{"id":20965,"date":"2025-02-27T15:22:41","date_gmt":"2025-02-27T07:22:41","guid":{"rendered":"https:\/\/steelprogroup.com\/?p=20965"},"modified":"2025-02-27T15:23:28","modified_gmt":"2025-02-27T07:23:28","slug":"all-about","status":"publish","type":"post","link":"https:\/\/steelprogroup.com\/ja\/galvanized-steel\/knowledge\/all-about\/","title":{"rendered":"\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc: \u4e9c\u925b\u30e1\u30c3\u30ad\u306e\u7a2e\u985e\u3001\u8868\u9762\u51e6\u7406\u3001\u7528\u9014"},"content":{"rendered":"<p class=\"wp-block-paragraph\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306f\u3001\u5f37\u5ea6\u3001\u8010\u4e45\u6027\u3001\u8010\u5019\u6027\u306b\u512a\u308c\u3066\u3044\u308b\u3053\u3068\u3067\u77e5\u3089\u308c\u308b\u7d20\u6750\u3067\u3059\u3002\u5efa\u8a2d\u3001\u81ea\u52d5\u8eca\u3001\u30a8\u30cd\u30eb\u30ae\u30fc\u7523\u696d\u306a\u3069\u3001\u3055\u307e\u3056\u307e\u306a\u5206\u91ce\u3067\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306f\u6b20\u304b\u305b\u307e\u305b\u3093\u3002<\/p><p class=\"wp-block-paragraph\">\u3053\u306e\u8a18\u4e8b\u3067\u306f\u3001\u3055\u307e\u3056\u307e\u306a\u30cb\u30fc\u30ba\u3092\u6e80\u305f\u3059\u4e9c\u925b\u30e1\u30c3\u30ad\u65b9\u6cd5\u3001\u51e6\u7406\u6280\u8853\u3001\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306e\u591a\u69d8\u306a\u7528\u9014\u306b\u3064\u3044\u3066\u8aac\u660e\u3057\u307e\u3059\u3002\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306e\u4e16\u754c\u306b\u98db\u3073\u8fbc\u3093\u3067\u307f\u307e\u305b\u3093\u304b\u3002<\/p><h2 class=\"wp-block-heading\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u3068\u306f\u4f55\u3067\u3059\u304b?<\/h2><p class=\"wp-block-paragraph\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306f\u3001\u70ad\u7d20\u92fc\u307e\u305f\u306f\u4f4e\u5408\u91d1\u92fc\u306b 99% \u92fc\u3068 1% \u4e9c\u925b\u3092\u52a0\u3048\u305f\u3082\u306e\u3067\u3001\u8010\u8150\u98df\u6027\u304c\u3042\u308a\u9280\u7070\u8272\u3067\u3059\u3002\u4e3b\u306b\u6eb6\u878d\u4e9c\u925b\u30e1\u30c3\u30ad\u3067\u88fd\u9020\u3055\u308c\u3001\u4e9c\u925b\u9244\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u306b\u3088\u308a\u6e7f\u6c17\u3084\u6e29\u5ea6\u306b\u3088\u308b\u640d\u50b7\u304b\u3089\u4fdd\u8b77\u3057\u307e\u3059\u3002\u5f37\u5ea6\u3001\u8010\u4e45\u6027\u3001\u6210\u5f62\u6027\u306b\u512a\u308c\u3066\u3044\u308b\u305f\u3081\u3001\u5efa\u8a2d\u3001\u81ea\u52d5\u8eca\u3001\u8fb2\u696d\u3001\u592a\u967d\u5149\u767a\u96fb\u696d\u754c\u3067\u5e83\u304f\u4f7f\u7528\u3055\u308c\u3066\u3044\u307e\u3059\u3002\u96fb\u6c17\u4e9c\u925b\u30e1\u30c3\u30ad\u3067\u306f\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u304c\u8584\u304f\u3001\u30b7\u30fc\u30c8\u3001\u30d1\u30a4\u30d7\u3001\u69cb\u9020\u90e8\u54c1\u306a\u3069\u306e\u5f62\u3067\u3055\u307e\u3056\u307e\u306a\u7528\u9014\u306b\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306e\u4f55\u304c\u7279\u5225\u306a\u306e\u3067\u3057\u3087\u3046\u304b?<\/h3><p class=\"wp-block-paragraph\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306b\u306f\u512a\u308c\u305f\u8010\u8150\u98df\u6027\u3092\u63d0\u4f9b\u3059\u308b\u4fdd\u8b77\u4e9c\u925b\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u304c\u65bd\u3055\u308c\u3066\u304a\u308a\u3001\u8010\u4e45\u6027\u306b\u512a\u308c\u3001\u5c4b\u5916\u3084\u904e\u9177\u306a\u74b0\u5883\u306b\u6700\u9069\u3067\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u92fc\u3068\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306e\u9055\u3044\u306f\u4f55\u3067\u3059\u304b?<\/h3><p class=\"wp-block-paragraph\">\u92fc\u306f\u30d9\u30fc\u30b9\u30e1\u30bf\u30eb\u3068\u3057\u3066\u6a5f\u80fd\u3057\u307e\u3059\u304c\u3001\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306f\u8010\u98df\u6027\u3092\u5411\u4e0a\u3055\u305b\u308b\u305f\u3081\u306b\u4e9c\u925b\u3067\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u3055\u308c\u305f\u92fc\u3067\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u3068\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306e\u3069\u3061\u3089\u304c\u5f37\u3044\u3067\u3059\u304b?<\/h3><p class=\"wp-block-paragraph\">\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u4e00\u822c\u306b\u3001\u7279\u306b\u904e\u9177\u306a\u6761\u4ef6\u4e0b\u3067\u306f\u3001\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u3088\u308a\u3082\u5f37\u5ea6\u304c\u9ad8\u304f\u3001\u8010\u8150\u98df\u6027\u306b\u512a\u308c\u3066\u3044\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306e\u6b74\u53f2<\/h2><ul class=\"wp-block-list\"><li><strong>17\u4e16\u7d00<\/strong>\u82f1\u56fd\u738b\u7acb\u6b66\u5668\u535a\u7269\u9928\u6240\u8535\u306e 17 \u4e16\u7d00\u30a4\u30f3\u30c9\u306e\u93a7\u306b\u4f7f\u308f\u308c\u3066\u3044\u305f\u6700\u53e4\u306e\u4e9c\u925b\u30e1\u30c3\u30ad\u9244\u3002<\/li>\n\n<li><strong>1837<\/strong>\u30b9\u30bf\u30cb\u30b9\u30e9\u30b9\u30fb\u30bd\u30ec\u30eb\u304c\u6eb6\u878d\u4e9c\u925b\u3081\u3063\u304d\u30d7\u30ed\u30bb\u30b9\u306e\u7279\u8a31\u3092\u53d6\u5f97\u3002<\/li>\n\n<li><strong>1850\u5e74\u4ee3<\/strong>: \u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u304c\u30e8\u30fc\u30ed\u30c3\u30d1\u3067\u5e02\u8ca9\u3055\u308c\u308b\u3088\u3046\u306b\u306a\u308b\u3002<\/li>\n\n<li><strong>20\u4e16\u7d00\u521d\u982d<\/strong>: \u5efa\u8a2d\u696d\u3084\u8fb2\u696d\u3067\u5e83\u304f\u4f7f\u7528\u3055\u308c\u3066\u3044\u307e\u3059\u3002<\/li>\n\n<li><strong>1970\u5e74\u4ee3<\/strong>\u3088\u308a\u8584\u3044\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u3092\u5b9f\u73fe\u3059\u308b\u305f\u3081\u306b\u96fb\u6c17\u4e9c\u925b\u30e1\u30c3\u30ad\u304c\u5c0e\u5165\u3055\u308c\u307e\u3057\u305f\u3002<\/li>\n\n<li><strong>\u73fe\u5728<\/strong>\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306f\u3001\u305d\u306e\u8010\u4e45\u6027\u3068\u30b3\u30b9\u30c8\u52b9\u7387\u306e\u826f\u3055\u304b\u3089\u4e16\u754c\u4e2d\u3067\u5e83\u304f\u4f7f\u7528\u3055\u308c\u3066\u3044\u307e\u3059\u3002<\/li><\/ul><h2 class=\"wp-block-heading\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306e\u7a2e\u985e<\/h2><p