{"id":10946,"date":"2024-09-30T05:14:00","date_gmt":"2024-09-29T21:14:00","guid":{"rendered":"https:\/\/app11147.cloudwayssites.com\/?p=10946"},"modified":"2024-09-30T13:10:06","modified_gmt":"2024-09-30T05:10:06","slug":"production","status":"publish","type":"post","link":"https:\/\/steelprogroup.com\/ja\/stainless-steel\/production\/","title":{"rendered":"\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u751f\u7523"},"content":{"rendered":"<p class=\"wp-block-paragraph\">\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u3001\u3055\u307e\u3056\u307e\u306a\u72b6\u6cc1\u3067\u9ad8\u3044\u8010\u8150\u98df\u6027\u3001\u9577\u671f\u306b\u308f\u305f\u308b\u8010\u4e45\u6027\u3001\u6700\u5c0f\u9650\u306e\u30e1\u30f3\u30c6\u30ca\u30f3\u30b9\u306e\u5fc5\u8981\u6027\u3092\u5099\u3048\u3066\u3044\u307e\u3059\u3002\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u88fd\u9020\u65b9\u6cd5\u3092\u7406\u89e3\u3059\u308b\u3053\u3068\u3067\u3001\u65e5\u5e38\u7684\u306a\u7528\u9014\u306b\u304a\u3051\u308b\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u4fa1\u5024\u3068\u6c4e\u7528\u6027\u3092\u7406\u89e3\u3059\u308b\u3053\u3068\u304c\u3067\u304d\u307e\u3059\u3002\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u88fd\u9020\u65b9\u6cd5\u3092\u6bb5\u968e\u7684\u306b\u898b\u3066\u3044\u304d\u307e\u3057\u3087\u3046\u3002<\/p><h2 class=\"wp-block-heading\">\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u4f55\u304b\u3089\u4f5c\u3089\u308c\u3066\u3044\u308b\u306e\u3067\u3059\u304b?<\/h2><p class=\"wp-block-paragraph\">\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u8907\u6570\u306e\u539f\u6750\u6599\u3092\u6df7\u5408\u3057\u3066\u4f5c\u3089\u308c\u3066\u304a\u308a\u3001\u6b63\u78ba\u306a\u7d44\u6210\u306f\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u7a2e\u985e\u306b\u3088\u3063\u3066\u7570\u306a\u308a\u307e\u3059\u3002&nbsp;<\/p><p class=\"wp-block-paragraph\">\u4ee5\u4e0b\u306f\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u4e3b\u306a\u6210\u5206\u3092\u793a\u3059\u8868\u3067\u3059\u3002<\/p><figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td><strong>\u539f\u6750\u6599<\/strong><\/td><td><strong>\u95a2\u9023\u30d7\u30ed\u30d1\u30c6\u30a3<\/strong><\/td><\/tr><tr><td>\u9244\u9271\u77f3<\/td><td>\u57fa\u790e\u7684\u306a\u5f37\u5ea6\u3068\u69cb\u9020<\/td><\/tr><tr><td>\u30af\u30ed\u30e0<\/td><td>\u8010\u98df\u6027<\/td><\/tr><tr><td>\u30cb\u30c3\u30b1\u30eb<\/td><td>\u5f37\u5ea6\u3001\u67d4\u8edf\u6027\u3001\u8010\u8150\u98df\u6027<\/td><\/tr><tr><td>\u30e2\u30ea\u30d6\u30c7\u30f3<\/td><td>\u5b54\u98df\u304a\u3088\u3073\u9699\u9593\u8150\u98df\u306b\u5bfe\u3059\u308b\u8010\u6027\u3001\u5f37\u5ea6<\/td><\/tr><tr><td>\u30ab\u30fc\u30dc\u30f3<\/td><td>\u8010\u8150\u98df\u6027\u306e\u4f4e\u4e0b<\/td><\/tr><tr><td>\u30de\u30f3\u30ac\u30f3<\/td><td>\u5f37\u5ea6\u3068\u786c\u3055<\/td><\/tr><tr><td>\u30b7\u30ea\u30b3\u30f3<\/td><td>\u5f37\u3055\u3068\u67d4\u8edf\u6027<\/td><\/tr><\/tbody><\/table><\/figure><ul class=\"wp-block-list\"><li>\u5f37\u5ea6\u306e\u5411\u4e0a\u3084\u6eb6\u63a5\u6027\u306e\u6539\u5584\u306a\u3069\u306e\u7279\u5b9a\u306e\u7279\u6027\u3092\u5b9f\u73fe\u3059\u308b\u305f\u3081\u306b\u3001\u7a92\u7d20\u3001\u30c1\u30bf\u30f3\u3001\u9285\u3001\u305d\u306e\u4ed6\u306e\u5143\u7d20\u304c\u6dfb\u52a0\u3055\u308c\u308b\u3053\u3068\u304c\u3042\u308a\u307e\u3059\u3002<\/li><\/ul><h2 class=\"wp-block-heading\">\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u3069\u306e\u3088\u3046\u306b\u4f5c\u3089\u308c\u308b\u306e\u3067\u3057\u3087\u3046\u304b?