{"id":20004,"date":"2024-12-23T05:18:00","date_gmt":"2024-12-22T21:18:00","guid":{"rendered":"https:\/\/steelprogroup.com\/?p=20004"},"modified":"2024-12-23T15:37:55","modified_gmt":"2024-12-23T07:37:55","slug":"applications","status":"publish","type":"post","link":"https:\/\/steelprogroup.com\/ja\/tool-steel\/grades\/h13\/use\/applications\/","title":{"rendered":"H13 \u5de5\u5177\u92fc\u306e\u7528\u9014: \u6b63\u3057\u3044\u9078\u629e\u306e\u305f\u3081\u306e\u30ac\u30a4\u30c9"},"content":{"rendered":"<p class=\"wp-block-paragraph\">SteelPro Group \u306f\u3001\u3055\u307e\u3056\u307e\u306a\u696d\u754c\u3067\u9577\u5e74\u306e\u7d4c\u9a13\u3092\u6d3b\u304b\u3057\u3001\u6570\u3048\u5207\u308c\u306a\u3044\u307b\u3069\u591a\u304f\u306e\u4f01\u696d\u304c\u30c4\u30fc\u30eb\u696d\u754c\u3067\u751f\u7523\u3092\u6700\u9069\u5316\u3067\u304d\u308b\u3088\u3046\u652f\u63f4\u3057\u3066\u304d\u307e\u3057\u305f\u3002\u9ad8\u5ea6\u306a\u88fd\u9020\u30d7\u30ed\u30bb\u30b9\u3068\u53b3\u683c\u306a\u54c1\u8cea\u7ba1\u7406\u306b\u3088\u308a\u3001\u5f53\u793e\u306e H13 \u92fc\u306f\u30c4\u30fc\u30eb\u7528\u9014\u306e\u6700\u3082\u53b3\u3057\u3044\u57fa\u6e96\u3092\u6e80\u305f\u3057\u3066\u3044\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">H13 \u5de5\u5177\u92fc\u306f\u4f55\u306b\u4f7f\u7528\u3055\u308c\u307e\u3059\u304b?<\/h2><p class=\"wp-block-paragraph\">H13 \u5de5\u5177\u92fc\u306f\u3001\u9ad8\u3044\u5f37\u5ea6\u3001\u8010\u71b1\u6027\u3001\u976d\u6027\u3067\u77e5\u3089\u308c\u3066\u304a\u308a\u3001\u4e3b\u306b\u30c0\u30a4\u30ab\u30b9\u30c8\u91d1\u578b\u3001\u30d7\u30e9\u30b9\u30c1\u30c3\u30af\u5c04\u51fa\u6210\u5f62\u91d1\u578b\u3001\u935b\u9020\u91d1\u578b\u306a\u3069\u306e\u9ad8\u6e29\u7528\u9014\u306b\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002&nbsp;<\/p><p class=\"wp-block-paragraph\">\u6700\u3082\u904e\u9177\u306a\u6761\u4ef6\u3067\u3082\u5f37\u5ea6\u3092\u7dad\u6301\u3057\u3001\u6469\u8017\u306b\u8010\u3048\u308b\u80fd\u529b\u304c\u4ed6\u3068\u4e00\u7dda\u3092\u753b\u3057\u3066\u3044\u307e\u3059\u3002\u3064\u307e\u308a\u3001\u6545\u969c\u3084\u30c0\u30a6\u30f3\u30bf\u30a4\u30e0\u304c\u6e1b\u308a\u3001\u751f\u7523\u30b5\u30a4\u30af\u30eb\u304c\u3088\u308a\u52b9\u7387\u7684\u306b\u306a\u308a\u307e\u3059\u3002&nbsp;<\/p><p class=\"wp-block-paragraph\">H13 \u92fc\u306e\u4e3b\u306a\u7279\u6027\u3068\u5229\u70b9\u306b\u3064\u3044\u3066\u8a73\u3057\u304f\u77e5\u308b\u306b\u306f\u3001\u5de5\u5177\u696d\u754c\u3067\u306e H13 \u92fc\u306e\u6f5c\u5728\u80fd\u529b\u3092\u8a73\u3057\u304f\u8aac\u660e\u3057\u305f\u5f53\u793e\u306e\u5305\u62ec\u7684\u306a\u30ac\u30a4\u30c9\u3092\u3054\u89a7\u304f\u3060\u3055\u3044\u3002<\/p><h2 