{"id":21044,"date":"2025-02-28T02:32:00","date_gmt":"2025-02-27T18:32:00","guid":{"rendered":"https:\/\/steelprogroup.com\/?p=21044"},"modified":"2025-02-28T14:43:50","modified_gmt":"2025-02-28T06:43:50","slug":"ppgi","status":"publish","type":"post","link":"https:\/\/steelprogroup.com\/ar\/galvanized-steel\/knowledge\/ppgi\/","title":{"rendered":"\u0645\u0627 \u0647\u0648 PPGI: \u0627\u0644\u062a\u0639\u0631\u064a\u0641 \u0648\u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0648\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a"},"content":{"rendered":"<p class=\"c2 wp-block-paragraph\"><span class=\"c6\">GI\u060c \u0648\u0647\u0648 \u0627\u062e\u062a\u0635\u0627\u0631 \u0641\u064a \u0627\u0644\u0623\u0635\u0644 \u0644\u0640 Galvanized Iron\u060c \u0643\u0627\u0646 \u064a\u064f\u0634\u0627\u0631 \u0625\u0644\u064a\u0647 \u062a\u0642\u0644\u064a\u062f\u064a\u064b\u0627 \u0628\u0627\u0644\u062d\u062f\u064a\u062f \u0627\u0644\u0645\u062c\u0644\u0641\u0646 \u0643\u0647\u0631\u0628\u0627\u0626\u064a\u064b\u0627 \u0648\u0644\u0643\u0646\u0647 \u0627\u0644\u0622\u0646 \u064a\u0639\u0646\u064a \u0639\u0645\u0648\u0645\u064b\u0627 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u062c\u0644\u0641\u0646. PPGI \u0647\u0648 \u0634\u0643\u0644 \u0645\u062a\u0642\u062f\u0645 \u0645\u0646 GI\u060c \u0645\u0645\u0627 \u064a\u0639\u0632\u0632 \u0623\u062f\u0627\u0626\u0647 \u0628\u0625\u0636\u0627\u0641\u0629 \u0637\u0628\u0642\u0627\u062a \u0625\u0636\u0627\u0641\u064a\u0629.<\/span><\/p><p class=\"c2 wp-block-paragraph\"><span class=\"c6\">\u062a\u062a\u0646\u0627\u0648\u0644 \u0647\u0630\u0647 \u0627\u0644\u0645\u0642\u0627\u0644\u0629 \u0623\u0633\u0627\u0633\u064a\u0627\u062a PPGI\u060c \u0628\u0645\u0627 \u0641\u064a \u0630\u0644\u0643 \u0645\u0639\u0646\u0627\u0647\u0627 \u0648\u062e\u0635\u0627\u0626\u0635\u0647\u0627 \u0627\u0644\u0631\u0626\u064a\u0633\u064a\u0629 \u0648\u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0627\u062a\u0647\u0627 \u0627\u0644\u0634\u0627\u0626\u0639\u0629. \u0643\u0645\u0627 \u062a\u0648\u0636\u062d \u0627\u0644\u0641\u0631\u0648\u0642 \u0628\u064a\u0646 PPGI \u0648PPGL\u060c \u0645\u0645\u0627 \u064a\u0648\u0641\u0631 \u0641\u0647\u0645\u064b\u0627 \u0643\u0627\u0645\u0644\u0627\u064b \u0644\u0645\u0643\u0627\u0646\u0629 \u0643\u0644 \u0645\u0627\u062f\u0629.<\/span><\/p><h2 class=\"wp-block-heading c1\" id=\"h.4z4133cmobip\"><span class=\"c12\">\u0645\u0627 \u0647\u064a \u0645\u0627\u062f\u0629 PPGI\u061f<\/span><\/h2><p class=\"c2 wp-block-paragraph\"><span class=\"c6\">PPGI\u060c \u0623\u0648 \u0627\u0644\u062d\u062f\u064a\u062f \u0627\u0644\u0645\u062c\u0644\u0641\u0646 \u0627\u0644\u0645\u0637\u0644\u064a \u0645\u0633\u0628\u0642\u064b\u0627\u060c \u0648\u0627\u0644\u0645\u0639\u0631\u0648\u0641 \u0623\u064a\u0636\u064b\u0627 \u0628\u0627\u0633\u0645 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u062c\u0644\u0641\u0646 \u0627\u0644\u0645\u0637\u0644\u064a \u0628\u0627\u0644\u0623\u0644\u0648\u0627\u0646\u060c \u0647\u0648 \u0641\u0648\u0644\u0627\u0630 \u0645\u062c\u0644\u0641\u0646 \u0645\u0637\u0644\u064a \u0645\u0633\u0628\u0642\u064b\u0627 \u0642\u0628\u0644 \u0627\u0644\u062a\u0634\u0643\u064a\u0644. \u064a\u062a\u0648\u0627\u0641\u0642 \u0645\u0639 \u0645\u0639\u0627\u064a\u064a\u0631 ASTM A755 \u0648EN 10169 \u0648GB\/T 12754. \u064a\u0642\u0627\u0648\u0645 PPGI \u0627\u0644\u062a\u0622\u0643\u0644 \u0648\u0627\u0644\u0637\u0642\u0633 \u0648\u0627\u0644\u0623\u0634\u0639\u0629 \u0641\u0648\u0642 \u0627\u0644\u0628\u0646\u0641\u0633\u062c\u064a\u0629\u060c \u0645\u0645\u0627 \u064a\u0648\u0641\u0631 \u0645\u062a\u0627\u0646\u0629 \u0645\u0645\u062a\u0627\u0632\u0629 \u0644\u0644\u0623\u0644\u0648\u0627\u0646 \u0648\u0633\u0637\u062d\u064b\u0627 \u0623\u0645\u0644\u0633\u064b\u0627. \u064a\u0633\u062a\u062e\u062f\u0645 \u0639\u0644\u0649 \u0646\u0637\u0627\u0642 \u0648\u0627\u0633\u0639 \u0641\u064a \u0627\u0644\u0628\u0646\u0627\u0621 \u0648\u0627\u0644\u0623\u062c\u0647\u0632\u0629 \u0648\u0627\u0644\u0623\u062b\u0627\u062b \u0648\u0623\u062c\u0632\u0627\u0621 \u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a \u0648\u064a\u062a\u0648\u0641\u0631 \u0628\u0634\u0643\u0644 \u0623\u0633\u0627\u0633\u064a \u0641\u064a \u0623\u0634\u0643\u0627\u0644 \u0644\u0641\u0627\u0626\u0641 \u0648\u0635\u0641\u0627\u0626\u062d.