{"id":20182,"date":"2025-01-04T06:45:00","date_gmt":"2025-01-03T22:45:00","guid":{"rendered":"https:\/\/steelprogroup.com\/?p=20182"},"modified":"2025-01-09T17:05:23","modified_gmt":"2025-01-09T09:05:23","slug":"dc53","status":"publish","type":"post","link":"https:\/\/steelprogroup.com\/ar\/tool-steel\/grades\/dc53\/","title":{"rendered":"DC53 \u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0623\u062f\u0648\u0627\u062a | \u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0634\u0641\u0631\u0629 \u0648\u0627\u0644\u0642\u0648\u0627\u0644\u0628 \u0648\u0627\u0644\u0642\u0637\u0639"},"content":{"rendered":"<p class=\"wp-block-paragraph\">\u062a\u0639\u062f SteelPro Group \u0631\u0627\u0626\u062f\u0629 \u0639\u0627\u0644\u0645\u064a\u0629 \u0641\u064a \u0645\u062c\u0627\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0643\u0631\u0628\u0648\u0646\u064a \u0639\u0627\u0644\u064a \u0627\u0644\u0623\u062f\u0627\u0621\u060c \u062d\u064a\u062b \u062a\u0642\u062f\u0645 \u0645\u0646\u062a\u062c\u0627\u062a \u0641\u0648\u0644\u0627\u0630\u064a\u0629 DC53 \u0645\u0646 \u0627\u0644\u062f\u0631\u062c\u0629 \u0627\u0644\u0623\u0648\u0644\u0649. \u064a\u0648\u0641\u0631 \u0641\u0648\u0644\u0627\u0630 DC53 \u0627\u0644\u062e\u0627\u0635 \u0628\u0646\u0627 \u0642\u0648\u0629 \u0648\u0645\u062a\u0627\u0646\u0629 \u0644\u0627 \u0645\u062b\u064a\u0644 \u0644\u0647\u0627 \u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a\u0643 \u0627\u0644\u0623\u0643\u062b\u0631 \u062a\u0637\u0644\u0628\u064b\u0627.<\/p><h2 class=\"wp-block-heading\">\u0645\u0627 \u0647\u0648 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 DC53\u061f<\/h2><p class=\"wp-block-paragraph\">DC53 \u0647\u0648 \u0641\u0648\u0644\u0627\u0630 \u0645\u0645\u062a\u0627\u0632 \u0644\u0644\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0645\u0633\u062a\u062e\u062f\u0645\u0629 \u0641\u064a \u0627\u0644\u0639\u0645\u0644 \u0627\u0644\u0628\u0627\u0631\u062f \u064a\u062a\u0645\u062a\u0639 \u0628\u0642\u0648\u0629 \u0648\u0635\u0644\u0627\u0628\u0629 \u0645\u0645\u0627\u062b\u0644\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0639\u0627\u0644\u064a \u0627\u0644\u0633\u0631\u0639\u0629. \u0648\u0647\u0648 \u064a\u0648\u0641\u0631 \u062a\u0634\u063a\u064a\u0644\u064b\u0627 \u0645\u0645\u062a\u0627\u0632\u064b\u0627 \u0648\u0645\u062a\u0627\u0646\u0629 \u0648\u0627\u062d\u062a\u0641\u0627\u0638\u064b\u0627 \u0628\u0627\u0644\u062d\u0627\u0641\u0629\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647 \u0645\u062b\u0627\u0644\u064a\u064b\u0627 \u0644\u0644\u0642\u0648\u0627\u0644\u0628. \u0648\u0647\u0648 \u064a\u0645\u062b\u0644 \u062a\u062d\u0633\u0646\u064b\u0627 \u0639\u0646 D2\u060c \u062d\u064a\u062b \u064a\u0637\u064a\u0644 \u0639\u0645\u0631 \u0627\u0644\u0623\u062f\u0627\u0629 \u0648\u0633\u0631\u0639\u0629 \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629. DC53 \u0645\u0646\u0627\u0633\u0628 \u0644\u0645\u0639\u0627\u0644\u062c\u0627\u062a \u0633\u0637\u062d PVD \u0648\u064a\u062f\u0639\u0645 \u0637\u0644\u0627\u0621\u0627\u062a CVD \u0648TD \u0645\u0639 \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629 \u0627\u0644\u0644\u0627\u062d\u0642\u0629.<\/p><h3 class=\"wp-block-heading\">\u0645\u0627 \u0647\u064a \u0627\u0644\u0627\u062e\u062a\u0644\u0627\u0641\u0627\u062a \u0628\u064a\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 DC53 \u0648 D2\u061f<\/h3><p class=\"wp-block-paragraph\">\u062a\u062a\u0645\u062a\u0639 DC53 \u0628\u0635\u0644\u0627\u0628\u0629 \u0623\u0641\u0636\u0644 \u0645\u0646 D2\u060c \u0645\u0645\u0627 \u064a\u0639\u0632\u0632 \u0642\u062f\u0631\u062a\u0647\u0627 \u0639\u0644\u0649 \u062a\u062d\u0645\u0644 \u0627\u0644\u0635\u062f\u0645\u0627\u062a \u0648\u0645\u0646\u0639 \u0627\u0644\u062a\u0634\u0642\u0642. \u0648\u0628\u064a\u0646\u0645\u0627 \u062a\u062a\u0645\u062a\u0639 D2 \u0628\u0645\u0642\u0627\u0648\u0645\u0629 \u0643\u0628\u064a\u0631\u0629 \u0644\u0644\u062a\u0622\u0643\u0644\u060c \u062a\u062d\u0642\u0642 DC53 \u062a\u0648\u0627\u0632\u0646\u064b\u0627 \u0623\u0641\u0636\u0644 \u0628\u064a\u0646 \u0627\u0644\u0635\u0644\u0627\u0628\u0629 \u0648\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644\u060c \u0648\u064a\u0645\u0643\u0646\u0647\u0627 \u0627\u0644\u0648\u0635\u0648\u0644 \u0625\u0644\u0649 \u0635\u0644\u0627\u0628\u0629 \u0623\u0639\u0644\u0649 (HRC 62 \u0645\u0642\u0627\u0631\u0646\u0629 \u0628\u0640 HRC 58-60 \u0627\u0644\u062e\u0627\u0635\u0629 \u0628\u0640 D2). \u062a\u062a\u0645\u062a\u0639 DC53 \u0623\u064a\u0636\u064b\u0627 \u0628\u0642\u062f\u0631\u0629 \u0623\u0641\u0636\u0644 \u0639\u0644\u0649 \u0627\u0644\u062a\u0635\u0646\u064a\u0639\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647\u0627 \u0623\u0643\u062b\u0631 \u0641\u0639\u0627\u0644\u064a\u0629 \u0645\u0646 \u062d\u064a\u062b \u0627\u0644\u062a\u0643\u0644\u0641\u0629 \u0641\u064a \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629.<\/p><h2 class=\"wp-block-heading\">\u0641\u0648\u0644\u0627\u0630 DC53 \u0645\u0627 \u064a\u0639\u0627\u062f\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630<\/h2><p class=\"wp-block-paragraph\">\u0641\u064a\u0645\u0627 \u064a\u0644\u064a \u0627\u0644\u0645\u0639\u0627\u062f\u0644\u0627\u062a \u0627\u0644\u0645\u0639\u062a\u0631\u0641 \u0628\u0647\u0627 \u0639\u0645\u0648\u0645\u064b\u0627 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 DC53:<\/p><ul class=\"wp-block-list\"><li>JIS: DC53 (JIS G4404)<\/li>\n\n<li>\u062f\u064a\u0646: 1.2379<\/li>\n\n<li>GB: Cr12MoV<\/li><\/ul><h2 class=\"wp-block-heading\">\u0645\u0648\u0627\u0635\u0641\u0627\u062a \u0645\u0646\u062a\u062c\u0627\u062a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 DC53<\/h2><p class=\"wp-block-paragraph\">\u062a\u0642\u062f\u0645 SteelPro Group \u0645\u0646\u062a\u062c\u0627\u062a \u0641\u0648\u0644\u0627\u0630\u064a\u0629 DC53 \u0639\u0627\u0644\u064a\u0629 \u0627\u0644\u062c\u0648\u062f\u0629 \u0645\u062b\u0644 \u0627\u0644\u0642\u0636\u0628\u0627\u0646 \u0648\u0627\u0644\u0623\u0644\u0648\u0627\u062d \u0648\u0627\u0644\u0623\u0644\u0648\u0627\u062d \u0648\u0627\u0644\u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u0645\u0633\u062a\u062f\u064a\u0631\u0629. \u0625\u0630\u0627 \u0643\u0646\u062a \u0628\u062d\u0627\u062c\u0629 \u0625\u0644\u0649 \u0623\u062d\u062c\u0627\u0645 \u0645\u0639\u064a\u0646\u0629 \u0623\u0648 \u0623\u0634\u0643\u0627\u0644 \u0645\u062e\u0635\u0635\u0629\u060c \u0641\u0644\u0627 \u062a\u062a\u0631\u062f\u062f \u0641\u064a \u0627\u0644\u062a\u0648\u0627\u0635\u0644 \u0645\u0639\u0646\u0627.