{"id":11752,"date":"2024-10-21T07:49:00","date_gmt":"2024-10-20T23:49:00","guid":{"rendered":"https:\/\/app11147.cloudwayssites.com\/?p=11752"},"modified":"2024-11-21T11:40:55","modified_gmt":"2024-11-21T03:40:55","slug":"grade-616","status":"publish","type":"post","link":"https:\/\/steelprogroup.com\/ja\/stainless-steel\/grades\/grade-616\/","title":{"rendered":"\u5408\u91d1 616 | AISI 616 | AISI 422 \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc"},"content":{"rendered":"<p class=\"wp-block-paragraph\">616 \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u3001\u9ad8\u6e29\u74b0\u5883\u3067\u512a\u308c\u305f\u6027\u80fd\u3092\u767a\u63ee\u3059\u308b\u3053\u3068\u3067\u77e5\u3089\u308c\u308b\u30de\u30eb\u30c6\u30f3\u30b5\u30a4\u30c8\u5408\u91d1\u3067\u3059\u3002\u3053\u306e\u30d6\u30ed\u30b0\u3067\u306f\u3001616 \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u7d44\u6210\u3068\u7279\u6027\u306b\u3064\u3044\u3066\u8aac\u660e\u3057\u307e\u3059\u3002\u307e\u305f\u3001\u305d\u306e\u5229\u70b9\u3001\u5236\u9650\u3001\u7528\u9014\u306b\u3064\u3044\u3066\u3082\u8aac\u660e\u3057\u3001\u30d7\u30ed\u30b8\u30a7\u30af\u30c8\u306b\u6700\u9069\u306a\u30aa\u30d7\u30b7\u30e7\u30f3\u3092\u9078\u629e\u3067\u304d\u308b\u3088\u3046\u306b\u652f\u63f4\u3057\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">616\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u3068\u306f\u4f55\u3067\u3059\u304b?<\/h2><p class=\"wp-block-paragraph\">AISI 616 \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u3001Alloy 616 \u307e\u305f\u306f UNS S42200 \u3068\u3082\u547c\u3070\u308c\u3001\u30de\u30eb\u30c6\u30f3\u30b5\u30a4\u30c8\u7cfb\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u3067\u3059\u3002\u5f37\u5ea6\u3068\u8010\u71b1\u6027\u306b\u512a\u308c\u3066\u3044\u307e\u3059\u3002\u71b1\u51e6\u7406\u306b\u3088\u3063\u3066\u786c\u5316\u3055\u305b\u308b\u3053\u3068\u304c\u3067\u304d\u307e\u3059\u3002AISI 616 \u306f\u9ad8\u6e29\u3067\u3082\u512a\u308c\u305f\u6027\u80fd\u3092\u767a\u63ee\u3057\u30011200\u00b0F \u307e\u3067\u7279\u6027\u3092\u7dad\u6301\u3057\u307e\u3059\u3002\u4e00\u822c\u7684\u306a\u7528\u9014\u306b\u306f\u3001\u30b8\u30a7\u30c3\u30c8 \u30a8\u30f3\u30b8\u30f3\u3001\u84b8\u6c17\u30bf\u30fc\u30d3\u30f3\u3001\u9ad8\u6e29\u30dc\u30eb\u30c8\u306a\u3069\u304c\u3042\u308a\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">616\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u76f8\u5f53\u54c1\uff08AMS 5655\uff09<\/h2><ul class=\"wp-block-list\"><li>422 \u306e<\/li>\n\n<li>\u56fd\u9023S42200<\/li>\n\n<li>ASTM A565 \u30b0\u30ec\u30fc\u30c9616<\/li>\n\n<li>EN 1.4935<\/li><\/ul><h2 class=\"wp-block-heading\">616\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u5316\u5b66\u7d44\u6210<\/h2><p class=\"wp-block-paragraph\">\u4ee5\u4e0b\u306f 616 \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u5316\u5b66\u7d44\u6210\u3092\u307e\u3068\u3081\u305f\u8868\u3067\u3059\u3002<\/p><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u30a8\u30ec\u30e1\u30f3\u30c8<\/strong><\/td><td><strong>\u30d5\u30a7<\/strong><\/td><td><strong>Cr<\/strong><\/td><td><strong>\u30e2<\/strong><\/td><td><strong>\u308f<\/strong><\/td><td><strong>\u4e94<\/strong><\/td><td><strong>C<\/strong><\/td><td><strong>\u30e0\u30f3<\/strong><\/td><td><strong>Si<\/strong><\/td><td><strong>P<\/strong><\/td><td><strong>S<\/strong><\/td><td><strong>\u30cb\u30fc<\/strong><\/td><\/tr><tr><td><strong>\u91cd\u91cf\uff08%\uff09<\/strong><\/td><td>81.9-85.8<\/td><td>11.0-12.5<\/td><td>0.9-1.25<\/td><td>0.9-1.25<\/td><td>0.2-0.3<\/td><td>0.20-0.25<\/td><td>0.5-1.0<\/td><td>0-0.5<\/td><td>0-0.025<\/td><td>0-0.025<\/td><td>0.5-1.0<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">616\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u7269\u7406\u7684\u7279\u6027<\/h2><p class=\"wp-block-paragraph\">\u4ee5\u4e0b\u306f 616 \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u7269\u7406\u7684\u7279\u6027\u3092\u793a\u3059\u8868\u3067\u3059\u3002<\/p><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u30d7\u30ed\u30d1\u30c6\u30a3<\/strong><\/td><td><strong>\u30e1\u30c8\u30ea\u30c3\u30af\u5024<\/strong><\/td><td><strong>\u30a4\u30f3\u30da\u30ea\u30a2\u30eb\u30fb\u30d0\u30ea\u30e5\u30fc<\/strong><\/td><\/tr><tr><td>\u5bc6\u5ea6<\/td><td>7.9 g\/cm\u00b3<\/td><td>490 \u30dd\u30f3\u30c9\/\u30d5\u30a3\u30fc\u30c8\u00b3<\/td><\/tr><tr><td>\u878d\u70b9<\/td><td>1480-1510 \u00b0C<\/td><td>2700\uff5e2750\u00b0F<\/td><\/tr><tr><td>\u71b1\u4f1d\u5c0e\u7387<\/td><td>24W\/m\u00b7K<\/td><td>14 BTU\/h\u00b7ft\u00b7\u00b0F<\/td><\/tr><tr><td>\u71b1\u81a8\u5f35<\/td><td>10 \u00b5m\/m\u00b7K<\/td><td>&#8211;<\/td><\/tr><tr><td>\u96fb\u6c17\u4f1d\u5c0e\u7387<\/td><td>4.7% IACS<\/td><td>5.3% IACS \u6bd4\u91cd<\/td><\/tr><tr><td>\u78c1\u6c17\u7279\u6027<\/td><td>\u5f37\u78c1\u6027<\/td><td>\u5f37\u78c1\u6027<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">616\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u6a5f\u68b0\u7684\u7279\u6027<\/h2><p class=\"wp-block-paragraph\">\u4ee5\u4e0b\u306f 616 \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u6a5f\u68b0\u7684\u7279\u6027\u3092\u307e\u3068\u3081\u305f\u8868\u3067\u3059\u3002<\/p><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u30d7\u30ed\u30d1\u30c6\u30a3<\/strong><\/td><td><strong>\u5178\u578b\u7684\u306a\u5024<\/strong><\/td><\/tr><tr><td>\u5f15\u5f35\u5f37\u5ea6<\/td><td>910-1080 MPa (130-160 ksi)<\/td><\/tr><tr><td>\u964d\u4f0f\u5f37\u5ea6<\/td><td>670-870 MPa (97-130 ksi)<\/td><\/tr><tr><td>\u30d6\u30ea\u30cd\u30eb\u786c\u5ea6<\/td><td>260-330<\/td><\/tr><tr><td>\u30ed\u30c3\u30af\u30a6\u30a7\u30eb\u786c\u5ea6<\/td><td>21<\/td><\/tr><tr><td>\u30d3\u30c3\u30ab\u30fc\u30b9\u786c\u5ea6<\/td><td>223<\/td><\/tr><tr><td>\u4f38\u3073<\/td><td>15-17%<\/td><\/tr><tr><td>\u5f3e\u6027\u4fc2\u6570<\/td><td>200 