<\/span><\/p><h2 class=\"wp-block-heading c1\" id=\"h.h8ii5y979n7r\"><span class=\"c12\">\u062e\u0635\u0627\u0626\u0635 \u0648\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 PPGI<\/span><\/h2><h3 class=\"wp-block-heading c1\" id=\"h.61xsewd9mln2\"><span class=\"c11\">\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644<\/span><\/h3><p class=\"c2 wp-block-paragraph\"><span class=\"c6\">\u062a\u062a\u0645\u064a\u0632 \u0645\u0627\u062f\u0629 PPGI \u0628\u0645\u0642\u0627\u0648\u0645\u0629 \u0639\u0627\u0644\u064a\u0629 \u0644\u0644\u062a\u0622\u0643\u0644\u060c \u0648\u0630\u0644\u0643 \u0628\u0641\u0636\u0644 \u0637\u0644\u0627\u0621 \u0627\u0644\u0632\u0646\u0643 \u0627\u0644\u0645\u062c\u0644\u0641\u0646 \u0648\u0637\u0628\u0642\u0627\u062a \u0627\u0644\u0637\u0644\u0627\u0621 \u0627\u0644\u0648\u0627\u0642\u064a\u0629. \u062a\u0639\u0645\u0644 \u0637\u0628\u0642\u0629 \u0627\u0644\u0632\u0646\u0643 \u0639\u0644\u0649 \u062d\u0645\u0627\u064a\u0629 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0648\u062a\u0648\u0641\u0631 \u062d\u0645\u0627\u064a\u0629 \u0636\u062f \u0627\u0644\u062a\u0644\u0641 \u0641\u064a \u062d\u0627\u0644\u0629 \u0627\u0644\u062e\u062f\u0634. \u0643\u0645\u0627 \u062a\u0639\u0645\u0644 \u0637\u0628\u0642\u0627\u062a \u0627\u0644\u0637\u0644\u0627\u0621 \u0639\u0644\u0649 \u0633\u062f \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0628\u0634\u0643\u0644 \u0623\u0643\u0628\u0631\u060c \u0645\u0645\u0627 \u064a\u062d\u0645\u064a\u0647 \u0645\u0646 \u0627\u0644\u0631\u0637\u0648\u0628\u0629 \u0648\u0627\u0644\u0645\u0648\u0627\u062f \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629 \u0648\u0627\u0644\u062a\u0639\u0631\u0636 \u0644\u0644\u0623\u0634\u0639\u0629 \u0641\u0648\u0642 \u0627\u0644\u0628\u0646\u0641\u0633\u062c\u064a\u0629. \u0648\u0647\u0630\u0627 \u064a\u062c\u0639\u0644 \u0645\u0627\u062f\u0629 PPGI \u0645\u062a\u064a\u0646\u0629 \u0648\u0645\u0648\u062b\u0648\u0642\u0629 \u0641\u064a \u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u0635\u0639\u0628\u0629\u060c \u0648\u062a\u062d\u0627\u0641\u0638 \u0639\u0644\u0649 \u0633\u0644\u0627\u0645\u062a\u0647\u0627 \u0648\u062c\u0627\u0630\u0628\u064a\u062a\u0647\u0627 \u0627\u0644\u0628\u0635\u0631\u064a\u0629 \u0644\u0641\u062a\u0631\u0629 \u0637\u0648\u064a\u0644\u0629.<\/span><\/p><h3 class=\"wp-block-heading c1\" id=\"h.p50736yu4wcg\"><span class=\"c11\">\u0627\u0644\u0645\u062a\u0627\u0646\u0629 \u0648\u0639\u0645\u0631 \u0627\u0644\u062e\u062f\u0645\u0629<\/span><\/h3><p class=\"c2 wp-block-paragraph\"><span class=\"c6\">\u062a\u0645 \u062a\u0635\u0645\u064a\u0645 PPGI \u0644\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0637\u0648\u064a\u0644 \u0627\u0644\u0623\u0645\u062f. \u062a\u0648\u0641\u0631 \u0637\u0628\u0642\u0627\u062a \u0627\u0644\u0637\u0644\u0627\u0621 \u0627\u0644\u0645\u062a\u0639\u062f\u062f\u0629 \u0645\u0642\u0627\u0648\u0645\u0629 \u0642\u0648\u064a\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0648\u0627\u0644\u0623\u0634\u0639\u0629 \u0641\u0648\u0642 \u0627\u0644\u0628\u0646\u0641\u0633\u062c\u064a\u0629 \u0648\u0627\u0644\u0639\u0648\u0627\u0645\u0644 \u0627\u0644\u062c\u0648\u064a\u0629\u060c \u0645\u0645\u0627 \u064a\u0633\u0627\u0639\u062f \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0639\u0644\u0649 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u0635\u062f\u0623 \u0648\u0627\u0644\u0628\u0647\u062a\u0627\u0646 \u0628\u0645\u0631\u0648\u0631 \u0627\u0644\u0648\u0642\u062a. \u0628\u0641\u0636\u0644 \u0627\u0644\u0625\u0646\u062a\u0627\u062c \u0639\u0627\u0644\u064a \u0627\u0644\u062c\u0648\u062f\u0629\u060c \u064a\u0645\u0643\u0646 \u0644\u0640 PPGI \u0627\u0644\u062d\u0641\u0627\u0638 \u0639\u0644\u0649 \u0645\u062a\u0627\u0646\u062a\u0647 \u0648\u0645\u0638\u0647\u0631\u0647 \u0644\u0633\u0646\u0648\u0627\u062a\u060c \u0645\u0645\u0627 \u064a\u0642\u0644\u0644 \u0645\u0646 \u0627\u062d\u062a\u064a\u0627\u062c\u0627\u062a \u0627\u0644\u0635\u064a\u0627\u0646\u0629 \u0648\u064a\u0637\u064a\u0644 \u0639\u0645\u0631 \u0627\u0644\u0647\u064a\u0627\u0643\u0644.<\/span><\/p><h3 class=\"wp-block-heading c1\" id=\"h.v5zq00f0hd2p\"><span class=\"c11\">\u0627\u0644\u0645\u0631\u0648\u0646\u0629 \u0648\u0627\u0644\u0642\u062f\u0631\u0629 \u0639\u0644\u0649 \u0627\u0644\u062a\u0634\u0643\u064a\u0644<\/span><\/h3><p class=\"c2 wp-block-paragraph\"><span class=\"c6\">\u0625\u0646 \u0645\u0631\u0648\u0646\u0629 PPGI \u0648\u0642\u0627\u0628\u0644\u064a\u062a\u0647\u0627 \u0644\u0644\u062a\u0634\u0643\u064a\u0644 \u062a\u062c\u0639\u0644\u0647\u0627 \u0645\u062a\u0639\u062f\u062f\u0629 \u0627\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0627\u062a \u0628\u0634\u0643\u0644 \u0643\u0628\u064a\u0631. \u062a\u0645 \u062a\u0635\u0645\u064a\u0645 \u0637\u0628\u0642\u0629 \u0627\u0644\u0632\u0646\u0643 \u0628\u062d\u064a\u062b \u062a\u0646\u062d\u0646\u064a \u062f\u0648\u0646 \u0623\u0646 \u062a\u0641\u0642\u062f \u062e\u0635\u0627\u0626\u0635\u0647\u0627 \u0627\u0644\u0648\u0642\u0627\u0626\u064a\u0629. \u062a\u0638\u0644 \u0637\u0628\u0642\u0629 \u0627\u0644\u0637\u0644\u0627\u0621\u060c \u0627\u0644\u0645\u0635\u0645\u0645\u0629 \u0644\u0644\u0645\u0631\u0648\u0646\u0629\u060c \u0633\u0644\u064a\u0645\u0629 \u0623\u062b\u0646\u0627\u0621 \u0627\u0644\u0627\u0646\u062d\u0646\u0627\u0621\u060c \u0645\u062f\u0639\u0648\u0645\u0629 \u0628\u0637\u0628\u0642\u0629 \u0623\u0633\u0627\u0633 \u062a\u0645\u0646\u0639 \u0627\u0644\u062a\u0634\u0642\u0642 \u0623\u0648 \u0627\u0644\u062a\u0642\u0634\u064a\u0631. \u062a\u0636\u0645\u0646 \u0647\u0630\u0647 \u0627\u0644\u0628\u0646\u064a\u0629 \u0627\u0644\u0637\u0628\u0642\u064a\u0629 \u0623\u0646 \u064a\u062d\u062a\u0641\u0638 PPGI \u0628\u0627\u0644\u0645\u062a\u0627\u0646\u0629 \u0648\u0627\u0644\u0645\u0638\u0647\u0631 \u0641\u064a \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0635\u0639\u0628\u0629.