<\/p><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u0646\u0645\u0648\u0630\u062c \u0627\u0644\u0645\u0646\u062a\u062c<\/strong><\/td><td><strong>\u0646\u0637\u0627\u0642 \u0627\u0644\u062d\u062c\u0645 (\u0645\u062a\u0631\u064a)<\/strong><\/td><td><strong>\u0646\u0637\u0627\u0642 \u0627\u0644\u062d\u062c\u0645 (\u0625\u0645\u0628\u0631\u0627\u0637\u0648\u0631\u064a)<\/strong><\/td><\/tr><tr><td>\u0642\u0636\u0628\u0627\u0646 \u0645\u0633\u062a\u062f\u064a\u0631\u0629<\/td><td>\u0627\u0644\u0642\u0637\u0631: 20 \u0645\u0644\u0645 \u0625\u0644\u0649 300 \u0645\u0644\u0645<\/td><td>0.8 \u0628\u0648\u0635\u0629 \u0625\u0644\u0649 11.8 \u0628\u0648\u0635\u0629<\/td><\/tr><tr><td>\u0642\u0636\u0628\u0627\u0646 \u0645\u0631\u0628\u0639\u0629<\/td><td>\u0627\u0644\u0642\u0637\u0631: 20 \u0645\u0644\u0645 \u0625\u0644\u0649 300 \u0645\u0644\u0645<\/td><td>0.8 \u0628\u0648\u0635\u0629 \u0625\u0644\u0649 11.8 \u0628\u0648\u0635\u0629<\/td><\/tr><tr><td>\u0642\u0636\u0628\u0627\u0646 \u0645\u0633\u0637\u062d\u0629<\/td><td>20 \u0645\u0645 \u00d7 20 \u0645\u0645 \u0625\u0644\u0649 200 \u0645\u0645 \u00d7 300 \u0645\u0645<\/td><td>0.8 \u0628\u0648\u0635\u0629 \u00d7 0.8 \u0628\u0648\u0635\u0629 \u0625\u0644\u0649 7.9 \u0628\u0648\u0635\u0629 \u00d7 11.8 \u0628\u0648\u0635\u0629<\/td><\/tr><tr><td rowspan=\"3\">\u0623\u0648\u0631\u0627\u0642<\/td><td>\u0627\u0644\u0633\u0645\u0643: 1 \u0645\u0645 \u0625\u0644\u0649 100 \u0645\u0645<\/td><td>0.04 \u0628\u0648\u0635\u0629 \u0625\u0644\u0649 3.9 \u0628\u0648\u0635\u0629<\/td><\/tr><tr><td>\u0627\u0644\u0639\u0631\u0636: 200 \u0645\u0644\u0645 \u0625\u0644\u0649 1500 \u0645\u0644\u0645<\/td><td>7.9 \u0628\u0648\u0635\u0629 \u0625\u0644\u0649 59 \u0628\u0648\u0635\u0629<\/td><\/tr><tr><td>\u0627\u0644\u0637\u0648\u0644: 500 \u0645\u0644\u0645 \u0625\u0644\u0649 4000 \u0645\u0644\u0645<\/td><td>19.7 \u0628\u0648\u0635\u0629 \u0625\u0644\u0649 157.5 \u0628\u0648\u0635\u0629<\/td><\/tr><tr><td rowspan=\"3\">\u0623\u0637\u0628\u0627\u0642<\/td><td>\u0627\u0644\u0633\u0645\u0643: 10 \u0645\u0644\u0645 \u0625\u0644\u0649 200 \u0645\u0644\u0645<\/td><td>0.4 \u0628\u0648\u0635\u0629 \u0625\u0644\u0649 7.9 \u0628\u0648\u0635\u0629<\/td><\/tr><tr><td>\u0627\u0644\u0639\u0631\u0636: 200 \u0645\u0644\u0645 \u0625\u0644\u0649 1500 \u0645\u0644\u0645<\/td><td>7.9 \u0628\u0648\u0635\u0629 \u0625\u0644\u0649 59 \u0628\u0648\u0635\u0629<\/td><\/tr><tr><td>\u0627\u0644\u0637\u0648\u0644: 500 \u0645\u0644\u0645 \u0625\u0644\u0649 4000 \u0645\u0644\u0645<\/td><td>19.7 \u0628\u0648\u0635\u0629 \u0625\u0644\u0649 157.5 \u0628\u0648\u0635\u0629<\/td><\/tr><tr><td rowspan=\"2\">\u0642\u0636\u0628\u0627\u0646 \u0645\u0633\u062a\u062f\u064a\u0631\u0629<\/td><td>\u0627\u0644\u0642\u0637\u0631: 10 \u0645\u0644\u0645 \u0625\u0644\u0649 200 \u0645\u0644\u0645<\/td><td>0.4 \u0628\u0648\u0635\u0629 \u0625\u0644\u0649 7.9 \u0628\u0648\u0635\u0629<\/td><\/tr><tr><td>\u0627\u0644\u0637\u0648\u0644: 1000 \u0645\u0644\u0645 \u0625\u0644\u0649 4000 \u0645\u0644\u0645<\/td><td>39.4 \u0628\u0648\u0635\u0629 \u0625\u0644\u0649 157.5 \u0628\u0648\u0635\u0629<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u0627\u0644\u062a\u0631\u0643\u064a\u0628 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a \u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0641\u0648\u0644\u0627\u0630\u064a DC53<\/h2><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u0639\u0646\u0635\u0631<\/strong><\/td><td><strong>\u0627\u0644\u0645\u062d\u062a\u0648\u0649 (%)<\/strong><\/td><\/tr><tr><td>\u0627\u0644\u0643\u0631\u0628\u0648\u0646 (C)<\/td><td>0.95<\/td><\/tr><tr><td>\u0627\u0644\u0643\u0631\u0648\u0645 (Cr)<\/td><td>8<\/td><\/tr><tr><td>\u0627\u0644\u062d\u062f\u064a\u062f (Fe)<\/td><td>87.35<\/td><\/tr><tr><td>\u0627\u0644\u0645\u0646\u063a\u0646\u064a\u0632 (Mn)<\/td><td>0.4<\/td><\/tr><tr><td>\u0627\u0644\u0645\u0648\u0644\u064a\u0628\u062f\u064a\u0646\u0648\u0645 (Mo)<\/td><td>2<\/td><\/tr><tr><td>\u0627\u0644\u0633\u064a\u0644\u064a\u0643\u0648\u0646 (Si)<\/td><td>1<\/td><\/tr><tr><td>\u0627\u0644\u0641\u0627\u0646\u0627\u062f\u064a\u0648\u0645 (V)<\/td><td>0.3<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0641\u064a\u0632\u064a\u0627\u0626\u064a\u0629 \u0644\u0641\u0648\u0644\u0627\u0630 DC53<\/h2><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u0645\u0644\u0643\u064a\u0629<\/strong><\/td><td><strong>\u0627\u0644\u0642\u064a\u0645\u0629 \u0627\u0644\u0645\u062a\u0631\u064a\u0629<\/strong><\/td><td><strong>\u0627\u0644\u0642\u064a\u0645\u0629 \u0627\u0644\u0625\u0645\u0628\u0631\u0627\u0637\u0648\u0631\u064a\u0629<\/strong><\/td><\/tr><tr><td>\u0643\u062b\u0627\u0641\u0629<\/td><td>7.87 \u062c\u0631\u0627\u0645\/\u0633\u0645 \u0645\u0643\u0639\u0628<\/td><td>0.284 \u0631\u0637\u0644\/\u0628\u0648\u0635\u0629 \u0645\u0643\u0639\u0628\u0629<\/td><\/tr><tr><td>\u0642\u0648\u0629 \u0627\u0644\u0634\u062f<\/td><td>1500 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644<\/td><td>217,500 \u0631\u0637\u0644\/\u0628\u0648\u0635\u0629 \u0645\u0631\u0628\u0639\u0629<\/td><\/tr><tr><td>\u0642\u0648\u0629 \u0627\u0644\u062e\u0636\u0648\u0639<\/td><td>1300 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644<\/td><td>188,500 \u0631\u0637\u0644\/\u0628\u0648\u0635\u0629 \u0645\u0631\u0628\u0639\u0629<\/td><\/tr><tr><td>\u0627\u0644\u0645\u0648\u0635\u0644\u064a\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629<\/td><td>23.8 \u0648\u0627\u0637\/\u0645\u00b7\u0643<\/td><td>165 \u0648\u062d\u062f\u0629 \u062d\u0631\u0627\u0631\u064a\u0629 \u0628\u0631\u064a\u0637\u0627\u0646\u064a\u0629\/\u0633\u0627\u0639\u0629 \u0642\u062f\u0645 \u0645\u0631\u0628\u0639 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a<\/td><\/tr><tr><td>\u0645\u0639\u0627\u0645\u0644 \u0627\u0644\u062a\u0645\u062f\u062f<\/td><td>12.2 \u0645\u064a\u0643\u0631\u0648\u0645\u062a\u0631\/\u0645\u062a\u0631\u00b7\u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (20-100 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629)<\/td><td>6.78 \u0645\u064a\u0643\u0631\u0648\u0646\/\u0628\u0648\u0635\u0629\u00b7\u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a (68-212 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u0627\u0644\u062e\u0648\u0627\u0635 \u0627\u0644\u0645\u064a\u0643\u0627\u0646\u064a\u0643\u064a\u0629 \u0644\u0641\u0648\u0644\u0627\u0630 DC53 \u0644\u0644\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0641\u0648\u0644\u0627\u0630\u064a\u0629<\/h2><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u0645\u0644\u0643\u064a\u0629<\/strong><\/td><td><strong>\u0627\u0644\u0642\u064a\u0645\u0629 \u0627\u0644\u0645\u062a\u0631\u064a\u0629<\/strong><\/td><td><strong>\u0627\u0644\u0642\u064a\u0645\u0629 \u0627\u0644\u0625\u0645\u0628\u0631\u0627\u0637\u0648\u0631\u064a\u0629<\/strong><\/td><\/tr><tr><td>\u0635\u0644\u0627\u0628\u0629 \u0628\u0631\u064a\u0646\u064a\u0644<\/td><td>210 \u2013 225 \u0647\u0640 \u0628<\/td><td>210 \u2013 225 \u0647\u0640 \u0628<\/td><\/tr><tr><td>\u0627\u0644\u0635\u0644\u0627\u0628\u0629(HRC)<\/td><td>62 \u2013 63 \u062d\u0642\u0648\u0642 \u0627\u0644\u0646\u0634\u0631<\/td><td>62 \u2013 63 \u062d\u0642\u0648\u0642 \u0627\u0644\u0646\u0634\u0631<\/td><\/tr><tr><td>\u0645\u0639\u0627\u0645\u0644 \u0627\u0644\u0645\u0631\u0648\u0646\u0629<\/td><td>150 \u062c\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644<\/td><td>21700 \u0643.\u0633.<\/td><\/tr><tr><td>\u0646\u0633\u0628\u0629 \u0628\u0648\u0627\u0633\u0648\u0646<\/td><td>0.28<\/td><td>0.28<\/td><\/tr><tr><td>\u0645\u0639\u0627\u0645\u0644 \u0627\u0644\u0642\u0635<\/td><td>58.5 \u062c\u064a\u062c\u0627\u0628\u0627\u0633\u0643\u0627\u0644<\/td><td>8,480 \u0643\u064a\u0644\u0648 \u0628\u0627\u0633\u0643\u0627\u0644<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629 \u0644\u0641\u0648\u0644\u0627\u0630 DC53<\/h2><p class=\"wp-block-paragraph\">\u0641\u064a SteelPro Group\u060c \u0646\u0639\u0637\u064a \u0627\u0644\u0623\u0648\u0644\u0648\u064a\u0629 \u0644\u0644\u062f\u0642\u0629 \u0641\u064a \u0643\u0644 \u062e\u0637\u0648\u0629 \u0645\u0646 \u062e\u0637\u0648\u0627\u062a \u0639\u0645\u0644\u064a\u0629 \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629 \u0644\u0644\u0635\u0644\u0628 DC53. \u0645\u0646 \u0627\u0644\u062a\u0644\u062f\u064a\u0646 \u0625\u0644\u0649 \u0627\u0644\u062a\u0635\u0644\u0628 \u0648\u0627\u0644\u062a\u062e\u0645\u064a\u0631\u060c \u064a\u0636\u0645\u0646 \u0641\u0631\u064a\u0642 \u0627\u0644\u062e\u0628\u0631\u0627\u0621 \u0644\u062f\u064a\u0646\u0627 \u0627\u0644\u0635\u0644\u0627\u0628\u0629 \u0648\u0627\u0644\u0635\u0644\u0627\u0628\u0629 \u0648\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644 \u0627\u0644\u0645\u062b\u0627\u0644\u064a\u0629.&nbsp;<\/p><h3 class=\"wp-block-heading\">\u0627\u0644\u062a\u0644\u062f\u064a\u0646<\/h3><p class=\"wp-block-paragraph\">\u0642\u0645 \u0628\u062a\u0633\u062e\u064a\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0625\u0644\u0649 \u062f\u0631\u062c\u0629 \u062d\u0631\u0627\u0631\u0629 \u062a\u062a\u0631\u0627\u0648\u062d \u0628\u064a\u0646 750 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \u0648800 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (1380 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a \u06481470 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a) \u0648\u0627\u062d\u062a\u0641\u0638 \u0628\u0647 \u0639\u0646\u062f \u0647\u0630\u0647 \u0627\u0644\u062f\u0631\u062c\u0629 \u0645\u0646 \u0627\u0644\u062d\u0631\u0627\u0631\u0629. \u062b\u0645 \u0642\u0645 \u0628\u062a\u0628\u0631\u064a\u062f\u0647 \u0628\u0628\u0637\u0621 \u0641\u064a \u0627\u0644\u0641\u0631\u0646 \u0623\u0648 \u0641\u064a \u0627\u0644\u0647\u0648\u0627\u0621 \u0627\u0644\u0633\u0627\u0643\u0646 \u0625\u0644\u0649 \u062f\u0631\u062c\u0629 \u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u063a\u0631\u0641\u0629. \u062a\u0639\u0645\u0644 \u0647\u0630\u0647 \u0627\u0644\u0639\u0645\u0644\u064a\u0629 \u0639\u0644\u0649 \u062a\u062e\u0641\u064a\u0641 \u0627\u0644\u0636\u063a\u0648\u0637 \u0627\u0644\u062f\u0627\u062e\u0644\u064a\u0629 \u0623\u0648 \u062a\u0642\u0644\u064a\u0644 \u0627\u0644\u0635\u0644\u0627\u0628\u0629 \u0644\u0623\u063a\u0631\u0627\u0636 \u0627\u0644\u062a\u0635\u0646\u064a\u0639.<\/p><h3 class=\"wp-block-heading\">\u0627\u0644\u062a\u0635\u0644\u0628 \u0627\u0644\u0647\u0648\u0627\u0626\u064a<\/h3><p class=\"wp-block-paragraph\"><strong>\u0627\u0644\u062a\u0633\u062e\u064a\u0646 \u0627\u0644\u0645\u0633\u0628\u0642 \u0648\u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0628\u0627\u0644\u0623\u0633\u062a\u064a\u0646\u064a\u062a<\/strong><\/p><p class=\"wp-block-paragraph\">\u0642\u0645 \u0628\u062a\u0633\u062e\u064a\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0645\u0633\u0628\u0642\u064b\u0627 <strong>800 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \u0625\u0644\u0649 850 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (1475 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a \u0625\u0644\u0649 1560 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/strong> \u0644\u0636\u0645\u0627\u0646 \u0627\u0644\u062a\u0633\u062e\u064a\u0646 \u0627\u0644\u0645\u0648\u062d\u062f. \u0628\u0639\u062f \u0630\u0644\u0643\u060c \u0627\u0631\u0641\u0639 \u062f\u0631\u062c\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0625\u0644\u0649 <strong>1,030 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (1,885 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/strong> \u0644\u0644\u0625\u0636\u0641\u0627\u0621 \u0637\u0627\u0628\u0639 \u0627\u0644\u0623\u0648\u0633\u062a\u0646\u064a\u062a\u064a.