\u062a \u0627\u0644\u0645\u0646\u062a\u062c.<\/p><p class=\"wp-block-paragraph\"><strong>\u0642\u0631\u0627\u0621\u0629 \u0630\u0627\u062a \u0635\u0644\u0629<\/strong><\/p><p class=\"wp-block-paragraph\"><a href=\"https:\/\/steelprogroup.com\/ar\/stainless-steel\/production\/cut\/\">\u0643\u064a\u0641\u064a\u0629 \u0642\u0637\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623\u061f<\/a><\/p><ul class=\"wp-block-list\"><li>\u0627\u0644\u0644\u062d\u0627\u0645<\/li><\/ul><p class=\"wp-block-paragraph\">\u062a\u0636\u0645\u0646 \u062a\u0642\u0646\u064a\u0627\u062a \u0645\u062b\u0644 TIG \u0623\u0648 MIG \u0623\u0648 \u0627\u0644\u0644\u062d\u0627\u0645 \u0628\u0627\u0644\u0645\u0642\u0627\u0648\u0645\u0629 \u0645\u0641\u0627\u0635\u0644 \u0642\u0648\u064a\u0629 \u0648\u0645\u0642\u0627\u0648\u0645\u0629 \u0644\u0644\u062a\u0622\u0643\u0644.<\/p><h3 class=\"wp-block-heading\">\u0636\u0628\u0637 \u0627\u0644\u062c\u0648\u062f\u0629<\/h3><p class=\"wp-block-paragraph\">\u0645\u0646 \u062e\u0644\u0627\u0644 \u0627\u062e\u062a\u0628\u0627\u0631\u0627\u062a \u0645\u062e\u062a\u0644\u0641\u0629\u060c \u064a\u062a\u062d\u0642\u0642 \u0627\u0644\u0645\u0635\u0646\u0639\u0648\u0646 \u0645\u0646 \u062a\u0631\u0643\u064a\u0628\u0629 \u0627\u0644\u0645\u0627\u062f\u0629 \u0648\u0642\u0648\u062a\u0647\u0627 \u0648\u0633\u0644\u0627\u0645\u062a\u0647\u0627. \u0641\u064a \u0625\u0646\u062a\u0627\u062c \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623\u060c \u062a\u062a\u0636\u0645\u0646 \u0645\u0631\u062d\u0644\u0629 \u0645\u0631\u0627\u0642\u0628\u0629 \u0627\u0644\u062c\u0648\u062f\u0629 \u0639\u0627\u062f\u0629\u064b \u0627\u0644\u062e\u0637\u0648\u0627\u062a \u0627\u0644\u062a\u0627\u0644\u064a\u0629:<\/p><ul class=\"wp-block-list\"><li>\u0627\u0644\u062a\u062d\u0644\u064a\u0644 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a<\/li><\/ul><p class=\"wp-block-paragraph\">\u0648\u064a\u0636\u0645\u0646 \u0647\u0630\u0627 \u0623\u0646 \u0627\u0644\u062a\u0631\u0643\u064a\u0628 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a \u0644\u0644\u0645\u0627\u062f\u0629 \u064a\u0637\u0627\u0628\u0642 \u0627\u0644\u0645\u0648\u0627\u0635\u0641\u0627\u062a\u060c \u0648\u064a\u0624\u0643\u062f \u0648\u062c\u0648\u062f \u0627\u0644\u0645\u0632\u064a\u062c \u0627\u0644\u0635\u062d\u064a\u062d \u0645\u0646 \u0627\u0644\u0639\u0646\u0627\u0635\u0631 \u0645\u062b\u0644 \u0627\u0644\u0643\u0631\u0648\u0645 \u0648\u0627\u0644\u0646\u064a\u0643\u0644.