{"id":7833,"date":"2024-08-08T01:16:00","date_gmt":"2024-08-07T17:16:00","guid":{"rendered":"https:\/\/app11147.cloudwayssites.com\/?p=7833"},"modified":"2024-11-13T13:01:14","modified_gmt":"2024-11-13T05:01:14","slug":"rebar","status":"publish","type":"post","link":"https:\/\/steelprogroup.com\/ar\/steel-bar\/rebar-sizes-types-grades-uses\/","title":{"rendered":"\u0623\u0633\u0627\u0633\u064a\u0627\u062a \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d: \u0623\u062d\u062c\u0627\u0645 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0648\u0623\u0646\u0648\u0627\u0639\u0647 \u0648\u062f\u0631\u062c\u0627\u062a\u0647 \u0648\u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0627\u062a\u0647"},"content":{"rendered":"<p class=\"wp-block-paragraph\">\u062a\u062a\u0648\u0627\u062c\u062f \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0641\u064a \u0643\u0644 \u0645\u0643\u0627\u0646 \u0641\u064a \u062d\u064a\u0627\u062a\u0646\u0627\u060c \u0648\u0644\u0643\u0646 \u0646\u0627\u062f\u0631\u064b\u0627 \u0645\u0627 \u0646\u0631\u0649 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d. \u0648\u0630\u0644\u0643 \u0644\u0623\u0646\u0647\u0627 \u0639\u0646\u0635\u0631 \u0623\u0633\u0627\u0633\u064a \u0641\u064a \u0627\u0644\u0628\u0646\u0627\u0621 \u0648\u062a\u0633\u062a\u062e\u062f\u0645 \u0644\u062a\u0642\u0648\u064a\u0629 \u0627\u0644\u0647\u064a\u0627\u0643\u0644 \u0627\u0644\u062e\u0631\u0633\u0627\u0646\u064a\u0629 \u0644\u062a\u062d\u0645\u0644 \u0627\u0644\u0636\u063a\u0637 \u0627\u0644\u0647\u0627\u0626\u0644.<\/p><p class=\"wp-block-paragraph\">\u0633\u062a\u0642\u062f\u0645 \u0647\u0630\u0647 \u0627\u0644\u0645\u0642\u0627\u0644\u0629 \u0631\u0624\u0649 \u0645\u062a\u0639\u0645\u0642\u0629 \u062d\u0648\u0644 \u062a\u0631\u0643\u064a\u0628 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0648\u062a\u0635\u0646\u064a\u0639\u0647\u0627 \u0648\u0623\u0646\u0648\u0627\u0639\u0647\u0627 \u0648\u062f\u0631\u062c\u0627\u062a\u0647\u0627 \u0648\u0623\u062d\u062c\u0627\u0645\u0647\u0627 \u0648\u0627\u062a\u062c\u0627\u0647\u0627\u062a\u0647\u0627 \u0627\u0644\u0645\u0633\u062a\u0642\u0628\u0644\u064a\u0629 \u0644\u0645\u0633\u0627\u0639\u062f\u062a\u0643 \u0639\u0644\u0649 \u062a\u0639\u0645\u064a\u0642 \u0641\u0647\u0645\u0643 \u0644\u0647\u0627\u060c \u0648\u0627\u0644\u0633\u0645\u0627\u062d \u0644\u0643 \u0628\u0627\u062a\u062e\u0627\u0630 \u0642\u0631\u0627\u0631\u0627\u062a \u0645\u0633\u062a\u0646\u064a\u0631\u0629 \u062d\u0648\u0644 \u0645\u0645\u0627\u0631\u0633\u0627\u062a \u0627\u0644\u0628\u0646\u0627\u0621 \u0627\u0644\u062e\u0627\u0635\u0629 \u0628\u0643.<\/p><h2 class=\"wp-block-heading\">\u0645\u0627 \u0647\u0648 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d\u061f<\/h2><p class=\"wp-block-paragraph\">\u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d\u060c \u0627\u0644\u0645\u0639\u0631\u0648\u0641 \u0623\u064a\u0636\u064b\u0627 \u0628\u0627\u0633\u0645 \u0642\u0636\u064a\u0628 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0623\u0648 \u0642\u0636\u064a\u0628 \u0627\u0644\u062a\u0633\u0644\u064a\u062d\u060c \u0647\u0648 \u0642\u0636\u064a\u0628 \u0641\u0648\u0644\u0627\u0630\u064a \u0635\u0644\u0628 \u0645\u0635\u0646\u0648\u0639 \u0645\u0646 \u0627\u0644\u062d\u062f\u064a\u062f 99% \u0648\u0627\u0644\u0643\u0631\u0628\u0648\u0646 1%. \u064a\u062a\u0645 \u0625\u0646\u062a\u0627\u062c \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0639\u0627\u062f\u0629\u064b \u0645\u0646 \u062e\u0644\u0627\u0644 \u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0633\u0627\u062e\u0646\u0629\u060c \u0648\u064a\u062d\u0633\u0646 \u0633\u0637\u062d\u0647 \u0627\u0644\u0645\u0636\u0644\u0639 \u0645\u0646 \u0627\u0644\u0627\u0644\u062a\u0635\u0627\u0642 \u0628\u0627\u0644\u062e\u0631\u0633\u0627\u0646\u0629. \u062a\u0642\u0644\u0644 \u0642\u0648\u062a\u0647 \u0627\u0644\u0634\u062f \u0648\u0645\u062a\u0627\u0646\u062a\u0647 \u0648\u062e\u0635\u0627\u0626\u0635 \u0627\u0644\u062a\u0645\u062f\u062f \u0627\u0644\u062d\u0631\u0627\u0631\u064a \u0645\u0646 \u0645\u0634\u0643\u0644\u0627\u062a \u062a\u063a\u064a\u0631 \u062f\u0631\u062c\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629\u060c \u0645\u0645\u0627 \u064a\u0639\u0632\u0632 \u0642\u0648\u0629 \u0647\u064a\u0643\u0644 \u0627\u0644\u062e\u0631\u0633\u0627\u0646\u0629. \u064a\u0623\u062a\u064a \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0628\u0623\u0646\u0648\u0627\u0639 \u0648\u0623\u062d\u062c\u0627\u0645 \u0645\u062e\u062a\u0644\u0641\u0629\u060c \u0648\u064a\u0645\u0643\u0646 \u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0647 \u0641\u064a \u0647\u064a\u0627\u0643\u0644 \u0627\u0644\u0645\u0628\u0627\u0646\u064a \u0627\u0644\u0645\u062e\u062a\u0644\u0641\u0629.<\/p><h2 class=\"wp-block-heading\">\u062a\u0627\u0631\u064a\u062e \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d<\/h2><ul class=\"wp-block-list\"><li><strong>\u062e\u0645\u0633\u064a\u0646\u064a\u0627\u062a \u0627\u0644\u0642\u0631\u0646 \u0627\u0644\u062a\u0627\u0633\u0639 \u0639\u0634\u0631<\/strong>:\u0627\u062e\u062a\u0631\u0639 \u0627\u0644\u0628\u0633\u062a\u0627\u0646\u064a \u0627\u0644\u0641\u0631\u0646\u0633\u064a \u062c\u0648\u0632\u064a\u0641 \u0645\u0648\u0646\u064a\u064a\u0647 \u0627\u0644\u062e\u0631\u0633\u0627\u0646\u0629 \u0627\u0644\u0645\u0633\u0644\u062d\u0629\u060c \u0648\u0630\u0644\u0643 \u0628\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0644\u062a\u0642\u0648\u064a\u0629 \u0623\u0648\u0627\u0646\u064a \u0627\u0644\u0632\u0647\u0648\u0631 \u0627\u0644\u062e\u0631\u0633\u0627\u0646\u064a\u0629.<\/li>\n\n<li><strong>\u0623\u0648\u0627\u0626\u0644 \u0627\u0644\u0642\u0631\u0646 \u0627\u0644\u0639\u0634\u0631\u064a\u0646<\/strong>:\u062a\u0645 \u0627\u062e\u062a\u0631\u0627\u0639 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0645\u0644\u062a\u0648\u064a\u0629 \u0628\u0648\u0627\u0633\u0637\u0629 \u0625\u0631\u0646\u0633\u062a \u0625\u0644 \u0631\u0627\u0646\u0633\u0648\u0645\u060c \u0645\u0645\u0627 \u0623\u062f\u0649 \u0625\u0644\u0649 \u062a\u062d\u0633\u064a\u0646 \u0627\u0644\u0631\u0627\u0628\u0637\u0629 \u0628\u064a\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0648\u0627\u0644\u062e\u0631\u0633\u0627\u0646\u0629.<\/li>\n\n<li><strong>\u0645\u0646\u062a\u0635\u0641 \u0627\u0644\u0642\u0631\u0646 \u0627\u0644\u0639\u0634\u0631\u064a\u0646<\/strong>:\u062a\u062d\u0633\u064a\u0646 \u062c\u0648\u062f\u0629 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0648\u0637\u0631\u0642 \u0625\u0646\u062a\u0627\u062c\u0647 \u0623\u062f\u0649 \u0625\u0644\u0649 \u062a\u0648\u0633\u064a\u0639 \u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0641\u064a \u0645\u0634\u0627\u0631\u064a\u0639 \u0627\u0644\u0628\u0646\u064a\u0629 \u0627\u0644\u062a\u062d\u062a\u064a\u0629 \u0627\u0644\u0643\u0628\u0631\u0649.<\/li>\n\n<li><strong>\u0623\u0648\u0627\u062e\u0631 \u0627\u0644\u0642\u0631\u0646 \u0627\u0644\u0639\u0634\u0631\u064a\u0646<\/strong>:\u062a\u0645 \u062a\u0642\u062f\u064a\u0645 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0645\u0637\u0644\u064a\u0629 \u0628\u0627\u0644\u0625\u064a\u0628\u0648\u0643\u0633\u064a \u0648\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0644\u062a\u062d\u0633\u064a\u0646 \u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644.<\/li>\n\n<li><strong>\u0627\u0644\u0642\u0631\u0646 \u0627\u0644\u062d\u0627\u062f\u064a \u0648\u0627\u0644\u0639\u0634\u0631\u064a\u0646<\/strong>:\u0638\u0647\u0631\u062a \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0645\u0642\u0648\u0627\u0629 \u0628\u0627\u0644\u0628\u0648\u0644\u064a\u0645\u0631 (FRP) \u0643\u0628\u062f\u064a\u0644 \u062e\u0641\u064a\u0641 \u0627\u0644\u0648\u0632\u0646 \u0648\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u062a\u0622\u0643\u0644.<\/li><\/ul><h2 class=\"wp-block-heading\">\u0643\u064a\u0641 \u064a\u062a\u0645 \u062a\u0635\u0646\u064a\u0639 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d<\/h2><p class=\"wp-block-paragraph\">\u064a\u062a\u0645 \u062a\u0635\u0646\u064a\u0639 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0641\u064a \u0627\u0644\u0645\u0642\u0627\u0645 \u0627\u0644\u0623\u0648\u0644 \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0639\u0627\u062f \u062a\u062f\u0648\u064a\u0631\u0647\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647 \u0635\u062f\u064a\u0642\u064b\u0627 \u0644\u0644\u0628\u064a\u0626\u0629 \u0628\u062f\u0631\u062c\u0629 \u0643\u0628\u064a\u0631\u0629.&nbsp;<\/p><ol class=\"wp-block-list\"><li><strong>\u0627\u0644\u0630\u0648\u0628\u0627\u0646:<\/strong> \u062a\u0628\u062f\u0623 \u0627\u0644\u0639\u0645\u0644\u064a\u0629 \u0628\u0635\u0647\u0631 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u062e\u0631\u062f\u0629 \u0641\u064a \u0641\u0631\u0646 \u0627\u0644\u0642\u0648\u0633 \u0627\u0644\u0643\u0647\u0631\u0628\u0627\u0626\u064a\u060c \u0645\u0645\u0627 \u064a\u0624\u062f\u064a \u0625\u0644\u0649 \u062a\u062d\u0648\u064a\u0644 \u0627\u0644\u0645\u0639\u062f\u0646 \u0627\u0644\u0635\u0644\u0628 \u0625\u0644\u0649 \u0634\u0643\u0644 \u0633\u0627\u0626\u0644.<\/li>\n\n<li><strong>\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0646\u0635\u0647\u0631:<\/strong> \u064a\u062a\u0645 \u0628\u0639\u062f \u0630\u0644\u0643 \u062a\u062d\u0636\u064a\u0631 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0646\u0635\u0647\u0631 \u0644\u0644\u062a\u0637\u0647\u064a\u0631\u060c \u0645\u0639 \u0636\u0645\u0627\u0646 \u0625\u0632\u0627\u0644\u0629 \u0627\u0644\u0634\u0648\u0627\u0626\u0628 \u0644\u062a\u062d\u0633\u064a\u0646 \u0627\u0644\u062c\u0648\u062f\u0629.<\/li>\n\n<li><strong>\u0637\u0647\u0627\u0631\u0629:<\/strong> \u0628\u0645\u062c\u0631\u062f \u0630\u0648\u0628\u0627\u0646\u0647\u060c \u064a\u062a\u0645 \u062a\u0646\u0642\u064a\u0629 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u062b\u0645 \u0635\u0628\u0647 \u0641\u064a \u0634\u0643\u0644 \u0642\u0636\u0628\u0627\u0646\u060c \u0644\u062a\u0634\u0643\u064a\u0644 \u0627\u0644\u0634\u0643\u0644 \u0627\u0644\u0623\u0648\u0644\u064a \u0644\u0645\u0632\u064a\u062f \u0645\u0646 \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0629.<\/li>\n\n<li><strong>\u0627\u0644\u062a\u062f\u0641\u0626\u0629:<\/strong> \u064a\u062a\u0645 \u062a\u0633\u062e\u064a\u0646 \u0627\u0644\u0643\u062a\u0644 \u0625\u0644\u0649 \u062f\u0631\u062c\u0629 \u062d\u0631\u0627\u0631\u0629 \u0645\u0631\u062a\u0641\u0639\u0629 \u0644\u062a\u0644\u064a\u064a\u0646\u0647\u0627 \u0642\u0628\u0644 \u0639\u0645\u0644\u064a\u0629 \u0627\u0644\u062f\u0631\u0641\u0644\u0629\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647\u0627 \u0642\u0627\u0628\u0644\u0629 \u0644\u0644\u0637\u0631\u0642 \u0648\u0627\u0644\u062a\u0634\u0643\u064a\u0644.<\/li>\n\n<li><strong>\u0627\u0644\u062a\u062f\u062d\u0631\u062c:<\/strong> \u064a\u062a\u0645 \u062a\u0645\u0631\u064a\u0631 \u0627\u0644\u0643\u062a\u0644 \u0627\u0644\u0633\u0627\u062e\u0646\u0629 \u0639\u0628\u0631 \u0633\u0644\u0633\u0644\u0629 \u0645\u0646 \u0645\u0637\u0627\u062d\u0646 \u0627\u0644\u062f\u0631\u0641\u0644\u0629\u060c \u062b\u0645 \u064a\u062a\u0645 \u062f\u062d\u0631\u062c\u062a\u0647\u0627 \u062a\u062f\u0631\u064a\u062c\u064a\u064b\u0627 \u0625\u0644\u0649 \u0642\u0636\u0628\u0627\u0646 \u0645\u0633\u062a\u062f\u064a\u0631\u0629 \u0628\u0627\u0644\u0642\u0637\u0631 \u0627\u0644\u0645\u0637\u0644\u0648\u0628. \u062a\u0633\u0645\u0649 \u0647\u0630\u0647 \u0627\u0644\u0639\u0645\u0644\u064a\u0629 \u0627\u0644\u062f\u0631\u0641\u0644\u0629 \u0627\u0644\u0633\u0627\u062e\u0646\u0629.<\/li>\n\n<li><strong>\u0627\u0644\u062a\u0628\u0631\u064a\u062f \u0648\u0627\u0644\u0642\u0637\u0639:<\/strong> \u064a\u062a\u0645 \u062a\u0628\u0631\u064a\u062f \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0628\u0634\u0643\u0644 \u0637\u0628\u064a\u0639\u064a \u0639\u0644\u0649 \u0627\u0644\u0623\u0633\u0631\u0629 \u0623\u0648 \u0628\u0633\u0631\u0639\u0629 \u0628\u0627\u0644\u0645\u0627\u0621\u060c \u062b\u0645 \u064a\u062a\u0645 \u0642\u0637\u0639\u0647 \u0625\u0644\u0649 \u0627\u0644\u0637\u0648\u0644 \u0627\u0644\u0645\u0637\u0644\u0648\u0628\u060c \u0639\u0627\u062f\u0629 12 \u0645\u062a\u0631\u0627\u064b \u0623\u0648 \u0623\u0643\u062b\u0631.<\/li>\n\n<li><strong>\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0633\u0637\u062d:<\/strong> \u0623\u062b\u0646\u0627\u0621 \u0639\u0645\u0644\u064a\u0629 \u0627\u0644\u062f\u0631\u0641\u0644\u0629\u060c \u064a\u062a\u0645 \u0627\u0644\u0636\u063a\u0637 \u0639\u0644\u0649 \u0627\u0644\u0623\u0636\u0644\u0627\u0639 \u0623\u0648 \u0627\u0644\u062a\u0634\u0648\u0647\u0627\u062a \u0627\u0644\u0623\u062e\u0631\u0649 \u0639\u0644\u0649 \u0633\u0637\u062d \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0644\u062a\u0639\u0632\u064a\u0632 \u0627\u0631\u062a\u0628\u0627\u0637\u0647 \u0628\u0627\u0644\u062e\u0631\u0633\u0627\u0646\u0629.