<\/p><p class=\"wp-block-paragraph\">\u0628\u0627\u0644\u0646\u0633\u0628\u0629 \u0644\u0644\u0623\u062c\u0632\u0627\u0621 \u0627\u0644\u062a\u064a \u064a\u0635\u0644 \u0633\u0645\u0643\u0647\u0627 \u0625\u0644\u0649 100 \u0645\u0645 (4 \u0628\u0648\u0635\u0627\u062a)\u060c \u0627\u0646\u0642\u0639\u0647\u0627 \u0644\u0645\u062f\u0629 \u062a\u062a\u0631\u0627\u0648\u062d \u0645\u0646 25 \u0625\u0644\u0649 30 \u062f\u0642\u064a\u0642\u0629 \u0644\u0643\u0644 \u0628\u0648\u0635\u0629 (\u0633\u0627\u0639\u0629 \u0648\u0627\u062d\u062f\u0629 \u0644\u0644\u0623\u062c\u0632\u0627\u0621 \u0627\u0644\u062a\u064a \u064a\u0642\u0644 \u0633\u0645\u0643\u0647\u0627 \u0639\u0646 25 \u0645\u0645). \u0628\u0627\u0644\u0646\u0633\u0628\u0629 \u0644\u0644\u0623\u062c\u0632\u0627\u0621 \u0627\u0644\u0623\u0643\u062b\u0631 \u0633\u0645\u0643\u064b\u0627\u060c \u0627\u0646\u0642\u0639\u0647\u0627 \u0644\u0645\u062f\u0629 \u062a\u062a\u0631\u0627\u0648\u062d \u0645\u0646 10 \u0625\u0644\u0649 25 \u062f\u0642\u064a\u0642\u0629 \u0644\u0643\u0644 \u0628\u0648\u0635\u0629.<\/p><p class=\"wp-block-paragraph\"><strong>\u0625\u062e\u0645\u0627\u062f<\/strong><\/p><p class=\"wp-block-paragraph\">\u0627\u0633\u062a\u062e\u062f\u0645 \u0625\u062e\u0645\u0627\u062f \u0627\u0644\u063a\u0627\u0632 \u0627\u0644\u062e\u0627\u0645\u0644 \u0627\u0644\u0645\u0636\u063a\u0648\u0637 (\u0639\u0627\u062f\u0629 \u0627\u0644\u0646\u064a\u062a\u0631\u0648\u062c\u064a\u0646) \u0644\u062a\u062c\u0646\u0628 \u0627\u0644\u062a\u0644\u0648\u062b. \u0645\u0646 \u0627\u0644\u0645\u0647\u0645 \u0639\u062f\u0645 \u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0636\u063a\u0648\u0637 \u0625\u062e\u0645\u0627\u062f \u0623\u0639\u0644\u0649 \u0645\u0646 <strong>2 \u0628\u0627\u0631<\/strong> (\u0636\u0639\u0641 \u0627\u0644\u0636\u063a\u0637 \u0627\u0644\u062c\u0648\u064a) \u062d\u064a\u062b \u0623\u0646 \u0627\u0644\u0636\u063a\u0648\u0637 \u0627\u0644\u0623\u0639\u0644\u0649 \u064a\u0645\u0643\u0646 \u0623\u0646 \u062a\u0633\u0628\u0628 \u062a\u0634\u0648\u0647\u0627\u062a \u0648\u0632\u064a\u0627\u062f\u0629 \u0627\u0644\u0636\u063a\u0637.<\/p><p class=\"wp-block-paragraph\">\u062a\u062d\u0648\u0644 \u0647\u0630\u0647 \u0627\u0644\u062e\u0637\u0648\u0629 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0645\u0646 \u0627\u0644\u062d\u0627\u0644\u0629 \u0627\u0644\u0623\u0648\u0633\u062a\u0646\u064a\u062a\u064a\u0629 \u0625\u0644\u0649 \u0627\u0644\u062d\u0627\u0644\u0629 \u0627\u0644\u0645\u0627\u0631\u062a\u0646\u0633\u064a\u062a\u064a\u0629 \u063a\u064a\u0631 \u0627\u0644\u0645\u062e\u0641\u0641\u0629\u060c \u0645\u0645\u0627 \u064a\u0632\u064a\u062f \u0645\u0646 \u0635\u0644\u0627\u0628\u062a\u0647. \u0628\u0639\u062f \u0627\u0644\u0625\u062e\u0645\u0627\u062f\u060c \u064a\u062c\u0628 \u062a\u0628\u0631\u064a\u062f \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0625\u0644\u0649 \u062f\u0631\u062c\u0629<strong> 45 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \u0625\u0644\u0649 65 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (120 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a \u0625\u0644\u0649 150 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a) <\/strong>\u0642\u0628\u0644 \u0627\u0644\u062a\u0644\u0637\u064a\u0641.<\/p><h3 class=\"wp-block-heading\">\u062a\u0635\u0644\u0628 \u062d\u0645\u0627\u0645 \u0627\u0644\u0645\u0644\u062d<\/h3><p class=\"wp-block-paragraph\"><strong>\u0627\u0644\u062a\u0633\u062e\u064a\u0646 \u0627\u0644\u0645\u0633\u0628\u0642 \u0648\u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0628\u0627\u0644\u0623\u0633\u062a\u064a\u0646\u064a\u062a<\/strong><\/p><p class=\"wp-block-paragraph\">\u062a\u0633\u062e\u064a\u0646 \u0627\u0644\u062c\u0632\u0621 \u0645\u0633\u0628\u0642\u064b\u0627 <strong>850 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (1550 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/strong> \u062d\u062a\u0649 \u064a\u062a\u0645 \u062a\u0633\u062e\u064a\u0646\u0647 \u0628\u0627\u0644\u062a\u0633\u0627\u0648\u064a. \u062b\u0645 \u0627\u063a\u0645\u0631 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0641\u064a \u062d\u0645\u0627\u0645 \u0645\u0644\u062d \u0645\u0646\u0635\u0647\u0631 \u0639\u0646\u062f \u062f\u0631\u062c\u0629 \u062d\u0631\u0627\u0631\u0629 <strong>1,030 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (1,885 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/strong> \u0644\u0645\u062f\u0629 5 \u062f\u0642\u0627\u0626\u0642 \u0639\u0644\u0649 \u0627\u0644\u0623\u0642\u0644. \u064a\u062e\u062a\u0644\u0641 \u0648\u0642\u062a \u0627\u0644\u063a\u0645\u0631 \u0648\u0641\u0642\u064b\u0627 \u0644\u0633\u0645\u0643 \u0627\u0644\u062c\u0632\u0621\u060c \u0643\u0645\u0627 \u0647\u0648 \u0645\u0648\u0636\u062d \u0641\u064a \u0627\u0644\u062c\u062f\u0648\u0644 \u0623\u062f\u0646\u0627\u0647:<\/p><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u0633\u0645\u0627\u0643\u0629<\/strong><\/td><td><strong>\u0648\u0642\u062a \u0627\u0644\u0627\u0646\u063a\u0645\u0627\u0633<\/strong><\/td><\/tr><tr><td>5 \u0645\u0645 (1\/4 \u0628\u0648\u0635\u0629)<\/td><td>5 \u2013 8 \u062f\u0642\u0627\u0626\u0642<\/td><\/tr><tr><td>12 \u0645\u0644\u0645 (1\/2 \u0628\u0648\u0635\u0629)<\/td><td>10 \u2013 12 \u062f\u0642\u064a\u0642\u0629<\/td><\/tr><tr><td>20 \u0645\u0644\u0645 (3\/4 \u0628\u0648\u0635\u0629)<\/td><td>10 \u2013 15 \u062f\u0642\u064a\u0642\u0629<\/td><\/tr><tr><td>30 \u0645\u0644\u0645 (1 1\/2 \u0628\u0648\u0635\u0629)<\/td><td>15 \u2013 20 \u062f\u0642\u064a\u0642\u0629<\/td><\/tr><tr><td>50 \u0645\u0644\u0645 (2 \u0628\u0648\u0635\u0629)<\/td><td>20 \u2013 25 \u062f\u0642\u064a\u0642\u0629<\/td><\/tr><tr><td>100 \u0645\u0644\u0645 (4 \u0628\u0648\u0635\u0629)<\/td><td>30 \u2013 40 \u062f\u0642\u064a\u0642\u0629<\/td><\/tr><\/tbody><\/table><\/figure><p class=\"wp-block-paragraph\"><strong>\u0627\u0644\u062a\u0628\u0631\u064a\u062f \u0648\u0627\u0644\u062a\u0628\u0631\u064a\u062f<\/strong><\/p><p class=\"wp-block-paragraph\">\u0628\u0639\u062f \u0627\u0644\u0646\u0642\u0639 \u0641\u064a \u062d\u0645\u0627\u0645 \u0627\u0644\u0645\u0644\u062d\u060c \u064a\u062c\u0628 \u062a\u0628\u0631\u064a\u062f \u0627\u0644\u062c\u0632\u0621 \u0628\u0627\u0644\u0645\u0644\u062d \u062b\u0645 \u062a\u0631\u0643\u0647 \u0644\u064a\u0628\u0631\u062f \u0641\u064a \u0627\u0644\u0647\u0648\u0627\u0621 \u0627\u0644\u0633\u0627\u0643\u0646 \u062d\u062a\u0649 \u064a\u0635\u0644 \u0625\u0644\u0649 <strong>45 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \u0625\u0644\u0649 65 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629<\/strong> (<strong>120 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a \u0625\u0644\u0649 150 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a<\/strong>) \u0642\u0628\u0644 \u0627\u0644\u062a\u0644\u0637\u064a\u0641.<\/p><h4 class=\"wp-block-heading\"><strong>\u0627\u0644\u062a\u0644\u0637\u064a\u0641<\/strong><\/h4><p class=\"wp-block-paragraph\">\u064a\u062c\u0628 \u0623\u0646 \u064a\u062a\u0645 \u0630\u0644\u0643 \u0641\u064a \u0641\u0631\u0646 \u0627\u0644\u062d\u0645\u0644 \u0627\u0644\u062d\u0631\u0627\u0631\u064a \u0627\u0644\u0630\u064a \u0644\u0627 \u064a\u062a\u0645 \u0627\u0644\u062a\u062d\u0643\u0645 \u0641\u064a\u0647 \u0628\u0648\u0627\u0633\u0637\u0629 \u0627\u0644\u063a\u0644\u0627\u0641 \u0627\u0644\u062c\u0648\u064a. \u064a\u062c\u0628 \u0623\u0646 \u062a\u062a\u0645 \u0639\u0645\u0644\u064a\u0629 \u0627\u0644\u062a\u0644\u0637\u064a\u0641 \u0627\u0644\u0623\u0648\u0644\u064a\u0629 \u0628\u0645\u062c\u0631\u062f \u0623\u0646 \u064a\u0628\u0631\u062f \u0627\u0644\u062c\u0632\u0621 \u0625\u0644\u0649 \u0646\u0637\u0627\u0642 \u0645\u0646 <strong>45 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \u0625\u0644\u0649 65 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (120 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a \u0625\u0644\u0649 150 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/strong>\u060c \u0645\u062a\u0628\u0648\u0639\u064b\u0627 \u0628\u0627\u0644\u062a\u0628\u0631\u064a\u062f \u0625\u0644\u0649 \u062f\u0631\u062c\u0629 \u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u063a\u0631\u0641\u0629 \u0642\u0628\u0644 \u0625\u062c\u0631\u0627\u0621 \u062f\u0648\u0631\u0629 \u0627\u0644\u062a\u0644\u0637\u064a\u0641 \u0627\u0644\u062a\u0627\u0644\u064a\u0629.<\/p><ul class=\"wp-block-list\"><li><strong>\u0644\u0644\u0648\u0635\u0648\u0644 \u0625\u0644\u0649 HRC 60-62: <\/strong>\u0642\u0645 \u0628\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0628\u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0645\u0631\u062a\u064a\u0646<strong> 540 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (1005 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a) \u0644\u0645\u062f\u0629 60 \u0625\u0644\u0649 90 \u062f\u0642\u064a\u0642\u0629 \u0644\u0643\u0644 \u0628\u0648\u0635\u0629 \u0645\u0646 \u0627\u0644\u0633\u064f\u0645\u0643<\/strong>\u060c \u0645\u0639 \u0627\u0644\u062a\u0623\u0643\u062f \u0645\u0646 \u0623\u0646 \u0648\u0642\u062a \u0627\u0644\u062a\u0644\u0637\u064a\u0641 \u0644\u0627 \u064a\u0642\u0644 \u0639\u0646 90 \u062f\u0642\u064a\u0642\u0629.<\/li>\n\n<li><strong>\u0644\u062a\u062d\u0642\u064a\u0642 HRC 62-64:<\/strong> \u0642\u0645 \u0628\u062a\u0644\u0637\u064a\u0641 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0645\u0631\u062a\u064a\u0646 \u0639\u0646\u062f <strong>520 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (970 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/strong> \u0644\u0646\u0641\u0633 \u0627\u0644\u0645\u062f\u0629.<\/li>\n\n<li><strong>\u0644\u0632\u064a\u0627\u062f\u0629 \u0627\u0644\u0635\u0644\u0627\u0628\u0629:<\/strong> \u0645\u0632\u0627\u062c \u0645\u0632\u062f\u0648\u062c \u0641\u064a <strong>550 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (1020 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/strong> \u0644\u0644\u062d\u0635\u0648\u0644 \u0639\u0644\u0649 <strong>\u062d\u0642\u0648\u0642 \u0627\u0644\u0625\u0646\u0633\u0627\u0646 58-60<\/strong>.<\/li><\/ul><p class=\"wp-block-paragraph\">\u0625\u0630\u0627 \u0643\u0627\u0646\u062a \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0639\u0627\u0644\u064a\u0629 \u0627\u0644\u062f\u0642\u0629 \u062a\u062a\u0637\u0644\u0628 \u0627\u0633\u062a\u0642\u0631\u0627\u0631\u064b\u0627 \u0641\u064a \u0627\u0644\u0623\u0628\u0639\u0627\u062f \u0648\u062a\u0634\u0648\u064a\u0647\u064b\u0627 \u0636\u0626\u064a\u0644\u064b\u0627 \u0628\u0633\u0628\u0628 \u0627\u0644\u062a\u0634\u063a\u064a\u0644 \u0627\u0644\u0622\u0644\u064a \u0623\u0648 \u0645\u0639\u0627\u0644\u062c\u0627\u062a \u0627\u0644\u0633\u0637\u062d\u060c \u0641\u064a\u0645\u0643\u0646 \u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u062f\u0631\u062c\u0629 \u062d\u0631\u0627\u0631\u0629 \u0627\u062e\u062a\u064a\u0627\u0631\u064a\u0629 \u062b\u0627\u0644\u062b\u0629 \u0639\u0646\u062f <strong>400 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629<\/strong> (<strong>750 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a<\/strong>) \u064a\u0645\u0643\u0646 \u062a\u0637\u0628\u064a\u0642\u0647\u0627 \u0644\u062a\u062b\u0628\u064a\u062a \u0627\u0644\u0647\u064a\u0643\u0644.