{"id":20218,"date":"2025-01-07T08:46:00","date_gmt":"2025-01-07T00:46:00","guid":{"rendered":"https:\/\/steelprogroup.com\/?p=20218"},"modified":"2025-01-08T09:29:18","modified_gmt":"2025-01-08T01:29:18","slug":"grades-3","status":"publish","type":"post","link":"https:\/\/steelprogroup.com\/ja\/tool-steel\/grades\/","title":{"rendered":"\u5de5\u5177\u92fc\u306e\u4e00\u822c\u7684\u306a\u30b0\u30ec\u30fc\u30c9\u30ac\u30a4\u30c9: \u7279\u6027\u3001\u7528\u9014\u3001\u6bd4\u8f03"},"content":{"rendered":"<p class=\"wp-block-paragraph\">\u672c\u7269\u306e\u5de5\u5177\u92fc\u306f\u3001\u7279\u5225\u306b\u914d\u5408\u3055\u308c\u305f\u92fc\u5408\u91d1\u3067\u3059\u3002\u3053\u308c\u3089\u306e\u5408\u91d1\u306f\u3001\u88fd\u9020\u696d\u3084\u91d1\u5c5e\u52a0\u5de5\u696d\u5411\u3051\u306b\u7279\u5225\u306b\u8a2d\u8a08\u3055\u308c\u3066\u304a\u308a\u3001\u6975\u5ea6\u306e\u6a5f\u68b0\u7684\u30b9\u30c8\u30ec\u30b9\u3084\u9ad8\u6e29\u4e0b\u3067\u3082\u9ad8\u3044\u786c\u5ea6\u3001\u5f37\u5ea6\u3001\u8010\u6469\u8017\u6027\u3092\u7dad\u6301\u3057\u307e\u3059\u3002\u79c1\u305f\u3061\u304c\u65e5\u5e38\u751f\u6d3b\u3067\u4f7f\u7528\u3057\u3066\u3044\u308b\u4e00\u822c\u7684\u306a\u30cf\u30f3\u30de\u30fc\u3001\u4e00\u822c\u7684\u306a\u30e4\u30b9\u30ea\u3001\u30ce\u30df\u306f\u3001\u672c\u7269\u306e\u5de5\u5177\u92fc\u3067\u4f5c\u3089\u308c\u3066\u3044\u307e\u305b\u3093\u3002&nbsp;<\/p><p class=\"wp-block-paragraph\">\u5de5\u5177\u92fc\u306e\u4e16\u754c\u306f\u591a\u69d8\u3067\u3059\u300210 \u5e74\u3092\u8d85\u3048\u308b\u751f\u7523\u7d4c\u9a13\u3092\u6301\u3064\u5de5\u5177\u92fc\u30b5\u30d7\u30e9\u30a4\u30e4\u30fc\u3068\u3057\u3066\u3001SteelPro Group \u306f\u4e00\u822c\u7684\u306a\u5de5\u5177\u92fc\u306e\u30b0\u30ec\u30fc\u30c9\u3092\u7d39\u4ecb\u3057\u3001\u3053\u306e\u6750\u6599\u3092\u771f\u306b\u7406\u89e3\u3059\u308b\u304a\u624b\u4f1d\u3044\u3092\u3057\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">\u5de5\u5177\u92fc\u306e\u4e00\u822c\u7684\u306a\u7a2e\u985e<\/h2><h3 class=\"wp-block-heading\">\u6c34\u786c\u5316\u5de5\u5177\u92fc\uff08W\u30b7\u30ea\u30fc\u30ba\uff09<\/h3><p class=\"wp-block-paragraph\">\u3053\u308c\u3089\u306e\u92fc\u306f\u30b3\u30b9\u30c8\u52b9\u7387\u306b\u512a\u308c\u3001\u6c34\u4e2d\u3067\u713c\u304d\u5165\u308c\u3059\u308b\u3053\u3068\u3067\u786c\u5316\u3057\u307e\u3059\u3002\u786c\u5ea6\u306f\u4e2d\u7a0b\u5ea6\u3067\u3059\u304c\u3001\u9ad8\u5408\u91d1\u92fc\u306b\u6bd4\u3079\u308b\u3068\u3001\u6469\u8017\u3001\u71b1\u3001\u8150\u98df\u306b\u5bfe\u3059\u308b\u8010\u6027\u306f\u9650\u3089\u308c\u3066\u3044\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\">\u7528\u9014: \u624b\u5de5\u5177\u3001\u4f4e\uff5e\u4e2d\u5fdc\u529b\u306e\u5207\u524a\u5de5\u5177\u3001\u30ce\u30df\u306a\u3069\u306e\u6c4e\u7528\u5de5\u5177\u306b\u3088\u304f\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u51b7\u9593\u5de5\u5177\u92fc\uff08O\u3001A\u3001D\u30b7\u30ea\u30fc\u30ba\uff09<\/h3><p