GPa\uff0828 x 10\u2076 psi\uff09<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">616\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u305d\u306e\u4ed6\u306e\u7279\u6027<\/h2><h3 class=\"wp-block-heading\">\u8010\u71b1\u6027<\/h3><p class=\"wp-block-paragraph\">\u8010\u71b1\u6027\u306f 616 \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u6700\u3082\u91cd\u8981\u306a\u7279\u6027\u3067\u3059\u3002\u9ad8\u6e29\u7528\u9014\u5411\u3051\u306b\u7279\u5225\u306b\u8a2d\u8a08\u3055\u308c\u3066\u304a\u308a\u3001\u5f37\u5ea6\u3092\u5931\u3046\u3053\u3068\u306a\u304f 1200\u00b0F (650\u00b0C) \u3067\u9023\u7d9a\u7684\u306b\u52d5\u4f5c\u3067\u304d\u307e\u3059\u3002\u30af\u30ed\u30e0\u3068\u30e2\u30ea\u30d6\u30c7\u30f3\u306e\u542b\u6709\u91cf\u306b\u3088\u308a\u3001\u30b9\u30b1\u30fc\u30eb\u3084\u9178\u5316\u306b\u62b5\u6297\u3057\u3001\u6975\u7aef\u306a\u6e29\u5ea6\u3067\u3082\u8010\u4e45\u6027\u3092\u78ba\u4fdd\u3057\u307e\u3059\u3002\u30bf\u30fc\u30d3\u30f3\u3084\u30b8\u30a7\u30c3\u30c8 \u30a8\u30f3\u30b8\u30f3\u306a\u3069\u306e\u30b3\u30f3\u30dd\u30fc\u30cd\u30f3\u30c8\u306b\u6700\u9069\u3067\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u8010\u98df\u6027<\/h3><p class=\"wp-block-paragraph\">616\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u3001\u4e2d\u7a0b\u5ea6\u306e <a href=\"https:\/\/steelprogroup.com\/ja\/stainless-steel\/properties\/corrosion-resistant\/\">\u8010\u98df\u6027<\/a>\u30af\u30ed\u30e0\u542b\u6709\u91cf\uff0811-12.5%\uff09\u306f\u3001\u8efd\u5ea6\u306e\u8150\u98df\u74b0\u5883\u3067\u8868\u9762\u3092\u9306\u3084\u30b9\u30b1\u30fc\u30eb\u304b\u3089\u4fdd\u8b77\u3059\u308b\u306e\u306b\u5f79\u7acb\u3061\u307e\u3059\u3002\u305f\u3060\u3057\u3001316\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306a\u3069\u306e\u4ed6\u306e\u30b0\u30ec\u30fc\u30c9\u307b\u3069\u8010\u6027\u306f\u3042\u308a\u307e\u305b\u3093\u3002<\/p><h3 class=\"wp-block-heading\">\u4f5c\u696d\u6027<\/h3><p class=\"wp-block-paragraph\">616 \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u9069\u5ea6\u306a\u52a0\u5de5\u6027\u304c\u3042\u308a\u307e\u3059\u3002\u6a5f\u68b0\u52a0\u5de5\u3084\u6210\u5f62\u306f\u53ef\u80fd\u3067\u3059\u304c\u3001\u786c\u5ea6\u3068\u5f37\u5ea6\u304c\u9ad8\u3044\u305f\u3081\u3001\u30aa\u30fc\u30b9\u30c6\u30ca\u30a4\u30c8\u7cfb\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306b\u6bd4\u3079\u3066\u52a0\u5de5\u304c\u96e3\u3057\u304f\u306a\u308a\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">616\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u4e00\u822c\u7684\u306a\u7528\u9014<\/h2><p class=\"wp-block-paragraph\">616 \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u4e00\u822c\u7684\u306a\u7528\u9014\u306f\u3001\u4e3b\u306b\u9ad8\u5f37\u5ea6\u3068\u8010\u71b1\u6027\u304c\u6c42\u3081\u3089\u308c\u308b\u74b0\u5883\u3067\u3059\u3002\u4e3b\u306a\u7528\u9014\u306f\u6b21\u306e\u3068\u304a\u308a\u3067\u3059\u3002<\/p><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u7523\u696d<\/strong><\/td><td><strong>\u7533\u3057\u8fbc\u307f<\/strong><\/td><td><strong>\u7279\u5fb4<\/strong><\/td><\/tr><tr><td>\u822a\u7a7a\u5b87\u5b99<\/td><td>\u30bf\u30fc\u30d3\u30f3\u30d6\u30ec\u30fc\u30c9<\/td><td>\u9ad8\u5f37\u5ea6\u3001\u8010\u71b1\u6027<\/td><\/tr><tr><td>\u81ea\u52d5\u8eca<\/td><td>\u6392\u6c17\u30b7\u30b9\u30c6\u30e0<\/td><td>\u8010\u98df\u6027<\/td><\/tr><tr><td>\u30a8\u30cd\u30eb\u30ae\u30fc<\/td><td>\u30d0\u30eb\u30d6<\/td><td>\u8010\u6469\u8017\u6027\u3001\u8010\u4e45\u6027<\/td><\/tr><tr><td>\u77f3\u6cb9\u30fb\u30ac\u30b9<\/td><td>\u30dd\u30f3\u30d7\u90e8\u54c1<\/td><td>\u9ad8\u6e29\u5b89\u5b9a\u6027<\/td><\/tr><tr><td>\u88fd\u9020\u696d<\/td><td>\u6a5f\u68b0\u90e8\u54c1<\/td><td>\u5f37\u5316\u6a5f\u80fd<\/td><\/tr><tr><td>\u767a\u96fb<\/td><td>\u9ad8\u6e29\u30dc\u30eb\u30c8\u63a5\u5408<\/td><td>\u9ad8\u5f37\u5ea6\u3001\u71b1\u5b89\u5b9a\u6027<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">616\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u9577\u6240\u3068\u77ed\u6240<\/h2><p class=\"wp-block-paragraph\">616 \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u5229\u70b9\u306f\u6b21\u306e\u3068\u304a\u308a\u3067\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u9ad8\u3044\u8010\u71b1\u6027<\/li><\/ul><p class=\"wp-block-paragraph\">616 \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u6700\u9ad8 1200\u00b0F (650\u00b0C) \u306e\u6e29\u5ea6\u3067\u52d5\u4f5c\u3067\u304d\u308b\u305f\u3081\u3001\u30bf\u30fc\u30d3\u30f3\u30d6\u30ec\u30fc\u30c9\u3001\u30b8\u30a7\u30c3\u30c8\u30a8\u30f3\u30b8\u30f3\u3001\u305d\u306e\u4ed6\u306e\u822a\u7a7a\u5b87\u5b99\u90e8\u54c1\u306a\u3069\u306e\u9ad8\u6e29\u7528\u9014\u306b\u6700\u9069\u3067\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u512a\u308c\u305f\u6a5f\u68b0\u7684\u5f37\u5ea6<\/li><\/ul><p class=\"wp-block-paragraph\">\u3053\u306e\u5408\u91d1\u306f\u512a\u308c\u305f\u5f15\u5f35\u5f37\u5ea6\u3068\u964d\u4f0f\u5f37\u5ea6\u3092\u793a\u3057\u3001\u5ba4\u6e29\u3068\u9ad8\u6e29\u306e\u4e21\u65b9\u306e\u74b0\u5883\u3067\u6a5f\u68b0\u7684\u6027\u80fd\u3092\u7dad\u6301\u3057\u307e\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u826f\u597d\u306a\u8010\u6469\u8017\u6027<\/li><\/ul><p class=\"wp-block-paragraph\">616 \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u3001\u7279\u306b\u71b1\u51e6\u7406\u5f8c\u306e\u786c\u5ea6\u304c\u9ad8\u3044\u305f\u3081\u3001\u6469\u64e6\u306e\u5927\u304d\u3044\u74b0\u5883\u3067\u4e0d\u53ef\u6b20\u306a\u512a\u308c\u305f\u8010\u6469\u8017\u6027\u3092\u5099\u3048\u3066\u3044\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\">616 \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u6b20\u70b9\u306f\u6b21\u306e\u3068\u304a\u308a\u3067\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u8010\u8150\u98df\u6027\u306f\u9650\u3089\u308c\u3066\u3044\u308b<\/li><\/ul><p class=\"wp-block-paragraph\">616 \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u30af\u30ed\u30e0\u542b\u6709\u91cf\u306b\u3088\u308a\u4e2d\u7a0b\u5ea6\u306e\u8010\u8150\u98df\u6027\u3092\u5099\u3048\u3066\u3044\u307e\u3059\u304c\u3001\u8150\u98df\u6027\u306e\u9ad8\u3044\u74b0\u5883\u3084\u6d77\u6d0b\u74b0\u5883\u306b\u306f\u9069\u3057\u3066\u3044\u307e\u305b\u3093\u3002<\/p><ul class=\"wp-block-list\"><li>\u786c\u5316\u5f8c\u306e\u52a0\u5de5\u6027\u304c\u60aa\u3044<\/li><\/ul><p class=\"wp-block-paragraph\">616 \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u71b1\u51e6\u7406\u3059\u308b\u3068\u975e\u5e38\u306b\u786c\u304f\u306a\u308a\u3001\u6a5f\u68b0\u52a0\u5de5\u304c\u96e3\u3057\u304f\u306a\u308a\u307e\u3059\u3002\u3053\u306e\u786c\u5316\u72b6\u614b\u3067\u52b9\u679c\u7684\u306b\u5207\u65ad\u307e\u305f\u306f\u6210\u5f62\u3059\u308b\u306b\u306f\u3001\u7279\u6b8a\u306a\u30c4\u30fc\u30eb\u3068\u6280\u8853\u304c\u5fc5\u8981\u3067\u3059\u3002\u305f\u3060\u3057\u3001\u713c\u304d\u306a\u307e\u3057\u72b6\u614b\u306e\u65b9\u304c\u6a5f\u68b0\u52a0\u5de5\u304c\u5bb9\u6613\u3067\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u9650\u5b9a\u7684\u306a\u51b7\u9593\u52a0\u5de5\u6027<\/li><\/ul><p class=\"wp-block-paragraph\">616 \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u3001\u7279\u306b\u71b1\u51e6\u7406\u5f8c\u306f\u3001\u51b7\u9593\u52a0\u5de5\u30d7\u30ed\u30bb\u30b9 (\u51b7\u9593\u5727\u5ef6\u3084\u6210\u5f62\u306a\u3069) \u306b\u3088\u3063\u3066\u5909\u5f62\u3057\u306b\u304f\u304f\u306a\u308a\u307e\u3059\u3002\u3053\u306e\u6750\u6599\u306f\u5ba4\u6e29\u3067\u786c\u5ea6\u304c\u9ad8\u3044\u305f\u3081\u3001\u51b7\u9593\u72b6\u614b\u3067\u306f\u6210\u5f62\u3084\u6210\u5f62\u304c\u56f0\u96e3\u306b\u306a\u308a\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">616\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u52a0\u5de5\u65b9\u6cd5<\/h2><h3 class=\"wp-block-heading\">\u30db\u30c3\u30c8\u30ef\u30fc\u30ad\u30f3\u30b0<\/h3><p class=\"wp-block-paragraph\">\u71b1\u9593\u52a0\u5de5\u3068\u306f\u3001\u518d\u7d50\u6676\u70b9\u4ee5\u4e0a\u306e\u6e29\u5ea6\u3067\u91d1\u5c5e\u3092\u5909\u5f62\u304a\u3088\u3073\u6210\u5f62\u3059\u308b\u30d7\u30ed\u30bb\u30b9\u3067\u3042\u308a\u3001\u6750\u6599\u304c\u7834\u640d\u3059\u308b\u3053\u3068\u306a\u304f\u7c21\u5358\u306b\u6210\u5f62\u3067\u304d\u308b\u3088\u3046\u306b\u306a\u308a\u307e\u3059\u3002<\/p><h4 class=\"wp-block-heading\">\u935b\u9020<\/h4><p class=\"wp-block-paragraph\">\u92fc\u3092 1700 \uff5e 2150\u00b0F (927 \uff5e 