<\/p><h2 class=\"wp-block-heading\">\u062a\u0635\u0646\u064a\u0639 \u0648\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 DC53&nbsp;<\/h2><h3 class=\"wp-block-heading\">\u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0627\u062a \u0627\u0644\u0633\u0637\u062d\u064a\u0629<\/h3><h4 class=\"wp-block-heading\">\u0639\u0645\u0644\u064a\u0629 \u0627\u0644\u062a\u0628\u0631\u064a\u062f<\/h4><ul class=\"wp-block-list\"><li><strong>\u0627\u0644\u0646\u062a\u0631\u062a\u0629<\/strong><\/li><\/ul><p class=\"wp-block-paragraph\">\u0645\u062b\u0627\u0644\u064a\u0629 \u0644\u0644\u062a\u0635\u0644\u0628 \u0627\u0644\u0633\u0637\u062d\u064a\u060c \u064a\u0645\u0643\u0646 \u062a\u0637\u0628\u064a\u0642 \u0627\u0644\u0646\u062a\u0631\u062a\u0629 \u0639\u0646\u062f \u062f\u0631\u062c\u0627\u062a \u062d\u0631\u0627\u0631\u0629 \u0623\u0642\u0644 \u0645\u0646 <strong>500 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (930 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/strong> \u0644\u062a\u062c\u0646\u0628 \u0627\u0644\u0645\u0633\u0627\u0633 \u0628\u062e\u0635\u0627\u0626\u0635 \u0642\u0644\u0628 \u0627\u0644\u0641\u0648\u0644\u0627\u0630. \u0647\u0630\u0647 \u0627\u0644\u0639\u0645\u0644\u064a\u0629 \u0641\u0639\u0627\u0644\u0629 \u0644\u062a\u0639\u0632\u064a\u0632 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644 \u0645\u0639 \u0627\u0644\u062d\u0641\u0627\u0638 \u0639\u0644\u0649 \u0642\u0648\u0629 DC53.<\/p><ul class=\"wp-block-list\"><li><strong>\u0637\u0644\u0627\u0621\u0627\u062a PVD<\/strong><\/li><\/ul><p class=\"wp-block-paragraph\">\u0627\u0644\u0637\u0644\u0627\u0621\u0627\u062a \u0627\u0644\u0633\u0637\u062d\u064a\u0629 \u0645\u062b\u0644 <strong>\u062a\u064a\u0646<\/strong>, <strong>\u062a\u064a \u0633\u064a \u0625\u0646<\/strong>\u060c \u0648 <strong>\u0643\u0631 \u0646<\/strong> \u064a\u062a\u0645 \u062a\u0637\u0628\u064a\u0642\u0647\u0627 \u0639\u0627\u062f\u0629 \u0645\u0646 \u062e\u0644\u0627\u0644 \u0627\u0644\u062a\u0631\u0633\u064a\u0628 \u0627\u0644\u0641\u064a\u0632\u064a\u0627\u0626\u064a \u0644\u0644\u0628\u062e\u0627\u0631 (PVD). \u0644\u062a\u062d\u0642\u064a\u0642 \u0623\u0641\u0636\u0644 \u0627\u0644\u0646\u062a\u0627\u0626\u062c\u060c \u0642\u0645 \u0628\u062a\u0644\u0637\u064a\u0641 DC53 \u0625\u0644\u0649 \u0645\u0627 \u0644\u0627 \u064a\u0642\u0644 \u0639\u0646 <strong>520 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (970 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/strong> \u0642\u0628\u0644 \u062a\u0637\u0628\u064a\u0642 \u0647\u0630\u0647 \u0627\u0644\u0637\u0644\u0627\u0621\u0627\u062a.&nbsp;<\/p><p class=\"wp-block-paragraph\">\u0646\u0648\u0635\u064a \u0628\u062a\u0644\u0637\u064a\u0641 \u062b\u0627\u0644\u062b \u0639\u0646\u062f 400 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (750 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a) \u0644\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u062a\u064a \u062a\u062a\u0637\u0644\u0628 \u062f\u0642\u0629 \u0639\u0627\u0644\u064a\u0629\u060c \u062d\u064a\u062b \u064a\u0633\u0627\u0639\u062f \u0630\u0644\u0643 \u0641\u064a \u062a\u0642\u0644\u064a\u0644 \u0623\u064a \u062a\u063a\u064a\u064a\u0631\u0627\u062a \u0641\u064a \u0627\u0644\u0623\u0628\u0639\u0627\u062f.<\/p><h4 class=\"wp-block-heading\">\u0639\u0645\u0644\u064a\u0629 \u0633\u0627\u062e\u0646\u0629<\/h4><ul class=\"wp-block-list\"><li><strong>\u0637\u0644\u0627\u0621\u0627\u062a \u0627\u0644\u062a\u0631\u0633\u064a\u0628 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a \u0644\u0644\u0628\u062e\u0627\u0631<\/strong><\/li><\/ul><p class=\"wp-block-paragraph\">\u064a\u062a\u0645 \u062a\u0637\u0628\u064a\u0642 \u0637\u0644\u0627\u0621\u0627\u062a \u0627\u0644\u062a\u0631\u0633\u064a\u0628 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a \u0644\u0644\u0628\u062e\u0627\u0631 (CVD) \u0639\u0646\u062f \u062f\u0631\u062c\u0627\u062a \u062d\u0631\u0627\u0631\u0629 \u062a\u062a\u0631\u0627\u0648\u062d \u0628\u064a\u0646 <strong>925 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (1700 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/strong> \u0648 <strong>1040 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (1900 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/strong>. \u0628\u0639\u062f \u0637\u0644\u0627\u0621 \u0627\u0644\u062a\u0631\u0633\u064a\u0628 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a \u0644\u0644\u0628\u062e\u0627\u0631\u060c \u064a\u062a\u0645 \u0627\u0644\u062a\u0642\u0633\u064a\u0629 \u0639\u0646\u062f <strong>500 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (930 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a) \u0625\u0644\u0649 510 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (950 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/strong> \u0644\u0644\u062d\u0641\u0627\u0638 \u0639\u0644\u0649 \u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0645\u064a\u0643\u0627\u0646\u064a\u0643\u064a\u0629 \u0644\u0644\u0635\u0644\u0628.<\/p><ul class=\"wp-block-list\"><li><strong>\u0637\u0644\u0627\u0621\u0627\u062a \u0627\u0644\u0627\u0646\u062a\u0634\u0627\u0631 \u0627\u0644\u062d\u0631\u0627\u0631\u064a (TD)<\/strong><\/li><\/ul><p class=\"wp-block-paragraph\">\u064a\u062a\u0645 \u062a\u0637\u0628\u064a\u0642 \u0637\u0644\u0627\u0621\u0627\u062a TD \u0639\u0646\u062f \u062f\u0631\u062c\u0627\u062a \u062d\u0631\u0627\u0631\u0629 \u062a\u062a\u0631\u0627\u0648\u062d \u0628\u064a\u0646 <strong>1,010 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (1,850 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/strong> \u0648 <strong>1,030 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (1,886 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/strong>\u0644\u062a\u062d\u0642\u064a\u0642 \u0623\u0641\u0636\u0644 \u0635\u0644\u0627\u0628\u0629\u060c \u064a\u062c\u0628 \u062a\u0637\u0628\u064a\u0642 \u0637\u0644\u0627\u0621\u0627\u062a TD \u0639\u0646\u062f 1,030 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (1,886 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)\u060c \u0645\u062a\u0628\u0648\u0639\u0629 \u0628\u0639\u062f\u0629 \u062f\u0648\u0631\u0627\u062a \u062a\u0644\u0637\u064a\u0641 \u0639\u0646\u062f \u062f\u0631\u062c\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u0635\u062d\u064a\u062d\u0629.