<\/h2><p class=\"wp-block-paragraph\">\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u88fd\u9020\u306b\u306f\u3001\u3044\u304f\u3064\u304b\u306e\u9023\u7d9a\u3057\u305f\u30b9\u30c6\u30c3\u30d7\u304c\u542b\u307e\u308c\u307e\u3059\u3002\u5404\u6bb5\u968e\u306f\u3001\u6700\u7d42\u88fd\u54c1\u306e\u671b\u307e\u3057\u3044\u54c1\u8cea\u3068\u7279\u6027\u3092\u5b9f\u73fe\u3059\u308b\u305f\u3081\u306b\u975e\u5e38\u306b\u91cd\u8981\u3067\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u88fd\u9020<\/h3><ol class=\"wp-block-list\"><li>\u6eb6\u89e3\u3068\u92f3\u9020<\/li><\/ol><p class=\"wp-block-paragraph\">\u9244\u9271\u77f3\u3001\u30af\u30ed\u30e0\u3001\u30cb\u30c3\u30b1\u30eb\u306a\u3069\u306e\u539f\u6750\u6599\u3092\u96fb\u6c17\u30a2\u30fc\u30af\u7089\u306b\u6295\u5165\u3057\u307e\u3059\u3002\u7089\u306f\u6df7\u5408\u7269\u3092\u7d041,600\u2103\u306b\u52a0\u71b1\u3057\u307e\u3059\u3002\u6eb6\u3051\u308b\u3068\u3001\u3053\u308c\u3089\u306e\u6750\u6599\u304c\u7d50\u5408\u3057\u3066\u6eb6\u878d\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u3092\u5f62\u6210\u3057\u307e\u3059\u3002<\/p><ol start=\"2\" class=\"wp-block-list\"><li>\u8131\u70ad<\/li><\/ol><ul class=\"wp-block-list\"><li>\u30a2\u30eb\u30b4\u30f3\u9178\u7d20\u8131\u70ad\uff08AOD\uff09<\/li><\/ul><p class=\"wp-block-paragraph\">\u6eb6\u92fc\u3092 AOD \u5bb9\u5668\u306b\u79fb\u3057\u307e\u3059\u3002\u9178\u7d20\u3068\u30a2\u30eb\u30b4\u30f3\u306e\u30ac\u30b9\u304c\u6ce8\u5165\u3055\u308c\u307e\u3059\u3002\u9178\u7d20\u306f\u4e00\u9178\u5316\u70ad\u7d20\u30ac\u30b9\u3092\u5f62\u6210\u3057\u3066\u4f59\u5206\u306a\u70ad\u7d20\u3092\u9664\u53bb\u3057\u307e\u3059\u3002\u30a2\u30eb\u30b4\u30f3\u306f\u30ac\u30b9\u6df7\u5408\u7269\u3092\u5e0c\u91c8\u3057\u3066\u53cd\u5fdc\u901f\u5ea6\u3092\u5236\u5fa1\u3057\u307e\u3059\u3002&nbsp;<\/p><p class=\"wp-block-paragraph\">AOD \u306f\u307b\u3068\u3093\u3069\u306e\u30a2\u30d7\u30ea\u30b1\u30fc\u30b7\u30e7\u30f3\u306b\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u771f\u7a7a\u9178\u7d20\u8131\u70ad(VOD)<\/li><\/ul><p class=\"wp-block-paragraph\">\u6eb6\u878d\u92fc\u3092\u771f\u7a7a\u30c1\u30e3\u30f3\u30d0\u30fc\u306b\u79fb\u3057\u307e\u3059\u3002\u9178\u7d20\u3092\u6ce8\u5165\u3057\u3066\u70ad\u7d20\u3068\u53cd\u5fdc\u3055\u305b\u3001\u4e00\u9178\u5316\u70ad\u7d20\u30ac\u30b9\u3092\u5f62\u6210\u3057\u3001\u4f4e\u5727\u3067\u9664\u53bb\u3057\u307e\u3059\u3002&nbsp;<\/p><p class=\"wp-block-paragraph\">VOD \u306f\u3001304L \u306a\u3069\u306e\u9ad8\u7d1a\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306b\u6975\u4f4e\u70ad\u7d20\u542b\u6709\u91cf\u304c\u5fc5\u8981\u306a\u5834\u5408\u306b\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u70ad\u7d20\u542b\u6709\u91cf\u3092\u6e1b\u3089\u3059\u3053\u3068\u3067\u3001\u30e1\u30fc\u30ab\u30fc\u306f 304L \u3084 316L \u306a\u3069\u306e\u4f4e\u70ad\u7d20\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u3092\u88fd\u9020\u3057\u307e\u3059\u3002\u3053\u308c\u3089\u306e\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u6eb6\u63a5\u6027\u304c\u5411\u4e0a\u3057\u3001\u8150\u98df\u306e\u30ea\u30b9\u30af\u304c\u8efd\u6e1b\u3055\u308c\u307e\u3059\u3002<\/li><\/ul><ol start=\"3\" class=\"wp-block-list\"><li>\u69cb\u6210\u306e\u8abf\u6574<\/li><\/ol><p class=\"wp-block-paragraph\">\u30cb\u30c3\u30b1\u30eb\u3001\u30e2\u30ea\u30d6\u30c7\u30f3\u3001\u7a92\u7d20\u306a\u3069\u306e\u8ffd\u52a0\u5143\u7d20\u306f\u3001\u671b\u307e\u3057\u3044\u92fc\u306e\u7b49\u7d1a\u306b\u5fdc\u3058\u3066\u3001\u5f37\u5ea6\u3001\u67d4\u8edf\u6027\u3001\u8010\u8150\u98df\u6027\u3092\u9ad8\u3081\u308b\u305f\u3081\u306b\u6dfb\u52a0\u3055\u308c\u307e\u3059\u3002\u3053\u308c\u3089\u306e\u5143\u7d20\u306f\u6eb6\u878d\u92fc\u306b\u6eb6\u89e3\u3057\u3001\u305d\u306e\u7279\u6027\u3092\u5909\u3048\u307e\u3059\u3002<\/p><ol start=\"4\" class=\"wp-block-list\"><li>\u30ad\u30e3\u30b9\u30c6\u30a3\u30f3\u30b0<\/li><\/ol><p class=\"wp-block-paragraph\">\u6eb6\u3051\u305f\u92fc\u3092\u92f3\u578b\u306b\u79fb\u3057\u3001\u51dd\u56fa\u3055\u305b\u307e\u3059\u3002\u92f3\u9020\u4e2d\u306f\u51b7\u5374\u3055\u308c\u307e\u3059\u304c\u30011,200 \u5ea6\u4ee5\u4e0a\u306e\u6e29\u5ea6\u304c\u4fdd\u305f\u308c\u307e\u3059\u3002\u92f3\u9020\u4e2d\u306b\u751f\u6210\u3055\u308c\u308b\u5f62\u72b6\u306b\u3088\u3063\u3066\u3001\u677f\u3084\u68d2\u306a\u3069\u306e\u6700\u7d42\u88fd\u54c1\u306e\u5f62\u304c\u6c7a\u307e\u308a\u307e\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u30b9\u30e9\u30d6: \u30d7\u30ec\u30fc\u30c8\u3084\u30b7\u30fc\u30c8\u3092\u4f5c\u308b\u306e\u306b\u4f7f\u7528\u3057\u307e\u3059\u3002<\/li>\n\n<li>\u30d3\u30ec\u30c3\u30c8: \u68d2\u3084\u7dda\u6750\u306e\u88fd\u9020\u306b\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/li>\n\n<li>\u30d6\u30eb\u30fc\u30e0: \u69cb\u9020\u7684\u306a\u5f62\u72b6\u306b\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u52a0\u5de5<\/h3><ol class=\"wp-block-list\"><li>\u6210\u5f62<\/li><\/ol><ul class=\"wp-block-list\"><li>\u71b1\u9593\u5727\u5ef6<\/li><\/ul><p class=\"wp-block-paragraph\">\u534a\u5b8c\u6210\u92fc\u6750\u306f\u7d04 1,200 \u5ea6\u306b\u518d\u52a0\u71b1\u3055\u308c\u3001\u30ed\u30fc\u30e9\u30fc\u306b\u901a\u3055\u308c\u307e\u3059\u3002\u539a\u3055\u3092\u6e1b\u3089\u3057\u3001\u92fc\u6750\u3092\u30d7\u30ec\u30fc\u30c8\u3001\u30b7\u30fc\u30c8\u3001\u30b3\u30a4\u30eb\u3001\u30d0\u30fc\u3001\u307e\u305f\u306f\u30ef\u30a4\u30e4\u306b\u6210\u5f62\u3057\u307e\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u51b7\u9593\u5727\u5ef6<\/li><\/ul><p class=\"wp-block-paragraph\">\u92fc\u3092\u5ba4\u6e29\u3067\u5727\u5ef6\u3057\u307e\u3059\u3002\u3053\u308c\u306b\u3088\u308a\u3001\u6b63\u78ba\u306a\u5bf8\u6cd5\u304c\u9054\u6210\u3055\u308c\u3001\u8868\u9762\u4ed5\u4e0a\u3052\u304c\u5411\u4e0a\u3057\u307e\u3059\u3002\u92fc\u306f\u3072\u305a\u307f\u786c\u5316\u306b\u3088\u3063\u3066\u5f37\u5ea6\u304c\u5897\u3057\u307e\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u71b1\u9593\u5727\u5ef6\u306f\u3001\u30aa\u30fc\u30b9\u30c6\u30ca\u30a4\u30c8\u92fc\u3001\u30d5\u30a7\u30e9\u30a4\u30c8\u92fc\u3001\u4e8c\u76f8\u92fc\u306b\u9069\u3057\u3066\u3044\u307e\u3059\u3002\u51b7\u9593\u5727\u5ef6\u306f\u3001\u7279\u306b\u8868\u9762\u4ed5\u4e0a\u3052\u3068\u6b63\u78ba\u306a\u5bf8\u6cd5\u304c\u91cd\u8981\u306a\u5834\u5408\u3001\u30aa\u30fc\u30b9\u30c6\u30ca\u30a4\u30c8\u92fc\u3068\u30de\u30eb\u30c6\u30f3\u30b5\u30a4\u30c8\u92fc\u306b\u6700\u9069\u3067\u3059\u3002<\/li><\/ul><ol start=\"2\" class=\"wp-block-list\"><li>\u71b1\u51e6\u7406<\/li><\/ol><ul class=\"wp-block-list\"><li>\u30a2\u30cb\u30fc\u30ea\u30f3\u30b0<\/li><\/ul><p class=\"wp-block-paragraph\">\u9069\u7528\u92fc\u6750: \u30aa\u30fc\u30b9\u30c6\u30ca\u30a4\u30c8\u7cfb\u3001\u30d5\u30a7\u30e9\u30a4\u30c8\u7cfb\u3001\u4e8c\u76f8\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u3002<\/p><p class=\"wp-block-paragraph\">\u92fc\u306f 1,040\u00b0C \uff5e 1,120\u00b0C \u7a0b\u5ea6\u306b\u52a0\u71b1\u3055\u308c\u3001\u3086\u3063\u304f\u308a\u3068\u51b7\u5374\u3055\u308c\u3066\u5fdc\u529b\u304c\u7de9\u548c\u3055\u308c\u3001\u5ef6\u6027\u304c\u5411\u4e0a\u3057\u307e\u3059\u3002\u3053\u306e\u30d7\u30ed\u30bb\u30b9\u306b\u3088\u308a\u3001\u92fc\u306f\u67d4\u3089\u304b\u304f\u306a\u308a\u3001\u6210\u5f62\u6027\u3068\u8010\u8150\u98df\u6027\u304c\u5411\u4e0a\u3057\u307e\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u713c\u304d\u5165\u308c<\/li><\/ul><p class=\"wp-block-paragraph\">\u9069\u7528\u92fc\u6750: \u30aa\u30fc\u30b9\u30c6\u30ca\u30a4\u30c8\u7cfb\u304a\u3088\u3073\u4e8c\u76f8\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u3002<\/p><p class=\"wp-block-paragraph\">\u9ad8\u6e29\u306b\u52a0\u71b1\u3057\u3001\u305d\u306e\u5f8c\u3001\u30af\u30ed\u30e0\u70ad\u5316\u7269\u306e\u5f62\u6210\u3092\u9632\u3050\u305f\u3081\u306b\u6025\u901f\u306b\u51b7\u5374\uff08\u713c\u5165\u308c\uff09\u3057\u307e\u3059\u3002\u713c\u5165\u308c\u306b\u3088\u308a\u8010\u98df\u6027\u304c\u5411\u4e0a\u3057\u3001\u7c92\u754c\u8150\u98df\u304c\u9632\u6b62\u3055\u308c\u307e\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u713c\u304d\u623b\u3057<\/li><\/ul><p class=\"wp-block-paragraph\">\u9069\u7528\u92fc\u6750: 410 \u3084 420 \u306a\u3069\u306e\u30de\u30eb\u30c6\u30f3\u30b5\u30a4\u30c8\u7cfb\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u3002<\/p><p class=\"wp-block-paragraph\">\u92fc\u3092 200\u00b0C \uff5e 600\u00b0C \u306b\u518d\u52a0\u71b1\u3057\u307e\u3059\u3002\u3053\u308c\u306b\u3088\u308a\u8106\u3055\u304c\u8efd\u6e1b\u3055\u308c\u3001\u786c\u5ea6\u304c\u7dad\u6301\u3055\u308c\u307e\u3059\u3002\u3053\u306e\u30d7\u30ed\u30bb\u30b9\u306f\u3001\u786c\u5ea6\u3068\u976d\u6027\u306e\u30d0\u30e9\u30f3\u30b9\u3092\u3068\u308b\u305f\u3081\u306b\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u6790\u51fa\u786c\u5316<\/li><\/ul><p class=\"wp-block-paragraph\">\u9069\u7528\u92fc\u6750: 17-4PH \u306a\u3069\u306e\u6790\u51fa\u786c\u5316\u578b\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u3002<\/p><p