{"id":21083,"date":"2025-03-01T03:11:00","date_gmt":"2025-02-28T19:11:00","guid":{"rendered":"https:\/\/steelprogroup.com\/?p=21083"},"modified":"2025-03-18T13:40:39","modified_gmt":"2025-03-18T05:40:39","slug":"s250gd","status":"publish","type":"post","link":"https:\/\/steelprogroup.com\/ja\/galvanized-steel\/grades\/s250gd\/","title":{"rendered":"S250GD \u4e9c\u925b\u30e1\u30c3\u30ad\u92fc: \u5b9a\u7fa9\u3001\u7279\u6027\u3001\u7528\u9014"},"content":{"rendered":"<p class=\"wp-block-paragraph\">SteelPro Group\u306eS250GD\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306f\u3001\u5efa\u8a2d\u30fb\u88fd\u9020\u696d\u306b\u6700\u9069\u306a\u9078\u629e\u80a2\u3067\u3059\u3002\u5f37\u529b\u306a\u4e9c\u925b\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u306b\u3088\u308a\u3001\u8010\u98df\u6027\u3068\u8010\u4e45\u6027\u3092\u78ba\u4fdd\u3057\u3066\u3044\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\">\u8aad\u307f\u9032\u3081\u308b\u3068\u3001\u306a\u305c\u3053\u306e\u4e9c\u925b\u30e1\u30c3\u30ad\u91d1\u5c5e\u304c\u30a8\u30f3\u30b8\u30cb\u30a2\u3084\u5efa\u8a2d\u696d\u8005\u306b\u597d\u307e\u308c\u308b\u9078\u629e\u80a2\u306a\u306e\u304b\u304c\u308f\u304b\u308a\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">S250GD | 1.0242\u3068\u306f\u4f55\u3067\u3059\u304b\uff1f<\/h2><p class=\"wp-block-paragraph\">S250GD (1.0242) \u306f\u3001EN 10346 \u306b\u57fa\u3065\u304f\u69cb\u9020\u7528\u92fc\u306e\u7b49\u7d1a\u3067\u3001\u4e3b\u306b\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306b\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002\u300cS\u300d\u306f\u69cb\u9020\u7528\u92fc\u3001\u300c250\u300d\u306f MPa \u5358\u4f4d\u306e\u6700\u5c0f\u964d\u4f0f\u5f37\u5ea6\u3001\u300cGD\u300d\u306f\u4e9c\u925b\u30e1\u30c3\u30ad\u306b\u9069\u3057\u3066\u3044\u308b\u3053\u3068\u3092\u610f\u5473\u3057\u307e\u3059\u3002\u70ad\u7d20\u3001\u30de\u30f3\u30ac\u30f3\u3001\u30b7\u30ea\u30b3\u30f3\u3092\u542b\u307f\u3001\u786b\u9ec4\u3068\u30ea\u30f3\u306b\u306f\u53b3\u3057\u3044\u5236\u9650\u304c\u3042\u308a\u307e\u3059\u3002\u4e00\u822c\u7684\u306a\u65b9\u6cd5\u306b\u306f\u6eb6\u878d\u4e9c\u925b\u30e1\u30c3\u30ad\u3068\u96fb\u6c17\u4e9c\u925b\u30e1\u30c3\u30ad\u304c\u3042\u308a\u3001\u5efa\u8a2d\u3001\u5bb6\u96fb\u3001\u81ea\u52d5\u8eca\u7523\u696d\u5411\u3051\u306e\u4e9c\u925b\u30e1\u30c3\u30ad\u30b7\u30fc\u30c8\u307e\u305f\u306f\u30b3\u30a4\u30eb\u3092\u88fd\u9020\u3057\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">S250GD\u92fc\u76f8\u5f53\u30b0\u30ec\u30fc\u30c9<\/h2><figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td><strong>\u30b9\u30bf\u30f3\u30c0\u30fc\u30c9<\/strong><\/td><td><strong>\u540c\u7b49\u30b0\u30ec\u30fc\u30c9<\/strong><\/td><\/tr><tr><td>BS<\/td><td>\u6599\u91d1250G<\/td><\/tr><tr><td>ASTM<\/td><td>\u30b0\u30ec\u30fc\u30c9B\uff08ASTM A 466 M\uff09<\/td><\/tr><tr><td>\u30a4\u30ae\u30ea\u30b9<\/td><td>Q235<\/td><\/tr><tr><td>JIS<\/td><td>\uff33\uff27\uff23\uff13\uff14\uff10<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">S250GD | 1.0242 \u5316\u5b66\u7d44\u6210<\/h2><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u30a8\u30ec\u30e1\u30f3\u30c8<\/strong><\/td><td><strong>\u6700\u5927\u30b3\u30f3\u30c6\u30f3\u30c4\uff08%\uff09<\/strong><\/td><\/tr><tr><td>\u30ab\u30fc\u30dc\u30f3\uff08C\uff09<\/td><td>0.2<\/td><\/tr><tr><td>\u30de\u30f3\u30ac\u30f3 (Mn)<\/td><td>1.7<\/td><\/tr><tr><td>\u30b1\u30a4\u7d20 (Si)<\/td><td>0.5<\/td><\/tr><tr><td>\u30ea\u30f3 (P)<\/td><td>0.1<\/td><\/tr><tr><td>\u786b\u9ec4\uff08S\uff09<\/td><td>0.045<\/td><\/tr><tr><td>\u7a92\u7d20\uff08N\uff09<\/td><td>0.012<\/td><\/tr><tr><td>\u30a2\u30eb\u30df\u30cb\u30a6\u30e0\uff08Al\uff09<\/td><td>0.015<\/td><\/tr><\/tbody><\/table><\/figure><p class=\"wp-block-paragraph\">\u786b\u9ec4\u3001\u30ea\u30f3\u3001\u7a92\u7d20\u306a\u3069\u306e\u4e0d\u7d14\u7269\u306f S250GD \u306e\u6027\u80fd\u3092\u4f4e\u4e0b\u3055\u305b\u307e\u3059\u3002\u786b\u9ec4\u306f\u976d\u6027\u3092\u5f31\u3081\u3066\u5272\u308c\u3092\u5f15\u304d\u8d77\u3053\u3057\u3001\u30ea\u30f3\u306f\u8106\u3055\u3092\u5897\u5927\u3055\u305b\u307e\u3059\u3002\u7a92\u7d20\u306f\u92fc\u3092\u786c\u5316\u3055\u305b\u3001\u6642\u9593\u306e\u7d4c\u904e\u3068\u3068\u3082\u306b\u8106\u3055\u306b\u3064\u306a\u304c\u308a\u307e\u3059\u3002 <strong>\u30b9\u30c1\u30fc\u30eb\u30d7\u30ed\u30b0\u30eb\u30fc\u30d7<\/strong> \u3053\u308c\u3089\u306e\u4e0d\u7d14\u7269\u3092\u53b3\u5bc6\u306b\u7ba1\u7406\u3059\u308b\u3053\u3068\u3067\u3001\u9ad8\u6027\u80fd\u30a2\u30d7\u30ea\u30b1\u30fc\u30b7\u30e7\u30f3\u306b\u304a\u3051\u308b\u5b89\u5b9a\u3057\u305f\u54c1\u8cea\u3068\u8010\u4e45\u6027\u306e\u5411\u4e0a\u3092\u5b9f\u73fe\u3057\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">S250GD\u92fc\u306e\u6a5f\u68b0\u7684\u7279\u6027<\/h2><figure class=\"wp-block-table\"><table><tbody><tr><td rowspan=\"2\"><strong>\u92fc\u7a2e<\/strong><\/td><td rowspan=\"2\"><strong>\u964d\u4f0f\u5f37\u5ea6 MPa \u2265<\/strong><\/td><td rowspan=\"2\"><strong>\u5f15\u5f35\u5f37\u5ea6 MPa \u2265<\/strong><\/td><td colspan=\"2\"><strong>\u7834\u65ad\u5f8c\u4f38\u3073\u7387% \u2265<\/strong><\/td><td><strong>\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u63a5\u7740<\/strong><\/td><\/tr><tr><td><strong>\u516c\u79f0\u539a\u3055 mm \u2264 0.7<\/strong><\/td><td><strong>\u516c\u79f0\u539a\u3055 mm &gt; 0.7<\/strong><\/td><td><strong>\u66f2\u3052\u4e2d\u5fc3\u5f84\uff08a = \u677f\u539a\uff09<\/strong><\/td><\/tr><tr><td>S250GD+Z\u3001S250GD+ZF\u3001S250GD+ZA\u3001S250GD+ZM\u3001S250GD+AZ\u3001S250GD+AS<\/td><td>250<\/td><td>330<\/td><td>17<\/td><td>19<\/td><td>1a<\/td><\/tr><\/tbody><\/table><\/figure><h4 class=\"wp-block-heading\"><strong>S250GD\u306e\u7834\u65ad\u5f8c\u306e\u4f38\u3073<\/strong><\/h4><p class=\"wp-block-paragraph\">S250GD\u306e\u7834\u65ad\u4f38\u3073\u306f\u677f\u539a\u306b\u3088\u3063\u3066\u7570\u306a\u308a\u307e\u3059\u3002\u4f38\u3073\u304c\u5927\u304d\u3044\u307b\u3069\u92fc\u306e\u5ef6\u6027\u304c\u5411\u4e0a\u3057\u3001\u69d8\u3005\u306a\u6210\u5f62\u30d7\u30ed\u30bb\u30b9\u306b\u9069\u5fdc\u3057\u3001\u5272\u308c\u304c\u767a\u751f\u3057\u306b\u304f\u304f\u306a\u308a\u307e\u3059\u3002 <\/p><ul class=\"wp-block-list\"><li>\u539a\u30550.7mm\u4ee5\u4e0b\u3067\u306f\u4f38\u3073\u306f17%\u4ee5\u4e0a\u306b\u306a\u308a\u307e\u3059\u3002 <\/li>\n\n<li>\u539a\u3055\u304c0.7mm\u3092\u8d85\u3048\u308b\u3068\u4f38\u3073\u306f19%\u4ee5\u4e0a\u306b\u5897\u52a0\u3057\u307e\u3059\u3002<\/li><\/ul><p class=\"wp-block-paragraph\">\u3053\u306e\u4e26\u5916\u308c\u305f\u5ef6\u6027\u306b\u3088\u308a\u3001\u5f53\u793e\u306e S250GD \u306f\u3001\u52a0\u5de5\u4e2d\u306b\u5272\u308c\u305f\u308a\u58ca\u308c\u305f\u308a\u3059\u308b\u3053\u3068\u306a\u304f\u3001\u9ad8\u3044\u5ef6\u6027\u3068\u8010\u4e45\u6027\u304c\u6c42\u3081\u3089\u308c\u308b\u52a0\u5de5\u30cb\u30fc\u30ba\u306b\u7279\u306b\u9069\u3057\u3066\u3044\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">S250GD\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u677f\u306e\u5229\u70b9<\/h2><p class=\"wp-block-paragraph\">\u5f53\u793e\u306eS250GD\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306f\u3001\u5f37\u5ea6\u3001\u8010\u4e45\u6027\u3001\u52a0\u5de5\u6027\u306b\u512a\u308c\u3066\u304a\u308a\u3001\u9ad8\u3044\u6027\u80fd\u3068\u30b3\u30b9\u30c8\u52b9\u7387\u3067\u3001\u5efa\u8a2d\u30fb\u88fd\u9020\u5206\u91ce\u306e\u3055\u307e\u3056\u307e\u306a\u30cb\u30fc\u30ba\u306b\u7c21\u5358\u306b\u5bfe\u5fdc\u3067\u304d\u307e\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u9ad8\u3044\u5f37\u5ea6\u3068\u512a\u308c\u305f\u5b89\u5b9a\u6027: S250GD \u306f\u5c11\u306a\u304f\u3068\u3082 250 MPa \u306e\u964d\u4f0f\u5f37\u5ea6\u3092\u4fdd\u8a3c\u3057\u3001\u9ad8\u8ca0\u8377\u4e0b\u3067\u3082\u69cb\u9020\u7684\u5b89\u5b9a\u6027\u3092\u7dad\u6301\u3067\u304d\u307e\u3059\u3002\u4e00\u65b9\u3001\u591a\u304f\u306e\u985e\u4f3c\u88fd\u54c1\u306f\u5f37\u5ea6\u304c\u82e5\u5e72\u4e0d\u8db3\u3057\u3066\u3044\u307e\u3059\u3002<\/li><\/ul><ul class=\"wp-block-list\"><li>\u512a\u308c\u305f\u5ef6\u6027\u304c\u3042\u308a\u3001\u6210\u5f62\u306b\u9069\u3057\u3066\u3044\u307e\u3059\uff1aS250GD\u306f\u3001\u5e02\u8ca9\u306e\u4e00\u822c\u7684\u306a\u92fc\u3088\u308a\u3082\u7834\u65ad\u5f8c\u306e\u4f38\u3073\u304c\u9ad8\u304f\u3001\u6210\u5f62\u30d7\u30ed\u30bb\u30b9\u4e2d\u306b\u5272\u308c\u306b\u304f\u3044\u305f\u3081\u3001\u8907\u96d1\u306a\u52a0\u5de5\u306b\u975e\u5e38\u306b\u9069\u3057\u3066\u3044\u307e\u3059\u3002<\/li><\/ul><ul class=\"wp-block-list\"><li>\u512a\u308c\u305f\u8010\u8150\u98df\u6027: \u5f53\u793e\u306f\u4e9c\u925b\u30e1\u30c3\u30ad\u5de5\u7a0b\u3092\u6700\u9069\u5316\u3057\u3001\u6e7f\u6c17\u306e\u591a\u3044\u74b0\u5883\u3084\u6c5a\u67d3\u5ea6\u306e\u9ad8\u3044\u74b0\u5883\u3067\u3082\u9577\u671f\u9593\u92fc\u6750\u3092\u4f7f\u7528\u3067\u304d\u308b\u3088\u3046\u306b\u3059\u308b\u3053\u3068\u3067\u8150\u98df\u640d\u5931\u3092\u6e1b\u3089\u3057\u3066\u3044\u307e\u3059\u3002\u4e00\u65b9\u3001\u4ed6\u306e\u88fd\u54c1\u306f\u3053\u3046\u3057\u305f\u74b0\u5883\u3067\u306e\u8010\u7528\u5e74\u6570\u304c\u6bd4\u8f03\u7684\u77ed\u304f\u306a\u308a\u307e\u3059\u3002<\/li><\/ul><ul