<\/span><\/p><h3 class=\"wp-block-heading c1\" id=\"h.8nprd044p4qb\"><span class=\"c11\">\u0627\u0644\u062a\u0646\u0648\u0639 \u0627\u0644\u062c\u0645\u0627\u0644\u064a<\/span><\/h3><p class=\"c2 wp-block-paragraph\"><span class=\"c6\">\u062a\u0648\u0641\u0631 \u0645\u0627\u062f\u0629 PPGI \u062e\u064a\u0627\u0631\u0627\u062a \u062c\u0645\u0627\u0644\u064a\u0629 \u0645\u062a\u0639\u062f\u062f\u0629 \u0627\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0627\u062a \u0628\u0623\u0644\u0648\u0627\u0646 \u0648\u0623\u0646\u0633\u062c\u0629 \u0633\u0637\u062d\u064a\u0629 \u0648\u062a\u0634\u0637\u064a\u0628\u0627\u062a \u0645\u062e\u062a\u0644\u0641\u0629. \u064a\u0639\u0632\u0632 \u0637\u0644\u0627\u0621\u0647\u0627 \u0627\u0644\u0645\u0638\u0647\u0631 \u0648\u0627\u0644\u0645\u062a\u0627\u0646\u0629\u060c \u0645\u0639 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u0623\u0634\u0639\u0629 \u0641\u0648\u0642 \u0627\u0644\u0628\u0646\u0641\u0633\u062c\u064a\u0629 \u0627\u0644\u062a\u064a \u062a\u0636\u0645\u0646 \u0623\u0644\u0648\u0627\u0646\u064b\u0627 \u0646\u0627\u0628\u0636\u0629 \u0628\u0627\u0644\u062d\u064a\u0627\u0629 \u0648\u062f\u0627\u0626\u0645\u0629 \u0628\u0645\u0631\u0648\u0631 \u0627\u0644\u0648\u0642\u062a. \u062a\u062c\u0639\u0644 \u0647\u0630\u0647 \u0627\u0644\u0645\u0631\u0648\u0646\u0629 \u0645\u0627\u062f\u0629 PPGI \u0645\u062b\u0627\u0644\u064a\u0629 \u0644\u0644\u0645\u0634\u0627\u0631\u064a\u0639 \u0627\u0644\u062a\u064a \u062a\u062a\u0637\u0644\u0628 \u0627\u0644\u062d\u0645\u0627\u064a\u0629 \u0648\u0627\u0644\u062c\u0627\u0630\u0628\u064a\u0629 \u0627\u0644\u0628\u0635\u0631\u064a\u0629.<\/span><\/p><h3 class=\"wp-block-heading c1\" id=\"h.p0tucf1hbc5r\"><span class=\"c11\">\u064a\u0643\u0644\u0641<\/span><\/h3><p class=\"c2 wp-block-paragraph\"><span class=\"c6\">\u062a\u0648\u0627\u0632\u0646 \u062a\u0643\u0644\u0641\u0629 PPGI \u0628\u064a\u0646 \u0645\u062a\u0627\u0646\u062a\u0647\u0627 \u0648\u0642\u064a\u0645\u062a\u0647\u0627 \u0627\u0644\u062c\u0645\u0627\u0644\u064a\u0629 \u0648\u062d\u0645\u0627\u064a\u062a\u0647\u0627. \u0648\u0631\u063a\u0645 \u0623\u0646 \u062a\u0643\u0644\u0641\u062a\u0647\u0627 \u0641\u064a \u0627\u0644\u0628\u062f\u0627\u064a\u0629 \u0623\u0639\u0644\u0649 \u0645\u0646 \u062a\u0643\u0644\u0641\u0629 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u063a\u064a\u0631 \u0627\u0644\u0645\u0637\u0644\u064a\u060c \u0641\u0625\u0646 \u0637\u0648\u0644 \u0639\u0645\u0631\u0647\u0627 \u0648\u0627\u0646\u062e\u0641\u0627\u0636 \u062a\u0643\u0627\u0644\u064a\u0641 \u0635\u064a\u0627\u0646\u062a\u0647\u0627 \u064a\u0642\u0644\u0644\u0627\u0646 \u0645\u0646 \u0627\u0644\u0646\u0641\u0642\u0627\u062a \u0627\u0644\u0625\u062c\u0645\u0627\u0644\u064a\u0629. \u0643\u0645\u0627 \u062a\u0639\u0645\u0644 \u0645\u0642\u0627\u0648\u0645\u062a\u0647\u0627 \u0644\u0644\u062a\u0622\u0643\u0644 \u0639\u0644\u0649 \u062e\u0641\u0636 \u062a\u0643\u0627\u0644\u064a\u0641 \u0627\u0644\u0627\u0633\u062a\u0628\u062f\u0627\u0644\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647\u0627 \u0641\u0639\u0627\u0644\u0629 \u0645\u0646 \u062d\u064a\u062b \u0627\u0644\u062a\u0643\u0644\u0641\u0629 \u0644\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u0635\u0639\u0628\u0629.<\/span><\/p><h2 class=\"wp-block-heading c1\" id=\"h.wh4ijvcvfcqi\"><span class=\"c12\">\u062a\u0637\u0628\u064a\u0642\u0627\u062a PPGI<\/span><\/h2><p class=\"c2 wp-block-paragraph\"><span class=\"c4\">\u0628\u0646\u0627\u0621<\/span><span class=\"c6\">:\u064a\u062a\u0645 \u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0647 \u0639\u0644\u0649 \u0646\u0637\u0627\u0642 \u0648\u0627\u0633\u0639 \u0641\u064a \u0627\u0644\u0623\u0633\u0642\u0641 \u0648\u062a\u063a\u0644\u064a\u0641 \u0627\u0644\u062c\u062f\u0631\u0627\u0646 \u0648\u0627\u0644\u0648\u0627\u062c\u0647\u0627\u062a\u060c \u062d\u064a\u062b \u064a\u0648\u0641\u0631 \u0627\u0644\u0645\u062a\u0627\u0646\u0629 \u0648\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u0637\u0642\u0633 \u0645\u0639 \u062a\u0639\u0632\u064a\u0632 \u062c\u0645\u0627\u0644\u064a\u0627\u062a \u0627\u0644\u0628\u0646\u0627\u0621.