{"id":20477,"date":"2025-01-29T03:04:00","date_gmt":"2025-01-28T19:04:00","guid":{"rendered":"https:\/\/steelprogroup.com\/?p=20477"},"modified":"2025-01-21T10:51:23","modified_gmt":"2025-01-21T02:51:23","slug":"hsla-hr340la-sheets","status":"publish","type":"post","link":"https:\/\/steelprogroup.com\/ar\/automotive-steel\/hsla-hr340la-sheets\/","title":{"rendered":"\u0644\u0641\u0627\u0626\u0641 \u0627\u0644\u0635\u0644\u0628 GMW3032M HR340LA \u0627\u0644\u0635\u0644\u0628 \u0627\u0644\u0645\u062f\u0631\u0641\u0644 \u0639\u0644\u0649 \u0627\u0644\u0633\u0627\u062e\u0646"},"content":{"rendered":"<p class=\"wp-block-paragraph\">\u062a\u0642\u062f\u0645 \u0645\u062c\u0645\u0648\u0639\u0629 SteelPro \u0644\u0641\u0627\u0626\u0641 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 HR340LA\u060c \u0648\u0647\u064a \u0641\u0648\u0644\u0627\u0630 \u0645\u0646\u062e\u0641\u0636 \u0627\u0644\u0633\u0628\u0627\u0626\u0643 \u0639\u0627\u0644\u064a \u0627\u0644\u0642\u0648\u0629 \u0645\u0639\u062a\u0645\u062f \u0648\u0641\u0642\u064b\u0627 \u0644\u0645\u0639\u064a\u0627\u0631 GMW3032M. \u0648\u0647\u0648 \u0645\u0635\u0645\u0645 \u0644\u062a\u062d\u0642\u064a\u0642 \u0623\u062f\u0627\u0621 \u0627\u0633\u062a\u062b\u0646\u0627\u0626\u064a \u0641\u064a \u062a\u0635\u0646\u064a\u0639 \u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a \u0648\u0627\u0644\u0628\u0646\u0627\u0621 \u0648\u0627\u0644\u0622\u0644\u0627\u062a.<\/p><p class=\"wp-block-paragraph\">\u062a\u0633\u062a\u0643\u0634\u0641 \u0647\u0630\u0647 \u0627\u0644\u0645\u0642\u0627\u0644\u0629 \u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0641\u0631\u064a\u062f\u0629 \u0648\u0627\u0644\u0645\u0648\u0627\u0635\u0641\u0627\u062a \u0627\u0644\u0641\u0646\u064a\u0629 \u0648\u0639\u0645\u0644\u064a\u0627\u062a \u0627\u0644\u062a\u0635\u0646\u064a\u0639 \u0648\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0645\u0644\u0641\u0627\u062a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 HR340LA\u060c \u0627\u0644\u0645\u0635\u0645\u0645\u0629 \u062e\u0635\u064a\u0635\u064b\u0627 \u0644\u062a\u0644\u0628\u064a\u0629 \u0645\u062a\u0637\u0644\u0628\u0627\u062a \u0645\u0634\u0631\u0648\u0639\u0643.<\/p><h2 class=\"wp-block-heading\">\u0645\u0627 \u0647\u0648 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 HR340LA\u061f<\/h2><p class=\"wp-block-paragraph\">HR340LA \u0647\u0648 \u0641\u0648\u0644\u0627\u0630 \u0645\u0646\u062e\u0641\u0636 \u0627\u0644\u0633\u0628\u0627\u0626\u0643 \u0639\u0627\u0644\u064a \u0627\u0644\u0642\u0648\u0629\u060c \u062a\u0645\u062a \u0645\u0639\u0627\u0644\u062c\u062a\u0647 \u0628\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0637\u0631\u064a\u0642\u0629 \u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0633\u0627\u062e\u0646\u0629. \u0648\u0647\u0648 \u064a\u0648\u0641\u0631 \u062a\u0648\u0627\u0632\u0646\u064b\u0627 \u0645\u062b\u0627\u0644\u064a\u064b\u0627 \u0628\u064a\u0646 \u0627\u0644\u0642\u0648\u0629 \u0627\u0644\u0645\u064a\u0643\u0627\u0646\u064a\u0643\u064a\u0629 \u0648\u0642\u0627\u0628\u0644\u064a\u0629 \u0627\u0644\u0644\u062d\u0627\u0645 \u0627\u0644\u0645\u0645\u062a\u0627\u0632\u0629 \u0648\u0627\u0644\u0641\u0639\u0627\u0644\u064a\u0629 \u0645\u0646 \u062d\u064a\u062b \u0627\u0644\u062a\u0643\u0644\u0641\u0629. <strong>\u0627\u0644\u062d\u062f \u0627\u0644\u0623\u062f\u0646\u0649 \u0644\u0642\u0648\u0629 \u0627\u0644\u062e\u0636\u0648\u0639 340 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644<\/strong>\u064a\u0639\u062f \u0647\u0630\u0627 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0645\u0646\u0627\u0633\u0628\u064b\u0627 \u0644\u0644\u063a\u0627\u064a\u0629 \u0644\u0644\u0645\u0643\u0648\u0646\u0627\u062a \u0627\u0644\u062a\u064a \u062a\u062a\u0637\u0644\u0628 \u0627\u0644\u0645\u062a\u0627\u0646\u0629 \u062a\u062d\u062a \u0627\u0644\u0636\u063a\u0637\u060c \u0645\u062b\u0644 \u0627\u0644\u062a\u0639\u0632\u064a\u0632\u0627\u062a \u0627\u0644\u062e\u0627\u0635\u0629 \u0628\u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a\u060c \u0648\u0627\u0644\u0639\u0648\u0627\u0631\u0636 \u0627\u0644\u0647\u064a\u0643\u0644\u064a\u0629\u060c \u0648\u0627\u0644\u062f\u0639\u0627\u0645\u0627\u062a \u0627\u0644\u0635\u0646\u0627\u0639\u064a\u0629.<\/p><h2 class=\"wp-block-heading\">\u0627\u0644\u0645\u064a\u0632\u0627\u062a \u0627\u0644\u0631\u0626\u064a\u0633\u064a\u0629 \u0644\u0640 HR340LA Steel<\/h2><ul class=\"wp-block-list\"><li><strong>\u0642\u0648\u0629 \u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0633\u0627\u062e\u0646\u0629<\/strong>:\u0623\u062f\u0627\u0621 \u062b\u0627\u0628\u062a \u0641\u064a \u0627\u0644\u0634\u062f \u0648\u0627\u0644\u062e\u0636\u0648\u0639.<\/li>\n\n<li><strong>\u0645\u062d\u062a\u0648\u0649 \u0645\u0646\u062e\u0641\u0636 \u0627\u0644\u0643\u0631\u0628\u0648\u0646<\/strong>:\u064a\u0639\u0632\u0632 \u0642\u0627\u0628\u0644\u064a\u0629 \u0627\u0644\u062a\u0634\u0643\u064a\u0644 \u0648\u0633\u0647\u0648\u0644\u0629 \u0627\u0644\u0644\u062d\u0627\u0645.<\/li>\n\n<li><strong>\u0639\u0646\u0627\u0635\u0631 \u0627\u0644\u0633\u0628\u0627\u0626\u0643 \u0627\u0644\u062f\u0642\u064a\u0642\u0629<\/strong>:\u064a\u0636\u0645\u0646 \u0627\u0644\u062a\u064a\u062a\u0627\u0646\u064a\u0648\u0645 (Ti) \u0648\u0627\u0644\u0646\u064a\u0648\u0628\u064a\u0648\u0645 (Nb) \u0628\u0646\u064a\u0629 \u062d\u0628\u064a\u0628\u0627\u062a \u0648\u0645\u062a\u0627\u0646\u0629 \u0641\u0627\u0626\u0642\u0629.<\/li><\/ul><h2 class=\"wp-block-heading\">\u0623\u0628\u0639\u0627\u062f \u0648\u0645\u0639\u0627\u064a\u064a\u0631 \u0645\u0644\u0641\u0627\u062a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 HR340LA<\/h2><p class=\"wp-block-paragraph\">\u062a\u0642\u062f\u0645 \u0645\u062c\u0645\u0648\u0639\u0629 SteelPro \u0645\u0644\u0641\u0627\u062a \u0641\u0648\u0644\u0627\u0630\u064a\u0629 HR340LA \u0645\u062a\u0648\u0627\u0641\u0642\u0629 \u0645\u0639 <strong>\u062c\u064a \u0627\u0645 \u062f\u0628\u0644\u064a\u0648 3032 \u0627\u0645<\/strong>, <strong>EN 10149-2<\/strong>\u060c \u0648 <strong>\u0627\u064a\u0632\u0648 9001:2015<\/strong>\u062a\u0633\u0645\u062d \u0623\u0628\u0639\u0627\u062f\u0646\u0627 \u0627\u0644\u062f\u0642\u064a\u0642\u0629 \u0628\u0627\u0644\u062a\u0643\u0627\u0645\u0644 \u0627\u0644\u0633\u0644\u0633 \u0641\u064a \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0635\u0646\u0627\u0639\u064a\u0629 \u0627\u0644\u0645\u062e\u062a\u0644\u0641\u0629.