class=\"wp-block-paragraph\">\u3053\u308c\u3089\u306e\u92fc\u306f\u6cb9\u307e\u305f\u306f\u7a7a\u6c17\u4e2d\u3067\u786c\u5316\u3055\u308c\u3001\u512a\u308c\u305f\u8010\u6469\u8017\u6027\u3068\u4f4e\u6e29\u3067\u306e\u9ad8\u3044\u786c\u5ea6\u4fdd\u6301\u6027\u3092\u5099\u3048\u3066\u3044\u307e\u3059\u3002\u30af\u30ed\u30e0\u3001\u30d0\u30ca\u30b8\u30a6\u30e0\u3001\u30e2\u30ea\u30d6\u30c7\u30f3\u306a\u3069\u306e\u5408\u91d1\u5143\u7d20\u304c\u542b\u307e\u308c\u3066\u304a\u308a\u3001\u976d\u6027\u3068\u8010\u6469\u8017\u6027\u304c\u5411\u4e0a\u3057\u3066\u3044\u307e\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>O \u30b7\u30ea\u30fc\u30ba: \u512a\u308c\u305f\u976d\u6027\u3068\u6a5f\u68b0\u52a0\u5de5\u6027\u3092\u5099\u3048\u3001\u4e2d\u7a0b\u5ea6\u306e\u6469\u8017\u7528\u9014\u306b\u9069\u3057\u3066\u3044\u307e\u3059\u3002<\/li>\n\n<li>A \u30b7\u30ea\u30fc\u30ba: \u4f7f\u7528\u6642\u306e\u9ad8\u3044\u5b89\u5b9a\u6027\u3068\u8010\u6469\u8017\u6027\u304c\u5411\u4e0a\u3057\u307e\u3057\u305f\u3002<\/li>\n\n<li>D \u30b7\u30ea\u30fc\u30ba: \u8010\u6469\u8017\u6027\u3068\u786c\u5ea6\u4fdd\u6301\u6027\u306b\u512a\u308c\u3001\u30c0\u30a4\u30ab\u30b9\u30c8\u3084\u30b9\u30bf\u30f3\u30d4\u30f3\u30b0\u91d1\u578b\u306b\u6700\u9069\u3067\u3059\u3002<\/li><\/ul><p class=\"wp-block-paragraph\">\u7528\u9014: \u30d1\u30f3\u30c1\u3001\u30c0\u30a4\u3001\u305b\u3093\u65ad\u30d6\u30ec\u30fc\u30c9\u3001\u30b9\u30bf\u30f3\u30d4\u30f3\u30b0\u30c4\u30fc\u30eb\u306a\u3069\u3001\u4e2d\u7a0b\u5ea6\u306e\u30b9\u30c8\u30ec\u30b9\u3068\u6469\u8017\u3092\u53d7\u3051\u308b\u30c4\u30fc\u30eb\u306b\u6700\u9069\u3067\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u71b1\u9593\u5de5\u5177\u92fc\uff08H\u30b7\u30ea\u30fc\u30ba\uff09<\/h3><p class=\"wp-block-paragraph\">\u9ad8\u6e29\u3067\u3082\u786c\u5ea6\u3092\u7dad\u6301\u3059\u308b\u3088\u3046\u306b\u914d\u5408\u3055\u308c\u305f\u3053\u308c\u3089\u306e\u92fc\u306f\u3001\u71b1\u5909\u5f62\u306b\u5bfe\u3059\u308b\u8010\u6027\u3092\u9ad8\u3081\u308b\u305f\u3081\u306b\u3001\u30af\u30ed\u30e0\u3001\u30e2\u30ea\u30d6\u30c7\u30f3\u3001\u30bf\u30f3\u30b0\u30b9\u30c6\u30f3\u3068\u5408\u91d1\u5316\u3055\u308c\u308b\u3053\u3068\u304c\u3088\u304f\u3042\u308a\u307e\u3059\u3002\u7279\u5b9a\u306e\u30b0\u30ec\u30fc\u30c9\u306b\u5fdc\u3058\u3066\u3001\u7a7a\u6c17\u307e\u305f\u306f\u6cb9\u3067\u786c\u5316\u3067\u304d\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\">\u7528\u9014: \u9ad8\u6e29\u52d5\u4f5c\u304c\u6a19\u6e96\u3067\u3042\u308b\u30c0\u30a4\u30ab\u30b9\u30c8\u3001\u62bc\u3057\u51fa\u3057\u30c0\u30a4\u3001\u71b1\u9593\u935b\u9020\u30d7\u30ed\u30bb\u30b9\u3067\u4e00\u822c\u7684\u306b\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u9ad8\u901f\u5ea6\u5de5\u5177\u92fc\uff08T\u30b7\u30ea\u30fc\u30ba\uff09<\/h3><p