<\/li><\/ol><p class=\"wp-block-paragraph\">\u0639\u0644\u0649 \u0627\u0644\u0631\u063a\u0645 \u0645\u0646 \u062a\u0635\u0646\u064a\u0639\u0647\u0627 \u0645\u0646 \u0645\u0648\u0627\u062f \u0645\u0639\u0627\u062f \u062a\u062f\u0648\u064a\u0631\u0647\u0627\u060c \u0641\u0625\u0646 \u0623\u062f\u0627\u0621 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0644\u0627 \u064a\u062a\u0623\u062b\u0631\u060c \u0641\u0647\u064a \u062a\u062d\u062a\u0641\u0638 \u0628\u0642\u0648\u062a\u0647\u0627 \u0648\u0645\u062a\u0627\u0646\u062a\u0647\u0627 \u0648\u064a\u0645\u0643\u0646 \u0625\u0639\u0627\u062f\u0629 \u062a\u062f\u0648\u064a\u0631\u0647\u0627 \u0645\u0631\u0629 \u0623\u062e\u0631\u0649 \u0628\u0639\u062f \u0627\u0646\u062a\u0647\u0627\u0621 \u062f\u0648\u0631\u0629 \u062d\u064a\u0627\u062a\u0647\u0627 \u0641\u064a \u0627\u0644\u0628\u0646\u0627\u0621.<\/p><h2 class=\"wp-block-heading\">\u0623\u0646\u0648\u0627\u0639 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d<\/h2><p class=\"wp-block-paragraph\">\u062a\u0634\u062a\u0645\u0644 \u0623\u0646\u0648\u0627\u0639 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0639\u0644\u0649 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0643\u0631\u0628\u0648\u0646\u064a\u060c \u0648\u0627\u0644\u0645\u063a\u0644\u0641 \u0628\u0627\u0644\u0625\u064a\u0628\u0648\u0643\u0633\u064a\u060c \u0648GFRP\u060c \u0648\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623\u060c \u062d\u064a\u062b \u064a\u0648\u0641\u0631 GFRP \u0648\u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0623\u0641\u0636\u0644 \u0645\u0642\u0627\u0648\u0645\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0641\u064a \u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u0642\u0627\u0633\u064a\u0629.<\/p><h3 class=\"wp-block-heading\">\u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0643\u0631\u0628\u0648\u0646\u064a<\/h3><p class=\"wp-block-paragraph\">\u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0645\u0635\u0646\u0648\u0639\u0629 \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0643\u0631\u0628\u0648\u0646\u064a\u060c \u0648\u0627\u0644\u0645\u0639\u0631\u0648\u0641\u0629 \u0623\u064a\u0636\u064b\u0627 \u0628\u0627\u0633\u0645 \u0627\u0644\u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u0633\u0648\u062f\u0627\u0621\u060c \u0647\u064a \u0627\u0644\u0646\u0648\u0639 \u0627\u0644\u0633\u0627\u0626\u062f \u0645\u0646 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0645\u0633\u062a\u062e\u062f\u0645\u0629 \u0641\u064a \u0627\u0644\u0628\u0646\u0627\u0621. \u0648\u0647\u064a \u0645\u062a\u0639\u062f\u062f\u0629 \u0627\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0627\u062a \u0644\u0644\u063a\u0627\u064a\u0629\u060c \u0648\u0641\u0639\u0627\u0644\u0629 \u0645\u0646 \u062d\u064a\u062b \u0627\u0644\u062a\u0643\u0644\u0641\u0629\u060c \u0648\u062a\u0648\u0641\u0631 \u0642\u0648\u0629 \u0634\u062f \u0648\u0645\u062a\u0627\u0646\u0629 \u0645\u0645\u062a\u0627\u0632\u0629. \u0648\u0645\u0639 \u0630\u0644\u0643\u060c \u0641\u0647\u064a \u0639\u0631\u0636\u0629 \u0644\u0644\u0635\u062f\u0623 \u0639\u0646\u062f \u062a\u0639\u0631\u0636\u0647\u0627 \u0644\u0644\u0631\u0637\u0648\u0628\u0629 \u0648\u0627\u0644\u0645\u0648\u0627\u062f \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629.<\/p><h3 class=\"wp-block-heading\">\u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0645\u063a\u0637\u0649 \u0628\u0627\u0644\u0625\u064a\u0628\u0648\u0643\u0633\u064a<\/h3><p class=\"wp-block-paragraph\">\u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0645\u063a\u0637\u0649 \u0628\u0627\u0644\u0625\u064a\u0628\u0648\u0643\u0633\u064a \u0647\u0648 \u062d\u062f\u064a\u062f \u062a\u0633\u0644\u064a\u062d \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0643\u0631\u0628\u0648\u0646\u064a \u064a\u062a\u0645\u064a\u0632 \u0628\u0637\u0628\u0642\u0629 \u0625\u064a\u0628\u0648\u0643\u0633\u064a \u0644\u0645\u0646\u0639 \u0627\u0644\u062a\u0622\u0643\u0644. \u0647\u0630\u0627 \u0627\u0644\u0646\u0648\u0639 \u0645\u062b\u0627\u0644\u064a \u0644\u0644\u0628\u064a\u0626\u0627\u062a \u0630\u0627\u062a \u0645\u0633\u062a\u0648\u064a\u0627\u062a \u0627\u0644\u0631\u0637\u0648\u0628\u0629 \u0648\u0627\u0644\u0643\u0644\u0648\u0631\u064a\u062f \u0627\u0644\u0639\u0627\u0644\u064a\u0629\u060c \u0645\u062b\u0644 \u0627\u0644\u0647\u064a\u0627\u0643\u0644 \u0627\u0644\u0628\u062d\u0631\u064a\u0629 \u0648\u0627\u0644\u062c\u0633\u0648\u0631. \u064a\u0639\u0645\u0644 \u0627\u0644\u0637\u0644\u0627\u0621 \u0639\u0644\u0649 \u0625\u0637\u0627\u0644\u0629 \u0639\u0645\u0631 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0628\u0634\u0643\u0644 \u0643\u0628\u064a\u0631\u060c \u0648\u0644\u0643\u0646 \u064a\u0644\u0632\u0645 \u062a\u0648\u062e\u064a \u0639\u0646\u0627\u064a\u0629 \u0625\u0636\u0627\u0641\u064a\u0629 \u0623\u062b\u0646\u0627\u0621 \u0627\u0644\u0646\u0642\u0644 \u0644\u062a\u062c\u0646\u0628 \u0627\u0644\u062a\u0644\u0641.<\/p><h3 class=\"wp-block-heading\">\u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623<\/h3><p class=\"wp-block-paragraph\">\u062a\u062a\u0645\u062a\u0639 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0645\u0635\u0646\u0648\u0639\u0629 \u0645\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0628\u0645\u0642\u0627\u0648\u0645\u0629 \u0639\u0627\u0644\u064a\u0629 \u0644\u0644\u0635\u062f\u0623\u060c \u0648\u062a\u064f\u0633\u062a\u062e\u062f\u0645 \u0628\u0634\u0643\u0644 \u0645\u062a\u0643\u0631\u0631 \u0641\u064a \u0627\u0644\u0647\u064a\u0627\u0643\u0644 \u0627\u0644\u0645\u0639\u0631\u0636\u0629 \u0644\u0638\u0631\u0648\u0641 \u0628\u064a\u0626\u064a\u0629 \u0635\u0639\u0628\u0629\u060c \u0645\u062b\u0644 \u0627\u0644\u0645\u0646\u0627\u0637\u0642 \u0627\u0644\u0633\u0627\u062d\u0644\u064a\u0629 \u0648\u0627\u0644\u0645\u0635\u0627\u0646\u0639 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629. \u0648\u0631\u063a\u0645 \u0623\u0646\u0647\u0627 \u0623\u0643\u062b\u0631 \u062a\u0643\u0644\u0641\u0629 \u0645\u0646 \u0627\u0644\u0623\u0646\u0648\u0627\u0639 \u0627\u0644\u0623\u062e\u0631\u0649\u060c \u0641\u0625\u0646 \u0645\u062a\u0627\u0646\u062a\u0647\u0627 \u0648\u0623\u062f\u0627\u0626\u0647\u0627 \u0639\u0644\u0649 \u0627\u0644\u0645\u062f\u0649 \u0627\u0644\u0637\u0648\u064a\u0644 \u064a\u0645\u0643\u0646 \u0623\u0646 \u064a\u0628\u0631\u0631 \u0627\u0644\u062a\u0643\u0644\u0641\u0629 \u0641\u064a \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u062d\u0631\u062c\u0629.<\/p><h3 class=\"wp-block-heading\">\u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0645\u062c\u0644\u0641\u0646<\/h3><p class=\"wp-block-paragraph\">\u064a\u062a\u0643\u0648\u0646 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0645\u062c\u0644\u0641\u0646 \u0645\u0646 \u062d\u062f\u064a\u062f \u0641\u0648\u0644\u0627\u0630 \u0643\u0631\u0628\u0648\u0646\u064a \u0645\u0637\u0644\u064a \u0628\u0627\u0644\u0632\u0646\u0643 \u0644\u062d\u0645\u0627\u064a\u062a\u0647 \u0645\u0646 \u0627\u0644\u062a\u0622\u0643\u0644. \u064a\u0648\u0641\u0631 \u0647\u0630\u0627 \u0627\u0644\u0646\u0648\u0639 \u0645\u0642\u0627\u0648\u0645\u0629 \u0641\u0627\u0626\u0642\u0629 \u0644\u0644\u0635\u062f\u0623 \u0645\u0642\u0627\u0631\u0646\u0629 \u0628\u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0645\u0637\u0644\u064a \u0628\u0627\u0644\u0625\u064a\u0628\u0648\u0643\u0633\u064a \u0648\u064a\u0633\u062a\u062e\u062f\u0645 \u0628\u0634\u0643\u0644 \u0645\u062a\u0643\u0631\u0631 \u0641\u064a \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u062a\u064a \u062a\u062a\u0637\u0644\u0628 \u0645\u062a\u0627\u0646\u0629 \u0645\u0645\u062a\u062f\u0629\u060c \u0645\u062b\u0644 \u0628\u0646\u0627\u0621 \u0627\u0644\u0637\u0631\u0642 \u0627\u0644\u0633\u0631\u064a\u0639\u0629 \u0648\u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u0628\u062d\u0631\u064a\u0629.<\/p><h3 class=\"wp-block-heading\">\u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0645\u0642\u0648\u0649 \u0628\u0627\u0644\u0628\u0648\u0644\u064a\u0645\u0631\u0627\u062a \u0627\u0644\u0645\u0635\u0646\u0648\u0639\u0629 \u0645\u0646 \u0627\u0644\u0623\u0644\u064a\u0627\u0641 \u0627\u0644\u0632\u062c\u0627\u062c\u064a\u0629 (GFRP)<\/h3><p class=\"wp-block-paragraph\">\u064a\u062a\u0645 \u062a\u0635\u0646\u064a\u0639 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0645\u0635\u0646\u0648\u0639\u0629 \u0645\u0646 \u0627\u0644\u0628\u0644\u0627\u0633\u062a\u064a\u0643 \u0627\u0644\u0645\u0642\u0648\u0649 \u0628\u0623\u0644\u064a\u0627\u0641 \u0632\u062c\u0627\u062c\u064a\u0629 \u0639\u0627\u0644\u064a\u0629 \u0627\u0644\u0642\u0648\u0629 \u0645\u062d\u0627\u0637\u0629 \u0628\u0645\u0635\u0641\u0648\u0641\u0629 \u0628\u0648\u0644\u064a\u0645\u0631\u064a\u0629. \u0648\u0647\u064a \u062e\u0641\u064a\u0641\u0629 \u0627\u0644\u0648\u0632\u0646 \u0648\u063a\u064a\u0631 \u0642\u0627\u0628\u0644\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0648\u063a\u064a\u0631 \u0645\u0648\u0635\u0644\u0629 \u0644\u0644\u0643\u0647\u0631\u0628\u0627\u0621\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647\u0627 \u0645\u0646\u0627\u0633\u0628\u0629 \u0644\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0641\u064a \u0627\u0644\u0647\u064a\u0627\u0643\u0644 \u0627\u0644\u0645\u0639\u0631\u0636\u0629 \u0644\u0644\u062d\u0642\u0648\u0644 \u0627\u0644\u0643\u0647\u0631\u0648\u0645\u063a\u0646\u0627\u0637\u064a\u0633\u064a\u0629\u060c \u0645\u062b\u0644 \u063a\u0631\u0641 \u0627\u0644\u062a\u0635\u0648\u064a\u0631 \u0628\u0627\u0644\u0631\u0646\u064a\u0646 \u0627\u0644\u0645\u063a\u0646\u0627\u0637\u064a\u0633\u064a \u0648\u0645\u062d\u0637\u0627\u062a \u0627\u0644\u0643\u0647\u0631\u0628\u0627\u0621 \u0627\u0644\u0641\u0631\u0639\u064a\u0629. \u0643\u0645\u0627 \u062a\u0633\u0647\u0644 \u0646\u0633\u0628\u0629 \u0627\u0644\u0642\u0648\u0629 \u0625\u0644\u0649 \u0627\u0644\u0648\u0632\u0646 \u0627\u0644\u0645\u0645\u062a\u0627\u0632\u0629 \u0627\u0644\u062a\u0639\u0627\u0645\u0644 \u0645\u0639\u0647\u0627 \u0648\u062a\u0631\u0643\u064a\u0628\u0647\u0627.<\/p><h3 class=\"wp-block-heading\">\u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0645\u0635\u0646\u0648\u0639 \u0645\u0646 \u0623\u0633\u0644\u0627\u0643 \u0645\u0644\u062d\u0648\u0645\u0629 (WWF)<\/h3><p class=\"wp-block-paragraph\">\u062a\u062a\u0643\u0648\u0646 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0645\u0635\u0646\u0648\u0639\u0629 \u0645\u0646 \u0627\u0644\u0623\u0633\u0644\u0627\u0643 \u0627\u0644\u0645\u0644\u062d\u0648\u0645\u0629\u060c \u0648\u0627\u0644\u062a\u064a \u064a\u0634\u0627\u0631 \u0625\u0644\u064a\u0647\u0627 \u0623\u064a\u0636\u064b\u0627 \u0628\u0627\u0633\u0645 \u0634\u0628\u0643\u0629 \u0627\u0644\u0623\u0633\u0644\u0627\u0643 \u0627\u0644\u0645\u0644\u062d\u0648\u0645\u0629\u060c \u0645\u0646 \u0634\u0628\u0643\u0629 \u0645\u0646 \u0627\u0644\u0623\u0633\u0644\u0627\u0643 \u0627\u0644\u0641\u0648\u0644\u0627\u0630\u064a\u0629 \u0627\u0644\u0645\u0646\u062f\u0645\u062c\u0629 \u0645\u0639\u064b\u0627 \u0639\u0646\u062f \u0627\u0644\u062a\u0642\u0627\u0637\u0639\u0627\u062a. \u062a\u064f\u0633\u062a\u062e\u062f\u0645 \u0639\u0627\u062f\u0629\u064b \u0644\u062a\u0642\u0648\u064a\u0629 \u0623\u0644\u0648\u0627\u062d \u0627\u0644\u062e\u0631\u0633\u0627\u0646\u0629 \u0648\u0627\u0644\u062c\u062f\u0631\u0627\u0646 \u0648\u0627\u0644\u0623\u0631\u0635\u0641\u0629. \u062a\u0648\u0641\u0631 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d WWF \u0642\u0648\u0629 \u0645\u0648\u062d\u062f\u0629 \u0648\u0633\u0647\u0648\u0644\u0629 \u0627\u0644\u062a\u0631\u0643\u064a\u0628\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647\u0627 \u062e\u064a\u0627\u0631\u064b\u0627 \u0634\u0627\u0626\u0639\u064b\u0627 \u0644\u0645\u062c\u0645\u0648\u0639\u0629 \u0648\u0627\u0633\u0639\u0629 \u0645\u0646 \u0645\u0634\u0627\u0631\u064a\u0639 \u0627\u0644\u0628\u0646\u0627\u0621.<\/p><h3 class=\"wp-block-heading\">\u0642\u0636\u0628\u0627\u0646 \u0645\u0634\u0648\u0647\u0629 \u0639\u0627\u0644\u064a\u0629 \u0627\u0644\u0642\u0648\u0629<\/h3><p class=\"wp-block-paragraph\">\u062a\u062a\u0645\u064a\u0632 \u0642\u0636\u0628\u0627\u0646 HSD \u0627\u0644\u0645\u0634\u0648\u0647\u0629 \u0639\u0627\u0644\u064a\u0629 \u0627\u0644\u0642\u0648\u0629 \u0628\u0648\u062c\u0648\u062f \u062a\u062c\u0627\u0648\u064a\u0641 \u0639\u0644\u0649 \u0627\u0644\u0633\u0637\u062d \u0644\u062a\u0639\u0632\u064a\u0632 \u0627\u0644\u062a\u0635\u0627\u0642 \u0627\u0644\u062e\u0631\u0633\u0627\u0646\u0629. \u0648\u0647\u064a \u062a\u0648\u0641\u0631 \u0642\u0648\u0629 \u0634\u062f \u0648\u0645\u062a\u0627\u0646\u0629 \u0641\u0627\u0626\u0642\u0629\u060c \u0648\u0647\u064a \u0645\u062b\u0627\u0644\u064a\u0629 \u0644\u0644\u0625\u0646\u0634\u0627\u0621\u0627\u062a \u0627\u0644\u062b\u0642\u064a\u0644\u0629 \u0645\u062b\u0644 \u0627\u0644\u0645\u0628\u0627\u0646\u064a \u0627\u0644\u0634\u0627\u0647\u0642\u0629 \u0648\u0627\u0644\u062c\u0633\u0648\u0631. \u0648\u062a\u0636\u0645\u0646 \u0627\u0644\u062a\u0634\u0648\u0647\u0627\u062a \u0642\u0628\u0636\u0629 \u0623\u0642\u0648\u0649 \u0645\u0639 \u0627\u0644\u062e\u0631\u0633\u0627\u0646\u0629\u060c \u0645\u0645\u0627 \u064a\u0639\u0632\u0632 \u0633\u0644\u0627\u0645\u0629 \u0627\u0644\u0628\u0646\u064a\u0629.