{"id":11577,"date":"2024-10-09T23:33:00","date_gmt":"2024-10-09T15:33:00","guid":{"rendered":"https:\/\/app11147.cloudwayssites.com\/?p=11577"},"modified":"2024-10-11T09:22:46","modified_gmt":"2024-10-11T01:22:46","slug":"grade-201","status":"publish","type":"post","link":"https:\/\/steelprogroup.com\/ar\/stainless-steel\/grades\/grade-201\/","title":{"rendered":"\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201: \u0627\u0644\u062a\u0639\u0631\u064a\u0641 \u0648\u0627\u0644\u062a\u0631\u0643\u064a\u0628 \u0648\u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0648\u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0648\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0648\u0627\u0644\u0645\u0632\u064a\u062f"},"content":{"rendered":"<p class=\"wp-block-paragraph\"><strong><em>\u062a\u0642\u062f\u0645 \u0645\u062c\u0645\u0648\u0639\u0629 SteelPRO \u0645\u0646\u062a\u062c\u0627\u062a SS 201 (UNS S20100\/EN 1.4372) \u0627\u0644\u0645\u062e\u0632\u0646\u0629 \u0645\u0628\u0627\u0634\u0631\u0629 \u0645\u0646 \u0627\u0644\u0645\u0635\u0646\u0639: \u0644\u0648\u062d\u0629\u060c \u0635\u0641\u0627\u0626\u062d\u060c \u0644\u0641\u0627\u0626\u0641\u060c \u0634\u0631\u0627\u0626\u0637\u060c \u0631\u0642\u0627\u0626\u0642 \u0645\u0639\u062f\u0646\u064a\u0629\u060c \u0623\u0646\u0627\u0628\u064a\u0628\u060c \u0642\u0636\u0628\u0627\u0646\u060c \u0623\u0633\u0644\u0627\u0643\u060c \u0625\u0644\u062e. \u064a\u062a\u0645 \u0636\u0645\u0627\u0646 \u062c\u0648\u062f\u0629 \u0645\u0646\u062a\u062c 100% \u0628\u062e\u0635\u0645 \u062a\u0646\u0627\u0641\u0633\u064a \u0642\u0627\u0628\u0644 \u0644\u0644\u062a\u0641\u0627\u0648\u0636. <a href=\"https:\/\/steelprogroup.com\/ar\/contact-us\/\" target=\"_blank\" data-type=\"page\" data-id=\"177\" rel=\"noreferrer noopener\">\u0627\u062a\u0635\u0644 \u0628\u0646\u0627<\/a> \u0644\u062a\u062e\u0635\u064a\u0635 \u0645\u0646\u062a\u062c\u0627\u062a\u0643 \u0645\u0646 \u062d\u064a\u062b \u0627\u0644\u0634\u0643\u0644 \u0648\u0627\u0644\u062d\u0627\u0644\u0629 \u0648\u0627\u0644\u0644\u0645\u0633\u0629 \u0627\u0644\u0646\u0647\u0627\u0626\u064a\u0629 \u0648\u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0648\u0627\u0644\u0645\u0632\u064a\u062f.<\/em><\/strong><\/p><h2 class=\"wp-block-heading\">\u0646\u0638\u0631\u0629 \u0639\u0627\u0645\u0629 \u0639\u0644\u0649 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201<\/h2><p class=\"wp-block-paragraph\">\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201 \u0647\u0648 \u0633\u0644\u0633\u0644\u0629 200 \u0645\u0646 \u0627\u0644\u0643\u0631\u0648\u0645 \u0648\u0627\u0644\u0646\u064a\u0643\u0644 \u0648\u0627\u0644\u0645\u0646\u062c\u0646\u064a\u0632 <a href=\"https:\/\/steelprogroup.com\/ar\/stainless-steel\/type\/austenitic\/\" target=\"_blank\" rel=\"noreferrer noopener\">\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0623\u0648\u0633\u062a\u0646\u064a\u062a\u064a<\/a>\u064a\u062a\u0643\u0648\u0646 \u0628\u0634\u0643\u0644 \u0623\u0633\u0627\u0633\u064a \u0645\u0646 \u0627\u0644\u0643\u0631\u0648\u0645 16-18% \u0648\u0627\u0644\u0646\u064a\u0643\u0644 3.5-5.5% \u0648\u0627\u0644\u0645\u0646\u062c\u0646\u064a\u0632 5.5-7.5%. \u064a\u062a\u0648\u0627\u0641\u0642 \u0645\u0639 \u0645\u0639\u064a\u0627\u0631 ASTM A240 \u0648\u064a\u0639\u0627\u062f\u0644 1.4372 (EN) \u0648SUS 201 (JIS).<\/p><p class=\"wp-block-paragraph\">\u062a\u062a\u0645\u064a\u0632 \u0627\u0644\u062f\u0631\u062c\u0629 201 \u0628\u0645\u0642\u0627\u0648\u0645\u0629 \u062c\u064a\u062f\u0629 \u0644\u0644\u062a\u0622\u0643\u0644\u060c \u0648\u062e\u0627\u0635\u0629 \u0641\u064a \u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u0645\u0639\u062a\u062f\u0644\u0629\u060c \u0643\u0645\u0627 \u062a\u062a\u0645\u062a\u0639 \u0628\u0645\u062a\u0627\u0646\u0629 \u0648\u0642\u0648\u0629 \u0645\u0645\u062a\u0627\u0632\u062a\u064a\u0646. \u062a\u064f\u0633\u062a\u062e\u062f\u0645 \u0639\u0627\u062f\u0629\u064b \u0641\u064a \u0645\u0639\u062f\u0627\u062a \u0627\u0644\u0645\u0637\u0628\u062e\u060c \u0648\u0632\u062e\u0627\u0631\u0641 \u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a\u060c \u0648\u0627\u0644\u0647\u064a\u0627\u0643\u0644 \u0627\u0644\u0645\u0639\u0645\u0627\u0631\u064a\u0629. \u0648\u0631\u063a\u0645 \u0623\u0646\u0647\u0627 \u0623\u0631\u062e\u0635 \u0645\u0646 \u0627\u0644\u062f\u0631\u062c\u0629 304\u060c \u0625\u0644\u0627 \u0623\u0646\u0647\u0627 \u0644\u0627 \u064a\u0648\u0635\u0649 \u0628\u0647\u0627 \u0641\u064a \u0627\u0644\u0638\u0631\u0648\u0641 \u0627\u0644\u063a\u0646\u064a\u0629 \u0628\u0627\u0644\u0643\u0644\u0648\u0631\u064a\u062f \u0623\u0648 \u0634\u062f\u064a\u062f\u0629 \u0627\u0644\u062a\u0622\u0643\u0644 \u0628\u0633\u0628\u0628 \u0645\u062d\u062a\u0648\u0627\u0647\u0627 \u0627\u0644\u0645\u0646\u062e\u0641\u0636 \u0645\u0646 \u0627\u0644\u0646\u064a\u0643\u0644.<\/p><h3 class=\"wp-block-heading\">\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201<\/h3><figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td><strong>\u0635\u0646\u0627\u0639\u0629<\/strong><\/td><td><strong>\u0637\u0644\u0628<\/strong><\/td><\/tr><tr><td>\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0637\u0628\u062e<\/td><td>\u0627\u0644\u0623\u062d\u0648\u0627\u0636\u060c \u0648\u0623\u0648\u0627\u0646\u064a \u0627\u0644\u0637\u0628\u062e\u060c \u0648\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0627\u0626\u062f\u0629\u060c \u0648\u0645\u0639\u062f\u0627\u062a \u062a\u062c\u0647\u064a\u0632 \u0627\u0644\u0623\u063a\u0630\u064a\u0629\u060c \u0648\u0645\u0627 \u0625\u0644\u0649 \u0630\u0644\u0643.<\/td><\/tr><tr><td>\u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a<\/td><td>\u0632\u062e\u0627\u0631\u0641 \u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a\u060c \u0623\u0646\u0638\u0645\u0629 \u0627\u0644\u0639\u0627\u062f\u0645\u060c \u0627\u0644\u0623\u062c\u0632\u0627\u0621 \u0627\u0644\u0632\u062e\u0631\u0641\u064a\u0629\u060c \u0623\u063a\u0637\u064a\u0629 \u0627\u0644\u0639\u062c\u0644\u0627\u062a\u060c \u0648\u0645\u0627 \u0625\u0644\u0649 \u0630\u0644\u0643.<\/td><\/tr><tr><td>\u0628\u0646\u064a\u0627\u0646<\/td><td>\u062f\u0631\u0627\u0628\u0632\u064a\u0646\u060c \u0644\u0648\u062d\u0627\u062a \u0627\u0644\u0645\u0635\u0627\u0639\u062f\u060c \u0644\u0648\u062d\u0627\u062a \u0627\u0644\u062f\u064a\u0643\u0648\u0631\u060c \u0625\u0637\u0627\u0631\u0627\u062a \u0627\u0644\u0646\u0648\u0627\u0641\u0630\u060c \u0627\u0644\u062e.<\/td><\/tr><tr><td>\u0627\u0644\u0633\u0644\u0639 \u0627\u0644\u0627\u0633\u062a\u0647\u0644\u0627\u0643\u064a\u0629<\/td><td>\u0623\u063a\u0644\u0641\u0629 \u0627\u0644\u0623\u062c\u0647\u0632\u0629\u060c \u0648\u062a\u0631\u0643\u064a\u0628\u0627\u062a \u0627\u0644\u0623\u062b\u0627\u062b\u060c \u0648\u062a\u0631\u0643\u064a\u0628\u0627\u062a \u0627\u0644\u0625\u0636\u0627\u0621\u0629\u060c \u0648\u0645\u0642\u0627\u0628\u0636 \u0627\u0644\u0623\u0628\u0648\u0627\u0628\u060c \u0648\u0645\u0627 \u0625\u0644\u0649 \u0630\u0644\u0643.