class=\"wp-block-list\"><li>\u512a\u308c\u305f\u6eb6\u63a5\u6027\u3068\u3088\u308a\u4fbf\u5229\u306a\u65bd\u5de5\u6027\uff1a\u4e88\u71b1\u306a\u3057\u3067\u7c21\u5358\u306b\u6eb6\u63a5\u3067\u304d\u308b\u305f\u3081\u3001\u65bd\u5de5\u6642\u9593\u3068\u30b3\u30b9\u30c8\u3092\u7bc0\u7d04\u3067\u304d\u307e\u3059\u304c\u3001\u4ed6\u306e\u6750\u6599\u3067\u306f\u901a\u5e38\u3001\u3088\u308a\u591a\u304f\u306e\u5de5\u7a0b\u304c\u5fc5\u8981\u306b\u306a\u308a\u307e\u3059\u3002<\/li><\/ul><ul class=\"wp-block-list\"><li>\u74b0\u5883\u7684\u306b\u6301\u7d9a\u53ef\u80fd: S250GD \u306f\u30ea\u30b5\u30a4\u30af\u30eb\u7387\u304c\u9ad8\u304f\u3001\u30b0\u30ea\u30fc\u30f3\u88fd\u9020\u57fa\u6e96\u3092\u6e80\u305f\u3057\u3066\u3044\u308b\u305f\u3081\u3001\u74b0\u5883\u306b\u512a\u3057\u3044\u30d7\u30ed\u30b8\u30a7\u30af\u30c8\u306b\u6700\u9069\u3067\u3059\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">S250GD \u306f\u3001\u30b3\u30b9\u30c8\u3068\u6027\u80fd\u306e\u9762\u3067\u4ed6\u306e\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u30b0\u30ec\u30fc\u30c9\u3068\u6bd4\u3079\u3066\u3069\u3046\u3067\u3059\u304b?<\/h3><p class=\"wp-block-paragraph\">S250GD\u306f\u3001\u4e0a\u4f4d\u30b0\u30ec\u30fc\u30c9\u306eS250GD\u3068\u6bd4\u8f03\u3057\u3066\u4fa1\u683c\u7af6\u4e89\u529b\u304c\u3042\u308a\u307e\u3059\u3002 <a href=\"https:\/\/steelprogroup.com\/ja\/galvanized-steel\/grades\/s280gd\/\">\u578b\u756a<\/a>\u4e00\u822c\u7684\u306a\u69cb\u9020\u7528\u9014\u306b\u30d0\u30e9\u30f3\u30b9\u306e\u3068\u308c\u305f\u6027\u80fd\u3092\u63d0\u4f9b\u3057\u3001 <strong>\u8cbb\u7528\u5bfe\u52b9\u679c\u304c\u9ad8\u3044<\/strong> \u57fa\u672c\u7684\u306a\u5f37\u5ea6\u3068\u8010\u4e45\u6027\u3092\u72a0\u7272\u306b\u3059\u308b\u3053\u3068\u306a\u304f\u9078\u629e\u3067\u304d\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">S250GD\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u677f\u8868\u9762\u51e6\u7406<\/h2><p class=\"wp-block-paragraph\">S250GD \u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306f\u3001\u3055\u307e\u3056\u307e\u306a\u65b9\u6cd5\u3067\u51e6\u7406\u3057\u3066\u8010\u8150\u98df\u6027\u3068\u5916\u89b3\u3092\u5411\u4e0a\u3055\u305b\u308b\u3053\u3068\u304c\u3067\u304d\u307e\u3059\u3002SteelPRO Group \u3067\u306f\u3001\u3055\u307e\u3056\u307e\u306a\u8868\u9762\u51e6\u7406\u30aa\u30d7\u30b7\u30e7\u30f3\u3092\u63d0\u4f9b\u3057\u3066\u3044\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\"><strong>S250GD\u92fc<\/strong> <strong>\u8868\u9762\u54c1\u8cea\u7b49\u7d1a<\/strong><\/h3><p class=\"wp-block-paragraph\">\u7528\u9014\u3068\u8868\u9762\u8981\u4ef6\u306b\u5fdc\u3058\u3066\u3001S250GD \u306b\u306f 4 \u3064\u306e\u8868\u9762\u54c1\u8cea\u30b0\u30ec\u30fc\u30c9\u304c\u3042\u308a\u307e\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>FA \u30b0\u30ec\u30fc\u30c9: \u5185\u90e8\u69cb\u9020\u3084\u96a0\u308c\u305f\u90e8\u5206\u306a\u3069\u3001\u5916\u89b3\u304c\u8981\u6c42\u3055\u308c\u306a\u3044\u7528\u9014\u3067\u3042\u308c\u3070\u3001FA \u30b0\u30ec\u30fc\u30c9\u3067\u5341\u5206\u5bfe\u5fdc\u3067\u304d\u307e\u3059\u3002<\/li>\n\n<li>FB \u30b0\u30ec\u30fc\u30c9: \u6a5f\u68b0\u5185\u90e8\u90e8\u54c1\u306a\u3069\u3001\u4e2d\u7a0b\u5ea6\u306e\u8868\u9762\u51e6\u7406\u304c\u6c42\u3081\u3089\u308c\u308b\u7528\u9014\u306b\u9069\u3057\u3066\u3044\u307e\u3059\u3002<\/li>\n\n<li>FC \u30b0\u30ec\u30fc\u30c9: \u5916\u88c5\u90e8\u54c1\u306a\u3069\u3001\u92fc\u6750\u3092\u76f4\u63a5\u9732\u51fa\u3055\u305b\u308b\u5834\u5408\u306f\u3001\u8868\u9762\u304c\u3088\u308a\u304d\u308c\u3044\u3067\u6ed1\u3089\u304b\u306a FC \u30b0\u30ec\u30fc\u30c9\u304c\u63a8\u5968\u3055\u308c\u307e\u3059\u3002<\/li>\n\n<li>FD\u30b0\u30ec\u30fc\u30c9\uff1a\u8868\u9762\u6b20\u9665\u304c\u307b\u3068\u3093\u3069\u306a\u304f\u3001\u8996\u899a\u52b9\u679c\u306b\u512a\u308c\u3001\u81ea\u52d5\u8eca\u30d1\u30cd\u30eb\u3084\u88c5\u98fe\u9762\u306a\u3069\u306e\u9ad8\u54c1\u8cea\u5916\u89b3\u90e8\u54c1\u306b\u6700\u9069\u3067\u3059\u3002<\/li><\/ul><h3 class=\"wp-block-heading\"><strong>S250GD\u92fc<\/strong> <strong>\u8868\u9762\u51e6\u7406\u306e\u7a2e\u985e<\/strong><\/h3><p