class=\"wp-block-paragraph\">\u3053\u308c\u3089\u306e\u92fc\u306b\u306f\u3001\u30bf\u30f3\u30b0\u30b9\u30c6\u30f3\u3001\u30e2\u30ea\u30d6\u30c7\u30f3\u3001\u30d0\u30ca\u30b8\u30a6\u30e0\u304c\u5927\u91cf\u306b\u542b\u307e\u308c\u3066\u304a\u308a\u3001\u975e\u5e38\u306b\u9ad8\u3044\u6e29\u5ea6\u3067\u3082\u786c\u5ea6\u3092\u7dad\u6301\u3067\u304d\u307e\u3059\u3002\u3053\u308c\u3089\u306f\u3001\u9ad8\u901f\u304a\u3088\u3073\u9ad8\u6e29\u3067\u52d5\u4f5c\u3059\u308b\u5207\u524a\u5de5\u5177\u3084\u6a5f\u68b0\u5411\u3051\u306b\u7279\u5225\u306b\u8a2d\u8a08\u3055\u308c\u3066\u3044\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\">\u7528\u9014: \u30c9\u30ea\u30eb\u3001\u30d5\u30e9\u30a4\u30b9\u30ab\u30c3\u30bf\u30fc\u3001\u305d\u306e\u4ed6\u306e\u9ad8\u901f\u5207\u524a\u5de5\u5177\u306b\u6700\u9069\u3067\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u8010\u885d\u6483\u5de5\u5177\u92fc\uff08S\u30b7\u30ea\u30fc\u30ba\uff09<\/h3><p class=\"wp-block-paragraph\">\u7834\u640d\u3057\u305f\u308a\u7815\u3051\u305f\u308a\u3059\u308b\u3053\u3068\u306a\u304f\u3001\u6025\u6fc0\u306a\u885d\u6483\u3084\u63fa\u308c\u3092\u5438\u53ce\u3057\u3066\u8010\u3048\u3089\u308c\u308b\u3088\u3046\u8a2d\u8a08\u3055\u308c\u3066\u3044\u307e\u3059\u3002\u901a\u5e38\u3001\u976d\u6027\u3068\u8010\u885d\u6483\u6027\u3092\u9ad8\u3081\u308b\u305f\u3081\u306b\u30cb\u30c3\u30b1\u30eb\u3068\u30af\u30ed\u30e0\u304c\u542b\u307e\u308c\u3066\u3044\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\">\u7528\u9014: \u30cf\u30f3\u30de\u30fc\u3001\u30ce\u30df\u3001\u6253\u6483\u5de5\u5177\u306a\u3069\u3001\u7a81\u7136\u306e\u885d\u6483\u3084\u5468\u671f\u7684\u306a\u885d\u6483\u306b\u5bfe\u3059\u308b\u8010\u6027\u304c\u5fc5\u8981\u306a\u5de5\u5177\u306b\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">\u5de5\u5177\u92fc\u306e\u4e00\u822c\u7684\u306a\u30b0\u30ec\u30fc\u30c9\u306e\u6bd4\u8f03<\/h2><p class=\"wp-block-paragraph\">\u4ee5\u4e0b\u306e\u8868\u306f\u3001\u5e83\u304f\u4f7f\u7528\u3055\u308c\u3066\u3044\u308b\u3044\u304f\u3064\u304b\u306e\u5de5\u5177\u92fc\u30b0\u30ec\u30fc\u30c9\u306e\u91cd\u8981\u306a\u7279\u6027\u3092\u6982\u8aac\u3057\u3066\u304a\u308a\u3001\u3055\u307e\u3056\u307e\u306a\u6750\u6599\u3092\u6bd4\u8f03\u3059\u308b\u306e\u306b\u5f79\u7acb\u3061\u307e\u3059\u3002<\/p><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u30b0\u30ec\u30fc\u30c9<\/strong><\/td><td><strong>\u878d\u70b9 (\u00b0C)<\/strong><\/td><td><strong>\u786c\u5ea6\uff08HRC\uff09<\/strong><\/td><td><strong>\u964d\u4f0f\u5f37\u5ea6 (MPa)<\/strong><\/td><td><strong>\u885d\u6483\u976d\u6027\uff08J\uff09<\/strong><\/td><\/tr><tr><td>H13<\/td><td>1,350<\/td><td>50-55<\/td><td>1,500-1,800<\/td><td>\u30df\u30c7\u30a3\u30a2\u30e0<\/td><\/tr><tr><td>W1<\/td><td>1,420<\/td><td>55-64<\/td><td>1,200-1,400<\/td><td>\u4f4e\u3044<\/td><\/tr><tr><td>A2<\/td><td>1,200<\/td><td>57-62<\/td><td>1,400-1,600<\/td><td>\u30df\u30c7\u30a3\u30a2\u30e0<\/td><\/tr><tr><td>O1<\/td><td>1,200<\/td><td>58-64<\/td><td>1,200-1,400<\/td><td>\u4f4e\u3044<\/td><\/tr><tr><td>D2<\/td><td>1,250<\/td><td>58-62<\/td><td>1,600-2,000<\/td><td>\u4f4e\u3044<\/td><\/tr><tr><td>M2<\/td><td>1,410<\/td><td>62-65<\/td><td>1,800-2,200<\/td><td>\u30df\u30c7\u30a3\u30a2\u30e0<\/td><\/tr><tr><td>M42<\/td><td>1,470<\/td><td>64-66<\/td><td>2,100-2,400<\/td><td>\u30df\u30c7\u30a3\u30a2\u30e0<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u4e00\u822c\u7684\u306a\u5de5\u5177\u92fc\u30b0\u30ec\u30fc\u30c9\u306e\u4e3b\u306a\u7279\u6027<\/h2><h3 class=\"wp-block-heading\">W1\uff08\u6c34\u786c\u5316\u5de5\u5177\u92fc\uff09<\/h3><p class=\"wp-block-paragraph\">W1\u5de5\u5177\u92fc\u306f\u713c\u304d\u5165\u308c\u304c\u5bb9\u6613\u3067\u3001\u6c4e\u7528\u5de5\u5177\u306b\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002\u70ad\u7d20\u3092\u591a\u304f\u542b\u307f\u3001\u786c\u5ea6\u3092\u9ad8\u3081\u307e\u3059\u304c\u3001\u4ed6\u306e\u30b0\u30ec\u30fc\u30c9\u306b\u6bd4\u3079\u3066\u8106\u304f\u306a\u308a\u3084\u3059\u3044\u50be\u5411\u304c\u3042\u308a\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\"><strong>\u30a2\u30d7\u30ea\u30b1\u30fc\u30b7\u30e7\u30f3<\/strong>: \u30ce\u30df\u3001\u30dd\u30f3\u30c1\u3001\u8efd\u4f5c\u696d\u7528\u9014\u306e\u5207\u524a\u5de5\u5177\u306a\u3069\u3001\u30b7\u30f3\u30d7\u30eb\u3067\u30b9\u30c8\u30ec\u30b9\u306e\u5c11\u306a\u3044\u5de5\u5177\u306b\u6700\u9069\u3067\u3059\u3002<\/p><h3 class=\"wp-block-heading\">O1\uff08\u6cb9\u713c\u5165\u308c\u5de5\u5177\u92fc\uff09<\/h3><p class=\"wp-block-paragraph\">O1 \u306f\u3001\u9069\u5fdc\u6027\u306e\u9ad8\u3044\u5de5\u5177\u92fc\u3067\u3059\u3002\u786c\u5ea6\u3068\u976d\u6027\u306e\u597d\u307e\u3057\u3044\u7d44\u307f\u5408\u308f\u305b\u3068\u3001\u512a\u308c\u305f\u52a0\u5de5\u6027\u3092\u5099\u3048\u3066\u3044\u307e\u3059\u3002\u4e2d\u7a0b\u5ea6\u306e\u8010\u6469\u8017\u6027\u3068\u4e00\u822c\u7684\u306a\u6a5f\u68b0\u7684\u7279\u6027\u304c\u6c42\u3081\u3089\u308c\u308b\u5de5\u5177\u306b\u3088\u304f\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\"><strong>\u30a2\u30d7\u30ea\u30b1\u30fc\u30b7\u30e7\u30f3<\/strong>: \u5207\u524a\u5de5\u5177\u3001\u30c0\u30a4\u3001\u30d1\u30f3\u30c1\u3001\u305b\u3093\u65ad\u5203\u306a\u3069\u306b\u3088\u304f\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">A2\uff08\u7a7a\u6c17\u786c\u5316\u5de5\u5177\u92fc\uff09<\/h3><p class=\"wp-block-paragraph\">A2 \u5de5\u5177\u92fc\u306f\u7a7a\u6c17\u786c\u5316\u304c\u53ef\u80fd\u3067\u3001\u976d\u6027\u3068\u8010\u6469\u8017\u6027\u306e\u30d0\u30e9\u30f3\u30b9\u304c\u512a\u308c\u3066\u3044\u307e\u3059\u3002\u71b1\u51e6\u7406\u4e2d\u306b\u751f\u3058\u308b\u6b6a\u307f\u304c\u6700\u5c0f\u9650\u306b\u6291\u3048\u3089\u308c\u308b\u305f\u3081\u3001\u8907\u96d1\u306a\u5de5\u5177\u306b\u6700\u9069\u3067\u3059\u3002<\/p><p class=\"wp-block-paragraph\"><strong>\u30a2\u30d7\u30ea\u30b1\u30fc\u30b7\u30e7\u30f3<\/strong>: \u30c0\u30a4\u3001\u30d1\u30f3\u30c1\u3001\u30c4\u30fc\u30eb\u306b\u306f\u3001\u976d\u6027\u3068\u8010\u6469\u8017\u6027\u306e\u7d44\u307f\u5408\u308f\u305b\u304c\u5fc5\u8981\u3067\u3059\u3002<\/p><h3 class=\"wp-block-heading\">D2\uff08\u51b7\u9593\u5de5\u5177\u92fc\uff09<\/h3><p class=\"wp-block-paragraph\">D2 \u306f\u3001\u70ad\u7d20\u3068\u30af\u30ed\u30e0\u306e\u542b\u6709\u91cf\u304c\u591a\u3044\u305f\u3081\u3001\u8010\u6469\u8017\u6027\u306b\u512a\u308c\u3066\u3044\u308b\u3053\u3068\u3067\u77e5\u3089\u308c\u3066\u3044\u307e\u3059\u3002\u975e\u5e38\u306b\u786c\u3044\u3067\u3059\u304c\u3001A2 \u306b\u6bd4\u3079\u3066\u8106\u304f\u306a\u3063\u3066\u3044\u307e\u3059\u3002D2 \u306f\u8010\u6469\u8017\u6027\u304c\u9ad8\u304f\u3001\u5207\u524a\u5de5\u5177\u306b\u6700\u9069\u3067\u3059\u3002<\/p><p class=\"wp-block-paragraph\"><strong>\u30a2\u30d7\u30ea\u30b1\u30fc\u30b7\u30e7\u30f3<\/strong>: \u6253\u3061\u629c\u304d\u30d1\u30f3\u30c1\u3001\u30c0\u30a4\u3001\u5207\u524a\u5de5\u5177\u306a\u3069\u306e\u6469\u8017\u306e\u6fc0\u3057\u3044\u5de5\u5177\u306b\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">H13\uff08\u71b1\u9593\u5de5\u5177\u92fc\uff09<\/h3><p class=\"wp-block-paragraph\">H13 \u306f\u3001\u71b1\u75b2\u52b4\u3068\u9ad8\u6e29\u306b\u5bfe\u3059\u308b\u512a\u308c\u305f\u8010\u6027\u3092\u5099\u3048\u3066\u3044\u307e\u3059\u3002\u9ad8\u6e29\u4e0b\u3067\u3082\u786c\u5ea6\u3068\u976d\u6027\u3092\u7dad\u6301\u3059\u308b\u305f\u3081\u3001\u9ad8\u6e29\u4f5c\u696d\u7528\u9014\u306b\u6700\u9069\u3067\u3059\u3002<\/p><p class=\"wp-block-paragraph\"><strong>\u30a2\u30d7\u30ea\u30b1\u30fc\u30b7\u30e7\u30f3<\/strong>: \u935b\u9020\u7528\u91d1\u578b\u3001\u62bc\u3057\u51fa\u3057\u91d1\u578b\u3001\u30d7\u30e9\u30b9\u30c1\u30c3\u30af\u91d1\u578b\u306a\u3069\u306e\u71b1\u9593\u6210\u5f62\u7528\u9014\u3067\u3088\u304f\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">M2\uff08\u9ad8\u901f\u5ea6\u5de5\u5177\u92fc\uff09<\/h3><p class=\"wp-block-paragraph\">M2\u306f\u9ad8\u6e29\u4e0b\u3067\u3082\u786c\u5ea6\u3068\u8010\u6469\u8017\u6027\u3092\u7dad\u6301\u3059\u308b\u5de5\u5177\u92fc\u306e\u4e00\u7a2e\u3067\u3001\u4ed6\u306e\u5de5\u5177\u92fc\u306b\u6bd4\u3079\u3066\u9ad8\u901f\u57df\u3067\u3082\u5207\u308c\u5473\u3092\u7dad\u6301\u3067\u304d\u308b\u3053\u3068\u3067\u77e5\u3089\u308c\u3066\u3044\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\"><strong>\u30a2\u30d7\u30ea\u30b1\u30fc\u30b7\u30e7\u30f3<\/strong>: \u30c9\u30ea\u30eb\u3001\u30bf\u30c3\u30d7\u3001\u30d5\u30e9\u30a4\u30b9\u3001\u30ea\u30fc\u30de\u306a\u3069\u306e\u9ad8\u901f\u5207\u524a\u5de5\u5177\u306b\u5e83\u304f\u4f7f\u7528\u3055\u308c\u3066\u3044\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">M42\uff08\u9ad8\u901f\u5ea6\u5de5\u5177\u92fc\uff09<\/h3><p class=\"wp-block-paragraph\">M42 \u306f\u30b3\u30d0\u30eb\u30c8\u5408\u91d1\u9ad8\u901f\u5ea6\u92fc\u3067\u3001\u7279\u306b\u9ad8\u901f\u5207\u524a\u6642\u306b\u512a\u308c\u305f\u8010\u6469\u8017\u6027\u3068\u976d\u6027\u3092\u767a\u63ee\u3057\u307e\u3059\u3002\u30b3\u30d0\u30eb\u30c8\u542b\u6709\u91cf\u304c\u591a\u3044\u305f\u3081\u3001\u9ad8\u6e29\u74b0\u5883\u3067\u306e\u6027\u80fd\u304c\u5411\u4e0a\u3057\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\"><strong>\u30a2\u30d7\u30ea\u30b1\u30fc\u30b7\u30e7\u30f3<\/strong>: \u306e\u3053\u304e\u308a\u5203\u3001\u30c9\u30ea\u30eb\u3001\u30d5\u30e9\u30a4\u30b9\u30ab\u30c3\u30bf\u30fc\u306a\u3069\u306e\u9ad8\u6027\u80fd\u5207\u524a\u5de5\u5177\u306b\u6700\u9069\u3067\u3059\u3002<\/p><h2 class=\"wp-block-heading\">\u30d7\u30ed\u30b8\u30a7\u30af\u30c8\u306b\u6700\u9069\u306a\u5de5\u5177\u92fc\u30b0\u30ec\u30fc\u30c9\u3092\u9078\u629e\u3059\u308b\u306b\u306f\u3069\u3046\u3059\u308c\u3070\u3088\u3044\u3067\u3057\u3087\u3046\u304b?<\/h2><p class=\"wp-block-paragraph\">SteelPro Group \u306e\u7d4c\u9a13\u8c4a\u5bcc\u306a\u51b6\u91d1\u5b66\u8005\u3068\u3057\u3066\u3001\u79c1\u306f\u6570\u591a\u304f\u306e\u30af\u30e9\u30a4\u30a2\u30f3\u30c8\u304c\u30cb\u30fc\u30ba\u306b\u5408\u3063\u305f\u9069\u5207\u306a\u5de5\u5177\u92fc\u3092\u9078\u629e\u3059\u308b\u8907\u96d1\u306a\u30d7\u30ed\u30bb\u30b9\u3092\u9032\u3081\u308b\u306e\u3092\u652f\u63f4\u3057\u3066\u304d\u307e\u3057\u305f\u3002\u30d7\u30ed\u30b8\u30a7\u30af\u30c8\u306b\u9069\u3057\u305f\u9078\u629e\u3092\u884c\u3046\u305f\u3081\u306b\u5f79\u7acb\u3064\u5c02\u9580\u5bb6\u306e\u30a2\u30c9\u30d0\u30a4\u30b9\u3092\u3044\u304f\u3064\u304b\u3054\u7d39\u4ecb\u3057\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u52d5\u4f5c\u6e29\u5ea6\u3092\u8a55\u4fa1\u3059\u308b<\/h3><p class=\"wp-block-paragraph\">\u30c4\u30fc\u30eb\u304c\u9ad8\u6e29\u74b0\u5883\u3067\u52d5\u4f5c\u3059\u308b\u5834\u5408\u306f\u3001H13 \u306a\u3069\u306e\u71b1\u9593\u52a0\u5de5\u92fc\u306b\u6ce8\u76ee\u3057\u3066\u304f\u3060\u3055\u3044\u3002\u5e38\u6e29\u3067\u306e\u7528\u9014\u306b\u306f\u3001D2 \u3084 O1 \u306a\u3069\u306e\u51b7\u9593\u52a0\u5de5\u92fc\u306e\u65b9\u304c\u9069\u3057\u3066\u3044\u308b\u53ef\u80fd\u6027\u304c\u3042\u308a\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u8010\u6469\u8017\u6027\u306e\u30cb\u30fc\u30ba\u3092\u8a55\u4fa1\u3059\u308b<\/h3><p class=\"wp-block-paragraph\">\u7814\u78e8\u6750\u3084\u7e70\u308a\u8fd4\u3057\u6469\u64e6\u3092\u4f34\u3046\u7528\u9014\u3067\u306f\u3001\u8010\u6469\u8017\u6027\u306e\u9ad8\u3044\u92fc\u3092\u512a\u5148\u3057\u3066\u304f\u3060\u3055\u3044\u3002\u3053\u306e\u5206\u91ce\u3067\u306f