class=\"wp-block-heading\">\u71b1\u9593\u52a0\u5de5\u7528\u9014\u306b\u4f7f\u7528\u3055\u308c\u308bH13\u5de5\u5177\u92fc<\/h2><h3 class=\"wp-block-heading\">\u30c0\u30a4\u30ab\u30b9\u30c8\u91d1\u578b<\/h3><p class=\"wp-block-paragraph\">H13 \u92fc\u306f\u71b1\u75b2\u52b4\u306b\u5f37\u3044\u305f\u3081\u3001\u71b1\u30b5\u30a4\u30af\u30eb\u3092\u4f55\u5ea6\u3082\u7e70\u308a\u8fd4\u3057\u3066\u3082\u91d1\u578b\u306e\u5f37\u5ea6\u304c\u7dad\u6301\u3055\u308c\u307e\u3059\u3002\u3053\u308c\u306b\u3088\u308a\u3001\u30b3\u30b9\u30c8\u306e\u304b\u304b\u308b\u4fee\u7406\u3092\u56de\u907f\u3057\u3001\u751f\u7523\u30e9\u30a4\u30f3\u3092\u30b9\u30e0\u30fc\u30ba\u306b\u7a3c\u50cd\u3055\u305b\u308b\u3053\u3068\u304c\u3067\u304d\u307e\u3059\u3002\u307e\u305f\u3001\u30a2\u30eb\u30df\u30cb\u30a6\u30e0\u5408\u91d1\u306e\u9ad8\u3044\u53cd\u5fdc\u6027\u306b\u3088\u3063\u3066\u5f15\u304d\u8d77\u3053\u3055\u308c\u308b\u8150\u98df\u3084\u6d78\u98df\u306b\u3082\u8010\u3048\u308b\u305f\u3081\u3001\u8010\u4e45\u6027\u306e\u3042\u308b\u30a2\u30eb\u30df\u30cb\u30a6\u30e0 \u30c0\u30a4\u30ab\u30b9\u30c8\u91d1\u578b\u306b\u6700\u9069\u3067\u3059\u3002<\/p><p class=\"wp-block-paragraph\">\u5f53\u793e\u306e H13 \u92fc\u88fd\u54c1\u306b\u3088\u308a\u3001\u30c0\u30a4\u30ab\u30b9\u30c8\u88fd\u9020\u696d\u8005\u306f\u91d1\u578b\u5bff\u547d\u3092 25% \u4ee5\u4e0a\u5ef6\u3070\u3059\u3053\u3068\u304c\u3067\u304d\u307e\u3057\u305f\u3002SteelPro Group \u306f\u3001\u5358\u306b\u88fd\u54c1\u3092\u63d0\u4f9b\u3059\u308b\u3060\u3051\u3067\u306a\u304f\u3001\u30c4\u30fc\u30eb\u64cd\u4f5c\u3092\u6700\u9069\u5316\u3059\u308b\u6226\u7565\u7684\u30d1\u30fc\u30c8\u30ca\u30fc\u3082\u63d0\u4f9b\u3057\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u71b1\u9593\u935b\u9020\u91d1\u578b<\/h3><p class=\"wp-block-paragraph\">\u71b1\u9593\u935b\u9020\u3067\u306f\u3001\u71b1\u306b\u8010\u3048\u3089\u308c\u308b\u7d20\u6750\u304c\u5fc5\u8981\u3067\u3059\u3002H13 \u306f\u307e\u3055\u306b\u305d\u308c\u3092\u5b9f\u73fe\u3057\u307e\u3059\u3002\u3053\u306e\u7d20\u6750\u306f\u3001\u6975\u7aef\u306a\u6e29\u5ea6\u3084\u4e00\u5b9a\u306e\u5727\u529b\u306b\u3088\u308b\u6469\u8017\u306b\u8010\u3048\u308b\u307b\u3069\u306e\u5f37\u5ea6\u304c\u3042\u308a\u3001\u935b\u9020\u91d1\u578b\u306e\u5bff\u547d\u304c\u5ef6\u3073\u3001\u3088\u308a\u5f37\u529b\u306b\u6a5f\u80fd\u3057\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u62bc\u3057\u51fa\u3057\u30c0\u30a4\u30b9<\/h3><p class=\"wp-block-paragraph\">H13 \u306f\u8010\u71b1\u6027\u3068\u8010\u6469\u8017\u6027\u306b\u512a\u308c\u3066\u3044\u308b\u305f\u3081\u3001\u62bc\u3057\u51fa\u3057\u30c0\u30a4\u306b\u6700\u9069\u3067\u3059\u3002\u62bc\u3057\u51fa\u3057\u30d7\u30ed\u30bb\u30b9\u306b\u4f34\u3046\u9ad8\u6e29\u306b\u3082\u8010\u3048\u3001\u5f62\u72b6\u3084\u52b9\u679c\u3092\u5931\u308f\u306a\u3044\u305f\u3081\u3001\u4ea4\u63db\u56de\u6570\u304c\u5c11\u306a\u304f\u306a\u308a\u3001\u7d50\u679c\u304c\u5411\u4e0a\u3057\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u30db\u30c3\u30c8\u30b9\u30bf\u30f3\u30d7\u30c0\u30a4<\/h3><p class=\"wp-block-paragraph\">\u30db\u30c3\u30c8\u30b9\u30bf\u30f3\u30d4\u30f3\u30b0\u306e\u4f5c\u696d\u306b\u306f\u3001\u6025\u6fc0\u306a\u6e29\u5ea6\u5909\u5316\u306b\u8010\u3048\u3001\u6027\u80fd\u3092\u7dad\u6301\u3067\u304d\u308b\u30c4\u30fc\u30eb\u304c\u5fc5\u8981\u3067\u3059\u3002H13 \u92fc\u306f\u71b1\u885d\u6483\u306b\u8010\u3048\u308b\u3088\u3046\u306b\u4f5c\u3089\u308c\u3066\u304a\u308a\u3001\u30b9\u30bf\u30f3\u30d4\u30f3\u30b0\u91d1\u578b\u3092\u6700\u5927\u9650\u306b\u6d3b\u7528\u3057\u3001\u3088\u308a\u9ad8\u7cbe\u5ea6\u306e\u90e8\u54c1\u3092\u751f\u7523\u3059\u308b\u306e\u306b\u5f79\u7acb\u3061\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">\u51b7\u9593\u52a0\u5de5\u7528\u9014\u306b\u4f7f\u7528\u3055\u308c\u308bH13\u5de5\u5177\u92fc<\/h2><p class=\"wp-block-paragraph\">H13 \u306f\u9ad8\u6e29\u4f5c\u696d\u7528\u9014\u3067\u3088\u304f\u77e5\u3089\u308c\u3066\u3044\u307e\u3059\u304c\u3001\u4f4e\u6e29\u4f5c\u696d\u74b0\u5883\u3067\u3082\u975e\u5e38\u306b\u512a\u308c\u305f\u6027\u80fd\u3092\u767a\u63ee\u3057\u307e\u3059\u3002\u305d\u306e\u4ed8\u52a0\u4fa1\u5024\u306f\u6b21\u306e\u3068\u304a\u308a\u3067\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u30b9\u30bf\u30f3\u30d4\u30f3\u30b0\u30c0\u30a4<\/h3><p class=\"wp-block-paragraph\">H13 \u92fc\u306f\u976d\u6027\u3068\u8010\u6469\u8017\u6027\u306b\u512a\u308c\u3066\u304a\u308a\u3001\u30b9\u30bf\u30f3\u30d4\u30f3\u30b0 \u30c0\u30a4\u306b\u6700\u9069\u3067\u3059\u3002\u9ad8\u901f\u30b9\u30bf\u30f3\u30d4\u30f3\u30b0\u306e\u7e70\u308a\u8fd4\u3057\u30b9\u30c8\u30ec\u30b9\u306b\u3082\u8010\u3048\u3001\u5203\u5148\u304c\u5931\u308f\u308c\u308b\u3053\u3068\u306a\u304f\u3001\u6b63\u78ba\u306a\u30ab\u30c3\u30c8\u3068\u9ad8\u54c1\u8cea\u306e\u90e8\u54c1\u3092\u5b9f\u73fe\u3057\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u6df1\u7d5e\u308a\u30c0\u30a4\u30b9<\/h3><p class=\"wp-block-paragraph\">H13 \u92fc\u306f\u6469\u8017\u306b\u5f37\u304f\u3001\u5727\u529b\u4e0b\u3067\u3082\u5f37\u5ea6\u3092\u7dad\u6301\u3059\u308b\u305f\u3081\u3001\u6210\u5f62\u304c\u96e3\u3057\u3044\u6750\u6599\u3067\u3082\u6ed1\u3089\u304b\u3067\u4e00\u8cab\u3057\u305f\u7d50\u679c\u304c\u5f97\u3089\u308c\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u51b7\u9593\u62bc\u3057\u51fa\u3057\u30c0\u30a4\u30b9<\/h3><p