<\/p><h3 class=\"wp-block-heading\">\u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0628\u0627\u0632\u0644\u062a\u064a<\/h3><p class=\"wp-block-paragraph\">\u062a\u062a\u0645\u064a\u0632 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0628\u0627\u0632\u0644\u062a\u064a\u0629 \u0627\u0644\u0645\u0635\u0646\u0648\u0639\u0629 \u0645\u0646 \u0623\u0644\u064a\u0627\u0641 \u0627\u0644\u0635\u062e\u0648\u0631 \u0627\u0644\u0628\u0627\u0632\u0644\u062a\u064a\u0629 \u0628\u0642\u0648\u0629 \u0634\u062f \u0639\u0627\u0644\u064a\u0629 \u0648\u0645\u0642\u0627\u0648\u0645\u0629 \u0645\u0645\u062a\u0627\u0632\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u0648\u0627\u0644\u0642\u0644\u0648\u064a\u0627\u062a. \u0648\u0647\u064a \u0623\u062e\u0641 \u0648\u0632\u0646\u064b\u0627 \u0645\u0646 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0641\u0648\u0644\u0627\u0630\u064a\u0629\u060c \u0645\u0645\u0627 \u064a\u0633\u0647\u0644 \u0646\u0642\u0644\u0647\u0627 \u0648\u0645\u0646\u0627\u0648\u0644\u062a\u0647\u0627. \u0648\u0628\u0627\u0639\u062a\u0628\u0627\u0631\u0647\u0627 \u0645\u0627\u062f\u0629 \u062c\u062f\u064a\u062f\u0629\u060c \u0641\u0647\u064a \u0645\u062b\u0627\u0644\u064a\u0629 \u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u062e\u0631\u0633\u0627\u0646\u0629 \u0641\u064a \u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u0642\u0627\u0633\u064a\u0629. \u0648\u0645\u0646 \u0627\u0644\u0645\u062a\u0648\u0642\u0639 \u0623\u0646 \u064a\u0624\u062f\u064a \u0627\u0644\u0637\u0644\u0628 \u0627\u0644\u0645\u062a\u0632\u0627\u064a\u062f \u0639\u0644\u0649 \u0645\u0648\u0627\u062f \u0627\u0644\u0628\u0646\u0627\u0621 \u0645\u0646\u062e\u0641\u0636\u0629 \u0627\u0644\u0635\u064a\u0627\u0646\u0629 \u0625\u0644\u0649 \u0632\u064a\u0627\u062f\u0629 \u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0647\u0627.<\/p><h2 class=\"wp-block-heading\">\u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0623\u0633\u0627\u0633\u064a \u0648\u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u062b\u0627\u0646\u0648\u064a \u0641\u064a \u0627\u0644\u062a\u0635\u0645\u064a\u0645 \u0627\u0644\u0625\u0646\u0634\u0627\u0626\u064a<\/h2><p class=\"wp-block-paragraph\">\u062a\u0646\u0642\u0633\u0645 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0625\u0644\u0649 \u0646\u0648\u0639\u064a\u0646 \u0623\u0633\u0627\u0633\u064a \u0648\u062b\u0627\u0646\u0648\u064a. \u064a\u0648\u0641\u0631 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0623\u0633\u0627\u0633\u064a \u0627\u0644\u062f\u0639\u0645 \u0627\u0644\u0647\u064a\u0643\u0644\u064a \u0627\u0644\u0631\u0626\u064a\u0633\u064a\u060c \u0628\u064a\u0646\u0645\u0627 \u064a\u0639\u0632\u0632 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u062b\u0627\u0646\u0648\u064a \u0627\u0644\u0645\u062a\u0627\u0646\u0629 \u0645\u0646 \u062e\u0644\u0627\u0644 \u0645\u0646\u0639 \u0627\u0644\u062a\u0634\u0642\u0642\u0627\u062a \u0648\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u0636\u063a\u0648\u0637 \u0627\u0644\u0645\u0631\u062a\u0628\u0637\u0629 \u0628\u062f\u0631\u062c\u0627\u062a \u0627\u0644\u062d\u0631\u0627\u0631\u0629.<\/p><p class=\"wp-block-paragraph\"><strong>\u0627\u0644\u062a\u0639\u0632\u064a\u0632 \u0627\u0644\u0623\u0633\u0627\u0633\u064a<\/strong>:\u064a\u0636\u0645\u0646 \u0647\u0630\u0627 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0623\u0646 \u0627\u0644\u0647\u064a\u0643\u0644 \u0642\u0627\u062f\u0631 \u0639\u0644\u0649 \u062f\u0639\u0645 \u0627\u0644\u062d\u0645\u0644 \u0627\u0644\u0645\u0635\u0645\u0645\u060c \u0645\u0645\u0627 \u064a\u0648\u0641\u0631 \u0627\u0644\u0642\u0648\u0629 \u0627\u0644\u0623\u0633\u0627\u0633\u064a\u0629 \u0641\u064a \u0627\u0644\u0645\u0646\u0627\u0637\u0642 \u0627\u0644\u0631\u0626\u064a\u0633\u064a\u0629 \u0645\u062b\u0644 \u0627\u0644\u0639\u0648\u0627\u0631\u0636 \u0648\u0627\u0644\u0623\u0639\u0645\u062f\u0629.<\/p><p class=\"wp-block-paragraph\"><strong>\u0627\u0644\u062a\u0639\u0632\u064a\u0632 \u0627\u0644\u062b\u0627\u0646\u0648\u064a<\/strong>:\u062a\u0648\u0632\u064a\u0639 \u0623\u0648 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u062d\u0631\u0627\u0631\u064a \u064a\u062d\u062f \u0645\u0646 \u0627\u0644\u062a\u0634\u0642\u0642\u0627\u062a \u0627\u0644\u0646\u0627\u062a\u062c\u0629 \u0639\u0646 \u0627\u0644\u0627\u0646\u0643\u0645\u0627\u0634 \u0648\u062a\u063a\u064a\u0631\u0627\u062a \u062f\u0631\u062c\u0629 \u0627\u0644\u062d\u0631\u0627\u0631\u0629\u060c \u0645\u0645\u0627 \u064a\u062d\u0633\u0646 \u0627\u0644\u0645\u062a\u0627\u0646\u0629 \u0648\u0627\u0644\u0645\u0638\u0647\u0631.<\/p><p class=\"wp-block-paragraph\"><strong>\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0625\u0636\u0627\u0641\u064a\u0629<\/strong>:\u0641\u064a \u0627\u0644\u0628\u0646\u0627\u0621\u060c \u064a\u062a\u0645 \u0648\u0636\u0639 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0641\u064a \u0648\u0635\u0644\u0627\u062a \u0627\u0644\u0645\u0644\u0627\u0637 \u0623\u0648 \u0627\u0644\u0643\u062a\u0644 \u0627\u0644\u0645\u062c\u0648\u0641\u0629 \u0644\u062a\u0642\u0648\u064a\u0629 \u0627\u0644\u0647\u064a\u0643\u0644\u060c \u0639\u0644\u0649 \u063a\u0631\u0627\u0631 \u0627\u0644\u062e\u0631\u0633\u0627\u0646\u0629 \u0627\u0644\u0645\u0633\u0644\u062d\u0629.<\/p><p class=\"wp-block-paragraph\"><strong>\u0627\u0644\u062a\u0639\u0632\u064a\u0632 \u0627\u0644\u0632\u0644\u0632\u0627\u0644\u064a<\/strong>:\u064a\u062a\u0645 \u0625\u0636\u0627\u0641\u0629 \u062a\u0635\u0645\u064a\u0645\u0627\u062a \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u062f\u0627\u0626\u0631\u064a\u0629 \u0641\u064a \u0627\u0644\u0647\u064a\u0627\u0643\u0644 \u0627\u0644\u062d\u062f\u064a\u062b\u0629 \u0644\u0645\u0646\u0639 \u0627\u0644\u0641\u0634\u0644 \u0623\u062b\u0646\u0627\u0621 \u0627\u0644\u0632\u0644\u0627\u0632\u0644\u060c \u0645\u0645\u0627 \u064a\u0639\u0632\u0632 \u0627\u0644\u0633\u0644\u0627\u0645\u0629 \u0627\u0644\u0647\u064a\u0643\u0644\u064a\u0629.<\/p><h2 class=\"wp-block-heading\">\u062d\u062c\u0645 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d<\/h2><p class=\"wp-block-paragraph\">\u064a\u0639\u062f \u0627\u062e\u062a\u064a\u0627\u0631 \u0627\u0644\u062d\u062c\u0645 \u0627\u0644\u0645\u0646\u0627\u0633\u0628 \u0644\u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0623\u0645\u0631\u064b\u0627 \u0636\u0631\u0648\u0631\u064a\u064b\u0627 \u0644\u0642\u0648\u0629 \u0647\u064a\u0643\u0644 \u0627\u0644\u0645\u0628\u0646\u0649. \u064a\u0645\u0643\u0646 \u0644\u0639\u0648\u0627\u0645\u0644 \u0645\u062b\u0644 \u0642\u062f\u0631\u0629 \u062a\u062d\u0645\u0644 \u0627\u0644\u0623\u062d\u0645\u0627\u0644 \u0623\u0646 \u062a\u0624\u062b\u0631 \u0639\u0644\u0649 \u0627\u0644\u0627\u062e\u062a\u064a\u0627\u0631 \u0627\u0644\u0641\u0639\u0627\u0644 \u0644\u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0648\u0648\u0636\u0639\u0647:<\/p><h3 class=\"wp-block-heading\">\u0627\u0644\u0639\u0648\u0627\u0645\u0644 \u0627\u0644\u062a\u064a \u062a\u062d\u062f\u062f \u0627\u062e\u062a\u064a\u0627\u0631 \u062d\u062c\u0645 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d<\/h3><p class=\"wp-block-paragraph\">\u064a\u062a\u0645 \u062a\u062d\u062f\u064a\u062f \u062d\u062c\u0645 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0645\u0646 \u062e\u0644\u0627\u0644 \u0642\u062f\u0631\u0629 \u0627\u0644\u0647\u064a\u0643\u0644 \u0639\u0644\u0649 \u062a\u062d\u0645\u0644 \u0627\u0644\u0623\u062d\u0645\u0627\u0644 \u0648\u0645\u0648\u0627\u0635\u0641\u0627\u062a \u0627\u0644\u062a\u0635\u0645\u064a\u0645. \u0643\u0645\u0627 \u064a\u0624\u062b\u0631 \u0633\u0645\u0643 \u0627\u0644\u063a\u0637\u0627\u0621 \u0627\u0644\u062e\u0631\u0633\u0627\u0646\u064a \u0648\u062a\u0628\u0627\u0639\u062f \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0623\u064a\u0636\u064b\u0627 \u0639\u0644\u0649 \u0627\u062e\u062a\u064a\u0627\u0631 \u0627\u0644\u062d\u062c\u0645.<\/p><h4 class=\"wp-block-heading\">\u0645\u062a\u0637\u0644\u0628\u0627\u062a \u0627\u0644\u0642\u0648\u0629<\/h4><p class=\"wp-block-paragraph\">\u064a\u0631\u062a\u0628\u0637 \u062d\u062c\u0645 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0628\u0634\u0643\u0644 \u0645\u0628\u0627\u0634\u0631 \u0628\u0642\u062f\u0631\u0629 \u062a\u062d\u0645\u0644 \u0627\u0644\u0623\u062d\u0645\u0627\u0644 \u0627\u0644\u0645\u0637\u0644\u0648\u0628\u0629 \u0644\u0644\u0647\u064a\u0643\u0644. \u063a\u0627\u0644\u0628\u064b\u0627 \u0645\u0627 \u062a\u064f\u0633\u062a\u062e\u062f\u0645 \u0623\u0642\u0637\u0627\u0631 \u0623\u0643\u0628\u0631\u060c \u0645\u062b\u0644 32 \u0645\u0645 \u0623\u0648 40 \u0645\u0645 \u0623\u0648 50 \u0645\u0645\u060c \u0644\u062a\u062d\u0645\u0644 \u0627\u0644\u0623\u062d\u0645\u0627\u0644 \u0627\u0644\u062b\u0642\u064a\u0644\u0629.<\/p><h4 class=\"wp-block-heading\">\u0627\u0644\u062a\u0635\u0645\u064a\u0645 \u0627\u0644\u0647\u064a\u0643\u0644\u064a<\/h4><p class=\"wp-block-paragraph\">\u062a\u062a\u0637\u0644\u0628 \u0627\u0644\u0645\u0643\u0648\u0646\u0627\u062a \u0627\u0644\u0625\u0646\u0634\u0627\u0626\u064a\u0629 \u0627\u0644\u0645\u062e\u062a\u0644\u0641\u0629 \u0645\u062a\u0637\u0644\u0628\u0627\u062a \u0645\u062e\u062a\u0644\u0641\u0629 \u0641\u064a\u0645\u0627 \u064a\u062a\u0639\u0644\u0642 \u0628\u0623\u062d\u062c\u0627\u0645 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d. \u0639\u0644\u0649 \u0633\u0628\u064a\u0644 \u0627\u0644\u0645\u062b\u0627\u0644\u060c \u0642\u062f \u062a\u062a\u0637\u0644\u0628 \u0627\u0644\u0623\u0633\u0627\u0633\u0627\u062a \u0648\u0627\u0644\u0623\u0639\u0645\u062f\u0629\u060c \u0627\u0644\u062a\u064a \u062a\u062a\u062d\u0645\u0644 \u0623\u062d\u0645\u0627\u0644\u0627\u064b \u0643\u0628\u064a\u0631\u0629\u060c \u0623\u0642\u0637\u0627\u0631\u064b\u0627 \u0623\u0643\u0628\u0631. \u0648\u0639\u0644\u0649 \u0627\u0644\u0646\u0642\u064a\u0636 \u0645\u0646 \u0630\u0644\u0643\u060c \u0642\u062f \u062a\u0633\u062a\u062e\u062f\u0645 \u0627\u0644\u062c\u062f\u0631\u0627\u0646 \u0623\u0648 \u0623\u0644\u0648\u0627\u062d \u0627\u0644\u0623\u0631\u0636\u064a\u0627\u062a \u063a\u064a\u0631 \u0627\u0644\u062d\u0627\u0645\u0644\u0629 \u0642\u0636\u0628\u0627\u0646 \u062a\u0633\u0644\u064a\u062d \u0630\u0627\u062a \u0623\u0642\u0637\u0627\u0631 \u0623\u0635\u063a\u0631.<\/p><h4 class=\"wp-block-heading\">\u063a\u0637\u0627\u0621 \u062e\u0631\u0633\u0627\u0646\u064a<\/h4><p class=\"wp-block-paragraph\">\u064a\u0624\u062b\u0631 \u0642\u0637\u0631 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0639\u0644\u0649 \u0633\u0645\u0643 \u0627\u0644\u063a\u0637\u0627\u0621 \u0627\u0644\u062e\u0631\u0633\u0627\u0646\u064a \u0627\u0644\u0645\u0637\u0644\u0648\u0628 \u0644\u0645\u0646\u0639 \u0627\u0644\u062a\u0622\u0643\u0644. \u064a\u0639\u062f \u0636\u0645\u0627\u0646 \u0639\u0645\u0642 \u0627\u0644\u063a\u0637\u0627\u0621 \u0627\u0644\u0645\u0646\u0627\u0633\u0628 \u0623\u0645\u0631\u064b\u0627 \u0636\u0631\u0648\u0631\u064a\u064b\u0627 \u0644\u0644\u062d\u0641\u0627\u0638 \u0639\u0644\u0649 \u0645\u062a\u0627\u0646\u0629 \u0627\u0644\u0647\u064a\u0643\u0644.<\/p><h4 class=\"wp-block-heading\">\u0627\u0644\u062a\u0628\u0627\u0639\u062f \u0648\u0627\u0644\u0648\u0636\u0639<\/h4><p class=\"wp-block-paragraph\">\u062a\u0624\u062b\u0631 \u0645\u0633\u0627\u0641\u0627\u062a \u0648\u062a\u0631\u062a\u064a\u0628 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0639\u0644\u0649 \u0642\u0631\u0627\u0631\u0627\u062a \u062a\u062d\u062f\u064a\u062f \u0627\u0644\u062d\u062c\u0645. \u063a\u0627\u0644\u0628\u064b\u0627 \u0645\u0627 \u062a\u062a\u0637\u0644\u0628 \u0627\u0644\u0645\u0633\u0627\u0641\u0627\u062a \u0627\u0644\u0636\u064a\u0642\u0629 \u0648\u0627\u0644\u062a\u062e\u0637\u064a\u0637\u0627\u062a \u0627\u0644\u0645\u0639\u0642\u062f\u0629 \u0623\u0642\u0637\u0627\u0631 \u0642\u0636\u0628\u0627\u0646 \u062a\u0633\u0644\u064a\u062d \u0623\u0635\u063a\u0631 \u0644\u062a\u0646\u0627\u0633\u0628 \u0627\u0644\u0645\u0633\u0627\u062d\u0627\u062a \u0627\u0644\u0645\u062e\u0635\u0635\u0629 \u062f\u0648\u0646 \u0627\u0644\u0645\u0633\u0627\u0633 \u0628\u0641\u0639\u0627\u0644\u064a\u0629 \u0627\u0644\u062a\u0639\u0632\u064a\u0632.