<\/td><\/tr><\/tbody><\/table><\/figure><h3 class=\"wp-block-heading\">\u0645\u0645\u064a\u0632\u0627\u062a \u0648\u0639\u064a\u0648\u0628 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201<\/h3><p class=\"wp-block-paragraph\">\u0641\u064a\u0645\u0627 \u064a\u0644\u064a \u0645\u0645\u064a\u0632\u0627\u062a \u0648\u0641\u0648\u0627\u0626\u062f \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 321:<\/p><ol class=\"wp-block-list\"><li>\u0641\u0639\u0627\u0644\u0629 \u0645\u0646 \u062d\u064a\u062b \u0627\u0644\u062a\u0643\u0644\u0641\u0629 \u0628\u0633\u0628\u0628 \u0645\u062d\u062a\u0648\u0649 \u0627\u0644\u0646\u064a\u0643\u0644 \u0627\u0644\u0645\u0646\u062e\u0641\u0636.<\/li>\n\n<li>\u0645\u0642\u0627\u0648\u0645\u0629 \u0642\u0648\u064a\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0641\u064a \u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u0645\u0639\u062a\u062f\u0644\u0629.<\/li>\n\n<li>\u0642\u0648\u0629 \u0627\u0644\u0634\u062f \u0627\u0644\u0639\u0627\u0644\u064a\u0629\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647\u0627 \u0645\u062a\u064a\u0646\u0629 \u0648\u0642\u0648\u064a\u0629.<\/li>\n\n<li>\u0642\u0627\u0628\u0644\u064a\u0629 \u062c\u064a\u062f\u0629 \u0644\u0644\u062a\u0634\u0643\u064a\u0644 \u0648\u0633\u0647\u0648\u0644\u0629 \u0627\u0644\u062a\u0635\u0646\u064a\u0639.<\/li>\n\n<li>\u062e\u0641\u064a\u0641\u0629 \u0627\u0644\u0648\u0632\u0646\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647\u0627 \u0645\u0646\u0627\u0633\u0628\u0629 \u0644\u0645\u062c\u0645\u0648\u0639\u0629 \u0645\u0646 \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a.<\/li><\/ol><p class=\"wp-block-paragraph\">\u0641\u064a\u0645\u0627 \u064a\u0644\u064a \u0639\u064a\u0648\u0628 \u0648\u0642\u064a\u0648\u062f \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 321:<\/p><ol class=\"wp-block-list\"><li>\u0645\u0642\u0627\u0648\u0645\u0629 \u0623\u0642\u0644 \u0644\u0644\u062a\u0622\u0643\u0644 \u0641\u064a \u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u0642\u0627\u0633\u064a\u0629 \u0645\u0642\u0627\u0631\u0646\u0629 \u0628\u0627\u0644\u062f\u0631\u062c\u0627\u062a \u0627\u0644\u0623\u0639\u0644\u0649.<\/li>\n\n<li>\u0623\u0643\u062b\u0631 \u0639\u0631\u0636\u0629 \u0644\u0644\u0635\u062f\u0623 \u0639\u0646\u062f \u062a\u0639\u0631\u0636\u0647 \u0644\u0645\u064a\u0627\u0647 \u0627\u0644\u0628\u062d\u0631 \u0623\u0648 \u0627\u0644\u0638\u0631\u0648\u0641 \u0627\u0644\u062d\u0645\u0636\u064a\u0629.<\/li>\n\n<li>\u0623\u0642\u0644 \u0645\u062a\u0627\u0646\u0629 \u0641\u064a \u062f\u0631\u062c\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u0642\u0635\u0648\u0649.<\/li>\n\n<li>\u064a\u0645\u0643\u0646 \u0623\u0646 \u064a\u0643\u0648\u0646 \u0627\u0644\u0644\u062d\u0627\u0645 \u0623\u0643\u062b\u0631 \u0635\u0639\u0648\u0628\u0629 \u0645\u0642\u0627\u0631\u0646\u0629 \u0628\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0639\u0627\u0644\u064a \u0627\u0644\u062c\u0648\u062f\u0629.<\/li>\n\n<li>\u0627\u0646\u062e\u0641\u0627\u0636 \u0642\u0627\u0628\u0644\u064a\u0629 \u0627\u0644\u062a\u0634\u063a\u064a\u0644 \u0644\u0628\u0639\u0636 \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u062b\u0642\u064a\u0644\u0629 \u0628\u0633\u0628\u0628 \u0627\u0646\u062e\u0641\u0627\u0636 \u0645\u062d\u062a\u0648\u0649 \u0627\u0644\u0646\u064a\u0643\u0644.<\/li><\/ol><h3 class=\"wp-block-heading\">\u0627\u0644\u062f\u0631\u062c\u0627\u062a \u0627\u0644\u0645\u0643\u0627\u0641\u0626\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201<\/h3><figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td><strong>\u0627\u0644\u0628\u0644\u062f\/\u0627\u0644\u0645\u0646\u0637\u0642\u0629<\/strong><\/td><td><strong>\u0627\u0644\u0645\u0639\u064a\u0627\u0631\/\u0627\u0644\u0645\u0648\u0627\u0635\u0641\u0627\u062a<\/strong><\/td><td><strong>\u0627\u0644\u062f\u0631\u062c\u0629 \u0627\u0644\u0645\u0643\u0627\u0641\u0626\u0629<\/strong><\/td><\/tr><tr><td>\u0627\u0644\u0627\u062a\u062d\u0627\u062f \u0627\u0644\u0623\u0648\u0631\u0648\u0628\u064a<\/td><td>EN 10088-2<\/td><td>X12CrMnNiN17-7-5 (1.4372)<\/td><\/tr><tr><td>\u0627\u0644\u0648\u0644\u0627\u064a\u0627\u062a \u0627\u0644\u0645\u062a\u062d\u062f\u0629 \u0627\u0644\u0623\u0645\u0631\u064a\u0643\u064a\u0629<\/td><td>\u0645\u0639\u0627\u064a\u064a\u0631 ASTM A240<\/td><td>201<\/td><\/tr><tr><td>\u0627\u0644\u064a\u0627\u0628\u0627\u0646<\/td><td>\u062c\u064a \u0627\u064a \u0627\u0633 \u062c\u064a 4304<\/td><td>\u0625\u0633 \u064a\u0648 \u0625\u0633 201<\/td><\/tr><tr><td>\u0641\u0631\u0646\u0633\u0627<\/td><td>\u0646 \u0641 \u062336-711<\/td><td>Z12CMN17-07Az<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0648\u0627\u0644\u062a\u0622\u0643\u0644 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201<\/h2><h3 class=\"wp-block-heading\">\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u0629<\/h3><p class=\"wp-block-paragraph\">201 \u0639\u0631\u0648\u0636 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 <strong>\u0645\u0642\u0627\u0648\u0645\u0629 \u0644\u0644\u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u0645\u0639\u062a\u062f\u0644\u0629\u060c<\/strong> \u0627\u0644\u062a\u0639\u0627\u0645\u0644 \u0645\u0639 \u0645\u0627 \u064a\u0635\u0644 \u0625\u0644\u0649 \u062d\u0648\u0627\u0644\u064a <strong>500 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (1112 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/strong>\u0642\u062f \u064a\u0624\u062f\u064a \u062a\u062c\u0627\u0648\u0632 \u0647\u0630\u0647 \u0627\u0644\u062f\u0631\u062c\u0629 \u0645\u0646 \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0625\u0644\u0649 \u062e\u0633\u0627\u0631\u0629 \u0643\u0628\u064a\u0631\u0629 \u0641\u064a \u0627\u0644\u0642\u0648\u0629 \u0648\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u0623\u0643\u0633\u062f\u0629. \u0648\u064a\u0624\u062f\u064a \u0627\u0646\u062e\u0641\u0627\u0636 \u0645\u062d\u062a\u0648\u0649 \u0627\u0644\u0646\u064a\u0643\u0644 \u0625\u0644\u0649 \u0627\u0646\u062e\u0641\u0627\u0636 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0645\u0642\u0627\u0631\u0646\u0629 \u0628\u062f\u0631\u062c\u0627\u062a \u0645\u062b\u0644 304 \u0648316. \u0644\u0630\u0644\u0643\u060c \u0641\u0625\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201 \u0623\u0643\u062b\u0631 \u0645\u0644\u0627\u0621\u0645\u0629 \u0644\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u062a\u064a \u062a\u062a\u0639\u0631\u0636 \u0644\u0644\u062d\u0631\u0627\u0631\u0629 \u0645\u0646 \u062d\u064a\u0646 \u0644\u0622\u062e\u0631 \u0623\u0648 \u062d\u064a\u062b \u062a\u0643\u0648\u0646 \u0627\u0644\u062a\u0643\u0644\u0641\u0629 \u0647\u064a \u0627\u0644\u0634\u0627\u063a\u0644 \u0627\u0644\u0623\u0633\u0627\u0633\u064a \u0648\u0644\u064a\u0633 \u0644\u0644\u0628\u064a\u0626\u0627\u062a \u0630\u0627\u062a \u062f\u0631\u062c\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u0639\u0627\u0644\u064a\u0629 \u0627\u0644\u0645\u0633\u062a\u0645\u0631\u0629.