{"id":20863,"date":"2025-02-27T04:28:00","date_gmt":"2025-02-26T20:28:00","guid":{"rendered":"https:\/\/steelprogroup.com\/?p=20863"},"modified":"2025-03-04T17:52:28","modified_gmt":"2025-03-04T09:52:28","slug":"weld","status":"publish","type":"post","link":"https:\/\/steelprogroup.com\/ja\/alloy-steel\/weld\/","title":{"rendered":"\u5408\u91d1\u92fc\u3092\u6eb6\u63a5\u3067\u304d\u307e\u3059\u304b?\u00a0"},"content":{"rendered":"<p class=\"wp-block-paragraph\">\u306f\u3044\u3001\u5408\u91d1\u92fc\u306f\u3046\u307e\u304f\u6eb6\u63a5\u3067\u304d\u307e\u3059\u304c\u3001\u5f37\u304f\u3066\u8010\u4e45\u6027\u306e\u3042\u308b\u6eb6\u63a5\u3092\u5b9f\u73fe\u3059\u308b\u306b\u306f\u7279\u6b8a\u306a\u6280\u8853\u304c\u5fc5\u8981\u3067\u3059\u3002\u71b1\u306b\u5bfe\u3059\u308b\u654f\u611f\u3055\u3084\u5408\u91d1\u306e\u7d44\u6210\u306a\u3069\u306e\u8981\u56e0\u306b\u3088\u308a\u3001\u5408\u91d1\u92fc\u306e\u6eb6\u63a5\u306b\u306f\u7279\u6709\u306e\u8ab2\u984c\u304c\u3042\u308a\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\">SteelPro Group \u306b\u306f\u3001\u3053\u308c\u3089\u306e\u8ab2\u984c\u306b\u5bfe\u51e6\u3057\u3001\u9ad8\u54c1\u8cea\u3067\u898f\u683c\u306b\u6e96\u62e0\u3057\u305f\u6eb6\u63a5\u3092\u63d0\u4f9b\u3059\u308b\u5c02\u9580\u77e5\u8b58\u304c\u3042\u308a\u307e\u3059\u3002\u3053\u306e\u30ac\u30a4\u30c9\u3067\u306f\u3001\u5408\u91d1\u92fc\u3092\u6271\u3046\u969b\u306b\u6700\u826f\u306e\u7d50\u679c\u3092\u5f97\u308b\u305f\u3081\u306b\u5f79\u7acb\u3064\u3001\u6700\u9069\u306a\u6eb6\u63a5\u65b9\u6cd5\u3001\u4e00\u822c\u7684\u306a\u969c\u5bb3\u3001\u5c02\u9580\u7684\u306a\u30bd\u30ea\u30e5\u30fc\u30b7\u30e7\u30f3\u306b\u3064\u3044\u3066\u8aac\u660e\u3057\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">\u5408\u91d1\u92fc\u3068\u306f\u4f55\u304b\uff1f\u7c21\u5358\u306a\u6982\u8981<\/h2><p class=\"wp-block-paragraph\">\u5408\u91d1\u92fc\u306f\u3001\u7279\u6027\u3092\u5411\u4e0a\u3055\u305b\u308b\u305f\u3081\u306b\u9244\u3001\u70ad\u7d20\u3001\u304a\u3088\u3073\u5408\u91d1\u5143\u7d20\u3068\u547c\u3070\u308c\u308b\u8ffd\u52a0\u5143\u7d20\u306e\u6df7\u5408\u7269\u3092\u53d6\u308a\u5165\u308c\u305f\u92fc\u306e\u4e00\u7a2e\u3067\u3059\u3002\u30af\u30ed\u30e0\u3001\u30cb\u30c3\u30b1\u30eb\u3001\u30de\u30f3\u30ac\u30f3\u3001\u30d0\u30ca\u30b8\u30a6\u30e0\u306a\u3069\u306e\u5143\u7d20\u306f\u3001\u5f37\u5ea6\u3001\u976d\u6027\u3001\u8010\u8150\u98df\u6027\u3001\u9ad8\u6e29\u3067\u306e\u8010\u4e45\u6027\u306a\u3069\u306e\u7279\u5b9a\u306e\u7279\u6027\u3092\u5f97\u308b\u305f\u3081\u306b\u6b63\u78ba\u306a\u91cf\u3067\u542b\u307e\u308c\u3066\u3044\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">\u5408\u91d1\u92fc\u306e\u6eb6\u63a5\u306b\u304a\u3051\u308b\u8ab2\u984c<\/h2><h3 