class=\"wp-block-paragraph\">\u5f53\u793e\u3067\u306f\u3001\u3055\u307e\u3056\u307e\u306a\u4fdd\u8b77\u304a\u3088\u3073\u7f8e\u89b3\u306e\u30cb\u30fc\u30ba\u3092\u6e80\u305f\u3059\u305f\u3081\u306b\u3001\u3055\u307e\u3056\u307e\u306a\u8868\u9762\u51e6\u7406\u3092\u63d0\u4f9b\u3057\u3066\u3044\u307e\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u30af\u30ed\u30e1\u30fc\u30c8\u51e6\u7406: \u92fc\u6750\u3092\u6e7f\u6c17\u306e\u591a\u3044\u74b0\u5883\u3084\u8150\u98df\u6027\u306e\u74b0\u5883\u306b\u9577\u6642\u9593\u3055\u3089\u3059\u5fc5\u8981\u304c\u3042\u308b\u5834\u5408\u306f\u3001\u30af\u30ed\u30e1\u30fc\u30c8\u51e6\u7406\u306b\u3088\u3063\u3066\u8010\u8150\u98df\u6027\u304c\u5927\u5e45\u306b\u5411\u4e0a\u3057\u307e\u3059\u3002<\/li>\n\n<li>\u30ea\u30f3\u9178\u51e6\u7406: \u5857\u88c5\u304c\u5fc5\u8981\u306a\u30d7\u30ed\u30b8\u30a7\u30af\u30c8\u306b\u9069\u3057\u3066\u304a\u308a\u3001\u5857\u6599\u306e\u5bc6\u7740\u6027\u3092\u9ad8\u3081\u3001\u5857\u88c5\u9762\u306e\u5f37\u5ea6\u3092\u9ad8\u3081\u307e\u3059\u3002<\/li>\n\n<li>\u7d66\u6cb9: \u88fd\u54c1\u306e\u4fdd\u7ba1\u304a\u3088\u3073\u8f38\u9001\u4e2d\u306b\u4e00\u6642\u7684\u306a\u9632\u9306\u52b9\u679c\u3092\u767a\u63ee\u3057\u3001\u77ed\u671f\u9593\u306e\u4fdd\u8b77\u304c\u5fc5\u8981\u306a\u92fc\u6750\u306b\u9069\u3057\u3066\u3044\u307e\u3059\u3002<\/li>\n\n<li>\u5857\u88c5: \u4fdd\u8b77\u3068\u7f8e\u89b3\u306e\u4e21\u65b9\u304c\u5411\u4e0a\u3057\u307e\u3059\u3002\u30d7\u30ed\u30b8\u30a7\u30af\u30c8\u306e\u5916\u89b3\u306b\u88c5\u98fe\u7684\u306a\u8981\u4ef6\u304c\u3042\u308b\u5834\u5408\u306f\u3001\u5857\u88c5\u3092\u9078\u629e\u3067\u304d\u307e\u3059\u3002<\/li><\/ul><h3 class=\"wp-block-heading\"><strong>S250GD \u4e9c\u925b\u30e1\u30c3\u30ad\u92fc<\/strong> <strong>\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u306e\u7a2e\u985e<\/strong><\/h3><p class=\"wp-block-paragraph\">\u3055\u307e\u3056\u307e\u306a\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u30bf\u30a4\u30d7\u304c\u3055\u307e\u3056\u307e\u306a\u7528\u9014\u30b7\u30ca\u30ea\u30aa\u306b\u5bfe\u5fdc\u3057\u307e\u3059\u3002\u30cb\u30fc\u30ba\u306b\u5fdc\u3058\u3066\u9069\u5207\u306a\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u3092\u9078\u629e\u3067\u304d\u307e\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>+Z\uff08\u4e9c\u925b\uff09\uff1a\u4e00\u822c\u7684\u306a\u74b0\u5883\u3067\u306e\u4fdd\u8b77\u30cb\u30fc\u30ba\u306b\u9069\u3057\u3066\u304a\u308a\u3001\u6700\u3082\u57fa\u672c\u7684\u306a\u9078\u629e\u80a2\u3067\u3059\u3002<\/li>\n\n<li>+ZF\uff08\u4e9c\u925b\u9244\u5408\u91d1\uff09\uff1a\u30d7\u30ed\u30b8\u30a7\u30af\u30c8\u3067\u6eb6\u63a5\u65bd\u5de5\u304c\u5fc5\u8981\u306a\u5834\u5408\u306f\u3001\u6eb6\u63a5\u6027\u80fd\u304c\u512a\u308c\u3066\u3044\u308b+ZF\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u3092\u9078\u629e\u3059\u308b\u3053\u3068\u3092\u304a\u52e7\u3081\u3057\u307e\u3059\u3002<\/li>\n\n<li>+ZA\uff08\u4e9c\u925b\u30a2\u30eb\u30df\u30cb\u30a6\u30e0\uff09\uff1a\u512a\u308c\u305f\u9632\u9306\u52b9\u679c\u304c\u3042\u308a\u3001\u5c4b\u5916\u306e\u5efa\u7269\u306a\u3069\u904e\u9177\u306a\u74b0\u5883\u306b\u3055\u3089\u3055\u308c\u308b\u69cb\u9020\u7269\u306b\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/li>\n\n<li>+ZM (\u4e9c\u925b\u30de\u30b0\u30cd\u30b7\u30a6\u30e0): \u8907\u96d1\u306a\u6210\u5f62\u3092\u5fc5\u8981\u3068\u3059\u308b\u7528\u9014\u3067\u306f\u3001+ZM \u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u306b\u3088\u308a\u6210\u5f62\u6027\u304c\u5411\u4e0a\u3057\u307e\u3059\u3002<\/li>\n\n<li>+AZ (\u30a2\u30eb\u30df\u30cb\u30a6\u30e0-\u4e9c\u925b): \u8010\u8150\u98df\u6027\u3068\u8010\u9178\u5316\u6027\u306e\u4e21\u65b9\u3092\u5099\u3048\u3001\u5c4b\u6839\u306a\u3069\u306e\u5efa\u7bc9\u7528\u9014\u306b\u6700\u9069\u3067\u3059\u3002<\/li>\n\n<li>+AS\uff08\u30a2\u30eb\u30df\u30cb\u30a6\u30e0\u30b7\u30ea\u30b3\u30f3\uff09\uff1a\u8010\u71b1\u6027\u306b\u512a\u308c\u3001\u5de5\u696d\u7528\u52a0\u71b1\u6a5f\u5668\u306e\u90e8\u54c1\u306a\u3069\u3001\u9ad8\u6e29\u74b0\u5883\u3067\u306e\u4f7f\u7528\u306b\u9069\u3057\u3066\u3044\u307e\u3059\u3002<\/li><\/ul><p class=\"wp-block-paragraph\"><strong>\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u7bc4\u56f2<\/strong><strong> <\/strong><strong>S250GD\u92fc\u306e\u5f62\u72b6<\/strong><\/p><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u30d5\u30a9\u30fc\u30e0<\/strong><\/td><td><strong>\u9069\u7528\u53ef\u80fd\u306a\u8868\u9762\u69cb\u9020<\/strong><\/td><td><strong>\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u306e\u91cd\u91cf\u7bc4\u56f2 