<\/p><h3 class=\"wp-block-heading\">\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644<\/h3><p class=\"wp-block-paragraph\">\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201 \u0645\u0646\u0627\u0633\u0628 \u0644\u0640 <strong>\u0628\u064a\u0626\u0627\u062a \u0645\u0639\u062a\u062f\u0644\u0629<\/strong>\u060c \u0645\u062b\u0644 \u0627\u0644\u0638\u0631\u0648\u0641 \u0627\u0644\u062f\u0627\u062e\u0644\u064a\u0629 \u0623\u0648 \u0627\u0644\u062c\u0627\u0641\u0629. \u0641\u064a \u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u0623\u0643\u062b\u0631 \u0639\u062f\u0648\u0627\u0646\u064a\u0629\u060c \u0645\u062b\u0644 \u062a\u0644\u0643 \u0627\u0644\u062a\u064a \u062a\u062a\u0639\u0631\u0636 \u0644\u0644\u0631\u0637\u0648\u0628\u0629 \u0623\u0648 \u0627\u0644\u0645\u064a\u0627\u0647 \u0627\u0644\u0645\u0627\u0644\u062d\u0629 \u0623\u0648 \u0627\u0644\u0623\u062d\u0645\u0627\u0636\u060c \u0642\u062f \u064a\u062a\u0622\u0643\u0644. \u062a\u0634\u0645\u0644 \u0627\u0644\u0623\u0634\u0643\u0627\u0644 \u0627\u0644\u0634\u0627\u0626\u0639\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0627\u0644\u062a\u0622\u0643\u0644 \u0627\u0644\u0646\u0642\u0637\u064a \u0648\u062a\u0622\u0643\u0644 \u0627\u0644\u0634\u0642\u0648\u0642 \u0648\u0627\u0644\u0635\u062f\u0623 \u0627\u0644\u0633\u0637\u062d\u064a. \u064a\u0639\u0645\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201 \u0628\u0634\u0643\u0644 \u0623\u0641\u0636\u0644 \u0641\u064a \u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u062a\u064a \u0644\u0627 \u062a\u062a\u0639\u0631\u0636 \u0644\u0645\u0648\u0627\u062f \u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629 \u0643\u0628\u064a\u0631\u0629.<\/p><h2 class=\"wp-block-heading\">\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201<\/h2><h3 class=\"wp-block-heading\">\u062a\u0634\u0643\u064a\u0644<\/h3><p class=\"wp-block-paragraph\">\u062a\u0634\u0643\u064a\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201 <strong>\u064a\u062a\u0636\u0645\u0646 \u0627\u0644\u0639\u0645\u0644 \u0627\u0644\u0628\u0627\u0631\u062f<\/strong>\u060c \u062d\u064a\u062b \u064a\u062a\u0635\u0644\u0628 \u0628\u0633\u0631\u0639\u0629. \u0627\u0644\u0633\u0628\u0627\u0626\u0643 \u0623\u0642\u0644 \u0642\u0627\u0628\u0644\u064a\u0629 \u0644\u0644\u0637\u0631\u0642 \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 304 \u0628\u0633\u0628\u0628 \u0645\u062d\u062a\u0648\u0627\u0647\u0627 \u0627\u0644\u0645\u0646\u062e\u0641\u0636 \u0645\u0646 \u0627\u0644\u0646\u064a\u0643\u0644. \u0642\u062f \u062a\u062a\u0637\u0644\u0628 \u0627\u0644\u0645\u0632\u064a\u062f \u0645\u0646 \u0627\u0644\u0642\u0648\u0629 \u0623\u0648 \u0627\u0644\u0645\u0639\u062f\u0627\u062a \u0627\u0644\u0645\u062a\u062e\u0635\u0635\u0629 \u0623\u062b\u0646\u0627\u0621 \u0627\u0644\u0627\u0646\u062d\u0646\u0627\u0621 \u0623\u0648 \u0627\u0644\u062a\u0645\u062f\u062f \u0623\u0648 \u0627\u0644\u0633\u062d\u0628 \u0627\u0644\u0639\u0645\u064a\u0642. \u064a\u0645\u0643\u0646 \u0623\u0646 \u062a\u0633\u0627\u0639\u062f \u0627\u0644\u062a\u0644\u062f\u064a\u0646 \u0641\u064a \u062a\u0642\u0644\u064a\u0644 \u0627\u0644\u0625\u062c\u0647\u0627\u062f \u0627\u0644\u062f\u0627\u062e\u0644\u064a \u0628\u0639\u062f \u0627\u0644\u062a\u0634\u0643\u064a\u0644. \u0646\u0638\u0631\u064b\u0627 \u0644\u0645\u0639\u062f\u0644 \u0627\u0644\u062a\u0635\u0644\u0628 \u0639\u0646\u062f \u0627\u0644\u0639\u0645\u0644\u060c \u0642\u062f \u064a\u0643\u0648\u0646 \u0627\u0644\u062a\u0644\u062f\u064a\u0646 \u0627\u0644\u0645\u062a\u0648\u0633\u0637 \u0636\u0631\u0648\u0631\u064a\u064b\u0627 \u0644\u0644\u0623\u0634\u0643\u0627\u0644 \u0627\u0644\u0623\u0643\u062b\u0631 \u062a\u0639\u0642\u064a\u062f\u064b\u0627.<\/p><h3 class=\"wp-block-heading\">\u0627\u0644\u0644\u062d\u0627\u0645<\/h3><p class=\"wp-block-paragraph\">\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201 \u0647\u0648 \u0639\u0645\u0648\u0645\u0627 <strong>\u0645\u0646 \u0627\u0644\u0633\u0647\u0644 \u0627\u0644\u0644\u062d\u0627\u0645<\/strong>\u0648\u0644\u0643\u0646 \u0627\u0644\u062a\u062d\u0643\u0645 \u0627\u0644\u0645\u0646\u0627\u0633\u0628 \u0641\u064a \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0636\u0631\u0648\u0631\u064a \u0644\u0645\u0646\u0639 \u0627\u0644\u0627\u0646\u062d\u0646\u0627\u0621 \u0623\u0648 \u0627\u0644\u062a\u0634\u0642\u0642. \u062a\u064f\u0633\u062a\u062e\u062f\u0645 \u0639\u0627\u062f\u0629\u064b \u0645\u0648\u0627\u062f \u062d\u0634\u0648 \u0645\u0634\u0627\u0628\u0647\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201 \u0623\u0648 304. \u064a\u0645\u0643\u0646 \u0644\u0644\u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u0632\u0627\u0626\u062f\u0629 \u0623\u0646 \u062a\u0642\u0644\u0644 \u0645\u0646 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644\u060c \u0644\u0630\u0627 \u0641\u0625\u0646 \u0625\u062f\u0627\u0631\u0629 \u0645\u062f\u062e\u0644\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0648\u0627\u0644\u062a\u0628\u0631\u064a\u062f \u0628\u064a\u0646 \u0627\u0644\u062a\u0645\u0631\u064a\u0631\u0627\u062a \u0623\u0645\u0631 \u0636\u0631\u0648\u0631\u064a. \u064a\u0639\u062f \u0627\u0644\u062a\u0646\u0638\u064a\u0641 \u0642\u0628\u0644 \u0627\u0644\u0644\u062d\u0627\u0645 \u0623\u0645\u0631\u064b\u0627 \u0645\u0647\u0645\u064b\u0627 \u0644\u062a\u062c\u0646\u0628 \u0627\u0644\u062a\u0644\u0648\u062b. \u064a\u0633\u0627\u0639\u062f \u0627\u0644\u062a\u062d\u0643\u0645 \u0641\u064a \u0645\u0639\u0644\u0645\u0627\u062a \u0627\u0644\u0644\u062d\u0627\u0645 \u0648\u0645\u062f\u062e\u0644\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0641\u064a \u0645\u0646\u0639 \u0627\u0644\u062a\u0634\u0642\u0642 \u0627\u0644\u0633\u0627\u062e\u0646\u060c \u0645\u0645\u0627 \u064a\u0636\u0645\u0646 \u062c\u0648\u062f\u0629 \u0627\u0644\u0644\u062d\u0627\u0645.<\/p><h3 class=\"wp-block-heading\">\u0627\u0644\u062a\u0635\u0646\u064a\u0639<\/h3><p class=\"wp-block-paragraph\">201 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 <strong>\u0642\u0627\u0628\u0644\u064a\u0629 \u0627\u0644\u062a\u0635\u0646\u064a\u0639 \u0645\u0639\u062a\u062f\u0644\u0629<\/strong>\u0625\u0646\u0647 \u0623\u0643\u062b\u0631 \u0635\u0644\u0627\u0628\u0629 \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 304 \u0628\u0633\u0628\u0628 \u0645\u062d\u062a\u0648\u0627\u0647 \u0627\u0644\u0639\u0627\u0644\u064a \u0645\u0646 \u0627\u0644\u0645\u0646\u062c\u0646\u064a\u0632\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647 <strong>\u0623\u0635\u0639\u0628 \u0641\u064a \u0627\u0644\u0642\u0637\u0639<\/strong>\u0648\u062a\u0634\u0645\u0644 \u0627\u0644\u0639\u0648\u0627\u0645\u0644 \u0627\u0644\u0631\u0626\u064a\u0633\u064a\u0629 \u0645\u0627 \u064a\u0644\u064a:<\/p><ol class=\"wp-block-list\"><li><strong>\u062a\u0642\u0648\u064a\u0629 \u0627\u0644\u0639\u0645\u0644<\/strong>:\u064a\u0645\u064a\u0644 \u0625\u0644\u0649 \u0627\u0644\u062a\u0635\u0644\u0628 \u0623\u062b\u0646\u0627\u0621 \u0627\u0644\u062a\u0635\u0646\u064a\u0639\u060c \u0645\u0645\u0627 \u064a\u0632\u064a\u062f \u0645\u0646 \u0635\u0639\u0648\u0628\u0629 \u0627\u0644\u0642\u0637\u0639 \u0645\u0639 \u062a\u0642\u062f\u0645 \u0627\u0644\u0639\u0645\u0644\u064a\u0629.<\/li>\n\n<li><strong>\u0633\u0631\u0639\u0629 \u0627\u0644\u0642\u0637\u0639<\/strong>:\u062a\u062a\u0637\u0644\u0628 \u0633\u0631\u0639\u0627\u062a \u0642\u0637\u0639 \u0623\u0642\u0644 \u0644\u062a\u062c\u0646\u0628 \u0627\u0631\u062a\u0641\u0627\u0639 \u062f\u0631\u062c\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0648\u062a\u0644\u0641 \u0627\u0644\u0623\u062f\u0648\u0627\u062a\u060c \u0648\u062e\u0627\u0635\u0629 \u0623\u062b\u0646\u0627\u0621 \u062d\u062f\u0648\u062b \u0627\u0644\u062a\u0635\u0644\u0628 \u0623\u062b\u0646\u0627\u0621 \u0627\u0644\u0639\u0645\u0644.