{"id":20179,"date":"2025-01-03T09:04:00","date_gmt":"2025-01-03T01:04:00","guid":{"rendered":"https:\/\/steelprogroup.com\/?p=20179"},"modified":"2025-01-14T11:35:00","modified_gmt":"2025-01-14T03:35:00","slug":"5160","status":"publish","type":"post","link":"https:\/\/steelprogroup.com\/ar\/tool-steel\/grades\/5160\/","title":{"rendered":"\u0641\u0648\u0644\u0627\u0630 \u0632\u0646\u0628\u0631\u0643\u064a \u0639\u0627\u0644\u064a \u0627\u0644\u0643\u0631\u0628\u0648\u0646 5160: \u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0648\u0627\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0627\u062a \u0648\u0627\u0644\u0645\u0646\u062a\u062c\u0627\u062a"},"content":{"rendered":"<p class=\"wp-block-paragraph\">\u0641\u064a SteelPro Group\u060c \u0646\u062d\u0646 \u0645\u062a\u062e\u0635\u0635\u0648\u0646 \u0641\u064a \u062a\u0648\u0631\u064a\u062f \u0627\u0644\u0641\u0648\u0644\u0627\u0630 1045 \u0639\u0627\u0644\u064a \u0627\u0644\u062c\u0648\u062f\u0629\u060c \u0627\u0644\u0645\u062a\u0648\u0641\u0631 \u0628\u0623\u0634\u0643\u0627\u0644 \u0645\u062e\u062a\u0644\u0641\u0629 \u0628\u0645\u0627 \u0641\u064a \u0630\u0644\u0643 \u0623\u0644\u0648\u0627\u062d \u0648\u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630. \u0646\u062d\u0646 \u0646\u0642\u062f\u0645 \u062d\u0644\u0648\u0644\u0627\u064b \u0645\u062a\u0639\u062f\u062f\u0629 \u0627\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0627\u062a \u0645\u062b\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u062f\u0631\u0641\u0644 \u0639\u0644\u0649 \u0627\u0644\u0633\u0627\u062e\u0646 \u0623\u0648 \u0627\u0644\u0628\u0627\u0631\u062f \u0623\u0648 \u0627\u0644\u0645\u064f\u0644\u064e\u062f\u064e\u0651\u0646 \u0644\u062a\u0644\u0628\u064a\u0629 \u0645\u062a\u0637\u0644\u0628\u0627\u062a\u0643 \u0627\u0644\u0645\u062d\u062f\u062f\u0629.&nbsp;<\/p><h2 class=\"wp-block-heading\">\u0645\u0627 \u0647\u0648 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0643\u0631\u0628\u0648\u0646\u064a 5160\u061f<\/h2><p class=\"wp-block-paragraph\">\u0627\u0644\u0641\u0648\u0644\u0627\u0630 5160 \u0639\u0628\u0627\u0631\u0629 \u0639\u0646 \u0633\u0628\u064a\u0643\u0629 \u0643\u0631\u0648\u0645 \u0639\u0627\u0644\u064a\u0629 \u0627\u0644\u0643\u0631\u0628\u0648\u0646 \u062a\u0633\u062a\u062e\u062f\u0645 \u0628\u0634\u0643\u0644 \u0623\u0633\u0627\u0633\u064a \u0641\u064a \u0627\u0644\u064a\u0646\u0627\u0628\u064a\u0639\u060c \u0648\u0647\u064a \u0645\u0639\u0631\u0648\u0641\u0629 \u0628\u0642\u0648\u062a\u0647\u0627 \u0648\u0645\u0631\u0648\u0646\u062a\u0647\u0627 \u0648\u0645\u0642\u0627\u0648\u0645\u062a\u0647\u0627 \u0644\u0644\u062a\u0639\u0628. \u062a\u064f\u0633\u062a\u062e\u062f\u0645 \u0628\u0634\u0643\u0644 \u0623\u0633\u0627\u0633\u064a \u0641\u064a \u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u064a\u0646\u0627\u0628\u064a\u0639 \u0627\u0644\u062b\u0642\u064a\u0644\u0629 \u0641\u064a \u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a\u060c \u0648\u062e\u0627\u0635\u0629 \u0627\u0644\u064a\u0646\u0627\u0628\u064a\u0639 \u0627\u0644\u0648\u0631\u0642\u064a\u0629\u060c \u0648\u0641\u064a \u0625\u0646\u062a\u0627\u062c \u0627\u0644\u0633\u0643\u0627\u0643\u064a\u0646 \u0648\u0627\u0644\u0633\u064a\u0648\u0641. \u064a\u062a\u0637\u0644\u0628 \u0627\u0644\u0623\u0645\u0631 \u0627\u0647\u062a\u0645\u0627\u0645\u064b\u0627 \u062e\u0627\u0635\u064b\u0627 \u0623\u062b\u0646\u0627\u0621 \u0627\u0644\u0644\u062d\u0627\u0645 \u0648\u0627\u0644\u062a\u0634\u063a\u064a\u0644 \u0628\u0633\u0628\u0628 \u0642\u0627\u0628\u0644\u064a\u062a\u0647\u0627 \u0644\u0644\u062a\u0635\u0644\u0628.<\/p><h2 class=\"wp-block-heading\">\u0625\u064a\u062c\u0627\u0628\u064a\u0627\u062a \u0648\u0633\u0644\u0628\u064a\u0627\u062a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0643\u0631\u0628\u0648\u0646\u064a 5160<\/h2><h3 class=\"wp-block-heading\">\u0645\u0645\u064a\u0632\u0627\u062a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0643\u0631\u0628\u0648\u0646\u064a 5160<\/h3><p class=\"wp-block-paragraph\"><strong>\u0635\u0644\u0627\u0628\u0629 \u0639\u0627\u0644\u064a\u0629<\/strong>:\u0645\u0642\u0627\u0648\u0645\u0629 \u0645\u0645\u062a\u0627\u0632\u0629 \u0644\u0623\u062d\u0645\u0627\u0644 \u0627\u0644\u0635\u062f\u0645\u0627\u062a \u0648\u0627\u0644\u062a\u0623\u062b\u064a\u0631\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647\u0627 \u0645\u062b\u0627\u0644\u064a\u0629 \u0644\u0644\u0623\u062c\u0632\u0627\u0621 \u0627\u0644\u062b\u0642\u064a\u0644\u0629 \u0645\u062b\u0644 \u0645\u0643\u0648\u0646\u0627\u062a \u0627\u0644\u062a\u0639\u0644\u064a\u0642 \u0648\u0646\u0648\u0627\u0628\u0636 \u0627\u0644\u0623\u0648\u0631\u0627\u0642.