<\/span><\/p><p class=\"c2 wp-block-paragraph\"><span class=\"c4\">\u0627\u0644\u0623\u062c\u0647\u0632\u0629 \u0627\u0644\u0645\u0646\u0632\u0644\u064a\u0629<\/span><span class=\"c6\">:\u0645\u062b\u0627\u0644\u064a \u0644\u0644\u0645\u0646\u062a\u062c\u0627\u062a \u0645\u062b\u0644 \u0627\u0644\u062b\u0644\u0627\u062c\u0627\u062a \u0648\u0627\u0644\u063a\u0633\u0627\u0644\u0627\u062a \u0648\u0645\u0643\u064a\u0641\u0627\u062a \u0627\u0644\u0647\u0648\u0627\u0621 \u0628\u0633\u0628\u0628 \u0645\u0644\u0645\u0633\u0647 \u0627\u0644\u0646\u0627\u0639\u0645 \u0648\u0645\u0642\u0627\u0648\u0645\u062a\u0647 \u0644\u0644\u0635\u062f\u0623.<\/span><\/p><p class=\"c2 wp-block-paragraph\"><span class=\"c4\">\u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a<\/span><span class=\"c6\">:\u064a\u062a\u0645 \u062a\u0637\u0628\u064a\u0642\u0647 \u0639\u0644\u0649 \u0623\u062c\u0632\u0627\u0621 \u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a \u0627\u0644\u0645\u0639\u0631\u0636\u0629 \u0644\u0644\u0631\u0637\u0648\u0628\u0629 \u0648\u0627\u0644\u0645\u0648\u0627\u062f \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629\u060c \u0645\u0645\u0627 \u064a\u0648\u0641\u0631 \u062d\u0645\u0627\u064a\u0629 \u0623\u0633\u0627\u0633\u064a\u0629 \u0645\u0646 \u0627\u0644\u062a\u0622\u0643\u0644.<\/span><\/p><p class=\"c2 wp-block-paragraph\"><span class=\"c4\">\u0623\u062b\u0627\u062b<\/span><span class=\"c6\">:\u0634\u0627\u0626\u0639 \u0641\u064a \u0627\u0644\u062e\u0632\u0627\u0626\u0646 \u0648\u0648\u062d\u062f\u0627\u062a \u0627\u0644\u062a\u062e\u0632\u064a\u0646 \u0648\u063a\u064a\u0631\u0647\u0627 \u0645\u0646 \u0627\u0644\u0623\u062b\u0627\u062b \u0627\u0644\u0645\u0639\u062f\u0646\u064a \u062d\u064a\u062b \u062a\u0643\u0648\u0646 \u0647\u0646\u0627\u0643 \u062d\u0627\u062c\u0629 \u0625\u0644\u0649 \u0627\u0644\u0645\u062a\u0627\u0646\u0629 \u0648\u0627\u0644\u0644\u0645\u0633\u0629 \u0627\u0644\u0646\u0647\u0627\u0626\u064a\u0629 \u0627\u0644\u062c\u0630\u0627\u0628\u0629.<\/span><\/p><p class=\"c2 wp-block-paragraph\"><span class=\"c4\">\u0627\u0644\u0644\u0627\u0641\u062a\u0627\u062a \u0648\u0627\u0644\u0644\u0648\u062d\u0627\u062a \u0627\u0644\u0625\u0639\u0644\u0627\u0646\u064a\u0629<\/span><span class=\"c6\">:\u0645\u0645\u062a\u0627\u0632 \u0644\u0644\u0639\u0644\u0627\u0645\u0627\u062a \u0627\u0644\u062e\u0627\u0631\u062c\u064a\u0629 \u0628\u0633\u0628\u0628 \u062b\u0628\u0627\u062a \u0627\u0644\u0644\u0648\u0646 \u0648\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u0637\u0642\u0633\u060c \u0648\u0627\u0644\u062d\u0641\u0627\u0638 \u0639\u0644\u0649 \u0627\u0644\u0645\u0638\u0647\u0631 \u0628\u0645\u0631\u0648\u0631 \u0627\u0644\u0648\u0642\u062a.<\/span><\/p><h2 class=\"wp-block-heading c1\" id=\"h.oixma3qkvzic\"><span class=\"c12\">\u0644\u0641\u0627\u0626\u0641 \u0648\u0635\u0641\u0627\u0626\u062d PPGI<\/span><\/h2><h3 class=\"wp-block-heading c1\" id=\"h.v2a7a0yd7ed2\"><span class=\"c11\">\u0645\u0627 \u0647\u064a \u0645\u0644\u0641\u0627\u062a PPGI\u061f<\/span><\/h3><p class=\"c2 wp-block-paragraph\"><span class=\"c4\">\u0645\u0644\u0641\u0627\u062a PPGI<\/span><span class=\"c6\">&nbsp;\u0647\u064a \u0639\u0628\u0627\u0631\u0629 \u0639\u0646 \u0644\u0641\u0627\u062a \u0645\u062a\u0648\u0627\u0635\u0644\u0629 \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u062c\u0644\u0641\u0646 \u0627\u0644\u0645\u0637\u0644\u064a \u0645\u0633\u0628\u0642\u064b\u0627\u060c \u062a\u064f\u0633\u062a\u062e\u062f\u0645 \u0639\u0627\u062f\u0629\u064b \u0644\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0648\u0627\u0633\u0639\u0629 \u0627\u0644\u0646\u0637\u0627\u0642. \u064a\u0633\u0645\u062d \u0634\u0643\u0644 \u0627\u0644\u0644\u0641\u0629 \u0628\u0627\u0644\u0646\u0642\u0644 \u0627\u0644\u0633\u0647\u0644 \u0648\u0627\u0644\u062a\u062e\u0632\u064a\u0646 \u0627\u0644\u0641\u0639\u0651\u0627\u0644. \u062a\u0648\u0641\u0631 \u0627\u0644\u0644\u0641\u0627\u062a \u062a\u0646\u0648\u0639\u064b\u0627 \u0641\u064a \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629\u060c \u062d\u064a\u062b \u064a\u0645\u0643\u0646 \u0642\u0637\u0639\u0647\u0627 \u0623\u0648 \u062a\u0634\u0643\u064a\u0644\u0647\u0627 \u0623\u0648 \u062a\u0634\u0643\u064a\u0644\u0647\u0627 \u0641\u064a \u0645\u0646\u062a\u062c\u0627\u062a \u0645\u062e\u062a\u0644\u0641\u0629 \u0645\u062b\u0644 \u0627\u0644\u0623\u0633\u0642\u0641 \u0648\u0623\u0644\u0648\u0627\u062d \u0627\u0644\u062c\u062f\u0631\u0627\u0646 \u0648\u0627\u0644\u0623\u062c\u0647\u0632\u0629. \u0648\u0647\u064a \u0645\u062b\u0627\u0644\u064a\u0629 \u0644\u0644\u0645\u0634\u0627\u0631\u064a\u0639 \u0627\u0644\u062a\u064a \u062a\u062d\u062a\u0627\u062c \u0625\u0644\u0649 \u0643\u0645\u064a\u0627\u062a \u0643\u0628\u064a\u0631\u0629 \u0645\u0646 \u0627\u0644\u0645\u0648\u0627\u062f \u0628\u062c\u0648\u062f\u0629 \u0648\u0644\u0648\u0646 \u062b\u0627\u0628\u062a\u064a\u0646.