class=\"wp-block-heading\">\u71b1\u611f\u5ea6<\/h3><p class=\"wp-block-paragraph\">\u5408\u91d1\u92fc\u306f\u3001\u305d\u306e\u8907\u96d1\u306a\u7d44\u6210\u306e\u305f\u3081\u3001\u71b1\u306b\u654f\u611f\u3067\u3059\u3002\u6eb6\u63a5\u4e2d\u306b\u9ad8\u6e29\u306b\u3055\u3089\u3055\u308c\u308b\u3068\u3001\u92fc\u306f\u6025\u901f\u306b\u81a8\u5f35\u304a\u3088\u3073\u53ce\u7e2e\u3057\u3001\u3072\u3073\u5272\u308c\u3084\u6b6a\u307f\u304c\u751f\u3058\u308b\u53ef\u80fd\u6027\u304c\u3042\u308a\u307e\u3059\u3002\u3053\u308c\u306f\u3001\u5408\u91d1\u5143\u7d20 (\u30af\u30ed\u30e0\u3084\u30cb\u30c3\u30b1\u30eb\u306a\u3069) \u304c\u9ad8\u6e29\u3067\u306e\u92fc\u306e\u6319\u52d5\u306b\u5f71\u97ff\u3092\u4e0e\u3048\u308b\u9ad8\u5408\u91d1\u92fc\u306e\u5834\u5408\u306b\u7279\u306b\u5f53\u3066\u306f\u307e\u308a\u307e\u3059\u3002\u305d\u306e\u305f\u3081\u3001\u640d\u50b7\u3092\u9632\u3050\u305f\u3081\u306b\u3001\u6eb6\u63a5\u4e2d\u306e\u5165\u71b1\u3068\u51b7\u5374\u901f\u5ea6\u3092\u614e\u91cd\u306b\u5236\u5fa1\u3059\u308b\u3053\u3068\u304c\u4e0d\u53ef\u6b20\u3067\u3059\u3002<\/p><p class=\"wp-block-paragraph\">\u71b1\u5272\u308c\u3084\u53cd\u308a\u3092\u9632\u3050\u305f\u3081\u306b\u306f\u3001\u5165\u71b1\u3068\u51b7\u5374\u901f\u5ea6\u3092\u7ba1\u7406\u3059\u308b\u3053\u3068\u304c\u4e0d\u53ef\u6b20\u3067\u3059\u3002\u6eb6\u63a5\u524d\u306b\u92fc\u3092\u4e88\u71b1\u3059\u308b\u3068\u71b1\u5fdc\u529b\u3092\u6700\u5c0f\u9650\u306b\u6291\u3048\u308b\u3053\u3068\u304c\u3067\u304d\u3001\u6eb6\u63a5\u5f8c\u306e\u71b1\u51e6\u7406 (PWHT) \u306b\u3088\u308a\u6b8b\u7559\u5fdc\u529b\u3092\u8efd\u6e1b\u3057\u3001\u6750\u6599\u3092\u3055\u3089\u306b\u4fdd\u8b77\u3059\u308b\u3053\u3068\u304c\u3067\u304d\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u6c34\u7d20\u8106\u5316<\/h3><p class=\"wp-block-paragraph\">\u6c34\u7d20\u8106\u5316\u306f\u3001\u6eb6\u63a5\u4e2d\u306b\u6c34\u7d20\u30ac\u30b9\u304c\u92fc\u306b\u5438\u53ce\u3055\u308c\u308b\u3068\u767a\u751f\u3057\u307e\u3059\u3002\u3053\u308c\u306b\u3088\u308a\u6750\u6599\u304c\u5f31\u304f\u306a\u308a\u3001\u5272\u308c\u3084\u3059\u304f\u306a\u308a\u307e\u3059\u3002\u3053\u308c\u306f\u3001\u3088\u308a\u591a\u304f\u306e\u6c34\u7d20\u3092\u5438\u53ce\u3059\u308b\u50be\u5411\u304c\u3042\u308b\u9ad8\u5f37\u5ea6\u5408\u91d1\u306e\u5834\u5408\u306b\u7279\u306b\u554f\u984c\u3068\u306a\u308a\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\">\u3053\u306e\u30ea\u30b9\u30af\u3092\u6700\u5c0f\u9650\u306b\u6291\u3048\u308b\u306b\u306f\u3001\u6eb6\u63a5\u30d7\u30ed\u30bb\u30b9\u4e2d\u306e\u6c34\u5206\u3092\u53ef\u80fd\u306a\u9650\u308a\u4f4e\u304f\u4fdd\u3064\u5fc5\u8981\u304c\u3042\u308a\u307e\u3059\u3002\u4f4e\u6c34\u7d20\u96fb\u6975\u3092\u4f7f\u7528\u3057\u3001\u9069\u5207\u306a\u6eb6\u63a5\u5f8c\u71b1\u51e6\u7406 (PWHT) \u3092\u78ba\u5b9f\u306b\u884c\u3046\u3053\u3068\u3067\u3001\u8106\u5316\u306e\u53ef\u80fd\u6027\u3092\u52b9\u679c\u7684\u306b\u4f4e\u6e1b\u3057\u3001\u6eb6\u63a5\u306e\u5f37\u5ea6\u3092\u78ba\u4fdd\u3067\u304d\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u9178\u5316<\/h3><p class=\"wp-block-paragraph\">\u6eb6\u63a5\u306b\u3088\u308a\u9ad8\u6e29\u304c\u767a\u751f\u3057\u3001\u92fc\u306e\u8868\u9762\u304c\u9178\u7d20\u3068\u53cd\u5fdc\u3057\u3066\u9178\u5316\u7269\u304c\u5f62\u6210\u3055\u308c\u308b\u53ef\u80fd\u6027\u304c\u3042\u308a\u307e\u3059\u3002\u3053\u308c\u3089\u306e\u9178\u5316\u7269\u306f\u6eb6\u63a5\u3092\u5f31\u3081\u3001\u6bcd\u6750\u3068\u30d5\u30a3\u30e9\u30fc\u91d1\u5c5e\u9593\u306e\u7d50\u5408\u3092\u5f31\u3081\u308b\u53ef\u80fd\u6027\u304c\u3042\u308a\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\">\u6eb6\u63a5\u90e8\u3092\u9178\u5316\u304b\u3089\u4fdd\u8b77\u3059\u308b\u306b\u306f\u3001\u6eb6\u63a5\u524d\u306b\u6750\u6599\u3092\u6d17\u6d44\u3057\u3001\u30b7\u30fc\u30eb\u30c9\u30ac\u30b9\uff08\u30a2\u30eb\u30b4\u30f3\u3084\u4e8c\u9178\u5316\u70ad\u7d20\u306a\u3069\uff09\u3092\u4f7f\u7528\u3057\u3066\u6eb6\u878d\u6eb6\u63a5\u30d7\u30fc\u30eb\u3092\u9178\u7d20\u304b\u3089\u4fdd\u8b77\u3059\u308b\u3053\u3068\u304c\u4e0d\u53ef\u6b20\u3067\u3059\u3002\u3053\u308c\u306b\u3088\u308a\u3001\u6eb6\u63a5\u306e\u5b8c\u5168\u6027\u304c\u7dad\u6301\u3055\u308c\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u5408\u91d1\u7d44\u6210\u306b\u3088\u308b\u6eb6\u63a5\u6027\u306e\u9055\u3044<\/h3><p class=\"wp-block-paragraph\">\u92fc\u9244\u306b\u542b\u307e\u308c\u308b\u3055\u307e\u3056\u307e\u306a\u5408\u91d1\u5143\u7d20\u306f\u3001\u305d\u306e\u6eb6\u63a5\u6027\u306b\u5f71\u97ff\u3057\u307e\u3059\u3002\u305f\u3068\u3048\u3070\u3001\u30af\u30ed\u30e0\u3068\u30cb\u30c3\u30b1\u30eb\u306e\u542b\u6709\u91cf\u304c\u591a\u3044\u3068\u30aa\u30fc\u30b9\u30c6\u30ca\u30a4\u30c8\u306e\u5f62\u6210\u304c\u4fc3\u9032\u3055\u308c\u3001\u3088\u308a\u7cbe\u5bc6\u306a\u6eb6\u63a5\u6280\u8853\u304c\u5fc5\u8981\u306b\u306a\u308a\u307e\u3059\u3002\u5408\u91d1\u7d44\u6210\u306b\u3088\u3063\u3066\u306f\u3001\u6eb6\u63a5\u4e2d\u306b\u6750\u6599\u304c\u5272\u308c\u3084\u3059\u304f\u306a\u308b\u3053\u3068\u3082\u3042\u308a\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\">\u5408\u91d1\u306e\u7d44\u6210\u3092\u7406\u89e3\u3059\u308b\u3053\u3068\u3067\u3001\u6eb6\u63a5\u5de5\u306f\u9069\u5207\u306a\u6eb6\u63a5\u65b9\u6cd5\u3001\u30d5\u30a3\u30e9\u30fc\u6750\u6599\u3001\u71b1\u5236\u5fa1\u624b\u9806\u3092\u9078