<\/p><p class=\"wp-block-paragraph\"><strong>\u0645\u0642\u0627\u0648\u0645\u0629 \u062c\u064a\u062f\u0629 \u0644\u0644\u062a\u0622\u0643\u0644<\/strong>:\u064a\u0648\u0641\u0631 \u062a\u0648\u0627\u0632\u0646\u064b\u0627 \u0642\u0648\u064a\u064b\u0627 \u0628\u064a\u0646 \u0627\u0644\u0635\u0644\u0627\u0628\u0629 \u0648\u0627\u0644\u0645\u062a\u0627\u0646\u0629 \u0628\u0639\u062f \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629\u060c \u0648\u0647\u0648 \u0645\u0646\u0627\u0633\u0628 \u0644\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0630\u0627\u062a \u0627\u0644\u0627\u062d\u062a\u0643\u0627\u0643 \u0627\u0644\u0639\u0627\u0644\u064a \u0645\u062b\u0644 \u0627\u0644\u0623\u062f\u0648\u0627\u062a \u0648\u0627\u0644\u062a\u0631\u0648\u0633.<\/p><p class=\"wp-block-paragraph\"><strong>\u0641\u0639\u0627\u0644\u0629 \u0645\u0646 \u062d\u064a\u062b \u0627\u0644\u062a\u0643\u0644\u0641\u0629<\/strong>:\u064a\u0648\u0641\u0631 \u062e\u0635\u0627\u0626\u0635 \u0645\u064a\u0643\u0627\u0646\u064a\u0643\u064a\u0629 \u0642\u0648\u064a\u0629 \u0628\u062a\u0643\u0644\u0641\u0629 \u0623\u0642\u0644 \u0645\u0642\u0627\u0631\u0646\u0629 \u0628\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0630\u064a \u0627\u0644\u0633\u0628\u0627\u0626\u0643 \u0627\u0644\u0623\u0639\u0644\u0649.<\/p><p class=\"wp-block-paragraph\"><strong>\u0642\u0627\u0628\u0644\u0629 \u0644\u0644\u062a\u0634\u0643\u064a\u0644 \u0628\u0639\u062f \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629<\/strong>:\u064a\u062d\u062a\u0641\u0638 \u0628\u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0645\u064a\u0643\u0627\u0646\u064a\u0643\u064a\u0629 \u0627\u0644\u0645\u0631\u063a\u0648\u0628\u0629 \u0644\u0644\u0623\u0634\u0643\u0627\u0644 \u0627\u0644\u0645\u0639\u0642\u062f\u0629 \u0648\u0627\u0644\u0645\u0643\u0648\u0646\u0627\u062a \u0639\u0627\u0644\u064a\u0629 \u0627\u0644\u0636\u063a\u0637.<\/p><h3 class=\"wp-block-heading\">\u0639\u064a\u0648\u0628 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0643\u0631\u0628\u0648\u0646\u064a 5160<\/h3><p class=\"wp-block-paragraph\"><strong>\u0645\u0639\u0631\u0636 \u0644\u0644\u062a\u0622\u0643\u0644 \u0628\u062f\u0648\u0646 \u0637\u0644\u0627\u0621 \u0648\u0627\u0642\u064a<\/strong>:\u064a\u062a\u0637\u0644\u0628 \u0637\u0644\u0627\u0621\u0627\u062a \u0648\u0627\u0642\u064a\u0629 \u0623\u0648 \u0635\u064a\u0627\u0646\u0629 \u0645\u0646\u062a\u0638\u0645\u0629 \u0644\u0645\u0646\u0639 \u0627\u0644\u0635\u062f\u0623<\/p><p class=\"wp-block-paragraph\"><strong>\u0627\u0633\u062a\u0642\u0631\u0627\u0631 \u0645\u062d\u062f\u0648\u062f \u0641\u064a \u062f\u0631\u062c\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u0639\u0627\u0644\u064a\u0629<\/strong>:\u064a\u062a\u0645\u064a\u0632 5160 \u0628\u0645\u0642\u0627\u0648\u0645\u0629 \u0645\u0646\u062e\u0641\u0636\u0629 \u0644\u0644\u062a\u0644\u0637\u064a\u0641 \u0639\u0646\u062f \u062f\u0631\u062c\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u0645\u0631\u062a\u0641\u0639\u0629. \u0641\u0647\u0648 \u064a\u0644\u064a\u0646 \u0648\u064a\u0641\u0642\u062f \u0635\u0644\u0627\u0628\u062a\u0647 \u0639\u0646\u062f \u062f\u0631\u062c\u0627\u062a \u062d\u0631\u0627\u0631\u0629 \u062a\u062a\u062c\u0627\u0648\u0632 400 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629\u060c \u0648\u0647\u0648 \u0623\u0642\u0644 \u0645\u0644\u0627\u0621\u0645\u0629 \u0644\u0644\u0628\u064a\u0626\u0627\u062a \u0630\u0627\u062a \u062f\u0631\u062c\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u0645\u0631\u062a\u0641\u0639\u0629.<\/p><p class=\"wp-block-paragraph\"><strong>\u0647\u0634 \u0641\u064a \u062f\u0631\u062c\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u0645\u0646\u062e\u0641\u0636\u0629<\/strong>:\u062a\u0642\u0644 \u0642\u0648\u0629 \u062a\u062d\u0645\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 5160 \u0644\u0644\u0635\u062f\u0645\u0627\u062a \u0628\u0634\u0643\u0644 \u0643\u0628\u064a\u0631 \u0641\u064a \u062f\u0631\u062c\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u0645\u0646\u062e\u0641\u0636\u0629 \u0644\u0644\u063a\u0627\u064a\u0629.<\/p><p class=\"wp-block-paragraph\"><strong>\u0627\u0646\u062e\u0641\u0627\u0636 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0639\u0628<\/strong>:\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0639\u0628 \u0641\u064a 5160 \u0623\u0642\u0644 \u0645\u0646 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0630\u064a \u0627\u0644\u0633\u0628\u0627\u0626\u0643 \u0627\u0644\u0623\u0639\u0644\u0649 \u0645\u062b\u0644 4340 \u0623\u0648 8620\u060c \u0648\u062e\u0627\u0635\u0629 \u0641\u064a \u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u062a\u062d\u0645\u064a\u0644 \u0627\u0644\u062f\u0648\u0631\u064a.