g\/m\u00b2 (A\/B)<\/strong><\/td><\/tr><tr><td>\u5747\u4e00\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\uff08\u4e9c\u925b\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\\Zn-Fe\u5408\u91d1\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\uff09<\/td><td>Z\u3001G\u3001GX\u3001N\u3001R\u3001S\u3001O<\/td><td>40\/40~225\/225<\/td><\/tr><tr><td>\u30c7\u30a3\u30d5\u30a1\u30ec\u30f3\u30b7\u30e3\u30eb\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0b<\/td><td>N\u3001R\u3001S\u3001O<\/td><td>30\u301c150\uff08\u7247\u5074\uff09<\/td><\/tr><\/tbody><\/table><\/figure><p class=\"wp-block-paragraph\">S250GD \u92fc\u306e\u4e9c\u925b\u30e1\u30c3\u30ad\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u306f\u3001\u6e7f\u6c17\u3084\u74b0\u5883\u8981\u56e0\u306b\u5bfe\u3059\u308b\u4fdd\u8b77\u30b7\u30fc\u30eb\u30c9\u3092\u5f62\u6210\u3059\u308b\u3053\u3068\u3067\u3001\u8010\u8150\u98df\u6027\u3092\u5927\u5e45\u306b\u5411\u4e0a\u3055\u305b\u307e\u3059\u3002\u3053\u308c\u306b\u3088\u308a\u3001\u3055\u307e\u3056\u307e\u306a\u7528\u9014\u3067\u8010\u4e45\u6027\u3068\u4fe1\u983c\u6027\u304c\u78ba\u4fdd\u3055\u308c\u307e\u3059\u3002\u5f53\u793e\u306f\u3001S250GD \u306e\u30d1\u30d5\u30a9\u30fc\u30de\u30f3\u30b9\u3092\u3055\u3089\u306b\u6700\u9069\u5316\u3059\u308b\u9ad8\u5ea6\u306a\u8868\u9762\u51e6\u7406\u3068\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u3092\u63a1\u7528\u3057\u3066\u3044\u308b\u3053\u3068\u306b\u8a87\u308a\u3092\u6301\u3063\u3066\u304a\u308a\u3001\u3055\u307e\u3056\u307e\u306a\u696d\u754c\u306e\u8981\u6c42\u306e\u53b3\u3057\u3044\u30d7\u30ed\u30b8\u30a7\u30af\u30c8\u3067\u597d\u307e\u308c\u308b\u9078\u629e\u80a2\u3068\u306a\u3063\u3066\u3044\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">S250GD\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u677f\u52a0\u5de5<\/h2><p class=\"wp-block-paragraph\">S250GD\u306e\u52a0\u5de5\u65b9\u6cd5\u306b\u3064\u3044\u3066\u3054\u4e0d\u660e\u306a\u70b9\u304c\u3054\u3056\u3044\u307e\u3057\u305f\u3089\u3001\u5f53\u793e\u3067\u306f\u304a\u5ba2\u69d8\u306e\u30cb\u30fc\u30ba\u306b\u5408\u308f\u305b\u3066\u92fc\u6750\u306e\u6027\u80fd\u3068\u5916\u89b3\u3092\u30ab\u30b9\u30bf\u30de\u30a4\u30ba\u3059\u308b\u305f\u3081\u306e\u3055\u307e\u3056\u307e\u306a\u52a0\u5de5\u30aa\u30d7\u30b7\u30e7\u30f3\u3092\u3054\u7528\u610f\u3057\u3066\u304a\u308a\u307e\u3059\u3002\u5f53\u793e\u306e\u88fd\u54c1\u52a0\u5de5\u6280\u8853\u306b\u3055\u3089\u306b\u81ea\u4fe1\u3092\u6301\u3063\u3066\u3044\u305f\u3060\u3051\u308b\u3088\u3046\u3001\u524d\u51e6\u7406\u304b\u3089\u5f8c\u51e6\u7406\u307e\u3067\u306e\u30d7\u30ed\u30bb\u30b9\u30d5\u30ed\u30fc\u3092\u7c21\u5358\u306b\u3054\u7d39\u4ecb\u3057\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">1. \u524d\u51e6\u7406<\/h3><ul class=\"wp-block-list\"><li>\u9178\u6d17\uff1a60\uff5e80\u2103\u306e\u5869\u9178\u3067\u92fc\u6750\u8868\u9762\u306e\u9306\u3092\u9664\u53bb\u3057\u3001\u305d\u306e\u5f8c\u306e\u52a0\u5de5\u306b\u5099\u3048\u307e\u3059\u3002<\/li>\n\n<li>\u4e0d\u52d5\u614b\u5316: \u92fc\u306e\u8010\u8150\u98df\u6027\u3092\u9ad8\u3081\u3001\u6e7f\u6c17\u3084\u8150\u98df\u6027\u306e\u9ad8\u3044\u74b0\u5883\u3067\u306e\u4f7f\u7528\u306b\u9069\u3057\u3066\u3044\u307e\u3059\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">2. \u51e6\u7406\u30d7\u30ed\u30bb\u30b9<\/h3><ul class=\"wp-block-list\"><li>\u305b\u3093\u65ad: \u51b7\u9593\u5207\u65ad\u306b\u3088\u308a\u92fc\u3092\u5fc5\u8981\u306a\u5f62\u72b6\u306b\u5207\u65ad\u3057\u307e\u3059\u3002<\/li>\n\n<li>\u30b9\u30bf\u30f3\u30d4\u30f3\u30b0: S250GD \u306f\u512a\u308c\u305f\u5ef6\u6027\u3092\u5099\u3048\u3066\u3044\u308b\u305f\u3081\u3001\u5ba4\u6e29\u3067\u6210\u5f62\u3059\u308b\u3053\u3068\u304c\u3067\u304d\u3001\u3055\u307e\u3056\u307e\u306a\u6210\u5f62\u30cb\u30fc\u30ba\u306b\u975e\u5e38\u306b\u9069\u3057\u3066\u3044\u307e\u3059\u3002<\/li>\n\n<li>\u6eb6\u63a5\uff1aS250GD\u306f\u30b9\u30dd\u30c3\u30c8\u6eb6\u63a5\u3068\u30a2\u30fc\u30af\u6eb6\u63a5\u3092\u30b5\u30dd\u30fc\u30c8\u3057\u3001\u4e88\u71b1\u304c\u4e0d\u8981\u306a\u306e\u3067\u65bd\u5de5\u306b\u4fbf\u5229\u3067\u30b3\u30b9\u30c8\u3082\u7bc0\u7d04\u3067\u304d\u307e\u3059\u3002<\/li>\n\n<li>\u66f2\u3052\uff1a\u51b7\u9593\u66f2\u3052\u304c\u53ef\u80fd\u3067\u3001\u66f2\u3052\u534a\u5f84\u306f\u92fc\u677f\u306e\u539a\u3055\u3068\u4e00\u81f4\u3057\u3066\u3044\u308b\u305f\u3081\u3001\u52a0\u5de5\u4e2d\u306b\u5272\u308c\u308b\u3053\u3068\u306f\u3042\u308a\u307e\u305b\u3093\u3002<\/li>\n\n<li>\u30b9\u30c8\u30ec\u30c3\u30c1\u6210\u5f62: \u7834\u640d\u3059\u308b\u3053\u3068\u306a\u304f\u8907\u96d1\u306a\u5f62\u72b6\u306b\u5f15\u304d\u4f38\u3070\u3059\u3053\u3068\u304c\u3067\u304d\u3001\u7279\u6b8a\u306a\u6210\u5f62\u8981\u4ef6\u306e\u3042\u308b\u30d7\u30ed\u30b8\u30a7\u30af\u30c8\u306b\u9069\u3057\u3066\u3044\u307e\u3059\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">3. \u5f8c\u51e6\u7406<\/h3><ul class=\"wp-block-list\"><li>\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\/\u5857\u88c5: \u8010\u8150\u98df\u6027\u304c\u3055\u3089\u306b\u5411\u4e0a\u3057\u3001\u5857\u6599\u306e\u5bc6\u7740\u6027\u304c\u5411\u4e0a\u3057\u3001\u7f8e\u89b3\u3068\u4fdd\u8b77\u304c\u6c42\u3081\u3089\u308c\u308b\u7528\u9014\u306b\u9069\u3057\u3066\u3044\u307e\u3059\u3002<\/li>\n\n<li>\u9632\u9306\u30aa\u30a4\u30eb\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\uff1a\u4fdd\u7ba1\u4e2d\u304a\u3088\u3073\u8f38\u9001\u4e2d\u306e\u77ed\u671f\u7684\u306a\u9632\u9306\u52b9\u679c\u3092\u767a\u63ee\u3057\u307e\u3059\u3002<\/li>\n\n<li>\u6307\u7d0b\u9632\u6b62\u51e6\u7406: \u8868\u9762\u306e\u6307\u7d0b\u3084\u6c5a\u308c\u3092\u8efd\u6e1b\u3057\u3001\u5916\u89b3\u8981\u4ef6\u304c\u9ad8\u3044\u90e8\u54c1\u306b\u9069\u3057\u3066\u3044\u307e\u3059\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">4. \u71b1\u51e6\u7406\uff08\u30aa\u30d7\u30b7\u30e7\u30f3\uff09<\/h3><ul class=\"wp-block-list\"><li>\u5fdc\u529b\u7de9\u548c: \u3088\u308a\u9ad8\u3044\u976d\u6027\u304c\u5fc5\u8981\u306a\u5834\u5408\u3001\u92fc\u306e\u8106\u3055\u3068\u5185\u90e8\u5fdc\u529b\u3092 500 \uff5e 600\u2103 \u3067\u9664\u53bb\u3067\u304d\u307e\u3059\u304c\u3001\u3053\u308c\u306f\u901a\u5e38\u3001\u7279\u5225\u306a\u5fc5\u8981\u304c\u3042\u308b\u5834\u5408\u306b\u306e\u307f\u4f7f\u7528\u3055\u308c\u307e\u3059\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">\u4e9c\u925b\u30e1\u30c3\u30ad\u51e6\u7406\u306b\u3088\u3063\u3066 S250GD \u306e\u30d1\u30d5\u30a9\u30fc\u30de\u30f3\u30b9\u306f\u3069\u306e\u3088\u3046\u306b\u5411\u4e0a\u3059\u308b\u306e\u3067\u3057\u3087\u3046\u304b?<\/h3><p class=\"wp-block-paragraph\">\u5f53\u793e\u306e S250GD \u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306f\u3001\u9ad8\u5ea6\u306a\u4e9c\u925b\u30e1\u30c3\u30ad\u51e6\u7406\u306b\u3088\u308a\u5747\u4e00\u3067\u5bc6\u7740\u6027\u306e\u9ad8\u3044\u4e9c\u925b\u5c64\u3092\u5f62\u6210\u3057\u3001\u8010\u8150\u98df\u6027\u3092\u52b9\u679c\u7684\u306b\u5411\u4e0a\u3055\u305b\u307e\u3059\u3002\u8868\u9762\u306b\u50b7\u304c\u4ed8\u3044\u3066\u3082\u3001\u4e9c\u925b\u5c64\u304c\u512a\u308c\u305f\u9670\u6975\u4fdd\u8b77\u3092\u63d0\u4f9b\u3057\u3001\u92fc\u306e\u3055\u3089\u306a\u308b\u8150\u98df\u3092\u9632\u304e\u3001\u904e\u9177\u306a\u74b0\u5883\u3067\u3082\u8010\u4e45\u6027\u3068\u4fe1\u983c\u6027\u3092\u9ad8\u3081\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">S250GD\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u88fd\u54c1<\/h2><p class=\"wp-block-paragraph\">\u5f53\u793e\u306e S250GD \u306f\u3001\u5efa\u8a2d\u3084\u88fd\u9020\u696d\u306b\u6700\u9069\u306a\u9ad8\u6027\u80fd\u92fc\u3067\u3042\u308a\u3001\u30d7\u30ec\u30fc\u30c8\u3001\u30b3\u30a4\u30eb\u3001\u30c1\u30e5\u30fc\u30d6\u306e\u5e45\u5e83\u3044\u30e9\u30a4\u30f3\u30ca\u30c3\u30d7\u306b\u3088\u308a\u3001\u3055\u307e\u3056\u307e\u306a\u7528\u9014\u306e\u30cb\u30fc\u30ba\u306b\u5bfe\u5fdc\u3067\u304d\u307e\u3059\u3002<\/p><h3 class=\"wp-block-heading\">S250GD\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u88fd\u54c1\u306e\u5bf8\u6cd5<\/h3><figure class=\"wp-block-table\"><table class=\"has-fixed-layout\"><tbody><tr><td>\u88fd\u54c1\u30bf\u30a4\u30d7<\/td><td>\u539a\u3055\uff08mm \/ \u30a4\u30f3\u30c1\uff09<\/td><td>\u5e45\/\u5916\u5f84\uff08mm\/\u30a4\u30f3\u30c1\uff09<\/td><td>\u9577\u3055\uff08mm \/ \u30d5\u30a3\u30fc\u30c8\uff09<\/td><\/tr><tr><td><a href=\"https:\/\/steelprogroup.com\/ja\/galvanized-steel\/sheet\/s250gd\/\"><strong>S250GD\u30b7\u30fc\u30c8<\/strong><\/a><\/td><td>0.30\uff5e3.00 mm\uff080.012\uff5e0.118\u30a4\u30f3\u30c1\uff09<\/td><td>800\uff5e1830 mm\uff0831.5\uff5e72\u30a4\u30f3\u30c1\uff09<\/td><td>\u6700\u59276,000 mm\uff08\u6700\u592719.69\u30d5\u30a3\u30fc\u30c8\uff09<\/td><\/tr><tr><td><a