{"id":20130,"date":"2024-12-30T01:59:00","date_gmt":"2024-12-29T17:59:00","guid":{"rendered":"https:\/\/steelprogroup.com\/?p=20130"},"modified":"2025-01-14T13:16:12","modified_gmt":"2025-01-14T05:16:12","slug":"cpm-15v","status":"publish","type":"post","link":"https:\/\/steelprogroup.com\/ja\/tool-steel\/grades\/cpm-15v\/","title":{"rendered":"CPM 15V \u5de5\u5177\u92fc\u7c89\u672b\u91d1\u5c5e"},"content":{"rendered":"<p class=\"wp-block-paragraph\">SteelPro Group \u306f\u3001\u9ad8\u6027\u80fd CPM 15V \u5de5\u5177\u92fc\u306e\u4fe1\u983c\u3067\u304d\u308b\u30b5\u30d7\u30e9\u30a4\u30e4\u30fc\u3067\u3042\u308b\u3053\u3068\u3092\u8a87\u308a\u306b\u601d\u3063\u3066\u3044\u307e\u3059\u3002\u5f53\u793e\u306f\u3001\u5353\u8d8a\u6027\u3068\u4fe1\u983c\u6027\u3092\u91cd\u8996\u3057\u3001\u6700\u3082\u56f0\u96e3\u306a\u7523\u696d\u8981\u4ef6\u306b\u5bfe\u5fdc\u3059\u308b\u3088\u3046\u306b\u8a2d\u8a08\u3055\u308c\u305f\u30ab\u30b9\u30bf\u30de\u30a4\u30ba\u3055\u308c\u305f\u30bd\u30ea\u30e5\u30fc\u30b7\u30e7\u30f3\u3092\u63d0\u4f9b\u3057\u307e\u3059\u3002\u5f53\u793e\u306f\u3001\u304a\u5ba2\u69d8\u306e\u30d7\u30ed\u30b8\u30a7\u30af\u30c8\u3092\u6b63\u78ba\u306b\u63a8\u9032\u3057\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">CPM 15V \u30b9\u30c1\u30fc\u30eb\u3068\u306f\u4f55\u3067\u3059\u304b?<\/h2><p class=\"wp-block-paragraph\">CPM 15V \u92fc\u306f\u3001Crucible \u793e\u304c\u958b\u767a\u3057\u305f\u9ad8\u6027\u80fd\u7c89\u672b\u51b6\u91d1\u5de5\u5177\u92fc\u3067\u3059\u3002CPM 10V \u3088\u308a\u3082 50% \u591a\u3044\u70ad\u5316\u30d0\u30ca\u30b8\u30a6\u30e0\u3092\u542b\u6709\u3057\u3001\u8010\u6469\u8017\u6027\u304c\u5411\u4e0a\u3057\u3001\u5de5\u5177\u5bff\u547d\u304c\u9577\u304f\u306a\u308a\u307e\u3059\u3002CPM \u30d7\u30ed\u30bb\u30b9\u306b\u3088\u3063\u3066\u5b9f\u73fe\u3055\u308c\u305f\u92fc\u306e\u5747\u4e00\u306a\u5fae\u7d30\u69cb\u9020\u306b\u3088\u308a\u3001\u512a\u308c\u305f\u5bf8\u6cd5\u5b89\u5b9a\u6027\u3001\u7814\u524a\u6027\u3001\u976d\u6027\u304c\u78ba\u4fdd\u3055\u308c\u307e\u3059\u3002&nbsp;<\/p><p class=\"wp-block-paragraph\">CPM 15V \u306f\u3001\u7834\u640d\u3084\u8907\u96d1\u306a\u8a2d\u8a08\u306b\u3088\u308a\u8d85\u786c\u5de5\u5177\u304c\u6a5f\u80fd\u3057\u306a\u304f\u306a\u308b\u7528\u9014\u3067\u3001\u8d85\u786c\u5de5\u5177\u306e\u4ee3\u66ff\u3068\u3057\u3066\u6700\u9069\u3067\u3059\u3002\u4e3b\u306b\u51b7\u9593\u52a0\u5de5\u5de5\u5177\u3084\u305d\u306e\u4ed6\u306e\u6469\u8017\u306e\u6fc0\u3057\u3044\u7528\u9014\u3067\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">CPM 15V \u9244\u92fc\u88fd\u54c1\u306e\u5f62\u614b\u3068\u4f9b\u7d66\u7bc4\u56f2<\/h2><p class=\"wp-block-paragraph\">\u5f53\u793e\u306e CPM 15V \u5de5\u5177\u92fc\u306f\u3001ASTM\u3001SAE\u3001JIS \u306a\u3069\u306e\u696d\u754c\u6a19\u6e96\u8981\u4ef6\u3092\u6e80\u305f\u3057\u3066\u304a\u308a\u3001\u6469\u8017\u306e\u6fc0\u3057\u3044\u7528\u9014\u3067\u3082\u4fe1\u983c\u6027\u306e\u9ad8\u3044\u30d1\u30d5\u30a9\u30fc\u30de\u30f3\u30b9\u3092\u4fdd\u8a3c\u3057\u307e\u3059\u3002\u4ee5\u4e0b\u3067\u306f\u3001\u3055\u307e\u3056\u307e\u306a\u88fd\u54c1\u5f62\u72b6\u3068\u30b5\u30a4\u30ba\u3092\u53d6\u308a\u63c3\u3048\u3066\u304a\u308a\u3001\u7279\u5b9a\u306e\u30d7\u30ed\u30b8\u30a7\u30af\u30c8\u306e\u30cb\u30fc\u30ba\u306b\u5408\u308f\u305b\u3066\u30ab\u30b9\u30bf\u30e0\u5bf8\u6cd5\u306b\u3082\u5bfe\u5fdc\u3067\u304d\u308b\u67d4\u8edf\u6027\u3092\u5099\u3048\u3066\u3044\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\"><strong>\u30d0\u30fc\u3068\u30ed\u30c3\u30c9<\/strong>:<\/p><ul class=\"wp-block-list\"><li>\u76f4\u5f84: 6 mm \uff5e 300 mm (0.24 \u30a4\u30f3\u30c1 \uff5e 11.81 \u30a4\u30f3\u30c1)<\/li>\n\n<li>\u9577\u3055: 500 mm \uff5e 3,000 mm (19.69 \u30a4\u30f3\u30c1 \uff5e 118.11 \u30a4\u30f3\u30c1)<\/li><\/ul><p class=\"wp-block-paragraph\"><strong>\u30d5\u30e9\u30c3\u30c8\u30b9\u30c8\u30c3\u30af:<\/strong><\/p><ul class=\"wp-block-list\"><li>\u539a\u3055: 3 mm \uff5e 100 mm (0.12 \u30a4\u30f3\u30c1 \uff5e 3.94 \u30a4\u30f3\u30c1)<\/li>\n\n<li>\u5e45: 50 mm \uff5e 300 mm (1.97 \u30a4\u30f3\u30c1 \uff5e 11.81 \u30a4\u30f3\u30c1)<\/li>\n\n<li>\u9577\u3055: 200 mm \uff5e 3,000 mm (7.87 \u30a4\u30f3\u30c1 \uff5e 118.11 \u30a4\u30f3\u30c1)<\/li><\/ul><p class=\"wp-block-paragraph\"><strong>\u30e9\u30a6\u30f3\u30c9:<\/strong><\/p><ul class=\"wp-block-list\"><li>\u76f4\u5f84: 10 mm \uff5e 250 mm (0.39 \u30a4\u30f3\u30c1 \uff5e 9.84 \u30a4\u30f3\u30c1)<\/li>\n\n<li>\u9577\u3055: 300 mm \uff5e 3,000 mm (11.81 \u30a4\u30f3\u30c1 \uff5e 118.11 \u30a4\u30f3\u30c1)<\/li><\/ul><h2 class=\"wp-block-heading\">CPM 15V \u92fc\u306e\u5316\u5b66\u6210\u5206<\/h2><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u30a8\u30ec\u30e1\u30f3\u30c8<\/strong><\/td><td><strong>\u30b3\u30f3\u30c6\u30f3\u30c4\uff08%\uff09<\/strong><\/td><\/tr><tr><td>\u30ab\u30fc\u30dc\u30f3\uff08C\uff09<\/td><td>3.4<\/td><\/tr><tr><td>\u30af\u30ed\u30e0\uff08Cr\uff09<\/td><td>5.25<\/td><\/tr><tr><td>\u9244\uff08Fe\uff09<\/td><td>75.55\u3001\u6b8b\u9ad8\u3068\u3057\u3066<\/td><\/tr><tr><td>\u30e2\u30ea\u30d6\u30c7\u30f3 (Mo)<\/td><td>1.3<\/td><\/tr><tr><td>\u30d0\u30ca\u30b8\u30a6\u30e0 (V)<\/td><td>14.5<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">CPM 15V \u92fc\u306e\u7269\u7406\u7684\u7279\u6027<\/h2><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u30d7\u30ed\u30d1\u30c6\u30a3<\/strong><\/td><td><strong>\u30e1\u30c8\u30ea\u30c3\u30af\u5024<\/strong><\/td><td><strong>\u30a4\u30f3\u30da\u30ea\u30a2\u30eb\u30fb\u30d0\u30ea\u30e5\u30fc<\/strong><\/td><\/tr><tr><td>\u5bc6\u5ea6<\/td><td>7.25g\/cc<\/td><td>0.262 \u30dd\u30f3\u30c9\/\u30a4\u30f3\u30c1\u00b3<\/td><\/tr><tr><td>\u878d\u70b9<\/td><td>1,340\u2103<\/td><td>2,443\u00b0F<\/td><\/tr><tr><td>\u71b1\u4f1d\u5c0e\u7387<\/td><td>25.3W\/m\u00b7K<\/td><td>17.5 BTU\u00b7ft\/hr\u00b7\u00b0F\u00b7ft\u00b2<\/td><\/tr><tr><td>\u6bd4\u71b1<\/td><td>0.46 J\/g-K<\/td><td>0.11 BTU\/lb-\u00b0F<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">CPM 15V\u92fc\u306e\u6a5f\u68b0\u7684\u7279\u6027<\/h2><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u30d7\u30ed\u30d1\u30c6\u30a3<\/strong><\/td><td><strong>\u30e1\u30c8\u30ea\u30c3\u30af\u5024<\/strong><\/td><td><strong>\u30a4\u30f3\u30da\u30ea\u30a2\u30eb\u30fb\u30d0\u30ea\u30e5\u30fc<\/strong><\/td><\/tr><tr><td>\u786c\u5ea6\uff08HB\uff09<\/td><td>255 &#8211; 277<\/td><td>255 &#8211; 277<\/td><\/tr><tr><td>\u786c\u5ea6\uff08HRC\uff09<\/td><td>61 &#8211; 63<\/td><td>61 &#8211; 63<\/td><\/tr><tr><td>\u5f3e\u6027\u4fc2\u6570<\/td><td>235GPa<\/td><td>34,100 ksi<\/td><\/tr><tr><td>\u30b7\u30e3\u30eb\u30d4\u30fc\u885d\u6483\uff08\u30aa\u30fc\u30b9\u30c6\u30ca\u30a4\u30c8\u5316\u6e29\u5ea6 \u2013 1175\u00b0C\uff09<\/td><td>11.0 \u30b8\u30e5\u30fc\u30eb<\/td><td>8.11 \u30d5\u30a3\u30fc\u30c8\u30dd\u30f3\u30c9<\/td><\/tr><tr><td>\u30b7\u30e3\u30eb\u30d4\u30fc\u885d\u6483\uff08\u30aa\u30fc\u30b9\u30c6\u30ca\u30a4\u30c8\u5316\u6e29\u5ea6 \u2013 1120\u00b0C\uff09<\/td><td>12.0 \u30b8\u30e5\u30fc\u30eb<\/td><td>8.85 \u30d5\u30a3\u30fc\u30c8\u30dd\u30f3\u30c9<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">CPM 15V \u92fc\u71b1\u51e6\u7406<\/h2><h3 class=\"wp-block-heading\">\u30a2\u30cb\u30fc\u30ea\u30f3\u30b0<\/h3><p class=\"wp-block-paragraph\">\u5185\u90e8\u5fdc\u529b\u3092\u4f4e\u6e1b\u3057\u3001\u4e00\u8cab\u3057\u305f\u5fae\u7d30\u69cb\u9020\u3092\u5f97\u308b\u305f\u3081\u306b\u3001CPM 15V\u306f\u3001 <strong>1600\u00b0F\uff08870\u00b0C\uff09<\/strong> 2\u6642\u9593\u3002\u305d\u306e\u5f8c\u3001\u92fc\u306f\u6700\u5927\u901f\u5ea6\u3067\u3086\u3063\u304f\u308a\u3068\u51b7\u5374\u3059\u308b\u5fc5\u8981\u304c\u3042\u308a\u307e\u3059\u3002 <strong>30\u00b0F (15\u00b0C)<\/strong> 1\u6642\u9593\u3042\u305f\u308a <strong>1000\u00b0F\uff08540\u00b0C\uff09<\/strong>\u305d\u306e\u5f8c\u3001\u7a7a\u51b7\u307e\u305f\u306f\u7089\u51b7\u3059\u308b\u3002\u3053\u308c\u306b\u3088\u308a\u3001\u786c\u5ea6\u306f <strong>255\/277 \u5186<\/strong>.<\/p><h3 class=\"wp-block-heading\">\u30b9\u30c8\u30ec\u30b9\u89e3\u6d88<\/h3><p class=\"wp-block-paragraph\">\u6a5f\u68b0\u52a0\u5de5\u5f8c\u3001CPM 15V\u306f\u6b8b\u7559\u5fdc\u529b\u3092\u8efd\u6e1b\u3059\u308b\u305f\u3081\u306b\u5fdc\u529b\u7de9\u548c\u51e6\u7406\u3092\u53d7\u3051\u308b\u5fc5\u8981\u304c\u3042\u308a\u307e\u3059\u3002\u3053\u308c\u306f\u3001\u6750\u6599\u3092\u4ee5\u4e0b\u306e\u6e29\u5ea6\u7bc4\u56f2\u306b\u52a0\u71b1\u3059\u308b\u3053\u3068\u306b\u3088\u3063\u3066\u9054\u6210\u3055\u308c\u307e\u3059\u3002 <strong>1100\uff5e1300\u00b0F\uff08595\uff5e740\u00b0C\uff09 <\/strong>\u305d\u3057\u3066\u305d\u308c\u3092\u7dad\u6301\u3059\u308b<strong> 2\u6642\u9593<\/strong>\u305d\u306e\u5f8c\u3001\u7a7a\u6c17\u307e\u305f\u306f\u7089\u306e\u4e2d\u3067\u51b7\u5374\u3057\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u786c\u5316<\/h3><h3 class=\"wp-block-heading\"><strong>\u4e88\u71b1<\/strong><\/h3><p class=\"wp-block-paragraph\">\u307e\u305a\u92fc\u3092\u52a0\u71b1\u3057\u3066 <strong>1500\uff5e1550\u00b0F\uff08816\uff5e845\u00b0C\uff09<\/strong> \u5b89\u5b9a\u3055\u305b\u308b\u305f\u3081\u30012\u56de\u76ee\u306e\u4e88\u71b1\u6bb5\u968e\u3092\u304a\u52e7\u3081\u3057\u307e\u3059\u3002 <strong>1850\uff5e1900\u00b0F\uff081010\uff5e1040\u00b0C\uff09<\/strong>\u7279\u306b\u771f\u7a7a\u307e\u305f\u306f\u5927\u6c17\u5727\u786c\u5316\u306e\u5834\u5408\u3001\u6700\u9069\u306a\u7d50\u679c\u304c\u4fdd\u8a3c\u3055\u308c\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\"><strong>\u30aa\u30fc\u30b9\u30c6\u30ca\u30a4\u30c8\u5316<\/strong><\/p><p class=\"wp-block-paragraph\">\u92fc\u3092\u4e88\u71b1\u304b\u3089\u6025\u901f\u306b\u52a0\u71b1\u3057\u3001\u901a\u5e38\u306f2\u756a\u76ee\u306e\u7089\u306b\u79fb\u3057\u307e\u3059\u3002\u9ad8\u71b1\u30aa\u30fc\u30b9\u30c6\u30ca\u30a4\u30c8\u5316\u6bb5\u968e\u306f\u3001\u7089\u307e\u305f\u306f\u5869\u6d74\u3067\u3001 <strong>1950\uff5e2150\u00b0F\uff081065\uff5e1175\u00b0C\uff09<\/strong> \u306e\u305f\u3081\u306b <strong>10\u301c30\u5206<\/strong>\u92fc\u304c\u6240\u671b\u306e\u6e29\u5ea6\u3068\u5747\u4e00\u6027\u306b\u9054\u3059\u308b\u3053\u3068\u3092\u4fdd\u8a3c\u3057\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\"><strong>\u713c\u304d\u5165\u308c<\/strong><\/h3><p class=\"wp-block-paragraph\">\u30aa\u30fc\u30b9\u30c6\u30ca\u30a4\u30c8\u5316\u5f8c\u3001CPM 15V \u306f\u6700\u5927\u306e\u786c\u5ea6\u3092\u5f97\u308b\u305f\u3081\u306b\u713c\u304d\u5165\u308c\u3059\u308b\u5fc5\u8981\u304c\u3042\u308a\u307e\u3059\u3002\u65ad\u9762\u306e\u539a\u3055\u306b\u5fdc\u3058\u3066\u6b21\u306e\u3088\u3046\u306b\u306a\u308a\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\"><strong>\u539a\u30553\u30a4\u30f3\u30c1\u4ee5\u4e0b\u306e\u30bb\u30af\u30b7\u30e7\u30f3\u306e\u5834\u5408\u3001 <\/strong>\u6700\u9ad8\u306e\u786c\u5ea6\u3092\u9054\u6210\u3059\u308b\u306b\u306f\u3001\u7a7a\u6c17\u4e2d\u306e\u81ea\u7136\u51b7\u5374\u3067\u5341\u5206\u3067\u3059\u3002<\/p><p class=\"wp-block-paragraph\"><strong>\u539a\u3044\u90e8\u5206\u306e\u5834\u5408<\/strong>\u6240\u671b\u306e\u786c\u5ea6\u3092\u5f97\u308b\u306b\u306f\u3001\u52a0\u5727\u30ac\u30b9\u3001\u6e29\u6cb9\u3001\u5869\u306a\u3069\u306e\u3088\u308a\u901f\u3044\u65b9\u6cd5\u3092\u4f7f\u7528\u3057\u3066\u713c\u5165\u308c\u3092\u884c\u3046\u5fc5\u8981\u304c\u3042\u308a\u307e\u3059\u3002&nbsp;<\/p><ul class=\"wp-block-list\"><li>\u9069\u5207\u306a\u786c\u5ea6\u3092\u78ba\u4fdd\u3059\u308b\u306b\u306f\u3001\u52a0\u5727\u30ac\u30b9\u306b\u6700\u4f4e\u3067\u3082\u4ee5\u4e0b\u306e\u6025\u51b7\u5727\u529b\u304c\u5fc5\u8981\u3067\u3059\u3002 <strong>4\u30d0\u30fc<\/strong> \u81e8\u754c\u51b7\u5374\u901f\u5ea6\u306f\u4ee5\u4e0b <strong>1000\u00b0F\uff08538\u00b0C\uff09<\/strong>.