<\/p><ul class=\"wp-block-list\"><li><strong>\u0633\u0645\u0627\u0643\u0629<\/strong>: 1.5 \u2013 12.0 \u0645\u0644\u0645 (0.059 \u2013 0.472 \u0628\u0648\u0635\u0629)<\/li>\n\n<li><strong>\u0639\u0631\u0636<\/strong>: 900 \u2013 2000 \u0645\u0644\u0645 (35.43 \u2013 78.74 \u0628\u0648\u0635\u0629)<\/li>\n\n<li><strong>\u0637\u0648\u0644<\/strong>:\u0645\u062a\u063a\u064a\u0631\u060c \u062d\u0633\u0628 \u062d\u062c\u0645 \u0627\u0644\u0645\u0644\u0641<\/li><\/ul><p class=\"wp-block-paragraph\">\u062a\u062a\u0648\u0641\u0631 \u0645\u0644\u0641\u0627\u062a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 HR340LA \u0627\u0644\u062e\u0627\u0635\u0629 \u0628\u0646\u0627 \u0645\u0639 \u062e\u064a\u0627\u0631\u0627\u062a \u0637\u0644\u0627\u0621 \u0627\u0644\u0632\u0646\u0643 \u0627\u0644\u0634\u0627\u0626\u0639\u0629 \u0645\u062b\u0644 <strong>\u0632\u062f120<\/strong> (\u0648\u0632\u0646 \u0627\u0644\u0637\u0644\u0627\u0621 \u0627\u0644\u0625\u062c\u0645\u0627\u0644\u064a 120 \u062c\u0645\/\u0645\u00b2)\u060c <strong>\u0632\u062f180<\/strong> (180 \u062c\u0645\/\u0645\u00b2)\u060c \u0648 <strong>\u0632275<\/strong> (275 \u062c\u0631\u0627\u0645\/\u0645\u00b2).&nbsp;<\/p><h2 class=\"wp-block-heading\">\u0627\u0644\u062a\u0631\u0643\u064a\u0628 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a \u0644\u0644\u0641\u0648\u0644\u0627\u0630 HR340LA<\/h2><p class=\"wp-block-paragraph\">\u062a\u0645 \u062a\u0635\u0645\u064a\u0645 HR340LA \u0644\u062a\u062d\u0642\u064a\u0642 \u062a\u0648\u0627\u0632\u0646 \u0645\u062b\u0627\u0644\u064a \u0628\u064a\u0646 \u0627\u0644\u0642\u0648\u0629 \u0648\u0627\u0644\u0642\u062f\u0631\u0629 \u0639\u0644\u0649 \u0627\u0644\u062a\u0634\u063a\u064a\u0644 \u0627\u0644\u0622\u0644\u064a. \u0643\u0645\u0627 \u0623\u0646 \u0645\u062d\u062a\u0648\u0627\u0647 \u0627\u0644\u0645\u0646\u062e\u0641\u0636 \u0645\u0646 \u0627\u0644\u0643\u0631\u0628\u0648\u0646 \u064a\u062f\u0639\u0645 \u0642\u0627\u0628\u0644\u064a\u0629 \u0627\u0644\u0644\u062d\u0627\u0645 \u0627\u0644\u0641\u0627\u0626\u0642\u0629 \u0648\u062a\u0642\u0644\u064a\u0644 \u062a\u0622\u0643\u0644 \u0627\u0644\u0623\u062f\u0648\u0627\u062a \u0623\u062b\u0646\u0627\u0621 \u0627\u0644\u062a\u0634\u063a\u064a\u0644 \u0627\u0644\u0622\u0644\u064a.<\/p><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u0639\u0646\u0635\u0631<\/strong><\/td><td><strong>\u0627\u0644\u0645\u062d\u062a\u0648\u0649 (%)<\/strong><\/td><td><strong>\u063a\u0627\u064a\u0629<\/strong><\/td><\/tr><tr><td>\u0627\u0644\u0643\u0631\u0628\u0648\u0646 (C)<\/td><td>\u2264 0.12<\/td><td>\u064a\u062d\u0627\u0641\u0638 \u0639\u0644\u0649 \u0642\u0627\u0628\u0644\u064a\u0629 \u0627\u0644\u0644\u062d\u0627\u0645 \u0648\u0627\u0644\u062a\u0634\u063a\u064a\u0644 \u0627\u0644\u0622\u0644\u064a.<\/td><\/tr><tr><td>\u0627\u0644\u0645\u0646\u063a\u0646\u064a\u0632 (Mn)<\/td><td>0.80 \u2013 1.50<\/td><td>\u064a\u0639\u0632\u0632 \u0642\u0648\u0629 \u0627\u0644\u0634\u062f \u0648\u0627\u0644\u0635\u0644\u0627\u0628\u0629.