<\/li>\n\n<li><strong>\u062a\u0622\u0643\u0644 \u0627\u0644\u0623\u062f\u0648\u0627\u062a<\/strong>:\u062a\u062a\u0622\u0643\u0644 \u0627\u0644\u0623\u062f\u0648\u0627\u062a \u0628\u0634\u0643\u0644 \u0623\u0633\u0631\u0639 \u0628\u0633\u0628\u0628 \u0642\u0648\u062a\u0647\u0627 \u0627\u0644\u0639\u0627\u0644\u064a\u0629 \u0648\u0635\u0644\u0627\u0628\u062a\u0647\u0627 \u0648\u0645\u062a\u0627\u0646\u062a\u0647\u0627\u060c \u0645\u0645\u0627 \u064a\u0633\u062a\u0644\u0632\u0645 \u062a\u063a\u064a\u064a\u0631 \u0627\u0644\u0623\u062f\u0648\u0627\u062a \u0628\u0634\u0643\u0644 \u0645\u062a\u0643\u0631\u0631.<\/li>\n\n<li><strong>\u062a\u0634\u0643\u064a\u0644 \u0627\u0644\u0631\u0642\u0627\u0642\u0629<\/strong>:\u064a\u0646\u062a\u062c \u0631\u0642\u0627\u0626\u0642 \u0635\u0644\u0628\u0629 \u0648\u0637\u0648\u064a\u0644\u0629\u060c \u0645\u0645\u0627 \u0642\u062f \u064a\u0624\u062f\u064a \u0625\u0644\u0649 \u062a\u0639\u0642\u064a\u062f \u0639\u0645\u0644\u064a\u0629 \u0625\u0632\u0627\u0644\u0629 \u0627\u0644\u0631\u0642\u0627\u0626\u0642 \u0648\u0642\u062f \u064a\u062a\u062f\u0627\u062e\u0644 \u0645\u0639 \u0639\u0645\u0644\u064a\u0629 \u0627\u0644\u062a\u0635\u0646\u064a\u0639.<\/li>\n\n<li><strong>\u062a\u0634\u062d\u064a\u0645<\/strong>:\u0627\u0644\u062a\u0628\u0631\u064a\u062f \u0648\u0627\u0644\u062a\u0632\u064a\u064a\u062a \u0627\u0644\u0645\u0646\u0627\u0633\u0628\u0627\u0646 \u0636\u0631\u0648\u0631\u064a\u0627\u0646 \u0644\u0645\u0646\u0639 \u062a\u0644\u0641 \u0627\u0644\u0623\u062f\u0648\u0627\u062a \u0648\u062a\u0642\u0644\u064a\u0644 \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0648\u062a\u062d\u0633\u064a\u0646 \u062a\u0634\u0637\u064a\u0628 \u0627\u0644\u0633\u0637\u062d.<\/li><\/ol><h3 class=\"wp-block-heading\">\u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629<\/h3><p class=\"wp-block-paragraph\">\u0644\u0627 \u064a\u0645\u0643\u0646 \u062a\u0642\u0648\u064a\u0629 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201 \u0639\u0646 \u0637\u0631\u064a\u0642 \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629\u060c \u0648\u0644\u0643\u0646 \u064a\u0645\u0643\u0646 \u062a\u0642\u0648\u064a\u062a\u0647 \u0645\u0646 \u062e\u0644\u0627\u0644 \u0627\u0644\u0639\u0645\u0644 \u0627\u0644\u0628\u0627\u0631\u062f.<\/p><p class=\"wp-block-paragraph\">\u0644\u0644\u062a\u0644\u062f\u064a\u0646\u060c \u0642\u0645 \u0628\u062a\u0633\u062e\u064a\u0646\u0647 \u0625\u0644\u0649 1850-1950 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a (1010-1066 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629)\u060c \u062b\u0645 \u0642\u0645 \u0628\u062a\u0628\u0631\u064a\u062f\u0647 \u0628\u0633\u0631\u0639\u0629 \u0639\u0646 \u0637\u0631\u064a\u0642 \u0627\u0644\u062a\u0628\u0631\u064a\u062f \u0628\u0627\u0644\u0645\u0627\u0621 \u0623\u0648 \u0627\u0644\u062a\u0628\u0631\u064a\u062f \u0628\u0627\u0644\u0647\u0648\u0627\u0621. \u062d\u0627\u0641\u0638 \u0639\u0644\u0649 \u062f\u0631\u062c\u0629 \u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u062a\u0644\u062f\u064a\u0646 \u0645\u0646\u062e\u0641\u0636\u0629 \u0642\u062f\u0631 \u0627\u0644\u0625\u0645\u0643\u0627\u0646 \u0644\u062a\u0642\u0644\u064a\u0644 \u0627\u0644\u062a\u0643\u0644\u0633\u060c \u062d\u064a\u062b \u0623\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201 \u0623\u0643\u062b\u0631 \u0639\u0631\u0636\u0629 \u0644\u0644\u062a\u0643\u0644\u0633\u0627\u062a \u0645\u0646 \u0627\u0644\u062f\u0631\u062c\u0629 301. \u0628\u0639\u062f \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629\u060c \u0642\u062f \u062a\u0643\u0648\u0646 \u0647\u0646\u0627\u0643 \u062d\u0627\u062c\u0629 \u0625\u0644\u0649 \u0645\u0639\u0627\u0644\u062c\u0627\u062a \u0633\u0637\u062d\u064a\u0629 \u0645\u062b\u0644 \u0627\u0644\u062a\u062e\u0644\u064a\u0644 \u0623\u0648 \u0627\u0644\u062a\u062e\u0645\u064a\u062f \u0644\u062a\u062d\u0633\u064a\u0646 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644\u060c \u062d\u064a\u062b \u0623\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201 \u0623\u0643\u062b\u0631 \u0639\u0631\u0636\u0629 \u0644\u0644\u0623\u0643\u0633\u062f\u0629.<\/p><h2 class=\"wp-block-heading\">\u0627\u0644\u062a\u0631\u0643\u064a\u0628 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201<\/h2><p class=\"wp-block-paragraph\">\u0642\u0645 \u0628\u0641\u062d\u0635 \u0627\u0644\u062c\u062f\u0648\u0644 \u0623\u062f\u0646\u0627\u0647 \u0644\u0645\u0639\u0631\u0641\u0629 \u0627\u0644\u062a\u0631\u0643\u064a\u0628 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201:<\/p><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u0639\u0646\u0635\u0631<\/strong><\/td><td><strong>\u0627\u0644\u0643\u0631\u0628\u0648\u0646\u060c \u062c<\/strong><\/td><td><strong>\u0627\u0644\u0643\u0631\u0648\u0645\u060c \u0627\u0644\u0643\u0631\u0648\u0645<\/strong><\/td><td><strong>\u0627\u0644\u062d\u062f\u064a\u062f\u060c Fe<\/strong><\/td><td><strong>\u0627\u0644\u0645\u0646\u063a\u0646\u064a\u0632\u060c \u0627\u0644\u0645\u0646\u063a\u0646\u064a\u0632<\/strong><\/td><td><strong>\u0627\u0644\u0646\u064a\u0643\u0644\u060c \u0646\u064a<\/strong><\/td><td><strong>\u0627\u0644\u0646\u064a\u062a\u0631\u0648\u062c\u064a\u0646\u060c \u0646<\/strong><\/td><td><strong>\u0627\u0644\u0641\u0648\u0633\u0641\u0648\u0631\u060c \u0641<\/strong><\/td><td><strong>\u0627\u0644\u0633\u064a\u0644\u064a\u0643\u0648\u0646<\/strong><\/td><td><strong>\u0627\u0644\u0643\u0628\u0631\u064a\u062a\u060c \u0633<\/strong><\/td><\/tr><tr><td>\u0648%<\/td><td>\u2264 0.15 %<\/td><td>16 &#8211; 18 %<\/td><td>67.51 \u2013 75 % (\u0643\u0628\u0627\u0642\u064a)<\/td><td>5.5 &#8211; 7.5 %<\/td><td>3.5 &#8211; 5.5 %<\/td><td>\u2264 0.25 %<\/td><td>\u2264 0.060 %<\/td><td>\u2264 1.0 %<\/td><td>\u2264 0.030 %<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201<\/h2><h3 class=\"wp-block-heading\">\u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0641\u064a\u0632\u064a\u0627\u0626\u064a\u0629<\/h3><p class=\"wp-block-paragraph\">\u0642\u0645 \u0628\u0641\u062d\u0635 \u0627\u0644\u062c\u062f\u0648\u0644 \u0623\u062f\u0646\u0627\u0647 \u0644\u0645\u0639\u0631\u0641\u0629 \u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0641\u064a\u0632\u064a\u0627\u0626\u064a\u0629 \u0627\u0644\u0623\u0633\u0627\u0633\u064a\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201:<\/p><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u0645\u0644\u0643\u064a\u0629<\/strong><\/td><td><strong>\u0642\u064a\u0645\u0629<\/strong><\/td><td><strong>\u0623\u062f\u0627\u0621<\/strong><\/td><\/tr><tr><td>\u0643\u062b\u0627\u0641\u0629<\/td><td>7.81 \u062c\u0631\u0627\u0645\/\u0633\u0645 \u0645\u0643\u0639\u0628 (0.282 \u0631\u0637\u0644\/\u0628\u0648\u0635\u0629 \u0645\u0643\u0639\u0628\u0629)<\/td><td>\u0623\u062e\u0641 \u0648\u0632\u0646\u0627 \u0645\u0646 \u0645\u0639\u0638\u0645 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0643\u0631\u0628\u0648\u0646\u064a\u060c \u0648\u0645\u0645\u0627\u062b\u0644 \u0644\u0623\u0646\u0648\u0627\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0623\u062e\u0631\u0649.<\/td><\/tr><tr><td>\u0646\u0642\u0637\u0629 \u0627\u0644\u0627\u0646\u0635\u0647\u0627\u0631<\/td><td>1399 \u2013 1454 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (2550 \u2013 2650 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/td><td>\u0646\u0642\u0637\u0629 \u0627\u0646\u0635\u0647\u0627\u0631 \u0639\u0627\u0644\u064a\u0629\u060c \u0645\u0645\u0627\u062b\u0644\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 304.