{"id":21370,"date":"2025-03-05T16:46:05","date_gmt":"2025-03-05T08:46:05","guid":{"rendered":"https:\/\/steelprogroup.com\/?p=21370"},"modified":"2025-03-05T16:46:08","modified_gmt":"2025-03-05T08:46:08","slug":"s30408-vs-304","status":"publish","type":"post","link":"https:\/\/steelprogroup.com\/ar\/stainless-steel\/grades\/comparisons\/s30408-vs-304\/","title":{"rendered":"\u062f\u0644\u064a\u0644 \u0627\u0644\u0627\u062e\u062a\u0644\u0627\u0641\u0627\u062a \u0628\u064a\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 S30408 \u0648304"},"content":{"rendered":"<p class=\"wp-block-paragraph\">\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 S30408 \u0648304 \u0645\u062a\u0645\u0627\u062b\u0644\u0627\u0646 \u062a\u0642\u0631\u064a\u0628\u064b\u0627 \u0641\u064a \u0627\u0644\u062a\u0631\u0643\u064a\u0628\u060c \u0648\u0627\u0644\u0641\u0631\u0642 \u0627\u0644\u0631\u0626\u064a\u0633\u064a \u0628\u064a\u0646\u0647\u0645\u0627 \u0647\u0648 \u0627\u0644\u0645\u0639\u0627\u064a\u064a\u0631 \u0627\u0644\u062a\u064a \u064a\u062a\u0628\u0639\u0627\u0646\u0647\u0627. \u064a\u062a\u0648\u0627\u0641\u0642 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 S30408 \u0645\u0639 \u0645\u0639\u064a\u0627\u0631 GB\/T 20878 \u0627\u0644\u0635\u064a\u0646\u064a\u060c \u0628\u064a\u0646\u0645\u0627 \u064a\u062a\u0648\u0627\u0641\u0642 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 304 \u0645\u0639 \u0645\u0639\u064a\u0627\u0631 ASTM A240\/AISI.&nbsp;<\/p><p class=\"wp-block-paragraph\">\u0648\u0627\u0635\u0644 \u0627\u0644\u0642\u0631\u0627\u0621\u0629! \u2014\u062a\u0639\u0631\u0641 \u0639\u0644\u0649 \u0627\u0644\u062f\u0631\u062c\u0629 \u0627\u0644\u062a\u064a \u062a\u0646\u0627\u0633\u0628 \u0645\u0634\u0631\u0648\u0639\u0643\u060c \u0648\u0627\u0633\u062a\u0643\u0634\u0641 \u0627\u0644\u0645\u0642\u0627\u0631\u0646\u0627\u062a \u0627\u0644\u0641\u0646\u064a\u0629\u060c \u0648\u0627\u0643\u062a\u0634\u0641 \u0644\u0645\u0627\u0630\u0627 SteelPro Group \u0647\u064a \u0627\u0644\u0645\u0648\u0631\u062f \u0627\u0644\u0645\u0648\u062b\u0648\u0642 \u0628\u0647.<\/p><h2 class=\"wp-block-heading\">\u0645\u0627 \u0647\u0648 S30408\u061f<\/h2><p class=\"wp-block-paragraph\">S30408 \u0647\u0648 \u0646\u0648\u0639 \u0645\u062d\u062f\u062f \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 304 \u0627\u0644\u0645\u0633\u062a\u062e\u062f\u0645 \u0641\u064a \u0628\u0639\u0636 \u0627\u0644\u0645\u0639\u0627\u064a\u064a\u0631 \u0627\u0644\u0625\u0642\u0644\u064a\u0645\u064a\u0629 \u0623\u0648 \u0627\u0644\u0635\u0646\u0627\u0639\u064a\u0629. \u0644\u0647 \u0646\u0641\u0633 \u0627\u0644\u062a\u0631\u0643\u064a\u0628 \u0648\u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0645\u062b\u0644 304\u060c \u0648\u064a\u0648\u0641\u0631 \u0645\u0642\u0627\u0648\u0645\u0629 \u0642\u0648\u064a\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0648\u0642\u0648\u0629 \u0645\u064a\u0643\u0627\u0646\u064a\u0643\u064a\u0629 \u062c\u064a\u062f\u0629. \u063a\u0627\u0644\u0628\u064b\u0627 \u0645\u0627 \u064a\u0633\u062a\u062e\u062f\u0645 \u0641\u064a \u0623\u062c\u0632\u0627\u0621 \u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a \u0648\u0645\u0635\u0627\u0631\u0641 \u0627\u0644\u0645\u0637\u0628\u062e \u0648\u0623\u0646\u0638\u0645\u0629 \u0627\u0644\u0639\u0627\u062f\u0645 \u0628\u0633\u0628\u0628 \u0642\u0627\u0628\u0644\u064a\u062a\u0647 \u0644\u0644\u062a\u0644\u062d\u064a\u0645 \u0648\u0633\u0647\u0648\u0644\u0629 \u0627\u0644\u062a\u0635\u0646\u064a\u0639. \u0645\u0639 \u0642\u0648\u0629 \u062e\u0636\u0648\u0639 \u062a\u0628\u0644\u063a 205 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644 \u0648\u0642\u0648\u0629 \u0634\u062f \u062a\u062a\u0631\u0627\u0648\u062d \u0628\u064a\u0646 520 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644 \u0648680 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644\u060c \u064a\u0648\u0641\u0631 S30408 \u0623\u062f\u0627\u0621\u064b \u0645\u0634\u0627\u0628\u0647\u064b\u0627 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 304.