1177\u00b0C) \u306b\u52a0\u71b1\u3057\u3001\u30cf\u30f3\u30de\u30fc\u307e\u305f\u306f\u30d7\u30ec\u30b9\u3092\u4f7f\u7528\u3057\u3066\u5727\u7e2e\u3057\u307e\u3059\u3002&nbsp;<\/p><p class=\"wp-block-paragraph\">\u3053\u306e\u30d7\u30ed\u30bb\u30b9\u306b\u3088\u308a\u3001\u30bf\u30fc\u30d3\u30f3\u30d6\u30ec\u30fc\u30c9\u306e\u3088\u3046\u306a\u8907\u96d1\u306a\u90e8\u54c1\u304c\u6210\u5f62\u3055\u308c\u3001\u92fc\u306e\u7d50\u6676\u69cb\u9020\u304c\u6539\u5584\u3055\u308c\u307e\u3059\u3002<\/p><h4 class=\"wp-block-heading\">\u30ed\u30fc\u30ea\u30f3\u30b0<\/h4><p class=\"wp-block-paragraph\">\u92fc\u3092\u540c\u3058\u6e29\u5ea6\u7bc4\u56f2\u306b\u52a0\u71b1\u3057\u3001\u30ed\u30fc\u30e9\u30fc\u306b\u901a\u3057\u3066\u539a\u3055\u3092\u6e1b\u3089\u3057\u3001\u677f\u307e\u305f\u306f\u68d2\u306b\u6210\u5f62\u3057\u307e\u3059\u3002&nbsp;<\/p><p class=\"wp-block-paragraph\">\u5727\u5ef6\u306b\u3088\u308a\u6750\u6599\u306e\u5f37\u5ea6\u3068\u7d50\u6676\u7c92\u306e\u5fae\u7d30\u5316\u304c\u5411\u4e0a\u3057\u307e\u3059\u3002<\/p><h4 class=\"wp-block-heading\">\u62bc\u3057\u51fa\u3057<\/h4><p class=\"wp-block-paragraph\">\u92fc\u306f 1700 \uff5e 2150\u00b0F (927 \uff5e 1177\u00b0C) \u306b\u52a0\u71b1\u3055\u308c\u3001\u91d1\u578b\u306b\u62bc\u3057\u8fbc\u307e\u308c\u3066\u3001\u68d2\u3084\u30c1\u30e5\u30fc\u30d6\u306a\u3069\u306e\u5747\u4e00\u306a\u5f62\u72b6\u306b\u6210\u5f62\u3055\u308c\u307e\u3059\u3002&nbsp;<\/p><p class=\"wp-block-paragraph\">\u3053\u306e\u30d7\u30ed\u30bb\u30b9\u306f\u3001\u5f93\u6765\u306e\u30d7\u30ed\u30bb\u30b9\u3067\u306f\u5b9f\u73fe\u304c\u96e3\u3057\u3044\u3001\u3088\u308a\u8907\u96d1\u306a\u5f62\u72b6\u306b\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u71b1\u51e6\u7406<\/h3><p class=\"wp-block-paragraph\">616 \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u71b1\u51e6\u7406\u30d7\u30ed\u30bb\u30b9\u306f\u3001\u305d\u306e\u6a5f\u68b0\u7684\u7279\u6027\u3001\u7279\u306b\u786c\u5ea6\u3001\u5f37\u5ea6\u3001\u8010\u6469\u8017\u6027\u3092\u5411\u4e0a\u3055\u305b\u308b\u305f\u3081\u306b\u975e\u5e38\u306b\u91cd\u8981\u3067\u3059\u3002&nbsp;<\/p><h4 class=\"wp-block-heading\">\u30a2\u30cb\u30fc\u30ea\u30f3\u30b0<\/h4><p class=\"wp-block-paragraph\">\u92fc\u3092 790 \uff5e 850\u00b0C (1450 \uff5e 1560\u00b0F) \u306b\u52a0\u71b1\u3057\u3001\u3053\u306e\u6e29\u5ea6\u3092\u7dad\u6301\u3057\u3066\u52a0\u71b1\u304c\u5747\u4e00\u306b\u306a\u308b\u3088\u3046\u306b\u3057\u307e\u3059\u3002\u305d\u306e\u5f8c\u3001\u7a7a\u6c17\u4e2d\u3067\u3086\u3063\u304f\u308a\u3068\u51b7\u5374\u3057\u307e\u3059\u3002&nbsp;<\/p><p class=\"wp-block-paragraph\">\u3053\u306e\u30d7\u30ed\u30bb\u30b9\u306b\u3088\u308a\u3001\u5185\u90e8\u5fdc\u529b\u304c\u7de9\u548c\u3055\u308c\u3001\u92fc\u304c\u67d4\u3089\u304b\u304f\u306a\u308a\u3001\u6a5f\u68b0\u52a0\u5de5\u304c\u5bb9\u6613\u306b\u306a\u308a\u307e\u3059\u3002<\/p><h4 