class=\"wp-block-paragraph\">\u6eb6\u4f53\u5316\u51e6\u7406\u5f8c\u3001\u92fc\u306f\u6642\u52b9\u51e6\u7406\uff08\u7d04 480\u00b0C \uff5e 620\u00b0C \u306b\u52a0\u71b1\uff09\u3055\u308c\u307e\u3059\u3002\u3053\u306e\u51e6\u7406\u306b\u3088\u308a\u3001\u8010\u98df\u6027\u3092\u640d\u306a\u3046\u3053\u3068\u306a\u304f\u6a5f\u68b0\u7684\u7279\u6027\u304c\u5411\u4e0a\u3057\u307e\u3059\u3002&nbsp;<\/p><ol start=\"3\" class=\"wp-block-list\"><li>\u30b9\u30b1\u30fc\u30eb\u9664\u53bb<\/li><\/ol><p class=\"wp-block-paragraph\">\u71b1\u51e6\u7406\u5f8c\u3001\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u591a\u304f\u306e\u5834\u5408\u3001\u9178\u5316\u30b9\u30b1\u30fc\u30eb\u3067\u8986\u308f\u308c\u307e\u3059\u3002\u30b9\u30b1\u30fc\u30eb\u9664\u53bb\u3067\u306f\u3001\u9178\u6d17\u3044\u307e\u305f\u306f\u30b7\u30e7\u30c3\u30c8\u30d6\u30e9\u30b9\u30c8\u306a\u3069\u306e\u6a5f\u68b0\u7684\u65b9\u6cd5\u3092\u4f7f\u7528\u3057\u3066\u3053\u306e\u30b9\u30b1\u30fc\u30eb\u3092\u9664\u53bb\u3057\u307e\u3059\u3002\u3053\u306e\u30d7\u30ed\u30bb\u30b9\u306b\u3088\u308a\u3001\u305d\u306e\u5f8c\u306e\u52a0\u5de5\u3084\u4ed5\u4e0a\u3052\u306e\u305f\u3081\u306b\u304d\u308c\u3044\u306a\u8868\u9762\u304c\u78ba\u4fdd\u3055\u308c\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u30b9\u30c6\u30f3\u30ec\u30b9\u4ed5\u4e0a\u3052<\/h3><p class=\"wp-block-paragraph\">\u9244\u92fc\u696d\u754c\u3067\u306f\u3001\u6700\u7d42\u88fd\u54c1\u306e\u8868\u9762\u54c1\u8cea\u3001\u5916\u89b3\u3001\u6027\u80fd\u3092\u5411\u4e0a\u3055\u305b\u308b\u305f\u3081\u306b\u4ed5\u4e0a\u3052\u5de5\u7a0b\u304c\u91cd\u8981\u3067\u3059\u3002\u3053\u308c\u3089\u306e\u65b9\u6cd5\u306b\u3088\u308a\u3001\u7cbe\u5ea6\u3068\u8010\u4e45\u6027\u304c\u6c42\u3081\u3089\u308c\u308b\u7528\u9014\u306e\u7279\u5b9a\u306e\u57fa\u6e96\u3092\u9244\u92fc\u304c\u6e80\u305f\u3059\u3053\u3068\u304c\u4fdd\u8a3c\u3055\u308c\u307e\u3059\u3002\u4e00\u822c\u7684\u306a\u4ed5\u4e0a\u3052\u65b9\u6cd5\u306b\u306f\u6b21\u306e\u3082\u306e\u304c\u3042\u308a\u307e\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u7814\u524a\u3068\u7814\u78e8<\/li><\/ul><p class=\"wp-block-paragraph\">\u7814\u524a\u306f\u3001\u50b7\u3084\u3056\u3089\u3056\u3089\u3057\u305f\u30a8\u30c3\u30b8\u306a\u3069\u306e\u8868\u9762\u306e\u6b20\u9665\u3092\u9664\u53bb\u3059\u308b\u3082\u306e\u3067\u3001\u591a\u304f\u306e\u5834\u5408\u3001\u7814\u78e8\u5de5\u5177\u3084\u7814\u524a\u30db\u30a4\u30fc\u30eb\u3092\u4f7f\u7528\u3057\u3066\u884c\u308f\u308c\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\">\u7814\u78e8\u306b\u3088\u308a\u3001\u6ed1\u3089\u304b\u3067\u53cd\u5c04\u6027\u306e\u9ad8\u3044\u8868\u9762\u304c\u751f\u307e\u308c\u307e\u3059\u3002\u3053\u306e\u30d7\u30ed\u30bb\u30b9\u306f\u3001\u3055\u307e\u3056\u307e\u306a\u30b0\u30ec\u30fc\u30c9\u306e\u7814\u78e8\u5264\u3092\u4f7f\u7528\u3057\u3066\u5b9f\u884c\u3059\u308b\u3053\u3068\u3067\u3001\u93e1\u306e\u3088\u3046\u306a\u4ed5\u4e0a\u304c\u308a\u3092\u5b9f\u73fe\u3067\u304d\u307e\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u30d6\u30e9\u30c3\u30b7\u30f3\u30b0<\/li><\/ul><p class=\"wp-block-paragraph\">\u3053\u306e\u65b9\u6cd5\u3067\u306f\u3001\u7814\u78e8\u30d6\u30e9\u30b7\u3092\u4f7f\u7528\u3057\u3066\u92fc\u9244\u306e\u8868\u9762\u306b\u30b5\u30c6\u30f3\u4ed5\u4e0a\u3052\u307e\u305f\u306f\u30de\u30c3\u30c8\u4ed5\u4e0a\u3052\u3092\u65bd\u3057\u307e\u3059\u3002\u6ed1\u3089\u304b\u3067\u3042\u308a\u306a\u304c\u3089\u53cd\u5c04\u3057\u306a\u3044\u4ed5\u4e0a\u3052\u304c\u6c42\u3081\u3089\u308c\u308b\u5bb6\u96fb\u88fd\u54c1\u306a\u3069\u306e\u7528\u9014\u3067\u3088\u304f\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u30d4\u30af\u30eb\u30b9<\/li><\/ul><p class=\"wp-block-paragraph\">\u71b1\u51e6\u7406\u3084\u71b1\u9593\u5727\u5ef6\u306b\u3088\u308b\u9178\u5316\u30b9\u30b1\u30fc\u30eb\u3092\u9664\u53bb\u3059\u308b\u305f\u3081\u306b\u3001\u901a\u5e38\u306f\u785d\u9178\u3068\u30d5\u30c3\u5316\u6c34\u7d20\u9178\u306e\u6df7\u5408\u7269\u3067\u3042\u308b\u9178\u6d74\u306b\u92fc\u3092\u6d78\u3057\u307e\u3059\u3002\u3053\u306e\u30d7\u30ed\u30bb\u30b9\u306b\u3088\u308a\u3001\u92fc\u306e\u8868\u9762\u304c\u5fa9\u5143\u3055\u308c\u3001\u8010\u8150\u98df\u6027\u304c\u5411\u4e0a\u3057\u307e\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u96fb\u89e3\u7814\u78e8<\/li><\/ul><p