\u629e\u3067\u304d\u308b\u3088\u3046\u306b\u306a\u308a\u307e\u3059\u3002\u3053\u308c\u306b\u3088\u308a\u3001\u6bcd\u6750\u3068\u30d5\u30a3\u30e9\u30fc\u91d1\u5c5e\u306e\u9069\u5408\u6027\u304c\u78ba\u4fdd\u3055\u308c\u3001\u3072\u3073\u5272\u308c\u3084\u6eb6\u63a5\u306e\u5f31\u5316\u306e\u30ea\u30b9\u30af\u304c\u6700\u5c0f\u9650\u306b\u6291\u3048\u3089\u308c\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">\u5408\u91d1\u92fc\u3092\u6eb6\u63a5\u3059\u308b\u6700\u826f\u306e\u65b9\u6cd5<\/h2><ol class=\"wp-block-list\"><li>TIG\u6eb6\u63a5\uff08\u30ac\u30b9\u30bf\u30f3\u30b0\u30b9\u30c6\u30f3\u30a2\u30fc\u30af\u6eb6\u63a5\uff09<\/li><\/ol><p class=\"wp-block-paragraph\">TIG \u6eb6\u63a5\u306f\u7cbe\u5bc6\u3067\u3001\u8584\u3044\u90e8\u5206\u3084\u91cd\u8981\u306a\u63a5\u5408\u90e8\u306b\u6700\u9069\u3067\u3059\u3002\u975e\u6d88\u8017\u6027\u306e\u30bf\u30f3\u30b0\u30b9\u30c6\u30f3\u96fb\u6975\u3068\u4e0d\u6d3b\u6027\u30ac\u30b9 (\u901a\u5e38\u306f\u30a2\u30eb\u30b4\u30f3) \u3092\u4f7f\u7528\u3057\u3066\u6eb6\u63a5\u3092\u4fdd\u8b77\u3057\u307e\u3059\u3002\u3053\u306e\u6280\u8853\u3067\u306f\u71b1\u3092\u6b63\u78ba\u306b\u5236\u5fa1\u3067\u304d\u308b\u305f\u3081\u3001\u304d\u308c\u3044\u3067\u9ad8\u54c1\u8cea\u306e\u6eb6\u63a5\u304c\u5b9f\u73fe\u3057\u307e\u3059\u3002TIG \u6eb6\u63a5\u306f\u3001\u822a\u7a7a\u5b87\u5b99\u3084\u81ea\u52d5\u8eca\u306a\u3069\u306e\u5206\u91ce\u3067\u4f7f\u7528\u3055\u308c\u308b\u5408\u91d1\u306b\u7279\u306b\u6709\u52b9\u3067\u3059\u3002<\/p><ol start=\"2\" class=\"wp-block-list\"><li>MIG\u6eb6\u63a5\uff08\u30ac\u30b9\u30e1\u30bf\u30eb\u30a2\u30fc\u30af\u6eb6\u63a5\uff09<\/li><\/ol><p class=\"wp-block-paragraph\">MIG \u6eb6\u63a5\u306f\u9ad8\u901f\u304b\u3064\u52b9\u7387\u7684\u3067\u3001\u539a\u3044\u5408\u91d1\u92fc\u30bb\u30af\u30b7\u30e7\u30f3\u306b\u6700\u9069\u3067\u3059\u3002\u6eb6\u63a5\u30ac\u30f3\u306b\u901a\u3055\u308c\u308b\u3068\u6eb6\u3051\u308b\u30ef\u30a4\u30e4\u96fb\u6975\u3092\u4f7f\u7528\u3057\u307e\u3059\u3002MIG \u306f\u5806\u7a4d\u7387\u304c\u9ad8\u3044\u305f\u3081\u3001\u88fd\u9020\u304a\u3088\u3073\u5efa\u8a2d\u30d7\u30ed\u30b8\u30a7\u30af\u30c8\u306b\u9069\u3057\u3066\u3044\u307e\u3059\u3002TIG \u307b\u3069\u6b63\u78ba\u3067\u306f\u3042\u308a\u307e\u305b\u3093\u304c\u3001MIG \u6eb6\u63a5\u306f\u6c4e\u7528\u6027\u304c\u9ad8\u304f\u3001\u3055\u307e\u3056\u307e\u306a\u6750\u6599\u306e\u539a\u3055\u3067\u52b9\u679c\u7684\u306b\u6a5f\u80fd\u3057\u307e\u3059\u3002<\/p><ol start=\"3\" class=\"wp-block-list\"><li>\u30b9\u30c6\u30a3\u30c3\u30af\u6eb6\u63a5\uff08SMAW \u2013 \u30b7\u30fc\u30eb\u30c9\u30e1\u30bf\u30eb\u30a2\u30fc\u30af\u6eb6\u63a5\uff09<\/li><\/ol><p