class=\"wp-block-heading\">\u786c\u5316<\/h4><p class=\"wp-block-paragraph\">\u92fc\u30921000\uff5e1065\u2103\u306e\u713c\u5165\u308c\u6e29\u5ea6\u307e\u3067\u52a0\u71b1\u3057\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\">\u92fc\u304c\u5e0c\u671b\u306e\u6e29\u5ea6\u306b\u9054\u3057\u305f\u3089\u3001\u90e8\u54c1\u306e\u539a\u3055\u306b\u5fdc\u3058\u3066\u6cb9\u307e\u305f\u306f\u7a7a\u6c17\u3092\u4f7f\u7528\u3057\u3066\u6025\u901f\u306b\u6025\u51b7\u3059\u308b\u5fc5\u8981\u304c\u3042\u308a\u307e\u3059\u3002\u539a\u3044\u90e8\u54c1\u306f\u3001\u901a\u5e38\u3001\u5341\u5206\u306a\u901f\u3055\u3067\u51b7\u5374\u3059\u308b\u305f\u3081\u306b\u6cb9\u306b\u3088\u308b\u6025\u51b7\u304c\u5fc5\u8981\u3067\u3059\u3002<\/p><h4 class=\"wp-block-heading\">\u713c\u304d\u623b\u3057<\/h4><p class=\"wp-block-paragraph\">\u5e0c\u671b\u3059\u308b\u786c\u5ea6\u3068\u5f37\u5ea6\u306b\u5fdc\u3058\u3066\u3001540\uff5e650\u00b0C (1000\uff5e1200\u00b0F) \u306b\u518d\u52a0\u71b1\u3057\u307e\u3059\u3002\u3053\u306e\u6e29\u5ea6\u3067\u6307\u5b9a\u6642\u9593\u4fdd\u6301\u3057\u305f\u5f8c\u3001\u7a7a\u51b7\u3057\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\">\u713c\u304d\u5165\u308c\u5f8c\u306e\u92fc\u306f\u975e\u5e38\u306b\u8106\u3044\u305f\u3081\u3001\u976d\u6027\u3092\u56de\u5fa9\u3059\u308b\u306b\u306f\u713c\u304d\u623b\u3057\u304c\u5fc5\u8981\u3067\u3059\u3002<\/p><h4 class=\"wp-block-heading\">\u30b9\u30c8\u30ec\u30b9\u89e3\u6d88<\/h4><p class=\"wp-block-paragraph\">\u786c\u5316\u5f8c\u3001\u6b8b\u7559\u5fdc\u529b\u3092\u8efd\u6e1b\u3059\u308b\u305f\u3081\u306b 200 \uff5e 300\u00b0C (390 \uff5e 570\u00b0F) \u306b\u52a0\u71b1\u3057\u3066\u5fdc\u529b\u7de9\u548c\u3092\u65bd\u3059\u3053\u3068\u304c\u3067\u304d\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u6a5f\u68b0<\/h3><p class=\"wp-block-paragraph\">\u5e0c\u671b\u306e\u5f62\u72b6\u3092\u5b9f\u73fe\u3059\u308b\u305f\u3081\u306e\u30d7\u30ed\u30bb\u30b9\u306b\u306f\u3001\u65cb\u524a\u3001\u30d5\u30e9\u30a4\u30b9\u52a0\u5de5\u3001\u7a74\u3042\u3051\u52a0\u5de5\u304c\u542b\u307e\u308c\u307e\u3059\u3002&nbsp;<\/p><p class=\"wp-block-paragraph\">AISI 422 \u3092\u52a0\u5de5\u3059\u308b\u5834\u5408\u306f\u3001\u8010\u4e45\u6027\u3068\u6469\u64e6\u4f4e\u6e1b\u306e\u305f\u3081\u3001\u8d85\u786c\u5207\u524a\u5de5\u5177\u307e\u305f\u306f TiN \u3084 TiAlN \u306a\u3069\u306e\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u3092\u65bd\u3057\u305f\u5de5\u5177\u3092\u4f7f\u7528\u3059\u308b\u3053\u3068\u3092\u304a\u52e7\u3081\u3057\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\">\u5207\u524a\u6db2\u306a\u3069\u306e\u52b9\u679c\u7684\u306a\u51b7\u5374\u65b9\u6cd5\u306f\u3001\u71b1\u3092\u7ba1\u7406\u3057\u3001\u8868\u9762\u54c1\u8cea\u3092\u5411\u4e0a\u3055\u305b\u308b\u305f\u3081\u306b\u4e0d\u53ef\u6b20\u3067\u3059\u3002<\/p><h2 