<\/p><ul class=\"wp-block-list\"><li>\u0627\u0644\u0627\u062e\u062a\u0628\u0627\u0631\u0627\u062a \u0627\u0644\u0645\u064a\u0643\u0627\u0646\u064a\u0643\u064a\u0629<\/li><\/ul><p class=\"wp-block-paragraph\">\u064a\u062a\u0645 \u0625\u062c\u0631\u0627\u0621 \u0627\u0644\u0627\u062e\u062a\u0628\u0627\u0631\u0627\u062a \u0644\u0644\u062a\u062d\u0642\u0642 \u0645\u0646 \u0642\u0648\u0629 \u0627\u0644\u0634\u062f \u0648\u0627\u0644\u0635\u0644\u0627\u0628\u0629 \u0648\u0627\u0644\u0645\u0631\u0648\u0646\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623\u060c \u0644\u0636\u0645\u0627\u0646 \u0623\u0646\u0647 \u064a\u0644\u0628\u064a \u0645\u0639\u0627\u064a\u064a\u0631 \u0627\u0644\u0623\u062f\u0627\u0621 \u0627\u0644\u0645\u064a\u0643\u0627\u0646\u064a\u0643\u064a.<\/p><ul class=\"wp-block-list\"><li>\u0627\u0644\u0627\u062e\u062a\u0628\u0627\u0631\u0627\u062a \u063a\u064a\u0631 \u0627\u0644\u0645\u062f\u0645\u0631\u0629 (NDT)<\/li><\/ul><p class=\"wp-block-paragraph\">\u062a\u0643\u062a\u0634\u0641 \u0627\u0644\u0637\u0631\u0642 \u0628\u0627\u0644\u0645\u0648\u062c\u0627\u062a \u0641\u0648\u0642 \u0627\u0644\u0635\u0648\u062a\u064a\u0629 \u0648\u0627\u0644\u062a\u0635\u0648\u064a\u0631 \u0627\u0644\u0625\u0634\u0639\u0627\u0639\u064a \u0627\u0644\u0639\u064a\u0648\u0628 \u0627\u0644\u062f\u0627\u062e\u0644\u064a\u0629 \u062f\u0648\u0646 \u0627\u0644\u0625\u0636\u0631\u0627\u0631 \u0628\u0627\u0644\u0645\u0627\u062f\u0629.<\/p><h2 class=\"wp-block-heading\">\u0645\u0646\u062a\u062c\u0627\u062a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623<\/h2><h3 class=\"wp-block-heading\">\u0623\u0648\u0631\u0627\u0642<\/h3><ul class=\"wp-block-list\"><li>\u062a\u064f\u0639\u062f \u0635\u0641\u0627\u0626\u062d \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0642\u0637\u0639\u064b\u0627 \u0631\u0642\u064a\u0642\u0629 \u0648\u0645\u0633\u0637\u062d\u0629 \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630\u060c \u062a\u064f\u0633\u062a\u062e\u062f\u0645 \u0639\u0627\u062f\u0629\u064b \u0641\u064a \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u062a\u064a \u062a\u062a\u0637\u0644\u0628 \u062f\u0631\u062c\u0629 \u0639\u0627\u0644\u064a\u0629 \u0645\u0646 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644 \u0648\u0633\u0637\u062d\u064b\u0627 \u0623\u0645\u0644\u0633\u064b\u0627 \u0648\u0645\u062a\u0633\u0627\u0648\u064a\u064b\u0627.<\/li>\n\n<li>\u062a\u0628\u0644\u063a \u0633\u0645\u0627\u0643\u0629 \u0647\u0630\u0647 \u0627\u0644\u0623\u0644\u0648\u0627\u062d \u0639\u0627\u062f\u0629 \u0623\u0642\u0644 \u0645\u0646 6 \u0645\u0645\u060c \u0648\u064a\u0645\u0643\u0646 \u062f\u062d\u0631\u062c\u062a\u0647\u0627 \u0625\u0645\u0627 \u0639\u0644\u0649 \u0627\u0644\u0633\u0627\u062e\u0646 \u0623\u0648 \u0639\u0644\u0649 \u0627\u0644\u0628\u0627\u0631\u062f\u060c \u062d\u064a\u062b \u062a\u0648\u0641\u0631 \u0627\u0644\u062f\u062d\u0631\u062c\u0629 \u0627\u0644\u0628\u0627\u0631\u062f\u0629 \u062c\u0648\u062f\u0629 \u0633\u0637\u062d \u0648\u0642\u0648\u0629 \u0623\u0641\u0636\u0644.