<\/p><h2 class=\"wp-block-heading\">\u0645\u0627 \u064a\u0639\u0627\u062f\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 5160<\/h2><p class=\"wp-block-paragraph\">\u0648\u0641\u064a\u0645\u0627 \u064a\u0644\u064a \u0627\u0644\u0645\u0643\u0627\u0641\u0626\u0627\u062a \u0644\u0644\u0641\u0648\u0644\u0627\u0630 5160:<\/p><ul class=\"wp-block-list\"><li>\u0631\u0642\u0645 \u0627\u0644\u0623\u0645\u0645 \u0627\u0644\u0645\u062a\u062d\u062f\u0629: G10950<\/li>\n\n<li>ASTM A29\/A29M: 1095<\/li>\n\n<li>DIN 17222\/EN: Ck101\/1.1274<\/li>\n\n<li>JIS G4801: SUP4<\/li><\/ul><h2 class=\"wp-block-heading\">5160 \u0623\u0634\u0643\u0627\u0644 \u0648\u062a\u0634\u0643\u064a\u0644\u0627\u062a \u0645\u0646\u062a\u062c\u0627\u062a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0632\u0646\u0628\u0631\u0643\u064a<\/h2><p class=\"wp-block-paragraph\">\u062a\u0642\u062f\u0645 \u0645\u062c\u0645\u0648\u0639\u0629 SteelPro \u0645\u062c\u0645\u0648\u0639\u0629 \u0645\u062a\u0646\u0648\u0639\u0629 \u0645\u0646 \u0623\u0634\u0643\u0627\u0644 \u0627\u0644\u0645\u0646\u062a\u062c\u0627\u062a\u060c \u0628\u0645\u0627 \u0641\u064a \u0630\u0644\u0643 \u0627\u0644\u0642\u0636\u0628\u0627\u0646 \u0648\u0627\u0644\u0635\u0641\u0627\u0626\u062d \u0648\u0627\u0644\u0623\u0644\u0648\u0627\u062d \u0648\u0627\u0644\u0644\u0641\u0627\u0626\u0641. \u0643\u0645\u0627 \u0646\u0642\u062f\u0645 \u0623\u064a\u0636\u064b\u0627 \u0623\u0628\u0639\u0627\u062f\u064b\u0627 \u0645\u062e\u0635\u0635\u0629.<\/p><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u0646\u0645\u0648\u0630\u062c \u0627\u0644\u0645\u0646\u062a\u062c<\/strong><\/td><td><strong>\u0646\u0637\u0627\u0642 \u0627\u0644\u0633\u064f\u0645\u0643\/\u0627\u0644\u0642\u0637\u0631<\/strong><\/td><td><strong>\u0646\u0637\u0627\u0642 \u0627\u0644\u0639\u0631\u0636<\/strong><\/td><td><strong>\u0645\u062f\u0649 \u0627\u0644\u0637\u0648\u0644<\/strong><\/td><\/tr><tr><td>\u0642\u0636\u0628\u0627\u0646 \u0645\u0633\u062a\u062f\u064a\u0631\u0629<\/td><td>10 \u0645\u0644\u0645 (0.39 \u0628\u0648\u0635\u0629) \u0625\u0644\u0649 300 \u0645\u0644\u0645 (11.81 \u0628\u0648\u0635\u0629)<\/td><td>&#8211;<\/td><td>3000 \u0645\u0644\u0645 (118 \u0628\u0648\u0635\u0629) \u0625\u0644\u0649 6000 \u0645\u0644\u0645 (236 \u0628\u0648\u0635\u0629)<\/td><\/tr><tr><td>\u0642\u0636\u0628\u0627\u0646 \u0645\u0633\u0637\u062d\u0629<\/td><td>3 \u0645\u0645 (0.12 \u0628\u0648\u0635\u0629) \u0625\u0644\u0649 80 \u0645\u0645 (3.15 \u0628\u0648\u0635\u0629)<\/td><td>20 \u0645\u0644\u0645 (0.79 \u0628\u0648\u0635\u0629) \u0625\u0644\u0649 300 \u0645\u0644\u0645 (11.81 \u0628\u0648\u0635\u0629)<\/td><td>3000 \u0645\u0644\u0645 (118 \u0628\u0648\u0635\u0629) \u0625\u0644\u0649 6000 \u0645\u0644\u0645 (236 \u0628\u0648\u0635\u0629)<\/td><\/tr><tr><td>\u0627\u0644\u0635\u0641\u0627\u0626\u062d \u0648\u0627\u0644\u0623\u0644\u0648\u0627\u062d<\/td><td>3 \u0645\u0645 (0.12 \u0628\u0648\u0635\u0629) \u0625\u0644\u0649 100 \u0645\u0645 (3.94 \u0628\u0648\u0635\u0629)<\/td><td>1000 \u0645\u0644\u0645 (39.37 \u0628\u0648\u0635\u0629) \u0625\u0644\u0649 2000 \u0645\u0644\u0645 (78.74 \u0628\u0648\u0635\u0629)<\/td><td>2500 \u0645\u0644\u0645 (98.43 \u0628\u0648\u0635\u0629) \u0625\u0644\u0649 6000 \u0645\u0644\u0645 (236 \u0628\u0648\u0635\u0629)<\/td><\/tr><tr><td>\u0627\u0644\u0645\u0644\u0641\u0627\u062a<\/td><td>1.5 \u0645\u0644\u0645 (0.06 \u0628\u0648\u0635\u0629) \u0625\u0644\u0649 6 \u0645\u0644\u0645 (0.24 \u0628\u0648\u0635\u0629)<\/td><td>1000 \u0645\u0644\u0645 (39.37 \u0628\u0648\u0635\u0629) \u0625\u0644\u0649 1500 \u0645\u0644\u0645 (59.06 \u0628\u0648\u0635\u0629)<\/td><td>&#8211;<\/td><\/tr><tr><td>\u0642\u0636\u0628\u0627\u0646 \u0645\u0632\u0648\u0631\u0629<\/td><td>20 \u0645\u0644\u0645 (0.79 \u0628\u0648\u0635\u0629) \u0625\u0644\u0649 250 \u0645\u0644\u0645 (9.84 \u0628\u0648\u0635\u0629)<\/td><td>&#8211;<\/td><td>3000 \u0645\u0644\u0645 (118 \u0628\u0648\u0635\u0629) \u0625\u0644\u0649 6000 \u0645\u0644\u0645 (236 \u0628\u0648\u0635\u0629)<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u0627\u0644\u062a\u0631\u0643\u064a\u0628 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0643\u0631\u0628\u0648\u0646\u064a 5160<\/h2><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u0639\u0646\u0635\u0631<\/strong><\/td><td><strong>\u062a\u0639\u0628\u064a\u0631<\/strong><\/td><\/tr><tr><td>\u0627\u0644\u0643\u0631\u0628\u0648\u0646 (C)<\/td><td>0.56 &#8211; 0.64 %<\/td><\/tr><tr><td>\u0627\u0644\u0643\u0631\u0648\u0645 (Cr)<\/td><td>0.70 &#8211; 0.90 %<\/td><\/tr><tr><td>\u0627\u0644\u062d\u062f\u064a\u062f (Fe)<\/td><td>97.085 &#8211; 97.84 %<\/td><\/tr><tr><td>\u0627\u0644\u0645\u0646\u063a\u0646\u064a\u0632 (Mn)<\/td><td>0.75 &#8211; 1.0 %<\/td><\/tr><tr><td>\u0627\u0644\u0641\u0648\u0633\u0641\u0648\u0631 (P)<\/td><td>\u2264 0.035 %<\/td><\/tr><tr><td>\u0627\u0644\u0633\u064a\u0644\u064a\u0643\u0648\u0646 (Si)<\/td><td>0.15 &#8211; 0.30 %<\/td><\/tr><tr><td>\u0627\u0644\u0643\u0628\u0631\u064a\u062a (S)<\/td><td>\u2264 0.040 %<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0641\u064a\u0632\u064a\u0627\u0626\u064a\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0643\u0631\u0628\u0648\u0646\u064a 5160<\/h2><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u0645\u0644\u0643\u064a\u0629<\/strong><\/td><td><strong>\u0627\u0644\u0642\u064a\u0645\u0629 \u0627\u0644\u0645\u062a\u0631\u064a\u0629<\/strong><\/td><td><strong>\u0627\u0644\u0642\u064a\u0645\u0629 \u0627\u0644\u0625\u0645\u0628\u0631\u0627\u0637\u0648\u0631\u064a\u0629<\/strong><\/td><\/tr><tr><td>\u0643\u062b\u0627\u0641\u0629<\/td><td>7.85 \u062c\u0631\u0627\u0645\/\u0633\u06453<\/td><td>0.284 \u0631\u0637\u0644\/\u0628\u0648\u0635\u0629 \u0645\u0643\u0639\u0628\u0629<\/td><\/tr><tr><td>\u0646\u0642\u0637\u0629 \u0627\u0644\u0627\u0646\u0635\u0647\u0627\u0631<\/td><td>1425 \u2013 1540 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629<\/td><td>2597 \u2013 2800 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a<\/td><\/tr><tr><td>\u0627\u0644\u0645\u0648\u0635\u0644\u064a\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629<\/td><td>42 \u0648\u0627\u0637\/\u0645\u00b7\u0643<\/td><td>24 \u0648\u062d\u062f\u0629 \u062d\u0631\u0627\u0631\u064a\u0629 \u0628\u0631\u064a\u0637\u0627\u0646\u064a\u0629\/\u0633\u0627\u0639\u0629 \u0642\u062f\u0645 \u0645\u0643\u0639\u0628 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a<\/td><\/tr><tr><td>\u0627\u0644\u0633\u0639\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629 \u0627\u0644\u0646\u0648\u0639\u064a\u0629<\/td><td>46.6 \u0648\u0627\u0637\/\u0645\u062a\u0631 \u0643\u0644\u0641\u0646<\/td><td>323 \u0648\u062d\u062f\u0629 \u062d\u0631\u0627\u0631\u064a\u0629 \u0628\u0631\u064a\u0637\u0627\u0646\u064a\u0629\/\u0633\u0627\u0639\u0629\/\u0642\u062f\u0645 \u0645\u0631\u0628\u0639-\u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a<\/td><\/tr><tr><td>\u0627\u0644\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u0643\u0647\u0631\u0628\u0627\u0626\u064a\u0629<\/td><td>0.0000219 \u0623\u0648\u0645-\u0633\u0645<\/td><td>0.0000219 \u0623\u0648\u0645-\u0633\u0645<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u0627\u0644\u062e\u0648\u0627\u0635 \u0627\u0644\u0645\u064a\u0643\u0627\u0646\u064a\u0643\u064a\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0643\u0631\u0628\u0648\u0646\u064a 5160<\/h2><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u0645\u0644\u0643\u064a\u0629<\/strong><\/td><td><strong>\u0627\u0644\u0642\u064a\u0645\u0629 \u0627\u0644\u0645\u062a\u0631\u064a\u0629<\/strong><\/td><td><strong>\u0627\u0644\u0642\u064a\u0645\u0629 \u0627\u0644\u0625\u0645\u0628\u0631\u0627\u0637\u0648\u0631\u064a\u0629<\/strong><\/td><\/tr><tr><td>\u0642\u0648\u0629 \u0627\u0644\u0634\u062f<\/td><td>930 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644<\/td><td>135000 \u0631\u0637\u0644\/\u0628\u0648\u0635\u0629 \u0645\u0631\u0628\u0639\u0629<\/td><\/tr><tr><td>\u0642\u0648\u0629 \u0627\u0644\u062e\u0636\u0648\u0639<\/td><td>690 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644<\/td><td>100000 \u0631\u0637\u0644 \u0644\u0643\u0644 \u0628\u0648\u0635\u0629 \u0645\u0631\u0628\u0639\u0629<\/td><\/tr><tr><td>\u0627\u0633\u062a\u0637\u0627\u0644\u0629<\/td><td>0.12<\/td><td>0.12<\/td><\/tr><tr><td>\u0627\u0644\u0635\u0644\u0627\u0628\u0629 (HRC)<\/td><td>57 \u2013 58 \u0633\u0627\u0639\u0629 \u0645\u0639\u062a\u0645\u062f\u0629<\/td><td>57 \u2013 58 \u0633\u0627\u0639\u0629 \u0645\u0639\u062a\u0645\u062f\u0629<\/td><\/tr><tr><td>\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0623\u062b\u064a\u0631 (\u0634\u0642 \u0639\u0644\u0649 \u0634\u0643\u0644 \u062d\u0631\u0641 V \u0639\u0646\u062f -20 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \/ -4 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/td><td>30 \u2013 40 \u062c<\/td><td>22 \u2013 29 \u0642\u062f\u0645-\u0631\u0637\u0644<\/td><\/tr><tr><td>\u0645\u0639\u0627\u0645\u0644 \u0627\u0644\u0645\u0631\u0648\u0646\u0629<\/td><td>190-210 \u062c\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644<\/td><td>27557-30458 \u0643.\u0633.<\/td><\/tr><tr><td>\u0645\u0639\u0627\u0645\u0644 \u0627\u0644\u062d\u062c\u0645<\/td><td>160 \u062c\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644<\/td><td>23200 \u0643\u064a\u0644\u0648 \u0628\u0627\u0633\u0643\u0627\u0644<\/td><\/tr><tr><td>\u0646\u0633\u0628\u0629 \u0628\u0648\u0627\u0633\u0648\u0646<\/td><td>0.29<\/td><td>0.29<\/td><\/tr><tr><td>\u0642\u0627\u0628\u0644\u064a\u0629 \u0627\u0644\u062a\u0635\u0646\u064a\u0639<\/td><td>55 %<\/td><td>55 %<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u0643\u064a\u0641\u064a\u0629 \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 5160\u061f<\/h2><h3 class=\"wp-block-heading\">\u0627\u0644\u062a\u0644\u062f\u064a\u0646<\/h3><p class=\"wp-block-paragraph\">\u0628\u0627\u0644\u0646\u0633\u0628\u0629 \u0644\u0644\u0635\u0644\u0628 \u0627\u0644\u0623\u0643\u062b\u0631 \u0644\u064a\u0648\u0646\u0629\u060c \u0648\u062e\u0627\u0635\u0629 \u0639\u0646\u062f\u0645\u0627 \u064a\u0643\u0648\u0646 \u0627\u0644\u062a\u0634\u0643\u064a\u0644 \u0623\u0648 \u0627\u0644\u062a\u0635\u0646\u064a\u0639 \u0645\u0637\u0644\u0648\u0628\u064b\u0627\u060c \u0642\u0645 \u0628\u062a\u0644\u062f\u064a\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0639\u0646 \u0637\u0631\u064a\u0642 \u062a\u0633\u062e\u064a\u0646\u0647 \u0625\u0644\u0649 \u062d\u0648\u0627\u0644\u064a <strong>700 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (1292 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/strong> \u0648\u0627\u0644\u0627\u062d\u062a\u0641\u0627\u0638 \u0628\u0647\u0627 <strong>1-2 \u0633\u0627\u0639\u0629<\/strong>. \u062b\u0645 \u0627\u062a\u0631\u0643 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u064a\u0628\u0631\u062f \u062a\u062f\u0631\u064a\u062c\u064a\u064b\u0627 \u0641\u064a \u0627\u0644\u0641\u0631\u0646 \u0623\u0648 \u0628\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u062a\u0628\u0631\u064a\u062f \u0627\u0644\u0647\u0648\u0627\u0626\u064a \u0627\u0644\u0645\u062a\u062d\u0643\u0645 \u0641\u064a\u0647. \u0647\u0630\u0647 \u0627\u0644\u0637\u0631\u064a\u0642\u0629 \u062a\u0639\u0645\u0644 \u0639\u0644\u0649 \u062a\u0644\u064a\u064a\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647 \u0623\u0633\u0647\u0644 \u0641\u064a \u0627\u0644\u062a\u0639\u0627\u0645\u0644 \u0645\u0639\u0647.<\/p><h3 class=\"wp-block-heading\">\u0627\u0644\u062a\u0635\u0644\u0628<\/h3><h4 class=\"wp-block-heading\"><strong>\u0627\u0644\u062a\u0633\u062e\u064a\u0646 \u0627\u0644\u0645\u0633\u0628\u0642<\/strong><\/h4><p class=\"wp-block-paragraph\">\u0642\u0628\u0644 \u0639\u0645\u0644\u064a\u0629 \u0627\u0644\u0623\u0648\u0633\u062a\u0646\u064a\u062a\u060c \u0642\u0645 \u0628\u062a\u0633\u062e\u064a\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0645\u0633\u0628\u0642\u064b\u0627 \u0625\u0644\u0649 <strong>500 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (932 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/strong> \u0644 <strong>700 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (1292 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/strong>\u064a\u0633\u0627\u0639\u062f \u0647\u0630\u0627 \u0627\u0644\u062a\u0633\u062e\u064a\u0646 \u0627\u0644\u062a\u062f\u0631\u064a\u062c\u064a \u0639\u0644\u0649 \u062a\u0642\u0644\u064a\u0644 \u0627\u0644\u0635\u062f\u0645\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629 \u0623\u062b\u0646\u0627\u0621 \u0627\u0644\u062a\u0628\u0631\u064a\u062f \u0648\u064a\u0636\u0645\u0646 \u062a\u0648\u0632\u064a\u0639\u064b\u0627 \u0623\u0643\u062b\u0631 \u062a\u0646\u0627\u0633\u0642\u064b\u0627 \u0644\u062f\u0631\u062c\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0641\u064a \u062c\u0645\u064a\u0639 \u0623\u0646\u062d\u0627\u0621 \u0627\u0644\u0641\u0648\u0644\u0627\u0630.<\/p><h4 class=\"wp-block-heading\"><strong>\u0627\u0644\u062a\u0633\u062e\u064a\u0646 \u0628\u0627\u0644\u0623\u0633\u062a\u064a\u0646\u064a\u062a<\/strong><\/h4><p class=\"wp-block-paragraph\">\u0642\u0645 \u0628\u062a\u0633\u062e\u064a\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 5160 \u0625\u0644\u0649 \u0646\u0637\u0627\u0642 \u062f\u0631\u062c\u0629 \u062d\u0631\u0627\u0631\u0629 <strong>800 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (1472 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/strong> \u0644 <strong>850 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (1562 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/strong> \u0644\u0645\u062f\u0629 \u062a\u0642\u0631\u064a\u0628\u064a\u0629 <strong>10-15 \u062f\u0642\u064a\u0642\u0629<\/strong>\u064a\u0624\u062f\u064a \u0647\u0630\u0627 \u0625\u0644\u0649 \u062a\u062d\u0648\u064a\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0625\u0644\u0649 \u0623\u0648\u0633\u062a\u064a\u0646\u064a\u062a\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647 \u062c\u0627\u0647\u0632\u064b\u0627 \u0644\u0644\u062a\u0635\u0644\u0628.<\/p><p class=\"wp-block-paragraph\"><strong>\u0625\u062e\u0645\u0627\u062f<\/strong><\/p><p class=\"wp-block-paragraph\">\u0628\u0639\u062f \u0639\u0645\u0644\u064a\u0629 \u0627\u0644\u0623\u0648\u0633\u062a\u0646\u064a\u062a \u0645\u0628\u0627\u0634\u0631\u0629\u060c \u0642\u0645 \u0628\u0625\u062e\u0645\u0627\u062f \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0641\u064a <strong>\u0632\u064a\u062a<\/strong>\u064a\u0633\u0627\u0639\u062f \u0627\u0644\u062a\u0628\u0631\u064a\u062f \u0628\u0627\u0644\u0632\u064a\u062a \u0639\u0644\u0649 \u0645\u0646\u0639 \u0627\u0644\u062a\u0634\u0642\u0642 \u0648\u064a\u0636\u0645\u0646 \u0645\u0639\u062f\u0644 \u062a\u0628\u0631\u064a\u062f \u0623\u0643\u062b\u0631 \u062a\u062d\u0643\u0645\u064b\u0627 \u0645\u0646 \u0627\u0644\u0645\u0627\u0621. \u064a\u062c\u0628 \u0623\u0646 \u064a\u0628\u0631\u062f \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0625\u0644\u0649 <strong>\u062f\u0631\u062c\u0629 \u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u063a\u0631\u0641\u0629<\/strong> (\u062d\u0648\u0644 <strong>20-30 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \/ 68-86 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a<\/strong>).