<\/p><h3 class=\"wp-block-heading\">\u0643\u064a\u0641\u064a\u0629 \u0642\u064a\u0627\u0633 \u062d\u062c\u0645 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d<\/h3><p class=\"wp-block-paragraph\">\u0644\u0642\u064a\u0627\u0633 \u062d\u062c\u0645 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d\u060c \u0648\u0639\u0627\u062f\u0629 \u0645\u0627 \u064a\u062a\u0645 \u0642\u064a\u0627\u0633 \u0627\u0644\u0642\u0637\u0631\u060c \u0647\u0646\u0627\u0643 \u0639\u062f\u0629 \u0637\u0631\u0642 \u064a\u0645\u0643\u0646 \u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0647\u0627:<\/p><ul class=\"wp-block-list\"><li><strong>\u0637\u0631\u064a\u0642\u0629 \u0627\u0644\u0641\u0631\u062c\u0627\u0631:<\/strong> \u0627\u0633\u062a\u062e\u062f\u0645 \u0627\u0644\u0641\u0631\u062c\u0627\u0631 \u0644\u0642\u064a\u0627\u0633 \u0642\u0637\u0631 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0645\u0628\u0627\u0634\u0631\u0629. \u062a\u0623\u0643\u062f \u0645\u0646 \u0645\u0639\u0627\u064a\u0631\u0629 \u0627\u0644\u0641\u0631\u062c\u0627\u0631 \u0648\u0642\u0645 \u0628\u062a\u0637\u0628\u064a\u0642\u0647 \u0628\u0634\u0643\u0644 \u0639\u0645\u0648\u062f\u064a \u0639\u0644\u0649 \u0645\u062d\u0648\u0631 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0644\u0644\u062d\u0635\u0648\u0644 \u0639\u0644\u0649 \u0642\u064a\u0627\u0633 \u062f\u0642\u064a\u0642.<\/li>\n\n<li><strong>\u0637\u0631\u064a\u0642\u0629 \u0627\u0644\u0648\u0632\u0646:<\/strong> \u0642\u0645 \u0628\u0642\u064a\u0627\u0633 \u0648\u0632\u0646 \u0637\u0648\u0644 \u0645\u0639\u0631\u0648\u0641 \u0645\u0646 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0648\u0627\u0633\u062a\u062e\u062f\u0645 \u0635\u064a\u063a\u0629 \u0644\u062d\u0633\u0627\u0628 \u0627\u0644\u0642\u0637\u0631 \u0628\u0646\u0627\u0621\u064b \u0639\u0644\u0649 \u0627\u0644\u0648\u0632\u0646 \u0644\u0643\u0644 \u0648\u062d\u062f\u0629 \u0637\u0648\u0644\u060c \u0648\u0641\u0642\u064b\u0627 \u0644\u0644\u0645\u0639\u0627\u064a\u064a\u0631 \u0627\u0644\u0648\u0637\u0646\u064a\u0629.<\/li>\n\n<li><strong>\u0642\u064a\u0627\u0633 \u0627\u0644\u0642\u0637\u0631 \u0627\u0644\u062f\u0627\u062e\u0644\u064a:<\/strong> \u0642\u0645 \u0628\u0625\u062f\u062e\u0627\u0644 \u0645\u0642\u064a\u0627\u0633 \u0641\u064a \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0644\u0642\u064a\u0627\u0633 \u0642\u0637\u0631\u0647 \u0627\u0644\u062f\u0627\u062e\u0644\u064a\u060c \u0648\u0645\u0642\u0627\u0631\u0646\u0629 \u0627\u0644\u0646\u062a\u064a\u062c\u0629 \u0628\u0627\u0644\u0645\u0639\u0627\u064a\u064a\u0631 \u0627\u0644\u0648\u0637\u0646\u064a\u0629 \u0644\u0644\u062f\u0642\u0629.<\/li>\n\n<li><strong>\u0637\u0631\u0642 \u0623\u062e\u0631\u0649:<\/strong> \u0648\u062a\u062a\u0636\u0645\u0646 \u0627\u0644\u0637\u0631\u0642 \u0627\u0644\u0625\u0636\u0627\u0641\u064a\u0629 \u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0645\u0642\u0627\u064a\u064a\u0633 \u0633\u0645\u0643 \u0627\u0644\u0645\u0648\u062c\u0627\u062a \u0641\u0648\u0642 \u0627\u0644\u0635\u0648\u062a\u064a\u0629 \u0644\u0642\u064a\u0627\u0633 \u0642\u0637\u0631 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0628\u0634\u0643\u0644 \u063a\u064a\u0631 \u0645\u0628\u0627\u0634\u0631 \u0645\u0646 \u062e\u0644\u0627\u0644 \u0627\u0643\u062a\u0634\u0627\u0641 \u0627\u0644\u062a\u063a\u064a\u0631\u0627\u062a \u0641\u064a \u0627\u0644\u0645\u0648\u062c\u0627\u062a \u0641\u0648\u0642 \u0627\u0644\u0635\u0648\u062a\u064a\u0629 \u0627\u0644\u062a\u064a \u062a\u0645\u0631 \u0639\u0628\u0631 \u0627\u0644\u0645\u0627\u062f\u0629.<\/li><\/ul><p class=\"wp-block-paragraph\">\u062a\u0648\u0641\u0631 \u0647\u0630\u0647 \u0627\u0644\u0637\u0631\u0642 \u062e\u064a\u0627\u0631\u0627\u062a \u0645\u062e\u062a\u0644\u0641\u0629 \u0628\u0646\u0627\u0621\u064b \u0639\u0644\u0649 \u0627\u0644\u0645\u0639\u062f\u0627\u062a \u0627\u0644\u0645\u062a\u0648\u0641\u0631\u0629 \u0648\u0627\u0644\u062f\u0642\u0629 \u0627\u0644\u0644\u0627\u0632\u0645\u0629 \u0644\u0644\u0642\u064a\u0627\u0633.<\/p><h3 class=\"wp-block-heading\">\u062c\u062f\u0648\u0644 \u0645\u0642\u0627\u0633\u0627\u062a \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0634\u0627\u0626\u0639<\/h3><p class=\"wp-block-paragraph\">\u064a\u0639\u062f \u0627\u062e\u062a\u064a\u0627\u0631 \u0627\u0644\u062d\u062c\u0645 \u0627\u0644\u0635\u062d\u064a\u062d \u0644\u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0623\u0645\u0631\u064b\u0627 \u0628\u0627\u0644\u063a \u0627\u0644\u0623\u0647\u0645\u064a\u0629. \u0639\u0627\u062f\u0629\u064b \u0645\u0627 \u064a\u062a\u0645 \u0627\u0644\u0625\u0634\u0627\u0631\u0629 \u0625\u0644\u0649 \u0623\u062d\u062c\u0627\u0645 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0625\u0645\u0628\u0631\u0627\u0637\u0648\u0631\u064a\u0629 \u0628\u0627\u0644\u0623\u0631\u0642\u0627\u0645\u060c \u0628\u062f\u0621\u064b\u0627 \u0645\u0646 #3. \u064a\u0632\u064a\u062f \u0643\u0644 \u0631\u0642\u0645 \u0645\u062a\u062a\u0627\u0644\u064a \u0627\u0644\u0642\u0637\u0631 \u0628\u0645\u0642\u062f\u0627\u0631 1\/8 \u0628\u0648\u0635\u0629\u060c \u062d\u062a\u0649 #8.&nbsp;<\/p><p class=\"wp-block-paragraph\">\u0625\u0646 \u0641\u0647\u0645 \u0647\u0630\u0627 \u0627\u0644\u0646\u0645\u0637 \u064a\u0633\u0647\u0644 \u062a\u0642\u062f\u064a\u0631 \u0623\u0642\u0637\u0627\u0631 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0645\u0631\u0642\u0645\u0629 \u0627\u0644\u0645\u062e\u062a\u0644\u0641\u0629 \u0628\u0633\u0631\u0639\u0629. \u064a\u0648\u062c\u062f \u0623\u062f\u0646\u0627\u0647 \u0645\u062e\u0637\u0637 \u0642\u0645\u0646\u0627 \u0628\u062a\u062c\u0645\u064a\u0639\u0647 \u0644\u0631\u0627\u062d\u062a\u0643\u060c \u0645\u0645\u0627 \u064a\u0648\u0641\u0631 \u0645\u0631\u062c\u0639\u064b\u0627 \u0648\u0627\u0636\u062d\u064b\u0627 \u0644\u0644\u0645\u0639\u0644\u0648\u0645\u0627\u062a \u0627\u0644\u062a\u064a \u062a\u062d\u062a\u0627\u062c\u0647\u0627.<\/p><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u062d\u062c\u0645 \u0627\u0644\u0628\u0627\u0631 \u0627\u0644\u0625\u0645\u0628\u0631\u0627\u0637\u0648\u0631\u064a<\/strong><\/td><td><strong>\u0627\u0644\u0648\u0632\u0646 (\u0631\u0637\u0644\/\u0642\u062f\u0645)<\/strong><\/td><td><strong>\u0627\u0644\u0648\u0632\u0646 (\u0643\u062c\u0645\/\u0645)<\/strong><\/td><td><strong>\u0627\u0644\u0642\u0637\u0631 \u0627\u0644\u0627\u0633\u0645\u064a (\u0628\u0648\u0635\u0629)<\/strong><\/td><td><strong>\u0627\u0644\u0642\u0637\u0631 \u0627\u0644\u0627\u0633\u0645\u064a (\u0645\u0645)<\/strong><\/td><td><strong>\u0627\u0644\u0645\u0633\u0627\u062d\u0629 \u0627\u0644\u0625\u0633\u0645\u064a\u0629 (\u0628\u0627\u0644\u0625\u0646\u0634\u00b2)<\/strong><\/td><td><strong>\u0627\u0644\u0645\u0633\u0627\u062d\u0629 \u0627\u0644\u0625\u0633\u0645\u064a\u0629 (\u0645\u0645\u00b2)<\/strong><\/td><\/tr><tr><td>#3<\/td><td>0.376<\/td><td>0.561<\/td><td>0.375<\/td><td>9.525<\/td><td>0.11<\/td><td>71<\/td><\/tr><tr><td>#4<\/td><td>0.668<\/td><td>0.996<\/td><td>0.5<\/td><td>12.7<\/td><td>0.2<\/td><td>129<\/td><\/tr><tr><td>#5<\/td><td>1.043<\/td><td>1.556<\/td><td>0.625<\/td><td>15.875<\/td><td>0.31<\/td><td>200<\/td><\/tr><tr><td>#6<\/td><td>1.502<\/td><td>2.24<\/td><td>0.75<\/td><td>19.05<\/td><td>0.44<\/td><td>284<\/td><\/tr><tr><td>#7<\/td><td>2.044<\/td><td>3.049<\/td><td>0.875<\/td><td>22.225<\/td><td>0.6<\/td><td>387<\/td><\/tr><tr><td>#8<\/td><td>2.67<\/td><td>3.982<\/td><td>1<\/td><td>25.4<\/td><td>0.79<\/td><td>509<\/td><\/tr><tr><td>#9<\/td><td>3.4<\/td><td>5.071<\/td><td>1.128<\/td><td>28.65<\/td><td>1<\/td><td>645<\/td><\/tr><tr><td>#10<\/td><td>4.303<\/td><td>6.418<\/td><td>1.27<\/td><td>32.26<\/td><td>1.27<\/td><td>819<\/td><\/tr><tr><td>#11<\/td><td>5.313<\/td><td>7.907<\/td><td>1.41<\/td><td>35.81<\/td><td>1.56<\/td><td>1006<\/td><\/tr><tr><td>#14<\/td><td>7.65<\/td><td>11.41<\/td><td>1.693<\/td><td>43<\/td><td>2.25<\/td><td>1452<\/td><\/tr><tr><td>#18<\/td><td>13.6<\/td><td>20.27<\/td><td>2.257<\/td><td>57.33<\/td><td>4<\/td><td>2581<\/td><\/tr><\/tbody><\/table><\/figure><p class=\"wp-block-paragraph\">\u062a\u064f\u0633\u062a\u062e\u062f\u0645 \u0623\u062d\u062c\u0627\u0645 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0645\u0646 #3 \u0625\u0644\u0649 #18 \u0628\u0634\u0643\u0644 \u0634\u0627\u0626\u0639 \u0641\u064a \u0627\u0644\u0628\u0646\u0627\u0621 \u0644\u0645\u062c\u0645\u0648\u0639\u0629 \u0645\u0646 \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a. \u0648\u0641\u064a\u0645\u0627 \u064a\u0644\u064a \u062e\u0645\u0633\u0629 \u0623\u062d\u062c\u0627\u0645 \u0634\u0627\u0626\u0639\u0629 \u0648\u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0627\u062a\u0647\u0627 \u0627\u0644\u0634\u0627\u0626\u0639\u0629:<\/p><ul class=\"wp-block-list\"><li><strong>#3 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d:<\/strong> \u064a\u062a\u0645 \u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0647 \u0641\u064a \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u062e\u0641\u064a\u0641\u0629 \u0645\u062b\u0644 \u0627\u0644\u0623\u0631\u0635\u0641\u0629\u060c \u0648\u0627\u0644\u0623\u0644\u0648\u0627\u062d \u0627\u0644\u062e\u0631\u0633\u0627\u0646\u064a\u0629 \u0627\u0644\u0635\u063a\u064a\u0631\u0629\u060c \u0648\u0627\u0644\u0628\u0646\u0627\u0621 \u0627\u0644\u0633\u0643\u0646\u064a.<\/li>\n\n<li><strong>#4 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d:<\/strong> \u062a\u0648\u062c\u062f \u0639\u0627\u062f\u0629 \u0641\u064a \u0627\u0644\u0623\u0633\u0627\u0633\u0627\u062a \u0648\u0627\u0644\u062c\u062f\u0631\u0627\u0646 \u0648\u0627\u0644\u062f\u0639\u0627\u0645\u0627\u062a \u0627\u0644\u0647\u064a\u0643\u0644\u064a\u0629 \u0627\u0644\u062e\u0641\u064a\u0641\u0629 \u0641\u064a \u0627\u0644\u0645\u0628\u0627\u0646\u064a.<\/li>\n\n<li><strong>#5 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d:<\/strong> \u064a\u062a\u0645 \u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0647 \u0641\u064a \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0645\u062a\u0648\u0633\u0637\u0629 \u0625\u0644\u0649 \u0627\u0644\u062b\u0642\u064a\u0644\u0629\u060c \u0628\u0645\u0627 \u0641\u064a \u0630\u0644\u0643 \u0627\u0644\u0623\u0631\u0636\u064a\u0627\u062a \u0627\u0644\u062e\u0631\u0633\u0627\u0646\u064a\u0629\u060c \u0648\u0627\u0644\u0645\u0645\u0631\u0627\u062a\u060c \u0648\u0627\u0644\u062c\u062f\u0631\u0627\u0646 \u0627\u0644\u0623\u0633\u0627\u0633\u064a\u0629.<\/li>\n\n<li><strong>#6 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d:<\/strong> \u062a\u0648\u062c\u062f \u0641\u064a \u0627\u0644\u0647\u064a\u0627\u0643\u0644 \u0627\u0644\u062e\u0631\u0633\u0627\u0646\u064a\u0629 \u0627\u0644\u0623\u0643\u0628\u0631 \u0645\u062b\u0644 \u0627\u0644\u062c\u0633\u0648\u0631\u060c \u0648\u062d\u0635\u0627\u0626\u0631 \u0627\u0644\u0623\u0633\u0627\u0633 \u0627\u0644\u062b\u0642\u064a\u0644\u0629\u060c \u0648\u0627\u0644\u062c\u062f\u0631\u0627\u0646 \u0627\u0644\u0627\u062d\u062a\u064a\u0627\u0637\u064a\u0629.<\/li>\n\n<li><strong>#8 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d:<\/strong> \u062a\u064f\u0633\u062a\u062e\u062f\u0645 \u0639\u0627\u062f\u0629\u064b \u0641\u064a \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0630\u0627\u062a \u0627\u0644\u0623\u062d\u0645\u0627\u0644 \u0627\u0644\u0639\u0627\u0644\u064a\u0629 \u0645\u062b\u0644 \u0627\u0644\u0623\u0639\u0645\u062f\u0629 \u0648\u0627\u0644\u0623\u0631\u0635\u0641\u0629 \u0648\u0627\u0644\u0628\u0646\u0627\u0621 \u0627\u0644\u0635\u0646\u0627\u0639\u064a \u0627\u0644\u062b\u0642\u064a\u0644.<\/li><\/ul><p class=\"wp-block-paragraph\">\u062a\u0644\u0628\u064a \u0647\u0630\u0647 \u0627\u0644\u0623\u062d\u062c\u0627\u0645 \u0645\u062c\u0645\u0648\u0639\u0629 \u0648\u0627\u0633\u0639\u0629 \u0645\u0646 \u0627\u0644\u0627\u062d\u062a\u064a\u0627\u062c\u0627\u062a \u0627\u0644\u0647\u064a\u0643\u0644\u064a\u0629\u060c \u0648\u062a\u0636\u0645\u0646 \u0627\u0644\u0645\u062a\u0627\u0646\u0629 \u0648\u0627\u0644\u0642\u0648\u0629 \u0641\u064a \u0645\u0634\u0627\u0631\u064a\u0639 \u0627\u0644\u062e\u0631\u0633\u0627\u0646\u0629 \u0627\u0644\u0645\u062e\u062a\u0644\u0641\u0629.<\/p><h2 class=\"wp-block-heading\">\u062f\u0631\u062c\u0627\u062a \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d<\/h2><p class=\"wp-block-paragraph\">\u062a\u062d\u062f\u062f \u062f\u0631\u062c\u0627\u062a \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d\u060c \u0627\u0644\u062a\u064a \u062a\u062d\u062f\u062f\u0647\u0627 \u0645\u0639\u0627\u064a\u064a\u0631 ASTM\u060c \u062e\u0635\u0627\u0626\u0635 \u0623\u0633\u0627\u0633\u064a\u0629 \u0645\u062b\u0644 \u0642\u0648\u0629 \u0627\u0644\u062e\u0636\u0648\u0639 \u0648\u0627\u0644\u0627\u0633\u062a\u0637\u0627\u0644\u0629\u060c \u0645\u0645\u0627 \u064a\u0648\u062c\u0647 \u0627\u062e\u062a\u064a\u0627\u0631 \u0627\u0644\u062a\u0639\u0632\u064a\u0632\u0627\u062a \u0644\u062a\u062d\u0642\u064a\u0642 \u0633\u0644\u0627\u0645\u0629 \u0647\u064a\u0643\u0644\u064a\u0629 \u0645\u062b\u0627\u0644\u064a\u0629 \u0641\u064a \u0645\u0634\u0627\u0631\u064a\u0639 \u0627\u0644\u0628\u0646\u0627\u0621.