class=\"wp-block-paragraph\">\u30b9\u30c6\u30a3\u30c3\u30af\u6eb6\u63a5\u306f\u67d4\u8edf\u6027\u304c\u3042\u308a\u3001\u6301\u3061\u904b\u3073\u304c\u7c21\u5358\u306a\u305f\u3081\u3001\u5c4b\u5916\u3067\u306e\u4f5c\u696d\u306b\u6700\u9069\u3067\u3059\u3002\u6eb6\u63a5\u30d7\u30ed\u30bb\u30b9\u4e2d\u306b\u6d88\u8cbb\u3055\u308c\u308b\u96fb\u6975\u306b\u306f\u30d5\u30e9\u30c3\u30af\u30b9\u304c\u5857\u5e03\u3055\u308c\u3066\u304a\u308a\u3001\u6eb6\u3051\u308b\u969b\u306b\u30b7\u30fc\u30eb\u30c9\u30ac\u30b9\u304c\u767a\u751f\u3057\u307e\u3059\u3002&nbsp;<\/p><p class=\"wp-block-paragraph\">\u30b9\u30c6\u30a3\u30c3\u30af\u6eb6\u63a5\u306f\u3001\u74b0\u5883\u304c\u53b3\u3057\u3044\u5efa\u8a2d\u3084\u9020\u8239\u306a\u3069\u306e\u8981\u6c42\u306e\u53b3\u3057\u3044\u4f5c\u696d\u3067\u983b\u7e41\u306b\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002TIG \u3084 MIG \u307b\u3069\u306e\u7cbe\u5ea6\u306f\u5f97\u3089\u308c\u306a\u3044\u304b\u3082\u3057\u308c\u307e\u305b\u3093\u304c\u3001\u539a\u3044\u6750\u6599\u306b\u9069\u3057\u3066\u3044\u307e\u3059\u3002<\/p><ol start=\"4\" class=\"wp-block-list\"><li>\u4e88\u71b1\u304a\u3088\u3073\u6eb6\u63a5\u5f8c\u71b1\u51e6\u7406\uff08PWHT\uff09<\/li><\/ol><p class=\"wp-block-paragraph\">\u5408\u91d1\u92fc\u306f\u3001\u4e88\u71b1\u3068\u6eb6\u63a5\u5f8c\u306e\u71b1\u51e6\u7406\u306b\u3088\u3063\u3066\u52b9\u679c\u304c\u5f97\u3089\u308c\u307e\u3059\u3002\u4e88\u71b1\u306b\u3088\u308a\u3001\u71b1\u885d\u6483\u3092\u6700\u5c0f\u9650\u306b\u6291\u3048\u3001\u6eb6\u63a5\u4e2d\u306e\u7834\u640d\u3092\u56de\u907f\u3067\u304d\u307e\u3059\u3002\u6eb6\u63a5\u5f8c\u306e\u71b1\u51e6\u7406 (PWHT) \u306f\u3001\u5fdc\u529b\u3092\u7de9\u548c\u3057\u3001\u6750\u6599\u306e\u7279\u6027\u3092\u9ad8\u3081\u308b\u305f\u3081\u306b\u6eb6\u63a5\u5f8c\u306b\u9069\u7528\u3055\u308c\u307e\u3059\u3002\u3053\u306e\u30d7\u30ed\u30bb\u30b9\u306f\u3001\u6c34\u7d20\u8106\u5316\u3092\u8efd\u6e1b\u3057\u3001\u6eb6\u63a5\u3092\u5f37\u5316\u3059\u308b\u306e\u306b\u3082\u5f79\u7acb\u3061\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">\u5408\u91d1\u92fc\u306e\u6eb6\u63a5\u65b9\u6cd5\u306f\uff1f<\/h2><ol class=\"wp-block-list\"><li>\u6750\u6599\u306e\u6e96\u5099<\/li><\/ol><p class=\"wp-block-paragraph\">\u307e\u305a\u3001\u92fc\u6750\u3092\u6d17\u6d44\u3057\u3066\u6c5a\u308c\u3001\u9306\u3001\u6c5a\u67d3\u7269\u8cea\u3092\u53d6\u308a\u9664\u304d\u307e\u3059\u3002\u3053\u308c\u306b\u3088\u308a\u3001\u6eb6\u63a5\u306b\u9069\u3057\u305f\u6ed1\u3089\u304b\u306a\u8868\u9762\u304c\u78ba\u4fdd\u3055\u308c\u3001\u5145\u586b\u6750\u306e\u9069\u5207\u306a\u63a5\u7740\u304c\u4fc3\u9032\u3055\u308c\u307e\u3059\u3002\u5fc5\u8981\u306b\u5fdc\u3058\u3066\u3001\u92fc\u6750\u306e\u7aef\u306b\u89d2\u5ea6\u3092\u4ed8\u3051\u3066\u3001\u63a5\u5408\u90e8\u306e\u8010\u4e45\u6027\u3068\u6d78\u900f\u6027\u3092\u9ad8\u3081\u307e\u3059\u3002\u9069\u5207\u306a\u6e96\u5099\u306b\u3088\u308a\u3001\u591a\u5b54\u6027\u3084\u6eb6\u63a5\u90e8\u306e\u5f31\u3055\u306a\u3069\u306e\u6b20\u9665\u3092\u9632\u3050\u3053\u3068\u304c\u3067\u304d\u307e\u3059\u3002<\/p><ol