<\/li><\/ul><h3 class=\"wp-block-heading\">\u0623\u0637\u0628\u0627\u0642<\/h3><ul class=\"wp-block-list\"><li>\u062a\u0639\u062a\u0628\u0631 \u0627\u0644\u0623\u0644\u0648\u0627\u062d \u0623\u0643\u062b\u0631 \u0633\u0645\u0643\u064b\u0627 \u0645\u0646 \u0627\u0644\u0635\u0641\u0627\u0626\u062d\u060c \u0648\u0647\u064a \u0645\u0635\u0645\u0645\u0629 \u0644\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0635\u0646\u0627\u0639\u064a\u0629 \u0627\u0644\u0623\u0643\u062b\u0631 \u0635\u0639\u0648\u0628\u0629.<\/li>\n\n<li>\u062a\u0643\u0648\u0646 \u0627\u0644\u0623\u0644\u0648\u0627\u062d \u0641\u064a \u0623\u063a\u0644\u0628 \u0627\u0644\u0623\u062d\u064a\u0627\u0646 \u0623\u0643\u062b\u0631 \u0633\u0645\u0643\u064b\u0627 \u0645\u0646 6 \u0645\u0645 \u0648\u062a\u0648\u0641\u0631 \u0642\u0648\u0629 \u0641\u0627\u0626\u0642\u0629 \u0644\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u062d\u0627\u0645\u0644\u0629 \u0644\u0644\u0623\u062d\u0645\u0627\u0644.<\/li><\/ul><h3 class=\"wp-block-heading\">\u0627\u0644\u0645\u0644\u0641\u0627\u062a<\/h3><ul class=\"wp-block-list\"><li>\u0645\u0644\u0641\u0627\u062a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0647\u064a \u0639\u0628\u0627\u0631\u0629 \u0639\u0646 \u0634\u0631\u0627\u0626\u062d \u0637\u0648\u064a\u0644\u0629 \u0645\u062a\u0648\u0627\u0635\u0644\u0629 \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0645\u0644\u0641\u0648\u0641\u0629 \u0639\u0644\u0649 \u0634\u0643\u0644 \u0644\u0641\u0627\u0626\u0641 \u0644\u0633\u0647\u0648\u0644\u0629 \u0627\u0644\u0646\u0642\u0644 \u0648\u0627\u0644\u062a\u062e\u0632\u064a\u0646.<\/li>\n\n<li>\u064a\u0645\u0643\u0646 \u0623\u0646 \u062a\u0643\u0648\u0646 \u0627\u0644\u0645\u0644\u0641\u0627\u062a \u0645\u062f\u0644\u0641\u0646\u0629 \u0639\u0644\u0649 \u0627\u0644\u0633\u0627\u062e\u0646 \u0623\u0648 \u0627\u0644\u0628\u0627\u0631\u062f\u060c \u0648\u062a\u0623\u062a\u064a \u0628\u0623\u062d\u062c\u0627\u0645 \u0648\u0633\u0645\u0643 \u0645\u062e\u062a\u0644\u0641\u0629.<\/li><\/ul><h3 class=\"wp-block-heading\">\u0627\u0644\u062d\u0627\u0646\u0627\u062a<\/h3><ul class=\"wp-block-list\"><li>\u062a\u0623\u062a\u064a \u0627\u0644\u0642\u0636\u0628\u0627\u0646 \u0628\u0623\u0634\u0643\u0627\u0644 \u0645\u062e\u062a\u0644\u0641\u0629\u060c \u0645\u062b\u0644 \u0627\u0644\u062f\u0627\u0626\u0631\u064a\u0629\u060c \u0648\u0627\u0644\u0645\u0631\u0628\u0639\u0629\u060c \u0648\u0627\u0644\u0633\u062f\u0627\u0633\u064a\u0629.&nbsp;<\/li>\n\n<li>\u064a\u062a\u0645 \u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0647\u0627 \u0641\u064a \u0645\u062c\u0645\u0648\u0639\u0629 \u0648\u0627\u0633\u0639\u0629 \u0645\u0646 \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0625\u0646\u0634\u0627\u0626\u064a\u0629 \u0648\u0627\u0644\u0635\u0646\u0627\u0639\u064a\u0629.