<\/p><h3 class=\"wp-block-heading\">\u0645\u0627 \u0647\u064a \u062f\u0631\u062c\u0627\u062a \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d\u061f<\/h3><p class=\"wp-block-paragraph\">\u062a\u062d\u062f\u062f \u062f\u0631\u062c\u0627\u062a \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0641\u064a \u0627\u0644\u0648\u0644\u0627\u064a\u0627\u062a \u0627\u0644\u0645\u062a\u062d\u062f\u0629\u060c \u0648\u0641\u0642\u064b\u0627 \u0644\u0645\u0639\u0627\u064a\u064a\u0631 ASTM\u060c \u0627\u0644\u062d\u062f \u0627\u0644\u0623\u062f\u0646\u0649 \u0644\u0642\u0648\u0629 \u0627\u0644\u062e\u0636\u0648\u0639 \u0648\u0627\u0644\u062a\u0631\u0643\u064a\u0628 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a \u0648\u0627\u0644\u0627\u0633\u062a\u0637\u0627\u0644\u0629. \u064a\u062a\u0645 \u062a\u0633\u0645\u064a\u0629 \u0627\u0644\u062f\u0631\u062c\u0627\u062a \u0627\u0644\u0634\u0627\u0626\u0639\u0629 \u0645\u062b\u0644 40 \u064860 \u064875 \u0628\u0646\u0627\u0621\u064b \u0639\u0644\u0649 \u0627\u0644\u062d\u062f \u0627\u0644\u0623\u062f\u0646\u0649 \u0644\u0642\u0648\u0629 \u0627\u0644\u062e\u0636\u0648\u0639 \u0628\u0648\u062d\u062f\u0629 ksi (1000 \u0631\u0637\u0644\/\u0628\u0648\u0635\u0629 \u0645\u0631\u0628\u0639\u0629). \u064a\u0639\u062f \u0641\u0647\u0645 \u0647\u0630\u0647 \u0627\u0644\u0645\u0639\u0627\u064a\u064a\u0631 \u0623\u0645\u0631\u064b\u0627 \u0628\u0627\u0644\u063a \u0627\u0644\u0623\u0647\u0645\u064a\u0629 \u0644\u0627\u062e\u062a\u064a\u0627\u0631 \u0627\u0644\u062a\u0639\u0632\u064a\u0632\u0627\u062a \u0644\u0636\u0645\u0627\u0646 \u0627\u0644\u0633\u0644\u0627\u0645\u0629 \u0648\u0627\u0644\u0642\u0648\u0629 \u0627\u0644\u0647\u064a\u0643\u0644\u064a\u0629.<\/p><p class=\"wp-block-paragraph\">\u064a\u0642\u062f\u0645 \u0645\u0627 \u064a\u0644\u064a \u0646\u0638\u0631\u0629 \u0639\u0627\u0645\u0629 \u0623\u0643\u062b\u0631 \u0639\u0645\u0642\u064b\u0627 \u0639\u0644\u0649 \u0627\u0644\u0645\u0639\u0627\u064a\u064a\u0631 \u0627\u0644\u062a\u0646\u0638\u064a\u0645\u064a\u0629 \u0644\u0644\u0635\u0646\u0627\u0639\u0629:<\/p><ul class=\"wp-block-list\"><li><strong>\u0645\u0639\u0627\u064a\u064a\u0631 ASTM:<\/strong> \u062a\u062d\u062f\u062f ASTM A615\/A615M \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0643\u0631\u0628\u0648\u0646\u064a (\u0627\u0644\u0645\u0634\u0648\u0647\u0629 \u0648\u0627\u0644\u0639\u0627\u062f\u064a\u0629)\u060c \u0628\u064a\u0646\u0645\u0627 \u062a\u063a\u0637\u064a ASTM A706\/A706M \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0645\u0646\u062e\u0641\u0636\u0629 \u0627\u0644\u0633\u0628\u0627\u0626\u0643. \u0648\u062a\u0648\u0636\u062d \u0643\u0644\u062a\u0627 \u0627\u0644\u0645\u0648\u0627\u0635\u0641\u0629 \u0645\u062a\u0637\u0644\u0628\u0627\u062a \u0627\u0644\u062d\u062f \u0627\u0644\u0623\u062f\u0646\u0649 \u0644\u0642\u0648\u0629 \u0627\u0644\u062e\u0636\u0648\u0639 \u0648\u0627\u0644\u062a\u0631\u0643\u064a\u0628 \u0627\u0644\u0643\u064a\u0645\u064a\u0627\u0626\u064a \u0648\u0627\u0644\u0627\u0633\u062a\u0637\u0627\u0644\u0629.<\/li><\/ul><h3 class=\"wp-block-heading\"><strong>\u0645\u0639\u0627\u064a\u064a\u0631 \u062a\u0634\u0648\u0647 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d<\/strong><\/h3><p class=\"wp-block-paragraph\">\u0645\u062a\u0637\u0644\u0628\u0627\u062a \u0627\u0644\u062a\u0634\u0648\u0647\u060c \u0627\u0644\u0645\u0648\u062c\u0648\u062f\u0629 \u0641\u064a <strong>\u0645\u0639\u0627\u064a\u064a\u0631 ASTM A615<\/strong> \u0648 <strong>\u0645\u0639\u0627\u064a\u064a\u0631 ASTM A706<\/strong>\u060c \u062a\u062d\u062f\u064a\u062f \u0627\u0644\u0645\u0633\u0627\u0641\u0627\u062a \u0648\u0627\u0631\u062a\u0641\u0627\u0639 \u0627\u0644\u0623\u0636\u0644\u0627\u0639 \u0623\u0648 \u0627\u0644\u0639\u0631\u0648\u0627\u062a \u0639\u0644\u0649 \u0623\u0633\u0637\u062d \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d. \u062a\u0639\u0645\u0644 \u0647\u0630\u0647 \u0627\u0644\u062a\u0634\u0648\u0647\u0627\u062a \u0639\u0644\u0649 \u062a\u062d\u0633\u064a\u0646 \u0627\u0644\u062a\u0631\u0627\u0628\u0637 \u0628\u064a\u0646 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0648\u0627\u0644\u062e\u0631\u0633\u0627\u0646\u0629\u060c \u0645\u0645\u0627 \u064a\u0639\u0632\u0632 \u0627\u0644\u0642\u0648\u0629 \u0648\u0627\u0644\u0627\u0633\u062a\u0642\u0631\u0627\u0631 \u0627\u0644\u0639\u0627\u0645 \u0644\u0644\u0647\u064a\u0643\u0644.<\/p><p class=\"wp-block-paragraph\">\u064a\u062a\u0645 \u062a\u062d\u062f\u064a\u062f \u062f\u0631\u062c\u0627\u062a \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0634\u0627\u0626\u0639\u0629 \u0645\u0646 \u062e\u0644\u0627\u0644 \u0627\u0644\u062d\u062f \u0627\u0644\u0623\u062f\u0646\u0649 \u0644\u0642\u0648\u0629 \u0627\u0644\u062e\u0636\u0648\u0639\u060c \u0645\u0639 \u0623\u0645\u062b\u0644\u0629 \u0628\u0645\u0627 \u0641\u064a \u0630\u0644\u0643 <strong>\u0627\u0644\u0635\u0641 40<\/strong>, <strong>\u0627\u0644\u0635\u0641 60<\/strong>\u060c \u0648 <strong>\u0627\u0644\u0635\u0641 75<\/strong>\u0625\u0646 \u0641\u0647\u0645 \u0647\u0630\u0647 \u0627\u0644\u0645\u0639\u0627\u064a\u064a\u0631 \u0623\u0645\u0631 \u0636\u0631\u0648\u0631\u064a \u0644\u0627\u062e\u062a\u064a\u0627\u0631 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0645\u0646\u0627\u0633\u0628 \u0644\u0644\u062d\u0641\u0627\u0638 \u0639\u0644\u0649 \u0627\u0644\u0633\u0644\u0627\u0645\u0629 \u0648\u0627\u0644\u0623\u062f\u0627\u0621 \u0627\u0644\u0647\u064a\u0643\u0644\u064a.<\/p><h3 class=\"wp-block-heading\">\u062c\u062f\u0648\u0644 \u0627\u0644\u062f\u0631\u062c\u0627\u062a \u0627\u0644\u0634\u0627\u0626\u0639\u0629 \u0648\u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a<\/h3><p class=\"wp-block-paragraph\">\u064a\u0648\u0641\u0631 \u0647\u0630\u0627 \u0627\u0644\u0631\u0633\u0645 \u0627\u0644\u0628\u064a\u0627\u0646\u064a \u0645\u0642\u0627\u0631\u0646\u0629 \u0648\u0627\u0636\u062d\u0629 \u0628\u064a\u0646 \u0647\u0630\u0647 \u0627\u0644\u062f\u0631\u062c\u0627\u062a\u060c \u0645\u0645\u0627 \u064a\u0633\u0627\u0639\u062f \u0641\u064a \u0627\u0644\u0627\u062e\u062a\u064a\u0627\u0631 \u0627\u0644\u062f\u0642\u064a\u0642 \u0644\u0644\u062d\u062f\u064a\u062f \u0627\u0644\u0635\u0644\u0628 \u0644\u0645\u062a\u0637\u0644\u0628\u0627\u062a \u0627\u0644\u0647\u064a\u0627\u0643\u0644 \u0627\u0644\u0645\u062e\u062a\u0644\u0641\u0629 \u0641\u064a \u0645\u0634\u0627\u0631\u064a\u0639 \u0627\u0644\u0628\u0646\u0627\u0621 \u0648\u0627\u0644\u0628\u0646\u064a\u0629 \u0627\u0644\u062a\u062d\u062a\u064a\u0629.<\/p><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u0645\u0639\u064a\u0627\u0631<\/strong><\/td><td><strong>\u062f\u0631\u062c\u0629<\/strong><\/td><td><strong>\u0642\u0648\u0629 \u0627\u0644\u062e\u0636\u0648\u0639<\/strong><strong><br><\/strong><strong> (\u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644 \/ \u0643\u064a\u0644\u0648 \u0628\u0648\u0635\u0629 \u0645\u0631\u0628\u0639\u0629)<\/strong><\/td><td><strong>\u0642\u0648\u0629 \u0627\u0644\u0634\u062f <\/strong><strong><br><\/strong><strong>(\u0645\u064a\u062c\u0627 \u0628\u0627\u0633\u0643\u0627\u0644 \/ \u0643\u064a\u0644\u0648 \u0628\u0648\u0635\u0629 \u0645\u0631\u0628\u0639\u0629)<\/strong><\/td><td><strong>\u0627\u0644\u0627\u0633\u062a\u0637\u0627\u0644\u0629 (%)<\/strong><\/td><\/tr><tr><td>\u0645\u0639\u0627\u064a\u064a\u0631 ASTM A615\/A615M<\/td><td>\u0627\u0644\u0635\u0641 40<\/td><td>280 \/ 40.6<\/td><td>420 \/ 60.9<\/td><td>7<\/td><\/tr><tr><td>\u0645\u0639\u0627\u064a\u064a\u0631 ASTM A615\/A615M<\/td><td>\u0627\u0644\u0635\u0641 60<\/td><td>420 \/ 60.9<\/td><td>620 \/ 89.9<\/td><td>9<\/td><\/tr><tr><td>\u0645\u0639\u0627\u064a\u064a\u0631 ASTM A615\/A615M<\/td><td>\u0627\u0644\u0635\u0641 75<\/td><td>520 \/ 75.4<\/td><td>690 \/ 100.0<\/td><td>11<\/td><\/tr><tr><td>\u0645\u0639\u0627\u064a\u064a\u0631 ASTM A706\/A706M<\/td><td>\u0627\u0644\u0635\u0641 60<\/td><td>420 \/ 60.9<\/td><td>550 \/ 79.8<\/td><td>14<\/td><\/tr><tr><td>\u0645\u0639\u0627\u064a\u064a\u0631 ASTM A706\/A706M<\/td><td>\u0627\u0644\u0635\u0641 80<\/td><td>550 \/ 79.8<\/td><td>690 \/ 100.0<\/td><td>14<\/td><\/tr><tr><td>\u0645\u0639\u0627\u064a\u064a\u0631 ASTM A615\/A615M<\/td><td>\u0627\u0644\u0635\u0641 100<\/td><td>690 \/ 100.0<\/td><td>830 \/ 120.3<\/td><td>&#8211;<\/td><\/tr><\/tbody><\/table><\/figure><p class=\"wp-block-paragraph\">\u0641\u064a\u0645\u0627 \u064a\u0644\u064a \u0633\u064a\u0646\u0627\u0631\u064a\u0648\u0647\u0627\u062a \u062a\u0637\u0628\u064a\u0642 \u0645\u062e\u062a\u0644\u0641\u0629 \u0644\u062f\u0631\u062c\u0627\u062a \u0645\u062e\u062a\u0644\u0641\u0629 \u0645\u0646 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d:<\/p><h4 class=\"wp-block-heading\">\u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0645\u0646 \u0627\u0644\u062f\u0631\u062c\u0629 40<\/h4><p class=\"wp-block-paragraph\">\u062a\u064f\u0633\u062a\u062e\u062f\u0645 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0645\u0646 \u0627\u0644\u062f\u0631\u062c\u0629 40 \u0628\u0634\u0643\u0644 \u0645\u062a\u0643\u0631\u0631 \u0641\u064a \u0627\u0644\u0647\u064a\u0627\u0643\u0644 \u0630\u0627\u062a \u0627\u0644\u0623\u062d\u0645\u0627\u0644 \u0627\u0644\u062e\u0641\u064a\u0641\u0629 \u0648\u0645\u0634\u0627\u0631\u064a\u0639 \u0627\u0644\u0645\u0628\u0627\u0646\u064a \u0627\u0644\u0633\u0643\u0646\u064a\u0629. \u0648\u0647\u064a \u0645\u0646\u0627\u0633\u0628\u0629 \u0644\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0645\u062b\u0644 \u0627\u0644\u0623\u0631\u0635\u0641\u0629 \u0648\u0627\u0644\u0623\u0644\u0648\u0627\u062d \u0627\u0644\u062e\u0631\u0633\u0627\u0646\u064a\u0629 \u0627\u0644\u0635\u063a\u064a\u0631\u0629 \u0648\u0627\u0644\u0645\u0628\u0627\u0646\u064a \u0627\u0644\u0645\u0646\u062e\u0641\u0636\u0629 \u0627\u0644\u0627\u0631\u062a\u0641\u0627\u0639 \u062d\u064a\u062b \u062a\u0643\u0648\u0646 \u0627\u0644\u0642\u0648\u0629 \u0627\u0644\u0645\u062a\u0648\u0633\u0637\u0629 \u0643\u0627\u0641\u064a\u0629.<\/p><h4 class=\"wp-block-heading\">\u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0645\u0646 \u0627\u0644\u062f\u0631\u062c\u0629 60<\/h4><p class=\"wp-block-paragraph\">\u064a\u0648\u0641\u0631 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0645\u0646 \u0627\u0644\u062f\u0631\u062c\u0629 60 \u0642\u0648\u0629 \u0648\u0645\u062a\u0627\u0646\u0629 \u0645\u062a\u0632\u0627\u064a\u062f\u0629\u060c \u0645\u0645\u0627 \u064a\u062c\u0639\u0644\u0647 \u0645\u0646\u0627\u0633\u0628\u064b\u0627 \u0644\u0644\u0647\u064a\u0627\u0643\u0644 \u0630\u0627\u062a \u0627\u0644\u0623\u062d\u0645\u0627\u0644 \u0627\u0644\u0645\u062a\u0648\u0633\u0637\u0629 \u0625\u0644\u0649 \u0627\u0644\u062b\u0642\u064a\u0644\u0629. \u0648\u064a\u064f\u0633\u062a\u062e\u062f\u0645 \u0639\u0627\u062f\u0629\u064b \u0641\u064a \u0627\u0644\u0645\u0628\u0627\u0646\u064a \u0627\u0644\u062a\u062c\u0627\u0631\u064a\u0629 \u0648\u0627\u0644\u062c\u0633\u0648\u0631 \u0648\u0623\u0631\u0635\u0641\u0629 \u0627\u0644\u0637\u0631\u0642 \u0627\u0644\u0633\u0631\u064a\u0639\u0629.<\/p><h4 class=\"wp-block-heading\">\u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u062f\u0631\u062c\u0629 75<\/h4><p class=\"wp-block-paragraph\">\u062a\u0648\u0641\u0631 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0645\u0646 \u0627\u0644\u062f\u0631\u062c\u0629 75 \u0642\u0648\u0629 \u0645\u062a\u0632\u0627\u064a\u062f\u0629 \u0648\u0647\u064a \u0645\u0635\u0645\u0645\u0629 \u0644\u0644\u0647\u064a\u0627\u0643\u0644 \u0627\u0644\u062b\u0642\u064a\u0644\u0629 \u0648\u0627\u0644\u0645\u0628\u0627\u0646\u064a \u0627\u0644\u0634\u0627\u0647\u0642\u0629. \u0648\u0647\u064a \u0645\u0646\u0627\u0633\u0628\u0629 \u0644\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u062a\u064a \u062a\u062a\u0637\u0644\u0628 \u0623\u062f\u0627\u0621\u064b \u0647\u064a\u0643\u0644\u064a\u064b\u0627 \u0645\u062a\u0641\u0648\u0642\u064b\u0627\u060c \u0645\u062b\u0644 \u0627\u0644\u0645\u0631\u0627\u0641\u0642 \u0627\u0644\u0635\u0646\u0627\u0639\u064a\u0629 \u0648\u0645\u0634\u0627\u0631\u064a\u0639 \u0627\u0644\u0628\u0646\u064a\u0629 \u0627\u0644\u062a\u062d\u062a\u064a\u0629 \u0648\u0627\u0633\u0639\u0629 \u0627\u0644\u0646\u0637\u0627\u0642.<\/p><h4 class=\"wp-block-heading\">\u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u062f\u0631\u062c\u0629 80<\/h4><p class=\"wp-block-paragraph\">\u062a\u064f\u0633\u062a\u062e\u062f\u0645 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0645\u0646 \u0627\u0644\u062f\u0631\u062c\u0629 80 \u0628\u0634\u0643\u0644 \u0623\u0633\u0627\u0633\u064a \u0641\u064a \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0632\u0644\u0632\u0627\u0644\u064a\u0629 \u062d\u064a\u062b \u062a\u0643\u0648\u0646 \u0627\u0644\u0645\u0631\u0648\u0646\u0629 \u0648\u0627\u0644\u0642\u0648\u0629 \u0623\u0645\u0631\u064a\u0646 \u0628\u0627\u0644\u063a\u064a \u0627\u0644\u0623\u0647\u0645\u064a\u0629. \u0648\u0647\u064a \u0645\u0646\u0627\u0633\u0628\u0629 \u0644\u0644\u0647\u064a\u0627\u0643\u0644 \u0641\u064a \u0627\u0644\u0645\u0646\u0627\u0637\u0642 \u0627\u0644\u0645\u0639\u0631\u0636\u0629 \u0644\u0644\u0632\u0644\u0627\u0632\u0644\u060c \u0645\u0645\u0627 \u064a\u0636\u0645\u0646 \u0633\u0644\u0627\u0645\u0629 \u0627\u0644\u0647\u064a\u0627\u0643\u0644 \u0641\u064a \u0638\u0644 \u0638\u0631\u0648\u0641 \u0627\u0644\u062a\u062d\u0645\u064a\u0644 \u0627\u0644\u062f\u064a\u0646\u0627\u0645\u064a\u0643\u064a.