{"id":21579,"date":"2025-03-11T07:19:00","date_gmt":"2025-03-10T23:19:00","guid":{"rendered":"https:\/\/steelprogroup.com\/?p=21579"},"modified":"2025-03-11T13:44:40","modified_gmt":"2025-03-11T05:44:40","slug":"protect","status":"publish","type":"post","link":"https:\/\/steelprogroup.com\/ja\/galvanized-steel\/maintenance\/protect\/","title":{"rendered":"\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u3092\u9306\u304b\u3089\u5b88\u308b\u306b\u306f\uff1f"},"content":{"rendered":"<p class=\"c1 wp-block-paragraph\"><span class=\"c0\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u677f\u306e\u9306\u3092\u9632\u3050\u79d8\u8a23\u306f\u30b7\u30f3\u30d7\u30eb\u3067\u3059\u3002\u6e7f\u6c17\u3001\u7570\u7a2e\u91d1\u5c5e\u3001\u305d\u3057\u3066\u8150\u98df\u6027\u306e\u9ad8\u3044\u74b0\u5883\u304b\u3089\u9060\u3056\u3051\u308b\u3053\u3068\u3067\u3059\u3002\u5b9a\u671f\u7684\u306a\u30e1\u30f3\u30c6\u30ca\u30f3\u30b9\u3092\u884c\u3046\u3053\u3068\u3067\u3001\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u677f\u306f\u8010\u4e45\u6027\u3068\u9306\u3073\u306b\u512a\u308c\u305f\u72b6\u614b\u3092\u9577\u5e74\u4fdd\u3064\u3053\u3068\u304c\u3067\u304d\u307e\u3059\u3002 <\/span><\/p><p class=\"c1 wp-block-paragraph\"><span class=\"c0\">\u52b9\u679c\u7684\u306a\u4fdd\u8b77\u65b9\u6cd5\u3092\u8a73\u3057\u304f\u77e5\u308b\u305f\u3081\u306b\u3001\u3053\u306e\u30ac\u30a4\u30c9\u3067\u306f\u3001\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u3092\u6700\u9ad8\u306e\u72b6\u614b\u306b\u4fdd\u3064\u305f\u3081\u306b\u5fc5\u8981\u306a\u3059\u3079\u3066\u306e\u5bfe\u7b56\u3092\u8aac\u660e\u3057\u307e\u3059\u3002<\/span><\/p><h2 class=\"wp-block-heading c1 c5\" id=\"h.cmyjs0g59ql2\"><span class=\"c2\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306f\u9306\u3073\u307e\u3059\u304b\uff1f<\/span><\/h2><p class=\"c1 wp-block-paragraph\"><span class=\"c0\">\u306f\u3044\u3001\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u677f\u306f\u9306\u3073\u307e\u3059\u304c\u3001\u4e9c\u925b\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u306b\u3088\u308a\u3001\u672a\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u92fc\u677f\u306b\u6bd4\u3079\u3066\u8010\u98df\u6027\u304c\u5927\u5e45\u306b\u5411\u4e0a\u3057\u3066\u3044\u307e\u3059\u3002\u4e9c\u925b\u306f\u30d0\u30ea\u30a2\u3068\u3057\u3066\u6a5f\u80fd\u3057\u3001\u6c34\u5206\u3084\u9178\u7d20\u304c\u4e0b\u5730\u306e\u92fc\u677f\u306b\u5230\u9054\u3059\u308b\u306e\u3092\u9632\u304e\u307e\u3059\u3002<\/span><\/p><p class=\"c1 wp-block-paragraph\"><span class=\"c14\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306e\u8150\u98df\u306b\u3064\u306a\u304c\u308b\u8981\u56e0<\/span><span class=\"c0\">&nbsp;\u542b\u3080\uff1a<\/span><\/p><h3 class=\"wp-block-heading c1 c5\" id=\"h.a7i6dtc3ljm\"><span class=\"c3\">\u6c34\u5206<\/span><\/h3><p class=\"c1 wp-block-paragraph\"><span class=\"c0\">\u6e7f\u5ea6\u304c\u9ad8\u3044\u3068\u8150\u98df\u306e\u30ea\u30b9\u30af\u304c\u9ad8\u307e\u308a\u307e\u3059\u3002\u6e7f\u5ea6\u304c70%\u3092\u8d85\u3048\u308b\u74b0\u5883\u3067\u306f\u3001\u8150\u98df\u304c\u8457\u3057\u304f\u52a0\u901f\u3057\u307e\u3059\u3002<\/span><\/p><h3 