class=\"wp-block-paragraph\">\u3053\u306e\u30bb\u30af\u30b7\u30e7\u30f3\u3067\u306f\u3001\u3055\u307e\u3056\u307e\u306a\u696d\u754c\u306e\u30cb\u30fc\u30ba\u306b\u5408\u308f\u305b\u3066\u305d\u308c\u305e\u308c\u7570\u306a\u308b\u30d7\u30ed\u30bb\u30b9\u3001\u5229\u70b9\u3001\u30bd\u30ea\u30e5\u30fc\u30b7\u30e7\u30f3\u3092\u5099\u3048\u305f\u4e3b\u8981\u306a\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306e\u7a2e\u985e\u306b\u3064\u3044\u3066\u8aac\u660e\u3057\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u7c89\u4f53\u5857\u88c5\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc<\/h3><ul class=\"wp-block-list\"><li><strong>\u30d7\u30ed\u30bb\u30b9<\/strong>\u4e9c\u925b\u30e1\u30c3\u30ad\u5f8c\u3001\u92fc\u9244\u306b\u4e7e\u71e5\u7c89\u672b\u3092\u9759\u96fb\u5857\u88c5\u3057\u3001\u71b1\u3067\u786c\u5316\u3055\u305b\u3066\u56fa\u3044\u5c64\u3092\u4f5c\u308a\u307e\u3059\u3002<\/li>\n\n<li><strong>\u30e1\u30ea\u30c3\u30c8<\/strong>: \u8010\u8150\u98df\u6027\u304c\u5f37\u5316\u3055\u308c\u3001\u8272\u3082\u30ab\u30b9\u30bf\u30de\u30a4\u30ba\u53ef\u80fd\u3002<\/li><\/ul><p class=\"wp-block-paragraph\">\u63a5\u7740\u306b\u306f\u9069\u5207\u306a\u8868\u9762\u51e6\u7406\u304c\u5fc5\u8981\u3067\u3059\u3002\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u306e\u63a5\u7740\u6027\u3068\u8010\u4e45\u6027\u3092\u6700\u9069\u306b\u3059\u308b\u305f\u3081\u306b\u3001\u5fb9\u5e95\u3057\u305f\u524d\u51e6\u7406\u3092\u5b9f\u65bd\u3057\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u6eb6\u878d\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc<\/h3><ul class=\"wp-block-list\"><li><strong>\u30d7\u30ed\u30bb\u30b9<\/strong>\u92fc\u9244\u3092\u6eb6\u878d\u4e9c\u925b\u306b\u6d78\u3057\u3001\u6bcd\u6750\u3068\u7d50\u5408\u3059\u308b\u539a\u3044\u4e9c\u925b\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u3092\u5f62\u6210\u3057\u307e\u3059\u3002<\/li>\n\n<li><strong>\u30e1\u30ea\u30c3\u30c8<\/strong>: \u6c34\u7d20\u8106\u5316\u306e\u5371\u967a\u6027\u304c\u3042\u308b\u9ad8\u5f37\u5ea6\u92fc\u3092\u9664\u304d\u3001\u5f37\u5ea6\u3092\u5927\u5e45\u306b\u4f4e\u4e0b\u3055\u305b\u308b\u3053\u3068\u306a\u304f\u512a\u308c\u305f\u8010\u8150\u98df\u6027\u3092\u767a\u63ee\u3057\u307e\u3059\u3002<\/li><\/ul><p class=\"wp-block-paragraph\">\u9ad8\u5f37\u5ea6\u92fc\u306b\u304a\u3051\u308b\u6f5c\u5728\u7684\u306a\u6c34\u7d20\u8106\u5316\u3002\u7279\u306b\u9ad8\u5f37\u5ea6\u6750\u6599\u306e\u5834\u5408\u3001\u30ea\u30b9\u30af\u3092\u6700\u5c0f\u9650\u306b\u6291\u3048\u308b\u305f\u3081\u306b\u30d7\u30ed\u30bb\u30b9\u3092\u614e\u91cd\u306b\u7ba1\u7406\u3057\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u5857\u88c5\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc<\/h3><ul class=\"wp-block-list\"><li><strong>\u30d7\u30ed\u30bb\u30b9<\/strong>\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306f\u4e0b\u5857\u308a\u3055\u308c\u3001\u305d\u306e\u5f8c\u3001\u4fdd\u8b77\u5f37\u5316\u307e\u305f\u306f\u7f8e\u89b3\u5411\u4e0a\u306e\u305f\u3081\u306b\u5857\u6599\u3067\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u3055\u308c\u307e\u3059\u3002<\/li>\n\n<li><strong>\u30e1\u30ea\u30c3\u30c8<\/strong>: \u7f8e\u89b3\u8981\u4ef6\u3092\u6e80\u305f\u3059\u80fd\u529b\u3092\u5099\u3048\u305f\u8010\u8150\u98df\u6027\u304c\u8ffd\u52a0\u3055\u308c\u307e\u3057\u305f\u3002<\/li><\/ul><p class=\"wp-block-paragraph\">\u5857\u88c5\u304c\u6469\u8017\u3059\u308b\u53ef\u80fd\u6027\u304c\u3042\u308b\u305f\u3081\u3001\u6642\u9593\u306e\u7d4c\u904e\u3068\u3068\u3082\u306b\u30e1\u30f3\u30c6\u30ca\u30f3\u30b9\u304c\u5fc5\u8981\u306b\u306a\u308a\u307e\u3059\u3002\u5f53\u793e\u3067\u306f\u3001\u8010\u4e45\u6027\u306e\u3042\u308b\u4ed5\u4e0a\u304c\u308a\u3092\u4fdd\u8a3c\u3059\u308b\u305f\u3081\u306b\u3001\u9ad8\u7d1a\u5857\u6599\u3068\u6700\u5148\u7aef\u306e\u65b9\u6cd5\u3092\u63a1\u7528\u3057\u3066\u3044\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u4e9c\u925b\u3081\u3063\u304d\u92fc<\/h3><ul class=\"wp-block-list\"><li><strong>\u30d7\u30ed\u30bb\u30b9<\/strong>\u6eb6\u878d\u4e9c\u925b\u30e1\u30c3\u30ad\u5f8c\u3001\u92fc\u3092\u52a0\u71b1\u3057\u3066\u4e9c\u925b\u3092\u9244\u3068\u5b8c\u5168\u306b\u5408\u91d1\u5316\u3057\u3001\u4e9c\u925b\u9244\u5c64\u3092\u5f62\u6210\u3057\u307e\u3059\u3002<\/li>\n\n<li><strong>\u30e1\u30ea\u30c3\u30c8<\/strong>: \u901a\u5e38\u306e\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306b\u6bd4\u3079\u3066\u3001\u5857\u6599\u306e\u5bc6\u7740\u6027\u304a\u3088\u3073\u6eb6\u63a5\u6027\u306b\u512a\u308c\u3066\u3044\u307e\u3059\u3002<\/li><\/ul><p class=\"wp-block-paragraph\">\u6eb6\u878d\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u3068\u6bd4\u8f03\u3059\u308b\u3068\u8010\u98df\u6027\u304c\u4f4e\u4e0b\u3057\u307e\u3059\u3002\u5f53\u793e\u3067\u306f\u3001\u7279\u5b9a\u306e\u7528\u9014\u306b\u5408\u308f\u305b\u3066\u8010\u98df\u6027\u3092\u9ad8\u3081\u308b\u30ab\u30b9\u30bf\u30de\u30a4\u30ba\u3055\u308c\u305f\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u3068\u51e6\u7406\u3092\u63d0\u4f9b\u3057\u3066\u3044\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306f\u9306\u3073\u307e\u3059\u304b\uff1f<\/h3><p class=\"wp-block-paragraph\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306f\u6700\u7d42\u7684\u306b\u306f\u9306\u3073\u307e\u3059\u304c\u3001\u4e9c\u925b\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u304c\u72a0\u7272\u4fdd\u8b77\u3092\u63d0\u4f9b\u3059\u308b\u3053\u3068\u3067\u9306\u3073\u308b\u30d7\u30ed\u30bb\u30b9\u3092\u5927\u5e45\u306b\u9045\u3089\u305b\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306e\u5f62\u72b6<\/h2><p class=\"wp-block-paragraph\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306f\u591a\u69d8\u306a\u5f62\u72b6\u3092\u3057\u3066\u3044\u308b\u305f\u3081\u3001\u3055\u307e\u3056\u307e\u306a\u696d\u754c\u3067\u5e45\u5e83\u304f\u4f7f\u7528\u3067\u304d\u3001\u3055\u307e\u3056\u307e\u306a\u69cb\u9020\u7684\u304a\u3088\u3073\u6a5f\u80fd\u7684\u30cb\u30fc\u30ba\u3092\u6e80\u305f\u3057\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u677f<\/h3><ul class=\"wp-block-list\"><li><strong>\u30d5\u30e9\u30c3\u30c8\u30b7\u30fc\u30c4<\/strong>: \u8584\u304f\u5e73\u3089\u306a\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u677f\u3002\u5c4b\u6839\u3001\u5916\u88c5\u6750\u3001\u30c0\u30af\u30c8\u306a\u3069\u306b\u3088\u304f\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/li>\n\n<li><strong>\u30d7\u30ec\u30fc\u30c8<\/strong>: \u539a\u3044\u30b7\u30fc\u30c8\u306a\u306e\u3067\u3001\u6a4b\u6881\u3001\u9020\u8239\u3001\u5927\u898f\u6a21\u5efa\u8a2d\u30d7\u30ed\u30b8\u30a7\u30af\u30c8\u306a\u3069\u306e\u9ad8\u8ca0\u8377\u7528\u9014\u306b\u6700\u9069\u3067\u3059\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">\u4e9c\u925b\u30e1\u30c3\u30ad\u30b3\u30a4\u30eb<\/h3><ul class=\"wp-block-list\"><li><strong>\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u30b3\u30a4\u30eb<\/strong>: \u81ea\u52d5\u8eca\u30d1\u30cd\u30eb\u3001\u5bb6\u96fb\u88fd\u54c1\u3001\u7523\u696d\u6a5f\u68b0\u306b\u3088\u304f\u4f7f\u7528\u3055\u308c\u308b\u9023\u7d9a\u30ed\u30fc\u30eb\u92fc\u3002\u30b3\u30a4\u30eb\u306f\u88fd\u9020\u6642\u306b\u7c21\u5358\u306b\u5207\u65ad\u304a\u3088\u3073\u6210\u5f62\u3067\u304d\u307e\u3059\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">\u4e9c\u925b\u30e1\u30c3\u30ad\u30d1\u30a4\u30d7\u3068\u30c1\u30e5\u30fc\u30d6<\/h3><ul class=\"wp-block-list\"><li><strong>\u4e38\u30d1\u30a4\u30d7<\/strong>: \u914d\u7ba1\u3001\u704c\u6f11\u30b7\u30b9\u30c6\u30e0\u3001\u69cb\u9020\u30d5\u30ec\u30fc\u30e0\u30ef\u30fc\u30af\u306a\u3069\u306b\u4f7f\u7528\u3055\u308c\u308b\u5186\u5f62\u306e\u30c1\u30e5\u30fc\u30d6\u3002<\/li>\n\n<li><strong>\u6b63\u65b9\u5f62\/\u9577\u65b9\u5f62\u30c1\u30e5\u30fc\u30d6<\/strong>: \u91d1\u5c5e\u30d5\u30ec\u30fc\u30e0\u3001\u30d5\u30a7\u30f3\u30b9\u3001\u652f\u6301\u69cb\u9020\u7269\u306e\u5efa\u8a2d\u3067\u3088\u304f\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/li>\n\n<li><strong>\u5c0e\u7ba1\u30d1\u30a4\u30d7<\/strong>: \u5efa\u8a2d\u73fe\u5834\u3084\u7523\u696d\u73fe\u5834\u3067\u306e\u96fb\u6c17\u914d\u7dda\u4fdd\u8b77\u7528\u306b\u7279\u5225\u306b\u8a2d\u8a08\u3055\u308c\u3066\u3044\u307e\u3059\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">\u4e9c\u925b\u30e1\u30c3\u30ad\u30d0\u30fc\u3068\u30ed\u30c3\u30c9<\/h3><ul class=\"wp-block-list\"><li><strong>\u4e38\u68d2<\/strong>: \u5efa\u8a2d\u3001\u67f5\u3001\u8fb2\u696d\u6a5f\u68b0\u306a\u3069\u306b\u4f7f\u7528\u3055\u308c\u308b\u5186\u7b52\u5f62\u306e\u68d2\u3002<\/li>\n\n<li><strong>\u30b9\u30af\u30a8\u30a2\u30d0\u30fc<\/strong>: \u88c5\u98fe\u69cb\u9020\u7269\u3001\u9580\u3001\u91d1\u5c5e\u52a0\u5de5\u306a\u3069\u3067\u3088\u304f\u4f7f\u7528\u3055\u308c\u308b\u89d2\u578b\u30d7\u30ed\u30d5\u30a1\u30a4\u30eb\u306e\u30d0\u30fc\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">\u4e9c\u925b\u30e1\u30c3\u30ad\u69cb\u9020\u5f62\u72b6<\/h3><ul class=\"wp-block-list\"><li><strong>I\u30d3\u30fc\u30e0<\/strong>\u6a4b\u6881\u3001\u30d3\u30eb\u3001\u7523\u696d\u65bd\u8a2d\u306a\u3069\u306e\u5927\u898f\u6a21\u306a\u5efa\u8a2d\u30d7\u30ed\u30b8\u30a7\u30af\u30c8\u3067\u4f7f\u7528\u3055\u308c\u308b\u5927\u578b\u306eI\u5b57\u578b\u92fc\u6881\u3002<\/li>\n\n<li><strong>H\u5f62\u6881<\/strong>: I \u30d3\u30fc\u30e0\u306b\u4f3c\u3066\u3044\u307e\u3059\u304c\u3001\u3088\u308a\u5e45\u5e83\u306e\u30d5\u30e9\u30f3\u30b8\u3092\u5099\u3048\u3066\u304a\u308a\u3001\u5805\u7262\u306a\u69cb\u9020\u30d5\u30ec\u30fc\u30e0\u30ef\u30fc\u30af\u306b\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/li>\n\n<li><strong>\u30c1\u30e3\u30f3\u30cd\u30eb\uff08C\u5b57\u578b\uff09<\/strong>: C \u5b57\u578b\u306e\u6881\u3002\u5efa\u8a2d\u3001\u91d1\u5c5e\u30d5\u30ec\u30fc\u30e0\u3001\u8eca\u4e21\u90e8\u54c1\u306b\u3088\u304f\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/li>\n\n<li><strong>\u30a2\u30f3\u30b0\u30eb\uff08L\u5b57\u578b\uff09<\/strong>\u5efa\u7269\u3001\u6a4b\u6881\u3001\u7523\u696d\u65bd\u8a2d\u306e\u69cb\u9020\u3001\u30d5\u30ec\u30fc\u30e0\u3001\u30d6\u30ec\u30fc\u30b9\u3092\u5f37\u5316\u3059\u308b\u305f\u3081\u306e L \u5b57\u578b\u30bb\u30af\u30b7\u30e7\u30f3\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">\u4e9c\u925b\u30e1\u30c3\u30ad\u30ef\u30a4\u30e4\u30fc\u3068\u30e1\u30c3\u30b7\u30e5<\/h3><ul class=\"wp-block-list\"><li><strong>\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u7dda<\/strong>: \u30d5\u30a7\u30f3\u30b9\u3001\u30b1\u30fc\u30d6\u30eb\u3001\u30d6\u30c9\u30a6\u5712\u306e\u30c8\u30ec\u30ea\u30b9\u306e\u652f\u67f1\u306a\u3069\u306b\u3088\u304f\u4f7f\u7528\u3055\u308c\u308b\u7d30\u3044\u92fc\u7dda\u3002<\/li>\n\n<li><strong>\u91d1\u7db2<\/strong>: \u4e9c\u925b\u30e1\u30c3\u30ad\u3055\u308c\u305f\u30ef\u30a4\u30e4\u30fc\u3092\u7e54\u308a\u5408\u308f\u305b\u3066\u4f5c\u3089\u308c\u3001\u30d5\u30a7\u30f3\u30b9\u3001\u30b9\u30af\u30ea\u30fc\u30f3\u3001\u30b3\u30f3\u30af\u30ea\u30fc\u30c8\u306e\u88dc\u5f37\u6750\u3068\u3057\u3066\u3088\u304f\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">\u4e9c\u925b\u30e1\u30c3\u30ad\u30d7\u30ed\u30d5\u30a1\u30a4\u30eb\u3068\u30ab\u30b9\u30bf\u30e0\u30bb\u30af\u30b7\u30e7\u30f3<\/h3><ul class=\"wp-block-list\"><li><strong>U\u30d7\u30ed\u30d5\u30a1\u30a4\u30eb<\/strong>: \u30d5\u30ec\u30fc\u30df\u30f3\u30b0\u304a\u3088\u3073\u30c1\u30e3\u30cd\u30ea\u30f3\u30b0 \u30b7\u30b9\u30c6\u30e0\u306e\u5efa\u8a2d\u306b\u4f7f\u7528\u3055\u308c\u308b U \u5b57\u578b\u30bb\u30af\u30b7\u30e7\u30f3\u3002<\/li>\n\n<li><strong>Z\u30d7\u30ed\u30d5\u30a1\u30a4\u30eb<\/strong>Z \u5f62\u92fc\u306f\u3001\u5916\u88c5\u6750\u3001\u5c4b\u6839\u6750\u3001\u69cb\u9020\u652f\u6301\u6750\u3068\u3057\u3066\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/li>\n\n<li><strong>\u30ab\u30b9\u30bf\u30e0\u30d7\u30ed\u30d5\u30a1\u30a4\u30eb<\/strong>: \u7279\u5b9a\u306e\u7523\u696d\u307e\u305f\u306f\u5efa\u7bc9\u306e\u30cb\u30fc\u30ba\u306b\u5408\u308f\u305b\u3066\u8a2d\u8a08\u3055\u308c\u305f\u30ab\u30b9\u30bf\u30de\u30a4\u30ba\u3055\u308c\u305f\u5f62\u72b6\u3002<\/li><\/ul><p class=\"wp-block-paragraph\">\u4e0a\u8a18\u306e\u5f62\u72b6\u306b\u52a0\u3048\u3066\u3001 <strong>\u30b9\u30c1\u30fc\u30eb\u30d7\u30ed\u30b0\u30eb\u30fc\u30d7<\/strong> \u72ec\u81ea\u306e\u8981\u4ef6\u3092\u6e80\u305f\u3059\u30ab\u30b9\u30bf\u30de\u30a4\u30ba\u3055\u308c\u305f\u7279\u6b8a\u5f62\u72b6\u3092\u63d0\u4f9b\u3057\u307e\u3059\u3002 <a href=\"https:\/\/steelprogroup.com\/ja\/product-category\/galvanized-steel\/\"><strong>\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc<\/strong><\/a> \u30da\u30fc\u30b8\uff01<\/p><h2 class=\"wp-block-heading\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u677f\u306e\u7279\u6027<\/h2><p