<\/p><h4 class=\"wp-block-heading\">\u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0645\u0646 \u0627\u0644\u062f\u0631\u062c\u0629 100<\/h4><p class=\"wp-block-paragraph\">\u062a\u064f\u0633\u062a\u062e\u062f\u0645 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0645\u0646 \u0627\u0644\u062f\u0631\u062c\u0629 100 \u0641\u064a \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0645\u062a\u062e\u0635\u0635\u0629 \u0627\u0644\u062a\u064a \u062a\u062a\u0637\u0644\u0628 \u0642\u0648\u0629 \u0648\u0645\u062a\u0627\u0646\u0629 \u0639\u0627\u0644\u064a\u0629 \u0644\u0644\u063a\u0627\u064a\u0629. \u0648\u062a\u0648\u062c\u062f \u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0644\u0647\u0627 \u0641\u064a \u0627\u0644\u0625\u0646\u0634\u0627\u0621\u0627\u062a \u0627\u0644\u0635\u0646\u0627\u0639\u064a\u0629 \u0627\u0644\u062b\u0642\u064a\u0644\u0629 \u0645\u062b\u0644 \u0627\u0644\u0645\u0646\u0635\u0627\u062a \u0627\u0644\u0628\u062d\u0631\u064a\u0629 \u0648\u0627\u0644\u0633\u062f\u0648\u062f \u0648\u0645\u062d\u0637\u0627\u062a \u0627\u0644\u0637\u0627\u0642\u0629 \u0627\u0644\u0646\u0648\u0648\u064a\u0629\u060c \u062d\u064a\u062b \u064a\u0643\u0648\u0646 \u0627\u0644\u062a\u0639\u0632\u064a\u0632 \u0627\u0644\u0642\u0648\u064a \u0636\u0631\u0648\u0631\u064a\u064b\u0627 \u0644\u062a\u062d\u0645\u0644 \u0627\u0644\u0638\u0631\u0648\u0641 \u0627\u0644\u0642\u0627\u0633\u064a\u0629.<\/p><p class=\"wp-block-paragraph\">\u062a\u0644\u0628\u064a \u0647\u0630\u0647 \u0627\u0644\u062f\u0631\u062c\u0627\u062a \u0627\u0644\u0645\u062e\u062a\u0644\u0641\u0629 \u0645\u0646 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0645\u062c\u0645\u0648\u0639\u0629 \u0648\u0627\u0633\u0639\u0629 \u0645\u0646 \u0627\u0644\u0645\u062a\u0637\u0644\u0628\u0627\u062a \u0627\u0644\u0647\u064a\u0643\u0644\u064a\u0629\u060c \u0645\u0645\u0627 \u064a\u0636\u0645\u0646 \u0627\u0644\u0633\u0644\u0627\u0645\u0629 \u0648\u0627\u0644\u0645\u062a\u0627\u0646\u0629 \u0648\u0627\u0644\u0623\u062f\u0627\u0621 \u0641\u064a \u0645\u062e\u062a\u0644\u0641 \u0645\u0634\u0627\u0631\u064a\u0639 \u0627\u0644\u0628\u0646\u0627\u0621.<\/p><h3 class=\"wp-block-heading\">\u0643\u064a\u0641\u064a\u0629 \u0627\u0644\u062a\u0639\u0631\u0641 \u0639\u0644\u0649 \u0627\u0644\u0639\u0644\u0627\u0645\u0627\u062a \u0627\u0644\u0645\u0648\u062c\u0648\u062f\u0629 \u0639\u0644\u0649 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d<\/h3><p class=\"wp-block-paragraph\">\u0628\u0645\u062c\u0631\u062f \u0623\u0646 \u062a\u0643\u062a\u0633\u0628 \u0641\u0647\u0645\u064b\u0627 \u0643\u0627\u0645\u0644\u0627\u064b \u0644\u062a\u0635\u0646\u064a\u0641\u0627\u062a \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d\u060c \u0641\u0623\u0646\u062a \u0628\u062d\u0627\u062c\u0629 \u0623\u064a\u0636\u064b\u0627 \u0625\u0644\u0649 \u0625\u062a\u0642\u0627\u0646 \u0627\u0644\u062a\u0639\u0631\u0641 \u0639\u0644\u0649 \u0627\u0644\u0639\u0644\u0627\u0645\u0627\u062a \u0627\u0644\u0645\u0648\u062c\u0648\u062f\u0629 \u0639\u0644\u0649 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d. \u062a\u0636\u0645\u0646 \u0639\u0644\u0627\u0645\u0627\u062a \u0627\u0644\u0634\u0631\u0643\u0627\u062a \u0627\u0644\u0645\u0635\u0646\u0639\u0629\u060c \u0645\u062b\u0644 \u062a\u0648\u0627\u0631\u064a\u062e \u0627\u0644\u0625\u0646\u062a\u0627\u062c \u0648\u0623\u0631\u0642\u0627\u0645 \u0627\u0644\u062f\u0641\u0639\u0627\u062a\u060c \u0625\u0645\u0643\u0627\u0646\u064a\u0629 \u0627\u0644\u062a\u062a\u0628\u0639 \u0648\u0636\u0645\u0627\u0646 \u0627\u0644\u062c\u0648\u062f\u0629\u060c \u0648\u0647\u0648 \u0623\u0645\u0631 \u0628\u0627\u0644\u063a \u0627\u0644\u0623\u0647\u0645\u064a\u0629 \u0644\u0633\u0644\u0627\u0645\u0629 \u0627\u0644\u0628\u0646\u064a\u0629 \u0648\u0627\u0644\u0627\u0645\u062a\u062b\u0627\u0644 \u0644\u0644\u0645\u0639\u0627\u064a\u064a\u0631.<\/p><h4 class=\"wp-block-heading\">\u0627\u0644\u062f\u0631\u062c\u0627\u062a \u0627\u0644\u0639\u0644\u0627\u0645\u0627\u062a<\/h4><p class=\"wp-block-paragraph\">\u064a\u062a\u0645 \u0639\u0627\u062f\u0629\u064b \u0648\u0636\u0639 \u0639\u0644\u0627\u0645\u0627\u062a \u0639\u0644\u0649 \u062f\u0631\u062c\u0627\u062a \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0639\u0644\u0649 \u0627\u0644\u0633\u0637\u062d\u060c \u0645\u062b\u0644 &quot;40&quot; \u0644\u0644\u062f\u0631\u062c\u0629 40\u060c \u0645\u0645\u0627 \u064a\u0634\u064a\u0631 \u0625\u0644\u0649 \u0627\u0644\u062d\u062f \u0627\u0644\u0623\u062f\u0646\u0649 \u0644\u0642\u0648\u0629 \u0627\u0644\u062e\u0636\u0648\u0639 \u0644\u0644\u0635\u0644\u0628.<\/p><h4 class=\"wp-block-heading\">\u0639\u0644\u0627\u0645\u0627\u062a \u0627\u0644\u0642\u0637\u0631<\/h4><p class=\"wp-block-paragraph\">\u063a\u0627\u0644\u0628\u064b\u0627 \u0645\u0627 \u064a\u062a\u0645 \u0627\u0644\u0625\u0634\u0627\u0631\u0629 \u0625\u0644\u0649 \u0642\u0637\u0631 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0639\u0644\u0649 \u0627\u0644\u0633\u0637\u062d \u0628\u0627\u0644\u0623\u0631\u0642\u0627\u0645 \u0623\u0648 \u0627\u0644\u062e\u0637\u0648\u0637\u060c \u0645\u062b\u0644 \u062b\u0644\u0627\u062b\u0629 \u062e\u0637\u0648\u0637 \u0645\u062a\u0648\u0627\u0632\u064a\u0629 \u0644\u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d #3 (\u0642\u0637\u0631 9.5 \u0645\u0645) \u0623\u0648 \u0633\u062a\u0629 \u062e\u0637\u0648\u0637 \u0645\u062a\u0648\u0627\u0632\u064a\u0629 \u0644\u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d #6 (\u0642\u0637\u0631 19 \u0645\u0645).<\/p><h4 class=\"wp-block-heading\">\u0627\u0644\u062a\u0639\u0631\u064a\u0641 \u0627\u0644\u0642\u064a\u0627\u0633\u064a<\/h4><p class=\"wp-block-paragraph\">\u064a\u062d\u0645\u0644 \u0643\u0644 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u062a\u0633\u0645\u064a\u0629 \u0642\u064a\u0627\u0633\u064a\u0629\u060c \u0645\u062b\u0644 ASTM A615 \u0623\u0648 ISO 6935-2\u060c \u0645\u0645\u0627 \u064a\u0636\u0645\u0646 \u0627\u0644\u0627\u0645\u062a\u062b\u0627\u0644 \u0644\u0645\u0639\u0627\u064a\u064a\u0631 \u0627\u0644\u062a\u0635\u0646\u064a\u0639 \u0648\u0627\u0644\u0623\u062f\u0627\u0621 \u0627\u0644\u0645\u062d\u062f\u062f\u0629.<\/p><p class=\"wp-block-paragraph\">\u0642\u062f \u064a\u0642\u0648\u0645 \u0627\u0644\u0645\u0635\u0646\u0639\u0648\u0646 \u0623\u064a\u0636\u064b\u0627 \u0628\u0637\u0628\u0627\u0639\u0629 \u0639\u0644\u0627\u0645\u0627\u062a\u0647\u0645 \u0627\u0644\u062e\u0627\u0635\u0629\u060c \u0628\u0645\u0627 \u0641\u064a \u0630\u0644\u0643 \u062a\u0648\u0627\u0631\u064a\u062e \u0627\u0644\u0625\u0646\u062a\u0627\u062c \u0648\u0623\u0631\u0642\u0627\u0645 \u0627\u0644\u062f\u0641\u0639\u0627\u062a\u060c \u0644\u062a\u062a\u0628\u0639 \u0627\u0644\u062c\u0648\u062f\u0629 \u0648\u0636\u0645\u0627\u0646 \u0625\u0645\u0643\u0627\u0646\u064a\u0629 \u062a\u062a\u0628\u0639\u0647\u0627 \u0637\u0648\u0627\u0644 \u0633\u0644\u0633\u0644\u0629 \u0627\u0644\u062a\u0648\u0631\u064a\u062f.<\/p><h2 class=\"wp-block-heading\">\u0643\u064a\u0641\u064a\u0629 \u0641\u062d\u0635 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0648\u0645\u0627 \u0627\u0644\u0630\u064a \u064a\u062c\u0628 \u0627\u0644\u062a\u062d\u0642\u0642 \u0645\u0646\u0647<\/h2><p class=\"wp-block-paragraph\">\u0639\u0646\u062f \u0627\u0633\u062a\u0644\u0627\u0645 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d\u060c \u0645\u0646 \u0627\u0644\u0645\u0647\u0645 \u0627\u0644\u062a\u0645\u064a\u064a\u0632 \u0628\u064a\u0646\u0647\u0627 \u0648\u0628\u064a\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0639\u0627\u062f\u064a \u0628\u0633\u0628\u0628 \u0639\u0645\u0644\u064a\u0629 \u062a\u0635\u0646\u064a\u0639\u0647\u0627 \u0648\u0645\u0638\u0647\u0631\u0647\u0627.<\/p><h3 class=\"wp-block-heading\">\u0627\u0644\u062a\u0641\u062a\u064a\u0634 \u0627\u0644\u0628\u0635\u0631\u064a<\/h3><p class=\"wp-block-paragraph\">\u0627\u0641\u062d\u0635 \u0627\u0644\u0633\u0637\u062d \u0628\u062d\u062b\u064b\u0627 \u0639\u0646 \u0623\u064a \u0635\u062f\u0623 \u0623\u0648 \u062a\u0622\u0643\u0644 \u0623\u0648 \u0636\u0631\u0631 \u0645\u0627\u062f\u064a \u0642\u062f \u064a\u0624\u062b\u0631 \u0639\u0644\u0649 \u0633\u0644\u0627\u0645\u0629 \u0627\u0644\u0647\u064a\u0643\u0644. \u0648\u0647\u0630\u0627 \u064a\u0636\u0645\u0646 \u062e\u0644\u0648 \u0633\u0637\u062d \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0645\u0646 \u0627\u0644\u0639\u064a\u0648\u0628 \u0627\u0644\u062a\u064a \u0642\u062f \u062a\u0636\u0639\u0641 \u0623\u062f\u0627\u0626\u0647 \u0628\u0645\u0631\u0648\u0631 \u0627\u0644\u0648\u0642\u062a.<\/p><h3 class=\"wp-block-heading\">\u0627\u0644\u062a\u062d\u0642\u0642 \u0645\u0646 \u0627\u0644\u0645\u0648\u0627\u0635\u0641\u0627\u062a<\/h3><p class=\"wp-block-paragraph\">\u062a\u062d\u0642\u0642 \u0645\u0646 \u0642\u0637\u0631 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0648\u0637\u0648\u0644\u0647 \u0648\u0634\u0643\u0644\u0647\u0627 \u0644\u0644\u062a\u0623\u0643\u062f \u0645\u0646 \u0623\u0646\u0647 \u064a\u0644\u0628\u064a \u0645\u0639\u0627\u064a\u064a\u0631 \u0627\u0644\u062a\u0635\u0645\u064a\u0645 \u0627\u0644\u0645\u0637\u0644\u0648\u0628\u0629. \u064a\u0636\u0645\u0646 \u0627\u0644\u062a\u062d\u0642\u0642 \u0645\u0646 \u0627\u0644\u0645\u0648\u0627\u0635\u0641\u0627\u062a \u0627\u0644\u0645\u0646\u0627\u0633\u0628\u0629 \u0623\u0646 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0633\u0648\u0641 \u064a\u062a\u0646\u0627\u0633\u0628 \u0648\u064a\u0639\u0645\u0644 \u0628\u0634\u0643\u0644 \u0635\u062d\u064a\u062d \u0636\u0645\u0646 \u0645\u0634\u0631\u0648\u0639 \u0627\u0644\u0628\u0646\u0627\u0621.<\/p><h3 class=\"wp-block-heading\">\u0627\u062e\u062a\u0628\u0627\u0631 \u0627\u0644\u0639\u064a\u0646\u0627\u062a<\/h3><p class=\"wp-block-paragraph\">\u0633\u064a\u062a\u0645 \u0625\u062c\u0631\u0627\u0621 \u0627\u062e\u062a\u0628\u0627\u0631\u0627\u062a \u0623\u062e\u0630 \u0627\u0644\u0639\u064a\u0646\u0627\u062a \u0627\u0644\u0639\u0634\u0648\u0627\u0626\u064a\u0629 \u0644\u062a\u0642\u064a\u064a\u0645 \u0627\u0644\u062e\u0635\u0627\u0626\u0635 \u0645\u062b\u0644 \u0642\u0648\u0629 \u0627\u0644\u062e\u0636\u0648\u0639 \u0648\u0627\u0644\u0627\u0633\u062a\u0637\u0627\u0644\u0629. \u0648\u064a\u0636\u0645\u0646 \u0647\u0630\u0627 \u0627\u0644\u0625\u062c\u0631\u0627\u0621 \u0644\u0645\u0631\u0627\u0642\u0628\u0629 \u0627\u0644\u062c\u0648\u062f\u0629 \u0623\u0646 \u062f\u0641\u0639\u0629 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u062a\u0644\u0628\u064a \u0645\u0639\u0627\u064a\u064a\u0631 \u0627\u0644\u0623\u062f\u0627\u0621 \u0627\u0644\u0645\u062a\u0648\u0642\u0639\u0629 \u0648\u0645\u062a\u0637\u0644\u0628\u0627\u062a \u0627\u0644\u0645\u062a\u0627\u0646\u0629.<\/p><p class=\"wp-block-paragraph\">\u0648\u0623\u062e\u064a\u0631\u064b\u0627\u060c \u0642\u0645 \u0628\u062a\u062e\u0632\u064a\u0646 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0641\u064a \u0628\u064a\u0626\u0629 \u062c\u0627\u0641\u0629 \u0648\u062e\u0627\u0644\u064a\u0629 \u0645\u0646 \u0627\u0644\u0635\u062f\u0623\u060c \u0648\u0645\u0631\u062a\u0641\u0639\u0629 \u0639\u0646 \u0627\u0644\u0623\u0631\u0636\u060c \u062d\u062a\u0649 \u062a\u0635\u0628\u062d \u062c\u0627\u0647\u0632\u0629 \u0644\u0644\u0627\u0633\u062a\u062e\u062f\u0627\u0645.<\/p><h2 class=\"wp-block-heading\">\u0623\u0643\u0633\u062f\u0629 \u0648\u062a\u0622\u0643\u0644 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d<\/h2><p class=\"wp-block-paragraph\"><strong>\u0627\u0644\u0623\u0633\u0628\u0627\u0628<\/strong>:<\/p><ol class=\"wp-block-list\"><li><strong>\u0627\u0644\u0639\u0648\u0627\u0645\u0644 \u0627\u0644\u0628\u064a\u0626\u064a\u0629<\/strong>:\u064a\u062a\u0639\u0631\u0636 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0628\u0634\u0643\u0644 \u0623\u0643\u0628\u0631 \u0644\u0644\u0623\u0643\u0633\u062f\u0629 \u0641\u064a \u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u0631\u0637\u0628\u0629 \u0623\u0648 \u0627\u0644\u0645\u0627\u0644\u062d\u0629. \u064a\u0624\u062f\u064a \u0648\u062c\u0648\u062f \u0627\u0644\u0645\u0627\u0621 \u0648\u0627\u0644\u0623\u0643\u0633\u062c\u064a\u0646 \u0625\u0644\u0649 \u062a\u0633\u0631\u064a\u0639 \u0627\u0644\u062a\u0622\u0643\u0644.