class=\"wp-block-paragraph\">\u51b7\u9593\u62bc\u3057\u51fa\u3057\u306b\u306f\u3001\u5ba4\u6e29\u3067\u91d1\u5c5e\u3092\u6210\u5f62\u3059\u308b\u5727\u529b\u306b\u8010\u3048\u3089\u308c\u308b\u6750\u6599\u304c\u5fc5\u8981\u3067\u3059\u3002H13 \u306f\u3001\u51b7\u9593\u62bc\u3057\u51fa\u3057\u30d7\u30ed\u30bb\u30b9\u306b\u5fc5\u8981\u306a\u8010\u4e45\u6027\u3068\u7cbe\u5ea6\u3092\u63d0\u4f9b\u3057\u3001\u9577\u671f\u9593\u306b\u308f\u305f\u3063\u3066\u92ed\u3055\u3092\u7dad\u6301\u3057\u306a\u304c\u3089\u3001\u3053\u306e\u8ab2\u984c\u306b\u5fdc\u3048\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u5207\u524a\u5de5\u5177<\/h3><p class=\"wp-block-paragraph\">\u5207\u524a\u5de5\u5177\u306e\u5834\u5408\u3001H13 \u306f\u3001\u53b3\u3057\u3044\u5207\u524a\u7528\u9014\u3067\u3082\u6469\u8017\u306b\u8010\u3048\u308b\u305f\u3081\u306b\u5fc5\u8981\u306a\u786c\u5ea6\u3068\u976d\u6027\u3092\u63d0\u4f9b\u3057\u307e\u3059\u3002\u3053\u308c\u306b\u3088\u308a\u3001\u5de5\u5177\u306e\u92ed\u3044\u72b6\u614b\u304c\u9577\u6301\u3061\u3057\u3001\u751f\u7523\u6027\u304c\u5411\u4e0a\u3057\u3001\u30c0\u30a6\u30f3\u30bf\u30a4\u30e0\u304c\u77ed\u7e2e\u3055\u308c\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">\u9069\u5207\u306a\u6750\u6599\u306e\u9078\u629e: H13 vs H11 vs D2<\/h2><p class=\"wp-block-paragraph\">SteelPro Group \u3067\u306f\u3001\u3053\u3046\u3057\u305f\u9078\u629e\u3092\u304a\u624b\u4f1d\u3044\u3057\u3001\u304a\u5ba2\u69d8\u306e\u7279\u5b9a\u306e\u30cb\u30fc\u30ba\u3068\u8981\u4ef6\u306b\u57fa\u3065\u3044\u3066\u3001\u4f5c\u696d\u306b\u9069\u3057\u305f\u6750\u6599\u3092\u78ba\u5b9f\u306b\u5165\u624b\u3067\u304d\u308b\u3088\u3046\u306b\u3057\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">H13 \u5bfe H11<\/h3><p class=\"wp-block-paragraph\">H13 \u92fc\u306f\u3001\u512a\u308c\u305f\u8010\u71b1\u75b2\u52b4\u6027\u3068\u904e\u9177\u306a\u6761\u4ef6\u4e0b\u3067\u306e\u512a\u308c\u305f\u8010\u4e45\u6027\u3092\u5099\u3048\u3066\u3044\u307e\u3059\u3002\u4e00\u65b9\u3001H11 \u306f\u6a5f\u68b0\u52a0\u5de5\u304c\u5bb9\u6613\u3067\u30b3\u30b9\u30c8\u52b9\u7387\u306b\u512a\u308c\u3066\u3044\u308b\u305f\u3081\u3001\u305d\u308c\u307b\u3069\u8981\u6c42\u306e\u53b3\u3057\u304f\u306a\u3044\u9ad8\u6e29\u4f5c\u696d\u7528\u9014\u306b\u9069\u3057\u3066\u3044\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">H13 \u5bfe D2<\/h3><p class=\"wp-block-paragraph\">\u51b7\u9593\u52a0\u5de5\u3067\u306f\u3001D2 \u306e\u65b9\u304c\u5207\u308c\u5473\u3068\u8010\u4e45\u6027\u306b\u512a\u308c\u3066\u3044\u307e\u3059\u3002\u5207\u524a\u5de5\u5177\u3084\u30b9\u30bf\u30f3\u30d4\u30f3\u30b0 \u30c0\u30a4\u306b\u306f D2 \u306e\u65b9\u304c\u9069\u3057\u3066\u3044\u307e\u3059\u3002\u305f\u3060\u3057\u3001\u9ad8\u6e29\u4f5c\u696d\u306e\u5834\u5408\u306f\u3001\u8010\u71b1\u6027\u306b\u512a\u308c\u305f