<\/li>\n\n<li>\u062a\u0648\u0641\u0631 \u0627\u0644\u0642\u0636\u0628\u0627\u0646 \u062a\u0646\u0648\u0639\u064b\u0627 \u0641\u064a \u0627\u0644\u0634\u0643\u0644 \u0648\u063a\u0627\u0644\u0628\u064b\u0627 \u0645\u0627 \u064a\u062a\u0645 \u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0647\u0627 \u0639\u0646\u062f\u0645\u0627 \u062a\u0643\u0648\u0646 \u0647\u0646\u0627\u0643 \u062d\u0627\u062c\u0629 \u0625\u0644\u0649 \u062e\u0635\u0627\u0626\u0635 \u0623\u0648 \u0623\u0634\u0643\u0627\u0644 \u0645\u064a\u0643\u0627\u0646\u064a\u0643\u064a\u0629 \u0645\u062d\u062f\u062f\u0629.<\/li><\/ul><h3 class=\"wp-block-heading\">\u0627\u0644\u0623\u0633\u0644\u0627\u0643<\/h3><ul class=\"wp-block-list\"><li>\u0627\u0644\u0623\u0633\u0644\u0627\u0643 \u0627\u0644\u0645\u0635\u0646\u0648\u0639\u0629 \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0639\u0628\u0627\u0631\u0629 \u0639\u0646 \u062e\u064a\u0648\u0637 \u0637\u0648\u064a\u0644\u0629 \u0648\u0631\u0641\u064a\u0639\u0629 \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630. \u062a\u064f\u0633\u062a\u062e\u062f\u0645 \u0639\u0627\u062f\u0629\u064b \u0641\u064a \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u062a\u064a \u062a\u062a\u0637\u0644\u0628 \u0627\u0644\u0645\u0631\u0648\u0646\u0629 \u0648\u0642\u0648\u0629 \u0627\u0644\u0634\u062f.<\/li>\n\n<li>\u064a\u0639\u0645\u0644 \u0639\u0644\u0649 \u062a\u0642\u0648\u064a\u0629 \u0627\u0644\u0645\u0627\u062f\u0629 \u0648\u062a\u062d\u0633\u064a\u0646 \u062a\u0634\u0637\u064a\u0628 \u0633\u0637\u062d\u0647\u0627.<\/li><\/ul><h3 class=\"wp-block-heading\">\u0627\u0644\u0623\u0646\u0627\u0628\u064a\u0628<\/h3><ul class=\"wp-block-list\"><li>\u0623\u0646\u0627\u0628\u064a\u0628 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0647\u064a \u0623\u0646\u0627\u0628\u064a\u0628 \u0645\u062c\u0648\u0641\u0629 \u062a\u0633\u062a\u062e\u062f\u0645 \u0644\u0646\u0642\u0644 \u0627\u0644\u0633\u0648\u0627\u0626\u0644 \u0623\u0648 \u0627\u0644\u063a\u0627\u0632\u0627\u062a \u0623\u0648 \u0627\u0644\u0645\u0648\u0627\u062f \u0627\u0644\u0623\u062e\u0631\u0649.<\/li>\n\n<li>\u062a\u062a\u0648\u0641\u0631 \u0627\u0644\u0623\u0646\u0627\u0628\u064a\u0628 \u0628\u0623\u062d\u062c\u0627\u0645 \u0645\u062e\u062a\u0644\u0641\u0629\u060c \u0648\u064a\u062a\u0645 \u062a\u0635\u0646\u064a\u0639\u0647\u0627 \u0639\u0627\u062f\u0629\u064b \u0639\u0646 \u0637\u0631\u064a\u0642 \u0627\u0644\u0644\u062d\u0627\u0645 \u0623\u0648 \u0627\u0644\u0644\u062d\u0627\u0645\u0627\u062a \u0627\u0639\u062a\u0645\u0627\u062f\u064b\u0627 \u0639\u0644\u0649 \u0627\u0644\u062a\u0637\u0628\u064a\u0642.<\/li><\/ul><h3 class=\"wp-block-heading\">\u0623\u0646\u0627\u0628\u064a\u0628<\/h3><ul class=\"wp-block-list\"><li>\u0645\u0634\u0627\u0628\u0647\u0629 \u0644\u0644\u0623\u0646\u0627\u0628\u064a\u0628 \u0648\u0644\u0643\u0646\u0647\u0627 \u063a\u0627\u0644\u0628\u064b\u0627 \u0645\u0627 \u062a\u0643\u0648\u0646 \u0623\u0631\u0642 \u0648\u062a\u0633\u062a\u062e\u062f\u0645 \u0641\u064a \u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0623\u0643\u062b\u0631 \u062f\u0642\u0629 \u0623\u0648 \u0639\u0644\u0649 \u0646\u0637\u0627\u0642 \u0623\u0635\u063a\u0631.