<\/li>\n\n<li><strong>\u062f\u0631\u062c\u0629 \u062d\u0645\u0648\u0636\u0629 \u0627\u0644\u062e\u0631\u0633\u0627\u0646\u0629<\/strong>:\u062a\u062a\u0645\u064a\u0632 \u0627\u0644\u062e\u0631\u0633\u0627\u0646\u0629 \u0639\u0627\u062f\u0629 \u0628\u062f\u0631\u062c\u0629 \u062d\u0645\u0648\u0636\u0629 \u0639\u0627\u0644\u064a\u0629\u060c \u0645\u0645\u0627 \u064a\u0634\u0643\u0644 \u0637\u0628\u0642\u0629 \u0633\u0644\u0628\u064a\u0629 \u0648\u0627\u0642\u064a\u0629 \u0639\u0644\u0649 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d. \u0648\u0645\u0639 \u0630\u0644\u0643\u060c \u0641\u0625\u0646 \u0648\u062c\u0648\u062f \u0623\u064a\u0648\u0646\u0627\u062a \u0627\u0644\u0643\u0644\u0648\u0631\u064a\u062f \u064a\u0645\u0643\u0646 \u0623\u0646 \u064a\u0624\u062f\u064a \u0625\u0644\u0649 \u062a\u062d\u0644\u0644 \u0647\u0630\u0647 \u0627\u0644\u0637\u0628\u0642\u0629\u060c \u0645\u0645\u0627 \u064a\u0624\u062f\u064a \u0625\u0644\u0649 \u0627\u0644\u062a\u0622\u0643\u0644.<\/li>\n\n<li><strong>\u0645\u0639\u0627\u0644\u062c\u0629 \u0627\u0644\u0633\u0637\u062d<\/strong>:\u064a\u0639\u062a\u0628\u0631 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u063a\u064a\u0631 \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u060c \u0645\u062b\u0644 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u063a\u064a\u0631 \u0627\u0644\u0645\u0637\u0644\u064a \u0623\u0648 \u063a\u064a\u0631 \u0627\u0644\u0645\u062c\u0644\u0641\u0646\u060c \u0623\u0643\u062b\u0631 \u0639\u0631\u0636\u0629 \u0644\u0644\u062a\u0622\u0643\u0644.<\/li><\/ol><p class=\"wp-block-paragraph\"><strong>\u0639\u0648\u0627\u0642\u0628<\/strong>:<\/p><ol class=\"wp-block-list\"><li><strong>\u0627\u0644\u0633\u0644\u0627\u0645\u0629 \u0627\u0644\u0628\u0646\u064a\u0648\u064a\u0629<\/strong>:\u064a\u0624\u062f\u064a \u0627\u0644\u062a\u0622\u0643\u0644 \u0641\u064a \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0625\u0644\u0649 \u0625\u0636\u0639\u0627\u0641\u0647\u0627\u060c \u0645\u0645\u0627 \u064a\u0642\u0644\u0644 \u0645\u0646 \u0642\u062f\u0631\u062a\u0647\u0627 \u0639\u0644\u0649 \u062a\u062d\u0645\u0644 \u0627\u0644\u0623\u062d\u0645\u0627\u0644 \u0648\u064a\u0639\u0631\u0636 \u0627\u0644\u0633\u0644\u0627\u0645\u0629 \u0627\u0644\u0639\u0627\u0645\u0629 \u0644\u0644\u0647\u064a\u0643\u0644 \u0644\u0644\u062e\u0637\u0631.<\/li>\n\n<li><strong>\u0627\u0644\u062a\u0623\u062b\u064a\u0631 \u0627\u0644\u0627\u0642\u062a\u0635\u0627\u062f\u064a<\/strong>:\u064a\u0645\u0643\u0646 \u0623\u0646 \u062a\u0643\u0648\u0646 \u0627\u0644\u0625\u0635\u0644\u0627\u062d\u0627\u062a \u0648\u0627\u0644\u062a\u0639\u0632\u064a\u0632\u0627\u062a \u0627\u0644\u0645\u0631\u062a\u0628\u0637\u0629 \u0628\u0627\u0644\u062a\u0622\u0643\u0644 \u0645\u0643\u0644\u0641\u0629\u060c \u0648\u062e\u0627\u0635\u0629 \u0641\u064a \u0645\u0634\u0627\u0631\u064a\u0639 \u0627\u0644\u0628\u0646\u064a\u0629 \u0627\u0644\u062a\u062d\u062a\u064a\u0629 \u0627\u0644\u0643\u0628\u064a\u0631\u0629.<\/li>\n\n<li><strong>\u0627\u0644\u062a\u0634\u0642\u0642 \u0648\u0627\u0644\u062a\u0642\u0634\u0631<\/strong>:\u0645\u0639 \u062a\u0648\u0633\u0639 \u0627\u0644\u0635\u062f\u0623\u060c \u0641\u0625\u0646\u0647 \u064a\u0648\u0644\u062f \u0636\u063a\u0637\u064b\u0627 \u062f\u0627\u062e\u0644\u064a\u064b\u0627\u060c \u0645\u0645\u0627 \u064a\u062a\u0633\u0628\u0628 \u0641\u064a \u062a\u0634\u0642\u0642 \u0627\u0644\u062e\u0631\u0633\u0627\u0646\u0629 \u0648\u062a\u0641\u062a\u062a\u0647\u0627\u060c \u0645\u0645\u0627 \u0642\u062f \u064a\u0624\u062f\u064a \u0625\u0644\u0649 \u0641\u0634\u0644 \u0647\u064a\u0643\u0644\u064a.<\/li><\/ol><p class=\"wp-block-paragraph\"><strong>\u0637\u0631\u0642 \u0627\u0644\u0648\u0642\u0627\u064a\u0629<\/strong>:<\/p><ol class=\"wp-block-list\"><li><strong>\u0627\u0644\u0637\u0644\u0627\u0621\u0627\u062a \u0627\u0644\u0645\u0636\u0627\u062f\u0629 \u0644\u0644\u062a\u0622\u0643\u0644<\/strong>:\u0625\u0646 \u0648\u0636\u0639 \u0627\u0644\u0637\u0644\u0627\u0621\u0627\u062a \u0645\u062b\u0644 \u0627\u0644\u0625\u064a\u0628\u0648\u0643\u0633\u064a \u0639\u0644\u0649 \u0623\u0633\u0637\u062d \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u064a\u0645\u0643\u0646 \u0623\u0646 \u064a\u0645\u0646\u0639 \u0627\u0644\u0631\u0637\u0648\u0628\u0629 \u0648\u0627\u0644\u0623\u0643\u0633\u062c\u064a\u0646 \u0645\u0646 \u0627\u0644\u0648\u0635\u0648\u0644 \u0625\u0644\u0649 \u0627\u0644\u0641\u0648\u0644\u0627\u0630.<\/li>\n\n<li><strong>\u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0639\u0627\u0644\u064a \u0627\u0644\u0645\u0642\u0627\u0648\u0645\u0629<\/strong>:\u0625\u0646 \u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623 \u0623\u0648 \u0627\u0644\u0633\u0628\u0627\u0626\u0643 \u0627\u0644\u0645\u0642\u0627\u0648\u0645\u0629 \u0644\u0644\u062a\u0622\u0643\u0644 \u064a\u062d\u0633\u0646 \u0628\u0634\u0643\u0644 \u0643\u0628\u064a\u0631 \u0645\u0646 \u0645\u062a\u0627\u0646\u0629 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d.<\/li>\n\n<li><strong>\u062e\u0644\u0637\u0629 \u0627\u0644\u062e\u0631\u0633\u0627\u0646\u0629 \u0627\u0644\u0645\u062b\u0627\u0644\u064a\u0629<\/strong>:\u064a\u0645\u0643\u0646 \u0623\u0646 \u064a\u0624\u062f\u064a \u062a\u0642\u0644\u064a\u0644 \u0645\u062d\u062a\u0648\u0649 \u0627\u0644\u0643\u0644\u0648\u0631\u064a\u062f \u0641\u064a \u0627\u0644\u062e\u0631\u0633\u0627\u0646\u0629 \u0648\u0625\u0636\u0627\u0641\u0629 \u0645\u062b\u0628\u0637\u0627\u062a \u0627\u0644\u062a\u0622\u0643\u0644 \u0625\u0644\u0649 \u062a\u0642\u0644\u064a\u0644 \u062e\u0637\u0631 \u062a\u0622\u0643\u0644 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d.<\/li>\n\n<li><strong>\u0635\u064a\u0627\u0646\u0629<\/strong>:\u062a\u0633\u0627\u0639\u062f \u0639\u0645\u0644\u064a\u0627\u062a \u0627\u0644\u0641\u062d\u0635 \u0648\u0627\u0644\u0635\u064a\u0627\u0646\u0629 \u0627\u0644\u0645\u0646\u062a\u0638\u0645\u0629 \u0641\u064a \u062a\u062d\u062f\u064a\u062f \u0627\u0644\u0639\u0644\u0627\u0645\u0627\u062a \u0627\u0644\u0645\u0628\u0643\u0631\u0629 \u0644\u0644\u062a\u0622\u0643\u0644\u060c \u0645\u0645\u0627 \u064a\u0633\u0645\u062d \u0628\u0627\u0644\u062a\u062f\u062e\u0644 \u0641\u064a \u0627\u0644\u0648\u0642\u062a \u0627\u0644\u0645\u0646\u0627\u0633\u0628 \u0644\u062a\u0645\u062f\u064a\u062f \u0639\u0645\u0631 \u0627\u0644\u0647\u064a\u0643\u0644.<\/li><\/ol><h2 class=\"wp-block-heading\">\u0643\u064a\u0641\u064a\u0629 \u0645\u0646\u0639 \u0627\u0646\u0632\u0644\u0627\u0642 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0641\u064a \u0627\u0644\u062e\u0631\u0633\u0627\u0646\u0629<\/h2><p class=\"wp-block-paragraph\">\u064a\u0639\u062f \u0627\u0644\u0648\u0636\u0639 \u0627\u0644\u0645\u0646\u0627\u0633\u0628 \u0648\u0627\u0644\u062a\u0639\u0632\u064a\u0632 \u0627\u0644\u0647\u064a\u0643\u0644\u064a \u0623\u0645\u0631\u064b\u0627 \u0623\u0633\u0627\u0633\u064a\u064b\u0627 \u0644\u0645\u0646\u0639 \u0633\u062d\u0628 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u062a\u062d\u062a \u0627\u0644\u0636\u063a\u0637 \u0627\u0644\u0639\u0627\u0644\u064a.<\/p><ol class=\"wp-block-list\"><li><strong>\u0639\u0645\u0642 \u0627\u0644\u062a\u0636\u0645\u064a\u0646<\/strong>:\u064a\u062c\u0628 \u0623\u0646 \u064a\u0643\u0648\u0646 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0645\u062f\u0641\u0648\u0646\u064b\u0627 \u0628\u0639\u0645\u0642 \u0641\u064a \u0627\u0644\u0639\u0646\u0627\u0635\u0631 \u0627\u0644\u0647\u064a\u0643\u0644\u064a\u0629 \u0627\u0644\u0645\u062c\u0627\u0648\u0631\u0629\u060c \u0648\u0639\u0627\u062f\u0629 \u0645\u0627 \u064a\u0643\u0648\u0646 \u0642\u0637\u0631 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0623\u0643\u0628\u0631 \u0645\u0646 \u0642\u0637\u0631 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0628\u0645\u0642\u062f\u0627\u0631 40 \u0625\u0644\u0649 60 \u0645\u0631\u0629. \u0648\u0647\u0630\u0627 \u064a\u0632\u064a\u062f \u0645\u0646 \u0627\u0644\u0627\u062d\u062a\u0643\u0627\u0643 \u0627\u0644\u0630\u064a \u064a\u062d\u0627\u0641\u0638 \u0639\u0644\u0649 \u062b\u0628\u0627\u062a \u0627\u0644\u062d\u062f\u064a\u062f \u0641\u064a \u0645\u0643\u0627\u0646\u0647.<\/li>\n\n<li><strong>\u0627\u0644\u062e\u0637\u0627\u0641\u0627\u062a \u0648\u0627\u0644\u0627\u0646\u062d\u0646\u0627\u0621\u0627\u062a<\/strong>:\u0625\u0646 \u062b\u0646\u064a \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0648\u062a\u062b\u0628\u064a\u062a\u0647\u0627 \u0641\u064a \u0627\u0644\u0623\u0637\u0631\u0627\u0641 \u064a\u0624\u062f\u064a \u0625\u0644\u0649 \u062d\u0628\u0633\u0647\u0627 \u062f\u0627\u062e\u0644 \u0627\u0644\u062e\u0631\u0633\u0627\u0646\u0629\u060c \u0648\u0627\u0644\u0627\u0633\u062a\u0641\u0627\u062f\u0629 \u0645\u0646 \u0642\u0648\u062a\u0647\u0627 \u0627\u0644\u0627\u0646\u0636\u063a\u0627\u0637\u064a\u0629 \u0644\u0645\u0646\u0639 \u0627\u0646\u0633\u062d\u0627\u0628\u0647\u0627.<\/li>\n\n<li><strong>\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u0631\u0643\u0627\u0626\u0628 \u0648\u0627\u0644\u0631\u0648\u0627\u0628\u0637<\/strong>:\u0625\u0646 \u0625\u0636\u0627\u0641\u0629 \u0627\u0644\u0631\u0643\u0627\u0626\u0628 \u0648\u0627\u0644\u0631\u0648\u0627\u0628\u0637 \u062d\u0648\u0644 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u062a\u0639\u0645\u0644 \u0639\u0644\u0649 \u0632\u064a\u0627\u062f\u0629 \u0627\u0644\u0627\u062d\u062a\u062c\u0627\u0632 \u0648\u062a\u0648\u0632\u064a\u0639 \u0627\u0644\u0623\u062d\u0645\u0627\u0644 \u0628\u0634\u0643\u0644 \u0623\u0643\u062b\u0631 \u062a\u0648\u0627\u0632\u0646\u0627\u064b\u060c \u0645\u0645\u0627 \u064a\u0642\u0644\u0644 \u0645\u0646 \u062e\u0637\u0631 \u0627\u0644\u0627\u0646\u0632\u0644\u0627\u0642.<\/li>\n\n<li><strong>\u0637\u0644\u0627\u0621 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d<\/strong>:\u064a\u0645\u0643\u0646 \u0623\u0646 \u064a\u0624\u062f\u064a \u062a\u0637\u0628\u064a\u0642 \u0627\u0644\u0645\u0639\u0627\u0644\u062c\u0627\u062a \u0627\u0644\u0633\u0637\u062d\u064a\u0629 \u0645\u062b\u0644 \u0627\u0644\u0637\u0644\u0627\u0621\u0627\u062a \u0627\u0644\u0625\u064a\u0628\u0648\u0643\u0633\u064a \u0625\u0644\u0649 \u062a\u062d\u0633\u064a\u0646 \u0627\u0644\u062a\u0631\u0627\u0628\u0637 \u0645\u0639 \u0627\u0644\u062e\u0631\u0633\u0627\u0646\u0629 \u0648\u062a\u0639\u0632\u064a\u0632 \u0627\u0644\u0642\u0628\u0636\u0629.<\/li><\/ol><p class=\"wp-block-paragraph\">\u062a\u0633\u0627\u0639\u062f \u0643\u0644 \u0637\u0631\u064a\u0642\u0629 \u0639\u0644\u0649 \u0636\u0645\u0627\u0646 \u0628\u0642\u0627\u0621 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0645\u062b\u0628\u062a\u064b\u0627 \u0628\u0634\u0643\u0644 \u0622\u0645\u0646\u060c \u0645\u0645\u0627 \u064a\u0645\u0646\u0639 \u062d\u062f\u0648\u062b \u0623\u0639\u0637\u0627\u0644 \u0647\u064a\u0643\u0644\u064a\u0629.<\/p><h2 class=\"wp-block-heading\">\u0643\u064a\u0641 \u064a\u062a\u0639\u0627\u0645\u0644 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0645\u0639 \u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u0645\u0633\u0628\u0628\u0629 \u0644\u0644\u062a\u0622\u0643\u0644<\/h2><p class=\"wp-block-paragraph\">\u0641\u064a \u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0634\u062f\u064a\u062f\u0629 \u0627\u0644\u062a\u0622\u0643\u0644\u060c \u0645\u062b\u0644 \u0627\u0644\u062c\u0633\u0648\u0631 \u0627\u0644\u0645\u0639\u0631\u0636\u0629 \u0644\u0645\u0644\u062d \u0627\u0644\u0637\u0631\u064a\u0642 \u0623\u0648 \u0627\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0628\u062d\u0631\u064a\u0629\u060c \u064a\u0645\u0643\u0646 \u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u062e\u064a\u0627\u0631\u0627\u062a \u0645\u062e\u062a\u0644\u0641\u0629 \u0645\u0646 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0644\u0645\u0643\u0627\u0641\u062d\u0629 \u0627\u0644\u062a\u0622\u0643\u0644:<\/p><ol class=\"wp-block-list\"><li><strong>\u0633\u0628\u0627\u0626\u0643 \u063a\u064a\u0631 \u0645\u0637\u0644\u064a\u0629 \u0645\u0642\u0627\u0648\u0645\u0629 \u0644\u0644\u062a\u0622\u0643\u0644<\/strong>:\u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0645\u0631\u0643\u0628 \u0627\u0644\u062f\u0642\u064a\u0642 \u0645\u0646\u062e\u0641\u0636 \u0627\u0644\u0643\u0631\u0628\u0648\u0646\/\u0627\u0644\u0643\u0631\u0648\u0645.<\/li>\n\n<li><strong>\u0628\u0631\u0648\u0646\u0632 \u0627\u0644\u0633\u064a\u0644\u064a\u0643\u0648\u0646<\/strong>:\u064a\u0648\u0641\u0631 \u0645\u0642\u0627\u0648\u0645\u0629 \u0645\u0645\u062a\u0627\u0632\u0629 \u0644\u0644\u062a\u0622\u0643\u0644.<\/li>\n\n<li><strong>\u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0645\u063a\u0637\u0649 \u0628\u0627\u0644\u0625\u064a\u0628\u0648\u0643\u0633\u064a<\/strong>:\u064a\u062d\u0645\u064a \u0645\u0646 \u0627\u0644\u0631\u0637\u0648\u0628\u0629 \u0648\u0627\u0644\u062a\u0639\u0631\u0636 \u0644\u0644\u0623\u0645\u0644\u0627\u062d.<\/li>\n\n<li><strong>\u0627\u0644\u062d\u0645\u0627\u064a\u0629 \u0627\u0644\u0643\u0627\u062b\u0648\u062f\u064a\u0629<\/strong>:\u064a\u0645\u0646\u0639 \u0627\u0644\u062a\u0622\u0643\u0644 \u0645\u0646 \u062e\u0644\u0627\u0644 \u0627\u0644\u0637\u0631\u0642 \u0627\u0644\u0643\u0647\u0631\u0648\u0643\u064a\u0645\u064a\u0627\u0626\u064a\u0629.