H13 \u306e\u65b9\u304c D2 \u3088\u308a\u512a\u308c\u3066\u3044\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">\u6700\u9069\u306a\u30d1\u30d5\u30a9\u30fc\u30de\u30f3\u30b9\u3092\u5b9f\u73fe\u3059\u308b\u4fe1\u983c\u6027\u306e\u9ad8\u3044H13\u5de5\u5177\u92fc<\/h2><p class=\"wp-block-paragraph\">SteelPro Group\u3067\u306f\u3001 <a href=\"https:\/\/steelprogroup.com\/ja\/tool-steel\/h13\/\">\u30d7\u30ec\u30df\u30a2\u30e0H13\u5de5\u5177\u92fc<\/a> \u6b63\u78ba\u306a\u4ed5\u69d8\u3068\u4fe1\u983c\u6027\u306e\u9ad8\u3044\u7d0d\u54c1\u3002\u5f53\u793e\u306f\u54c1\u8cea\u3068\u9867\u5ba2\u30b5\u30dd\u30fc\u30c8\u306b\u91cd\u70b9\u3092\u7f6e\u3044\u3066\u304a\u308a\u3001\u304a\u5ba2\u69d8\u306e\u30c4\u30fc\u30eb\u306e\u30cb\u30fc\u30ba\u304c\u52b9\u7387\u7684\u306b\u6e80\u305f\u3055\u308c\u308b\u3088\u3046\u306b\u3057\u3066\u3044\u307e\u3059\u3002\u5f53\u793e\u306e\u7d20\u6750\u304c\u304a\u5ba2\u69d8\u306e\u751f\u7523\u3092\u6700\u9069\u5316\u3059\u308b\u65b9\u6cd5\u306b\u3064\u3044\u3066\u306f\u3001\u4eca\u3059\u3050\u304a\u554f\u3044\u5408\u308f\u305b\u304f\u3060\u3055\u3044\u3002<\/p><p class=\"wp-block-paragraph\"><\/p>","protected":false},"excerpt":{"rendered":"<p>SteelPro Group \u306f\u3001\u3055\u307e\u3056\u307e\u306a\u696d\u754c\u3067\u9577\u5e74\u306e\u7d4c\u9a13\u3092\u6d3b\u304b\u3057\u3001\u6570\u3048\u5207\u308c\u306a\u3044\u307b\u3069\u591a\u304f\u306e\u4f01\u696d\u304c\u30c4\u30fc\u30eb\u696d\u754c\u3067\u751f\u7523\u3092\u6700\u9069\u5316\u3067\u304d\u308b\u3088\u3046\u652f\u63f4\u3057\u3066\u304d\u307e\u3057\u305f\u3002[\u2026]<\/p>","protected":false},"author":1,"featured_media":19986,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"_eb_attr":"","rank_math_lock_modified_date":false,"site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"categories":[4298,4294,4296,4293],"tags":[],"class_list":["post-20004","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-use","category-grades-tool-steel","category-h13","category-tool-steel"],"acf":[],"_links":{"self":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts\/20004","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/comments?post=20004"}],"version-history":[{"count":0,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts\/20004\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/media\/19986"}],"wp:attachment":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/media?parent=20004"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/categories?post=20004"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/tags?post=20004"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}