class=\"wp-block-paragraph\">\u96fb\u6c17\u5316\u5b66\u6d74\u3092\u4f7f\u7528\u3057\u3066\u6750\u6599\u8868\u9762\u306e\u8584\u3044\u5c64\u3092\u9664\u53bb\u3057\u307e\u3059\u3002\u3053\u306e\u30d7\u30ed\u30bb\u30b9\u306b\u3088\u308a\u3001\u92fc\u306e\u5916\u89b3\u304c\u5411\u4e0a\u3057\u3001\u5fae\u7d30\u306a\u7c97\u3055\u304c\u6e1b\u5c11\u3057\u3001\u8010\u8150\u98df\u6027\u304c\u5411\u4e0a\u3057\u307e\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u4e0d\u52d5\u614b\u5316<\/li><\/ul><p class=\"wp-block-paragraph\">\u9178\u6027\u6eb6\u6db2\u3092\u4f7f\u7528\u3057\u3066\u3001\u904a\u96e2\u9244\u3068\u4e0d\u7d14\u7269\u3092\u9664\u53bb\u3057\u3066\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u8868\u9762\u3092\u6d17\u6d44\u3057\u307e\u3059\u3002\u3053\u306e\u30d7\u30ed\u30bb\u30b9\u306b\u3088\u308a\u3001\u4fdd\u8b77\u9178\u5316\u30af\u30ed\u30e0\u5c64\u306e\u5f62\u6210\u304c\u4fc3\u9032\u3055\u308c\u3001\u8010\u8150\u98df\u6027\u304c\u5411\u4e0a\u3057\u307e\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0<\/li><\/ul><p class=\"wp-block-paragraph\">\u3053\u308c\u306b\u3088\u308a\u3001\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u8010\u4e45\u6027\u3001\u8010\u6469\u8017\u6027\u3001\u307e\u305f\u306f\u7f8e\u89b3\u304c\u5411\u4e0a\u3057\u307e\u3059\u3002\u7c89\u4f53\u5857\u88c5\u3001\u4e9c\u925b\u30e1\u30c3\u30ad\u3001\u30e1\u30c3\u30ad\u304c\u4e00\u822c\u7684\u306a\u65b9\u6cd5\u3067\u3059\u3002\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u306e\u7a2e\u985e\u306b\u3088\u3063\u3066\u3001\u4fdd\u8b77\u30ec\u30d9\u30eb\u3084\u88c5\u98fe\u4ed5\u4e0a\u3052\u306e\u30ec\u30d9\u30eb\u304c\u7570\u306a\u308a\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u52a0\u5de5<\/h3><ul start=\"8\" class=\"wp-block-list\"><li>\u30ab\u30c3\u30c6\u30a3\u30f3\u30b0<\/li><\/ul><p class=\"wp-block-paragraph\">\u92fc\u6750\u306f\u3001\u305b\u3093\u65ad\u3001\u92f8\u5f15\u304d\u3001\u30ec\u30fc\u30b6\u30fc\u5207\u65ad\u306a\u3069\u306e\u65b9\u6cd5\u3092\u4f7f\u7528\u3057\u3066\u3001\u7279\u5b9a\u306e\u30b5\u30a4\u30ba\u3068\u5f62\u72b6\u306b\u5207\u65ad\u3055\u308c\u307e\u3059\u3002\u3053\u306e\u30b9\u30c6\u30c3\u30d7\u306e\u7cbe\u5ea6\u306f\u3001\u88fd\u54c1\u4ed5\u69d8\u3092\u6e80\u305f\u3059\u305f\u3081\u306b\u4e0d\u53ef\u6b20\u3067\u3059\u3002<\/p><p class=\"wp-block-paragraph\"><strong>\u95a2\u9023\u8a18\u4e8b<\/strong><\/p><p class=\"wp-block-paragraph\"><a href=\"https:\/\/steelprogroup.com\/ja\/stainless-steel\/production\/cut\/\">\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u3092\u5207\u308b\u306b\u306f\u3069\u3046\u3059\u308c\u3070\u3044\u3044\u3067\u3059\u304b?<\/a><\/p><ul class=\"wp-block-list\"><li>\u6eb6\u63a5<\/li><\/ul><p class=\"wp-block-paragraph\">TIG\u3001MIG\u3001\u62b5\u6297\u6eb6\u63a5\u306a\u3069\u306e\u6280\u8853\u306b\u3088\u308a\u3001\u5f37\u5ea6\u3068\u8010\u8150\u98df\u6027\u306b\u512a\u308c\u305f\u63a5\u5408\u90e8\u304c\u78ba\u4fdd\u3055\u308c\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u54c1\u8cea\u7ba1\u7406<\/h3><p class=\"wp-block-paragraph\">\u30e1\u30fc\u30ab\u30fc\u306f\u3055\u307e\u3056\u307e\u306a\u30c6\u30b9\u30c8\u3092\u901a\u3058\u3066\u3001\u6750\u6599\u306e\u7d44\u6210\u3001\u5f37\u5ea6\u3001\u5b8c\u5168\u6027\u3092\u691c\u8a3c\u3057\u307e\u3059\u3002\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u751f\u7523\u3067\u306f\u3001\u54c1\u8cea\u7ba1\u7406\u6bb5\u968e\u306b\u306f\u901a\u5e38\u3001\u6b21\u306e\u624b\u9806\u304c\u542b\u307e\u308c\u307e\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u5316\u5b66\u5206\u6790<\/li><\/ul><p class=\"wp-block-paragraph\">\u3053\u308c\u306b\u3088\u308a\u3001\u6750\u6599\u306e\u5316\u5b66\u7d44\u6210\u304c\u4ed5\u69d8\u3068\u4e00\u81f4\u3057\u3001\u30af\u30ed\u30e0\u3084\u30cb\u30c3\u30b1\u30eb\u306a\u3069\u306e\u5143\u7d20\u304c\u9069\u5207\u306a\u5272\u5408\u3067\u542b\u307e\u308c\u3066\u3044\u308b\u3053\u3068\u304c\u78ba\u8a8d\u3055\u308c\u307e\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u6a5f\u68b0\u8a66\u9a13<\/li><\/ul><p