<\/span><\/p><h3 class=\"wp-block-heading c1\" id=\"h.im7b4i5vjhod\"><span class=\"c11\">\u0645\u0627 \u0647\u064a \u0623\u0648\u0631\u0627\u0642 PPGI\u061f<\/span><\/h3><p class=\"c2 wp-block-paragraph\"><span class=\"c4\">\u0623\u0648\u0631\u0627\u0642 PPGI<\/span><span class=\"c6\">&nbsp;\u062a\u064f\u0639\u064e\u062f \u0627\u0644\u0623\u0644\u0648\u0627\u062d \u0627\u0644\u0645\u0639\u062f\u0646\u064a\u0629 \u0639\u0628\u0627\u0631\u0629 \u0639\u0646 \u0642\u0637\u0639 \u0645\u0633\u0637\u062d\u0629 \u0645\u0642\u0637\u0648\u0639\u0629 \u0645\u0646 \u0644\u0641\u0627\u0626\u0641\u060c \u0648\u063a\u0627\u0644\u0628\u064b\u0627 \u0645\u0627 \u064a\u062a\u0645 \u062a\u062d\u062f\u064a\u062f \u062d\u062c\u0645\u0647\u0627 \u0645\u0633\u0628\u0642\u064b\u0627 \u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0645\u062d\u062f\u062f\u0629. \u0648\u0647\u064a \u0623\u0643\u062b\u0631 \u0645\u0644\u0627\u0621\u0645\u0629 \u0644\u0644\u0625\u062f\u0627\u0631\u0629 \u0648\u0627\u0644\u062a\u0631\u0643\u064a\u0628\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647\u0627 \u0645\u062b\u0627\u0644\u064a\u0629 \u0644\u0644\u0645\u0634\u0627\u0631\u064a\u0639 \u0627\u0644\u0635\u063a\u064a\u0631\u0629 \u0623\u0648 \u0627\u0644\u0645\u0647\u0627\u0645 \u0627\u0644\u0645\u0639\u0642\u062f\u0629. \u062a\u064f\u0633\u062a\u062e\u062f\u0645 \u0639\u0627\u062f\u0629\u064b \u0641\u064a \u062a\u0634\u064a\u064a\u062f \u0627\u0644\u0645\u0628\u0627\u0646\u064a \u0644\u0644\u0643\u0633\u0648\u0629 \u0627\u0644\u062e\u0627\u0631\u062c\u064a\u0629 \u0648\u0623\u063a\u0637\u064a\u0629 \u0627\u0644\u062c\u062f\u0631\u0627\u0646 \u0627\u0644\u062f\u0627\u062e\u0644\u064a\u0629 \u0648\u0627\u0644\u0645\u064a\u0632\u0627\u062a \u0627\u0644\u0632\u062e\u0631\u0641\u064a\u0629. \u062a\u0648\u0641\u0631 \u0627\u0644\u0623\u0644\u0648\u0627\u062d \u0646\u0641\u0633 \u0627\u0644\u0645\u062a\u0627\u0646\u0629 \u0648\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644 \u0645\u062b\u0644 \u0627\u0644\u0644\u0641\u0627\u0626\u0641 \u0648\u0644\u0643\u0646\u0647\u0627 \u062a\u0648\u0641\u0631 \u0631\u0627\u062d\u0629 \u0625\u0636\u0627\u0641\u064a\u0629 \u0644\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0623\u0635\u063a\u0631 \u062d\u062c\u0645\u064b\u0627 \u0648\u0627\u0644\u062c\u0627\u0647\u0632\u0629 \u0644\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645.<\/span><\/p><h2 class=\"wp-block-heading c1\" id=\"h.ziffwbx0pc12\"><span class=\"c12\">\u0645\u0644\u062e\u0635 \u0628\u064a\u0627\u0646\u0627\u062a \u0627\u0644\u0645\u0631\u062c\u0639 \u0627\u0644\u0642\u064a\u0627\u0633\u064a \u0644\u0640 PPGI<\/span><\/h2><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u0645\u0644\u0643\u064a\u0629<\/strong><\/td><td><strong>\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u062c\u0644\u0641\u0646<\/strong><\/td><td><strong>\u0627\u0644\u0623\u0644\u0648\u0645\u0646\u064a\u0648\u0645<\/strong><\/td><\/tr><tr><td>\u0646\u0642\u0637\u0629 \u0627\u0644\u0627\u0646\u0635\u0647\u0627\u0631<\/td><td>~1370 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629 \u2013 1510 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629<\/td><td>~660 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629<\/td><\/tr><tr><td>\u0627\u0644\u0645\u0648\u0635\u0644\u064a\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629<\/td><td>~50 \u0648\u0627\u0637\/\u0645\u00b7\u0643<\/td><td>~235 \u0648\u0627\u0637\/\u0645\u062a\u0631\u00b7\u0643<\/td><\/tr><tr><td>\u0627\u0644\u0645\u0648\u0635\u0644\u064a\u0629 \u0627\u0644\u0643\u0647\u0631\u0628\u0627\u0626\u064a\u0629<\/td><td>~6-7 \u0645\u0644\u0644\u064a \u062b\u0627\u0646\u064a\u0629\/\u0645<\/td><td>~36 \u0645\u064a\u062c\u0627 \u0645\u064a\u0643\u0631\u0648\u062b\u0627\u0646\u064a\u0629\/\u0645<\/td><\/tr><tr><td>\u0642\u0648\u0629 \u0627\u0644\u0634\u062f<\/td><td>370 \u2013 600 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644 (\u064a\u062e\u062a\u0644\u0641 \u062d\u0633\u0628 \u0627\u0644\u062f\u0631\u062c\u0629)<\/td><td>70 \u2013 700 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644 (\u064a\u062e\u062a\u0644\u0641 \u062d\u0633\u0628 \u0627\u0644\u0633\u0628\u0627\u0626\u0643)<\/td><\/tr><tr><td>\u0642\u0648\u0629 \u0627\u0644\u062e\u0636\u0648\u0639<\/td><td>205 \u2013 345 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644 (\u064a\u062e\u062a\u0644\u0641 \u062d\u0633\u0628 \u0627\u0644\u062f\u0631\u062c\u0629)<\/td><td>30 \u2013 400 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644 (\u064a\u062e\u062a\u0644\u0641 \u062d\u0633\u0628 \u0627\u0644\u0633\u0628\u0627\u0626\u0643)<\/td><\/tr><tr><td>\u0645\u0639\u0627\u0645\u0644 \u0627\u0644\u0645\u0631\u0648\u0646\u0629<\/td><td>~200 \u062c\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644<\/td><td>~69 \u062c\u064a\u062c\u0627\u0628\u0627\u0633\u0643\u0627\u0644<\/td><\/tr><tr><td>\u0645\u0639\u0627\u0645\u0644 \u0627\u0644\u062a\u0645\u062f\u062f \u0627\u0644\u062d\u0631\u0627\u0631\u064a<\/td><td>~11-12 \u0645\u064a\u0643\u0631\u0648\u0645\u062a\u0631\/\u0645\u062a\u0631\u00b7\u0643<\/td><td>~23 \u0645\u064a\u0643\u0631\u0648\u0645\u062a\u0631\/\u0645\u062a\u0631\u00b7\u0643<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading c1\" id=\"h.pbe5uuwo8sm8\"><span class=\"c12\">PPGI \u0645\u0642\u0627\u0628\u0644 PPGL Steel<\/span><\/h2><p class=\"c2 wp-block-paragraph\"><span class=\"c6\">\u0627\u0644\u0641\u0631\u0642 \u0627\u0644\u0631\u0626\u064a\u0633\u064a \u0628\u064a\u0646 PPGI \u0648PPGL \u0647\u0648 \u0631\u0643\u0627\u0626\u0632\u0647\u0645\u0627. \u064a\u0633\u062a\u062e\u062f\u0645 PPGI \u0642\u0627\u0639\u062f\u0629 \u0645\u0646 \u0627\u0644\u062d\u062f\u064a\u062f \u0627\u0644\u0645\u062c\u0644\u0641\u0646 \u0627\u0644\u0645\u0637\u0644\u064a \u0628\u0627\u0644\u0632\u0646\u0643\u060c \u0648\u0647\u0648 \u0645\u0646\u0627\u0633\u0628 \u0644\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0639\u0627\u0645\u0629. \u064a\u0633\u062a\u062e\u062f\u0645 PPGL \u0642\u0627\u0639\u062f\u0629 \u0645\u0646 \u0633\u0628\u0627\u0626\u0643 \u0627\u0644\u0623\u0644\u0648\u0645\u0646\u064a\u0648\u0645 \u0648\u0627\u0644\u0632\u0646\u0643 (\u062d\u0648\u0627\u0644\u064a 55% \u0645\u0646 \u0627\u0644\u0623\u0644\u0648\u0645\u0646\u064a\u0648\u0645 \u064843.4% \u0645\u0646 \u0627\u0644\u0632\u0646\u0643)\u060c \u0645\u0645\u0627 \u064a\u0648\u0641\u0631 \u0645\u062a\u0627\u0646\u0629 \u0641\u0627\u0626\u0642\u0629 \u0641\u064a \u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u0645\u0633\u0628\u0628\u0629 \u0644\u0644\u062a\u0622\u0643\u0644. \u0648\u0628\u0627\u0644\u062a\u0627\u0644\u064a\u060c \u064a\u0639\u062f PPGI \u0645\u062b\u0627\u0644\u064a\u064b\u0627 \u0644\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0627\u062a \u0627\u0644\u0642\u064a\u0627\u0633\u064a\u0629\u060c \u0628\u064a\u0646\u0645\u0627 \u064a\u0641\u0636\u0644 PPGL \u0627\u0644\u0638\u0631\u0648\u0641 \u0627\u0644\u0635\u0639\u0628\u0629 \u0627\u0644\u062a\u064a \u062a\u062a\u0637\u0644\u0628 \u0639\u0645\u0631\u064b\u0627 \u0627\u0641\u062a\u0631\u0627\u0636\u064a\u064b\u0627 \u0645\u0645\u062a\u062f\u064b\u0627.<\/span><\/p><h3 class=\"wp-block-heading c1\" id=\"h.e2yrwkojswts\"><span class=\"c11\">\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644<\/span><\/h3><p class=\"c2 wp-block-paragraph\"><span class=\"c6\">\u064a\u062a\u0641\u0648\u0642 PPGL \u0639\u0644\u0649 PPGI \u0641\u064a \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644.<\/span><\/p><p class=\"c2 wp-block-paragraph\">\u0633\u0628\u064a\u0643\u0629 \u0627\u0644\u0623\u0644\u0648\u0645\u0646\u064a\u0648\u0645 \u0648\u0627\u0644\u0632\u0646\u0643 \u0641\u064a <span class=\"c4\">\u0628\u064a \u0628\u064a \u062c\u064a \u0625\u0644 <\/span><span class=\"c6\">\u064a\u0634\u0643\u0644 \u0637\u0628\u0642\u0629 \u0648\u0627\u0642\u064a\u0629 \u0645\u062a\u064a\u0646\u0629 \u062a\u062d\u0645\u064a \u0627\u0644\u0631\u0643\u064a\u0632\u0629 \u0627\u0644\u0641\u0648\u0644\u0627\u0630\u064a\u0629 \u0628\u0634\u0643\u0644 \u0623\u0643\u062b\u0631 \u0641\u0639\u0627\u0644\u064a\u0629 \u0645\u0646 \u062e\u0644\u0627\u0644 \u0639\u0643\u0633 \u0639\u0648\u0627\u0645\u0644 \u0627\u0644\u062a\u0622\u0643\u0644 \u0648\u0625\u0628\u0637\u0627\u0626\u0647\u0627. \u064a\u0639\u0645\u0644 \u0627\u0644\u0623\u0644\u0648\u0645\u0646\u064a\u0648\u0645 \u0627\u0644\u0645\u0648\u062c\u0648\u062f \u0641\u064a \u0627\u0644\u0633\u0628\u0627\u0626\u0643 \u0643\u062d\u0627\u062c\u0632\u060c \u0645\u0645\u0627 \u064a\u0645\u0646\u0639 \u062a\u0643\u0648\u064a\u0646 \u0627\u0644\u0635\u062f\u0623 \u0627\u0644\u0633\u0631\u064a\u0639 \u0648\u064a\u0648\u0641\u0631 \u062d\u0645\u0627\u064a\u0629 \u062a\u062f\u0648\u0645 \u0644\u0641\u062a\u0631\u0629 \u0623\u0637\u0648\u0644.<\/span><\/p><p class=\"c2 wp-block-paragraph\"><span class=\"c4\">\u0628 \u0628 \u062c\u0649 \u0627\u0649<\/span><span class=\"c6\">\u064a\u0648\u0641\u0631 \u0637\u0644\u0627\u0621 \u0627\u0644\u0632\u0646\u0643 \u0627\u0644\u0646\u0642\u064a \u0645\u0642\u0627\u0648\u0645\u0629 \u0642\u0648\u064a\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0648\u0644\u0643\u0646\u0647 \u0623\u0642\u0644 \u0645\u062a\u0627\u0646\u0629 \u0641\u064a \u0627\u0644\u0638\u0631\u0648\u0641 \u0627\u0644\u0642\u0627\u0633\u064a\u0629\u060c \u062d\u064a\u062b \u0644\u0627 \u064a\u0634\u0643\u0644 \u0627\u0644\u0632\u0646\u0643 \u0648\u062d\u062f\u0647 \u062d\u0627\u062c\u0632\u064b\u0627 \u0642\u0648\u064a\u064b\u0627 \u0636\u062f \u0627\u0644\u0639\u0646\u0627\u0635\u0631 \u0627\u0644\u0645\u0633\u0628\u0628\u0629 \u0644\u0644\u062a\u0622\u0643\u0644.<\/span><\/p><h3 class=\"wp-block-heading c1\" id=\"h.fm6wbytvv5q8\"><span class=\"c11\">\u0642\u0648\u0629<\/span><\/h3><p class=\"c2 wp-block-paragraph\"><span class=\"c6\">\u0628\u0627\u0644\u0646\u0633\u0628\u0629 \u0644\u0646\u0641\u0633 \u0627\u0644\u0633\u0645\u0643\u060c \u0641\u0625\u0646 PPGL \u0623\u0642\u0648\u0649 \u0628\u0637\u0628\u064a\u0639\u062a\u0647 \u0645\u0646 PPGI.