{"id":11758,"date":"2024-10-21T11:45:00","date_gmt":"2024-10-21T03:45:00","guid":{"rendered":"https:\/\/app11147.cloudwayssites.com\/?p=11758"},"modified":"2024-11-21T11:43:51","modified_gmt":"2024-11-21T03:43:51","slug":"grade-430fr","status":"publish","type":"post","link":"https:\/\/steelprogroup.com\/ja\/stainless-steel\/grades\/grade-430fr\/","title":{"rendered":"430FR\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc: \u9ad8\u54c1\u8cea\u306e\u30bd\u30ec\u30ce\u30a4\u30c9\u30b5\u30d7\u30e9\u30a4\u30e4\u30fc"},"content":{"rendered":"<p class=\"wp-block-paragraph\">430FR \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u3001\u5f37\u529b\u306a\u78c1\u6027\u3068\u512a\u308c\u305f\u52a0\u5de5\u6027\u3067\u77e5\u3089\u308c\u308b\u30d5\u30a7\u30e9\u30a4\u30c8\u5408\u91d1\u3067\u3059\u3002\u30bd\u30ec\u30ce\u30a4\u30c9\u3001\u30ea\u30ec\u30fc\u3001\u96fb\u78c1\u5f01\u306a\u3069\u306e\u7528\u9014\u306b\u3088\u304f\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\">\u3053\u306e\u8a18\u4e8b\u3067\u306f\u3001430FR \u306e\u69cb\u6210\u3068\u4e3b\u306a\u7279\u6027\u306b\u3064\u3044\u3066\u8aac\u660e\u3057\u307e\u3059\u3002\u307e\u305f\u3001\u3053\u306e\u6750\u6599\u306e\u5229\u70b9\u3068\u9650\u754c\u3001\u4e00\u822c\u7684\u306a\u7528\u9014\u306b\u3064\u3044\u3066\u3082\u8aac\u660e\u3057\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">430FR\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u3068\u306f\u4f55\u3067\u3059\u304b?<\/h2><p class=\"wp-block-paragraph\">430FR \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u3001\u7d04 80% \u306e\u9244\u3068 16-18% \u306e\u30af\u30ed\u30e0\u3067\u4f5c\u3089\u308c\u305f\u30d5\u30a7\u30e9\u30a4\u30c8\u7cfb\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u3067\u3059\u3002\u3053\u306e\u5408\u91d1\u306f\u8edf\u78c1\u6027\u90e8\u54c1\u306b\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002\u512a\u308c\u305f\u78c1\u6c17\u7279\u6027\u3068\u52a0\u5de5\u6027\u3067\u77e5\u3089\u308c\u3066\u3044\u307e\u3059\u3002\u30bd\u30ec\u30ce\u30a4\u30c9\u3001\u30ea\u30ec\u30fc\u3001\u96fb\u78c1\u5f01\u306a\u3069\u306e\u7528\u9014\u306b\u6700\u9069\u3067\u3059\u3002<\/p><h2 class=\"wp-block-heading\">430FR\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u5316\u5b66\u7d44\u6210<\/h2><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u30a8\u30ec\u30e1\u30f3\u30c8<\/strong><\/td><td><strong>C<\/strong><\/td><td><strong>\u30e0\u30f3<\/strong><\/td><td><strong>P<\/strong><\/td><td><strong>S<\/strong><\/td><td><strong>Si<\/strong><\/td><td><strong>Cr<\/strong><\/td><td><strong>\u30cb\u30fc<\/strong><\/td><td><strong>\u30d5\u30a7<\/strong><\/td><\/tr><tr><td><strong>wt%<\/strong><\/td><td>\u6700\u59270.06<\/td><td>\u6700\u59270.80<\/td><td>\u6700\u59270.03<\/td><td>0.25-0.40<\/td><td>1.00-1.50<\/td><td>17.25-18.25<\/td><td>0.5<\/td><td>\u30d0\u30e9\u30f3\u30b9<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">430FR\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u7269\u7406\u7684\u7279\u6027<\/h2><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u30d7\u30ed\u30d1\u30c6\u30a3<\/strong><\/td><td><strong>\u5178\u578b\u7684\u306a\u5024<\/strong><\/td><td><strong>\u30d1\u30d5\u30a9\u30fc\u30de\u30f3\u30b9<\/strong><\/td><\/tr><tr><td>\u5bc6\u5ea6<\/td><td>7.7 g\/cm\u00b3 (0.278 \u30dd\u30f3\u30c9\/\u30a4\u30f3\u30c1\u00b3)<\/td><td>\u9ad8\u5bc6\u5ea6\u3067\u512a\u308c\u305f\u6a5f\u68b0\u7684\u5f37\u5ea6\u3092\u5b9f\u73fe<\/td><\/tr><tr><td>\u878d\u70b9<\/td><td>1425-1510\u00b0C (2600-2750\u00b0F)<\/td><td>\u878d\u70b9\u304c\u9ad8\u304f\u3001\u9ad8\u6e29\u7528\u9014\u306b\u9069\u3057\u3066\u3044\u307e\u3059<\/td><\/tr><tr><td>\u71b1\u4f1d\u5c0e\u7387<\/td><td>26.1 W\/m\u00b7K (@100\u00b0C) (15.1 BTU\u00b7ft\/hr\u00b7\u00b0F)<\/td><td>\u4e2d\u7a0b\u5ea6\u306e\u71b1\u4f1d\u5c0e\u7387<\/td><\/tr><tr><td>\u71b1\u81a8\u5f35<\/td><td>10.4 \u00b5m\/m\u00b7\u00b0C (5.8 \u00b5in\/in\u00b7\u00b0F) (0-100\u00b0C)<\/td><td>\u4f4e\u81a8\u5f35\u3067\u71b1\u30b5\u30a4\u30af\u30eb\u4e2d\u306e\u5b89\u5b9a\u6027\u3092\u7dad\u6301<\/td><\/tr><tr><td>\u96fb\u6c17\u4f1d\u5c0e\u7387<\/td><td>0.60 \u00b5\u03a9\u00b7m\uff08@20\u00b0C\uff09<\/td><td>\u4e2d\u7a0b\u5ea6\u306e\u62b5\u6297\u6027\u3001\u96fb\u78c1\u7528\u9014\u306b\u9069\u3057\u3066\u3044\u308b<\/td><\/tr><tr><td>\u78c1\u6c17\u7279\u6027<\/td><td>\u900f\u78c1\u7387600\uff5e1100<\/td><td>\u5f37\u529b\u306a\u78c1\u6027<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">430FR\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u6a5f\u68b0\u7684\u7279\u6027<\/h2><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u30d7\u30ed\u30d1\u30c6\u30a3<\/strong><\/td><td><strong>\u5178\u578b\u7684\u306a\u5024<\/strong><\/td><td><strong>\u30d1\u30d5\u30a9\u30fc\u30de\u30f3\u30b9<\/strong><\/td><\/tr><tr><td>\u5f15\u5f35\u5f37\u5ea6<\/td><td>78 ksi (538 MPa)<\/td><td>\u3055\u307e\u3056\u307e\u306a\u7528\u9014\u306b\u9069\u3057\u305f\u5f37\u5ea6<\/td><\/tr><tr><td>\u964d\u4f0f\u5f37\u5ea6<\/td><td>50 ksi (345 MPa)<\/td><td>\u90e8\u54c1\u306e\u9069\u5ea6\u306a\u964d\u4f0f\u5f37\u5ea6<\/td><\/tr><tr><td>\u30d6\u30ea\u30cd\u30eb\u786c\u5ea6<\/td><td>160 HB<\/td><td>\u8010\u6469\u8017\u6027\u3068\u52a0\u5de5\u6027\u306b\u512a\u308c\u3066\u3044\u307e\u3059<\/td><\/tr><tr><td>\u30d3\u30c3\u30ab\u30fc\u30b9\u786c\u5ea6<\/td><td>160 HV<\/td><td>\u30d6\u30ea\u30cd\u30eb\u786c\u5ea6\u3068\u540c\u7b49\u306e\u9069\u5ea6\u306a\u786c\u5ea6<\/td><\/tr><tr><td>\u4f38\u3073<\/td><td>30%<\/td><td>\u512a\u308c\u305f\u5f3e\u529b\u6027\u3068\u67d4\u8edf\u6027<\/td><\/tr><tr><td>\u5f3e\u6027\u4fc2\u6570<\/td><td>200 GPa\uff0829 x 10\u2076 psi\uff09<\/td><td>\u9ad8\u3044\u525b\u6027\u3001\u69cb\u9020\u7528\u9014\u3067\u306e\u5b89\u5b9a\u6027<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">430FR\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u78c1\u6c17\u7279\u6027<\/h2><p class=\"wp-block-paragraph\">\u78c1\u6027\u7279\u6027\u306f 430FR \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u6700\u3082\u91cd\u8981\u306a\u7279\u5fb4\u3067\u3042\u308a\u3001\u3053\u308c\u304c\u4ed6\u306e\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u3068\u7570\u306a\u308b\u70b9\u3067\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u9ad8\u3044\u900f\u78c1\u7387<\/h3><p class=\"wp-block-paragraph\">430FR \u306f\u5f37\u529b\u306a\u78c1\u6c17\u7279\u6027\u3092\u6301\u3061\u307e\u3059\u3002\u5916\u90e8\u78c1\u5834\u3092\u53d7\u3051\u308b\u3068\u3059\u3050\u306b\u78c1\u5316\u3057\u307e\u3059\u3002\u3053\u306e\u7279\u6027\u306f\u3001\u30bd\u30ec\u30ce\u30a4\u30c9 \u30b3\u30a2\u3001\u30ea\u30ec\u30fc\u3001\u96fb\u78c1\u30a2\u30af\u30c1\u30e5\u30a8\u30fc\u30bf\u306a\u3069\u306e\u30b3\u30f3\u30dd\u30fc\u30cd\u30f3\u30c8\u306b\u3068\u3063\u3066\u975e\u5e38\u306b\u91cd\u8981\u3067\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u4f4e\u3044\u4fdd\u78c1\u529b<\/h3><p class=\"wp-block-paragraph\">430FR \u306e\u4fdd\u78c1\u529b\u306f\u4f4e\u304f\u3001\u901a\u5e38\u306f 150 \uff5e 240 A\/m \u306e\u7bc4\u56f2\u3067\u3059\u3002\u3064\u307e\u308a\u3001\u78c1\u5316\u3068\u6d88\u78c1\u306e\u4e21\u65b9\u306b\u5fc5\u8981\u306a\u30a8\u30cd\u30eb\u30ae\u30fc\u306f\u975e\u5e38\u306b\u5c11\u306a\u304f\u3066\u6e08\u307f\u307e\u3059\u3002\u3053\u308c\u306f\u3001AC \u30bd\u30ec\u30ce\u30a4\u30c9\u3084\u30ea\u30ec\u30fc\u306a\u3069\u3001\u78c1\u5834\u3092\u983b\u7e41\u306b\u5207\u308a\u66ff\u3048\u308b\u5fc5\u8981\u304c\u3042\u308b\u30c7\u30d0\u30a4\u30b9\u3067\u7279\u306b\u5f79\u7acb\u3061\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u8edf\u78c1\u6027\u6750\u6599<\/h3><p class=\"wp-block-paragraph\">430FR \u306f\u8edf\u78c1\u6027\u6750\u6599\u3067\u3042\u308b\u305f\u3081\u3001\u78c1\u5316\u3068\u6d88\u78c1\u304c\u5bb9\u6613\u306b\u884c\u3048\u308b\u3088\u3046\u306b\u8a2d\u8a08\u3055\u308c\u3066\u3044\u307e\u3059\u3002\u305d\u306e\u305f\u3081\u3001\u78c1\u6c17\u72b6\u614b\u306e\u9ad8\u901f\u5207\u308a\u66ff\u3048\u304c\u6c42\u3081\u3089\u308c\u308b\u7528\u9014\u3067\u975e\u5e38\u306b\u52b9\u7387\u7684\u3067\u3059\u3002\u3053\u306e\u7279\u6027\u306f\u3001\u30bd\u30ec\u30ce\u30a4\u30c9\u3084\u30ea\u30ec\u30fc\u3092\u4f7f\u7528\u3059\u308b\u696d\u754c\u3067\u306f\u4e0d\u53ef\u6b20\u3067\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u5b89\u5b9a\u3057\u305f\u78c1\u6c17\u6319\u52d5<\/h3><p class=\"wp-block-paragraph\">430FR \u306f\u3001\u7e70\u308a\u8fd4\u3057\u4f7f\u7528\u3084\u5468\u671f\u7684\u306a\u4f7f\u7528\u306b\u304a\u3044\u3066\u3082\u5b89\u5b9a\u3057\u305f\u78c1\u6c17\u6027\u80fd\u3092\u767a\u63ee\u3057\u307e\u3059\u3002\u3053\u306e\u5b89\u5b9a\u6027\u306f\u3001\u30a4\u30f3\u30b8\u30a7\u30af\u30bf\u30fc\u3084\u30a2\u30af\u30c1\u30e5\u30a8\u30fc\u30bf\u30fc\u306a\u3069\u306e\u96fb\u78c1\u30b3\u30f3\u30dd\u30fc\u30cd\u30f3\u30c8\u3092\u4f7f\u7528\u3059\u308b\u696d\u754c\u3067\u306f\u975e\u5e38\u306b\u91cd\u8981\u3067\u3059\u3002<\/p><h2 class=\"wp-block-heading\">430FR\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u305d\u306e\u4ed6\u306e\u7279\u6027<\/h2><h3 class=\"wp-block-heading\">\u786c\u5ea6<\/h3><p class=\"wp-block-paragraph\">\u306b\u3064\u3044\u3066 <a href=\"https:\/\/steelprogroup.com\/ja\/stainless-steel\/properties\/hardness\/\">\u786c\u5ea6<\/a> 430FR \u306e\u786c\u5ea6\u306f\u4e2d\u7a0b\u5ea6\u3067\u3001\u5178\u578b\u7684\u306a\u30d6\u30ea\u30cd\u30eb\u786c\u5ea6\u306f 160 HB \u3067\u3059\u3002\u3053\u306e\u786c\u5ea6\u30ec\u30d9\u30eb\u306f\u30b7\u30ea\u30b3\u30f3\u542b\u6709\u91cf\u304c\u591a\u3044\u305f\u3081\u3067\u3001\u3053\u308c\u306b\u3088\u308a\u78c1\u6c17\u7279\u6027\u3082\u5411\u4e0a\u3057\u307e\u3059\u3002\u8010\u4e45\u6027\u3068\u6a5f\u68b0\u52a0\u5de5\u6027\u306e\u30d0\u30e9\u30f3\u30b9\u304c\u52b9\u679c\u7684\u306b\u53d6\u308c\u3066\u3044\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u8010\u98df\u6027<\/h3><p class=\"wp-block-paragraph\">430FR\u306f\u826f\u3044 <a href=\"https:\/\/steelprogroup.com\/ja\/stainless-steel\/properties\/corrosion-resistant\/\">\u8010\u98df\u6027<\/a> \u4e2d\u7a0b\u5ea6\u306e\u8150\u98df\u6027\u74b0\u5883\u3067\u306f\u3001\u6de1\u6c34\u3001\u4f4e\u5869\u7d20\u3001\u5f31\u9178\u6027\u306e\u74b0\u5883\u3067\u512a\u308c\u305f\u6027\u80fd\u3092\u767a\u63ee\u3057\u307e\u3059\u3002\u3055\u307e\u3056\u307e\u306a\u7523\u696d\u304a\u3088\u3073\u81ea\u52d5\u8eca\u7528\u9014\u306b\u6700\u9069\u3067\u3059\u3002\u305f\u3060\u3057\u3001\u30aa\u30fc\u30b9\u30c6\u30ca\u30a4\u30c8\u7cfb\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306b\u6bd4\u3079\u308b\u3068\u8010\u8150\u98df\u6027\u306f\u4f4e\u304f\u306a\u308a\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u52a0\u5de5\u6027<\/h3><p class=\"wp-block-paragraph\">430FR \u306f\u512a\u308c\u305f\u52a0\u5de5\u6027\u3092\u5099\u3048\u3066\u3044\u307e\u3059\u3002\u30d5\u30a7\u30e9\u30a4\u30c8\u7cfb\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u4e2d\u3067\u3082\u969b\u7acb\u3063\u305f\u5b58\u5728\u3067\u3059\u3002\u5408\u91d1\u306b\u786b\u9ec4\u304c\u542b\u307e\u308c\u3066\u3044\u308b\u305f\u3081\u3001\u52a0\u5de5\u6027\u304c\u5411\u4e0a\u3057\u307e\u3059\u3002\u3053\u308c\u306f\u7cbe\u5bc6\u52a0\u5de5\u7528\u9014\u3067\u306f\u7279\u306b\u91cd\u8981\u3067\u3059\u3002<\/p><h2 class=\"wp-block-heading\">430FR \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u7528\u9014\u306f\u4f55\u3067\u3059\u304b?