D2 \u304a\u3088\u3073 M2 \u30b0\u30ec\u30fc\u30c9\u304c\u512a\u308c\u3066\u3044\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u5f37\u976d\u6027\u8981\u4ef6\u3092\u8003\u616e\u3059\u308b<\/h3><p class=\"wp-block-paragraph\">\u30c4\u30fc\u30eb\u304c\u885d\u6483\u8377\u91cd\u3084\u7a81\u7136\u306e\u30b9\u30c8\u30ec\u30b9\u306b\u3055\u3089\u3055\u308c\u308b\u5834\u5408\u306f\u3001S7 \u306a\u3069\u306e\u8010\u885d\u6483\u30b0\u30ec\u30fc\u30c9\u3092\u691c\u8a0e\u3057\u3066\u304f\u3060\u3055\u3044\u3002\u3053\u308c\u3089\u306e\u92fc\u306f\u3001\u786c\u5ea6\u3092\u72a0\u7272\u306b\u3059\u308b\u3053\u3068\u306a\u304f\u512a\u308c\u305f\u976d\u6027\u3092\u63d0\u4f9b\u3057\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u52a0\u5de5\u6027\u3092\u8003\u616e\u3059\u308b<\/h3><p class=\"wp-block-paragraph\">\u9ad8\u6027\u80fd\u92fc\u306e\u4e2d\u306b\u306f\u3001\u6a5f\u68b0\u52a0\u5de5\u304c\u96e3\u3057\u3044\u3082\u306e\u304c\u3042\u308b\u3053\u3068\u306b\u6ce8\u610f\u3057\u3066\u304f\u3060\u3055\u3044\u3002\u30d7\u30ed\u30b8\u30a7\u30af\u30c8\u3067\u8907\u96d1\u306a\u5f62\u72b6\u3084\u7d30\u304b\u3044\u30c7\u30a3\u30c6\u30fc\u30eb\u304c\u5fc5\u8981\u306a\u5834\u5408\u306f\u3001\u6a5f\u68b0\u52a0\u5de5\u6027\u306b\u512a\u308c\u305f O1 \u3084 A2 \u306a\u3069\u306e\u30b0\u30ec\u30fc\u30c9\u3092\u691c\u8a0e\u3057\u3066\u304f\u3060\u3055\u3044\u3002<\/p><h3 class=\"wp-block-heading\">\u30d1\u30d5\u30a9\u30fc\u30de\u30f3\u30b9\u3068\u30b3\u30b9\u30c8\u306e\u30d0\u30e9\u30f3\u30b9<\/h3><p class=\"wp-block-paragraph\">\u6700\u3082\u9ad8\u6027\u80fd\u306a\u92fc\u6750\u3092\u9078\u629e\u3059\u308b\u306e\u306f\u9b45\u529b\u7684\u3067\u3059\u304c\u3001\u6027\u80fd\u3068\u30b3\u30b9\u30c8\u52b9\u7387\u306e\u30d0\u30e9\u30f3\u30b9\u3092\u53d6\u308b\u3053\u3068\u304c\u91cd\u8981\u3067\u3059\u3002&nbsp;<\/p><p class=\"wp-block-paragraph\">\u5834\u5408\u306b\u3088\u3063\u3066\u306f\u3001\u4e2d\u7a0b\u5ea6\u306e\u92fc\u6750\u3067\u3082\u3001\u3088\u308a\u30ea\u30fc\u30ba\u30ca\u30d6\u30eb\u306a\u4fa1\u683c\u3067\u5341\u5206\u306a\u6027\u80fd\u3092\u767a\u63ee\u3067\u304d\u307e\u3059\u3002\u9ad8\u7d1a\u92fc\u6750\u306f\u521d\u671f\u8cbb\u7528\u304c\u9ad8\u304f\u306a\u308b\u304b\u3082\u3057\u308c\u307e\u305b\u3093\u304c\u3001\u5de5\u5177\u5bff\u547d\u306e\u5ef6\u9577\u3084\u30c0\u30a6\u30f3\u30bf\u30a4\u30e0\u306e\u77ed\u7e2e\u3068\u3044\u3046\u70b9\u3067\u5927\u5e45\u306a\u7bc0\u7d04\u304c\u671f\u5f85\u3067\u304d\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u5c02\u9580\u5bb6\u306b\u76f8\u8ac7\u3059\u308b<\/h3><p class=\"wp-block-paragraph\">\u30d7\u30ed\u30b8\u30a7\u30af\u30c8\u306f\u305d\u308c\u305e\u308c\u7570\u306a\u308a\u307e\u3059\u3002SteelPro