class=\"wp-block-paragraph\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306f\u3001\u8010\u8150\u98df\u6027\u3001\u6210\u5f62\u6027\u3001\u30b3\u30b9\u30c8\u52b9\u7387\u306a\u3069\u3001\u3055\u307e\u3056\u307e\u306a\u8010\u4e45\u6027\u3068\u6c4e\u7528\u6027\u3092\u5099\u3048\u3066\u3044\u307e\u3059\u3002\u3053\u308c\u3089\u306e\u91cd\u8981\u306a\u7279\u6027\u306b\u3088\u308a\u3001\u3055\u307e\u3056\u307e\u306a\u696d\u754c\u3067\u4fe1\u983c\u3067\u304d\u308b\u9078\u629e\u80a2\u3068\u306a\u3063\u3066\u3044\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\"><strong>\u8010\u98df\u6027<\/strong><\/h3><p class=\"wp-block-paragraph\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306f\u72a0\u7272\u967d\u6975\u4fdd\u8b77\u6a5f\u80fd\u3092\u5099\u3048\u3066\u304a\u308a\u3001\u640d\u50b7\u3057\u305f\u5834\u5408\u3067\u3082\u4e9c\u925b\u304c\u4e0b\u5730\u306e\u91d1\u5c5e\u3092\u4fdd\u8b77\u3057\u307e\u3059\u3002\u624b\u306e\u5c4a\u304d\u306b\u304f\u3044\u90e8\u5206\u3082\u542b\u3081\u3001\u5b8c\u5168\u306b\u30ab\u30d0\u30fc\u3055\u308c\u3066\u3044\u308b\u305f\u3081\u3001\u512a\u308c\u305f\u8010\u8150\u98df\u6027\u304c\u4fdd\u8a3c\u3055\u308c\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\"><strong>\u8010\u6469\u8017\u6027\u3068\u8010\u4e45\u6027<\/strong><\/h3><p class=\"wp-block-paragraph\">\u4e9c\u925b\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u306b\u3088\u308a\u3001\u512a\u308c\u305f\u8010\u6469\u8017\u6027\u3068\u9577\u671f\u306b\u308f\u305f\u308b\u8010\u4e45\u6027\u304c\u52a0\u308f\u308a\u3001\u53b3\u3057\u3044\u74b0\u5883\u306b\u3082\u9069\u3057\u3066\u3044\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\"><strong>\u6210\u5f62\u6027\u3068\u5f37\u5ea6<\/strong><\/h3><p class=\"wp-block-paragraph\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306f\u3001\u30d9\u30fc\u30b9\u6750\u6599\u306e\u5f37\u5ea6\u3092\u7dad\u6301\u3057\u3001\u7279\u306b\u8584\u3044\u4e9c\u925b\u5c64\u3067\u512a\u308c\u305f\u6df1\u7d5e\u308a\u6027\u80fd\u3092\u767a\u63ee\u3057\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\"><strong>\u8868\u9762\u54c1\u8cea\u3068\u5916\u89b3<\/strong><\/h3><p class=\"wp-block-paragraph\">\u8868\u9762\u306e\u5916\u89b3\u304c\u512a\u308c\u3066\u304a\u308a\u3001\u30dd\u30ea\u30de\u30fc\u307e\u305f\u306f\u30bb\u30e9\u30df\u30c3\u30af\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u304c\u65bd\u3055\u308c\u3066\u3044\u308b\u305f\u3081\u3001\u7f8e\u89b3\u3068\u8010\u8150\u98df\u6027\u304c\u5411\u4e0a\u3057\u3066\u3044\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\"><strong>\u6eb6\u63a5\u6027\u3068\u5857\u88c5\u6027<\/strong><\/h3><p class=\"wp-block-paragraph\">\u3053\u306e\u7d20\u6750\u306f\u7c21\u5358\u306b\u6eb6\u63a5\u3067\u304d\u3001\u74b0\u5883\u306b\u512a\u3057\u3044\u30af\u30ed\u30e0\u30d5\u30ea\u30fc\u306e\u4e0d\u52d5\u614b\u5316\u65b9\u6cd5\u306b\u3088\u308a\u5857\u6599\u306e\u5bc6\u7740\u6027\u304c\u5411\u4e0a\u3057\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\"><strong>\u30ea\u30b5\u30a4\u30af\u30eb\u6027\u3068\u30b3\u30b9\u30c8\u52b9\u7387<\/strong><\/h3><p class=\"wp-block-paragraph\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306f\u5b8c\u5168\u306b\u30ea\u30b5\u30a4\u30af\u30eb\u53ef\u80fd\u3067\u7d4c\u6e08\u7684\u3067\u3042\u308a\u3001\u624b\u9803\u306a\u30b3\u30b9\u30c8\u3067\u9577\u671f\u4f7f\u7528\u304c\u53ef\u80fd\u3067\u3059\u3002<\/p><h3 class=\"wp-block-heading\"><strong>\u8fc5\u901f\u306a\u51e6\u7406\u3068\u7c21\u5358\u306a\u691c\u67fb<\/strong><\/h3><p class=\"wp-block-paragraph\">\u4e9c\u925b\u30e1\u30c3\u30ad\u51e6\u7406\u306f\u9ad8\u901f\u3067\u3001\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u306f\u76ee\u8996\u307e\u305f\u306f\u7c21\u5358\u306a\u30c6\u30b9\u30c8\u3067\u7c21\u5358\u306b\u691c\u67fb\u3067\u304d\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306e\u6b20\u70b9\u306f\u4f55\u3067\u3059\u304b?<\/h2><p class=\"wp-block-paragraph\">\u904e\u9177\u306a\u6761\u4ef6\u4e0b\u3067\u306f\u9306\u3073\u3084\u3059\u304f\u3001\u4e9c\u925b\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u304c\u640d\u50b7\u3057\u3066\u3044\u308b\u5834\u5408\u306f\u3001\u9ad8\u6e29\u306e\u7528\u9014\u3067\u306f\u5f37\u5ea6\u304c\u4f4e\u4e0b\u3059\u308b\u53ef\u80fd\u6027\u304c\u3042\u308a\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306e\u5316\u5b66\u7684\u6027\u8cea<\/h2><p class=\"wp-block-paragraph\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306e\u4e3b\u306a\u7279\u6027\u306f\u3001\u8150\u98df\u3092\u9632\u3050\u72a0\u7272\u967d\u6975\u3068\u3057\u3066\u6a5f\u80fd\u3059\u308b\u4e9c\u925b\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u3067\u3059\u3002\u4e9c\u925b\u9244\u5c64\u306f\u9577\u671f\u7684\u306a\u4fdd\u8b77\u3092\u63d0\u4f9b\u3057\u307e\u3059\u3002\u30d9\u30fc\u30b9\u7d20\u6750\u3068\u306e\u4e3b\u306a\u9055\u3044\u306f\u3001\u8010\u8150\u98df\u6027\u3092\u5927\u5e45\u306b\u9ad8\u3081\u308b\u4e9c\u925b\u5c64\u3067\u3059\u3002<\/p><p class=\"wp-block-paragraph\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306e\u4e00\u822c\u7684\u306a\u5316\u5b66\u6210\u5206\u8868\uff08%\u91cd\u91cf\u57fa\u6e96\uff09<\/p><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u30a8\u30ec\u30e1\u30f3\u30c8<\/strong><\/td><td><strong>\u30d1\u30fc\u30bb\u30f3\u30c6\u30fc\u30b8 (%) (\u30e1\u30fc\u30c8\u30eb\u6cd5)<\/strong><\/td><td><strong>\u30d1\u30fc\u30bb\u30f3\u30c6\u30fc\u30b8 (%) (\u5e1d\u56fd)<\/strong><\/td><\/tr><tr><td>\u30ab\u30fc\u30dc\u30f3\uff08C\uff09<\/td><td>0.05<\/td><td>0.05<\/td><\/tr><tr><td>\u30de\u30f3\u30ac\u30f3 (Mn)<\/td><td>0.2<\/td><td>0.2<\/td><\/tr><tr><td>\u30ea\u30f3 (P)<\/td><td>0.04<\/td><td>0.04<\/td><\/tr><tr><td>\u786b\u9ec4\uff08S\uff09<\/td><td>0.05<\/td><td>0.05<\/td><\/tr><tr><td>\u4e9c\u925b\uff08Zn\uff09<\/td><td>99<\/td><td>99<\/td><\/tr><tr><td>\u9244\uff08Fe\uff09<\/td><td>\u30d0\u30e9\u30f3\u30b9<\/td><td>\u30d0\u30e9\u30f3\u30b9<\/td><\/tr><\/tbody><\/table><\/figure><p