<\/li>\n\n<li><strong>\u0645\u062c\u0644\u0641\u0646 \u0623\u0648 \u0641\u0648\u0644\u0627\u0630 \u0645\u0642\u0627\u0648\u0645 \u0644\u0644\u0635\u062f\u0623<\/strong>:\u0623\u0643\u062b\u0631 \u062a\u0643\u0644\u0641\u0629 \u0641\u064a \u0627\u0644\u0628\u062f\u0627\u064a\u0629\u060c \u0644\u0643\u0646\u0647 \u064a\u0642\u0644\u0644 \u0628\u0634\u0643\u0644 \u0643\u0628\u064a\u0631 \u0645\u0646 \u062a\u0643\u0627\u0644\u064a\u0641 \u0627\u0644\u0635\u064a\u0627\u0646\u0629 \u0639\u0644\u0649 \u0627\u0644\u0645\u062f\u0649 \u0627\u0644\u0637\u0648\u064a\u0644.<\/li><\/ol><h2 class=\"wp-block-heading\">\u0647\u0644 \u062a\u062d\u062a\u0627\u062c \u0625\u0644\u0649 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0644\u0644\u0645\u0645\u0631 \u0627\u0644\u0630\u064a \u064a\u0628\u0644\u063a \u0639\u0631\u0636\u0647 4 \u0628\u0648\u0635\u0627\u062a\u061f\u00a0<\/h2><p class=\"wp-block-paragraph\">\u0646\u0639\u0645\u060c \u0644\u0627 \u062a\u0643\u0648\u0646 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0645\u0637\u0644\u0648\u0628\u0629 \u0639\u0627\u062f\u0629\u064b \u0644\u0645\u0645\u0631\u0627\u062a \u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a \u0627\u0644\u062a\u064a \u064a\u0628\u0644\u063a \u0633\u0645\u0643\u0647\u0627 4 \u0628\u0648\u0635\u0627\u062a\u060c \u062d\u064a\u062b \u0625\u0646 \u0645\u0645\u0631\u0627\u062a \u0627\u0644\u0633\u064a\u0627\u0631\u0627\u062a \u0628\u0647\u0630\u0627 \u0627\u0644\u0633\u0645\u0643 \u0644\u0627 \u062a\u062a\u0639\u0631\u0636 \u0639\u0627\u062f\u0629\u064b \u0644\u0636\u063a\u0637 \u0647\u064a\u0643\u0644\u064a \u0643\u0628\u064a\u0631 \u0645\u0646 \u0634\u0623\u0646\u0647 \u0623\u0646 \u064a\u0633\u062a\u0644\u0632\u0645 \u0627\u0644\u062a\u0639\u0632\u064a\u0632 \u0628\u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d.<\/p><h2 class=\"wp-block-heading\">\u0645\u0627 \u0647\u0648 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0645\u0646 \u0627\u0644\u0646\u0648\u0639 1 \u0648\u0627\u0644\u0646\u0648\u0639 2\u061f&nbsp;<\/h2><p class=\"wp-block-paragraph\">\u0627\u0644\u0646\u0648\u0639 \u0627\u0644\u0623\u0648\u0644 \u0645\u0646 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0647\u0648 \u0639\u0628\u0627\u0631\u0629 \u0639\u0646 \u0642\u0636\u0628\u0627\u0646 \u0645\u0633\u062a\u062f\u064a\u0631\u0629 \u0639\u0627\u062f\u064a\u0629\u060c \u0641\u064a \u062d\u064a\u0646 \u0623\u0646 \u0627\u0644\u0646\u0648\u0639 \u0627\u0644\u062b\u0627\u0646\u064a \u0645\u0646 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u064a\u062d\u062a\u0648\u064a \u0639\u0644\u0649 \u062a\u0634\u0648\u0647\u0627\u062a \u0645\u0646 \u0623\u062c\u0644 \u0627\u0644\u062a\u0635\u0627\u0642 \u0623\u0641\u0636\u0644 \u0628\u0627\u0644\u062e\u0631\u0633\u0627\u0646\u0629.<\/p><h2 class=\"wp-block-heading\">\u0645\u0627 \u0647\u0648 \u0627\u0644\u0641\u0631\u0642 \u0628\u064a\u0646 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0645\u0646 \u0627\u0644\u062f\u0631\u062c\u0629 75 \u0648\u0627\u0644\u062f\u0631\u062c\u0629 60\u061f\u00a0<\/h2><p class=\"wp-block-paragraph\">\u062a\u0639\u062a\u0628\u0631 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0645\u0646 \u0627\u0644\u062f\u0631\u062c\u0629 75 \u0623\u0642\u0648\u0649 \u0645\u0646 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0645\u0646 \u0627\u0644\u062f\u0631\u062c\u0629 60\u060c \u0645\u0645\u0627 \u064a\u0648\u0641\u0631 \u0642\u0648\u0629 \u0634\u062f \u0623\u0639\u0644\u0649 \u0644\u0644\u062a\u0637\u0628\u064a\u0642\u0627\u062a \u0627\u0644\u0623\u0643\u062b\u0631 \u062a\u0637\u0644\u0628\u064b\u0627.<\/p><h2 class=\"wp-block-heading\">\u0645\u062a\u0649 \u064a\u062c\u0628 \u0639\u0644\u064a\u0651 \u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d\u061f<\/h2><p class=\"wp-block-paragraph\">\u064a\u062a\u0645 \u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0639\u0627\u062f\u0629 \u0644\u062a\u0642\u0648\u064a\u0629 \u0627\u0644\u062e\u0631\u0633\u0627\u0646\u0629 \u0641\u064a \u0627\u0644\u0645\u0646\u0627\u0637\u0642 \u0627\u0644\u0645\u0639\u0631\u0636\u0629 \u0644\u0644\u062a\u0634\u0642\u0642 \u0623\u0648 \u0627\u0644\u0625\u062c\u0647\u0627\u062f \u0627\u0644\u0647\u064a\u0643\u0644\u064a\u060c \u0645\u062b\u0644 \u0627\u0644\u0645\u0645\u0631\u0627\u062a\u060c \u0648\u0627\u0644\u0623\u0633\u0627\u0633\u0627\u062a\u060c \u0648\u0627\u0644\u0639\u0648\u0627\u0631\u0636 \u0627\u0644\u0647\u064a\u0643\u0644\u064a\u0629.<\/p><h2 class=\"wp-block-heading\">\u0645\u0627 \u0627\u0644\u0641\u0631\u0642 \u0628\u064a\u0646 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0648\u0627\u0644\u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630\u064a\u0629\u061f<\/h2><p class=\"wp-block-paragraph\">\u0642\u0636\u064a\u0628 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0647\u0648 \u0642\u0636\u064a\u0628 \u0641\u0648\u0644\u0627\u0630\u064a \u0623\u0648 \u0634\u0631\u064a\u0637 \u0641\u0648\u0644\u0627\u0630\u064a \u0628\u0623\u0634\u0643\u0627\u0644 \u0648\u0623\u062d\u062c\u0627\u0645 \u0645\u062e\u062a\u0644\u0641\u0629 \u064a\u0633\u062a\u062e\u062f\u0645 \u0641\u064a \u0627\u0644\u0628\u0646\u0627\u0621 \u0648\u0627\u0644\u062a\u0635\u0646\u064a\u0639 \u0648\u0627\u0644\u0635\u0646\u0627\u0639\u0629. \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0647\u0648 \u0646\u0648\u0639 \u0645\u062d\u062f\u062f \u0645\u0646 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0627\u0644\u0645\u0635\u0645\u0645\u0629 \u0644\u062a\u0642\u0648\u064a\u0629 \u0627\u0644\u0647\u064a\u0627\u0643\u0644 \u0627\u0644\u062e\u0631\u0633\u0627\u0646\u064a\u0629. \u0641\u064a \u062d\u064a\u0646 \u0623\u0646 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u064a\u0642\u0648\u064a \u0627\u0644\u062e\u0631\u0633\u0627\u0646\u0629\u060c \u0641\u0625\u0646 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0644\u0647\u0627 \u0627\u0633\u062a\u062e\u062f\u0627\u0645\u0627\u062a \u0623\u0648\u0633\u0639. \u0642\u0645 \u0628\u0632\u064a\u0627\u0631\u0629 \u0645\u0648\u0642\u0639 SteelPRO Group <a href=\"https:\/\/steelprogroup.com\/ar\/steel-bar\/\">\u0635\u0641\u062d\u0629 \u0634\u0631\u064a\u0637 \u0627\u0644\u0641\u0648\u0644\u0627\u0630<\/a> \u0644\u0645\u0632\u064a\u062f \u0645\u0646 \u0627\u0644\u062a\u0641\u0627\u0635\u064a\u0644.<\/p><h2 class=\"wp-block-heading\">\u0627\u0644\u062a\u0642\u0627\u0637 \u0627\u0644\u0627\u062a\u062c\u0627\u0647\u0627\u062a \u0627\u0644\u0645\u0633\u062a\u0642\u0628\u0644\u064a\u0629 \u0641\u064a \u062a\u0643\u0646\u0648\u0644\u0648\u062c\u064a\u0627 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d<\/h2><p class=\"wp-block-paragraph\"><strong>\u0627\u0644\u0645\u0648\u0627\u062f \u0627\u0644\u0645\u062a\u0642\u062f\u0645\u0629<\/strong>:\u062a\u062a\u0636\u0645\u0646 \u0627\u0644\u0627\u062a\u062c\u0627\u0647\u0627\u062a \u0627\u0644\u0645\u0633\u062a\u0642\u0628\u0644\u064a\u0629 \u0641\u064a \u0645\u062c\u0627\u0644 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u062a\u062d\u0633\u064a\u0646 \u0627\u0644\u0633\u0628\u0627\u0626\u0643 \u0648\u0627\u0644\u0645\u0631\u0643\u0628\u0627\u062a \u0644\u062a\u062d\u0642\u064a\u0642 \u0646\u0633\u0628\u0629 \u0623\u0641\u0636\u0644 \u0628\u064a\u0646 \u0627\u0644\u0642\u0648\u0629 \u0648\u0627\u0644\u0648\u0632\u0646 \u0648\u0645\u0642\u0627\u0648\u0645\u0629 \u0627\u0644\u062a\u0622\u0643\u0644.<\/p><p class=\"wp-block-paragraph\"><strong>\u0627\u0644\u0627\u0633\u062a\u062f\u0627\u0645\u0629<\/strong>:\u0647\u0646\u0627\u0643 \u062a\u062d\u0648\u0644 \u0646\u062d\u0648 \u0627\u0633\u062a\u062e\u062f\u0627\u0645 \u0627\u0644\u0645\u0648\u0627\u062f \u0627\u0644\u0645\u0639\u0627\u062f \u062a\u062f\u0648\u064a\u0631\u0647\u0627 \u0648\u062a\u0642\u0644\u064a\u0644 \u0627\u0644\u0628\u0635\u0645\u0629 \u0627\u0644\u0643\u0631\u0628\u0648\u0646\u064a\u0629 \u0641\u064a \u0625\u0646\u062a\u0627\u062c \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d.<\/p><p class=\"wp-block-paragraph\"><strong>\u0627\u0644\u0637\u0644\u0627\u0621\u0627\u062a<\/strong>:\u062a\u0632\u062f\u0627\u062f \u0634\u0639\u0628\u064a\u0629 \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0627\u0644\u0645\u063a\u0644\u0641\u0629 \u0628\u0627\u0644\u0625\u064a\u0628\u0648\u0643\u0633\u064a \u0648\u0627\u0644\u0645\u062c\u0644\u0641\u0646\u0629 \u0628\u0634\u0643\u0644 \u0645\u062a\u0632\u0627\u064a\u062f \u0628\u0633\u0628\u0628 \u0645\u062a\u0627\u0646\u062a\u0647\u0627 \u0641\u064a \u0627\u0644\u0628\u064a\u0626\u0627\u062a \u0627\u0644\u0645\u0633\u0628\u0628\u0629 \u0644\u0644\u062a\u0622\u0643\u0644.<\/p><p class=\"wp-block-paragraph\"><strong>\u062a\u0643\u0646\u0648\u0644\u0648\u062c\u064a\u0627<\/strong>:\u0625\u0646 \u0627\u0644\u0627\u0628\u062a\u0643\u0627\u0631\u0627\u062a \u0645\u062b\u0644 \u0627\u0644\u062a\u062a\u0628\u0639 \u0627\u0644\u0631\u0642\u0645\u064a \u0648\u0623\u062c\u0647\u0632\u0629 \u0627\u0644\u0627\u0633\u062a\u0634\u0639\u0627\u0631 \u062a\u0639\u0645\u0644 \u0639\u0644\u0649 \u062a\u062d\u0633\u064a\u0646 \u0645\u0631\u0627\u0642\u0628\u0629 \u0627\u0644\u062c\u0648\u062f\u0629 \u0623\u062b\u0646\u0627\u0621 \u0625\u0646\u062a\u0627\u062c \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0648\u062a\u0631\u0643\u064a\u0628\u0647.<\/p><p class=\"wp-block-paragraph\"><a href=\"https:\/\/steelprogroup.com\/ar\">\u0645\u062c\u0645\u0648\u0639\u0629 \u0633\u062a\u064a\u0644\u0628\u0631\u0648<\/a> \u062a\u0642\u062f\u0645 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0639\u0627\u0644\u064a \u0627\u0644\u062c\u0648\u062f\u0629 \u0644\u0644\u062e\u0631\u0633\u0627\u0646\u0629 \u0648\u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0644\u0644\u0628\u0646\u0627\u0621 \u0648\u0627\u0644\u0630\u064a \u064a\u0636\u0645\u0646 \u0645\u062a\u0627\u0646\u0629 \u0648\u0645\u0631\u0648\u0646\u0629 \u0645\u0634\u0627\u0631\u064a\u0639 \u0627\u0644\u0628\u0646\u0627\u0621 \u0627\u0644\u062e\u0627\u0635\u0629 \u0628\u0643 \u0645\u0639 \u0627\u0644\u062a\u0648\u0627\u0641\u0642 \u0645\u0639 \u0623\u0647\u062f\u0627\u0641 \u0627\u0644\u062a\u0646\u0645\u064a\u0629 \u0627\u0644\u0645\u0633\u062a\u062f\u0627\u0645\u0629. \u0644\u0645\u0632\u064a\u062f \u0645\u0646 \u0627\u0644\u0645\u0639\u0644\u0648\u0645\u0627\u062a \u062d\u0648\u0644 \u062f\u0648\u0631 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d \u0641\u064a \u0628\u0646\u0627\u0621 \u0645\u0633\u062a\u0642\u0628\u0644 \u0645\u0631\u0646 \u0648\u0648\u0627\u0639\u064a \u0628\u0627\u0644\u0628\u064a\u0626\u0629\u060c <a href=\"https:\/\/steelprogroup.com\/ar\/blog\/\">\u064a\u0631\u062c\u0649 \u0632\u064a\u0627\u0631\u0629 \u0635\u0641\u062d\u0629 \u0645\u062f\u0648\u0646\u062a\u0646\u0627<\/a>. <a href=\"https:\/\/steelprogroup.com\/ar\/contact-us\/\">\u0627\u062a\u0635\u0644 \u0628\u0646\u0627 \u0627\u0644\u064a\u0648\u0645<\/a> \u0644\u062a\u0642\u062f\u064a\u0645 \u0637\u0644\u0628\u0643 \u0648\u0627\u0644\u0627\u0646\u0636\u0645\u0627\u0645 \u0625\u0644\u064a\u0646\u0627 \u0641\u064a \u0647\u0630\u0647 \u0627\u0644\u0631\u062d\u0644\u0629 \u0627\u0644\u0645\u0633\u062a\u062f\u0627\u0645\u0629!<\/p><p class=\"wp-block-paragraph\"><\/p>","protected":false},"excerpt":{"rendered":"<p>\u062a\u062a\u0648\u0627\u062c\u062f \u0642\u0636\u0628\u0627\u0646 \u0627\u0644\u0641\u0648\u0644\u0627\u0630 \u0641\u064a \u0643\u0644 \u0645\u0643\u0627\u0646 \u0641\u064a \u062d\u064a\u0627\u062a\u0646\u0627\u060c \u0648\u0644\u0643\u0646 \u0646\u0627\u062f\u0631\u064b\u0627 \u0645\u0627 \u0646\u0631\u0649 \u062d\u062f\u064a\u062f \u0627\u0644\u062a\u0633\u0644\u064a\u062d. \u0648\u0630\u0644\u0643 \u0644\u0623\u0646\u0647 \u0639\u0646\u0635\u0631 \u0623\u0633\u0627\u0633\u064a \u0641\u064a [\u2026]<\/p>","protected":false},"author":1,"featured_media":7832,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"_eb_attr":"","rank_math_lock_modified_date":false,"site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"categories":[111],"tags":[4275],"class_list":["post-7833","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-steel-bar","tag-featured"],"acf":[],"_links":{"self":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts\/7833","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/comments?post=7833"}],"version-history":[{"count":0,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/posts\/7833\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/media\/7832"}],"wp:attachment":[{"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/media?parent=7833"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/categories?post=7833"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/steelprogroup.com\/ar\/wp-json\/wp\/v2\/tags?post=7833"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}