<\/li>\n\n<li>\u063a\u0627\u0644\u0628\u064b\u0627 \u0645\u0627 \u062a\u0643\u0648\u0646 \u0627\u0644\u0623\u0646\u0627\u0628\u064a\u0628 \u063a\u064a\u0631 \u0645\u0644\u062d\u0648\u0645\u0629 \u0623\u0648 \u0645\u0644\u062d\u0648\u0645\u0629. \u0648\u0644\u0647\u0627 \u0623\u0634\u0643\u0627\u0644 \u0645\u062e\u062a\u0644\u0641\u0629\u060c \u0645\u062b\u0644 \u0627\u0644\u062f\u0627\u0626\u0631\u064a\u0629 \u0623\u0648 \u0627\u0644\u0645\u0631\u0628\u0639\u0629 \u0623\u0648 \u0627\u0644\u0645\u0633\u062a\u0637\u064a\u0644\u0629.<\/li><\/ul><h3 class=\"wp-block-heading\">\u0631\u0642\u0627\u0626\u0642 \u0645\u0639\u062f\u0646\u064a\u0629<\/h3><ul class=\"wp-block-list\"><li>\u0635\u0641\u0627\u0626\u062d \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0631\u0642\u064a\u0642\u0629 \u0644\u0644\u063a\u0627\u064a\u0629. \u062a\u064f\u0633\u062a\u062e\u062f\u0645 \u0639\u0627\u062f\u0629\u064b \u0641\u064a \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0645\u062a\u062e\u0635\u0635\u0629.<\/li>\n\n<li>\u062a\u064f\u0633\u062a\u062e\u062f\u0645 \u0627\u0644\u0631\u0642\u0627\u0626\u0642\u060c \u0627\u0644\u062a\u064a \u064a\u0628\u0644\u063a \u0633\u0645\u0643\u0647\u0627 \u0639\u0627\u062f\u0629 \u0623\u0642\u0644 \u0645\u0646 0.15 \u0645\u0645\u060c \u0641\u064a \u0628\u064a\u0626\u0627\u062a \u062f\u0642\u064a\u0642\u0629 \u0648\u0639\u0627\u0644\u064a\u0629 \u0627\u0644\u0623\u062f\u0627\u0621.<\/li><\/ul><h3 class=\"wp-block-heading\">\u0627\u0644\u0623\u0642\u0633\u0627\u0645 \u0627\u0644\u0647\u064a\u0643\u0644\u064a\u0629<\/h3><ul class=\"wp-block-list\"><li>\u062a\u0634\u0645\u0644 \u0627\u0644\u0645\u0642\u0627\u0637\u0639 \u0627\u0644\u0647\u064a\u0643\u0644\u064a\u0629 \u0627\u0644\u0645\u0635\u0646\u0648\u0639\u0629 \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0639\u0648\u0627\u0631\u0636 \u0648\u0627\u0644\u0632\u0648\u0627\u064a\u0627 \u0648\u0627\u0644\u0642\u0646\u0648\u0627\u062a. \u062a\u064f\u0633\u062a\u062e\u062f\u0645 \u0641\u064a \u0645\u0634\u0627\u0631\u064a\u0639 \u0627\u0644\u0628\u0646\u0627\u0621 \u0648\u0627\u0644\u0628\u0646\u064a\u0629 \u0627\u0644\u062a\u062d\u062a\u064a\u0629.<\/li>\n\n<li>\u062a\u062a\u0645\u062a\u0639 \u0647\u0630\u0647 \u0627\u0644\u0623\u0642\u0633\u0627\u0645 \u0628\u0642\u0648\u0629 \u062a\u062d\u0645\u0644 \u0627\u0644\u0623\u062d\u0645\u0627\u0644 \u0648\u064a\u062a\u0645 \u062a\u0635\u0646\u064a\u0639\u0647\u0627 \u0645\u0646 \u062e\u0644\u0627\u0644 \u0639\u0645\u0644\u064a\u0627\u062a \u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0633\u0627\u062e\u0646\u0629.