class=\"wp-block-heading\">\u6982\u8981<\/h2><p class=\"wp-block-paragraph\">616 \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc (AISI 422 \u3068\u3082\u547c\u3070\u308c\u308b) \u306f\u3001\u9ad8\u6e29\u6027\u80fd\u3068\u8010\u6469\u8017\u6027\u3092\u8003\u616e\u3057\u3066\u8a2d\u8a08\u3055\u308c\u305f\u5408\u91d1\u3067\u3059\u3002\u30bf\u30fc\u30d3\u30f3\u3001\u30b8\u30a7\u30c3\u30c8 \u30a8\u30f3\u30b8\u30f3\u3001\u71b1\u4ea4\u63db\u5668\u306b\u6700\u9069\u306a\u6750\u6599\u3067\u3059\u3002<\/p><p class=\"wp-block-paragraph\">Steel Pro Group\u3067\u306f\u3001\u9ad8\u6027\u80fd\u306a\u7523\u696d\u30cb\u30fc\u30ba\u306b\u5fdc\u3048\u308b\u6700\u9ad8\u54c1\u8cea\u306e\u6750\u6599\u3092\u63d0\u4f9b\u3059\u308b\u3053\u3068\u306b\u5c3d\u529b\u3057\u3066\u3044\u307e\u3059\u3002\u30d7\u30ed\u30b8\u30a7\u30af\u30c8\u306b\u4fe1\u983c\u3067\u304d\u308b\u30bd\u30ea\u30e5\u30fc\u30b7\u30e7\u30f3\u3092\u304a\u63a2\u3057\u306e\u5834\u5408\u306f\u3001 <a href=\"https:\/\/steelprogroup.com\/ja\">\u30a6\u30a7\u30d6\u30b5\u30a4\u30c8\u3092\u898b\u308b<\/a> \u307e\u305f\u306f <a href=\"https:\/\/steelprogroup.com\/ja\/contact-us\/\">\u304a\u554f\u3044\u5408\u308f\u305b<\/a> \u500b\u5225\u306e\u3054\u76f8\u8ac7\u3068\u304a\u898b\u7a4d\u308a\u3092\u627f\u308a\u307e\u3059\u3002\u304a\u5ba2\u69d8\u306e\u7279\u5b9a\u306e\u8981\u4ef6\u306b\u6700\u9069\u306a\u6750\u6599\u306e\u9078\u629e\u3092\u304a\u624b\u4f1d\u3044\u3044\u305f\u3057\u307e\u3059\u3002<\/p>","protected":false},"excerpt":{"rendered":"<p>616 \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u3001\u9ad8\u6e29\u74b0\u5883\u3067\u512a\u308c\u305f\u6027\u80fd\u3092\u767a\u63ee\u3059\u308b\u3053\u3068\u3067\u77e5\u3089\u308c\u308b\u30de\u30eb\u30c6\u30f3\u30b5\u30a4\u30c8\u5408\u91d1\u3067\u3059\u3002\u3053\u306e\u30d6\u30ed\u30b0\u3067\u306f\u3001[\u2026]<\/p>","protected":false},"author":1,"featured_media":11751,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"_eb_attr":"","rank_math_lock_modified_date":false,"site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"categories":[4191,112],"tags":[],"class_list":["post-11752","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-grades","category-stainless-steel"],"acf":[],"_links":{"self":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts\/11752","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/comments?post=11752"}],"version-history":[{"count":0,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts\/11752\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/media\/11751"}],"wp:attachment":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/media?parent=11752"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/categories?post=11752"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/tags?post=11752"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}