<\/td><\/tr><tr><td>\u0627\u0644\u0633\u064a\u0644\u064a\u0643\u0648\u0646 (Si)<\/td><td>\u2264 0.50<\/td><td>\u064a\u062d\u0633\u0646 \u0625\u0632\u0627\u0644\u0629 \u0627\u0644\u0623\u0643\u0633\u062f\u0629 \u0623\u062b\u0646\u0627\u0621 \u0627\u0644\u0625\u0646\u062a\u0627\u062c.<\/td><\/tr><tr><td>\u0627\u0644\u0641\u0648\u0633\u0641\u0648\u0631 (P)<\/td><td>\u2264 0.020<\/td><td>\u064a\u062a\u062d\u0643\u0645 \u0641\u064a \u0646\u0645\u0648 \u0627\u0644\u062d\u0628\u0648\u0628 \u0644\u062a\u062d\u0633\u064a\u0646 \u0642\u0627\u0628\u0644\u064a\u0629 \u0627\u0644\u062a\u0634\u0643\u064a\u0644.<\/td><\/tr><tr><td>\u0627\u0644\u0643\u0628\u0631\u064a\u062a (S)<\/td><td>\u2264 0.015<\/td><td>\u064a\u0642\u0644\u0644 \u0645\u0646 \u0647\u0634\u0627\u0634\u0629 \u0627\u0644\u0645\u0646\u062a\u062c\u0627\u062a \u0627\u0644\u0646\u0647\u0627\u0626\u064a\u0629.<\/td><\/tr><tr><td>\u0627\u0644\u062a\u064a\u062a\u0627\u0646\u064a\u0648\u0645 (Ti)<\/td><td>0.015 \u2013 0.060<\/td><td>\u064a\u0642\u0648\u0645 \u0628\u062a\u0646\u0642\u064a\u0629 \u0628\u0646\u064a\u0629 \u0627\u0644\u062d\u0628\u0648\u0628 \u0644\u0644\u062d\u0635\u0648\u0644 \u0639\u0644\u0649 \u0642\u0648\u0629 \u0625\u0636\u0627\u0641\u064a\u0629.<\/td><\/tr><tr><td>\u0627\u0644\u0646\u064a\u0648\u0628\u064a\u0648\u0645 (Nb)<\/td><td>0.010 \u2013 0.050<\/td><td>\u062a\u0642\u0648\u064a\u0629 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0645\u0646 \u062e\u0644\u0627\u0644 \u0627\u0644\u0633\u0628\u0627\u0626\u0643 \u0627\u0644\u062f\u0642\u064a\u0642\u0629.<\/td><\/tr><tr><td>\u0627\u0644\u0623\u0644\u0648\u0645\u0646\u064a\u0648\u0645<\/td><td>\u2265 0.015<\/td><td>\u064a\u0639\u0645\u0644 \u0643\u0645\u0646\u0642\u064a \u0644\u0644\u062d\u0628\u0648\u0628\u060c \u0645\u0645\u0627 \u064a\u0639\u0632\u0632 \u0644\u064a\u0648\u0646\u062a\u0647\u0627.<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0645\u064a\u0643\u0627\u0646\u064a\u0643\u064a\u0629 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 HR340LA<\/h2><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u0645\u0644\u0643\u064a\u0629<\/strong><\/td><td><strong>\u0642\u064a\u0645\u0629<\/strong><\/td><\/tr><tr><td>\u0642\u0648\u0629 \u0627\u0644\u062e\u0636\u0648\u0639 (\u0625\u0639\u0627\u062f\u0629)<\/td><td>340 - 460 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644 (52.2 - 66.7 \u0643\u064a\u0644\u0648 \u0628\u0627\u0633\u0643\u0627\u0644)<\/td><\/tr><tr><td>\u0642\u0648\u0629 \u0627\u0644\u0634\u062f (Rm)<\/td><td>440 \u2013 580 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644 (63.8 \u2013 84.1 \u0643\u064a\u0644\u0648 \u0628\u0627\u0633\u0643\u0627\u0644)<\/td><\/tr><tr><td>\u0627\u0644\u0627\u0633\u062a\u0637\u0627\u0644\u0629 (A80)<\/td><td>\u2265 18%<\/td><\/tr><tr><td>\u0627\u0644\u0635\u0644\u0627\u0628\u0629 (HRB)<\/td><td>\u2264 85<\/td><\/tr><tr><td>\u0637\u0627\u0642\u0629 \u0627\u0644\u062a\u0623\u062b\u064a\u0631 (\u062a\u0634\u0627\u0631\u0628\u064a \u0627\u0644\u062e\u0627\u0645\u0633)<\/td><td>\u2265 30 \u062c\u0648\u0644 \u0639\u0646\u062f -20 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 (22.1 \u0642\u062f\u0645 \u0631\u0637\u0644 \u0639\u0646\u062f -4 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a)<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u0625\u0646\u062a\u0627\u062c \u0648\u0645\u0639\u0627\u0644\u062c\u0629 \u0644\u0641\u0627\u0626\u0641 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 HR340LA<\/h2><p class=\"wp-block-paragraph\">\u062a\u062a\u0636\u0645\u0646 \u0639\u0645\u0644\u064a\u0629 \u0625\u0646\u062a\u0627\u062c \u0645\u0644\u0641\u0627\u062a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 HR340LA \u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0633\u0627\u062e\u0646\u0629 \u0648\u0627\u0644\u062a\u062e\u0644\u064a\u0644 \u0648\u062d\u0644\u0648\u0644 \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0645\u062e\u0635\u0635\u0629 \u0627\u0644\u0645\u0635\u0645\u0645\u0629 \u062e\u0635\u064a\u0635\u064b\u0627 \u0644\u062a\u0644\u0628\u064a\u0629 \u0627\u0644\u0645\u062a\u0637\u0644\u0628\u0627\u062a \u0627\u0644\u0635\u0646\u0627\u0639\u064a\u0629.<\/p><p class=\"wp-block-paragraph\">\u0628\u0627\u0644\u0645\u0642\u0627\u0631\u0646\u0629 \u0645\u0639 \u0641\u0648\u0644\u0627\u0630 CR340LA\u060c \u0644\u0627 \u062a\u062e\u0636\u0639 \u0644\u0641\u0627\u0626\u0641 \u0641\u0648\u0644\u0627\u0630 HR340LA \u0644\u0644\u062a\u0635\u0644\u0628 \u0623\u062b\u0646\u0627\u0621 \u0639\u0645\u0644\u064a\u0629 \u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0633\u0627\u062e\u0646\u0629\u060c \u0648\u0628\u0627\u0644\u062a\u0627\u0644\u064a \u0641\u0647\u064a \u0623\u0643\u062b\u0631 \u0644\u064a\u0648\u0646\u0629 \u0648\u0641\u0639\u0627\u0644\u064a\u0629 \u0645\u0646 \u062d\u064a\u062b \u0627\u0644\u062a\u0643\u0644\u0641\u0629. \u0648\u0645\u0639 \u0630\u0644\u0643\u060c \u0641\u0625\u0646 \u0633\u0637\u062d\u0647\u0627 \u0623\u0643\u062b\u0631 \u062e\u0634\u0648\u0646\u0629 \u0648\u0642\u062f \u062a\u062d\u062a\u0627\u062c \u0625\u0644\u0649 \u0645\u0639\u0627\u0644\u062c\u0629 \u0625\u0636\u0627\u0641\u064a\u0629\u060c \u0645\u062b\u0644 \u0627\u0644\u062a\u062e\u0644\u064a\u0644 \u0648\u0627\u0644\u0632\u064a\u062a\u060c \u0644\u062a\u062d\u0633\u064a\u0646 \u0627\u0644\u062a\u0634\u0637\u064a\u0628.<\/p><p class=\"wp-block-paragraph\">\u0641\u064a SteelPro Group\u060c \u0646\u0633\u062a\u062e\u062f\u0645 \u062a\u0642\u0646\u064a\u0627\u062a \u0645\u062a\u0642\u062f\u0645\u0629 \u0644\u0636\u0645\u0627\u0646 \u062c\u0648\u062f\u0629 \u0639\u0627\u0644\u064a\u0629 \u0644\u0645\u0644\u0641\u0627\u062a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 HR340LA. \u0625\u0644\u064a\u0643 \u0643\u064a\u0641 \u062a\u064f\u062d\u062f\u062b \u0639\u0645\u0644\u064a\u0627\u062a\u0646\u0627 \u0641\u0631\u0642\u064b\u0627:<\/p><ul class=\"wp-block-list\"><li>\u0628\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0623\u062d\u062f\u062b \u062a\u0642\u0646\u064a\u0627\u062a \u0627\u0644\u062a\u0628\u0631\u064a\u062f \u0628\u0627\u0644\u0645\u0627\u0621\u060c \u0646\u0642\u0648\u0645 \u0628\u062a\u0628\u0631\u064a\u062f \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0628\u0633\u0631\u0639\u0627\u062a \u22651000 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629\/\u062b\u0627\u0646\u064a\u0629. \u064a\u0639\u0645\u0644 \u0647\u0630\u0627 \u0627\u0644\u062a\u0628\u0631\u064a\u062f \u0627\u0644\u0633\u0631\u064a\u0639 \u0639\u0644\u0649 \u062a\u062d\u0633\u064a\u0646 \u0642\u0648\u0629 \u0648\u0645\u062a\u0627\u0646\u0629 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 HR340LA.