start=\"2\" class=\"wp-block-list\"><li>\u30d5\u30a3\u30e9\u30fc\u91d1\u5c5e\u306e\u9078\u629e<\/li><\/ol><p class=\"wp-block-paragraph\">\u92fc\u306e\u5408\u91d1\u7d44\u6210\u306b\u5408\u308f\u305b\u3066\u9069\u5207\u306a\u30d5\u30a3\u30e9\u30fc\u91d1\u5c5e\u3092\u9078\u629e\u3057\u307e\u3059\u3002\u6eb6\u63a5\u306e\u5f37\u5ea6\u3068\u7279\u6027\u3092\u7dad\u6301\u3059\u308b\u305f\u3081\u306b\u3001\u30d5\u30a3\u30e9\u30fc\u306b\u306f\u540c\u69d8\u306e\u5143\u7d20 (\u30af\u30ed\u30e0\u3084\u30cb\u30c3\u30b1\u30eb\u306a\u3069) \u304c\u542b\u307e\u308c\u3066\u3044\u308b\u5fc5\u8981\u304c\u3042\u308a\u307e\u3059\u3002&nbsp;<\/p><p class=\"wp-block-paragraph\">\u3055\u3089\u306b\u3001 <strong>\u4f4e\u6c34\u7d20\u30d5\u30a3\u30e9\u30fc\u91d1\u5c5e<\/strong> \u9ad8\u5f37\u5ea6\u5408\u91d1\u7528\u3002\u3053\u308c\u3089\u306e\u6dfb\u52a0\u5264\u306f\u3001\u6eb6\u63a5\u90e8\u306e\u5f37\u5ea6\u3092\u4f4e\u4e0b\u3055\u305b\u3001\u5272\u308c\u3092\u5f15\u304d\u8d77\u3053\u3059\u53ef\u80fd\u6027\u306e\u3042\u308b\u6c34\u7d20\u8106\u5316\u306e\u53ef\u80fd\u6027\u3092\u6700\u5c0f\u9650\u306b\u6291\u3048\u308b\u305f\u3081\u306b\u7279\u5225\u306b\u958b\u767a\u3055\u308c\u307e\u3057\u305f\u3002&nbsp;<\/p><p class=\"wp-block-paragraph\">\u5408\u91d1\u92fc\u306b\u6700\u9069\u306a\u30d5\u30a3\u30e9\u30fc\u91d1\u5c5e\u3092\u9078\u629e\u3059\u308b\u306b\u306f\u3001\u5fc5\u305a\u6750\u6599\u4ed5\u69d8\u3068\u6eb6\u63a5\u624b\u9806\u3092\u53c2\u7167\u3057\u3066\u304f\u3060\u3055\u3044\u3002<\/p><ol start=\"3\" class=\"wp-block-list\"><li>\u71b1\u5165\u529b\u3068\u30d1\u30b9\u9593\u6e29\u5ea6\u306e\u5236\u5fa1<\/li><\/ol><p class=\"wp-block-paragraph\">\u71b1\u3092\u5236\u5fa1\u3059\u308b\u3053\u3068\u306f\u3001\u92fc\u306e\u5fae\u7d30\u69cb\u9020\u306e\u6b6a\u307f\u3001\u3072\u3073\u5272\u308c\u3001\u640d\u50b7\u3092\u9632\u3050\u305f\u3081\u306b\u4e0d\u53ef\u6b20\u3067\u3059\u3002\u71b1\u304c\u591a\u3059\u304e\u308b\u3068\u6eb6\u63a5\u304c\u5f31\u304f\u306a\u308b\u53ef\u80fd\u6027\u304c\u3042\u308a\u307e\u3059\u3002\u71b1\u5165\u529b\u3092\u53b3\u5bc6\u306b\u76e3\u8996\u3057\u3001\u6eb6\u63a5\u30d1\u30b9\u9593\u306e\u6e29\u5ea6\u3092\u5236\u5fa1\u3057\u307e\u3059\u3002\u71b1\u3092\u63a8\u5968\u7bc4\u56f2\u5185\u306b\u4fdd\u3064\u3068\u3001\u6eb6\u63a5\u54c1\u8cea\u304c\u7dad\u6301\u3055\u308c\u3001\u30b9\u30c8\u30ec\u30b9\u3092\u9632\u3050\u3053\u3068\u304c\u3067\u304d\u307e\u3059\u3002<\/p><ol