<\/td><\/tr><tr><td>CTE\u060c \u062e\u0637\u064a \u0639\u0646\u062f 0-100 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629\/32-212 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a<\/td><td>15.7 \u0645\u064a\u0643\u0631\u0648\u0645\u062a\u0631\/\u0645\u062a\u0631-\u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (8.7 \u0645\u064a\u0643\u0631\u0648\u0628\u0648\u0635\u0629\/\u0628\u0648\u0635\u0629-\u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/td><td>\u064a\u062a\u0645\u062f\u062f \u0623\u0643\u062b\u0631 \u0628\u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0645\u0646 304\u060c \u0648\u0623\u0642\u0644 \u0645\u0646 \u0633\u0628\u0627\u0626\u0643 \u0627\u0644\u0623\u0644\u0648\u0645\u0646\u064a\u0648\u0645.<\/td><\/tr><tr><td>\u0627\u0644\u0633\u0639\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629 \u0627\u0644\u0646\u0648\u0639\u064a\u0629 \u0639\u0646\u062f 0-100 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629\/212 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a<\/td><td>0.500 \u062c\u0648\u0644\/\u062c\u0645-\u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (0.12 \u0648\u062d\u062f\u0629 \u062d\u0631\u0627\u0631\u064a\u0629 \u0628\u0631\u064a\u0637\u0627\u0646\u064a\u0629\/\u0631\u0637\u0644-\u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/td><td>\u0627\u0645\u062a\u0635\u0627\u0635 \u062d\u0631\u0627\u0631\u064a \u0645\u0645\u0627\u062b\u0644 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0622\u062e\u0631 \u0645\u062b\u0644 304.<\/td><\/tr><tr><td>\u0627\u0644\u0645\u0648\u0635\u0644\u064a\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629 \u0639\u0646\u062f 100 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629\/212 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a<\/td><td>16.2 \u0648\u0627\u0637\/\u0645\u062a\u0631 \u0643\u0644\u0641\u0646 (112 \u0648\u062d\u062f\u0629 \u062d\u0631\u0627\u0631\u064a\u0629 \u0628\u0631\u064a\u0637\u0627\u0646\u064a\u0629\/\u0633\u0627\u0639\u0629\/\u0642\u062f\u0645 \u0645\u0631\u0628\u0639-\u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/td><td>\u0645\u0648\u0635\u0644\u064a\u0629 \u062d\u0631\u0627\u0631\u064a\u0629 \u0623\u0642\u0644 \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0643\u0631\u0628\u0648\u0646\u064a\u060c \u0645\u0645\u0627\u062b\u0644\u0629 \u0644\u0640 304.<\/td><\/tr><tr><td>\u0627\u0644\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u0643\u0647\u0631\u0628\u0627\u0626\u064a\u0629<\/td><td>0.0000685 \u0623\u0648\u0645-\u0633\u0645 (68.5 \u0645\u064a\u0643\u0631\u0648 \u0623\u0648\u0645-\u0633\u0645)<\/td><td>\u0645\u0648\u0635\u0644\u064a\u0629 \u0643\u0647\u0631\u0628\u0627\u0626\u064a\u0629 \u0645\u0646\u062e\u0641\u0636\u0629 \u0625\u0644\u0649 \u062d\u062f \u0645\u0627\u060c \u0648\u0647\u064a \u0633\u0645\u0629 \u0645\u0645\u064a\u0632\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623.<\/td><\/tr><tr><td>\u0627\u0644\u0646\u0641\u0627\u0630\u064a\u0629 \u0627\u0644\u0645\u063a\u0646\u0627\u0637\u064a\u0633\u064a\u0629<\/td><td>1.02\u060c H = 200 \u0623\u0648\u0631\u0633\u062a\u064a\u062f\u060c \u0645\u064f\u0644\u064e\u062f\u064e\u0651\u0646<\/td><td>\u0645\u063a\u0646\u0627\u0637\u064a\u0633\u064a\u0629 \u0642\u0644\u064a\u0644\u0627<\/td><\/tr><\/tbody><\/table><\/figure><h3 class=\"wp-block-heading\">\u0627\u0644\u062e\u0648\u0627\u0635 \u0627\u0644\u0645\u064a\u0643\u0627\u0646\u064a\u0643\u064a\u0629<\/h3><p class=\"wp-block-paragraph\">\u0642\u0645 \u0628\u0641\u062d\u0635 \u0627\u0644\u062c\u062f\u0648\u0644 \u0623\u062f\u0646\u0627\u0647 \u0644\u0645\u0639\u0631\u0641\u0629 \u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0645\u064a\u0643\u0627\u0646\u064a\u0643\u064a\u0629 \u0627\u0644\u0623\u0633\u0627\u0633\u064a\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201:<\/p><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u0645\u0644\u0643\u064a\u0629<\/strong><\/td><td><strong>\u0627\u0644\u0642\u064a\u0645\u0629 (\u0645\u062a\u0631\u064a\u0629\/\u0625\u0645\u0628\u0631\u0627\u0637\u0648\u0631\u064a\u0629)<\/strong><\/td><td><strong>\u0623\u062f\u0627\u0621<\/strong><\/td><\/tr><tr><td>\u0642\u0648\u0629 \u0627\u0644\u0634\u062f (\u0645\u064f\u0644\u064e\u062f\u064e\u0651\u062f\u0629)<\/td><td>758 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644 (110 \u0643\u064a\u0644\u0648\u0628\u0627\u0633\u0643\u0627\u0644)<\/td><td>\u0642\u0648\u064a\u0629 \u0628\u0645\u0627 \u064a\u0643\u0641\u064a \u0644\u062a\u062d\u0645\u0644 \u0627\u0644\u0623\u062d\u0645\u0627\u0644 \u0627\u0644\u0645\u0639\u062a\u062f\u0644\u0629 (\u0623\u0642\u0644 \u0645\u0646 316)\u060c \u0648\u0645\u0646\u0627\u0633\u0628\u0629 \u0644\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u0639\u0627\u0645.<\/td><\/tr><tr><td>\u0642\u0648\u0629 \u0627\u0644\u062e\u0636\u0648\u0639 (@Strain 0.2%\u060c \u0645\u064f\u0644\u064e\u062f\u064e\u0651\u0646)<\/td><td>379 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644 (55 \u0643\u064a\u0644\u0648\u0628\u0627\u0633\u0643\u0627\u0644)<\/td><td>\u064a\u062a\u062d\u0645\u0644 \u0627\u0644\u0636\u063a\u0648\u0637 \u0627\u0644\u064a\u0648\u0645\u064a\u0629 \u0628\u0634\u0643\u0644 \u062c\u064a\u062f\u060c \u0644\u0643\u0646\u0647 \u0633\u064a\u0646\u062d\u0646\u064a \u062a\u062d\u062a \u0627\u0644\u0623\u062d\u0645\u0627\u0644 \u0627\u0644\u062b\u0642\u064a\u0644\u0629 (\u0623\u0642\u0644 \u0645\u0646 304 \u0648316).<\/td><\/tr><tr><td>\u0635\u0644\u0627\u0628\u0629 \u0631\u0648\u0643\u0648\u064a\u0644 (\u0645\u064f\u0644\u064e\u062f\u064e\u0651\u062f\u0629)<\/td><td>87 \u0633\u0627\u0639\u0629<\/td><td>\u0645\u0642\u0627\u0648\u0645\u0629 \u062c\u064a\u062f\u0629 \u0644\u0644\u062a\u0622\u0643\u0644\u060c \u0645\u0646\u0627\u0633\u0628\u0629 \u0644\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u0642\u064a\u0627\u0633\u064a\u060c \u0645\u0645\u0627\u062b\u0644\u0629 \u0644\u0640 304.<\/td><\/tr><tr><td>\u0627\u0644\u0627\u0633\u062a\u0637\u0627\u0644\u0629 \u0639\u0646\u062f \u0627\u0644\u0643\u0633\u0631 (\u0628\u0642\u064a\u0627\u0633 2 \u0628\u0648\u0635\u0629\u060c \u0645\u064f\u0644\u064e\u062f\u064e\u0651\u0646)<\/td><td>52%<\/td><td>\u0645\u0631\u0646 \u0644\u0644\u063a\u0627\u064a\u0629\u060c \u064a\u0645\u062a\u062f \u0623\u0643\u062b\u0631 \u0645\u0646 304 \u0642\u0628\u0644 \u0623\u0646 \u064a\u0646\u0643\u0633\u0631\u060c \u0645\u062b\u0627\u0644\u064a \u0644\u0644\u062a\u0634\u0643\u064a\u0644.<\/td><\/tr><tr><td>\u0645\u0639\u0627\u0645\u0644 \u064a\u0648\u0646\u063a<\/td><td>197 \u062c\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644 (28.6 \u0645\u0644\u0644\u064a \u062b\u0627\u0646\u064a\u0629 \u0645\u0631\u0628\u0639\u0629)<\/td><td>\u064a\u0648\u0641\u0631 \u0635\u0644\u0627\u0628\u0629 \u0646\u0645\u0648\u0630\u062c\u064a\u0629 \u0644\u0644\u062f\u0639\u0645 \u0627\u0644\u0647\u064a\u0643\u0644\u064a\u060c \u0648\u0647\u0648 \u0645\u0639\u064a\u0627\u0631\u064a \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623.