<\/p><h2 class=\"wp-block-heading\">\u0645\u0627 \u0647\u0648 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 304\u061f<\/h2><p class=\"wp-block-paragraph\">\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 304\u060c \u0627\u0644\u0645\u0639\u0631\u0648\u0641 \u0623\u064a\u0636\u064b\u0627 \u0628\u0627\u0633\u0645 AISI 304\u060c \u0647\u0648 \u0645\u0627\u062f\u0629 \u0634\u062f\u064a\u062f\u0629 \u0627\u0644\u0645\u0642\u0627\u0648\u0645\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0645\u0635\u0646\u0648\u0639\u0629 \u0645\u0646 \u0627\u0644\u0643\u0631\u0648\u0645 \u0648\u0627\u0644\u0646\u064a\u0643\u0644. \u064a\u0645\u0646\u062d\u0647 \u0647\u0630\u0627 \u0627\u0644\u0645\u0632\u064a\u062c \u0645\u0642\u0627\u0648\u0645\u0629 \u0645\u0645\u062a\u0627\u0632\u0629 \u0644\u0644\u0635\u062f\u0623 \u0648\u0627\u0644\u0623\u0643\u0633\u062f\u0629. \u0645\u0646 \u0627\u0644\u0633\u0647\u0644 \u062a\u0634\u0643\u064a\u0644\u0647 \u0648\u062a\u0634\u0643\u064a\u0644\u0647\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647 \u0634\u0627\u0626\u0639\u064b\u0627 \u0641\u064a \u0627\u0644\u0635\u0646\u0627\u0639\u0627\u062a \u0645\u062b\u0644 \u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0623\u063a\u0630\u064a\u0629 \u0648\u0627\u0644\u0623\u062c\u0647\u0632\u0629 \u0627\u0644\u0637\u0628\u064a\u0629 \u0648\u0623\u062c\u0647\u0632\u0629 \u0627\u0644\u0645\u0637\u0628\u062e. \u062a\u062c\u0639\u0644\u0647 \u0642\u0648\u062a\u0647 \u0648\u0645\u0631\u0648\u0646\u062a\u0647 \u0645\u062b\u0627\u0644\u064a\u064b\u0627 \u0644\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0627\u062a \u0627\u0644\u062a\u064a \u062a\u062a\u0637\u0644\u0628 \u0627\u0644\u0646\u0638\u0627\u0641\u0629 \u0648\u0627\u0644\u0645\u062a\u0627\u0646\u0629 \u0627\u0644\u0645\u0645\u062a\u062f\u0629.<\/p><h2 class=\"wp-block-heading\">\u0645\u0648\u0627\u0635\u0641\u0627\u062a S30408 | 304 | S30400 | 06Cr19Ni10<\/h2><figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td><strong>\u062f\u0631\u062c\u0629<\/strong><\/td><td><strong>\u0631\u0645\u0632 \u0627\u0644\u0623\u0645\u0645 \u0627\u0644\u0645\u062a\u062d\u062f\u0629<\/strong><\/td><td><strong>\u0627\u0644\u0645\u0639\u0627\u064a\u064a\u0631<\/strong><\/td><td><strong>\u0627\u0644\u0628\u0644\u062f\/\u0627\u0644\u0645\u0646\u0637\u0642\u0629<\/strong><\/td><\/tr><tr><td>304<\/td><td>\u063330400<\/td><td>ASTM A240M-15a<\/td><td>\u0627\u0645\u0631\u064a\u0643\u064a<\/td><\/tr><tr><td>06Cr19Ni10<\/td><td>\u063330408<\/td><td>\u062c\u064a \u0628\u064a\/\u062a\u064a24511\u060c \u062c\u064a \u0628\u064a\/\u062a\u064a20878<\/td><td>\u0627\u0644\u0635\u064a\u0646<\/td><\/tr><tr><td>\u0625\u0633 \u064a\u0648 \u0625\u0633 304<\/td><td>&#8211;<\/td><td>JISG4305:2012<\/td><td>\u0627\u0644\u064a\u0627\u0628\u0627\u0646\u064a\u0629<\/td><\/tr><tr><td>1.4301<\/td><td>&#8211;<\/td><td>EN10028-7:2016<\/td><td>\u0623\u0648\u0631\u0648\u0628\u0627<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u0646\u0638\u0631\u0629 \u0639\u0627\u0645\u0629 \u0639\u0644\u0649 \u0627\u0644\u0627\u062e\u062a\u0644\u0627\u0641\u0627\u062a \u0627\u0644\u0631\u0626\u064a\u0633\u064a\u0629 \u0628\u064a\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 S30408 \u0648304<\/h2><p class=\"wp-block-paragraph\">\u0625\u0646 \u0627\u0644\u0641\u0631\u0648\u0642 \u0628\u064a\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 S30408 \u0648\u0627\u0644\u0641\u0648\u0644\u0627\u0630 304 \u0636\u0626\u064a\u0644\u0629\u060c \u062d\u064a\u062b \u064a\u062a\u0645\u062a\u0639 \u0643\u0644\u0627 \u0627\u0644\u0646\u0648\u0639\u064a\u0646 \u0628\u0645\u0642\u0627\u0648\u0645\u0629 \u0645\u0645\u0627\u062b\u0644\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0648\u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0645\u064a\u0643\u0627\u0646\u064a\u0643\u064a\u0629.&nbsp;<\/p><p class=\"wp-block-paragraph\">\u0627\u0644\u062a\u0645\u064a\u064a\u0632 \u0627\u0644\u0631\u0626\u064a\u0633\u064a \u064a\u0643\u0645\u0646 \u0641\u064a <strong>\u063330408<\/strong> \u064a\u062d\u062a\u0648\u064a \u0639\u0644\u0649 \u0646\u0633\u0628\u0629 \u0623\u0642\u0644 \u0645\u0646 \u0627\u0644\u0643\u0631\u0628\u0648\u0646 \u0648\u0645\u062d\u062a\u0648\u0649 \u0623\u0639\u0644\u0649 \u0642\u0644\u064a\u0644\u0627\u064b \u0645\u0646 \u0627\u0644\u0646\u064a\u0643\u0644\u060c \u0645\u0645\u0627 \u064a\u0645\u0643\u0646 \u0623\u0646 \u064a\u0639\u0632\u0632 \u0623\u062f\u0627\u0626\u0647 \u0641\u064a \u0638\u0631\u0648\u0641 \u0645\u0639\u064a\u0646\u0629\u060c \u0645\u062b\u0644 \u062f\u0631\u062c\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u0645\u0631\u062a\u0641\u0639\u0629.