<\/h2><p class=\"wp-block-paragraph\">430FR \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u3001\u96fb\u78c1\u6c17\u7528\u9014\u306e\u8981\u6c42\u3092\u6e80\u305f\u3059\u305f\u3081\u306b\u7279\u5225\u306b\u958b\u767a\u3055\u308c\u307e\u3057\u305f\u3002\u512a\u308c\u305f\u78c1\u6c17\u7279\u6027\u3068\u6a5f\u68b0\u52a0\u5de5\u6027\u306e\u7d44\u307f\u5408\u308f\u305b\u304c\u91cd\u8981\u3067\u3059\u3002&nbsp;<\/p><p class=\"wp-block-paragraph\">\u30bd\u30ec\u30ce\u30a4\u30c9\u3001\u30ea\u30ec\u30fc\u3001\u96fb\u78c1\u5f01\u306a\u3069\u3067\u3088\u304f\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002430FR \u304c\u9069\u7528\u3055\u308c\u308b\u4e3b\u306a\u5206\u91ce\u306f\u6b21\u306e\u3068\u304a\u308a\u3067\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u81ea\u52d5\u8eca\u7523\u696d<\/h3><p class=\"wp-block-paragraph\">\u81ea\u52d5\u8eca\u5206\u91ce\u306e\u30bb\u30f3\u30b5\u30fc\u90e8\u54c1\u3084\u96fb\u78c1\u30a2\u30af\u30c1\u30e5\u30a8\u30fc\u30bf\u30fc\u306b\u3088\u304f\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002\u3053\u308c\u3089\u306e\u7528\u9014\u3067\u306f\u3001430FR \u306e\u6a5f\u68b0\u52a0\u5de5\u6027\u3068\u78c1\u6c17\u6319\u52d5\u306e\u7d44\u307f\u5408\u308f\u305b\u304c\u3001\u7cbe\u5bc6\u3067\u8010\u4e45\u6027\u306e\u3042\u308b\u90e8\u54c1\u3092\u4f5c\u6210\u3059\u308b\u305f\u3081\u306b\u4e0d\u53ef\u6b20\u3067\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u96fb\u6c17\u6a5f\u5668<\/h3><p class=\"wp-block-paragraph\">\u78c1\u6c17\u30b9\u30a4\u30c3\u30c1\u3084\u5909\u5727\u5668\u30b3\u30a2\u306a\u3069\u306e\u90e8\u54c1\u306b\u306f 430FR \u304c\u4f7f\u7528\u3055\u308c\u3066\u3044\u307e\u3059\u3002\u3053\u308c\u306f\u3001\u9ad8\u3044\u900f\u78c1\u7387\u3068\u4f4e\u3044\u30d2\u30b9\u30c6\u30ea\u30b7\u30b9\u640d\u5931\u304c\u6c42\u3081\u3089\u308c\u308b\u305f\u3081\u3067\u3059\u3002\u3053\u308c\u3089\u306e\u7279\u6027\u306f\u3001\u96fb\u6c17\u56de\u8def\u3084\u30b3\u30f3\u30dd\u30fc\u30cd\u30f3\u30c8\u306e\u52b9\u7387\u5411\u4e0a\u306b\u5f79\u7acb\u3061\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u7523\u696d\u6a5f\u5668<\/h3><p class=\"wp-block-paragraph\">\u81ea\u52d5\u5316\u6a5f\u68b0\u3084\u30d7\u30ed\u30bb\u30b9\u5236\u5fa1\u30b7\u30b9\u30c6\u30e0\u306a\u3069\u3001\u7cbe\u5bc6\u306a\u96fb\u78c1\u5236\u5fa1\u3092\u5fc5\u8981\u3068\u3059\u308b\u696d\u754c\u3067\u4f7f\u7528\u3055\u308c\u3066\u3044\u307e\u3059\u3002430FR \u306f\u3001\u78c1\u6c17\u640d\u5931\u304c\u5c11\u306a\u304f\u3001\u52a0\u5de5\u6027\u306b\u512a\u308c\u3066\u3044\u308b\u305f\u3081\u3001\u975e\u5e38\u306b\u4fa1\u5024\u304c\u3042\u308a\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u30aa\u30d5\u30a3\u30b9\u30fb\u5bb6\u5ead\u7528\u96fb\u5316\u88fd\u54c1<\/h3><p class=\"wp-block-paragraph\">\u30e2\u30fc\u30bf\u30fc\u3001\u767a\u96fb\u6a5f\u3001\u78c1\u6c17\u76f8\u4e92\u4f5c\u7528\u3092\u5fc5\u8981\u3068\u3059\u308b\u305d\u306e\u4ed6\u306e\u5bb6\u96fb\u88fd\u54c1\u306a\u3069\u306e\u88fd\u54c1\u306b\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002430FR \u306f\u3001\u9ad8\u3044\u4fe1\u983c\u6027\u3068\u904b\u7528\u52b9\u7387\u3092\u78ba\u4fdd\u3059\u308b\u4e0a\u3067\u91cd\u8981\u306a\u5f79\u5272\u3092\u679c\u305f\u3057\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">430FR \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u88fd\u54c1<\/h2><h3 class=\"wp-block-heading\">430FR \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u677f<\/h3><p class=\"wp-block-paragraph\">\u69cb\u9020\u304a\u3088\u3073\u88fd\u9020\u7528\u9014\u3067\u4e00\u822c\u7684\u306b\u4f7f\u7528\u3055\u308c\u308b\u3053\u308c\u3089\u306e\u5e73\u3089\u306a\u30d5\u30a9\u30fc\u30e0\u306f\u3001\u6750\u6599\u306e\u78c1\u6c17\u7279\u6027\u3092\u6d3b\u7528\u3057\u306a\u304c\u3089\u5f37\u5ea6\u3068\u8010\u4e45\u6027\u3092\u63d0\u4f9b\u3057\u307e\u3059\u3002\u5207\u65ad\u3001\u6eb6\u63a5\u3001\u6210\u5f62\u304c\u7c21\u5358\u3067\u3059\u3002&nbsp;<\/p><h3 class=\"wp-block-heading\">430FR \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u30b3\u30a4\u30eb<\/h3><p