<\/li>\n\n<li>\u064a\u0633\u062a\u062e\u062f\u0645 \u0641\u0631\u0646 \u0627\u0644\u062a\u0644\u062f\u064a\u0646 \u0627\u0644\u0623\u0646\u0628\u0648\u0628\u064a \u0627\u0644\u0645\u0634\u0639 \u0639\u0645\u0648\u062f\u064a\u064b\u0627 \u0644\u062f\u064a\u0646\u0627 \u0639\u0646\u0627\u0635\u0631 \u062a\u062d\u0643\u0645 \u0623\u0648\u062a\u0648\u0645\u0627\u062a\u064a\u0643\u064a\u0629 \u0641\u064a \u062f\u0631\u062c\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0644\u0636\u0645\u0627\u0646 \u062e\u0635\u0627\u0626\u0635 \u0641\u0648\u0644\u0627\u0630\u064a\u0629 \u0645\u0648\u062d\u062f\u0629\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647 \u0623\u0642\u0648\u0649 \u0648\u0623\u0633\u0647\u0644 \u0641\u064a \u0627\u0644\u0639\u0645\u0644.<\/li>\n\n<li>\u062a\u0633\u0627\u0639\u062f\u0646\u0627 \u0645\u0639\u062f\u0627\u062a \u0627\u0644\u062a\u0628\u0631\u064a\u062f \u0627\u0644\u062e\u0627\u0635\u0629 \u0641\u064a \u0625\u0646\u0634\u0627\u0621 \u0641\u0648\u0644\u0627\u0630 \u0639\u0627\u0644\u064a \u0627\u0644\u0642\u0648\u0629 \u0628\u062c\u0648\u062f\u0629 \u0648\u0623\u062f\u0627\u0621 \u062b\u0627\u0628\u062a\u064a\u0646.<\/li><\/ul><p class=\"wp-block-paragraph\">\u064a\u0645\u0643\u0646\u0646\u0627 \u0623\u064a\u0636\u064b\u0627 \u062a\u0642\u062f\u064a\u0645 \u0645\u0639\u0627\u0644\u062c\u0627\u062a \u0633\u0637\u062d\u064a\u0629 \u0645\u062a\u0642\u062f\u0645\u0629 \u0645\u062b\u0644 \u0627\u0644\u062c\u0644\u0641\u0646\u0629 \u0648\u0637\u0644\u0627\u0621 \u0627\u0644\u0645\u0633\u062d\u0648\u0642 \u0648\u0627\u0644\u0641\u0648\u0633\u0641\u0627\u062a.<\/p><h2 class=\"wp-block-heading\">\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0645\u0644\u0641\u0627\u062a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 HR340LA<\/h2><p class=\"wp-block-paragraph\">\u062a\u062d\u0638\u0649 \u0645\u0644\u0641\u0627\u062a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 HR340LA \u0628\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0648\u0627\u0633\u0639 \u0627\u0644\u0646\u0637\u0627\u0642 \u0641\u064a \u0627\u0644\u0635\u0646\u0627\u0639\u0627\u062a \u0628\u0633\u0628\u0628 \u0642\u0648\u062a\u0647\u0627 \u0648\u0642\u062f\u0631\u062a\u0647\u0627 \u0639\u0644\u0649 \u0627\u0644\u062a\u0643\u064a\u0641 \u0648\u0641\u0639\u0627\u0644\u064a\u062a\u0647\u0627 \u0645\u0646 \u062d\u064a\u062b \u0627\u0644\u062a\u0643\u0644\u0641\u0629.<\/p><h3 class=\"wp-block-heading\">\u0635\u0646\u0627\u0639\u0629 \u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a<\/h3><ul class=\"wp-block-list\"><li><strong>\u0647\u064a\u0627\u0643\u0644 \u0645\u0642\u0627\u0648\u0645\u0629 \u0644\u0644\u0635\u062f\u0645\u0627\u062a<\/strong>:\u0639\u0648\u0627\u0631\u0636 \u0627\u0644\u062a\u0639\u0632\u064a\u0632 \u0648\u0645\u0646\u0627\u0637\u0642 \u0627\u0644\u062a\u062c\u0639\u064a\u062f \u0644\u062a\u0639\u0632\u064a\u0632 \u0627\u0644\u0633\u0644\u0627\u0645\u0629.