<\/li>\n\n<li>\u6cb9\u713c\u304d\u5165\u308c\u306e\u5834\u5408\u306f\u3001\u92fc\u304c\u9ed2\u304f\u306a\u308b\u307e\u3067\u7d04100\u2103\u3067\u51b7\u3084\u3057\u307e\u3059\u3002 <strong>900\u00b0F\uff08482\u00b0C\uff09<\/strong>\u305d\u306e\u5f8c\u3001\u7a7a\u6c17\u4e2d\u3067\u51b7\u3084\u3057\u3066 <strong>150\u301c125\u00b0F\uff0866\u301c51\u00b0C\uff09<\/strong>.<\/li>\n\n<li>\u5869\u713c\u304d\u5165\u308c\u306f\u3001 <strong>1000\uff5e1100\u00b0F\uff08538\uff5e593\u00b0C\uff09<\/strong>.<\/li><\/ul><h3 class=\"wp-block-heading\">\u713c\u304d\u623b\u3057<\/h3><p class=\"wp-block-paragraph\">\u6700\u5f8c\u306b\u3001CPM 15V\u306f\u3001\u786c\u5ea6\u3068\u976d\u6027\u306e\u671b\u307e\u3057\u3044\u30d0\u30e9\u30f3\u30b9\u3092\u5f97\u308b\u305f\u3081\u306b\u713c\u304d\u623b\u3057\u3092\u884c\u3046\u5fc5\u8981\u304c\u3042\u308a\u307e\u3059\u3002\u786c\u5316\u5f8c\u3001\u92fc\u3092\u6b21\u306e\u6e29\u5ea6\u3067\u713c\u304d\u623b\u3057\u3057\u307e\u3059\u3002 <strong>400\uff5e1000\u00b0F\uff08204\uff5e538\u00b0C\uff09<\/strong>\u7279\u5b9a\u306e\u7528\u9014\u306e\u8981\u4ef6\u306b\u5fdc\u3058\u3066\u7570\u306a\u308a\u307e\u3059\u3002\u786c\u5ea6\u3092\u9054\u6210\u3059\u308b\u305f\u3081\u306e\u6a19\u6e96\u7684\u306a\u63a8\u5968\u4e8b\u9805\u306f\u3001 <strong>60-62HRC<\/strong> \u3088\u308a\u9ad8\u3044\u7bc4\u56f2\u3067\u713c\u304d\u5165\u308c\u3059\u308b\u3053\u3068\u3067\u3059\u3002<\/p><h2 class=\"wp-block-heading\">CPM 15V \u30b9\u30c1\u30fc\u30eb\u30a2\u30d7\u30ea\u30b1\u30fc\u30b7\u30e7\u30f3<\/h2><h3 class=\"wp-block-heading\">\u51b7\u9593\u52a0\u5de5\u5de5\u5177<\/h3><ul class=\"wp-block-list\"><li><strong>\u30d1\u30f3\u30c1\u3068\u30c0\u30a4<\/strong>: \u9ad8\u3044\u8010\u6469\u8017\u6027\u304c\u8981\u6c42\u3055\u308c\u308b\u30b9\u30bf\u30f3\u30d4\u30f3\u30b0\u3084\u30d1\u30f3\u30c1\u30f3\u30b0\u52a0\u5de5\u306b\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/li>\n\n<li><strong>\u62bc\u3057\u51fa\u3057\u30c0\u30a4\u30b9<\/strong>: \u30c4\u30fc\u30eb\u306e\u5b8c\u5168\u6027\u3092\u7dad\u6301\u3057\u306a\u304c\u3089\u9ad8\u5727\u4e0b\u3067\u6750\u6599\u3092\u6210\u5f62\u3057\u307e\u3059\u3002<\/li>\n\n<li><strong>\u305b\u3093\u65ad\u30d6\u30ec\u30fc\u30c9<\/strong>: \u8010\u4e45\u6027\u304c\u91cd\u8981\u3068\u306a\u308b\u305b\u3093\u65ad\u7528\u9014\u306b\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/li>\n\n<li><strong>\u30b9\u30ea\u30c3\u30bf\u30fc\u30d6\u30ec\u30fc\u30c9<\/strong>: \u91d1\u5c5e\u3084\u305d\u306e\u4ed6\u306e\u6750\u6599\u3092\u9ad8\u901f\u30d7\u30ed\u30bb\u30b9\u3067\u5207\u65ad\u307e\u305f\u306f\u30b9\u30ea\u30c3\u30c8\u3057\u307e\u3059\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">\u5207\u524a\u5de5\u5177<\/h3><ul class=\"wp-block-list\"><li><strong>\u30c9\u30ea\u30eb: <\/strong>\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u3084\u9ad8\u5f37\u5ea6\u91d1\u5c5e\u306a\u3069\u306e\u5f37\u56fa\u306a\u6750\u6599\u306e\u7a74\u3042\u3051\u7528\u306b\u8a2d\u8a08\u3055\u308c\u3066\u3044\u307e\u3059\u3002<\/li>\n\n<li><strong>\u30ea\u30fc\u30de\u30fc<\/strong>: \u9ad8\u7cbe\u5ea6\u304b\u3064\u6700\u5c0f\u9650\u306e\u6469\u8017\u3067\u7a74\u3092\u4ed5\u4e0a\u3052\u307e\u3059\u3002<\/li>\n\n<li><strong>\u30bf\u30c3\u30d7<\/strong>: \u5203\u5148\u306e\u8010\u4e45\u6027\u304c\u8981\u6c42\u3055\u308c\u308b\u6750\u6599\u306e\u306d\u3058\u5207\u308a\u4f5c\u696d\u306b\u3002<\/li>\n\n<li><strong>\u30a8\u30f3\u30c9\u30df\u30eb<\/strong>: \u5203\u5148\u306e\u8010\u6469\u8017\u6027\u306b\u512a\u308c\u3001\u3055\u307e\u3056\u307e\u306a\u6750\u6599\u306e\u52a0\u5de5\u306b\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">\u6210\u5f62\u30c4\u30fc\u30eb<\/h3><ul class=\"wp-block-list\"><li><strong>\u935b\u9020\u91d1\u578b<\/strong>: \u91d1\u5c5e\u90e8\u54c1\u3092\u6210\u5f62\u3059\u308b\u305f\u3081\u306b\u71b1\u9593\u307e\u305f\u306f\u51b7\u9593\u935b\u9020\u30d7\u30ed\u30bb\u30b9\u3067\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/li>\n\n<li><strong>\u30b9\u30bf\u30f3\u30d4\u30f3\u30b0\u30c0\u30a4<\/strong>: \u30b9\u30bf\u30f3\u30d4\u30f3\u30b0\u91d1\u578b: \u7279\u306b\u81ea\u52d5\u8eca\u3084\u822a\u7a7a\u5b87\u5b99\u5206\u91ce\u3067\u306e\u91d1\u5c5e\u90e8\u54c1\u306e\u5927\u91cf\u751f\u7523\u306b\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/li>\n\n<li><strong>\u5727\u7e2e\u91d1\u578b<\/strong>: \u6210\u5f62\u5de5\u7a0b\u306b\u304a\u3044\u3066\u5727\u7e2e\u306b\u3088\u308a\u90e8\u54c1\u3092\u6210\u5f62\u3057\u307e\u3059\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">\u6469\u8017\u90e8\u54c1<\/h3><ul class=\"wp-block-list\"><li><strong>\u30ed\u30fc\u30e9\u30fc<\/strong>: \u6750\u6599\u304c\u9023\u7d9a\u7684\u306b\u79fb\u52d5\u3059\u308b\u30b3\u30f3\u30d9\u30a2 \u30b7\u30b9\u30c6\u30e0\u3084\u305d\u306e\u4ed6\u306e\u6a5f\u68b0\u3067\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/li>\n\n<li><strong>\u30e9\u30a4\u30ca\u30fc<\/strong>: \u7c89\u7815\u6a5f\u3084\u88fd\u7c89\u6a5f\u306a\u3069\u3001\u6fc0\u3057\u3044\u6469\u8017\u306b\u3055\u3089\u3055\u308c\u308b\u6a5f\u68b0\u7528\u3002<\/li>\n\n<li><strong>\u6469\u8017\u30d7\u30ec\u30fc\u30c8<\/strong>: \u9ad8\u30b9\u30c8\u30ec\u30b9\u4f5c\u696d\u6642\u306e\u6469\u8017\u306b\u8010\u3048\u308b\u8a2d\u5099\u3092\u8a2d\u7f6e\u3057\u307e\u3057\u305f\u3002<\/li>\n\n<li><strong>\u30d4\u30f3\u3068\u30d6\u30c3\u30b7\u30f3\u30b0<\/strong>: \u983b\u7e41\u306a\u6469\u8017\u306b\u8010\u3048\u308b\u6a5f\u68b0\u30b7\u30b9\u30c6\u30e0\u306b\u304a\u3044\u3066\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">\u713c\u7d50\u304a\u3088\u3073\u9ad8\u6e29\u30c4\u30fc\u30eb<\/h3><ul class=\"wp-block-list\"><li><strong>\u713c\u7d50\u30c0\u30a4\u30b9<\/strong>: \u7c89\u672b\u51b6\u91d1\u30d7\u30ed\u30bb\u30b9\u3067\u91d1\u5c5e\u7c89\u672b\u304b\u3089\u90e8\u54c1\u3092\u5f62\u6210\u3059\u308b\u305f\u3081\u306b\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/li>\n\n<li><strong>\u30db\u30c3\u30c8\u30d7\u30ec\u30b9\u30c4\u30fc\u30eb<\/strong>: \u88fd\u9020\u6642\u306b\u6750\u6599\u3092\u9ad8\u6e29\u3067\u30d7\u30ec\u30b9\u3059\u308b\u305f\u3081\u3002<\/li>\n\n<li><strong>\u30c0\u30a4\u30a4\u30f3\u30b5\u30fc\u30c8<\/strong>: \u9ad8\u3044\u8010\u6469\u8017\u6027\u3068\u71b1\u5b89\u5b9a\u6027\u304c\u6c42\u3081\u3089\u308c\u308b\u9ad8\u6e29\u6210\u5f62\u30d7\u30ed\u30bb\u30b9\u3002<\/li><\/ul><h2 class=\"wp-block-heading\">CPM 15V \u5bfe M390<\/h2><p class=\"wp-block-paragraph\">CPM 15V \u306f\u8010\u6469\u8017\u6027\u306b\u512a\u308c\u3001M390 \u306f\u8010\u8150\u98df\u6027\u306b\u512a\u308c\u3066\u3044\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\">CPM 15V \u306f\u8010\u6469\u8017\u6027\u306b\u512a\u308c\u305f\u5de5\u5177\u92fc\u3067\u3001\u51b7\u9593\u52a0\u5de5\u5de5\u5177\u306a\u3069\u3001\u512a\u308c\u305f\u8010\u6469\u8017\u6027\u304c\u6c42\u3081\u3089\u308c\u308b\u7528\u9014\u306b\u6700\u9069\u3067\u3059\u3002\u4e00\u65b9\u3001M390 \u306f\u512a\u308c\u305f\u8010\u8150\u98df\u6027\u3068\u5203\u6301\u3061\u306e\u826f\u3055\u3067\u77e5\u3089\u308c\u308b\u9ad8\u7d1a\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u3067\u3001\u6e7f\u6c17\u3084\u8150\u98df\u74b0\u5883\u306b\u3055\u3089\u3055\u308c\u308b\u30ca\u30a4\u30d5\u3084\u5de5\u5177\u306b\u9069\u3057\u3066\u3044\u307e\u3059\u3002&nbsp;<\/p><h2 class=\"wp-block-heading\">CPM 15V \u5bfe S30V<\/h2><p class=\"wp-block-paragraph\">CPM 15V\u306f\u8010\u6469\u8017\u6027\u306b\u512a\u308c\u3066\u304a\u308a\u3001 <a href=\"https:\/\/steelprogroup.com\/ja\/tool-steel\/grades\/cpm-s30v\/\">S30V<\/a> \u5168\u4f53\u7684\u306a\u976d\u6027\u3068\u8010\u8150\u98df\u6027\u306b\u512a\u308c\u3066\u3044\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\">CPM 15V \u306f\u30d0\u30ca\u30b8\u30a6\u30e0\u542b\u6709\u91cf\u304c\u591a\u3044\u305f\u3081\u8010\u6469\u8017\u6027\u306b\u512a\u308c\u3066\u304a\u308a\u3001\u5de5\u5177\u7528\u9014\u306b\u6700\u9069\u3067\u3059\u3002\u4e00\u65b9\u3001S30V \u306f\u8010\u6469\u8017\u6027\u3068\u8010\u8150\u98df\u6027\u306e\u30d0\u30e9\u30f3\u30b9\u304c\u53d6\u308c\u305f\u9ad8\u6027\u80fd\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u3067\u3001\u904e\u9177\u3067\u6e7f\u6c17\u306e\u591a\u3044\u74b0\u5883\u3067\u4f7f\u7528\u3055\u308c\u308b\u30ca\u30a4\u30d5\u3084\u5de5\u5177\u306b\u6700\u9069\u3067\u3059\u3002<\/p><h2 class=\"wp-block-heading\">\u3042\u3089\u3086\u308b\u30cb\u30fc\u30ba\u306b\u5fdc\u3048\u308bCPM 15V\u5de5\u5177\u92fc\u30bd\u30ea\u30e5\u30fc\u30b7\u30e7\u30f3<\/h2><p class=\"wp-block-paragraph\">SteelPro Group\u3067\u306f\u3001\u68d2\u92fc\u3001\u30ed\u30c3\u30c9\u3001\u5e73\u92fc\u306a\u3069\u3055\u307e\u3056\u307e\u306a\u5f62\u72b6\u306eCPM 15V\u5de5\u5177\u92fc\u3092\u63d0\u4f9b\u3057\u3066\u3044\u307e\u3059\u3002 <a href=\"https:\/\/steelprogroup.com\/ja\/tool-steel\/h13\/\">\u71b1\u3044\u4ed5\u4e8b<\/a>, <a href=\"https:\/\/steelprogroup.com\/ja\/tool-steel\/cr12mov\/\">\u51b7\u9593\u4f5c\u696d<\/a>\u305d\u3057\u3066 <a href=\"https:\/\/steelprogroup.com\/ja\/tool-steel\/w18cr4v\/\">\u9ad8\u901f\u5ea6\u5de5\u5177\u92fc<\/a>\u304a\u5ba2\u69d8\u306e\u7279\u5b9a\u306e\u8981\u4ef6\u3092\u6e80\u305f\u3059\u8868\u9762\u51e6\u7406\u304a\u3088\u3073\u7814\u78e8\u30b5\u30fc\u30d3\u30b9\u3082\u63d0\u4f9b\u3057\u3066\u3044\u307e\u3059\u3002&nbsp;<\/p><p class=\"wp-block-paragraph\">\u304a\u5ba2\u69d8\u306e\u30d7\u30ed\u30b8\u30a7\u30af\u30c8\u306e\u30cb\u30fc\u30ba\u304c\u4f55\u3067\u3042\u308c\u3001\u5f53\u793e\u306f\u7cbe\u5ea6\u3068\u4fe1\u983c\u6027\u3092\u5099\u3048\u305f\u9069\u5207\u306a\u92fc\u6750\u3092\u304a\u5c4a\u3051\u3057\u307e\u3059\u3002\u4eca\u3059\u3050\u304a\u554f\u3044\u5408\u308f\u305b\u3044\u305f\u3060\u304d\u3001\u59cb\u3081\u307e\u3057\u3087\u3046\u3002<\/p>","protected":false},"excerpt":{"rendered":"<p>At SteelPro Group, we are proud to be a trusted supplier of high-performance CPM 15V tool steel. Focusing on excellence [&hellip;]<\/p>","protected":false},"author":1,"featured_media":20156,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"_eb_attr":"","rank_math_lock_modified_date":false,"site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"categories":[4294,4293],"tags":[],"class_list":["post-20130","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-grades-tool-steel","category-tool-steel"],"acf":[],"_links":{"self":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts\/20130","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/comments?post=20130"}],"version-history":[{"count":0,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts\/20130\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/media\/20156"}],"wp:attachment":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/media?parent=20130"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/categories?post=20130"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/tags?post=20130"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}