start=\"4\" class=\"wp-block-list\"><li>\u6eb6\u63a5\u5f8c\u691c\u67fb<\/li><\/ol><p class=\"wp-block-paragraph\">\u6eb6\u63a5\u5f8c\u3001\u6eb6\u63a5\u90e8\u306e\u54c1\u8cea\u3068\u5b8c\u5168\u6027\u3092\u691c\u67fb\u3057\u307e\u3059\u3002X \u7dda\u3084\u8d85\u97f3\u6ce2\u691c\u67fb\u306a\u3069\u306e\u975e\u7834\u58ca\u691c\u67fb (NDT) \u65b9\u6cd5\u3092\u4f7f\u7528\u3059\u308b\u3068\u3001\u4e80\u88c2\u3084\u7a7a\u9699\u306a\u3069\u306e\u5185\u90e8\u6b20\u9665\u3092\u691c\u51fa\u3067\u304d\u307e\u3059\u3002\u76ee\u8996\u691c\u67fb\u3067\u306f\u3001\u591a\u5b54\u6027\u3084\u4e0d\u5b8c\u5168\u306a\u878d\u5408\u306a\u3069\u306e\u5916\u90e8\u306e\u554f\u984c\u3092\u30c1\u30a7\u30c3\u30af\u3057\u307e\u3059\u3002&nbsp;<\/p><ol start=\"5\" class=\"wp-block-list\"><li>\u6eb6\u63a5\u5f8c\u71b1\u51e6\u7406\uff08PWHT\uff09<\/li><\/ol><p class=\"wp-block-paragraph\">\u5834\u5408\u306b\u3088\u3063\u3066\u306f\u3001\u6eb6\u63a5\u5f8c\u306b\u5408\u91d1\u92fc\u306b\u6eb6\u63a5\u5f8c\u71b1\u51e6\u7406 (PWHT) \u304c\u5fc5\u8981\u306b\u306a\u308b\u3053\u3068\u304c\u3042\u308a\u307e\u3059\u3002PWHT \u304c\u5fc5\u8981\u304b\u3069\u3046\u304b\u3092\u5224\u65ad\u3059\u308b\u306b\u306f\u3001\u6750\u6599\u306e\u4ed5\u69d8\u3092\u78ba\u8a8d\u3057\u3001\u63a8\u5968\u624b\u9806\u306b\u5f93\u3046\u3053\u3068\u304c\u91cd\u8981\u3067\u3059\u3002<\/p><h3 class=\"wp-block-heading\"><strong>\u6eb6\u63a5\u5408\u91d1\u92fc\u306e\u4e00\u822c\u7684\u306a\u7528\u9014<\/strong><\/h3><ul class=\"wp-block-list\"><li><strong>\u77f3\u6cb9\u30fb\u30ac\u30b9\u30d1\u30a4\u30d7\u30e9\u30a4\u30f3:<\/strong> \u9ad8\u5727\u30d1\u30a4\u30d7\u30e9\u30a4\u30f3\u7528\u306e\u5f37\u529b\u3067\u6f0f\u308c\u306e\u306a\u3044\u30b8\u30e7\u30a4\u30f3\u30c8\u3002<\/li>\n\n<li><strong>\u91cd\u6a5f\u90e8\u54c1:<\/strong> \u5efa\u8a2d\u6a5f\u68b0\u3084\u9271\u5c71\u6a5f\u68b0\u306e\u30ae\u30a2\u3084\u30b7\u30e3\u30d5\u30c8\u306a\u3069\u306e\u8010\u4e45\u6027\u306e\u3042\u308b\u90e8\u54c1\u3002<\/li>\n\n<li><strong>\u822a\u7a7a\u5b87\u5b99\u304a\u3088\u3073\u9632\u885b:<\/strong> \u822a\u7a7a\u6a5f\u3084\u8ecd\u7528\u8eca\u4e21\u306e\u7740\u9678\u88c5\u7f6e\u3084\u30a8\u30f3\u30b8\u30f3\u90e8\u54c1\u306a\u3069\u306e\u7cbe\u5bc6\u90e8\u54c1\u3002<\/li><\/ul><p class=\"wp-block-paragraph\">SteelPro Group \u306f\u3001\u3053\u308c\u3089\u306e\u696d\u754c\u5411\u3051\u306b\u5408\u91d1\u92fc\u306e\u6eb6\u63a5\u30bd\u30ea\u30e5\u30fc\u30b7\u30e7\u30f3\u3092\u63d0\u4f9b\u3057\u3001\u9ad8\u54c1\u8cea\u3067\u4fe1\u983c\u6027\u306e\u9ad8\u3044\u30d1\u30d5\u30a9\u30fc\u30de\u30f3\u30b9\u3092\u4fdd\u8a3c\u3057\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">\u30aa\u30d7\u30b7\u30e7\u30f3\u306e\u6eb6\u63a5\u30b5\u30fc\u30d3\u30b9\u3092\u5099\u3048\u305f\u9ad8\u54c1\u8cea\u306e\u5408\u91d1\u92fc\u306e\u4f9b\u7d66<\/h2><p