Group \u306e\u30c1\u30fc\u30e0\u306e\u3088\u3046\u306a\u5de5\u5177\u92fc\u306e\u5c02\u9580\u5bb6\u306b\u9060\u616e\u306a\u304f\u304a\u554f\u3044\u5408\u308f\u305b\u304f\u3060\u3055\u3044\u3002\u304a\u5ba2\u69d8\u306e\u8981\u4ef6\u306b\u5408\u308f\u305b\u305f\u30a2\u30c9\u30d0\u30a4\u30b9\u3068\u30ab\u30b9\u30bf\u30e0 \u30bd\u30ea\u30e5\u30fc\u30b7\u30e7\u30f3\u3092\u63d0\u4f9b\u3067\u304d\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">\u5f0a\u793e\u306e\u652f\u63f4\u3092\u53d7\u3051\u3066\u9069\u5207\u306a\u5de5\u5177\u92fc\u30b0\u30ec\u30fc\u30c9\u3092\u9078\u629e\u3057\u3066\u304f\u3060\u3055\u3044&nbsp;<\/h2><p class=\"wp-block-paragraph\">SteelPro Group \u3067\u306f\u3001\u304a\u5ba2\u69d8\u306e\u7279\u5b9a\u306e\u30cb\u30fc\u30ba\u306b\u5408\u308f\u305b\u305f\u5e45\u5e83\u3044\u5de5\u5177\u92fc\u88fd\u54c1\u3092\u63d0\u4f9b\u3057\u3066\u3044\u307e\u3059\u3002\u5f53\u793e\u306e\u5c02\u9580\u5bb6\u30c1\u30fc\u30e0\u306f\u3001\u5207\u524a\u5de5\u5177\u3001\u91d1\u578b\u3001\u30ab\u30b9\u30bf\u30e0 \u30b3\u30f3\u30dd\u30fc\u30cd\u30f3\u30c8\u306e\u88fd\u9020\u306a\u3069\u3001\u304a\u5ba2\u69d8\u306e\u30d7\u30ed\u30b8\u30a7\u30af\u30c8\u306b\u6700\u9069\u306a\u6750\u6599\u306e\u9078\u629e\u3092\u304a\u624b\u4f1d\u3044\u3057\u307e\u3059\u3002SteelPro Group \u306f\u3001\u9069\u5207\u306a\u5de5\u5177\u92fc\u30b0\u30ec\u30fc\u30c9\u3067\u512a\u308c\u305f\u6027\u80fd\u3068\u8010\u4e45\u6027\u3092\u5b9f\u73fe\u3067\u304d\u308b\u3088\u3046\u304a\u5ba2\u69d8\u3092\u30b5\u30dd\u30fc\u30c8\u3057\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\"><\/p>","protected":false},"excerpt":{"rendered":"<p>Genuine tool steel is a specially formulated steel alloy. These alloys maintain high hardness, strength, and wear resistance even under [&hellip;]<\/p>","protected":false},"author":12,"featured_media":20212,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"_eb_attr":"","rank_math_lock_modified_date":false,"site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"categories":[4293],"tags":[],"class_list":["post-20218","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-tool-steel"],"acf":[],"_links":{"self":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts\/20218","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/users\/12"}],"replies":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/comments?post=20218"}],"version-history":[{"count":0,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts\/20218\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/media\/20212"}],"wp:attachment":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/media?parent=20218"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/categories?post=20218"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/tags?post=20218"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}