<\/p><h3 class=\"wp-block-heading\">\u0627\u0644\u062a\u0644\u0637\u064a\u0641<\/h3><p class=\"wp-block-paragraph\">\u0642\u0645 \u0628\u062a\u0644\u0637\u064a\u0641 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0639\u0646 \u0637\u0631\u064a\u0642 \u062a\u0633\u062e\u064a\u0646\u0647 \u0625\u0644\u0649 <strong>200 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629<\/strong> <strong>(392 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/strong> \u0644 <strong>300 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (572 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/strong> \u0644 <strong>1-2 \u0633\u0627\u0639\u0629 \u0644\u062a\u0642\u0644\u064a\u0644 \u0627\u0644\u0647\u0634\u0627\u0634\u0629 \u0627\u0644\u0646\u0627\u062a\u062c\u0629 \u0639\u0646 \u0627\u0644\u062a\u0628\u0631\u064a\u062f<\/strong>\u062a\u0639\u0645\u0644 \u0647\u0630\u0647 \u0627\u0644\u0639\u0645\u0644\u064a\u0629 \u0639\u0644\u0649 \u0632\u064a\u0627\u062f\u0629 \u0627\u0644\u0635\u0644\u0627\u0628\u0629 \u062f\u0648\u0646 \u0627\u0644\u062a\u0636\u062d\u064a\u0629 \u0628\u0627\u0644\u0643\u062b\u064a\u0631 \u0645\u0646 \u0627\u0644\u0635\u0644\u0627\u0628\u0629.<\/p><h2 class=\"wp-block-heading\">\u062a\u0635\u0646\u064a\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 5160<\/h2><p class=\"wp-block-paragraph\">\u0646\u0638\u0631\u064b\u0627 \u0644\u0635\u0644\u0627\u0628\u062a\u0647\u060c \u0642\u062f \u064a\u0643\u0648\u0646 \u0645\u0646 \u0627\u0644\u0635\u0639\u0628 \u062a\u0634\u063a\u064a\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 5160. \u0644\u062a\u0644\u064a\u064a\u0646\u0647 \u0648\u062a\u062d\u0633\u064a\u0646 \u0642\u0627\u0628\u0644\u064a\u0629 \u0627\u0644\u062a\u0634\u063a\u064a\u0644\u060c \u0645\u0646 \u0627\u0644\u0623\u0641\u0636\u0644 \u0627\u0633\u062a\u062e\u062f\u0627\u0645 <strong>\u0627\u0644\u062a\u0644\u062f\u064a\u0646<\/strong> \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0642\u0628\u0644 \u0627\u0644\u0642\u0637\u0639. \u0627\u0633\u062a\u062e\u062f\u0645 <strong>HSSS<\/strong> \u0623\u0648 <strong>\u0623\u062f\u0648\u0627\u062a \u0643\u0631\u0628\u064a\u062f<\/strong> \u0645\u0639 \u0633\u0631\u0639\u0627\u062a \u0642\u0637\u0639 \u0623\u0628\u0637\u0623 \u0648\u062a\u0628\u0631\u064a\u062f \u0645\u0646\u0627\u0633\u0628 \u0644\u0645\u0646\u0639 \u062a\u0622\u0643\u0644 \u0627\u0644\u0623\u062f\u0627\u0629.<\/p><h2 class=\"wp-block-heading\">\u0644\u062d\u0627\u0645 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 5160<\/h2><p class=\"wp-block-paragraph\">\u064a\u0645\u0643\u0646 \u0623\u0646 \u064a\u0643\u0648\u0646 \u0644\u062d\u0627\u0645 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 5160 \u0623\u0645\u0631\u064b\u0627 \u0635\u0639\u0628\u064b\u0627 \u0628\u0633\u0628\u0628 \u0645\u062d\u062a\u0648\u0627\u0647 \u0627\u0644\u0639\u0627\u0644\u064a \u0645\u0646 \u0627\u0644\u0643\u0631\u0628\u0648\u0646 \u0648\u0625\u0645\u0643\u0627\u0646\u064a\u0629 <strong>\u062a\u0643\u0633\u064a\u0631<\/strong> \u0641\u064a \u0627\u0644\u0645\u0646\u0637\u0642\u0629 \u0627\u0644\u0645\u062a\u0623\u062b\u0631\u0629 \u0628\u0627\u0644\u062d\u0631\u0627\u0631\u0629.&nbsp;<\/p><p class=\"wp-block-paragraph\">\u064a\u062a\u0637\u0644\u0628 \u0644\u062d\u0627\u0645 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 5160 \u0627\u0644\u062a\u0633\u062e\u064a\u0646 \u0627\u0644\u0645\u0633\u0628\u0642 <strong>200-300 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (392-572 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/strong> \u0644\u0645\u0646\u0639 \u0627\u0644\u062a\u0634\u0642\u0642. \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629 \u0628\u0639\u062f \u0627\u0644\u0644\u062d\u0627\u0645\u060c \u0645\u062b\u0644 <strong>\u0627\u0644\u062a\u0644\u0637\u064a\u0641<\/strong>\u060c \u063a\u0627\u0644\u0628\u064b\u0627 \u0645\u0627 \u064a\u0643\u0648\u0646 \u0630\u0644\u0643 \u0636\u0631\u0648\u0631\u064a\u064b\u0627 \u0644\u0644\u062d\u0641\u0627\u0638 \u0639\u0644\u0649 \u0627\u0644\u0635\u0644\u0627\u0628\u0629. \u0627\u0633\u062a\u062e\u062f\u0645 <strong>\u0633\u0645\u0627\u0648<\/strong> \u0623\u0648 <strong>\u062c\u064a \u062a\u064a \u0627\u064a\u0647 \u062f\u0628\u0644\u064a\u0648<\/strong> \u0645\u0639 \u0623\u0642\u0637\u0627\u0628 \u0627\u0644\u0647\u064a\u062f\u0631\u0648\u062c\u064a\u0646 \u0627\u0644\u0645\u0646\u062e\u0641\u0636\u0629 \u0644\u062a\u0642\u0644\u064a\u0644 \u0627\u0644\u0647\u0634\u0627\u0634\u0629.