class=\"wp-block-paragraph\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306e\u4e00\u822c\u7684\u306a\u5316\u5b66\u7684\u6027\u8cea\u306e\u8868<\/p><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u30d7\u30ed\u30d1\u30c6\u30a3<\/strong><\/td><td><strong>\u8aac\u660e<\/strong><\/td><\/tr><tr><td>\u53cd\u5fdc\u6027<\/td><td>\u4f4e\u3044<\/td><\/tr><tr><td>\u6bd2\u6027<\/td><td>\u7121\u6bd2<\/td><\/tr><tr><td>\u5f15\u706b\u6027<\/td><td>\u4e0d\u71c3\u6027<\/td><\/tr><tr><td>\u8010\u98df\u6027<\/td><td>\u9ad8\u3044<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306e\u7269\u7406\u7684\u7279\u6027<\/h2><p class=\"wp-block-paragraph\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306e\u6700\u3082\u91cd\u8981\u306a\u7269\u7406\u7684\u7279\u6027\u306f\u3001\u4e9c\u925b\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u306b\u3088\u308b\u8010\u4e45\u6027\u306e\u5411\u4e0a\u3067\u3059\u3002\u4e9c\u925b\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u306b\u3088\u308a\u3001\u6210\u5f62\u6027\u3092\u7dad\u6301\u3057\u306a\u304c\u3089\u69cb\u9020\u5f37\u5ea6\u304c\u5411\u4e0a\u3057\u307e\u3059\u3002\u3053\u306e\u7d44\u307f\u5408\u308f\u305b\u306b\u3088\u308a\u3001\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306f\u3055\u307e\u3056\u307e\u306a\u696d\u754c\u306e\u3055\u307e\u3056\u307e\u306a\u8981\u6c42\u306e\u53b3\u3057\u3044\u7528\u9014\u306b\u9069\u3057\u3066\u3044\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306e\u4e00\u822c\u7684\u306a\u7269\u7406\u7684\u6027\u8cea\u306e\u8868<\/p><figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td><strong>\u30d7\u30ed\u30d1\u30c6\u30a3<\/strong><\/td><td><strong>\u30e1\u30fc\u30c8\u30eb\u5358\u4f4d<\/strong><\/td><td><strong>\u5e1d\u56fd\u5358\u4f4d<\/strong><\/td><\/tr><tr><td>\u5bc6\u5ea6<\/td><td>7.85 g\/cm\u00b3<\/td><td>0.284 lb\/in\u00b3<\/td><\/tr><tr><td>\u878d\u70b9<\/td><td>1200\u2103<\/td><td>2192\u00b0F<\/td><\/tr><tr><td>\u6cb8\u70b9<\/td><td>\u7d042500\u2103<\/td><td>\u7d044532\u00b0F<\/td><\/tr><tr><td>\u71b1\u4f1d\u5c0e\u7387<\/td><td>110W\/m\u00b7K<\/td><td>63.5 BTU\u00b7ft\/h\u00b7\u00b0F<\/td><\/tr><tr><td>\u96fb\u6c17\u4f1d\u5c0e\u7387<\/td><td>1.4 x 10\u2077 \u79d2\/\u30e1\u30fc\u30c8\u30eb<\/td><td>8.14 x 10\u2076 \u79d2\/\u30e1\u30fc\u30c8\u30eb<\/td><\/tr><tr><td>\u6bd4\u71b1\u5bb9\u91cf<\/td><td>490 J\/kg-K<\/td><td>0.117 BTU\/lb-\u00b0F<\/td><\/tr><tr><td>\u71b1\u81a8\u5f35\u4fc2\u6570<\/td><td>12 \u00b5m\/m\u00b7K<\/td><td>6.7 \u00b5in\/in-\u00b0F<\/td><\/tr><tr><td>\u96fb\u6c17\u62b5\u6297\u7387<\/td><td>7.1 x 10\u207b\u2078 \u03a9\u00b7m<\/td><td>4.28 x 10\u207b\u2076 \u03a9\u00b7\u30a4\u30f3\u30c1<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306e\u6a5f\u68b0\u7684\u6027\u8cea<\/h2><p class=\"wp-block-paragraph\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306e\u6700\u3082\u91cd\u8981\u306a\u6a5f\u68b0\u7684\u7279\u6027\u306f\u3001\u6210\u5f62\u6027\u3092\u72a0\u7272\u306b\u3059\u308b\u3053\u3068\u306a\u304f\u3001\u5f37\u5316\u3055\u308c\u305f\u5f15\u5f35\u5f37\u5ea6\u3068\u8010\u4e45\u6027\u3092\u5b9f\u73fe\u3057\u3066\u3044\u308b\u3053\u3068\u3067\u3059\u3002\u5f37\u5ea6\u3068\u67d4\u8edf\u6027\u304c\u878d\u5408\u3057\u305f\u3053\u306e\u92fc\u306f\u3001\u976d\u6027\u3068\u8010\u8150\u98df\u6027\u304c\u91cd\u8981\u3068\u306a\u308b\u69cb\u9020\u7528\u9014\u306b\u6700\u9069\u3067\u3059\u3002<\/p><p class=\"wp-block-paragraph\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306e\u4e00\u822c\u7684\u306a\u6a5f\u68b0\u7684\u6027\u8cea\u306e\u8868<\/p><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u30d7\u30ed\u30d1\u30c6\u30a3<\/strong><\/td><td><strong>\u30e1\u30fc\u30c8\u30eb\u5358\u4f4d<\/strong><\/td><td><strong>\u5e1d\u56fd\u5358\u4f4d<\/strong><\/td><\/tr><tr><td>\u5f15\u5f35\u5f37\u5ea6<\/td><td>380-550 MPa<\/td><td>55\uff5e80\u30ad\u30ed\u30fb\u30b7\u30fc<\/td><\/tr><tr><td>\u964d\u4f0f\u5f37\u5ea6<\/td><td>220\uff5e500MPa<\/td><td>32-73 ksi<\/td><\/tr><tr><td>\u30d6\u30ea\u30cd\u30eb\u786c\u5ea6<\/td><td>120-180 HB<\/td><td>120-180 HB<\/td><\/tr><tr><td>\u30ed\u30c3\u30af\u30a6\u30a7\u30eb\u786c\u5ea6<\/td><td>70-85 HRB<\/td><td>70-85 HRB<\/td><\/tr><tr><td>\u30d3\u30c3\u30ab\u30fc\u30b9\u786c\u5ea6<\/td><td>120-170 \u30d8\u30eb\u30c4<\/td><td>120-170 \u30d8\u30eb\u30c4<\/td><\/tr><tr><td>\u4f38\u3073<\/td><td>15-25%<\/td><td>15-25%<\/td><\/tr><tr><td>\u5f3e\u6027\u4fc2\u6570<\/td><td>200 GPa<\/td><td>29,000\u30ad\u30ed\u30fb\u30b7\u30fc<\/td><\/tr><tr><td>\u30dd\u30a2\u30bd\u30f3\u6bd4<\/td><td>0.27-0.30<\/td><td>0.27-0.30<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306e\u4e00\u822c\u7684\u306a\u30b0\u30ec\u30fc\u30c9<\/h2><p class=\"wp-block-paragraph\">\u4ee5\u4e0b\u306f\u3001\u7279\u5b9a\u306e\u7528\u9014\u3068\u6027\u80fd\u30cb\u30fc\u30ba\u306b\u5408\u308f\u305b\u3066\u8a2d\u8a08\u3055\u308c\u305f\u4e00\u822c\u7684\u306a\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306e\u30b0\u30ec\u30fc\u30c9\u306e\u30ea\u30b9\u30c8\u3067\u3059\u3002<\/p><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u30b0\u30ec\u30fc\u30c9<\/strong><\/td><td><strong>\u8aac\u660e<\/strong><\/td><\/tr><tr><td>DX51D+Z \u306b\u3064\u3044\u3066<\/td><td>\u51b7\u9593\u6210\u5f62\u7528\u306e\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u3002\u81ea\u52d5\u8eca\u3084\u5efa\u7bc9\u8cc7\u6750\u306b\u3088\u304f\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/td><\/tr><tr><td>DX52D + Z<\/td><td>DX51D \u306b\u4f3c\u3066\u3044\u307e\u3059\u304c\u3001\u3088\u308a\u8907\u96d1\u306a\u5f62\u72b6\u306b\u5bfe\u5fdc\u3067\u304d\u308b\u6210\u5f62\u6027\u304c\u5411\u4e0a\u3057\u3066\u3044\u307e\u3059\u3002<\/td><\/tr><tr><td>DC51D+Z \u306f\u3001<\/td><td>\u51b7\u9593\u5727\u5ef6\u30d9\u30fc\u30b9\u306b\u4e9c\u925b\u30e1\u30c3\u30ad\u3092\u65bd\u3057\u305f\u92fc\u3067\u3001\u4e3b\u306b\u5bb6\u96fb\u88fd\u54c1\u3084\u8efd\u5de5\u696d\u3067\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/td><\/tr><tr><td>S350GD+Z \u306b\u3064\u3044\u3066<\/td><td>\u6700\u5c0f\u964d\u4f0f\u5f37\u5ea6 350 MPa \u306e\u69cb\u9020\u7528\u92fc\u3067\u3001\u8010\u8377\u91cd\u69cb\u9020\u306b\u9069\u3057\u3066\u3044\u307e\u3059\u3002<\/td><\/tr><tr><td>G550 (ASTM A653 \u30b0\u30ec\u30fc\u30c980)<\/td><td>\u6700\u5c0f\u964d\u4f0f\u5f37\u5ea6 550 MPa \u306e\u6eb6\u878d\u4e9c\u925b\u30e1\u30c3\u30ad\u69cb\u9020\u7528\u92fc\u3067\u3001\u8efd\u91cf\u92fc\u69cb\u9020\u7269\u306b\u5e83\u304f\u4f7f\u7528\u3055\u308c\u3066\u3044\u307e\u3059\u3002<\/td><\/tr><tr><td>SGHC\u3001SGH400\u3001SGCC\uff08JIS\u898f\u683c\uff09<\/td><td>\u3055\u307e\u3056\u307e\u306a\u7523\u696d\u7528\u9014\u306b\u4f7f\u7528\u3055\u308c\u308b\u3001\u65e5\u672c\u5de5\u696d\u898f\u683c\u306b\u6e96\u62e0\u3057\u305f\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u3002<\/td><\/tr><tr><td>S220GD\u3001S250GD\u3001S320GD\uff08DIN EN\u898f\u683c\uff09<\/td><td>\u3053\u308c\u3089\u306e\u30b0\u30ec\u30fc\u30c9\u306f\u3001\u5efa\u8a2d\u3084\u88fd\u9020\u3067\u4e00\u822c\u7684\u306b\u4f7f\u7528\u3055\u308c\u308b\u3055\u307e\u3056\u307e\u306a\u964d\u4f0f\u5f37\u5ea6\u306b\u5bfe\u5fdc\u3057\u3066\u3044\u307e\u3059\u3002<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u92fc\u306e\u4e9c\u925b\u30e1\u30c3\u30ad\u5de5\u7a0b<\/h2><ol class=\"wp-block-list\"><li><strong>\u8868\u9762\u6d17\u6d44<\/strong>: \u6c5a\u308c\u3001\u6cb9\u5206\u3001\u4e0d\u7d14\u7269\u3092\u53d6\u308a\u9664\u304d\u307e\u3059\u3002<\/li>\n\n<li><strong>\u30d4\u30af\u30eb\u30b9<\/strong>: \u92fc\u3092\u9178\u306b\u6d78\u3057\u3066\u9306\u3084\u30b9\u30b1\u30fc\u30eb\u3092\u9664\u53bb\u3057\u307e\u3059\u3002<\/li>\n\n<li><strong>\u3059\u3059\u304e<\/strong>: \u9178\u306e\u6b8b\u7559\u7269\u3092\u9664\u53bb\u3002<\/li>\n\n<li><strong>\u30d5\u30e9\u30c3\u30af\u30b9<\/strong>: \u4fdd\u8b77\u30d5\u30e9\u30c3\u30af\u30b9\u5c64\u3092\u5857\u5e03\u3057\u307e\u3059\u3002<\/li>\n\n<li><strong>\u4e7e\u71e5<\/strong>: \u4e9c\u925b\u6d78\u6f2c\u524d\u306b\u6c34\u5206\u3092\u9664\u53bb\u3057\u307e\u3059\u3002<\/li>\n\n<li><strong>\u6eb6\u878d\u4e9c\u925b\u3081\u3063\u304d<\/strong>: \u92fc\u3092\u6eb6\u878d\u4e9c\u925b\u306b\u6d78\u3057\u3066\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u3057\u307e\u3059\u3002<\/li>\n\n<li><strong>\u51b7\u5374<\/strong>: \u51b7\u5374\u3057\u3066\u4e9c\u925b\u5c64\u3092\u56fa\u3081\u307e\u3059\u3002<\/li>\n\n<li><strong>\u691c\u67fb<\/strong>: \u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u306e\u54c1\u8cea\u3068\u5747\u4e00\u6027\u3092\u4fdd\u8a3c\u3057\u307e\u3059\u3002<\/li><\/ol><h2 class=\"wp-block-heading\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u677f\u306e\u52a0\u5de5<\/h2><h3 class=\"wp-block-heading\">\u524d\u51e6\u7406\u30d7\u30ed\u30bb\u30b9<\/h3><ol class=\"wp-block-list\"><li><strong>\u6eb6\u63a5<\/strong><ul class=\"wp-block-list\"><li><strong>\u30d7\u30ed\u30bb\u30b9<\/strong>: \u30ed\u30fc\u30eb\u6eb6\u63a5\u3001\u30b7\u30fc\u30e0\u6eb6\u63a5\u3001\u5f93\u6765\u306e\u6eb6\u63a5\u6280\u8853\u306a\u3069\u3001\u3055\u307e\u3056\u307e\u306a\u65b9\u6cd5\u3092\u4f7f\u7528\u3057\u3066\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u90e8\u54c1\u3092\u63a5\u5408\u3057\u307e\u3059\u3002<\/li>\n\n<li><strong>\u6280\u8853\u7684\u306a\u5229\u70b9<\/strong>: \u4e9c\u925b\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u306e\u8150\u98df\u4fdd\u8b77\u3092\u7dad\u6301\u3057\u306a\u304c\u3089\u69cb\u9020\u306e\u5b8c\u5168\u6027\u3092\u78ba\u4fdd\u3057\u307e\u3059\u3002\u30b7\u30fc\u30e0\u6eb6\u63a5\u306f\u3001\u9577\u3044\u92fc\u6750\u30bb\u30af\u30b7\u30e7\u30f3\u306e\u9023\u7d9a\u63a5\u5408\u306b\u6700\u9069\u3067\u3059\u3002<\/li>\n\n<li><strong>\u6eb6\u63a5\u5f8c\u306e\u51e6\u7406<\/strong>: \u6eb6\u63a5\u90e8\u5206\u306e\u8010\u8150\u98df\u6027\u3092\u5411\u4e0a\u3055\u305b\u308b\u305f\u3081\u306e\u71b1\u51e6\u7406\u3084\u4e0d\u52d5\u614b\u5316\u304c\u542b\u307e\u308c\u308b\u5834\u5408\u304c\u3042\u308a\u307e\u3059\u3002<\/li><\/ul><\/li>\n\n<li><strong>\u30d4\u30af\u30eb\u30b9<\/strong><ul class=\"wp-block-list\"><li><strong>\u30d7\u30ed\u30bb\u30b9<\/strong>\u4e9c\u925b\u30e1\u30c3\u30ad\u306e\u524d\u306b\u3001\u92fc\u9244\u3092\u9178\u6027\u6eb6\u6db2\u306b\u6d78\u3057\u3066\u4e0d\u7d14\u7269\u3001\u9306\u3001\u30b9\u30b1\u30fc\u30eb\u3092\u9664\u53bb\u3057\u307e\u3059\u3002<\/li>\n\n<li><strong>\u6280\u8853\u7684\u306a\u5229\u70b9<\/strong>: \u4e9c\u925b\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u306e\u5bc6\u7740\u6027\u3092\u9ad8\u3081\u308b\u305f\u3081\u306b\u8868\u9762\u3092\u304d\u308c\u3044\u306b\u3057\u3001\u5747\u4e00\u306a\u4fdd\u8b77\u5c64\u3092\u78ba\u4fdd\u3057\u307e\u3059\u3002<\/li><\/ul><\/li>\n\n<li><strong>\u4e9c\u925b\u30e1\u30c3\u30ad\u65b9\u6cd5<\/strong><ul class=\"wp-block-list\"><li><strong>\u6eb6\u878d\u4e9c\u925b\u3081\u3063\u304d<\/strong>: \u6eb6\u878d\u4e9c\u925b\u306b\u92fc\u3092\u6d78\u6f2c\u3057\u3001\u8010\u8150\u98df\u6027\u306e\u305f\u3081\u306e\u539a\u304f\u3066\u8010\u4e45\u6027\u306e\u3042\u308b\u5c64\u3092\u5f62\u6210\u3057\u307e\u3059\u3002<\/li>\n\n<li><strong>\u96fb\u6c17\u3081\u3063\u304d<\/strong>: \u96fb\u6d41\u3092\u4f7f\u7528\u3057\u3066\u3088\u308a\u8584\u304f\u5747\u4e00\u306a\u4e9c\u925b\u5c64\u3092\u5857\u5e03\u3057\u307e\u3059\u3002\u5c0f\u578b\u90e8\u54c1\u3084\u7cbe\u5bc6\u90e8\u54c1\u306b\u9069\u3057\u3066\u3044\u307e\u3059\u3002<\/li>\n\n<li><strong>\u4e9c\u925b\u3081\u3063\u304d\u92fc<\/strong>\u6eb6\u878d\u4e9c\u925b\u30e1\u30c3\u30ad\u3068\u5f8c\u51e6\u7406\u713c\u920d\u51e6\u7406\u3092\u7d44\u307f\u5408\u308f\u305b\u3066\u4e9c\u925b\u9244\u5408\u91d1\u3092\u4f5c\u308a\u3001\u6eb6\u63a5\u6027\u3068\u5857\u6599\u306e\u5bc6\u7740\u6027\u3092\u9ad8\u3081\u307e\u3059\u3002<\/li>\n\n<li><strong>\u71b1\u62e1\u6563<\/strong>: \u71b1\u3092\u5229\u7528\u3057\u3066\u4e9c\u925b\u3092\u92fc\u306e\u8868\u9762\u306b\u62e1\u6563\u3055\u305b\u3001\u4e9c\u925b\u9244\u5408\u91d1\u3092\u5f62\u6210\u3057\u3066\u8010\u6469\u8017\u6027\u3092\u9ad8\u3081\u307e\u3059\u3002<\/li>\n\n<li><strong>\u305d\u306e\u4ed6\u306e\u65b9\u6cd5<\/strong>: \u4e9c\u925b\u6eb6\u5c04\u3001\u6a5f\u68b0\u4e9c\u925b\u30e1\u30c3\u30ad\u3001\u771f\u7a7a\u4e9c\u925b\u30e1\u30c3\u30ad\u306a\u3069\u304c\u3042\u308a\u3001\u305d\u308c\u305e\u308c\u4fee\u7406\u3084\u7279\u6b8a\u306a\u74b0\u5883 (\u822a\u7a7a\u5b87\u5b99\u306a\u3069) \u306a\u3069\u306e\u7279\u5b9a\u306e\u7528\u9014\u306b\u5408\u308f\u305b\u3066\u8abf\u6574\u3055\u308c\u3066\u3044\u307e\u3059\u3002<\/li><\/ul><\/li>\n\n<li><strong>\u6210\u5f62<\/strong><ul class=\"wp-block-list\"><li><strong>\u30d7\u30ed\u30bb\u30b9<\/strong>\u5727\u5ef6\u3084\u66f2\u3052\u306a\u3069\u306e\u51b7\u9593\u6210\u5f62\u6280\u8853\u3092\u4f7f\u7528\u3057\u3066\u3001\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u3092\u5fc5\u8981\u306a\u69cb\u9020\u306b\u6210\u5f62\u3057\u307e\u3059\u3002<\/li>\n\n<li><strong>\u6280\u8853\u7684\u306a\u5229\u70b9<\/strong>: \u4e9c\u925b\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u306e\u5b8c\u5168\u6027\u3092\u7dad\u6301\u3057\u306a\u304c\u3089\u3001\u5efa\u8a2d\u3084\u81ea\u52d5\u8eca\u7528\u9014\u306e\u8907\u96d1\u306a\u5f62\u72b6\u3092\u53ef\u80fd\u306b\u3057\u307e\u3059\u3002<\/li><\/ul><\/li>\n\n<li><strong>\u51b7\u5374\u3068\u4e0d\u6d3b\u6027\u5316<\/strong><ul class=\"wp-block-list\"><li><strong>\u30d7\u30ed\u30bb\u30b9<\/strong>\u4e9c\u925b\u30e1\u30c3\u30ad\u5f8c\u3001\u92fc\u6750\u306f\u51b7\u5374\u3055\u308c\u3001\u4fdd\u7ba1\u4e2d\u306b\u8868\u9762\u304c\u9178\u5316\u3055\u308c\u308b\u306e\u3092\u9632\u3050\u305f\u3081\u306b\u4e0d\u52d5\u614b\u5316\u5c64\u304c\u65bd\u3055\u308c\u307e\u3059\u3002<\/li>\n\n<li><strong>\u6280\u8853\u7684\u306a\u5229\u70b9<\/strong>: \u8010\u98df\u6027\u3092\u9ad8\u3081\u3001\u4e9c\u925b\u5c64\u306e\u9577\u671f\u8010\u4e45\u6027\u3092\u78ba\u4fdd\u3057\u307e\u3059\u3002<\/li><\/ul><\/li><\/ol><h3 class=\"wp-block-heading\">\u5f8c\u51e6\u7406\u30d7\u30ed\u30bb\u30b9<\/h3><ol class=\"wp-block-list\"><li><strong>\u8868\u9762\u51e6\u7406<\/strong><ul class=\"wp-block-list\"><li><strong>\u7d75\u753b<\/strong>: \u8010\u8150\u98df\u6027\u3092\u9ad8\u3081\u3001\u5c4b\u5916\u3067\u306e\u4f7f\u7528\u306b\u9069\u3057\u305f\u30ab\u30b9\u30bf\u30de\u30a4\u30ba\u53ef\u80fd\u306a\u30ab\u30e9\u30fc\u3092\u63d0\u4f9b\u3057\u307e\u3059\u3002<\/li>\n\n<li><strong>\u7c89\u4f53\u5857\u88c5<\/strong>: \u512a\u308c\u305f\u8010\u5019\u6027\u3092\u5099\u3048\u3001\u8010\u4e45\u6027\u3068\u6ed1\u3089\u304b\u306a\u4ed5\u4e0a\u304c\u308a\u3092\u5b9f\u73fe\u3057\u307e\u3059\u3002<\/li>\n\n<li><strong>\u30dd\u30ea\u30de\u30fc\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0<\/strong>: \u8ffd\u52a0\u306e\u8150\u98df\u4fdd\u8b77\u3092\u63d0\u4f9b\u3057\u3001\u7523\u696d\u74b0\u5883\u306b\u6700\u9069\u3067\u3059\u3002<\/li>\n\n<li><strong>\u30bb\u30e9\u30df\u30c3\u30af\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0<\/strong>: \u8010\u71b1\u6027\u3068\u8010\u6469\u8017\u6027\u3092\u5411\u4e0a\u3055\u305b\u3001\u9ad8\u6027\u80fd\u306a\u6761\u4ef6\u3067\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/li>\n\n<li><strong>\u30af\u30ed\u30e0\u30d5\u30ea\u30fc\u4e0d\u52d5\u614b\u5316<\/strong>: \u8010\u8150\u98df\u6027\u3068\u5857\u6599\u5bc6\u7740\u6027\u3092\u5411\u4e0a\u3055\u305b\u308b\u74b0\u5883\u306b\u512a\u3057\u3044\u51e6\u7406\u3067\u3059\u3002<\/li>\n\n<li><strong>\u96fb\u6c17\u3081\u3063\u304d<\/strong>: \u5c0f\u3055\u304f\u8907\u96d1\u306a\u90e8\u54c1\u306e\u305f\u3081\u306e\u8584\u304f\u5747\u4e00\u306a\u91d1\u5c5e\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u3002<\/li>\n\n<li><strong>\u30ac\u30eb\u30d0\u30cb\u30c3\u30af\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0<\/strong>: \u72a0\u7272\u8150\u98df\u9632\u6b62\u306e\u305f\u3081\u306e\u96fb\u6c17\u5316\u5b66\u7684\u5fdc\u7528\u3002<\/li><\/ul><\/li>\n\n<li><strong>\u30b9\u30bf\u30f3\u30d4\u30f3\u30b0\u3001\u30d1\u30f3\u30c1\u30f3\u30b0\u3001\u66f2\u3052<\/strong><ul class=\"wp-block-list\"><li><strong>\u30d7\u30ed\u30bb\u30b9<\/strong>\u30b9\u30bf\u30f3\u30d4\u30f3\u30b0\u3001\u30a8\u30c3\u30b8\u66f2\u3052\u3001\u30d1\u30f3\u30c1\u30f3\u30b0\u306a\u3069\u306e\u6a5f\u68b0\u7684\u306a\u6210\u5f62\u65b9\u6cd5\u3092\u4f7f\u7528\u3057\u3066\u3001\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u3092\u7cbe\u5bc6\u306a\u90e8\u54c1\u306b\u6210\u5f62\u3057\u307e\u3059\u3002<\/li>\n\n<li><strong>\u6280\u8853\u7684\u306a\u5229\u70b9<\/strong>: \u4e9c\u925b\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u306e\u4fdd\u8b77\u3092\u7dad\u6301\u3057\u306a\u304c\u3089\u3001\u8907\u96d1\u306a\u30c7\u30b6\u30a4\u30f3\u3084\u7a7f\u5b54\u3092\u4f5c\u6210\u3067\u304d\u307e\u3059\u3002<\/li><\/ul><\/li>\n\n<li><strong>\u5f8c\u51e6\u7406\u51e6\u7406<\/strong><ul class=\"wp-block-list\"><li><strong>\u30a2\u30cb\u30fc\u30ea\u30f3\u30b0<\/strong>\u3053\u306e\u71b1\u51e6\u7406\u306b\u3088\u308a\u6a5f\u68b0\u7684\u7279\u6027\u304c\u5411\u4e0a\u3057\u3001\u5185\u90e8\u5fdc\u529b\u304c\u8efd\u6e1b\u3055\u308c\u307e\u3059\u3002<\/li>\n\n<li><strong>\u6280\u8853\u7684\u306a\u5229\u70b9<\/strong>: \u6210\u5f62\u6027\u3001\u5ef6\u6027\u304c\u5411\u4e0a\u3057\u3001\u5185\u90e8\u5fdc\u529b\u304c\u8efd\u6e1b\u3055\u308c\u308b\u305f\u3081\u3001\u53d6\u308a\u6271\u3044\u3084\u52a0\u5de5\u304c\u5bb9\u6613\u306b\u306a\u308a\u307e\u3059\u3002<\/li><\/ul><\/li>\n\n<li><strong>\u30ab\u30c3\u30c6\u30a3\u30f3\u30b0<\/strong><ul class=\"wp-block-list\"><li><strong>\u30d7\u30ed\u30bb\u30b9<\/strong>: \u3055\u307e\u3056\u307e\u306a\u539a\u3055\u3084\u7528\u9014\u306b\u5408\u308f\u305b\u3066\u8abf\u6574\u3055\u308c\u305f\u30ec\u30fc\u30b6\u30fc\u5207\u65ad\u3001\u30a6\u30a9\u30fc\u30bf\u30fc\u30b8\u30a7\u30c3\u30c8\u5207\u65ad\u3001\u30d7\u30e9\u30ba\u30de\u5207\u65ad\u304c\u542b\u307e\u308c\u307e\u3059\u3002<\/li>\n\n<li><strong>\u6280\u8853\u7684\u306a\u5229\u70b9<\/strong>: \u4e9c\u925b\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u3092\u640d\u50b7\u3059\u308b\u3053\u3068\u306a\u304f\u7cbe\u5bc6\u306a\u5207\u65ad\u3092\u5b9f\u73fe\u3057\u307e\u3059\u3002\u3053\u308c\u306f\u3001\u304d\u308c\u3044\u306a\u30a8\u30c3\u30b8\u3068\u6700\u5c0f\u9650\u306e\u71b1\u5f71\u97ff\u3092\u5fc5\u8981\u3068\u3059\u308b\u7528\u9014\u306b\u3068\u3063\u3066\u91cd\u8981\u3067\u3059\u3002<\/li><\/ul><\/li><\/ol><h2 class=\"wp-block-heading\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306e\u7528\u9014<\/h2><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u7523\u696d<\/strong><\/td><td><strong>\u7533\u3057\u8fbc\u307f<\/strong><\/td><\/tr><tr><td>\u5efa\u8a2d<\/td><td>\u5c4b\u6839\u3001\u5916\u88c5\u6750\u3001\u69cb\u9020\u90e8\u54c1\u3001\u30d5\u30ec\u30fc\u30e0\u3001\u30c0\u30af\u30c8\u5de5\u4e8b\u3002<\/td><\/tr><tr><td>\u81ea\u52d5\u8eca<\/td><td>\u30dc\u30c7\u30a3\u30d1\u30cd\u30eb\u3001\u30b7\u30e3\u30fc\u30b7\u90e8\u54c1\u3001\u6392\u6c17\u30b7\u30b9\u30c6\u30e0\u3001\u69cb\u9020\u88dc\u5f37\u6750\u3002<\/td><\/tr><tr><td>\u8fb2\u696d<\/td><td>\u30d5\u30a7\u30f3\u30b9\u3001\u704c\u6f11\u30b7\u30b9\u30c6\u30e0\u3001\u30b5\u30a4\u30ed\u3001\u8fb2\u696d\u6a5f\u68b0\u3002<\/td><\/tr><tr><td>\u88fd\u9020\u696d<\/td><td>\u5bb6\u96fb\u88fd\u54c1\u3001HVAC \u30b7\u30b9\u30c6\u30e0\u3001\u91d1\u5c5e\u88fd\u5bb6\u5177\u3001\u4fdd\u7ba1\u30b3\u30f3\u30c6\u30ca\u3002<\/td><\/tr><tr><td>\u30a8\u30cd\u30eb\u30ae\u30fc\u3068\u592a\u967d\u5149<\/td><td>\u592a\u967d\u5149\u30d1\u30cd\u30eb\u30de\u30a6\u30f3\u30c8\u3001\u9001\u96fb\u5854\u3001\u98a8\u529b\u30bf\u30fc\u30d3\u30f3\u3002<\/td><\/tr><tr><td>\u4ea4\u901a<\/td><td>\u9244\u9053\u306e\u7dda\u8def\u3001\u6a4b\u3001\u5b89\u5168\u67f5\u3002<\/td><\/tr><tr><td>\u5bb6\u96fb\u88fd\u54c1<\/td><td>\u6d17\u6fef\u6a5f\u3001\u51b7\u8535\u5eab\u3001\u30aa\u30fc\u30d6\u30f3\u3001\u305d\u306e\u4ed6\u306e\u5bb6\u5ead\u7528\u6a5f\u5668\u3002<\/td><\/tr><tr><td>\u30de\u30ea\u30f3<\/td><td>\u9020\u8239\u3001\u30c9\u30c3\u30af\u3001\u6d77\u6d0b\u69cb\u9020\u7269\u306e\u8010\u8150\u98df\u6027\u3002<\/td><\/tr><tr><td>\u96fb\u6c17<\/td><td>\u30b1\u30fc\u30d6\u30eb\u30c8\u30ec\u30a4\u3001\u5c0e\u7ba1\u30d1\u30a4\u30d7\u3001\u96fb\u6c17\u7b50\u4f53\u3002<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u5c02\u9580\u7684\u3067\u4fe1\u983c\u3067\u304d\u308b\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u30e1\u30fc\u30ab\u30fc<\/h2><p class=\"wp-block-paragraph\">\u3067 <strong>\u30b9\u30c1\u30fc\u30eb\u30d7\u30ed\u30b0\u30eb\u30fc\u30d7<\/strong>\u3001\u5f53\u793e\u306f\u3088\u308a\u591a\u304f\u306e\u518d\u51e6\u7406\u30aa\u30d7\u30b7\u30e7\u30f3\u3092\u63d0\u4f9b\u3057\u3066\u3044\u307e\u3059:<\/p><ol class=\"wp-block-list\"><li><strong>\u30b3\u30a4\u30eb\u5dfb\u304d\u3068\u305b\u3093\u65ad<\/strong>: \u30b7\u30fc\u30c8\u304a\u3088\u3073\u30b3\u30a4\u30eb\u751f\u7523\u306e\u30ab\u30b9\u30bf\u30e0\u30b5\u30a4\u30ba\u3002<\/li>\n\n<li><strong>\u30ed\u30fc\u30eb\u6210\u5f62\u3001\u30d1\u30f3\u30c1\u30f3\u30b0\u3001\u30b9\u30bf\u30f3\u30d4\u30f3\u30b0<\/strong>: \u6b63\u78ba\u306a\u30d7\u30ed\u30d5\u30a1\u30a4\u30eb\u3001\u30b3\u30f3\u30dd\u30fc\u30cd\u30f3\u30c8\u3001\u30d1\u30cd\u30eb\u3002<\/li>\n\n<li><strong>\u30a8\u30c3\u30b8\u66f2\u3052\u3001\u6df1\u7d5e\u308a<\/strong>: \u5bb9\u5668\u3084\u7b50\u4f53\u306a\u3069\u306e\u90e8\u54c1\u306e\u8907\u96d1\u306a\u5f62\u72b6\u3092\u6210\u5f62\u3057\u307e\u3059\u3002<\/li>\n\n<li><strong>\u30ec\u30fc\u30b6\u30fc\u3001\u30a6\u30a9\u30fc\u30bf\u30fc\u30b8\u30a7\u30c3\u30c8\u3001EDM\u5207\u65ad<\/strong>: \u4e9c\u925b\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u3092\u640d\u50b7\u3059\u308b\u3053\u3068\u306a\u304f\u3001\u8907\u96d1\u306a\u30c7\u30b6\u30a4\u30f3\u3092\u7cbe\u5bc6\u306b\u30ab\u30c3\u30c8\u3057\u307e\u3059\u3002<\/li><\/ol><p class=\"wp-block-paragraph\">\u3053\u308c\u3089\u306e\u30b5\u30fc\u30d3\u30b9\u306b\u52a0\u3048\u3066\u3001\u5f53\u793e\u306f <a href=\"https:\/\/steelprogroup.com\/ja\/product-category\/galvanized-steel\/pipe\/\"><strong>\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u7ba1<\/strong><\/a><strong>, <\/strong><a href=\"https:\/\/steelprogroup.com\/ja\/product-category\/galvanized-steel\/wire\/\"><strong>\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u7dda<\/strong><\/a><strong>, <\/strong><a href=\"https:\/\/steelprogroup.com\/ja\/product-category\/galvanized-steel\/sheet\/\"><strong>\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u677f<\/strong><\/a><strong>, <\/strong><a href=\"https:\/\/steelprogroup.com\/ja\/product-category\/galvanized-steel\/coil\/\"><strong>\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u30b3\u30a4\u30eb<\/strong><\/a><strong>,<\/strong> \u305d\u3057\u3066 <a href=\"https:\/\/steelprogroup.com\/ja\/product-category\/galvanized-steel\/ppgi\/\"><strong>\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc<\/strong> <strong>PPGI<\/strong><\/a>\u3055\u307e\u3056\u307e\u306a\u30d7\u30ed\u30b8\u30a7\u30af\u30c8\u8981\u4ef6\u3092\u6e80\u305f\u3059\u8010\u4e45\u6027\u306e\u3042\u308b\u30bd\u30ea\u30e5\u30fc\u30b7\u30e7\u30f3\u3092\u63d0\u4f9b\u3057\u307e\u3059\u3002\u3053\u308c\u3089\u306e\u88fd\u54c1\u306f\u3001\u53b3\u3057\u3044\u74b0\u5883\u306b\u8010\u3048\u3089\u308c\u308b\u3088\u3046\u306b\u8abf\u6574\u3055\u308c\u3001\u8010\u8150\u98df\u6027\u3068\u5e45\u5e83\u3044\u7528\u9014\u3092\u63d0\u4f9b\u3057\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\">\u5f0a\u793e\u306f\u304a\u5ba2\u69d8\u306e\u30cb\u30fc\u30ba\u306b\u5408\u308f\u305b\u305f\u9ad8\u54c1\u8cea\u306e\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u3092\u4fdd\u8a3c\u3057\u307e\u3059\u3002\u30d7\u30ed\u30b8\u30a7\u30af\u30c8\u306b\u4fe1\u983c\u3067\u304d\u308b\u30bd\u30ea\u30e5\u30fc\u30b7\u30e7\u30f3\u3092\u304a\u63a2\u3057\u306e\u5834\u5408\u306f\u3001\u4eca\u3059\u3050\u5f0a\u793e\u306b\u3054\u9023\u7d61\u3044\u305f\u3060\u304d\u3001\u500b\u5225\u306e\u3054\u76f8\u8ac7\u3068\u304a\u898b\u7a4d\u308a\u3092\u3054\u4f9d\u983c\u304f\u3060\u3055\u3044\u3002<\/p>","protected":false},"excerpt":{"rendered":"<p>\u4e9c\u925b\u30e1\u30c3\u30ad\u306e\u7a2e\u985e\u3001\u8868\u9762\u51e6\u7406\u3001\u5e45\u5e83\u3044\u7528\u9014\u306a\u3069\u3001\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306e\u5f37\u5ea6\u3084\u7279\u6027\u306b\u3064\u3044\u3066\u5b66\u3073\u307e\u3057\u3087\u3046\u3002<\/p>","protected":false},"author":1,"featured_media":20966,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"_eb_attr":"","rank_math_lock_modified_date":false,"site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"categories":[4274,4273],"tags":[],"class_list":["post-20965","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-knowledge-galvanized-steel","category-galvanized-steel"],"acf":[],"_links":{"self":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts\/20965","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/comments?post=20965"}],"version-history":[{"count":0,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts\/20965\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/media\/20966"}],"wp:attachment":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/media?parent=20965"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/categories?post=20965"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/tags?post=20965"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}