<\/li><\/ul><h2 class=\"wp-block-heading\">\u0643\u0645 \u0645\u0646 \u0627\u0644\u0648\u0642\u062a \u064a\u0633\u062a\u063a\u0631\u0642 \u062a\u0635\u0646\u064a\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623\u061f<\/h2><p class=\"wp-block-paragraph\">\u064a\u0633\u062a\u063a\u0631\u0642 \u0625\u0646\u062a\u0627\u062c \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0641\u064a \u0641\u0631\u0646 \u0627\u0644\u0642\u0648\u0633 \u0627\u0644\u0643\u0647\u0631\u0628\u0627\u0626\u064a \u0639\u0627\u062f\u0629 \u0645\u0646 8 \u0625\u0644\u0649 12 \u0633\u0627\u0639\u0629. \u0648\u064a\u0634\u0645\u0644 \u0647\u0630\u0627 \u0627\u0644\u0648\u0642\u062a \u0635\u0647\u0631 \u0627\u0644\u0645\u0648\u0627\u062f \u0627\u0644\u062e\u0627\u0645 \u0648\u062e\u0637\u0648\u0627\u062a \u0625\u0636\u0627\u0641\u064a\u0629 \u0645\u062b\u0644 \u0625\u0632\u0627\u0644\u0629 \u0627\u0644\u0643\u0631\u0628\u0648\u0646 \u0648\u0627\u0644\u0635\u0628 \u0648\u0627\u0644\u062a\u0634\u0643\u064a\u0644. \u0648\u0645\u0639 \u0630\u0644\u0643\u060c \u0641\u0625\u0646 \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0625\u0636\u0627\u0641\u064a\u0629 \u0645\u062b\u0644 \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629 \u0648\u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0648\u0627\u0644\u062a\u0634\u0637\u064a\u0628 \u064a\u0645\u0643\u0646 \u0623\u0646 \u062a\u0632\u064a\u062f \u0645\u0646 \u0648\u0642\u062a \u0627\u0644\u0625\u0646\u062a\u0627\u062c \u0627\u0644\u0625\u062c\u0645\u0627\u0644\u064a.<\/p><h2 class=\"wp-block-heading\">\u0645\u0627 \u0627\u0644\u0630\u064a \u064a\u062c\u0639\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0628\u0627\u0647\u0638 \u0627\u0644\u062b\u0645\u0646\u061f<\/h2><p class=\"wp-block-paragraph\">\u064a\u0639\u062f \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0628\u0627\u0647\u0638 \u0627\u0644\u062b\u0645\u0646 \u0644\u0623\u0646\u0647 \u064a\u062d\u062a\u0648\u064a \u0639\u0644\u0649 \u0639\u0646\u0627\u0635\u0631 \u0633\u0628\u0627\u0626\u0643\u064a\u0629 \u0639\u0627\u0644\u064a\u0629 \u0627\u0644\u062a\u0643\u0644\u0641\u0629 \u0645\u062b\u0644 \u0627\u0644\u0643\u0631\u0648\u0645 \u0648\u0627\u0644\u0646\u064a\u0643\u0644 \u0648\u0623\u062d\u064a\u0627\u0646\u064b\u0627 \u0627\u0644\u0645\u0648\u0644\u064a\u0628\u062f\u064a\u0646\u0648\u0645. \u0628\u0627\u0644\u0625\u0636\u0627\u0641\u0629 \u0625\u0644\u0649 \u0630\u0644\u0643\u060c \u0641\u0625\u0646 \u0639\u0645\u0644\u064a\u0629 \u0627\u0644\u0625\u0646\u062a\u0627\u062c \u0627\u0644\u062a\u064a \u062a\u0633\u062a\u0647\u0644\u0643 \u0627\u0644\u0643\u062b\u064a\u0631 \u0645\u0646 \u0627\u0644\u0637\u0627\u0642\u0629\u060c \u0645\u062b\u0644 \u0627\u0644\u0635\u0647\u0631 \u0648\u0627\u0644\u062a\u0643\u0631\u064a\u0631\u060c \u062a\u0632\u064a\u062f \u0645\u0646 \u0627\u0644\u062a\u0643\u0644\u0641\u0629. \u0643\u0645\u0627 \u0623\u0646 \u0627\u0644\u062d\u0627\u062c\u0629 \u0625\u0644\u0649 \u0645\u0631\u0627\u0642\u0628\u0629 \u0627\u0644\u062c\u0648\u062f\u0629 \u0627\u0644\u0635\u0627\u0631\u0645\u0629 \u0648\u0639\u0645\u0644\u064a\u0627\u062a \u0627\u0644\u062a\u0634\u0637\u064a\u0628 \u0645\u062b\u0644 \u0627\u0644\u062a\u0644\u0645\u064a\u0639 \u0623\u0648 \u0627\u0644\u062a\u0644\u062f\u064a\u0646 \u062a\u0632\u064a\u062f \u0645\u0646 \u0627\u0644\u0633\u0639\u0631.<\/p><h2 class=\"wp-block-heading\">\u0645\u0646 \u0623\u064a\u0646 \u064a\u0623\u062a\u064a \u0645\u0639\u0638\u0645 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623\u061f<\/h2><p class=\"wp-block-paragraph\">\u0648\u0645\u0646 \u0628\u064a\u0646 \u0643\u0628\u0627\u0631 \u0627\u0644\u0645\u0646\u062a\u062c\u064a\u0646 \u0627\u0644\u0635\u064a\u0646\u060c \u0627\u0644\u062a\u064a \u062a\u0645\u062b\u0644 \u0623\u0643\u062b\u0631 \u0645\u0646 \u0646\u0635\u0641 \u0625\u0646\u062a\u0627\u062c \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0641\u064a \u0627\u0644\u0639\u0627\u0644\u0645. \u0648\u0645\u0646 \u0628\u064a\u0646 \u0643\u0628\u0627\u0631 \u0627\u0644\u0645\u0646\u062a\u062c\u064a\u0646 \u0627\u0644\u0622\u062e\u0631\u064a\u0646 \u0627\u0644\u0647\u0646\u062f \u0648\u0627\u0644\u064a\u0627\u0628\u0627\u0646 \u0648\u0643\u0648\u0631\u064a\u0627 \u0627\u0644\u062c\u0646\u0648\u0628\u064a\u0629 \u0648\u0628\u0639\u0636 \u0627\u0644\u062f\u0648\u0644 \u0627\u0644\u0623\u0648\u0631\u0648\u0628\u064a\u0629 \u0645\u062b\u0644 \u0623\u0644\u0645\u0627\u0646\u064a\u0627.<\/p><h2 class=\"wp-block-heading\">\u0645\u0644\u062e\u0635<\/h2><p class=\"wp-block-paragraph\">\u064a\u0639\u062f \u0636\u0645\u0627\u0646 \u0645\u0631\u0627\u0642\u0628\u0629 \u0627\u0644\u062c\u0648\u062f\u0629 \u0641\u064a \u0625\u0646\u062a\u0627\u062c \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0623\u0645\u0631\u064b\u0627 \u0636\u0631\u0648\u0631\u064a\u064b\u0627 \u0644\u0636\u0645\u0627\u0646 \u0627\u0633\u062a\u064a\u0641\u0627\u0621 \u0627\u0644\u0645\u0627\u062f\u0629 \u0644\u0644\u0645\u0639\u0627\u064a\u064a\u0631 \u0627\u0644\u0645\u0637\u0644\u0648\u0628\u0629. \u064a\u0633\u0627\u0639\u062f \u0630\u0644\u0643 \u0641\u064a \u0627\u0644\u062d\u0641\u0627\u0638 \u0639\u0644\u0649 \u0642\u0648\u0629 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0648\u0645\u0642\u0627\u0648\u0645\u062a\u0647 \u0644\u0644\u062a\u0622\u0643\u0644 \u0648\u0645\u062a\u0627\u0646\u062a\u0647.