&nbsp;<\/p><p class=\"wp-block-paragraph\">\u0648\u0645\u0639 \u0630\u0644\u0643\u060c \u0641\u0625\u0646 \u0647\u0630\u0647 \u0627\u0644\u0627\u062e\u062a\u0644\u0627\u0641\u0627\u062a \u0644\u064a\u0633\u062a \u0643\u0628\u064a\u0631\u0629 \u0628\u0645\u0627 \u064a\u0643\u0641\u064a \u0644\u0644\u062a\u0623\u062b\u064a\u0631 \u0628\u0634\u0643\u0644 \u0643\u0628\u064a\u0631 \u0639\u0644\u0649 \u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0627\u062a\u0647\u0627 \u0627\u0644\u0639\u0627\u0645\u0629.<\/p><figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td><strong>\u0645\u064a\u0632\u0629<\/strong><\/td><td><strong>\u063330408<\/strong><\/td><td><strong>304 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623<\/strong><\/td><\/tr><tr><td>\u0645\u0639\u064a\u0627\u0631<\/td><td>\u062c\u064a \u0628\u064a\/\u062a\u064a 20878<\/td><td>ASTM A240 \/ AISI 304<\/td><\/tr><tr><td>\u0645\u062d\u062a\u0648\u0649 \u0627\u0644\u0643\u0631\u0628\u0648\u0646<\/td><td>\u0645\u062d\u062a\u0648\u0649 \u0627\u0644\u0643\u0631\u0628\u0648\u0646 \u0623\u0642\u0644 (\u22640.06%)<\/td><td>\u0645\u062d\u062a\u0648\u0649 \u0643\u0631\u0628\u0648\u0646 \u0623\u0639\u0644\u0649 (\u062d\u062a\u0649 0.08%)<\/td><\/tr><tr><td>\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644<\/td><td>\u062a\u062d\u0633\u064a\u0646 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644 \u0628\u0633\u0628\u0628 \u0627\u0631\u062a\u0641\u0627\u0639 \u0646\u0633\u0628\u0629 \u0627\u0644\u0646\u064a\u0643\u0644<\/td><td>\u0645\u0642\u0627\u0648\u0645\u0629 \u0645\u0645\u062a\u0627\u0632\u0629 \u0644\u0644\u062a\u0622\u0643\u0644<\/td><\/tr><tr><td>\u0627\u0644\u062e\u0648\u0627\u0635 \u0627\u0644\u0645\u064a\u0643\u0627\u0646\u064a\u0643\u064a\u0629<\/td><td>\u0642\u0648\u0629 \u0623\u0641\u0636\u0644 \u0648\u0623\u062f\u0627\u0621 \u0623\u0641\u0636\u0644 \u0641\u064a \u062f\u0631\u062c\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u0639\u0627\u0644\u064a\u0629<\/td><td>\u0642\u0648\u0629 \u0627\u0644\u0623\u062f\u0627\u0621 \u0648\u062f\u0631\u062c\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u0642\u064a\u0627\u0633\u064a\u0629<\/td><\/tr><tr><td>\u0642\u0627\u0628\u0644\u064a\u0629 \u0627\u0644\u0644\u062d\u0627\u0645<\/td><td>\u0642\u0627\u0628\u0644\u064a\u0629 \u0627\u0644\u0644\u062d\u0627\u0645 \u0623\u0641\u0636\u0644 \u0628\u0633\u0628\u0628 \u0645\u062d\u062a\u0648\u0649 \u0627\u0644\u0646\u064a\u0643\u0644 \u0627\u0644\u0623\u0639\u0644\u0649<\/td><td>\u0642\u0627\u0628\u0644\u064a\u0629 \u0627\u0644\u0644\u062d\u0627\u0645 \u062c\u064a\u062f\u0629<\/td><\/tr><tr><td>\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a<\/td><td>\u0645\u0646\u0627\u0633\u0628 \u0644\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u0642\u0627\u0633\u064a\u0629 \u0648\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0630\u0627\u062a \u062f\u0631\u062c\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u0639\u0627\u0644\u064a\u0629<\/td><td>\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0639\u0627\u0645\u0629 (\u0645\u062b\u0644 \u0627\u0644\u0623\u063a\u0630\u064a\u0629 \u0648\u0627\u0644\u0637\u0628\u064a\u0629)<\/td><\/tr><tr><td>\u064a\u0643\u0644\u0641<\/td><td>\u0623\u0639\u0644\u0649 \u0642\u0644\u064a\u0644\u0627\u064b \u0628\u0633\u0628\u0628 \u0627\u0644\u062a\u0631\u0643\u064a\u0628\u0629 \u0627\u0644\u0645\u062d\u062f\u062f\u0629<\/td><td>\u0623\u0642\u0644 \u0646\u0633\u0628\u064a\u064b\u0627 \u0648\u0623\u0643\u062b\u0631 \u0634\u064a\u0648\u0639\u064b\u0627<\/td><\/tr><\/tbody><\/table><\/figure><h3 class=\"wp-block-heading\">\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644<\/h3><p class=\"wp-block-paragraph\"><strong>\u063330408<\/strong> \u0644\u062f\u064a\u0647 \u0645\u0642\u0627\u0648\u0645\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0623\u0641\u0636\u0644 \u0642\u0644\u064a\u0644\u0627\u064b \u0645\u0646 <strong>304<\/strong> \u0628\u0633\u0628\u0628:<\/p><ul class=\"wp-block-list\"><li><strong>\u0645\u062d\u062a\u0648\u0649 \u0627\u0644\u0643\u0631\u0628\u0648\u0646 \u0627\u0644\u0645\u0646\u062e\u0641\u0636<\/strong> (\u22640.07% \u0645\u0642\u0627\u0628\u0644 \u22640.08%)\u060c \u0645\u0645\u0627 \u064a\u0642\u0644\u0644 \u0645\u0646 \u062e\u0637\u0631 \u0627\u0644\u062a\u0622\u0643\u0644 \u0628\u064a\u0646 \u0627\u0644\u062d\u0628\u064a\u0628\u0627\u062a \u0628\u0639\u062f \u0627\u0644\u0644\u062d\u0627\u0645.