<\/li>\n\n<li><strong>\u0645\u0643\u0648\u0646\u0627\u062a \u0627\u0644\u062a\u0639\u0644\u064a\u0642<\/strong>:\u0623\u0630\u0631\u0639 \u0627\u0644\u062a\u062d\u0643\u0645 \u0648\u0627\u0644\u0645\u062b\u0628\u062a\u0627\u062a \u0644\u0644\u062d\u0635\u0648\u0644 \u0639\u0644\u0649 \u0623\u062f\u0627\u0621 \u0641\u0627\u0626\u0642.<\/li>\n\n<li><strong>\u0625\u0637\u0627\u0631\u0627\u062a \u0627\u0644\u0647\u064a\u0643\u0644<\/strong>:\u0636\u0645\u0627\u0646 \u0627\u0644\u0645\u062a\u0627\u0646\u0629 \u0627\u0644\u0647\u064a\u0643\u0644\u064a\u0629 \u0645\u0639 \u062a\u0642\u0644\u064a\u0644 \u0627\u0644\u0648\u0632\u0646.<\/li><\/ul><h3 class=\"wp-block-heading\">\u0642\u0637\u0627\u0639 \u0627\u0644\u0628\u0646\u0627\u0621<\/h3><ul class=\"wp-block-list\"><li><strong>\u0627\u0644\u0639\u0648\u0627\u0631\u0636 \u0648\u0627\u0644\u0623\u0639\u0645\u062f\u0629 \u0627\u0644\u0625\u0646\u0634\u0627\u0626\u064a\u0629<\/strong>:\u062f\u0639\u0645 \u0627\u0644\u0623\u0637\u0631 \u0630\u0627\u062a \u0627\u0644\u062a\u062d\u0645\u064a\u0644 \u0627\u0644\u0639\u0627\u0644\u064a.<\/li>\n\n<li><strong>\u0644\u0648\u062d\u0627\u062a \u0635\u0646\u0627\u0639\u064a\u0629<\/strong>:\u0623\u0644\u0648\u0627\u062d \u062e\u0641\u064a\u0641\u0629 \u0627\u0644\u0648\u0632\u0646 \u0648\u0637\u0648\u064a\u0644\u0629 \u0627\u0644\u0623\u0645\u062f \u0644\u0644\u0645\u0634\u0627\u0631\u064a\u0639 \u0648\u0627\u0633\u0639\u0629 \u0627\u0644\u0646\u0637\u0627\u0642.<\/li>\n\n<li><strong>\u0627\u0644\u062c\u0633\u0648\u0631<\/strong>:\u0645\u0643\u0648\u0646\u0627\u062a \u062a\u062d\u0645\u0644 \u0627\u0644\u0623\u062d\u0645\u0627\u0644 \u0630\u0627\u062a \u0645\u0642\u0627\u0648\u0645\u0629 \u0639\u0627\u0644\u064a\u0629 \u0644\u0644\u062a\u0639\u0628.<\/li><\/ul><h3 class=\"wp-block-heading\">\u062a\u0635\u0646\u064a\u0639 \u0627\u0644\u0622\u0644\u0627\u062a<\/h3><ul class=\"wp-block-list\"><li><strong>\u0642\u0637\u0639 \u063a\u064a\u0627\u0631 \u0627\u0644\u0645\u0639\u062f\u0627\u062a \u0627\u0644\u062b\u0642\u064a\u0644\u0629<\/strong>:\u0627\u0644\u0623\u0642\u0648\u0627\u0633 \u0648\u0627\u0644\u062f\u0639\u0627\u0645\u0627\u062a \u0648\u0627\u0644\u062a\u0639\u0632\u064a\u0632\u0627\u062a \u0644\u0644\u0622\u0644\u0627\u062a \u0630\u0627\u062a \u0627\u0644\u0636\u063a\u0637 \u0627\u0644\u0639\u0627\u0644\u064a.<\/li>\n\n<li><strong>\u0627\u0644\u0645\u0639\u062f\u0627\u062a \u0627\u0644\u0632\u0631\u0627\u0639\u064a\u0629<\/strong>:\u0645\u0643\u0648\u0646\u0627\u062a \u0645\u062a\u064a\u0646\u0629 \u0644\u0644\u0639\u0645\u0644\u064a\u0627\u062a \u0627\u0644\u0645\u064a\u062f\u0627\u0646\u064a\u0629 \u0627\u0644\u0635\u0639\u0628\u0629.