<\/p><h2 class=\"wp-block-heading\">\u0645\u0627 \u0647\u064a \u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0627\u062a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 5160\u061f<\/h2><p class=\"wp-block-paragraph\">\u0648\u0641\u064a\u0645\u0627 \u064a\u0644\u064a \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0639\u0645\u0644\u064a\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 5160:<\/p><ul class=\"wp-block-list\"><li><strong>\u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a<\/strong>:\u0646\u0648\u0627\u0628\u0636 \u0648\u0631\u0642\u064a\u0629 \u0648\u0646\u0648\u0627\u0628\u0636 \u0644\u0648\u0644\u0628\u064a\u0629 \u0644\u062a\u0639\u0644\u064a\u0642 \u0627\u0644\u0645\u0631\u0643\u0628\u0627\u062a.<\/li>\n\n<li><strong>\u0623\u062f\u0648\u0627\u062a \u0645\u0632\u0648\u0631\u0629<\/strong>:\u0627\u0644\u0645\u0637\u0627\u0631\u0642\u060c \u0627\u0644\u0641\u0624\u0648\u0633\u060c \u0627\u0644\u0633\u0648\u0627\u0637\u064a\u0631.<\/li>\n\n<li><strong>\u0646\u0648\u0627\u0628\u0636 \u062a\u0639\u0644\u064a\u0642 \u0627\u0644\u0634\u0627\u062d\u0646\u0627\u062a<\/strong>:\u0646\u0648\u0627\u0628\u0636 \u0634\u062f\u064a\u062f\u0629 \u0627\u0644\u062a\u062d\u0645\u0644 \u0644\u0644\u0634\u0627\u062d\u0646\u0627\u062a \u0648\u0627\u0644\u0645\u0631\u0643\u0628\u0627\u062a \u0627\u0644\u062a\u062c\u0627\u0631\u064a\u0629.<\/li>\n\n<li><strong>\u0634\u0641\u0631\u0627\u062a \u0627\u0644\u0633\u0643\u0627\u0643\u064a\u0646<\/strong>:\u0633\u0643\u0627\u0643\u064a\u0646 \u0627\u0644\u0628\u0642\u0627\u0621 \u0639\u0644\u0649 \u0642\u064a\u062f \u0627\u0644\u062d\u064a\u0627\u0629\u060c \u0648\u0627\u0644\u0633\u064a\u0648\u0641\u060c \u0648\u0627\u0644\u0633\u0643\u0627\u0643\u064a\u0646 \u0630\u0627\u062a \u0627\u0644\u0646\u0635\u0644 \u0627\u0644\u062b\u0627\u0628\u062a \u0627\u0644\u0643\u0628\u064a\u0631\u0629.<\/li>\n\n<li><strong>\u0627\u0644\u0622\u0644\u0627\u062a \u0627\u0644\u062b\u0642\u064a\u0644\u0629<\/strong>:\u0627\u0644\u0623\u063a\u0644\u0627\u0644\u060c \u0627\u0644\u062f\u0628\u0627\u0628\u064a\u0633\u060c \u0627\u0644\u0628\u0637\u0627\u0646\u0627\u062a\u060c \u0627\u0644\u0645\u0643\u0648\u0646\u0627\u062a \u0627\u0644\u0645\u064a\u0643\u0627\u0646\u064a\u0643\u064a\u0629.<\/li>\n\n<li><strong>\u0627\u0644\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0632\u0631\u0627\u0639\u064a\u0629<\/strong>:\u0627\u0644\u0645\u062c\u0627\u0631\u0641\u060c \u0634\u0641\u0631\u0627\u062a \u0627\u0644\u0645\u062d\u0631\u0627\u062b.<\/li><\/ul><h3 class=\"wp-block-heading\">\u0647\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 5160 \u062c\u064a\u062f \u0644\u0644\u0633\u0643\u0627\u0643\u064a\u0646\u061f<\/h3><p class=\"wp-block-paragraph\">\u0646\u0639\u0645\u060c \u0627\u0644\u0641\u0648\u0644\u0627\u0630 5160 \u0645\u0645\u062a\u0627\u0632 \u0644\u0640 <strong>\u0633\u0643\u0627\u0643\u064a\u0646 \u0643\u0628\u064a\u0631\u0629\u060c \u0642\u0648\u064a\u0629\u060c \u0623\u0648 \u0633\u0643\u0627\u0643\u064a\u0646 \u0644\u0644\u0628\u0642\u0627\u0621 \u0639\u0644\u0649 \u0642\u064a\u062f \u0627\u0644\u062d\u064a\u0627\u0629\u060c \u0623\u0648 \u0633\u0643\u0627\u0643\u064a\u0646 \u0630\u0627\u062a \u0634\u0641\u0631\u0629 \u062b\u0627\u0628\u062a\u0629<\/strong>. \u0625\u0646 \u0635\u0644\u0627\u0628\u062a\u0647\u0627 \u0627\u0644\u0639\u0627\u0644\u064a\u0629 \u0648\u0645\u0642\u0627\u0648\u0645\u062a\u0647\u0627 \u0644\u0644\u0635\u062f\u0645\u0627\u062a \u062a\u062c\u0639\u0644\u0647\u0627 \u0645\u062b\u0627\u0644\u064a\u0629 \u0644\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u0634\u0627\u0642\u060c \u0648\u0644\u0643\u0646\u0647\u0627 \u0644\u064a\u0633\u062a \u0627\u0644\u062e\u064a\u0627\u0631 \u0627\u0644\u0623\u0641\u0636\u0644 \u0644\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0627\u062a \u0627\u0644\u0634\u0627\u0642\u0629. <strong>\u0633\u0643\u0627\u0643\u064a\u0646 \u0635\u063a\u064a\u0631\u0629<\/strong> \u0623\u0648 \u0623\u0648\u0644\u0626\u0643 \u0627\u0644\u0630\u064a\u0646 \u064a\u062d\u062a\u0627\u062c\u0648\u0646 \u0625\u0644\u0649 \u062d\u0648\u0627\u0641 \u062f\u0642\u064a\u0642\u0629.<\/p><p class=\"wp-block-paragraph\">5160 \u0645\u0642\u0627\u0628\u0644 1095<\/p><p class=\"wp-block-paragraph\">\u062a\u062a\u0645\u064a\u0632 \u0645\u0627\u062f\u0629 5160 \u0628\u0627\u0644\u0635\u0644\u0627\u0628\u0629\u060c \u0628\u064a\u0646\u0645\u0627 \u062a\u062a\u0645\u064a\u0632 \u0645\u0627\u062f\u0629 1095 \u0628\u0642\u062f\u0631\u062a\u0647\u0627 \u0639\u0644\u0649 \u0627\u0644\u0627\u062d\u062a\u0641\u0627\u0638 \u0628\u0627\u0644\u062d\u0627\u0641\u0629 \u0648\u0633\u0647\u0648\u0644\u0629 \u0627\u0644\u0634\u062d\u0630. \u0648\u0641\u064a \u062d\u064a\u0646 \u062a\u0648\u0641\u0631 \u0645\u0627\u062f\u0629 5160 \u0645\u0642\u0627\u0648\u0645\u0629 \u0623\u0643\u0628\u0631 \u0644\u0644\u062a\u0622\u0643\u0644\u060c <a href=\"https:\/\/steelprogroup.com\/ar\/tool-steel\/grades\/1095\/\">1095<\/a> \u0623\u0643\u062b\u0631 \u0639\u0631\u0636\u0629 \u0644\u0644\u0635\u062f\u0623 \u0648\u064a\u062d\u062a\u0627\u062c \u0625\u0644\u0649 \u0645\u0632\u064a\u062f \u0645\u0646 \u0627\u0644\u0635\u064a\u0627\u0646\u0629.