class=\"wp-block-paragraph\">\u51e6\u7406\u3057\u3084\u3059\u3044\u3088\u3046\u306b\u30b3\u30a4\u30eb\u72b6\u306b\u5dfb\u304b\u308c\u3066\u304a\u308a\u3001\u5e83\u3044\u8868\u9762\u7a4d\u304c\u5fc5\u8981\u306a\u7528\u9014\u306b\u6700\u9069\u3067\u3059\u3002\u30b3\u30a4\u30eb\u306f\u81ea\u52d5\u8eca\u3084\u5bb6\u96fb\u88fd\u54c1\u306e\u88fd\u9020\u3067\u3088\u304f\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002&nbsp;<\/p><h3 class=\"wp-block-heading\">430FR \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u68d2<\/h3><p class=\"wp-block-paragraph\">\u4e38\u578b\u3001\u6b63\u65b9\u5f62\u3001\u9577\u65b9\u5f62\u306a\u3069\u3001\u3055\u307e\u3056\u307e\u306a\u5f62\u72b6\u306e\u30d0\u30fc\u304c\u3042\u308a\u3001\u6a5f\u68b0\u52a0\u5de5\u3084\u88fd\u9020\u5de5\u7a0b\u3067\u3088\u304f\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002\u78c1\u6c17\u7279\u6027\u304c\u3042\u308b\u305f\u3081\u3001\u78c1\u6c17\u5438\u5f15\u529b\u3092\u5fc5\u8981\u3068\u3059\u308b\u90e8\u54c1\u306b\u9069\u3057\u3066\u3044\u307e\u3059\u3002&nbsp;<\/p><h3 class=\"wp-block-heading\">430FR \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u7ba1\u304a\u3088\u3073\u30d1\u30a4\u30d7<\/h3><p class=\"wp-block-paragraph\">\u6db2\u4f53\u304a\u3088\u3073\u30ac\u30b9\u306e\u8f38\u9001\u306b\u4f7f\u7528\u3055\u308c\u308b\u3053\u308c\u3089\u306e\u30d5\u30a9\u30fc\u30e0\u306f\u3001430FR \u306e\u8010\u8150\u98df\u6027\u3068\u78c1\u6c17\u7279\u6027\u3092\u6d3b\u7528\u3057\u307e\u3059\u3002\u3053\u308c\u3089\u306f HVAC \u30b7\u30b9\u30c6\u30e0\u3084\u7523\u696d\u7528\u9014\u3067\u3088\u304f\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002&nbsp;<\/p><h3 class=\"wp-block-heading\">430FR \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u7d99\u624b\u304a\u3088\u3073\u30d5\u30a1\u30b9\u30ca\u30fc<\/h3><p class=\"wp-block-paragraph\">\u30dc\u30eb\u30c8\u3001\u30ca\u30c3\u30c8\u3001\u30d6\u30e9\u30b1\u30c3\u30c8\u306a\u3069\u306e\u3053\u308c\u3089\u306e\u30b3\u30f3\u30dd\u30fc\u30cd\u30f3\u30c8\u306f\u3001430FR \u306e\u5f37\u5ea6\u3068\u78c1\u6c17\u7279\u6027\u306e\u4e21\u65b9\u306e\u30e1\u30ea\u30c3\u30c8\u3092\u4eab\u53d7\u3057\u3066\u304a\u308a\u3001\u5efa\u8a2d\u3084\u6a5f\u68b0\u306b\u6700\u9069\u3067\u3059\u3002&nbsp;<\/p><h3 class=\"wp-block-heading\">430FR\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u96fb\u78c1\u90e8\u54c1<\/h3><p class=\"wp-block-paragraph\">\u30bd\u30ec\u30ce\u30a4\u30c9\u3084\u78c1\u6c17\u30bb\u30f3\u30b5\u30fc\u306a\u3069\u306e\u7279\u6b8a\u306a\u5f62\u72b6\u3067\u306f\u3001\u6750\u6599\u306e\u72ec\u81ea\u306e\u78c1\u6c17\u7279\u6027\u3092\u5229\u7528\u3057\u3066\u3001\u96fb\u5b50\u6a5f\u5668\u306e\u52b9\u7387\u7684\u306a\u30d1\u30d5\u30a9\u30fc\u30de\u30f3\u30b9\u3092\u5b9f\u73fe\u3057\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">430FR\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u9577\u6240\u3068\u77ed\u6240<\/h2><p class=\"wp-block-paragraph\">\u3053\u306e\u6750\u6599\u306e\u5229\u70b9\u3068\u9650\u754c\u3092\u307e\u3068\u3081\u307e\u3059\u3002\u3053\u308c\u306b\u3088\u308a\u3001430FR \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u3092\u660e\u78ba\u306b\u7406\u89e3\u3067\u304d\u308b\u3088\u3046\u306b\u306a\u308a\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\">430FR \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u5229\u70b9\u306f\u6b21\u306e\u3068\u304a\u308a\u3067\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u512a\u308c\u305f\u78c1\u6c17\u7279\u6027<\/li><\/ul><p class=\"wp-block-paragraph\">\u9ad8\u3044\u900f\u78c1\u7387\u3068\u4f4e\u3044\u4fdd\u78c1\u529b\u3002\u30bd\u30ec\u30ce\u30a4\u30c9\u306a\u3069\u306e\u8edf\u78c1\u6027\u7528\u9014\u306b\u6700\u9069\u3067\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u826f\u597d\u306a\u52a0\u5de5\u6027<\/li><\/ul><p