class=\"wp-block-paragraph\">\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u5f15\u5f35\u5f37\u5ea6\u3001\u786c\u5ea6\u3001\u5ef6\u6027\u3092\u30c1\u30a7\u30c3\u30af\u3059\u308b\u30c6\u30b9\u30c8\u3092\u5b9f\u65bd\u3057\u3001\u6a5f\u68b0\u7684\u6027\u80fd\u57fa\u6e96\u3092\u6e80\u305f\u3057\u3066\u3044\u308b\u3053\u3068\u3092\u78ba\u8a8d\u3057\u307e\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u975e\u7834\u58ca\u691c\u67fb\uff08NDT\uff09<\/li><\/ul><p class=\"wp-block-paragraph\">\u8d85\u97f3\u6ce2\u6cd5\u3068\u653e\u5c04\u7dda\u6cd5\u306f\u3001\u6750\u6599\u3092\u640d\u50b7\u3059\u308b\u3053\u3068\u306a\u304f\u5185\u90e8\u306e\u6b20\u9665\u3092\u691c\u51fa\u3057\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">\u30b9\u30c6\u30f3\u30ec\u30b9\u88fd\u54c1<\/h2><h3 class=\"wp-block-heading\">\u30b7\u30fc\u30c4<\/h3><ul class=\"wp-block-list\"><li>\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u677f\u306f\u8584\u304f\u5e73\u3089\u306a\u92fc\u677f\u3067\u3001\u9ad8\u3044\u8010\u8150\u98df\u6027\u3068\u6ed1\u3089\u304b\u3067\u5747\u4e00\u306a\u8868\u9762\u304c\u6c42\u3081\u3089\u308c\u308b\u7528\u9014\u3067\u3088\u304f\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/li>\n\n<li>\u901a\u5e38\u3001\u539a\u3055\u306f 6 mm \u672a\u6e80\u3067\u3001\u71b1\u9593\u5727\u5ef6\u307e\u305f\u306f\u51b7\u9593\u5727\u5ef6\u306e\u3044\u305a\u308c\u304b\u3067\u52a0\u5de5\u3067\u304d\u307e\u3059\u3002\u51b7\u9593\u5727\u5ef6\u3067\u306f\u3001\u8868\u9762\u54c1\u8cea\u3068\u5f37\u5ea6\u304c\u5411\u4e0a\u3057\u307e\u3059\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">\u30d7\u30ec\u30fc\u30c8<\/h3><ul class=\"wp-block-list\"><li>\u30d7\u30ec\u30fc\u30c8\u306f\u30b7\u30fc\u30c8\u3088\u308a\u3082\u539a\u304f\u3001\u3088\u308a\u9ad8\u8ca0\u8377\u306e\u5de5\u696d\u7528\u9014\u5411\u3051\u306b\u8a2d\u8a08\u3055\u308c\u3066\u3044\u307e\u3059\u3002<\/li>\n\n<li>\u30d7\u30ec\u30fc\u30c8\u306f 6mm \u3092\u8d85\u3048\u308b\u539a\u3055\u306b\u306a\u308b\u3053\u3068\u304c\u591a\u304f\u3001\u8010\u8377\u91cd\u7528\u9014\u306b\u512a\u308c\u305f\u5f37\u5ea6\u3092\u767a\u63ee\u3057\u307e\u3059\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">\u30b3\u30a4\u30eb<\/h3><ul class=\"wp-block-list\"><li>\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u30b3\u30a4\u30eb\u306f\u3001\u8f38\u9001\u3068\u4fdd\u7ba1\u3092\u5bb9\u6613\u306b\u3059\u308b\u305f\u3081\u306b\u30b3\u30a4\u30eb\u72b6\u306b\u5dfb\u304b\u308c\u305f\u9023\u7d9a\u3057\u305f\u9577\u3044\u92fc\u5e2f\u3067\u3059\u3002<\/li>\n\n<li>\u30b3\u30a4\u30eb\u306f\u71b1\u9593\u5727\u5ef6\u307e\u305f\u306f\u51b7\u9593\u5727\u5ef6\u306e\u3044\u305a\u308c\u304b\u3067\u88fd\u9020\u3055\u308c\u3001\u3055\u307e\u3056\u307e\u306a\u5e45\u3068\u539a\u3055\u306e\u3082\u306e\u304c\u3042\u308a\u307e\u3059\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">\u30d0\u30fc<\/h3><ul class=\"wp-block-list\"><li>\u30d0\u30fc\u306b\u306f\u4e38\u578b\u3001\u56db\u89d2\u578b\u3001\u516d\u89d2\u578b\u306a\u3069\u3055\u307e\u3056\u307e\u306a\u5f62\u304c\u3042\u308a\u307e\u3059\u3002&nbsp;<\/li>\n\n<li>\u5e45\u5e83\u3044\u5efa\u8a2d\u304a\u3088\u3073\u7523\u696d\u7528\u9014\u3067\u4f7f\u7528\u3055\u308c\u3066\u3044\u307e\u3059\u3002<\/li>\n\n<li>\u30d0\u30fc\u306f\u5f62\u72b6\u306b\u591a\u69d8\u6027\u304c\u3042\u308a\u3001\u7279\u5b9a\u306e\u6a5f\u68b0\u7684\u7279\u6027\u3084\u5f62\u72b6\u304c\u5fc5\u8981\u306a\u5834\u5408\u306b\u3088\u304f\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">\u30ef\u30a4\u30e4\u30fc<\/h3><ul class=\"wp-block-list\"><li>\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u7dda\u306f\u3001\u9577\u304f\u3066\u7d30\u3044\u92fc\u7dda\u3067\u3059\u3002\u901a\u5e38\u3001\u67d4\u8edf\u6027\u3068\u5f15\u5f35\u5f37\u5ea6\u304c\u6c42\u3081\u3089\u308c\u308b\u7528\u9014\u3067\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/li>\n\n<li>\u7d20\u6750\u3092\u5f37\u5316\u3057\u3001\u8868\u9762\u4ed5\u4e0a\u3052\u3092\u6539\u5584\u3057\u307e\u3059\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">\u30d1\u30a4\u30d7<\/h3><ul