<\/li>\n\n<li><strong>\u0645\u062d\u062a\u0648\u0649 \u0627\u0644\u0643\u0631\u0648\u0645 \u0627\u0644\u0639\u0627\u0644\u064a<\/strong> (18-20% \u0645\u0642\u0627\u0628\u0644 17.5-19.5%)\u060c \u0645\u0645\u0627 \u064a\u0639\u0632\u0632 \u0627\u0633\u062a\u0642\u0631\u0627\u0631 \u0637\u0628\u0642\u0629 \u0627\u0644\u062a\u062e\u0645\u064a\u062f.<\/li>\n\n<li><strong>\u0645\u062d\u062a\u0648\u0649 \u0627\u0644\u0633\u064a\u0644\u064a\u0643\u0648\u0646 \u0627\u0644\u0639\u0627\u0644\u064a<\/strong> (\u22641.00% \u0645\u0642\u0627\u0628\u0644 \u22640.75%)\u060c \u0645\u0645\u0627 \u064a\u062d\u0633\u0646 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u0623\u0643\u0633\u062f\u0629 \u0641\u064a \u062f\u0631\u062c\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0627\u0644\u0639\u0627\u0644\u064a\u0629.<\/li><\/ul><h3 class=\"wp-block-heading\">\u0642\u0627\u0628\u0644\u064a\u0629 \u0627\u0644\u0644\u062d\u0627\u0645<\/h3><p class=\"wp-block-paragraph\">\u0643\u0644\u0627\u0647\u0645\u0627 <strong>\u063330408<\/strong> \u0648 <strong>304 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623<\/strong> \u0645\u0646 \u0627\u0644\u0633\u0647\u0644 \u0644\u062d\u0627\u0645\u0647\u0627\u060c \u0648\u0644\u0643\u0646 \u0645\u0639 \u0648\u062c\u0648\u062f \u0627\u062e\u062a\u0644\u0627\u0641\u0627\u062a \u0635\u063a\u064a\u0631\u0629:<\/p><ul class=\"wp-block-list\"><li><strong>\u063330408<\/strong>:\u064a\u0624\u062f\u064a \u0645\u062d\u062a\u0648\u0649 \u0627\u0644\u0643\u0631\u0628\u0648\u0646 \u0627\u0644\u0645\u0646\u062e\u0641\u0636 (\u22640.07%) \u0625\u0644\u0649 \u062a\u0642\u0644\u064a\u0644 \u062e\u0637\u0631 \u0627\u0644\u062a\u062d\u0633\u0633\u060c \u0648\u0644\u0627 \u064a\u062a\u0637\u0644\u0628 \u0645\u0639\u0627\u0644\u062c\u0629 \u062d\u0631\u0627\u0631\u064a\u0629 \u0625\u0636\u0627\u0641\u064a\u0629 \u0628\u0639\u062f \u0627\u0644\u0644\u062d\u0627\u0645 \u0644\u0644\u062d\u0641\u0627\u0638 \u0639\u0644\u0649 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644.<\/li>\n\n<li><strong>304 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623<\/strong>:\u0642\u062f \u064a\u062a\u0637\u0644\u0628 \u0645\u062d\u062a\u0648\u0649 \u0627\u0644\u0643\u0631\u0628\u0648\u0646 \u0627\u0644\u0623\u0639\u0644\u0649 \u0642\u0644\u064a\u0644\u0627\u064b (\u22640.08%) \u0627\u0644\u062a\u062d\u0643\u0645 \u0641\u064a \u0645\u062f\u062e\u0644\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629 \u0623\u0648 \u0645\u0639\u0627\u0644\u062c\u0627\u062a \u0645\u0627 \u0628\u0639\u062f \u0627\u0644\u0644\u062d\u0627\u0645 \u0645\u062b\u0644 \u0627\u0644\u062a\u062e\u0644\u064a\u0644\u060c \u0648\u062e\u0627\u0635\u0629\u064b \u0628\u0627\u0644\u0646\u0633\u0628\u0629 \u0644\u0644\u0623\u0642\u0633\u0627\u0645 \u0627\u0644\u0623\u0643\u062b\u0631 \u0633\u0645\u0643\u064b\u0627.<\/li><\/ul><h2 class=\"wp-block-heading\">\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 S30408 \u0645\u0642\u0627\u0628\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 304: \u0627\u0644\u062a\u0631\u0643\u064a\u0628 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a<\/h2><figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td><strong>\u0639\u0646\u0635\u0631<\/strong><\/td><td><strong>S30408 (\u062c\u064a \u0628\u064a\/\u062a\u064a 20878)<\/strong><\/td><td><strong><a href=\"https:\/\/steelprogroup.com\/ar\/stainless-steel\/grades\/grade-304\/\">304 (S30400\u060c ASTM)<\/a><\/strong><\/td><td><strong><a href=\"https:\/\/steelprogroup.com\/ar\/nuclear-grade-steel\/304l\/\">304L (S30403\u060c ASTM)<\/a><\/strong><\/td><\/tr><tr><td>\u0627\u0644\u0643\u0631\u0628\u0648\u0646 (C)<\/td><td>\u2264 0.07%<\/td><td>\u2264 0.08%<\/td><td>\u2264 0.03%<\/td><\/tr><tr><td>\u0627\u0644\u0643\u0631\u0648\u0645 (Cr)<\/td><td>18.00\u201320.00%<\/td><td>17.5\u201319.5%<\/td><td>17.5\u201319.5%<\/td><\/tr><tr><td>\u0627\u0644\u0646\u064a\u0643\u0644 (Ni)<\/td><td>8.00\u201311.00%<\/td><td>8.0\u201310.5%<\/td><td>8.0\u201312.0%<\/td><\/tr><tr><td>\u0627\u0644\u0645\u0646\u063a\u0646\u064a\u0632 (Mn)<\/td><td>\u2264 2.00%<\/td><td>\u2264 2.00%<\/td><td>\u2264 2.00%<\/td><\/tr><tr><td>\u0627\u0644\u0633\u064a\u0644\u064a\u0643\u0648\u0646 (Si)<\/td><td>\u2264 1.00%<\/td><td>\u2264 0.75%<\/td><td>\u2264 0.75%<\/td><\/tr><tr><td>\u0627\u0644\u0641\u0648\u0633\u0641\u0648\u0631 (P)<\/td><td>\u2264 0.045%<\/td><td>\u2264 0.045%<\/td><td>\u2264 0.045%<\/td><\/tr><tr><td>\u0627\u0644\u0643\u0628\u0631\u064a\u062a (S)<\/td><td>\u2264 0.030%<\/td><td>\u2264 0.030%<\/td><td>\u2264 0.030%<\/td><\/tr><tr><td>\u0627\u0644\u0646\u064a\u062a\u0631\u0648\u062c\u064a\u0646 (\u0646)<\/td><td>\u2264 0.10%<\/td><td>\u2264 0.10%<\/td><td>\u2264 0.10%<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 S30408 \u0645\u0642\u0627\u0628\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 304: \u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0645\u064a\u0643\u0627\u0646\u064a\u0643\u064a\u0629<\/h2><ul class=\"wp-block-list\"><li>\u062d\u062f \u0635\u0644\u0627\u0628\u0629 ASTM 304 (\u2264201 HBW) \u0623\u0639\u0644\u0649 \u0642\u0644\u064a\u0644\u0627\u064b \u0645\u0646 \u062d\u062f \u0635\u0644\u0627\u0628\u0629 S30408 (\u2264187 HBW). \u0648\u0645\u0639 \u0630\u0644\u0643\u060c \u0643\u0644\u0627\u0647\u0645\u0627 \u0641\u064a \u062d\u0627\u0644\u0629 \u0627\u0644\u062a\u0644\u062f\u064a\u0646\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647\u0645\u0627 \u0645\u062b\u0627\u0644\u064a\u064a\u0646 \u0644\u0644\u0639\u0645\u0644 \u0627\u0644\u0628\u0627\u0631\u062f.<\/li><\/ul><figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td><strong>\u0645\u0644\u0643\u064a\u0629<\/strong><\/td><td><strong>\u0641\u0648\u0644\u0627\u0630 S30408<\/strong><\/td><td><strong>304 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623<\/strong><\/td><\/tr><tr><td>\u0642\u0648\u0629 \u0627\u0644\u0634\u062f<\/td><td>\u2265520 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644 (75 \u0643\u064a\u0644\u0648\u0628\u0627\u0633\u0643\u0627\u0644)<\/td><td>\u2265515 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644 (75 \u0643\u064a\u0644\u0648\u0628\u0627\u0633\u0643\u0627\u0644)<\/td><\/tr><tr><td>\u0642\u0648\u0629 \u0627\u0644\u062e\u0636\u0648\u0639<\/td><td>\u2265205 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644 (30 \u0643\u064a\u0644\u0648\u0628\u0627\u0633\u0643\u0627\u0644)<\/td><td>\u2265205 \u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644 (30 \u0643\u064a\u0644\u0648\u0628\u0627\u0633\u0643\u0627\u0644)<\/td><\/tr><tr><td>\u0627\u0633\u062a\u0637\u0627\u0644\u0629<\/td><td>\u226540%<\/td><td>\u226540%<\/td><\/tr><tr><td>\u0635\u0644\u0627\u0628\u0629<\/td><td>\u2264187 \u0648\u0632\u0646 \u0627\u0644\u062c\u0633\u0645<\/td><td>\u2264201 \u0648\u0632\u0646 \u0627\u0644\u062c\u0633\u0645<\/td><\/tr><tr><td>\u0645\u0639\u0627\u0645\u0644 \u0627\u0644\u0645\u0631\u0648\u0646\u0629<\/td><td>~193 \u062c\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644 (28 \u00d7 10\u2076 \u0631\u0637\u0644\/\u0628\u0648\u0635\u0629 \u0645\u0631\u0628\u0639\u0629)<\/td><td>~193 \u062c\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644 (28 \u00d7 10\u2076 \u0631\u0637\u0644\/\u0628\u0648\u0635\u0629 \u0645\u0631\u0628\u0639\u0629)<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 S30408 \u0645\u0642\u0627\u0628\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 304: \u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0641\u064a\u0632\u064a\u0627\u0626\u064a\u0629<\/h2><p class=\"wp-block-paragraph\">\u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u0641\u064a\u0632\u064a\u0627\u0626\u064a\u0629 \u0644 <strong>\u063330408<\/strong> \u0645\u062a\u0637\u0627\u0628\u0642\u0629 \u0645\u0639 \u062a\u0644\u0643 \u0627\u0644\u0645\u0648\u062c\u0648\u062f\u0629 \u0641\u064a <strong>ASTM 304<\/strong>. \u0643\u0644\u0627 \u0627\u0644\u062f\u0631\u062c\u062a\u064a\u0646 \u062a\u062d\u0627\u0641\u0638\u0627\u0646 \u0639\u0644\u0649 \u0627\u0644\u0646\u0648\u0627\u0629 <strong>\u0628\u0646\u064a\u0629 \u0623\u0648\u0633\u062a\u0646\u064a\u062a\u064a\u0629 18\/8 (\u0643\u0631\u0648\u0645\/\u0646\u064a\u0643\u0644)<\/strong>\u060c \u0645\u0645\u0627 \u064a\u0624\u062f\u064a \u0625\u0644\u0649 \u062e\u0635\u0627\u0626\u0635 \u0623\u062f\u0627\u0621 \u0642\u0627\u0628\u0644\u0629 \u0644\u0644\u0645\u0642\u0627\u0631\u0646\u0629.