<\/p><h3 class=\"wp-block-heading\">\u0627\u0644\u062a\u0635\u0646\u064a\u0639<\/h3><p class=\"wp-block-paragraph\">\u062a\u0634\u062a\u0647\u0631 DC53 \u0628\u0642\u062f\u0631\u062a\u0647\u0627 \u0627\u0644\u0645\u0645\u062a\u0627\u0632\u0629 \u0639\u0644\u0649 \u0627\u0644\u062a\u0635\u0646\u064a\u0639\u060c \u0648\u0627\u0644\u062a\u064a \u064a\u0645\u0643\u0646 \u0623\u0646 \u062a\u0643\u0648\u0646 <strong>20-40% \u0623\u0633\u0631\u0639<\/strong> \u0645\u0646 \u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0623\u062f\u0648\u0627\u062a D2. \u0628\u0627\u0644\u0625\u0636\u0627\u0641\u0629 \u0625\u0644\u0649 \u0630\u0644\u0643\u060c \u0641\u0625\u0646\u0647 \u064a\u062e\u062a\u0628\u0631 <strong>50% \u062a\u0622\u0643\u0644 \u0623\u0642\u0644 \u0644\u0644\u0623\u062f\u0627\u0629<\/strong>\u060c \u0645\u0645\u0627 \u064a\u0642\u0644\u0644 \u0628\u0634\u0643\u0644 \u0643\u0628\u064a\u0631 \u0645\u0646 \u062a\u0643\u0627\u0644\u064a\u0641 \u0627\u0644\u062a\u0635\u0646\u064a\u0639 \u0648\u064a\u062d\u0633\u0646 \u0627\u0644\u0643\u0641\u0627\u0621\u0629.<\/p><h3 class=\"wp-block-heading\">\u0627\u0644\u0644\u062d\u0627\u0645<\/h3><p class=\"wp-block-paragraph\">\u0639\u0644\u0649 \u0627\u0644\u0631\u063a\u0645 \u0645\u0646 \u0625\u0645\u0643\u0627\u0646\u064a\u0629 \u0644\u062d\u0627\u0645 DC53\u060c \u0625\u0644\u0627 \u0623\u0646\u0647 \u064a\u062a\u0637\u0644\u0628 \u0639\u0646\u0627\u064a\u0629 \u062e\u0627\u0635\u0629 \u0644\u0645\u0646\u0639 \u062d\u062f\u0648\u062b \u0645\u0634\u0643\u0644\u0627\u062a \u0645\u062b\u0644 \u0627\u0644\u062a\u0634\u0642\u0642 \u0623\u0648 \u0627\u0644\u062a\u0634\u0648\u0647.<\/p><p class=\"wp-block-paragraph\"><strong>\u0646\u0635\u0627\u0626\u062d \u0627\u0644\u0644\u062d\u0627\u0645<\/strong>:<\/p><ul class=\"wp-block-list\"><li><strong>\u0642\u0636\u064a\u0628 \u0627\u0644\u0644\u062d\u0627\u0645<\/strong>:\u0627\u0633\u062a\u062e\u062f\u0645 <strong>\u0642\u0636\u064a\u0628 \u0627\u0644\u0644\u062d\u0627\u0645 H72A<\/strong>\u060c \u062a\u0633\u062a\u062e\u062f\u0645 \u0639\u0627\u062f\u0629\u064b \u0641\u064a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0639\u0627\u0644\u064a \u0627\u0644\u0643\u0631\u0628\u0648\u0646 \u0648\u0639\u0627\u0644\u064a \u0627\u0644\u0643\u0631\u0648\u0645. \u0648\u0647\u0630\u0627 \u064a\u0636\u0645\u0646 \u0627\u0644\u062a\u0648\u0627\u0641\u0642 \u0645\u0639 \u062a\u0631\u0643\u064a\u0628\u0629 DC53.<\/li>\n\n<li><strong>\u062c\u0641\u0641 \u0627\u0644\u0642\u0636\u064a\u0628<\/strong>:\u0644\u0645\u0646\u0639 \u062a\u0634\u0642\u0642\u0627\u062a \u0627\u0644\u0644\u062d\u0627\u0645\u060c \u0642\u0645 \u062f\u0627\u0626\u0645\u064b\u0627 \u0628\u062a\u062c\u0641\u064a\u0641 \u0642\u0636\u064a\u0628 \u0627\u0644\u0644\u062d\u0627\u0645 \u0642\u0628\u0644 \u0627\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0639\u0646 \u0637\u0631\u064a\u0642 \u062a\u0633\u062e\u064a\u0646\u0647 \u0625\u0644\u0649 <strong>350 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (650 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/strong> \u0644\u0645\u062f\u0629 \u0633\u0627\u0639\u0629 \u062a\u0642\u0631\u064a\u0628\u0627.<\/li>\n\n<li><strong>\u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629 \u0628\u0639\u062f \u0627\u0644\u0644\u062d\u0627\u0645<\/strong>:\u0646\u0638\u0631\u064b\u0627 \u0644\u0623\u0646 \u0627\u0644\u0644\u062d\u0627\u0645 \u064a\u0645\u0643\u0646 \u0623\u0646 \u064a\u0633\u0628\u0628 \u0636\u063a\u0648\u0637\u064b\u0627\u060c \u0641\u0645\u0646 \u0627\u0644\u0645\u0647\u0645 \u0625\u062c\u0631\u0627\u0621 \u0639\u0645\u0644\u064a\u0629 \u062a\u0635\u0644\u0628 \u0628\u0639\u062f \u0627\u0644\u0644\u062d\u0627\u0645 \u0641\u064a <strong>500 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (930 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a) \u0625\u0644\u0649 510 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (950 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/strong> \u0644\u0627\u0633\u062a\u0639\u0627\u062f\u0629 \u0627\u0644\u0642\u0648\u0629 \u0648\u0627\u0644\u0645\u062a\u0627\u0646\u0629 \u0644\u0640 DC53.<\/li><\/ul><h2 class=\"wp-block-heading\">\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 DC53<\/h2><p class=\"wp-block-paragraph\">\u064a\u064f\u0633\u062a\u062e\u062f\u0645 DC53 \u0639\u0644\u0649 \u0646\u0637\u0627\u0642 \u0648\u0627\u0633\u0639 \u0641\u064a \u0627\u0644\u0635\u0646\u0627\u0639\u0627\u062a \u0627\u0644\u062a\u064a \u062a\u062a\u0637\u0644\u0628 \u0642\u0648\u0629 \u0639\u0627\u0644\u064a\u0629 \u0648\u0635\u0644\u0627\u0628\u0629 \u0648\u0645\u0642\u0627\u0648\u0645\u0629 \u0644\u0644\u062a\u0622\u0643\u0644. \u062a\u062a\u0636\u0645\u0646 \u0628\u0639\u0636 \u062a\u0637\u0628\u064a\u0642\u0627\u062a\u0647 \u0627\u0644\u0639\u0645\u0644\u064a\u0629 \u0645\u0627 \u064a\u0644\u064a:<\/p><ul class=\"wp-block-list\"><li>\u0642\u0648\u0627\u0644\u0628 \u0627\u0644\u062e\u062a\u0645<\/li>\n\n<li>\u0642\u0648\u0627\u0644\u0628 \u0627\u0644\u062d\u0642\u0646<\/li>\n\n<li>\u0642\u0648\u0627\u0644\u0628 \u062a\u0642\u062f\u0645\u064a\u0629<\/li>\n\n<li>\u0642\u0648\u0627\u0644\u0628 \u0627\u0644\u062a\u0642\u0637\u064a\u0639<\/li>\n\n<li>\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0628\u062b\u0642<\/li>\n\n<li>\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u062a\u0634\u0643\u064a\u0644<\/li>\n\n<li>\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u0642\u0637\u0639 (\u0639\u0644\u0649 \u0633\u0628\u064a\u0644 \u0627\u0644\u0645\u062b\u0627\u0644\u060c \u0634\u0641\u0631\u0627\u062a \u0627\u0644\u0642\u0635\u060c \u0648\u0627\u0644\u0645\u0642\u0635\u0627\u062a)<\/li><\/ul><h2 class=\"wp-block-heading\">\u0647\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 DC53 \u062c\u064a\u062f \u0644\u0644\u0633\u0643\u0627\u0643\u064a\u0646\u061f<\/h2><p class=\"wp-block-paragraph\">\u0646\u0639\u0645. \u064a\u064f\u0639\u062f DC53 \u062e\u064a\u0627\u0631\u064b\u0627 \u0645\u0648\u062b\u0648\u0642\u064b\u0627 \u0628\u0647 \u0644\u0644\u0633\u0643\u0627\u0643\u064a\u0646\u060c \u0648\u062e\u0627\u0635\u0629 \u0641\u064a \u0627\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0627\u062a \u0627\u0644\u0635\u0646\u0627\u0639\u064a\u0629 \u0623\u0648 \u0627\u0644\u0634\u0627\u0642\u0629. \u0641\u0647\u0648 \u064a\u062d\u0642\u0642 \u062a\u0648\u0627\u0632\u0646\u064b\u0627 \u0642\u0648\u064a\u064b\u0627 \u0628\u064a\u0646 \u0627\u0644\u0635\u0644\u0627\u0628\u0629 \u0648\u0627\u0644\u0645\u062a\u0627\u0646\u0629\u060c \u0645\u0645\u0627 \u064a\u0636\u0645\u0646 \u0627\u0644\u0627\u062d\u062a\u0641\u0627\u0638 \u0628\u0627\u0644\u062d\u0627\u0641\u0629 \u0628\u0634\u0643\u0644 \u0645\u0645\u062a\u0627\u0632. \u0648\u0645\u0639 \u0630\u0644\u0643\u060c \u0628\u0627\u0644\u0646\u0633\u0628\u0629 \u0644\u0644\u0633\u0643\u0627\u0643\u064a\u0646 \u0627\u0644\u0645\u0633\u062a\u062e\u062f\u0645\u0629 \u0641\u064a \u0627\u0644\u0637\u0647\u064a\u060c \u0641\u0625\u0646 \u0623\u0646\u0648\u0627\u0639 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0623\u062e\u0631\u0649 \u0645\u062b\u0644 VG10 \u0623\u0648 S30V \u0645\u0641\u0636\u0644\u0629 \u0646\u0638\u0631\u064b\u0627 \u0644\u0645\u0642\u0627\u0648\u0645\u062a\u0647\u0627 \u0627\u0644\u0623\u0641\u0636\u0644 \u0644\u0644\u062a\u0622\u0643\u0644 \u0648\u0633\u0647\u0648\u0644\u0629 \u0634\u062d\u0630\u0647\u0627.<\/p><h2 class=\"wp-block-heading\">\u0645\u0627 \u0647\u064a \u0627\u0644\u0627\u062e\u062a\u0644\u0627\u0641\u0627\u062a \u0628\u064a\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 DC53 \u0648 M390\u061f<\/h2><p class=\"wp-block-paragraph\">\u062a\u062a\u0645\u062a\u0639 \u0645\u0627\u062f\u0629 M390 \u0628\u0625\u0645\u0643\u0627\u0646\u064a\u0629 \u0635\u0644\u0627\u0628\u0629 \u0623\u0639\u0644\u0649 \u0645\u0646 \u0645\u0627\u062f\u0629 DC53\u060c \u0648\u0644\u0643\u0646\u0647\u0627 \u0623\u0643\u062b\u0631 \u0647\u0634\u0627\u0634\u0629. \u0645\u0646 \u0646\u0627\u062d\u064a\u0629 \u0623\u062e\u0631\u0649\u060c \u062a\u062a\u0645\u062a\u0639 \u0645\u0627\u062f\u0629 DC53 \u0628\u0635\u0644\u0627\u0628\u0629 \u0623\u0643\u0628\u0631 \u0648\u0645\u0642\u0627\u0648\u0645\u0629 \u0623\u0643\u0628\u0631 \u0644\u0644\u062a\u0634\u0642\u0642\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647\u0627 \u0623\u0641\u0636\u0644 \u0644\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u062a\u064a \u062a\u0646\u0637\u0648\u064a \u0639\u0644\u0649 \u0636\u063a\u0648\u0637 \u0639\u0627\u0644\u064a\u0629.&nbsp;<\/p><p class=\"wp-block-paragraph\">\u063a\u0627\u0644\u0628\u064b\u0627 \u0645\u0627 \u064a\u062a\u0645 \u0627\u0633\u062a\u062e\u062f\u0627\u0645 M390 \u0641\u064a \u0634\u0641\u0631\u0627\u062a \u0627\u0644\u0633\u0643\u0627\u0643\u064a\u0646\u060c \u0628\u064a\u0646\u0645\u0627 \u064a\u0643\u0648\u0646 DC53 \u0623\u0643\u062b\u0631 \u0645\u0644\u0627\u0621\u0645\u0629 \u0644\u0644\u0623\u062f\u0648\u0627\u062a \u0648\u0627\u0644\u0642\u0648\u0627\u0644\u0628.<\/p><h2 class=\"wp-block-heading\">\u0627\u0628\u062d\u062b \u0639\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0639\u0627\u0644\u064a \u0627\u0644\u062c\u0648\u062f\u0629 DC53 \u0641\u064a SteelPro Group<\/h2><p class=\"wp-block-paragraph\">\u062a\u0648\u0641\u0631 \u0645\u062c\u0645\u0648\u0639\u0629 SteelPro \u0645\u0646\u062a\u062c\u0627\u062a \u0641\u0648\u0644\u0627\u0630\u064a\u0629 DC53 \u0639\u0627\u0644\u064a\u0629 \u0627\u0644\u062c\u0648\u062f\u0629\u060c \u0628\u0645\u0627 \u0641\u064a \u0630\u0644\u0643 \u0627\u0644\u0642\u0636\u0628\u0627\u0646 \u0648\u0627\u0644\u0623\u0644\u0648\u0627\u062d \u0648\u0627\u0644\u0635\u0641\u0627\u0626\u062d \u0648\u0627\u0644\u0642\u0636\u0628\u0627\u0646\u060c \u0648\u0643\u0644\u0647\u0627 \u062a\u062e\u0636\u0639 \u0644\u0636\u0648\u0627\u0628\u0637 \u062c\u0648\u062f\u0629 \u0635\u0627\u0631\u0645\u0629. \u0643\u0645\u0627 \u0646\u0642\u062f\u0645 <a href=\"https:\/\/steelprogroup.com\/ar\/tool-steel\/cr12mov\/\">\u0623\u062f\u0627\u0629 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 D2<\/a> \u0644\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0630\u0627\u062a \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644 \u0627\u0644\u0639\u0627\u0644\u064a\u0629.&nbsp;<\/p><p class=\"wp-block-paragraph\">\u0647\u0644 \u062a\u062d\u062a\u0627\u062c \u0625\u0644\u0649 \u0641\u0648\u0644\u0627\u0630 \u0639\u0627\u0644\u064a \u0627\u0644\u062c\u0648\u062f\u0629 \u0623\u0648 \u062d\u0644\u0648\u0644 \u0645\u062e\u0635\u0635\u0629\u061f \u0627\u062a\u0635\u0644 \u0628\u0646\u0627 \u0627\u0644\u064a\u0648\u0645 \u0644\u0644\u062d\u0635\u0648\u0644 \u0639\u0644\u0649 \u062f\u0639\u0645 \u0645\u0646 \u0627\u0644\u062e\u0628\u0631\u0627\u0621 \u0648\u0645\u0646\u062a\u062c\u0627\u062a \u0645\u062a\u0645\u064a\u0632\u0629!<\/p>","protected":false},"excerpt":{"rendered":"<p>SteelPro Group is a global leader in high-performance carbon steel, offering top-tier DC53 steel products. Our DC53 steel delivers unmatched [&hellip;]<\/p>","protected":false},"author":12,"featured_media":20184,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"_eb_attr":"","rank_math_lock_modified_date":false,"site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"categories":[4294,4293],"tags":[],"class_list":["post-20182","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-grades-tool-steel","category-tool-steel"],"acf":[],"_links":{"self":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts\/20182","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/users\/12"}],"replies":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/comments?post=20182"}],"version-history":[{"count":0,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts\/20182\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/media\/20184"}],"wp:attachment":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/media?parent=20182"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/categories?post=20182"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/tags?post=20182"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}