<\/li><\/ul><h2 class=\"wp-block-heading\">\u0644\u0645\u0627\u0630\u0627 \u062a\u062e\u062a\u0627\u0631 SteelPro Group \u0644\u0645\u0646\u062a\u062c\u0627\u062a HR340LA \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630\u061f<\/h2><p class=\"wp-block-paragraph\">\u0641\u064a SteelPro Group\u060c \u0646\u0642\u062f\u0645 \u0644\u0641\u0627\u0626\u0641 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 HR340LA \u0627\u0644\u0645\u0639\u062a\u0645\u062f\u0629 \u0645\u0646 GMW3032M \u0628\u062c\u0648\u062f\u0629 \u0644\u0627 \u0645\u062b\u064a\u0644 \u0644\u0647\u0627. \u0643\u0645\u0627 \u0646\u0642\u062f\u0645 \u0645\u0646\u062a\u062c\u0627\u062a \u0623\u062e\u0631\u0649 \u0645\u062b\u0644 <a href=\"https:\/\/steelprogroup.com\/ar\/automotive-steel\/dp600\/\">\u0635\u0641\u0627\u0626\u062d \u0627\u0644\u0641\u0648\u0644\u0627\u0630 DP600<\/a>\u0645\u0646 \u062d\u0644\u0648\u0644 \u0627\u0644\u0642\u0637\u0639 \u0627\u0644\u0645\u0635\u0645\u0645\u0629 \u062e\u0635\u064a\u0635\u064b\u0627 \u0625\u0644\u0649 \u0645\u0639\u0627\u0644\u062c\u0627\u062a \u0627\u0644\u0623\u0633\u0637\u062d \u0627\u0644\u0645\u062a\u0642\u062f\u0645\u0629\u060c \u062a\u0636\u0645\u0646 \u062e\u062f\u0645\u0627\u062a\u0646\u0627 \u0627\u0644\u0634\u0627\u0645\u0644\u0629 \u0623\u0646 \u0643\u0644 \u0645\u0646\u062a\u062c \u064a\u0644\u0628\u064a \u0645\u0648\u0627\u0635\u0641\u0627\u062a\u0643 \u0627\u0644\u062f\u0642\u064a\u0642\u0629.<\/p><h3 class=\"wp-block-heading\">\u0645\u0632\u0627\u064a\u0627 \u0627\u0644\u0634\u0631\u0627\u0643\u0629 \u0645\u0639\u0646\u0627<\/h3><ul class=\"wp-block-list\"><li>\u0625\u0645\u062f\u0627\u062f \u062b\u0627\u0628\u062a \u0648\u0642\u062f\u0631\u0629 \u0625\u0646\u062a\u0627\u062c \u0643\u0628\u064a\u0631\u0629.<\/li>\n\n<li>\u062a\u0635\u0646\u064a\u0639 \u062f\u0642\u064a\u0642 \u0628\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u062a\u0643\u0646\u0648\u0644\u0648\u062c\u064a\u0627 \u0627\u0644\u0645\u062a\u0637\u0648\u0631\u0629.<\/li>\n\n<li>\u062d\u0644\u0648\u0644 \u0645\u0635\u0645\u0645\u0629 \u062e\u0635\u064a\u0635\u064b\u0627 \u0644\u0645\u062c\u0645\u0648\u0639\u0629 \u0645\u062a\u0646\u0648\u0639\u0629 \u0645\u0646 \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a.<\/li><\/ul><p class=\"wp-block-paragraph\"><\/p>","protected":false},"excerpt":{"rendered":"<p>SteelPro Group introduces HR340LA Steel Coils, a high-strength low-alloy (HSLA) steel certified to the GMW3032M standard. It is designed for [&hellip;]<\/p>","protected":false},"author":1,"featured_media":20481,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"_eb_attr":"","rank_math_lock_modified_date":false,"site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"categories":[4306],"tags":[],"class_list":["post-20477","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-automotive-steel"],"acf":[],"_links":{"self":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts\/20477","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/comments?post=20477"}],"version-history":[{"count":0,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts\/20477\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/media\/20481"}],"wp:attachment":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/media?parent=20477"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/categories?post=20477"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/tags?post=20477"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}