<\/span><\/p><p class=\"c2 wp-block-paragraph\">\u0637\u0628\u0642\u0629 \u0633\u0628\u0627\u0626\u0643 \u0627\u0644\u0623\u0644\u0648\u0645\u0646\u064a\u0648\u0645 \u0648\u0627\u0644\u0632\u0646\u0643 \u0641\u064a <span class=\"c4\">\u0628\u064a \u0628\u064a \u062c\u064a \u0625\u0644<\/span><span class=\"c6\">&nbsp;\u064a\u0648\u0641\u0631 \u0635\u0644\u0627\u0628\u0629 \u0625\u0636\u0627\u0641\u064a\u0629\u060c \u062d\u064a\u062b \u0623\u0646 \u0643\u062b\u0627\u0641\u0629 \u0627\u0644\u0623\u0644\u0648\u0645\u0646\u064a\u0648\u0645 \u0623\u0642\u0644 \u0645\u0646 \u0643\u062b\u0627\u0641\u0629 \u0627\u0644\u0632\u0646\u0643\u060c \u0645\u0645\u0627 \u064a\u0646\u062a\u062c \u0639\u0646\u0647 \u0637\u0644\u0627\u0621 \u0623\u0643\u062b\u0631 \u0643\u062b\u0627\u0641\u0629 \u0648\u0645\u0631\u0648\u0646\u0629. \u0648\u0647\u0630\u0627 \u064a\u062c\u0639\u0644 PPGL \u0645\u0646\u0627\u0633\u0628\u064b\u0627 \u0628\u0634\u0643\u0644 \u062e\u0627\u0635 \u0644\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u062d\u064a\u062b \u062a\u0643\u0648\u0646 \u0633\u0644\u0627\u0645\u0629 \u0627\u0644\u0628\u0646\u064a\u0629 \u0636\u0631\u0648\u0631\u064a\u0629.<\/span><\/p><p class=\"c2 wp-block-paragraph\"><span class=\"c6\">\u0639\u0644\u0649 \u0627\u0644\u0646\u0642\u064a\u0636 \u0645\u0646 \u0630\u0644\u0643\u060c \u064a\u062a\u0645\u062a\u0639 PPGI\u060c \u0628\u0637\u0644\u0627\u0626\u0647 \u0627\u0644\u0632\u0646\u0643\u064a \u0627\u0644\u0646\u0642\u064a\u060c \u0628\u0642\u0648\u0629 \u0645\u0639\u062a\u062f\u0644\u0629 \u0643\u0627\u0641\u064a\u0629 \u0644\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0627\u062a \u0627\u0644\u0642\u064a\u0627\u0633\u064a\u0629 \u0648\u0644\u0643\u0646\u0647 \u064a\u0641\u062a\u0642\u0631 \u0625\u0644\u0649 \u0627\u0644\u0635\u0644\u0627\u0628\u0629 \u0627\u0644\u0645\u0639\u0632\u0632\u0629 \u0644\u0640 PPGL.<\/span><\/p><h3 class=\"wp-block-heading c1\" id=\"h.lsagvzrbhln6\"><span class=\"c11\">\u0642\u0627\u0628\u0644\u064a\u0629 \u0627\u0644\u062a\u0634\u0643\u064a\u0644<\/span><\/h3><p class=\"c2 wp-block-paragraph\"><span class=\"c6\">\u064a\u0648\u0641\u0631 \u0643\u0644 \u0645\u0646 PPGI \u0648 PPGL \u0642\u0627\u0628\u0644\u064a\u0629 \u062a\u0634\u0643\u064a\u0644 \u062c\u064a\u062f\u0629\u060c \u0648\u0644\u0643\u0646 PPGI \u064a\u0645\u064a\u0644 \u0625\u0644\u0649 \u0623\u0646 \u064a\u0643\u0648\u0646 \u0623\u0633\u0647\u0644 \u0642\u0644\u064a\u0644\u0627\u064b \u0641\u064a \u0627\u0644\u062a\u0639\u0627\u0645\u0644 \u0645\u0639\u0647.<\/span><\/p><p class=\"c2 wp-block-paragraph\"><span class=\"c6\">\u062a\u0648\u0641\u0631 \u0637\u0628\u0642\u0629 \u0627\u0644\u0632\u0646\u0643 \u0627\u0644\u0646\u0642\u064a\u0629 \u0639\u0644\u0649 PPGI \u0645\u0631\u0648\u0646\u0629 \u0623\u0641\u0636\u0644 \u0623\u062b\u0646\u0627\u0621 \u0627\u0644\u0627\u0646\u062d\u0646\u0627\u0621 \u0648\u0627\u0644\u062a\u0634\u0643\u064a\u0644\u060c \u0645\u0645\u0627 \u0642\u062f \u064a\u0643\u0648\u0646 \u0645\u0641\u064a\u062f\u064b\u0627 \u0641\u064a \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u062a\u064a \u062a\u062a\u0637\u0644\u0628 \u0623\u0634\u0643\u0627\u0644\u064b\u0627 \u0645\u0639\u0642\u062f\u0629.<\/span><\/p><p class=\"c2 wp-block-paragraph\"><span class=\"c6\">\u0639\u0644\u0649 \u0627\u0644\u0631\u063a\u0645 \u0645\u0646 \u0623\u0646 PPGL \u0644\u0627 \u064a\u0632\u0627\u0644 \u0642\u0627\u0628\u0644\u0627\u064b \u0644\u0644\u062a\u0634\u0643\u064a\u0644\u060c \u0625\u0644\u0627 \u0623\u0646\u0647 \u064a\u062d\u062a\u0648\u064a \u0639\u0644\u0649 \u0637\u0628\u0642\u0629 \u0623\u0643\u062b\u0631 \u0635\u0644\u0627\u0628\u0629 \u0645\u0646 \u0627\u0644\u0623\u0644\u0648\u0645\u0646\u064a\u0648\u0645 \u0648\u0627\u0644\u0632\u0646\u0643\u060c \u0645\u0645\u0627 \u0642\u062f \u064a\u062d\u062f \u0645\u0646 \u0642\u062f\u0631\u062a\u0647 \u0639\u0644\u0649 \u0627\u0644\u062a\u0643\u064a\u0641 \u0641\u064a \u0627\u0644\u0623\u0634\u0643\u0627\u0644 \u0627\u0644\u0645\u0639\u0642\u062f\u0629.<\/span><\/p><h3 class=\"wp-block-heading c1\" id=\"h.jzu2wgvmylny\"><span class=\"c11\">\u064a\u0643\u0644\u0641<\/span><\/h3><p class=\"c2 wp-block-paragraph\"><span class=\"c6\">\u0625\u0646 \u0637\u0644\u0627\u0621 PPGI \u0623\u0631\u062e\u0635 \u0639\u0645\u0648\u0645\u064b\u0627 \u0645\u0646 \u0637\u0644\u0627\u0621 PPGL\u060c \u062d\u064a\u062b \u0625\u0646 \u062a\u0643\u0644\u0641\u0629 \u0625\u0646\u062a\u0627\u062c \u0627\u0644\u0637\u0644\u0627\u0621 \u0627\u0644\u0630\u064a \u064a\u062d\u062a\u0648\u064a \u0639\u0644\u0649 \u0627\u0644\u0632\u0646\u0643 \u0641\u0642\u0637 \u0623\u0642\u0644 \u0645\u0646 \u062a\u0643\u0644\u0641\u0629 \u0625\u0646\u062a\u0627\u062c \u0637\u0644\u0627\u0621 \u0633\u0628\u0627\u0626\u0643 \u0627\u0644\u0623\u0644\u0648\u0645\u0646\u064a\u0648\u0645 \u0648\u0627\u0644\u0632\u0646\u0643 \u0627\u0644\u0645\u0633\u062a\u062e\u062f\u0645 \u0641\u064a \u0637\u0644\u0627\u0621 PPGL. \u0648\u0647\u0630\u0627 \u064a\u062c\u0639\u0644 \u0637\u0644\u0627\u0621 PPGI \u062e\u064a\u0627\u0631\u064b\u0627 \u0623\u0643\u062b\u0631 \u0645\u0644\u0627\u0621\u0645\u0629 \u0644\u0644\u0645\u064a\u0632\u0627\u0646\u064a\u0629 \u0644\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0642\u064a\u0627\u0633\u064a\u0629\u060c \u0641\u064a \u062d\u064a\u0646 \u0623\u0646 \u062a\u0643\u0644\u0641\u0629 \u0637\u0644\u0627\u0621 PPGL \u0627\u0644\u0623\u0639\u0644\u0649 \u063a\u0627\u0644\u0628\u064b\u0627 \u0645\u0627 \u062a\u0643\u0648\u0646 \u0645\u0628\u0631\u0631\u0629 \u0628\u0623\u062f\u0627\u0626\u0647 \u0641\u064a \u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u0623\u0643\u062b\u0631 \u0642\u0633\u0648\u0629.