<\/td><\/tr><\/tbody><\/table><\/figure><h3 class=\"wp-block-heading\">\u0627\u0644\u062e\u0648\u0627\u0635 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629<\/h3><p class=\"wp-block-paragraph\">\u0642\u0645 \u0628\u0641\u062d\u0635 \u0627\u0644\u062c\u062f\u0648\u0644 \u0623\u062f\u0646\u0627\u0647 \u0644\u0645\u0639\u0631\u0641\u0629 \u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629 \u0627\u0644\u0623\u0633\u0627\u0633\u064a\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201:<\/p><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u0645\u0644\u0643\u064a\u0629<\/strong><\/td><td><strong>\u0648\u0635\u0641<\/strong><\/td><td><strong>\u0623\u062f\u0627\u0621<\/strong><\/td><\/tr><tr><td>\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644<\/td><td>\u0627\u0644\u0642\u062f\u0631\u0629 \u0639\u0644\u0649 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u0636\u0631\u0631 \u0627\u0644\u0646\u0627\u062a\u062c \u0639\u0646 \u0627\u0644\u0639\u0648\u0627\u0645\u0644 \u0627\u0644\u062e\u0627\u0631\u062c\u064a\u0629 \u0645\u062b\u0644 \u0627\u0644\u0631\u0637\u0648\u0628\u0629 \u0623\u0648 \u0627\u0644\u0645\u0648\u0627\u062f \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629 \u0623\u0648 \u0627\u0644\u0645\u0644\u062d.<\/td><td>\u0645\u062a\u0648\u0633\u0637\u060c \u0645\u0646\u0627\u0633\u0628 \u0644\u0644\u0628\u064a\u0626\u0627\u062a \u0630\u0627\u062a \u0627\u0644\u062a\u0639\u0631\u0636 \u0627\u0644\u0645\u0646\u062e\u0641\u0636 \u0625\u0644\u0649 \u0627\u0644\u0645\u062a\u0648\u0633\u0637 \u0644\u0644\u062a\u0622\u0643\u0644. \u0623\u0642\u0644 \u0645\u0642\u0627\u0648\u0645\u0629 \u0645\u0646 304.<\/td><\/tr><tr><td>\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u0623\u0643\u0633\u062f\u0629<\/td><td>\u0627\u0644\u0642\u062f\u0631\u0629 \u0639\u0644\u0649 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u0623\u0643\u0633\u062f\u0629 \u0623\u0648 \u0627\u0644\u0635\u062f\u0623 \u0639\u0646\u062f \u0627\u0644\u062a\u0639\u0631\u0636 \u0644\u0644\u0623\u0643\u0633\u062c\u064a\u0646 \u0641\u064a \u062f\u0631\u062c\u0627\u062a \u062d\u0631\u0627\u0631\u0629 \u0639\u0627\u0644\u064a\u0629.<\/td><td>\u0645\u0642\u0628\u0648\u0644 \u0628\u0634\u0643\u0644 \u0639\u0627\u0645 \u0641\u064a \u0638\u0644 \u0627\u0644\u0638\u0631\u0648\u0641 \u0627\u0644\u0642\u064a\u0627\u0633\u064a\u0629 \u0648\u0644\u0643\u0646\u0647 \u0623\u0642\u0644 \u0641\u0639\u0627\u0644\u064a\u0629 \u0641\u064a \u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0630\u0627\u062a \u062f\u0631\u062c\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u0639\u0627\u0644\u064a\u0629.<\/td><\/tr><tr><td>\u0627\u0644\u0627\u0633\u062a\u0642\u0631\u0627\u0631 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a<\/td><td>\u0627\u0644\u062e\u0627\u0635\u064a\u0629 \u0627\u0644\u062a\u064a \u062a\u0633\u0645\u062d \u0644\u0644\u0635\u0644\u0628 \u0628\u0627\u0644\u0628\u0642\u0627\u0621 \u062f\u0648\u0646 \u062a\u063a\u064a\u064a\u0631 \u0639\u0646\u062f \u062a\u0639\u0631\u0636\u0647 \u0644\u0645\u0648\u0627\u062f \u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629 \u0645\u062e\u062a\u0644\u0641\u0629.<\/td><td>\u0645\u0633\u062a\u0642\u0631 \u0641\u064a \u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u0645\u0639\u062a\u062f\u0644\u0629 \u0648\u0644\u0643\u0646 \u0623\u0642\u0644 \u0627\u0633\u062a\u0642\u0631\u0627\u0631\u064b\u0627 \u0641\u064a \u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629 \u0634\u062f\u064a\u062f\u0629 \u0627\u0644\u062a\u0622\u0643\u0644.<\/td><\/tr><tr><td>\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u0623\u062d\u0645\u0627\u0636 \u0648\u0627\u0644\u0642\u0644\u0648\u064a\u0627\u062a<\/td><td>\u0627\u0644\u0642\u062f\u0631\u0629 \u0639\u0644\u0649 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0644\u0641 \u0623\u0648 \u0627\u0644\u062a\u062f\u0647\u0648\u0631 \u0639\u0646\u062f \u0645\u0644\u0627\u0645\u0633\u062a\u0647\u0627 \u0644\u0644\u0645\u0648\u0627\u062f \u0627\u0644\u062d\u0645\u0636\u064a\u0629 \u0623\u0648 \u0627\u0644\u0642\u0644\u0648\u064a\u0629.<\/td><td>\u0645\u062d\u062f\u0648\u062f\u060c \u064a\u0639\u0645\u0644 \u0628\u0634\u0643\u0644 \u062c\u064a\u062f \u0641\u064a \u0627\u0644\u0623\u062d\u0645\u0627\u0636\/\u0627\u0644\u0642\u0644\u0648\u064a\u0627\u062a \u0627\u0644\u0636\u0639\u064a\u0641\u0629\u060c \u0648\u0644\u0643\u0646 \u0644\u0627 \u064a\u0646\u0635\u062d \u0628\u0647 \u0644\u0644\u0645\u0648\u0627\u062f \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629 \u0627\u0644\u0642\u0627\u0633\u064a\u0629.<\/td><\/tr><tr><td>\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u0635\u062f\u0623<\/td><td>\u0627\u0644\u0642\u062f\u0631\u0629 \u0639\u0644\u0649 \u0645\u0646\u0639 \u062a\u0643\u0648\u0651\u0646 \u0627\u0644\u0635\u062f\u0623\u060c \u0648\u062e\u0627\u0635\u0629\u064b \u0641\u064a \u0627\u0644\u0638\u0631\u0648\u0641 \u0627\u0644\u0631\u0637\u0628\u0629 \u0623\u0648 \u0627\u0644\u0645\u0628\u0644\u0644\u0629.<\/td><td>\u0645\u0642\u0627\u0648\u0645\u0629 \u0645\u0639\u062a\u062f\u0644\u0629 \u0644\u0644\u0635\u062f\u0623\u060c \u0623\u0642\u0644 \u0645\u0646 304\u060c \u0648\u0644\u0643\u0646\u0647\u0627 \u0645\u0646\u0627\u0633\u0628\u0629 \u0644\u0644\u0638\u0631\u0648\u0641 \u063a\u064a\u0631 \u0627\u0644\u0634\u062f\u064a\u062f\u0629.<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u0645\u0642\u0627\u0631\u0646\u0629 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201 \u0648304 \u0648316<\/h2><p class=\"wp-block-paragraph\">\u0642\u0645 \u0628\u0645\u0631\u0627\u062c\u0639\u0629 \u0627\u0644\u062c\u062f\u0648\u0644 \u0623\u062f\u0646\u0627\u0647 \u0644\u0625\u062c\u0631\u0627\u0621 \u0645\u0642\u0627\u0631\u0646\u0629 \u0633\u0631\u064a\u0639\u0629 \u0628\u064a\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201 \u0648304 \u0648316:<\/p><figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td><strong>\u0645\u0644\u0643\u064a\u0629<\/strong><\/td><td><strong>201<\/strong><\/td><td><strong><a href=\"https:\/\/steelprogroup.com\/ar\/stainless-steel\/grades\/grade-304\/\" target=\"_blank\" data-type=\"post\" data-id=\"8332\" rel=\"noreferrer noopener\">304<\/a><\/strong><\/td><td><strong><a href=\"https:\/\/steelprogroup.com\/ar\/stainless-steel\/grades\/grade-316\/\" target=\"_blank\" data-type=\"post\" data-id=\"10280\" rel=\"noreferrer noopener\">316<\/a><\/strong><\/td><\/tr><tr><td>\u064a\u0643\u062a\u0628<\/td><td>\u0623\u0648\u0633\u062a\u064a\u0646\u064a\u062a\u064a<\/td><td>\u0623\u0648\u0633\u062a\u064a\u0646\u064a\u062a\u064a<\/td><td>\u0623\u0648\u0633\u062a\u064a\u0646\u064a\u062a\u064a<\/td><\/tr><tr><td>\u0627\u0644\u0628\u0646\u064a\u0629 \u0627\u0644\u0628\u0644\u0648\u0631\u064a\u0629<\/td><td>\u0645\u0643\u0639\u0628 \u0645\u0631\u0643\u0632 \u0627\u0644\u0648\u062c\u0647 (FCC)<\/td><td>\u0645\u0643\u0639\u0628 \u0645\u0631\u0643\u0632 \u0627\u0644\u0648\u062c\u0647 (FCC)<\/td><td>\u0645\u0643\u0639\u0628 \u0645\u0631\u0643\u0632 \u0627\u0644\u0648\u062c\u0647 (FCC)<\/td><\/tr><tr><td>\u0627\u0644\u062a\u0631\u0643\u064a\u0628 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a<\/td><td>\u0643\u0631: 16-18%\u060c \u0646\u064a\u0643\u0644: 3.5-5.5%<\/td><td>\u0643\u0631: 18-20%\u060c \u0646\u064a: 8-10.5%<\/td><td>\u0627\u0644\u0643\u0631\u0648\u0645: 16-18%\u060c \u0627\u0644\u0646\u064a\u0643\u0644: 10-14%\u060c \u0627\u0644\u0645\u0648\u0644\u064a\u0628\u062f\u064a\u0646\u0648\u0645: 2-3%<\/td><\/tr><tr><td>\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644<\/td><td>\u0645\u0639\u062a\u062f\u0644<\/td><td>\u062c\u064a\u062f<\/td><td>\u0645\u0645\u062a\u0627\u0632<\/td><\/tr><tr><td>\u0642\u0648\u0629<\/td><td>\u0623\u0639\u0644\u0649<\/td><td>\u0648\u0627\u0633\u0637\u0629<\/td><td>\u0623\u062f\u0646\u0649<\/td><\/tr><tr><td>\u0635\u0644\u0627\u0628\u0629<\/td><td>\u0623\u0639\u0644\u0649<\/td><td>\u0648\u0627\u0633\u0637\u0629<\/td><td>\u0623\u062f\u0646\u0649<\/td><\/tr><tr><td>\u0642\u0627\u0628\u0644\u064a\u0629 \u0627\u0644\u062a\u0634\u0643\u064a\u0644<\/td><td>\u062c\u064a\u062f<\/td><td>\u0645\u0645\u062a\u0627\u0632<\/td><td>\u0645\u0645\u062a\u0627\u0632<\/td><\/tr><tr><td>\u0642\u0627\u0628\u0644\u064a\u0629 \u0627\u0644\u0644\u062d\u0627\u0645<\/td><td>\u0639\u062f\u0644<\/td><td>\u062c\u064a\u062f<\/td><td>\u062c\u064a\u062f<\/td><\/tr><tr><td>\u0642\u0627\u0628\u0644\u064a\u0629 \u0627\u0644\u062a\u0635\u0646\u064a\u0639<\/td><td>\u0639\u062f\u0644<\/td><td>\u062c\u064a\u062f<\/td><td>\u0639\u062f\u0644<\/td><\/tr><tr><td>\u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0645\u063a\u0646\u0627\u0637\u064a\u0633\u064a\u0629<\/td><td>\u0645\u063a\u0646\u0627\u0637\u064a\u0633\u064a\u0629 \u0642\u0644\u064a\u0644\u0627<\/td><td>\u063a\u064a\u0631 \u0645\u063a\u0646\u0627\u0637\u064a\u0633\u064a<\/td><td>\u063a\u064a\u0631 \u0645\u063a\u0646\u0627\u0637\u064a\u0633\u064a<\/td><\/tr><tr><td>\u064a\u0643\u0644\u0641<\/td><td>\u0623\u062f\u0646\u0649<\/td><td>\u0645\u0639\u062a\u062f\u0644<\/td><td>\u0623\u0639\u0644\u0649<\/td><\/tr><tr><td>\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a<\/td><td>\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0637\u0628\u062e \u0648\u0642\u0637\u0639 \u063a\u064a\u0627\u0631 \u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a<\/td><td>\u062a\u062c\u0647\u064a\u0632 \u0627\u0644\u0623\u063a\u0630\u064a\u0629 \u0648\u0645\u0639\u062f\u0627\u062a \u0627\u0644\u0623\u0644\u0628\u0627\u0646<\/td><td>\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629 \u0648\u0627\u0644\u0628\u062d\u0631\u064a\u0629<\/td><\/tr><\/tbody><\/table><\/figure><h3 class=\"wp-block-heading\">\u0623\u064a\u0647\u0645\u0627 \u0623\u0641\u0636\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201 \u0623\u0645 304\u061f<\/h3><p class=\"wp-block-paragraph\">\u064a\u0639\u062a\u0628\u0631 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 304 \u0623\u0641\u0636\u0644 \u0645\u0646 201 \u0645\u0646 \u062d\u064a\u062b \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644 \u0648\u0627\u0644\u0645\u062a\u0627\u0646\u0629 \u0648\u0627\u0644\u062c\u0648\u062f\u0629 \u0627\u0644\u0634\u0627\u0645\u0644\u0629. 201 \u0623\u0631\u062e\u0635 \u0648\u0644\u0643\u0646\u0647 \u0623\u0642\u0644 \u0645\u0642\u0627\u0648\u0645\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0648\u0623\u0643\u062b\u0631 \u0639\u0631\u0636\u0629 \u0644\u0644\u0635\u062f\u0623.<\/p><h2 class=\"wp-block-heading\">\u0645\u0627 \u0642\u062f \u064a\u062b\u064a\u0631 \u0642\u0644\u0642\u0643 \u0623\u064a\u0636\u064b\u0627<\/h2><h3 class=\"wp-block-heading\">\u0647\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201 \u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623\u061f<\/h3><p class=\"wp-block-paragraph\">\u0644\u0627\u060c \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201 \u0644\u064a\u0633 \u0645\u0642\u0627\u0648\u0645\u064b\u0627 \u0644\u0644\u0635\u062f\u0623 \u062a\u0645\u0627\u0645\u064b\u0627. \u0641\u0647\u0648 \u0623\u0643\u062b\u0631 \u0645\u0642\u0627\u0648\u0645\u0629 \u0644\u0644\u0635\u062f\u0623 \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0639\u0627\u062f\u064a \u0648\u0644\u0643\u0646\u0647 \u0623\u0642\u0644 \u0645\u0642\u0627\u0648\u0645\u0629 \u0645\u0646 \u0627\u0644\u062f\u0631\u062c\u0627\u062a \u0627\u0644\u0623\u0639\u0644\u0649 \u0645\u062b\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 304 \u0623\u0648 316.<\/p><h3 class=\"wp-block-heading\">\u0647\u0644 201 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0645\u063a\u0646\u0627\u0637\u064a\u0633\u064a\u061f<\/h3><p class=\"wp-block-paragraph\">\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201 \u0645\u063a\u0646\u0627\u0637\u064a\u0633\u064a. \u0648\u0631\u063a\u0645 \u0623\u0646\u0647 \u0645\u0646 \u0627\u0644\u062f\u0631\u062c\u0629 \u0627\u0644\u0623\u0648\u0633\u062a\u0646\u064a\u062a\u064a\u0629\u060c \u0625\u0644\u0627 \u0623\u0646 \u0645\u062d\u062a\u0648\u0627\u0647 \u0627\u0644\u0639\u0627\u0644\u064a \u0645\u0646 \u0627\u0644\u0645\u0646\u062c\u0646\u064a\u0632 \u0648\u0645\u062d\u062a\u0648\u0627\u0647 \u0627\u0644\u0645\u0646\u062e\u0641\u0636 \u0645\u0646 \u0627\u0644\u0646\u064a\u0643\u0644 \u0642\u062f \u064a\u0624\u062f\u064a \u0625\u0644\u0649 \u0628\u0639\u0636 \u0627\u0644\u0645\u063a\u0646\u0627\u0637\u064a\u0633\u064a\u0629\u060c \u062e\u0627\u0635\u0629 \u0628\u0639\u062f \u0627\u0644\u0639\u0645\u0644 \u0627\u0644\u0628\u0627\u0631\u062f.<\/p><p class=\"wp-block-paragraph\"><strong>\u0642\u0631\u0627\u0621\u0629 \u0630\u0627\u062a \u0635\u0644\u0629<\/strong><br><a href=\"https:\/\/steelprogroup.com\/ar\/stainless-steel\/properties\/magnetic\/\" data-type=\"post\" data-id=\"9889\">\u0647\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0645\u063a\u0646\u0627\u0637\u064a\u0633\u064a\u061f<\/a><a href=\"https:\/\/steelprogroup.com\/ar\/stainless-steel\/properties\/magnetic\/\" target=\"_blank\" data-type=\"post\" data-id=\"9889\" rel=\"noreferrer noopener\">?<\/a><\/p><h3 class=\"wp-block-heading\">\u0647\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201 \u0635\u0627\u0644\u062d \u0644\u0644\u0637\u0639\u0627\u0645\u061f<\/h3><p class=\"wp-block-paragraph\">\u0646\u0639\u0645\u060c \u064a\u0639\u062a\u0628\u0631 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201 \u0635\u0627\u0644\u062d\u064b\u0627 \u0644\u0644\u0623\u063a\u0630\u064a\u0629\u060c \u0648\u0644\u0643\u0646\u0647 \u064a\u062a\u0645\u062a\u0639 \u0628\u0645\u0642\u0627\u0648\u0645\u0629 \u0623\u0642\u0644 \u0644\u0644\u062a\u0622\u0643\u0644 \u0645\u0642\u0627\u0631\u0646\u0629 \u0628\u0623\u0646\u0648\u0627\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0623\u062e\u0631\u0649 \u0645\u062b\u0644 304\u060c \u0644\u0630\u0644\u0643 \u0642\u062f \u0644\u0627 \u064a\u0643\u0648\u0646 \u0645\u0646\u0627\u0633\u0628\u064b\u0627 \u0644\u062c\u0645\u064a\u0639 \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0645\u062a\u0639\u0644\u0642\u0629 \u0628\u0627\u0644\u0623\u063a\u0630\u064a\u0629.<\/p><h3 class=\"wp-block-heading\">\u0645\u0627 \u0647\u0648 \u0627\u0644\u0623\u0641\u0636\u0644 \u0643\u063a\u0630\u0627\u0621 201 \u0623\u0645 304\u061f<\/h3><p class=\"wp-block-paragraph\">\u0628\u0627\u0644\u0646\u0633\u0628\u0629 \u0644\u062f\u0631\u062c\u0629 \u0627\u0644\u063a\u0630\u0627\u0621\u060c \u0641\u0625\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 304 \u0623\u0641\u0636\u0644 \u0645\u0646 201 \u0644\u0623\u0646\u0647 \u064a\u062a\u0645\u062a\u0639 \u0628\u0645\u0642\u0627\u0648\u0645\u0629 \u0623\u0639\u0644\u0649 \u0644\u0644\u062a\u0622\u0643\u0644 \u0648\u0627\u0644\u0645\u062a\u0627\u0646\u0629\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647 \u0623\u0643\u062b\u0631 \u0623\u0645\u0627\u0646\u064b\u0627 \u0644\u0644\u0627\u062a\u0635\u0627\u0644 \u0628\u0627\u0644\u0637\u0639\u0627\u0645 \u0639\u0644\u0649 \u0627\u0644\u0645\u062f\u0649 \u0627\u0644\u0637\u0648\u064a\u0644.