<\/p><figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td><strong>\u0645\u0644\u0643\u064a\u0629<\/strong><\/td><td><strong>\u0627\u0644\u0642\u064a\u0645\u0629 (\u0627\u0644\u0625\u0645\u0628\u0631\u0627\u0637\u0648\u0631\u064a\u0629)<\/strong><\/td><td><strong>\u0627\u0644\u0642\u064a\u0645\u0629 (\u0645\u062a\u0631\u064a\u0629)<\/strong><\/td><\/tr><tr><td>\u0646\u0642\u0637\u0629 \u0627\u0644\u0627\u0646\u0635\u0647\u0627\u0631<\/td><td>2552~2650 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a<\/td><td>1398~1454 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629<\/td><\/tr><tr><td>\u0627\u0644\u0633\u0639\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629 \u0627\u0644\u0646\u0648\u0639\u064a\u0629<\/td><td>0.5 \u0643\u064a\u0644\u0648\u062c\u0648\u0644\/(\u0643\u062c\u0645\u00b7\u0643)<\/td><td>0.5 \u0643\u064a\u0644\u0648\u062c\u0648\u0644\/(\u0643\u062c\u0645\u00b7\u0643)<\/td><\/tr><tr><td>\u0627\u0644\u0645\u0648\u0635\u0644\u064a\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629 (212 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a\/100 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629)<\/td><td>10.7 \u0648\u062d\u062f\u0629 \u062d\u0631\u0627\u0631\u064a\u0629 \u0628\u0631\u064a\u0637\u0627\u0646\u064a\u0629\/(\u0633\u0627\u0639\u0629\u00b7\u0642\u062f\u0645\u00b7\u062f\u0631\u062c\u0629\u00b7\u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a\u00b7\u0628\u0648\u0635\u0629)<\/td><td>16.3 \u0648\u0627\u0637\/(\u0645\u00b7\u0643)<\/td><\/tr><tr><td>\u0627\u0644\u0645\u0648\u0635\u0644\u064a\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u064a\u0629 (932 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a\/500 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629)<\/td><td>15.5 \u0648\u062d\u062f\u0629 \u062d\u0631\u0627\u0631\u064a\u0629 \u0628\u0631\u064a\u0637\u0627\u0646\u064a\u0629\/(\u0633\u0627\u0639\u0629\u00b7\u0642\u062f\u0645\u00b7\u062f\u0631\u062c\u0629\u00b7\u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a\u00b7\u0628\u0648\u0635\u0629)<\/td><td>21.5 \u0648\u0627\u0637\/(\u0645\u00b7\u0643)<\/td><\/tr><tr><td>\u0645\u0639\u0627\u0645\u0644 \u0627\u0644\u062a\u0645\u062f\u062f \u0627\u0644\u062e\u0637\u064a<\/td><td>9.6 \u00d7 10\u207b\u2076\/\u00b0\u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a<\/td><td>17.2 \u00d7 10\u207b\u2076\/\u0643<\/td><\/tr><tr><td>\u0627\u0644\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u0643\u0647\u0631\u0628\u0627\u0626\u064a\u0629 (68 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a\/20 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629)<\/td><td>14.0 \u0645\u064a\u0643\u0631\u0648 \u0623\u0648\u0645\u00b7\u0628\u0648\u0635\u0629<\/td><td>18.4 \u0645\u064a\u0643\u0631\u0648 \u0623\u0648\u0645\u00b7\u0645\u00b2\/\u0645<\/td><\/tr><tr><td>\u0645\u0639\u0627\u0645\u0644 \u0627\u0644\u0645\u0631\u0648\u0646\u0629 \u0627\u0644\u0637\u0648\u0644\u064a (68 \u062f\u0631\u062c\u0629 \u0641\u0647\u0631\u0646\u0647\u0627\u064a\u062a\/20 \u062f\u0631\u062c\u0629 \u0645\u0626\u0648\u064a\u0629)<\/td><td>10539 \u0643.\u0633.<\/td><td>193 \u0643\u064a\u0644\u0648 \u0646\u064a\u0648\u062a\u0646\/\u0645\u0644\u0645\u00b2<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 S30408 \u0645\u0642\u0627\u0628\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 304: \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a<\/h2><p class=\"wp-block-paragraph\">\u0643\u0644\u0627 \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 S30408 \u0648 304 <strong>\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0627\u0644\u0623\u0648\u0633\u062a\u0646\u064a\u062a\u064a<\/strong> \u0645\u0639 \u0645\u0642\u0627\u0648\u0645\u0629 \u0645\u062a\u0637\u0627\u0628\u0642\u0629 \u062a\u0642\u0631\u064a\u0628\u064b\u0627 \u0644\u0644\u062a\u0622\u0643\u0644\u060c \u0648\u0642\u0627\u0628\u0644\u064a\u0629 \u0627\u0644\u062a\u0634\u0643\u064a\u0644\u060c \u0648\u0642\u0627\u0628\u0644\u064a\u0629 \u0627\u0644\u0644\u062d\u0627\u0645. \u062a\u064f\u0633\u062a\u062e\u062f\u0645 \u0639\u0644\u0649 \u0646\u0637\u0627\u0642 \u0648\u0627\u0633\u0639 \u0641\u064a:<\/p><ul class=\"wp-block-list\"><li><strong>\u0635\u0646\u0627\u0639\u0629 \u0627\u0644\u0623\u063a\u0630\u064a\u0629 \u0648\u0627\u0644\u0645\u0634\u0631\u0648\u0628\u0627\u062a<\/strong>:\u0627\u0644\u062e\u0632\u0627\u0646\u0627\u062a \u0648\u0627\u0644\u0623\u0646\u0627\u0628\u064a\u0628 \u0648\u0623\u0646\u0638\u0645\u0629 \u0627\u0644\u0646\u0642\u0644 \u0648\u0623\u0648\u0627\u0646\u064a \u0627\u0644\u0637\u0647\u064a<\/li>\n\n<li><strong>\u0627\u0644\u0647\u0646\u062f\u0633\u0629 \u0627\u0644\u0645\u0639\u0645\u0627\u0631\u064a\u0629 \u0648\u0627\u0644\u0628\u0646\u0627\u0621<\/strong>:\u0627\u0644\u0645\u0643\u0648\u0646\u0627\u062a \u0627\u0644\u0647\u064a\u0643\u0644\u064a\u0629 \u0648\u0627\u0644\u0648\u0627\u062c\u0647\u0627\u062a \u0648\u0627\u0644\u062f\u0631\u0627\u0628\u0632\u064a\u0646 \u0648\u0627\u0644\u0623\u0633\u0642\u0641.<\/li>\n\n<li><strong>\u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629<\/strong>:\u062e\u0632\u0627\u0646\u0627\u062a \u0627\u0644\u062a\u062e\u0632\u064a\u0646 \u0648\u0627\u0644\u0635\u0645\u0627\u0645\u0627\u062a \u0648\u0627\u0644\u0623\u0646\u0627\u0628\u064a\u0628 \u0644\u0644\u0645\u0648\u0627\u062f \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629 \u0627\u0644\u0645\u0633\u0628\u0628\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0627\u0644\u062e\u0641\u064a\u0641.<\/li>\n\n<li><strong>\u0627\u0644\u0623\u062c\u0647\u0632\u0629 \u0627\u0644\u0637\u0628\u064a\u0629<\/strong>:\u0627\u0644\u0623\u062f\u0648\u0627\u062a \u0627\u0644\u062c\u0631\u0627\u062d\u064a\u0629 \u0648\u0627\u0644\u0635\u0648\u0627\u0646\u064a \u0648\u0627\u0644\u0645\u0639\u062f\u0627\u062a \u0627\u0644\u0645\u062a\u0648\u0627\u0641\u0642\u0629 \u0645\u0639 \u0627\u0644\u062a\u0635\u0648\u064a\u0631 \u0628\u0627\u0644\u0631\u0646\u064a\u0646 \u0627\u0644\u0645\u063a\u0646\u0627\u0637\u064a\u0633\u064a.<\/li><\/ul><h2 class=\"wp-block-heading\">\u0623\u0628\u0639\u0627\u062f \u0645\u0646\u062a\u062c\u0627\u062a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 S30408<\/h2><p class=\"wp-block-paragraph\">\u062a\u0636\u0645\u0646 \u0645\u062c\u0645\u0648\u0639\u0629 SteelPro \u0623\u0646 \u062c\u0645\u064a\u0639 \u0645\u0646\u062a\u062c\u0627\u062a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 S30408 \u062a\u0644\u0628\u064a \u0645\u0639\u0627\u064a\u064a\u0631 \u0627\u0644\u062c\u0648\u062f\u0629 \u0627\u0644\u0639\u0627\u0644\u064a\u0629. \u0646\u062d\u0646 \u0646\u0642\u062f\u0645 \u0645\u0646\u062a\u062c\u0627\u062a \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 S30408 \u0628\u0623\u0628\u0639\u0627\u062f \u0645\u062e\u062a\u0644\u0641\u0629\u060c \u0628\u0645\u0627 \u0641\u064a \u0630\u0644\u0643 \u0627\u0644\u0623\u0644\u0648\u0627\u062d \u0648\u0627\u0644\u0623\u0644\u0648\u0627\u062d \u0648\u0627\u0644\u0623\u0646\u0627\u0628\u064a\u0628 \u063a\u064a\u0631 \u0627\u0644\u0645\u0644\u062d\u0648\u0645\u0629.<\/p><figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td><strong>\u0645\u0646\u062a\u062c<\/strong><\/td><td><strong>\u0627\u0644\u0628\u0639\u062f (\u0645\u062a\u0631\u064a)<\/strong><\/td><td><strong>\u0627\u0644\u0628\u0639\u062f (\u0625\u0645\u0628\u0631\u0627\u0637\u0648\u0631\u064a)<\/strong><\/td><\/tr><tr><td rowspan=\"3\"><strong><a href=\"https:\/\/steelprogroup.com\/ar\/stainless-steel\/sheet\/304-sheet\/\">\u0635\u0641\u0627\u0626\u062d\/\u0623\u0644\u0648\u0627\u062d<\/a><\/strong><\/td><td>\u0627\u0644\u0633\u0645\u0643: 0.5 \u0645\u0644\u0645 \u2013 100 \u0645\u0644\u0645<\/td><td>\u0627\u0644\u0633\u0645\u0643: 0.02 \u0628\u0648\u0635\u0629 \u2013 4 \u0628\u0648\u0635\u0629<\/td><\/tr><tr><td>\u0627\u0644\u0639\u0631\u0636: 100 \u0645\u0644\u0645 \u2013 2000 \u0645\u0644\u0645<\/td><td>\u0627\u0644\u0639\u0631\u0636: 4 \u0628\u0648\u0635\u0629 \u2013 79 \u0628\u0648\u0635\u0629<\/td><\/tr><tr><td>\u0627\u0644\u0637\u0648\u0644: 1000 \u0645\u0644\u0645 \u2013 6000 \u0645\u0644\u0645<\/td><td>\u0627\u0644\u0637\u0648\u0644: 39 \u0628\u0648\u0635\u0629 \u2013 236 \u0628\u0648\u0635\u0629<\/td><\/tr><tr><td rowspan=\"3\"><a href=\"https:\/\/steelprogroup.com\/ar\/stainless-steel\/tubing\/304-tubing\/\"><strong>\u0623\u0646\u0627\u0628\u064a\u0628 \u0628\u062f\u0648\u0646 \u062f\u0631\u0632\u0627\u062a<\/strong><\/a><\/td><td>\u0627\u0644\u0642\u0637\u0631 \u0627\u0644\u062e\u0627\u0631\u062c\u064a: 6 \u0645\u0645 \u2013 