<\/p><p class=\"wp-block-paragraph\">\u064a\u0639\u062a\u0628\u0631 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 5160 \u0623\u0643\u062b\u0631 \u0635\u0644\u0627\u0628\u0629 \u0648\u0645\u0642\u0627\u0648\u0645\u0629 \u0644\u0644\u0635\u062f\u0645\u0627\u062a \u0645\u0646 1095\u060c \u0648\u0630\u0644\u0643 \u0628\u0641\u0636\u0644 \u0645\u062d\u062a\u0648\u0627\u0647 \u0645\u0646 \u0627\u0644\u0643\u0631\u0648\u0645\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647 \u0645\u062b\u0627\u0644\u064a\u064b\u0627 \u0644\u0644\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u062b\u0642\u064a\u0644\u0629 \u0648\u0646\u0648\u0627\u0628\u0636 \u0627\u0644\u062a\u0639\u0644\u064a\u0642. \u0648\u0645\u0639 \u0630\u0644\u0643\u060c \u0641\u0625\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 1095 \u0623\u0633\u0647\u0644 \u0641\u064a \u0627\u0644\u0634\u062d\u0630 \u0648\u064a\u062d\u0627\u0641\u0638 \u0639\u0644\u0649 \u062d\u0627\u0641\u0629 \u0623\u062f\u0642\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647 \u0627\u0644\u062e\u064a\u0627\u0631 \u0627\u0644\u0623\u0641\u0636\u0644 \u0644\u0644\u0633\u0643\u0627\u0643\u064a\u0646 \u0627\u0644\u062a\u064a \u062a\u062a\u0637\u0644\u0628 \u062d\u062f\u0629.&nbsp;<\/p><h2 class=\"wp-block-heading\">\u0627\u062e\u062a\u0631 \u0623\u0641\u0636\u0644 \u0641\u0648\u0644\u0627\u0630 5160 \u0644\u0645\u0634\u0631\u0648\u0639\u0643 \u0627\u0644\u0642\u0627\u062f\u0645<\/h2><p class=\"wp-block-paragraph\">\u0641\u064a SteelPro Group\u060c \u0646\u0642\u062f\u0645 \u0641\u0648\u0644\u0627\u0630 5160 \u0639\u0627\u0644\u064a \u0627\u0644\u062c\u0648\u062f\u0629 \u0645\u0639 \u062e\u064a\u0627\u0631\u0627\u062a \u062a\u0635\u0646\u064a\u0639 \u0648\u062a\u0634\u0637\u064a\u0628 \u0645\u062e\u0635\u0635\u0629\u060c \u0628\u0645\u0627 \u0641\u064a \u0630\u0644\u0643 \u0627\u0644\u0642\u0637\u0639 \u0648\u0627\u0644\u0637\u062d\u0646 \u0648\u0627\u0644\u0635\u0642\u0644 \u0648\u0627\u0644\u062a\u0644\u0645\u064a\u0639 \u0644\u062a\u0644\u0628\u064a\u0629 \u0627\u062d\u062a\u064a\u0627\u062c\u0627\u062a\u0643 \u0627\u0644\u062f\u0642\u064a\u0642\u0629. \u0628\u0641\u0636\u0644 \u0633\u0646\u0648\u0627\u062a \u0627\u0644\u062e\u0628\u0631\u0629\u060c \u0646\u0642\u062f\u0645 \u0627\u0644\u062f\u0642\u0629 \u0648\u0627\u0644\u0645\u0648\u062b\u0648\u0642\u064a\u0629 \u0641\u064a \u0643\u0644 \u0645\u0634\u0631\u0648\u0639.&nbsp;<\/p><p class=\"wp-block-paragraph\">\u0646\u062d\u0646 \u0646\u0642\u062f\u0645 \u0623\u064a\u0636\u0627<strong> <\/strong><a href=\"https:\/\/steelprogroup.com\/ar\/tool-steel\/cr12mov\/\">\u0634\u0641\u0631\u0629 \u0641\u0648\u0644\u0627\u0630\u064a\u0629 D2<\/a><strong> <\/strong>\u0644\u0644\u062d\u0635\u0648\u0644 \u0639\u0644\u0649 \u0623\u062f\u0627\u0621 \u0642\u0637\u0639 \u0627\u0633\u062a\u062b\u0646\u0627\u0626\u064a. \u0627\u062a\u0635\u0644 \u0628\u0646\u0627 \u0627\u0644\u064a\u0648\u0645 \u0644\u0645\u0639\u0631\u0641\u0629 \u0643\u064a\u0641 \u064a\u0645\u0643\u0646\u0646\u0627 \u062f\u0639\u0645 \u0645\u0634\u0631\u0648\u0639\u0643 \u0628\u0645\u0648\u0627\u062f \u0639\u0627\u0644\u064a\u0629 \u0627\u0644\u062c\u0648\u062f\u0629 \u0648\u062e\u062f\u0645\u0629 \u0627\u0644\u062e\u0628\u0631\u0627\u0621.<\/p>","protected":false},"excerpt":{"rendered":"<p>\u0641\u064a SteelPro Group\u060c \u0646\u062d\u0646 \u0645\u062a\u062e\u0635\u0635\u0648\u0646 \u0641\u064a \u062a\u0648\u0631\u064a\u062f \u0627\u0644\u0641\u0648\u0644\u0627\u0630 1045 \u0639\u0627\u0644\u064a \u0627\u0644\u062c\u0648\u062f\u0629\u060c \u0627\u0644\u0645\u062a\u0648\u0641\u0631 \u0628\u0623\u0634\u0643\u0627\u0644 \u0645\u062e\u062a\u0644\u0641\u0629 \u0628\u0645\u0627 \u0641\u064a \u0630\u0644\u0643 \u0623\u0644\u0648\u0627\u062d \u0648\u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630. \u0646\u062d\u0646 [\u2026]<\/p>","protected":false},"author":12,"featured_media":20172,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"_eb_attr":"","rank_math_lock_modified_date":false,"site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"categories":[4294,4293],"tags":[],"class_list":["post-20179","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-grades-tool-steel","category-tool-steel"],"acf":[],"_links":{"self":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts\/20179","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/users\/12"}],"replies":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/comments?post=20179"}],"version-history":[{"count":0,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts\/20179\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/media\/20172"}],"wp:attachment":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/media?parent=20179"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/categories?post=20179"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/tags?post=20179"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}