&nbsp;<\/p><p class=\"wp-block-paragraph\">\u0641\u064a Steel Pro Group\u060c \u0646\u0641\u062e\u0631 \u0628\u062a\u0642\u062f\u064a\u0645 \u0645\u062c\u0645\u0648\u0639\u0629 \u0648\u0627\u0633\u0639\u0629 \u0645\u0646 \u0645\u0646\u062a\u062c\u0627\u062a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0639\u0627\u0644\u064a\u0629 \u0627\u0644\u062c\u0648\u062f\u0629\u060c \u0628\u0645\u0627 \u0641\u064a \u0630\u0644\u0643 \u0627\u0644\u0623\u0644\u0648\u0627\u062d \u0648\u0627\u0644\u0642\u0636\u0628\u0627\u0646 \u0648\u0627\u0644\u0645\u0644\u0641\u0627\u062a \u0648\u0627\u0644\u062d\u0644\u0648\u0644 \u0627\u0644\u0645\u062e\u0635\u0635\u0629 \u0627\u0644\u0645\u0635\u0645\u0645\u0629 \u062e\u0635\u064a\u0635\u064b\u0627 \u0644\u062a\u0644\u0628\u064a\u0629 \u0627\u062d\u062a\u064a\u0627\u062c\u0627\u062a\u0643. \u064a\u0633\u0639\u062f\u0646\u0627 \u0645\u0633\u0627\u0639\u062f\u062a\u0643 - \u0641\u0644\u0627 \u062a\u062a\u0631\u062f\u062f \u0641\u064a \u0627\u0644\u0627\u062a\u0635\u0627\u0644 \u0628\u0646\u0627. <a href=\"https:\/\/steelprogroup.com\/ar\">\u0642\u0645 \u0628\u0632\u064a\u0627\u0631\u0629 \u0645\u0648\u0642\u0639\u0646\u0627<\/a> \u0623\u0648 <a href=\"https:\/\/steelprogroup.com\/ar\/contact-us\/\">\u062a\u0648\u0627\u0635\u0644 \u0645\u0639\u0646\u0627<\/a> \u0644\u0645\u0632\u064a\u062f \u0645\u0646 \u0627\u0644\u062a\u0641\u0627\u0635\u064a\u0644 \u0623\u0648 \u0644\u0644\u062d\u0635\u0648\u0644 \u0639\u0644\u0649 \u0639\u0631\u0636 \u0623\u0633\u0639\u0627\u0631 \u0634\u062e\u0635\u064a.<\/p>","protected":false},"excerpt":{"rendered":"<p>\u064a\u0648\u0641\u0631 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0645\u0642\u0627\u0648\u0645\u0629 \u0639\u0627\u0644\u064a\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0648\u0645\u062a\u0627\u0646\u0629 \u0637\u0648\u064a\u0644\u0629 \u0627\u0644\u0623\u0645\u062f \u0648\u0627\u062d\u062a\u064a\u0627\u062c\u0627\u062a \u0635\u064a\u0627\u0646\u0629 \u0628\u0633\u064a\u0637\u0629 \u0641\u064a \u0638\u0631\u0648\u0641 \u0645\u062a\u0646\u0648\u0639\u0629. \u0625\u0646 \u0641\u0647\u0645 \u0643\u064a\u0641\u064a\u0629 \u062a\u0635\u0646\u064a\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 [\u2026]<\/p>","protected":false},"author":1,"featured_media":10933,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"_eb_attr":"","rank_math_lock_modified_date":false,"site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"categories":[112],"tags":[],"class_list":["post-10946","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-stainless-steel"],"acf":[],"_links":{"self":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts\/10946","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/comments?post=10946"}],"version-history":[{"count":0,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts\/10946\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/media\/10933"}],"wp:attachment":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/media?parent=10946"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/categories?post=10946"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/tags?post=10946"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}