class=\"wp-block-paragraph\">\u786b\u9ec4\u304c\u542b\u307e\u308c\u3066\u3044\u308b\u305f\u3081\u3001\u52a0\u5de5\u6027\u304c\u5411\u4e0a\u3057\u3001\u8907\u96d1\u306a\u90e8\u54c1\u306e\u52a0\u5de5\u304c\u5bb9\u6613\u306b\u306a\u308a\u307e\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u8010\u98df\u6027<\/li><\/ul><p class=\"wp-block-paragraph\">\u6de1\u6c34\u3001\u5f31\u9178\u3001\u4f4e\u5869\u7d20\u66b4\u9732\u306e\u74b0\u5883\u3067\u512a\u308c\u305f\u6027\u80fd\u3092\u767a\u63ee\u3057\u307e\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u8010\u4e45\u6027<\/li><\/ul><p class=\"wp-block-paragraph\">\u7e70\u308a\u8fd4\u3057\u306e\u885d\u6483\u3084\u30b9\u30c8\u30ec\u30b9\u4e0b\u3067\u3082\u5b89\u5b9a\u3057\u305f\u6a5f\u68b0\u7684\u6027\u80fd\u3092\u7dad\u6301\u3057\u3001\u52d5\u7684\u30b3\u30f3\u30dd\u30fc\u30cd\u30f3\u30c8\u306b\u6700\u9069\u3067\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u8cbb\u7528\u5bfe\u52b9\u679c<\/li><\/ul><p class=\"wp-block-paragraph\">\u9ad8\u7d1a\u5408\u91d1\u307b\u3069\u9ad8\u4fa1\u3067\u306f\u306a\u304f\u3001\u7279\u6b8a\u306a\u7528\u9014\u3067\u512a\u308c\u305f\u6027\u80fd\u3092\u767a\u63ee\u3057\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\">430FR \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u6b20\u70b9\u306f\u6b21\u306e\u3068\u304a\u308a\u3067\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u71b1\u51e6\u7406\u3067\u786c\u5316\u3057\u306a\u3044<\/li><\/ul><p class=\"wp-block-paragraph\">430FR \u306f\u71b1\u51e6\u7406\u3067\u786c\u5316\u3067\u304d\u307e\u305b\u3093\u3002\u975e\u5e38\u306b\u9ad8\u3044\u786c\u5ea6\u3092\u5fc5\u8981\u3068\u3059\u308b\u7528\u9014\u306b\u306f\u4f7f\u7528\u3055\u308c\u307e\u305b\u3093\u3002<\/p><ul class=\"wp-block-list\"><li>\u8010\u8150\u98df\u6027\u306f\u9650\u3089\u308c\u3066\u3044\u308b<\/li><\/ul><p class=\"wp-block-paragraph\">\u6d77\u6d0b\u3084\u5869\u7d20\u6fc3\u5ea6\u306e\u9ad8\u3044\u5834\u6240\u306a\u3069\u3001\u8150\u98df\u6027\u306e\u9ad8\u3044\u74b0\u5883\u306b\u306f\u9069\u3057\u3066\u3044\u307e\u305b\u3093\u3002<\/p><ul class=\"wp-block-list\"><li>\u6eb6\u63a5\u306e\u8ab2\u984c<\/li><\/ul><p class=\"wp-block-paragraph\">\u786b\u9ec4\u542b\u6709\u91cf\u304c\u591a\u3044\u305f\u3081\u3001\u6eb6\u63a5\u304c\u56f0\u96e3\u3067\u3059\u3002\u6eb6\u63a5\u4e2d\u306b\u5272\u308c\u304c\u751f\u3058\u308b\u30ea\u30b9\u30af\u304c\u9ad8\u307e\u308b\u305f\u3081\u3067\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u4e2d\u7a0b\u5ea6\u306e\u786c\u3055<\/li><\/ul><p class=\"wp-block-paragraph\">\u786c\u5ea6\u306f\u30de\u30eb\u30c6\u30f3\u30b5\u30a4\u30c8\u92fc\u3088\u308a\u3082\u4f4e\u3044\u305f\u3081\u3001\u6975\u5ea6\u306e\u786c\u5ea6\u304c\u6c42\u3081\u3089\u308c\u308b\u7528\u9014\u306b\u306f\u4f7f\u7528\u304c\u5236\u9650\u3055\u308c\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">430FR\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u52a0\u5de5\u65b9\u6cd5<\/h2><h3 class=\"wp-block-heading\">\u30db\u30c3\u30c8\u30ef\u30fc\u30ad\u30f3\u30b0<\/h3><ul class=\"wp-block-list\"><li>\u901a\u5e38\u30011,500\u00b0F (815\u00b0C) \uff5e 2,300\u00b0F (1,260\u00b0C) \u306e\u6e29\u5ea6\u3067\u5b9f\u884c\u3055\u308c\u307e\u3059\u3002<\/li>\n\n<li>\u5229\u70b9: \u5ef6\u6027\u3092\u9ad8\u3081\u3001\u786c\u5ea6\u3092\u4f4e\u4e0b\u3055\u305b\u307e\u3059\u3002\u8907\u96d1\u306a\u5f62\u72b6\u306e\u5f62\u6210\u306b\u5f79\u7acb\u3061\u307e\u3059\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">\u51b7\u9593\u52a0\u5de5<\/h3><ul class=\"wp-block-list\"><li>\u5ba4\u6e29\u3067\u5b9f\u65bd\u3057\u307e\u3059\u3002<\/li>\n\n<li>\u3072\u305a\u307f\u786c\u5316\u306b\u3088\u308a\u964d\u4f0f\u5f37\u5ea6\u3068\u786c\u5ea6\u304c\u5897\u52a0\u3057\u307e\u3059\u3002\u3053\u308c\u306b\u3088\u308a\u5ef6\u6027\u304c\u4f4e\u4e0b\u3057\u3001\u8106\u304f\u306a\u308b\u53ef\u80fd\u6027\u304c\u3042\u308a\u307e\u3059\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">\u71b1\u51e6\u7406<\/h3><ul