<\/p><h3 class=\"wp-block-heading\">\u0647\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201 \u0645\u0636\u0627\u062f \u0644\u0644\u062d\u0633\u0627\u0633\u064a\u0629\u061f<\/h3><p class=\"wp-block-paragraph\">\u0646\u0639\u0645\u060c \u064a\u0639\u062a\u0628\u0631 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201 \u0628\u0634\u0643\u0644 \u0639\u0627\u0645 \u0645\u0636\u0627\u062f\u064b\u0627 \u0644\u0644\u062d\u0633\u0627\u0633\u064a\u0629\u060c \u0648\u0644\u0643\u0646\u0647 \u0642\u062f \u064a\u0633\u0628\u0628 \u0631\u062f\u0648\u062f \u0641\u0639\u0644 \u0644\u062f\u0649 \u0628\u0639\u0636 \u0627\u0644\u0623\u0641\u0631\u0627\u062f \u0627\u0644\u062d\u0633\u0627\u0633\u064a\u0646 \u0628\u0633\u0628\u0628 \u0645\u062d\u062a\u0648\u0627\u0647 \u0645\u0646 \u0627\u0644\u0646\u064a\u0643\u0644.<\/p><h3 class=\"wp-block-heading\">\u0647\u0644 \u064a\u0645\u0643\u0646 \u0644\u062d\u0627\u0645 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201\u061f<\/h3><p class=\"wp-block-paragraph\">\u0646\u0639\u0645\u060c \u064a\u0645\u0643\u0646 \u0644\u062d\u0627\u0645 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201\u060c \u0648\u0644\u0643\u0646 \u0627\u0644\u0623\u0645\u0631 \u064a\u062a\u0637\u0644\u0628 \u062a\u0642\u0646\u064a\u0627\u062a \u0648\u0627\u0639\u062a\u0628\u0627\u0631\u0627\u062a \u0645\u0646\u0627\u0633\u0628\u0629 \u0628\u0633\u0628\u0628 \u0645\u062d\u062a\u0648\u0627\u0647 \u0627\u0644\u0645\u0646\u062e\u0641\u0636 \u0645\u0646 \u0627\u0644\u0646\u064a\u0643\u0644 \u0645\u0642\u0627\u0631\u0646\u0629 \u0628\u0623\u0646\u0648\u0627\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0623\u062e\u0631\u0649.<\/p><h3 class=\"wp-block-heading\">\u0647\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201 \u062c\u064a\u062f \u0644\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u062e\u0627\u0631\u062c\u064a\u061f<\/h3><p class=\"wp-block-paragraph\">\u0644\u0627\u060c \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201 \u0644\u064a\u0633 \u0645\u062b\u0627\u0644\u064a\u064b\u0627 \u0644\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u062e\u0627\u0631\u062c\u064a \u0644\u0623\u0646\u0647 \u0623\u0642\u0644 \u0645\u0642\u0627\u0648\u0645\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0645\u0642\u0627\u0631\u0646\u0629 \u0628\u0623\u0646\u0648\u0627\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0623\u062e\u0631\u0649 \u0645\u062b\u0644 304 \u0623\u0648 316. \u0648\u0642\u062f \u064a\u0635\u062f\u0623 \u0641\u064a \u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u062e\u0627\u0631\u062c\u064a\u0629 \u0627\u0644\u0642\u0627\u0633\u064a\u0629.<\/p><h2 class=\"wp-block-heading\">\u0627\u0644\u0645\u0644\u062e\u0635 \u0648 \u0627\u0644\u0645\u0632\u064a\u062f<\/h2><p class=\"wp-block-paragraph\">\u062a\u0634\u0631\u062d \u0647\u0630\u0647 \u0627\u0644\u0645\u0642\u0627\u0644\u0629 \u0628\u0625\u064a\u062c\u0627\u0632 \u062a\u0639\u0631\u064a\u0641 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 201 \u0648\u062a\u0631\u0643\u064a\u0628\u0647 \u0648\u062e\u0635\u0627\u0626\u0635\u0647 \u0648\u0645\u0639\u0627\u0644\u062c\u062a\u0647 \u0648\u062a\u0637\u0628\u064a\u0642\u0627\u062a\u0647 \u0648\u063a\u064a\u0631 \u0630\u0644\u0643 \u0645\u0646 \u0627\u0644\u062c\u0648\u0627\u0646\u0628 \u0627\u0644\u0645\u0647\u0645\u0629. \u0644\u0645\u0639\u0631\u0641\u0629 \u0627\u0644\u0645\u0632\u064a\u062f \u0639\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0623\u0648 \u0623\u0646\u0648\u0627\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0623\u062e\u0631\u0649\u060c \u0631\u0627\u062c\u0639 <a href=\"https:\/\/steelprogroup.com\/ar\/blog\/\" target=\"_blank\" rel=\"noreferrer noopener\">\u0645\u062f\u0648\u0646\u062a\u0646\u0627<\/a> \u0623\u0648 <a href=\"https:\/\/steelprogroup.com\/ar\/contact-us\/\" target=\"_blank\" rel=\"noreferrer noopener\">\u0627\u062a\u0635\u0644 \u0628\u062e\u0628\u0631\u0627\u0626\u0646\u0627 \u0641\u064a \u0645\u062c\u0627\u0644 \u0627\u0644\u0645\u0639\u0627\u062f\u0646<\/a>.<br>\u0628\u0627\u0639\u062a\u0628\u0627\u0631\u0647\u0627 \u0634\u0631\u0643\u0629 \u0631\u0627\u0626\u062f\u0629 \u0641\u064a \u062a\u0635\u0646\u064a\u0639 \u0648\u062a\u0648\u0631\u064a\u062f \u062d\u0644\u0648\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u062a\u062e\u0635\u0635\u060c \u062a\u0642\u062f\u0645 SteelPRO \u062d\u0644\u0648\u0644 \u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0645\u062a\u0639\u062f\u062f\u0629 \u0627\u0644\u0635\u0646\u0627\u0639\u0627\u062a \u0648\u062e\u062f\u0645\u0627\u062a \u0645\u062e\u0635\u0635\u0629. \u0646\u062d\u0646 \u0646\u0636\u0645\u0646 \u062c\u0648\u062f\u0629 \u0645\u0646\u062a\u062c 100% \u0648\u0646\u0644\u062a\u0632\u0645 \u0628\u0627\u0644\u0646\u0645\u0648 \u0645\u0639 \u0639\u0645\u0644\u0627\u0626\u0646\u0627. \u0642\u0645 \u0628\u0632\u064a\u0627\u0631\u0629 <a href=\"https:\/\/steelprogroup.com\/ar\" target=\"_blank\" rel=\"noreferrer noopener\">\u0645\u0648\u0642\u0639\u0646\u0627<\/a> \u0644\u062a\u0639\u0644\u0645 \u0627\u0644\u0645\u0632\u064a\u062f\u060c \u0623\u0648 <a href=\"https:\/\/steelprogroup.com\/ar\/contact-us\/\" target=\"_blank\" rel=\"noreferrer noopener\">\u0623\u0631\u0633\u0644 \u0644\u0646\u0627 \u0627\u0633\u062a\u0641\u0633\u0627\u0631<\/a>\u0633\u0648\u0641 \u0646\u062a\u0635\u0644 \u0628\u0643 \u0642\u0631\u064a\u0628\u0627!<\/p>","protected":false},"excerpt":{"rendered":"<p>\u062a\u0642\u062f\u0645 \u0645\u062c\u0645\u0648\u0639\u0629 SteelPRO \u0645\u0646\u062a\u062c\u0627\u062a SS 201 (UNS S20100\/EN 1.4372) \u0627\u0644\u0645\u062e\u0632\u0646\u0629 \u0645\u0628\u0627\u0634\u0631\u0629 \u0645\u0646 \u0627\u0644\u0645\u0635\u0646\u0639: \u0635\u0641\u0627\u0626\u062d\u060c \u0635\u0641\u0627\u0626\u062d\u060c \u0644\u0641\u0627\u0626\u0641\u060c \u0623\u0634\u0631\u0637\u0629\u060c \u0631\u0642\u0627\u0626\u0642 \u0645\u0639\u062f\u0646\u064a\u0629\u060c \u0623\u0646\u0627\u0628\u064a\u0628\u060c \u0642\u0636\u0628\u0627\u0646\u060c [\u2026]<\/p>","protected":false},"author":1,"featured_media":11578,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"_eb_attr":"","rank_math_lock_modified_date":false,"site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"categories":[4191,112],"tags":[],"class_list":["post-11577","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-grades","category-stainless-steel"],"acf":[],"_links":{"self":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts\/11577","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/comments?post=11577"}],"version-history":[{"count":0,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts\/11577\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/media\/11578"}],"wp:attachment":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/media?parent=11577"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/categories?post=11577"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/tags?post=11577"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}