class=\"wp-block-list\"><li>\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u7ba1\u306f\u3001\u6db2\u4f53\u3001\u6c17\u4f53\u3001\u307e\u305f\u306f\u305d\u306e\u4ed6\u306e\u7269\u8cea\u3092\u8f38\u9001\u3059\u308b\u305f\u3081\u306b\u4f7f\u7528\u3055\u308c\u308b\u4e2d\u7a7a\u306e\u7ba1\u3067\u3059\u3002<\/li>\n\n<li>\u30d1\u30a4\u30d7\u306f\u3055\u307e\u3056\u307e\u306a\u30b5\u30a4\u30ba\u304c\u3042\u308a\u3001\u7528\u9014\u306b\u5fdc\u3058\u3066\u901a\u5e38\u306f\u6eb6\u63a5\u307e\u305f\u306f\u30b7\u30fc\u30e0\u30ec\u30b9\u65b9\u5f0f\u3067\u88fd\u9020\u3055\u308c\u307e\u3059\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">\u30c1\u30e5\u30fc\u30d6<\/h3><ul class=\"wp-block-list\"><li>\u30d1\u30a4\u30d7\u306b\u4f3c\u3066\u3044\u307e\u3059\u304c\u3001\u3088\u308a\u8584\u304f\u3001\u3088\u308a\u7cbe\u5bc6\u306a\u7528\u9014\u3084\u5c0f\u898f\u6a21\u306a\u7528\u9014\u306b\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/li>\n\n<li>\u30c1\u30e5\u30fc\u30d6\u306f\u3001\u7d99\u304e\u76ee\u304c\u306a\u3044\u304b\u6eb6\u63a5\u3055\u308c\u3066\u3044\u308b\u3053\u3068\u304c\u591a\u304f\u3001\u5186\u5f62\u3001\u6b63\u65b9\u5f62\u3001\u9577\u65b9\u5f62\u306a\u3069\u3055\u307e\u3056\u307e\u306a\u5f62\u72b6\u304c\u3042\u308a\u307e\u3059\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">\u30d5\u30a9\u30a4\u30eb<\/h3><ul class=\"wp-block-list\"><li>\u975e\u5e38\u306b\u8584\u3044\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u677f\u3002\u901a\u5e38\u306f\u7279\u6b8a\u306a\u7528\u9014\u306b\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/li>\n\n<li>\u901a\u5e38\u3001\u539a\u3055\u306f 0.15 mm \u672a\u6e80\u3067\u3001\u7cbe\u5bc6\u3067\u9ad8\u6027\u80fd\u306a\u74b0\u5883\u3067\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">\u69cb\u9020\u30bb\u30af\u30b7\u30e7\u30f3<\/h3><ul class=\"wp-block-list\"><li>\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u69cb\u9020\u30bb\u30af\u30b7\u30e7\u30f3\u306b\u306f\u3001\u6881\u3001\u30a2\u30f3\u30b0\u30eb\u3001\u30c1\u30e3\u30cd\u30eb\u304c\u542b\u307e\u308c\u307e\u3059\u3002\u3053\u308c\u3089\u306f\u3001\u5efa\u8a2d\u304a\u3088\u3073\u30a4\u30f3\u30d5\u30e9\u30b9\u30c8\u30e9\u30af\u30c1\u30e3 \u30d7\u30ed\u30b8\u30a7\u30af\u30c8\u3067\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/li>\n\n<li>\u3053\u308c\u3089\u306e\u30bb\u30af\u30b7\u30e7\u30f3\u306f\u8010\u8377\u91cd\u5f37\u5ea6\u3092\u5099\u3048\u3066\u304a\u308a\u3001\u71b1\u9593\u5727\u5ef6\u30d7\u30ed\u30bb\u30b9\u306b\u3088\u3063\u3066\u88fd\u9020\u3055\u308c\u307e\u3059\u3002<\/li><\/ul><h2 class=\"wp-block-heading\">\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u88fd\u9020\u306b\u306f\u3069\u306e\u304f\u3089\u3044\u6642\u9593\u304c\u304b\u304b\u308a\u307e\u3059\u304b?<\/h2><p class=\"wp-block-paragraph\">\u96fb\u6c17\u30a2\u30fc\u30af\u7089\u3067\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u3092\u88fd\u9020\u3059\u308b\u306b\u306f\u901a\u5e38 8 \uff5e 12 \u6642\u9593\u304b\u304b\u308a\u307e\u3059\u3002\u3053\u306e\u6642\u9593\u306b\u306f\u3001\u539f\u6750\u6599\u306e\u6eb6\u89e3\u3068\u3001\u8131\u70ad\u3001\u92f3\u9020\u3001\u6210\u5f62\u306a\u3069\u306e\u8ffd\u52a0\u624b\u9806\u304c\u542b\u307e\u308c\u307e\u3059\u3002\u305f\u3060\u3057\u3001\u71b1\u51e6\u7406\u3001\u5727\u5ef6\u3001\u4ed5\u4e0a\u3052\u306a\u3069\u306e\u8ffd\u52a0\u51e6\u7406\u306b\u3088\u308a\u3001\u5168\u4f53\u7684\u306a\u88fd\u9020\u6642\u9593\u304c\u9577\u304f\u306a\u308b\u5834\u5408\u304c\u3042\u308a\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u304c\u9ad8\u4fa1\u306a\u7406\u7531\u306f\u4f55\u3067\u3059\u304b?<\/h2><p class=\"wp-block-paragraph\">\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u3001\u30af\u30ed\u30e0\u3001\u30cb\u30c3\u30b1\u30eb\u3001\u5834\u5408\u306b\u3088\u3063\u3066\u306f\u30e2\u30ea\u30d6\u30c7\u30f3\u306a\u3069\u306e\u9ad8\u4fa1\u306a\u5408\u91d1\u5143\u7d20\u3092\u542b\u3093\u3067\u3044\u308b\u305f\u3081\u9ad8\u4fa1\u3067\u3059\u3002\u3055\u3089\u306b\u3001\u6eb6\u89e3\u3084\u7cbe\u932c\u306a\u3069\u306e\u30a8\u30cd\u30eb\u30ae\u30fc\u3092\u5927\u91cf\u306b\u6d88\u8cbb\u3059\u308b\u88fd\u9020\u30d7\u30ed\u30bb\u30b9\u3082\u30b3\u30b9\u30c8\u3092\u5897\u5927\u3055\u305b\u307e\u3059\u3002\u53b3\u683c\u306a\u54c1\u8cea\u7ba1\u7406\u3068\u3001\u7814\u78e8\u3084\u713c\u304d\u306a\u307e\u3057\u306a\u3069\u306e\u4ed5\u4e0a\u3052\u30d7\u30ed\u30bb\u30b9\u3082\u4fa1\u683c\u3092\u5f15\u304d\u4e0a\u3052\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u307b\u3068\u3093\u3069\u306f\u3069\u3053\u304b\u3089\u6765\u3066\u3044\u308b\u306e\u3067\u3057\u3087\u3046\u304b?