href=\"https:\/\/steelprogroup.com\/ja\/galvanized-steel\/coil\/s250gd\/\"><strong>S250GD\u30b3\u30a4\u30eb<\/strong><\/a><\/td><td>0.30\uff5e3.00 mm\uff080.012\uff5e0.118\u30a4\u30f3\u30c1\uff09<\/td><td>800\uff5e1830 mm\uff0831.5\uff5e72\u30a4\u30f3\u30c1\uff09<\/td><td>\u9577\u3055\u306e\u30ab\u30b9\u30bf\u30de\u30a4\u30ba\u53ef\u80fd<\/td><\/tr><tr><td><a href=\"https:\/\/steelprogroup.com\/ja\/galvanized-steel\/pipe\/s250gd\/\"><strong>S250GD\u30d1\u30a4\u30d7<\/strong><\/a><\/td><td>1.5\uff5e12.0 mm\uff080.059\uff5e0.472\u30a4\u30f3\u30c1\uff09<\/td><td>21.3\uff5e219.1 mm\uff080.84\uff5e8.63\u30a4\u30f3\u30c1\uff09<\/td><td>\u6700\u592712,000 mm\uff08\u6700\u592739.37\u30d5\u30a3\u30fc\u30c8\uff09<\/td><\/tr><\/tbody><\/table><\/figure><h3 class=\"wp-block-heading\">S250GD\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u677f<\/h3><p class=\"wp-block-paragraph\">S250GD\u4e9c\u925b\u3081\u3063\u304d\u92fc\u677f\u306f\u3001\u5efa\u7bc9\u69cb\u9020\u7269\u3001\u5c4b\u6839\u6750\u3001\u58c1\u88c5\u6750\u3001\u7523\u696d\u7528\u9014\u306a\u3069\u3001\u5e45\u5e83\u3044\u7528\u9014\u306b\u4f7f\u7528\u3055\u308c\u3066\u3044\u307e\u3059\u3002\u5747\u4e00\u306a\u4e9c\u925b\u3081\u3063\u304d\u3068\u512a\u308c\u305f\u8010\u98df\u6027\u306b\u3088\u308a\u3001\u8010\u4e45\u6027\u3068\u7f8e\u89b3\u3092\u517c\u306d\u5099\u3048\u3066\u3044\u307e\u3059\u3002\u92fc\u677f\u306f\u305d\u306e\u307e\u307e\u4f7f\u7528\u3059\u308b\u3053\u3068\u3082\u3001\u5857\u88c5\u3084\u6210\u5f62\u52a0\u5de5\u3092\u65bd\u3059\u3053\u3068\u3082\u53ef\u80fd\u3067\u3059\u3002<\/p><h3 class=\"wp-block-heading\">S250GD \u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u30b3\u30a4\u30eb<\/h3><p class=\"wp-block-paragraph\">S250GD\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u677f\u30b3\u30a4\u30eb\u306f\u3001\u5927\u898f\u6a21\u52a0\u5de5\u3084\u69d8\u3005\u306a\u6210\u5f62\u7528\u9014\u5411\u3051\u306b\u8a2d\u8a08\u3055\u308c\u3066\u3044\u307e\u3059\u3002\u5207\u65ad\u3084\u6eb6\u63a5\u304c\u5bb9\u6613\u306a\u305f\u3081\u3001\u81ea\u52d5\u8eca\u90e8\u54c1\u3001\u5bb6\u96fb\u88fd\u54c1\u3001\u5efa\u7bc9\u8cc7\u6750\u306a\u3069\u306b\u6700\u9069\u3067\u3059\u3002<\/p><p class=\"wp-block-paragraph\">\u5f53\u793e\u3067\u306f 2 \u3064\u306e\u4e9c\u925b\u30e1\u30c3\u30ad \u30aa\u30d7\u30b7\u30e7\u30f3\u3092\u3054\u7528\u610f\u3057\u3066\u3044\u307e\u3059\u3002<\/p><ul class=\"wp-block-list\"><li><strong>\u6eb6\u878d\u4e9c\u925b\u3081\u3063\u304d<\/strong> \u2013 \u512a\u308c\u305f\u8010\u8150\u98df\u6027\u3092\u63d0\u4f9b\u3057\u307e\u3059\u3002<\/li>\n\n<li><strong>\u96fb\u6c17\u4e9c\u925b\u30e1\u30c3\u30ad<\/strong> \u2013 \u3088\u308a\u6ed1\u3089\u304b\u3067\u6d17\u7df4\u3055\u308c\u305f\u5916\u89b3\u3092\u5b9f\u73fe\u3057\u307e\u3059\u3002<\/li><\/ul><h3 class=\"wp-block-heading\">S250GD \u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u7ba1<\/h3><p class=\"wp-block-paragraph\">S250GD\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u7ba1\u306f\u3001\u69cb\u9020\u652f\u6301\u3001\u914d\u7ba1\u30b7\u30b9\u30c6\u30e0\u3001\u63db\u6c17\u8a2d\u5099\u306b\u6700\u9069\u3067\u3059\u3002\u7279\u5fb4\uff1a<\/p><ul class=\"wp-block-list\"><li>\u512a\u308c\u305f\u8010\u8150\u98df\u6027\u3068\u8010\u4e45\u6027\u306b\u512a\u308c\u3001\u904e\u9177\u306a\u74b0\u5883\u3067\u3082\u9577\u671f\u306b\u308f\u305f\u308b\u6027\u80fd\u3092\u4fdd\u8a3c\u3057\u307e\u3059\u3002<\/li>\n\n<li>\u8868\u9762\u304c\u6ed1\u3089\u304b\u3067\u6383\u9664\u304c\u7c21\u5358\u306a\u306e\u3067\u3001\u5efa\u8a2d\u3084\u5de5\u696d\u7528\u9014\u306b\u9069\u3057\u3066\u3044\u307e\u3059\u3002<\/li><\/ul><p class=\"wp-block-paragraph\">\u306b\u3064\u3044\u3066 <strong>\u30ab\u30b9\u30bf\u30e0\u30b5\u30a4\u30ba\u3068\u4ed5\u69d8<\/strong>\u304a\u6c17\u8efd\u306b\u304a\u554f\u3044\u5408\u308f\u305b\u304f\u3060\u3055\u3044\u3002\u304a\u5ba2\u69d8\u306e\u30cb\u30fc\u30ba\u306b\u6700\u9069\u306a\u30bd\u30ea\u30e5\u30fc\u30b7\u30e7\u30f3\u3092\u3054\u63d0\u6848\u3044\u305f\u3057\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">S250GD \u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306e\u7528\u9014<\/h2><p class=\"wp-block-paragraph\">\u5f53\u793e\u306e S250GD \u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u88fd\u54c1\u306f\u3001\u305d\u306e\u5f37\u5ea6\u3001\u8010\u8150\u98df\u6027\u3001\u512a\u308c\u305f\u52a0\u5de5\u6027\u306b\u3088\u308a\u3001\u4e3b\u306b\u4ee5\u4e0b\u306e\u3088\u3046\u306a\u5e45\u5e83\u3044\u7528\u9014\u306b\u4f7f\u7528\u3055\u308c\u3066\u3044\u307e\u3059\u3002<\/p><ul