class=\"wp-block-list\"><li>\u5fdc\u529b\u7de9\u548c\u713c\u920d\u306f\u4e00\u822c\u7684\u3067\u3059\u3002\u901a\u5e38\u306f\u3001\u7d04 1,200\u00b0F (650\u00b0C) \u3067\u7d04 1 \u6642\u9593\u884c\u308f\u308c\u307e\u3059\u3002<\/li>\n\n<li>\u5185\u90e8\u5fdc\u529b\u3092\u7de9\u548c\u3057\u307e\u3059\u304c\u3001\u30d5\u30a7\u30e9\u30a4\u30c8\u306e\u6027\u8cea\u306b\u3088\u308a\u786c\u5ea6\u3084\u5f37\u5ea6\u306f\u5927\u5e45\u306b\u5909\u5316\u3057\u307e\u305b\u3093\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">\u6eb6\u63a5<\/h3><ul class=\"wp-block-list\"><li>\u4e00\u822c\u7684\u306a\u65b9\u6cd5\u306b\u306f\u3001TIG (\u30bf\u30f3\u30b0\u30b9\u30c6\u30f3\u4e0d\u6d3b\u6027\u30ac\u30b9) \u6eb6\u63a5\u3068 MIG (\u91d1\u5c5e\u4e0d\u6d3b\u6027\u30ac\u30b9) \u6eb6\u63a5\u304c\u3042\u308a\u307e\u3059\u3002<\/li>\n\n<li>\u4e92\u63db\u6027\u3092\u78ba\u4fdd\u3059\u308b\u305f\u3081\u306b\u3001\u4e00\u81f4\u3059\u308b\u30d5\u30a3\u30e9\u30fc (\u901a\u5e38\u306f E308L \u307e\u305f\u306f\u985e\u4f3c\u30b0\u30ec\u30fc\u30c9) \u3092\u4f7f\u7528\u3059\u308b\u3053\u3068\u3092\u304a\u52e7\u3081\u3057\u307e\u3059\u3002<\/li>\n\n<li>\u3072\u3073\u5272\u308c\u3092\u9632\u3050\u305f\u3081\u306b\u4e88\u71b1\u304c\u5fc5\u8981\u306b\u306a\u308b\u5834\u5408\u304c\u3042\u308a\u307e\u3059\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">\u6a5f\u68b0\u52a0\u5de5<\/h3><ul class=\"wp-block-list\"><li>\u3088\u308a\u826f\u3044\u30d1\u30d5\u30a9\u30fc\u30de\u30f3\u30b9\u3092\u5f97\u308b\u306b\u306f\u3001\u8d85\u786c\u5de5\u5177\u3092\u4f7f\u7528\u3057\u3066\u304f\u3060\u3055\u3044\u3002<\/li>\n\n<li>\u6700\u9069\u306a\u901f\u5ea6\u306f\u6bce\u5206\u7d04 80 \uff5e 100 \u30d5\u30a3\u30fc\u30c8 (\u6bce\u5206 24 \uff5e 30 \u30e1\u30fc\u30c8\u30eb) \u3067\u3059\u3002<\/li>\n\n<li>\u71b1\u3068\u5de5\u5177\u306e\u6469\u8017\u3092\u8efd\u6e1b\u3059\u308b\u305f\u3081\u306b\u3001\u51b7\u5374\u6f64\u6ed1\u5264\u306e\u4f7f\u7528\u3092\u304a\u52e7\u3081\u3057\u307e\u3059\u3002<\/li><\/ul><h2 class=\"wp-block-heading\">430FR\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306b\u3064\u3044\u3066<\/h2><h3 class=\"wp-block-heading\">430FR \u304c\u30bd\u30ec\u30ce\u30a4\u30c9\u306b\u9069\u3057\u3066\u3044\u308b\u7406\u7531\u306f\u4f55\u3067\u3059\u304b?<\/h3><p class=\"wp-block-paragraph\">\u5f37\u529b\u306a\u78c1\u6c17\u7279\u6027\u3068\u4f4e\u3044\u4fdd\u78c1\u529b\u3092\u5099\u3048\u3066\u3044\u308b\u305f\u3081\u3001\u52b9\u7387\u7684\u306b\u78c1\u5316\u3068\u6d88\u78c1\u3092\u884c\u3046\u3053\u3068\u304c\u3067\u304d\u307e\u3059\u3002&nbsp;<\/p><p class=\"wp-block-paragraph\">\u52a0\u5de5\u6027\u3082\u826f\u597d\u3067\u3001\u7cbe\u5bc6\u306a\u30bd\u30ec\u30ce\u30a4\u30c9\u90e8\u54c1\u3078\u306e\u6210\u5f62\u3082\u5bb9\u6613\u3067\u3059\u3002<\/p><p class=\"wp-block-paragraph\">\u8010\u8150\u98df\u6027\u306b\u3088\u308a\u3001\u6e7f\u6c17\u3084\u5f31\u3044\u5316\u5b66\u7269\u8cea\u306e\u3042\u308b\u74b0\u5883\u3067\u3082\u8010\u4e45\u6027\u3092\u78ba\u4fdd\u3057\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">430 \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u30d0\u30ea\u30a8\u30fc\u30b7\u30e7\u30f3\u306f\u4f55\u3067\u3059\u304b?<\/h3><p class=\"wp-block-paragraph\">\u4ee5\u4e0b\u306f\u3001&nbsp; <a href=\"https:\/\/steelprogroup.com\/ja\/stainless-steel\/grades\/grade-430\/\">430\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc<\/a>:<\/p><ul class=\"wp-block-list\"><li>430F: \u786b\u9ec4\u3092\u6dfb\u52a0\u3057\u3066\u52a0\u5de5\u6027\u3092\u6539\u5584\u3002\u5e83\u7bc4\u56f2\u306e\u52a0\u5de5\u3092\u5fc5\u8981\u3068\u3059\u308b\u90e8\u54c1\u306b\u4f7f\u7528<\/li>\n\n<li>430FR: \u8edf\u78c1\u6027\u7528\u9014\u5411\u3051\u306b\u8a2d\u8a08\u3055\u308c\u305f 430FR \u306f\u3001\u3088\u308a\u9ad8\u3044\u900f\u78c1\u7387\u3092\u5099\u3048\u3066\u3044\u307e\u3059\u3002<\/li>\n\n<li>430L: 430 \u306e\u4f4e\u70ad\u7d20\u30d0\u30fc\u30b8\u30e7\u30f3\u3067\u3001\u8010\u98df\u6027\u3092\u7dad\u6301\u3057\u306a\u304c\u3089\u6eb6\u63a5\u6027\u304c\u5411\u4e0a\u3057\u307e\u3059\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">430F \u3068 430FR \u306e\u9055\u3044\u306f\u4f55\u3067\u3059\u304b?