<\/h2><p class=\"wp-block-paragraph\">\u4e3b\u8981\u751f\u7523\u56fd\u306b\u306f\u3001\u4e16\u754c\u306e\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u751f\u7523\u91cf\u306e\u534a\u5206\u4ee5\u4e0a\u3092\u5360\u3081\u308b\u4e2d\u56fd\u304c\u542b\u307e\u308c\u307e\u3059\u3002\u305d\u306e\u4ed6\u306e\u4e3b\u8981\u751f\u7523\u56fd\u306b\u306f\u3001\u30a4\u30f3\u30c9\u3001\u65e5\u672c\u3001\u97d3\u56fd\u3001\u30c9\u30a4\u30c4\u306a\u3069\u306e\u4e00\u90e8\u306e\u30e8\u30fc\u30ed\u30c3\u30d1\u8af8\u56fd\u304c\u542b\u307e\u308c\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">\u6982\u8981<\/h2><p class=\"wp-block-paragraph\">\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u751f\u7523\u306b\u304a\u3044\u3066\u54c1\u8cea\u7ba1\u7406\u3092\u78ba\u5b9f\u306b\u884c\u3046\u3053\u3068\u306f\u3001\u6750\u6599\u304c\u5fc5\u8981\u306a\u57fa\u6e96\u3092\u6e80\u305f\u3057\u3066\u3044\u308b\u3053\u3068\u3092\u4fdd\u8a3c\u3059\u308b\u305f\u3081\u306b\u4e0d\u53ef\u6b20\u3067\u3059\u3002\u3053\u308c\u306b\u3088\u308a\u3001\u92fc\u306e\u5f37\u5ea6\u3001\u8010\u8150\u98df\u6027\u3001\u8010\u4e45\u6027\u3092\u7dad\u6301\u3059\u308b\u3053\u3068\u304c\u3067\u304d\u307e\u3059\u3002&nbsp;<\/p><p class=\"wp-block-paragraph\">Steel Pro Group\u3067\u306f\u3001\u30d7\u30ec\u30fc\u30c8\u3001\u30d0\u30fc\u3001\u30b3\u30a4\u30eb\u3001\u304a\u5ba2\u69d8\u306e\u30cb\u30fc\u30ba\u306b\u5408\u308f\u305b\u305f\u30ab\u30b9\u30bf\u30e0\u30bd\u30ea\u30e5\u30fc\u30b7\u30e7\u30f3\u306a\u3069\u3001\u9ad8\u54c1\u8cea\u306e\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u88fd\u54c1\u3092\u5e45\u5e83\u304f\u53d6\u308a\u63c3\u3048\u3066\u3044\u307e\u3059\u3002\u559c\u3093\u3067\u304a\u624b\u4f1d\u3044\u3044\u305f\u3057\u307e\u3059\u306e\u3067\u3001\u304a\u6c17\u8efd\u306b\u304a\u554f\u3044\u5408\u308f\u305b\u304f\u3060\u3055\u3044\u3002 <a href=\"https:\/\/steelprogroup.com\/ja\">\u30a6\u30a7\u30d6\u30b5\u30a4\u30c8\u3092\u898b\u308b<\/a> \u307e\u305f\u306f <a href=\"https:\/\/steelprogroup.com\/ja\/contact-us\/\">\u3054\u9023\u7d61\u304f\u3060\u3055\u3044<\/a> \u8a73\u7d30\u307e\u305f\u306f\u500b\u5225\u306e\u898b\u7a4d\u3082\u308a\u306b\u3064\u3044\u3066\u306f\u3001\u304a\u554f\u3044\u5408\u308f\u305b\u304f\u3060\u3055\u3044\u3002<\/p>","protected":false},"excerpt":{"rendered":"<p>\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u3001\u3055\u307e\u3056\u307e\u306a\u72b6\u6cc1\u3067\u9ad8\u3044\u8010\u8150\u98df\u6027\u3001\u9577\u671f\u306b\u308f\u305f\u308b\u8010\u4e45\u6027\u3001\u6700\u5c0f\u9650\u306e\u30e1\u30f3\u30c6\u30ca\u30f3\u30b9\u306e\u5fc5\u8981\u6027\u3092\u5099\u3048\u3066\u3044\u307e\u3059\u3002\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u304c\u3069\u306e\u3088\u3046\u306b\u6a5f\u80fd\u3059\u308b\u304b\u3092\u7406\u89e3\u3059\u308b [\u2026]<\/p>","protected":false},"author":1,"featured_media":10933,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"_eb_attr":"","rank_math_lock_modified_date":false,"site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"categories":[112],"tags":[],"class_list":["post-10946","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-stainless-steel"],"acf":[],"_links":{"self":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts\/10946","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/comments?post=10946"}],"version-history":[{"count":0,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts\/10946\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/media\/10933"}],"wp:attachment":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/media?parent=10946"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/categories?post=10946"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/tags?post=10946"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}