class=\"wp-block-list\"><li>\u5efa\u8a2d: \u5efa\u7269\u306e\u8010\u4e45\u6027\u3068\u7f8e\u3057\u3055\u3092\u78ba\u4fdd\u3059\u308b\u305f\u3081\u306e\u5c4b\u6839\u3001\u58c1\u30d1\u30cd\u30eb\u3001\u30ac\u30ec\u30fc\u30b8\u30c9\u30a2\u306a\u3069\u306e\u69cb\u9020\u3002<\/li>\n\n<li>\u81ea\u52d5\u8eca\u88fd\u9020\uff1a\u30dc\u30c7\u30a3\u30d1\u30cd\u30eb\u3001\u30b7\u30e3\u30fc\u30b7\u3001\u305d\u306e\u4ed6\u306e\u90e8\u54c1\u3001\u8150\u98df\u304a\u3088\u3073\u885d\u6483\u4fdd\u8b77\u3092\u63d0\u4f9b\u3057\u307e\u3059\u3002<\/li>\n\n<li>\u5bb6\u96fb\u88fd\u54c1\uff1a\u51b7\u8535\u5eab\u3001\u6d17\u6fef\u6a5f\u306a\u3069\u306e\u30b7\u30a7\u30eb\u3001\u9306\u9632\u6b62\u3001\u8010\u7528\u5e74\u6570\u306e\u5ef6\u9577\u3002<\/li>\n\n<li>\u7523\u696d\u6a5f\u5668\uff1a\u63db\u6c17\u30c0\u30af\u30c8\u3001\u8caf\u8535\u30bf\u30f3\u30af\u306a\u3069\u3001\u9ad8\u6e7f\u5ea6\u307e\u305f\u306f\u8150\u98df\u6027\u74b0\u5883\u306b\u9069\u3057\u3066\u3044\u307e\u3059\u3002<\/li>\n\n<li>\u96fb\u6c17\u6a5f\u5668\u304a\u3088\u3073\u30cf\u30fc\u30c9\u30a6\u30a7\u30a2\uff1a\u63a5\u7d9a\u7bb1\u3001\u88c5\u98fe\u90e8\u54c1\u306a\u3069\u3001\u7f8e\u3057\u3044\u5916\u89b3\u3001\u8010\u8150\u98df\u6027\u3001\u8010\u4e45\u6027\u3002<\/li>\n\n<li>\u8fb2\u696d\u8a2d\u5099\uff1a\u6e29\u5ba4\u69cb\u9020\u7269\u3001\u8fb2\u696d\u6a5f\u68b0\u306a\u3069\u3001\u8010\u5019\u6027\u304c\u5f37\u304f\u3001\u5c4b\u5916\u3067\u306e\u4f7f\u7528\u306b\u9069\u3057\u3066\u3044\u307e\u3059\u3002<\/li><\/ul><h2 class=\"wp-block-heading\">S250GD \u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u30e1\u30fc\u30ab\u30fc<\/h2><p class=\"wp-block-paragraph\">SteelPRO \u30b0\u30eb\u30fc\u30d7\u306f\u3001\u3055\u307e\u3056\u307e\u306a\u7528\u9014\u306e\u30cb\u30fc\u30ba\u3092\u6e80\u305f\u3059\u305f\u3081\u306b\u3001\u30d7\u30ec\u30fc\u30c8\u3001\u30b3\u30a4\u30eb\u3001\u30c1\u30e5\u30fc\u30d6\u306a\u3069\u3001\u5e45\u5e83\u3044 S250GD \u88fd\u54c1\u3092\u63d0\u4f9b\u3057\u3066\u3044\u307e\u3059\u3002\u5f53\u793e\u306e S250GD \u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306f\u3001\u512a\u308c\u305f\u8010\u8150\u98df\u6027\u3068\u52a0\u5de5\u67d4\u8edf\u6027\u3092\u5099\u3048\u3066\u304a\u308a\u3001\u7279\u306b\u5efa\u7269\u69cb\u9020\u3001\u5c4b\u6839\u3001\u5916\u58c1\u88ab\u8986\u306a\u3069\u306e\u9ad8\u5f37\u5ea6\u3067\u8010\u4e45\u6027\u306e\u3042\u308b\u7528\u9014\u306b\u9069\u3057\u3066\u3044\u307e\u3059\u3002\u30b3\u30a4\u30eb\u306f\u5927\u898f\u6a21\u306a\u52a0\u5de5\u306b\u9069\u3057\u3066\u304a\u308a\u3001\u30c1\u30e5\u30fc\u30d6\u306f\u69cb\u9020\u30b5\u30dd\u30fc\u30c8\u3084\u914d\u7ba1\u30b7\u30b9\u30c6\u30e0\u306b\u9069\u3057\u3066\u3044\u307e\u3059\u3002\u3054\u8981\u671b\u3092\u304a\u77e5\u3089\u305b\u3044\u305f\u3060\u3051\u308c\u3070\u3001\u6700\u9069\u306a\u30bd\u30ea\u30e5\u30fc\u30b7\u30e7\u30f3\u3092\u3054\u63d0\u6848\u3044\u305f\u3057\u307e\u3059\u3002<\/p><p class=\"wp-block-paragraph\"><\/p>","protected":false},"excerpt":{"rendered":"<p>S250GD \u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u3092\u3054\u89a7\u304f\u3060\u3055\u3044\u3002\u8010\u4e45\u6027\u3068\u8010\u8150\u98df\u6027\u306b\u512a\u308c\u3001\u5efa\u8a2d\u3084\u81ea\u52d5\u8eca\u7528\u9014\u306b\u9069\u3057\u3066\u304a\u308a\u3001\u9577\u671f\u9593\u306b\u308f\u305f\u308b\u6027\u80fd\u3092\u4fdd\u8a3c\u3057\u307e\u3059\u3002<\/p>","protected":false},"author":1,"featured_media":21084,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"_eb_attr":"","rank_math_lock_modified_date":false,"site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"categories":[4307,4273],"tags":[],"class_list":["post-21083","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-grades-galvanized-steel","category-galvanized-steel"],"acf":[],"_links":{"self":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts\/21083","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/comments?post=21083"}],"version-history":[{"count":0,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts\/21083\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/media\/21084"}],"wp:attachment":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/media?parent=21083"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/categories?post=21083"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/tags?post=21083"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}