<\/h3><p class=\"wp-block-paragraph\">430F \u306f\u4e3b\u306b\u5207\u524a\u6027\u306b\u512a\u308c\u305f\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u3067\u3059\u3002 \u52a0\u5de5\u3057\u3084\u3059\u3044\u3088\u3046\u306b\u8a2d\u8a08\u3055\u308c\u3066\u3044\u307e\u3059\u304c\u3001\u78c1\u6c17\u7279\u6027\u306f\u9650\u3089\u308c\u3066\u3044\u307e\u3059\u3002&nbsp;<\/p><p class=\"wp-block-paragraph\">430FR \u306f\u3001\u8edf\u78c1\u6027\u30a2\u30d7\u30ea\u30b1\u30fc\u30b7\u30e7\u30f3\u5411\u3051\u306b\u7279\u5225\u306b\u8a2d\u8a08\u3055\u308c\u3066\u3044\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">\u6982\u8981<\/h2><p class=\"wp-block-paragraph\">430FR \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u3001\u30bd\u30ec\u30ce\u30a4\u30c9\u3001\u30ea\u30ec\u30fc\u3001\u30d0\u30eb\u30d6\u306a\u3069\u306e\u78c1\u6c17\u7528\u9014\u5411\u3051\u306b\u7279\u5225\u306b\u8a2d\u8a08\u3055\u308c\u305f\u9ad8\u6027\u80fd\u5408\u91d1\u3067\u3059\u3002\u78c1\u529b\u3068\u8010\u8150\u98df\u6027\u3092\u517c\u306d\u5099\u3048\u305f\u4fe1\u983c\u6027\u306e\u9ad8\u3044\u30b3\u30f3\u30dd\u30fc\u30cd\u30f3\u30c8\u3092\u5fc5\u8981\u3068\u3059\u308b\u4f01\u696d\u306b\u3068\u3063\u3066\u3001430FR \u306f\u6700\u9069\u306a\u9078\u629e\u80a2\u3067\u3059\u3002<\/p><p class=\"wp-block-paragraph\">Steel Pro Group\u3067\u306f\u3001\u9ad8\u6027\u80fd\u306a\u7523\u696d\u30cb\u30fc\u30ba\u306b\u5fdc\u3048\u308b\u6700\u9ad8\u54c1\u8cea\u306e\u6750\u6599\u3092\u63d0\u4f9b\u3059\u308b\u3053\u3068\u306b\u5c3d\u529b\u3057\u3066\u3044\u307e\u3059\u3002\u30d7\u30ed\u30b8\u30a7\u30af\u30c8\u306b\u4fe1\u983c\u3067\u304d\u308b\u30bd\u30ea\u30e5\u30fc\u30b7\u30e7\u30f3\u3092\u304a\u63a2\u3057\u306e\u5834\u5408\u306f\u3001 <a href=\"https:\/\/steelprogroup.com\/ja\">\u30a6\u30a7\u30d6\u30b5\u30a4\u30c8\u3092\u898b\u308b<\/a> \u307e\u305f\u306f <a href=\"https:\/\/steelprogroup.com\/ja\/contact-us\/\">\u304a\u554f\u3044\u5408\u308f\u305b<\/a> \u500b\u5225\u306e\u3054\u76f8\u8ac7\u3068\u304a\u898b\u7a4d\u308a\u3092\u627f\u308a\u307e\u3059\u3002\u304a\u5ba2\u69d8\u306e\u7279\u5b9a\u306e\u8981\u4ef6\u306b\u6700\u9069\u306a\u6750\u6599\u306e\u9078\u629e\u3092\u304a\u624b\u4f1d\u3044\u3044\u305f\u3057\u307e\u3059\u3002<\/p>","protected":false},"excerpt":{"rendered":"<p>430FR \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u3001\u5f37\u529b\u306a\u78c1\u6027\u3068\u512a\u308c\u305f\u52a0\u5de5\u6027\u3067\u77e5\u3089\u308c\u308b\u30d5\u30a7\u30e9\u30a4\u30c8\u5408\u91d1\u3067\u3059\u3002\u4e00\u822c\u7684\u306b\u306f [\u2026] \u306b\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/p>","protected":false},"author":1,"featured_media":11749,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"_eb_attr":"","rank_math_lock_modified_date":false,"site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"categories":[4191,112],"tags":[],"class_list":["post-11758","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-grades","category-stainless-steel"],"acf":[],"_links":{"self":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts\/11758","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/comments?post=11758"}],"version-history":[{"count":0,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts\/11758\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/media\/11749"}],"wp:attachment":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/media?parent=11758"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/categories?post=11758"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/tags?post=11758"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}