class=\"wp-block-paragraph\">\u30d7\u30ed\u30d5\u30a7\u30c3\u30b7\u30e7\u30ca\u30eb\u30b0\u30ec\u30fc\u30c9\u306e\u5408\u91d1\u92fc\u6eb6\u63a5\u30b5\u30fc\u30d3\u30b9\u306a\u3089\u3001SteelPro Group\u306b\u304a\u4efb\u305b\u304f\u3060\u3055\u3044\u3002\u5f53\u793e\u306f\u3001\u6b21\u306e\u3088\u3046\u306a\u9ad8\u54c1\u8cea\u306e\u5408\u91d1\u92fc\u3092\u63d0\u4f9b\u3059\u308b\u3053\u3068\u306b\u7279\u5316\u3057\u3066\u3044\u307e\u3059\u3002 <a href=\"https:\/\/steelprogroup.com\/ja\/steel-bar\/4140\/\">4140<\/a>, <a href=\"https:\/\/steelprogroup.com\/ja\/alloy-steel\/aisi-4130\/\">4130<\/a> \u69d8\u3005\u306a\u5f62\u614b\u306b\u5bfe\u5fdc\u3057\u307e\u3059\u3002\u5f53\u793e\u306e\u8a8d\u5b9a\u6eb6\u63a5\u5de5\u3068\u5148\u9032\u7684\u306a\u8a2d\u5099\u306f\u3001\u304a\u5ba2\u69d8\u306e\u30d7\u30ed\u30b8\u30a7\u30af\u30c8\u306b\u6700\u9ad8\u54c1\u8cea\u306e\u7d50\u679c\u3092\u4fdd\u8a3c\u3057\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\">\u5408\u91d1\u92fc\u306e\u30cb\u30fc\u30ba\u3084\u5f53\u793e\u306e\u6eb6\u63a5\u30b5\u30fc\u30d3\u30b9\u306b\u3064\u3044\u3066\u8a73\u3057\u304f\u77e5\u308a\u305f\u3044\u5834\u5408\u306f\u3001\u4eca\u3059\u3050 SteelPro Group \u306b\u304a\u554f\u3044\u5408\u308f\u305b\u304f\u3060\u3055\u3044\u3002<\/p>","protected":false},"excerpt":{"rendered":"<p>Yes, alloy steel can be welded successfully, but specialized techniques are required to ensure strong, durable welds. Due to factors [&hellip;]<\/p>","protected":false},"author":12,"featured_media":20855,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"_eb_attr":"","rank_math_lock_modified_date":false,"site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"categories":[4308],"tags":[],"class_list":["post-20863","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-alloy-steel"],"acf":[],"_links":{"self":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts\/20863","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/users\/12"}],"replies":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/comments?post=20863"}],"version-history":[{"count":0,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts\/20863\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/media\/20855"}],"wp:attachment":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/media?parent=20863"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/categories?post=20863"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/tags?post=20863"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}