120 \u0645\u0645<\/td><td>\u0627\u0644\u0642\u0637\u0631 \u0627\u0644\u062e\u0627\u0631\u062c\u064a: 0.24 \u0628\u0648\u0635\u0629 \u2013 4.7 \u0628\u0648\u0635\u0629<\/td><\/tr><tr><td>\u0633\u0645\u0643 \u0627\u0644\u062c\u062f\u0627\u0631: 0.5 \u0645\u0645 \u2013 20 \u0645\u0645<\/td><td>\u0633\u0645\u0643 \u0627\u0644\u062c\u062f\u0627\u0631: 0.02 \u0628\u0648\u0635\u0629 \u2013 0.79 \u0628\u0648\u0635\u0629<\/td><\/tr><tr><td>\u0627\u0644\u0637\u0648\u0644: 1000 \u0645\u0644\u0645 \u2013 12000 \u0645\u0644\u0645<\/td><td>\u0627\u0644\u0637\u0648\u0644: 39 \u0628\u0648\u0635\u0629 \u2013 472 \u0628\u0648\u0635\u0629<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u0645\u0648\u0631\u062f\u0643 \u0627\u0644\u0645\u0648\u062b\u0648\u0642 \u0628\u0647 \u0644\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 S30408 \u0648 304<\/h2><p class=\"wp-block-paragraph\">\u0639\u0646\u062f\u0645\u0627 \u062a\u0643\u0648\u0646 \u0627\u0644\u062f\u0642\u0629 \u0648\u0627\u0644\u0645\u062a\u0627\u0646\u0629 \u0623\u0645\u0631\u0627\u0646 \u0645\u0647\u0645\u0627\u0646\u060c \u0627\u062e\u062a\u0631 <strong>\u063330408<\/strong> \u0623\u0648 <strong>304 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623<\/strong> \u0645\u0646 \u0645\u062c\u0645\u0648\u0639\u0629 SteelPro. \u0646\u062d\u0646 \u0646\u0642\u062f\u0645 \u0645\u062c\u0645\u0648\u0639\u0629 \u0645\u062a\u0646\u0648\u0639\u0629 \u0645\u0646 \u0627\u0644\u0623\u062d\u062c\u0627\u0645\u060c \u0628\u0645\u0627 \u0641\u064a \u0630\u0644\u0643 \u0627\u0644\u0623\u0644\u0648\u0627\u062d \u0648\u0627\u0644\u0623\u0644\u0648\u0627\u062d \u0648\u0627\u0644\u0623\u0646\u0627\u0628\u064a\u0628 \u063a\u064a\u0631 \u0627\u0644\u0645\u0644\u062d\u0648\u0645\u0629.&nbsp;<\/p><p class=\"wp-block-paragraph\">\u0646\u062d\u0646 \u0646\u0642\u062f\u0645 \u0623\u064a\u0636\u064b\u0627 \u0645\u0646\u062a\u062c\u0627\u062a \u0623\u062e\u0631\u0649 \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0645\u062b\u0644 <strong><a href=\"https:\/\/steelprogroup.com\/ar\/stainless-steel\/plate\/304-304l-304h-plate\/\">\u0623\u0644\u0648\u0627\u062d 304L \u0648\u0623\u0644\u0648\u0627\u062d 304H<\/a><\/strong>\u0628\u0641\u0636\u0644 \u062e\u0628\u0631\u062a\u0646\u0627 \u0648\u0627\u0644\u0645\u0639\u0627\u064a\u064a\u0631 \u0627\u0644\u0639\u0627\u0644\u064a\u0629 \u0627\u0644\u062a\u064a \u0646\u0644\u062a\u0632\u0645 \u0628\u0647\u0627\u060c \u064a\u0645\u0643\u0646\u0643 \u0627\u0644\u0627\u0639\u062a\u0645\u0627\u062f \u0639\u0644\u0649 \u0627\u0644\u062e\u062f\u0645\u0629 \u0627\u0644\u0645\u0648\u062b\u0648\u0642\u0629 \u0648\u0627\u0644\u062a\u0633\u0644\u064a\u0645 \u0641\u064a \u0627\u0644\u0648\u0642\u062a \u0627\u0644\u0645\u062d\u062f\u062f.<\/p>","protected":false},"excerpt":{"rendered":"<p>\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 S30408 \u0648304 \u0645\u062a\u0637\u0627\u0628\u0642\u0627\u0646 \u062a\u0642\u0631\u064a\u0628\u064b\u0627 \u0641\u064a \u0627\u0644\u062a\u0631\u0643\u064a\u0628\u060c \u0648\u0627\u0644\u0641\u0631\u0642 \u0627\u0644\u0631\u0626\u064a\u0633\u064a \u064a\u0643\u0645\u0646 \u0641\u064a \u0627\u0644\u0645\u0639\u0627\u064a\u064a\u0631 \u0627\u0644\u062a\u064a \u064a\u062a\u0628\u0639\u0627\u0646\u0647\u0627. S30408 [\u2026]<\/p>","protected":false},"author":1,"featured_media":21371,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"_eb_attr":"","rank_math_lock_modified_date":false,"site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"categories":[4192,4191,112],"tags":[],"class_list":["post-21370","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-comparisons","category-grades","category-stainless-steel"],"acf":[],"_links":{"self":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts\/21370","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/comments?post=21370"}],"version-history":[{"count":0,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts\/21370\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/media\/21371"}],"wp:attachment":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/media?parent=21370"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/categories?post=21370"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/tags?post=21370"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}