<\/span><\/p><h3 class=\"wp-block-heading c1\" id=\"h.omguqlc8c0h6\"><span class=\"c11\">\u062e\u0627\u062a\u0645\u0629<\/span><\/h3><p class=\"c2 wp-block-paragraph\"><span class=\"c6\">\u062a\u062a\u0645\u064a\u0632 \u0645\u0627\u062f\u0629 PPGI \u0628\u0623\u0646\u0647\u0627 \u0641\u0639\u0627\u0644\u0629 \u0645\u0646 \u062d\u064a\u062b \u0627\u0644\u062a\u0643\u0644\u0641\u0629 \u0648\u0645\u0631\u0646\u0629\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647\u0627 \u0645\u0646\u0627\u0633\u0628\u0629 \u0644\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0642\u064a\u0627\u0633\u064a\u0629. \u0643\u0645\u0627 \u0623\u0646 \u0645\u0627\u062f\u0629 PPGL\u060c \u0627\u0644\u062a\u064a \u062a\u062a\u0645\u064a\u0632 \u0628\u0645\u0642\u0627\u0648\u0645\u062a\u0647\u0627 \u0627\u0644\u0639\u0627\u0644\u064a\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0648\u0642\u0648\u062a\u0647\u0627\u060c \u0645\u0641\u0636\u0644\u0629 \u0644\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u0635\u0639\u0628\u0629 \u0627\u0644\u062a\u064a \u062a\u062a\u0637\u0644\u0628 \u0645\u062a\u0627\u0646\u0629 \u0637\u0648\u064a\u0644\u0629 \u0627\u0644\u0623\u0645\u062f.<\/span><\/p><h2 class=\"wp-block-heading c1\" id=\"h.pk9loqqeirp5\"><span class=\"c12\">\u062d\u0644\u0648\u0644 PPGI \u0648 PPGL \u0627\u0644\u0645\u062a\u0645\u064a\u0632\u0629<\/span><\/h2><p class=\"c2 wp-block-paragraph\">\u064a\u062e\u062a\u0627\u0631<a class=\"c16\" href=\"https:\/\/www.google.com\/url?q=https:\/\/steelprogroup.com\/&amp;sa=D&amp;source=editors&amp;ust=1740727946852452&amp;usg=AOvVaw018hI79bQoARyty-0SNVA9\">&nbsp;<\/a><span class=\"c10\"><a class=\"c16\" href=\"https:\/\/www.google.com\/url?q=https:\/\/steelprogroup.com\/&amp;sa=D&amp;source=editors&amp;ust=1740727946852552&amp;usg=AOvVaw1dY1eZprOkok_Yj9ijjFjq\">\u0645\u062c\u0645\u0648\u0639\u0629 \u0633\u062a\u064a\u0644 \u0628\u0631\u0648<\/a><\/span><span class=\"c6\">&nbsp;\u0644\u0644\u062d\u0635\u0648\u0644 \u0639\u0644\u0649 \u0645\u0646\u062a\u062c\u0627\u062a PPGI \u0648 PPGL \u0639\u0627\u0644\u064a\u0629 \u0627\u0644\u062c\u0648\u062f\u0629\u060c \u062d\u064a\u062b \u064a\u062a\u0645 \u0636\u0645\u0627\u0646 \u0633\u0645\u0643 \u0627\u0644\u0637\u0644\u0627\u0621 \u0627\u0644\u0645\u0648\u062d\u062f \u0648\u0627\u0644\u0627\u0645\u062a\u062b\u0627\u0644 \u0627\u0644\u0635\u0627\u0631\u0645 \u0644\u0644\u0645\u0639\u0627\u064a\u064a\u0631. <\/span><\/p><p class=\"wp-block-paragraph\">&nbsp;<\/p><p class=\"wp-block-paragraph\"><\/p>","protected":false},"excerpt":{"rendered":"<p>\u062a\u0639\u0631\u0641 \u0639\u0644\u0649 PPGI \u0648\u062e\u0635\u0627\u0626\u0635\u0647 \u0648\u0641\u0648\u0627\u0626\u062f\u0647 \u0648\u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0627\u062a\u0647 \u0627\u0644\u0634\u0627\u0626\u0639\u0629 \u0641\u064a \u0627\u0644\u0628\u0646\u0627\u0621 \u0648\u0627\u0644\u0623\u062c\u0647\u0632\u0629 \u0648\u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a \u0648\u0627\u0644\u0645\u0632\u064a\u062f. \u062a\u0639\u0631\u0641 \u0639\u0644\u0649 \u0627\u0644\u0627\u062e\u062a\u0644\u0627\u0641\u0627\u062a \u0627\u0644\u0631\u0626\u064a\u0633\u064a\u0629 \u0645\u0639 PPGL.<\/p>","protected":false},"author":1,"featured_media":21045,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"_eb_attr":"","rank_math_lock_modified_date":false,"site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"categories":[4274,4273],"tags":[],"class_list":["post-21044","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-knowledge-galvanized-steel","category-galvanized-steel"],"acf":[],"_links":{"self":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts\/21044","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/comments?post=21044"}],"version-history":[{"count":0,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts\/21044\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/media\/21045"}],"wp:attachment":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/media?parent=21044"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/categories?post=21044"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/tags?post=21044"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}