class=\"wp-block-heading c1 c5\" id=\"h.6sjj9gh49y9p\"><span class=\"c3\">\u6e29\u5ea6<\/span><\/h3><p class=\"c1 wp-block-paragraph\"><span class=\"c0\">\u6c17\u6e29\u304c\u9ad8\u3044\u307b\u3069\u8150\u98df\u304c\u9032\u307f\u307e\u3059\u3002\u4f8b\u3048\u3070\u3001\u6c17\u6e29\u304c25\u2103\uff0877\u00b0F\uff09\u3092\u8d85\u3048\u308b\u6cbf\u5cb8\u5730\u57df\u3067\u306f\u3001\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306e\u8150\u98df\u304c\u65e9\u307e\u308b\u53ef\u80fd\u6027\u304c\u3042\u308a\u307e\u3059\u3002<\/span><\/p><h3 class=\"wp-block-heading c1 c5\" id=\"h.3vrqagwo1995\"><span class=\"c3\">\u5869\u3078\u306e\u66dd\u9732<\/span><\/h3><p class=\"c1 wp-block-paragraph\"><span class=\"c0\">\u6d77\u6d0b\u74b0\u5883\u3067\u306f\u7a7a\u6c17\u4e2d\u3084\u6c34\u4e2d\u306e\u5869\u5206\u6fc3\u5ea6\u304c\u9ad8\u304f\u3001\u8150\u98df\u901f\u5ea6\u304c\u4e0a\u6607\u3057\u307e\u3059\u3002\u7814\u7a76\u306b\u3088\u308b\u3068\u3001\u5869\u5206\u6fc3\u5ea6\u306e\u9ad8\u3044\u5730\u57df\u3067\u306f\u3001\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u677f\u306e\u4e9c\u925b\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u304c\u5e74\u959315\u30de\u30a4\u30af\u30ed\u30e1\u30fc\u30c8\u30eb\u3082\u5265\u304c\u308c\u308b\u53ef\u80fd\u6027\u304c\u3042\u308a\u307e\u3059\u3002<\/span><\/p><h3 class=\"wp-block-heading c1 c5\" id=\"h.vjfjma2v94n3\"><span class=\"c3\">\u6c5a\u67d3\u7269\u8cea<\/span><\/h3><p class=\"c1 wp-block-paragraph\"><span class=\"c0\">\u4e8c\u9178\u5316\u786b\u9ec4\u306a\u3069\u306e\u5927\u6c17\u6c5a\u67d3\u7269\u8cea\u306f\u4e9c\u925b\u3068\u53cd\u5fdc\u3057\u3001\u8150\u98df\u3092\u52a0\u901f\u3055\u305b\u307e\u3059\u3002\u5de5\u696d\u5730\u5e2f\u3067\u306f\u3053\u306e\u5f71\u97ff\u304c\u3088\u308a\u9855\u8457\u306b\u306a\u308a\u3001\u8150\u98df\u901f\u5ea6\u304c2\u500d\u306b\u306a\u308b\u3053\u3068\u3082\u3042\u308a\u307e\u3059\u3002<\/span><\/p><h3 class=\"wp-block-heading c1 c5\" id=\"h.ajc18sytzv8x\"><span class=\"c3\">pH\u30ec\u30d9\u30eb<\/span><\/h3><p class=\"c1 wp-block-paragraph\"><span class=\"c0\">\u6975\u7aef\u306a\u9178\u6027\u307e\u305f\u306f\u30a2\u30eb\u30ab\u30ea\u6027\u306e\u6761\u4ef6\u306f\u3001\u4e9c\u925b\u5c64\u306b\u30c0\u30e1\u30fc\u30b8\u3092\u4e0e\u3048\u308b\u53ef\u80fd\u6027\u304c\u3042\u308a\u307e\u3059\u3002\u4f8b\u3048\u3070\u3001pH\u5024\u304c6\u672a\u6e80\u307e\u305f\u306f12\u3092\u8d85\u3048\u308b\u3068\u3001\u4e9c\u925b\u30e1\u30c3\u30ad\u5c64\u306b\u5bfe\u3057\u3066\u975e\u5e38\u306b\u8150\u98df\u6027\u304c\u9ad8\u304f\u306a\u308a\u307e\u3059\u3002<\/span><\/p><h2 class=\"wp-block-heading c5 c12\" id=\"h.4cx7m6vmx2ml\"><span class=\"c2\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306e\u9306\u3092\u9632\u3050\u306b\u306f\u3069\u3046\u3059\u308c\u3070\u3088\u3044\u3067\u3057\u3087\u3046\u304b?<\/span><\/h2><h3 class=\"wp-block-heading c1 c5\" id=\"h.6rf81bwbcuyc\"><span class=\"c3\">\u904e\u9177\u306a\u74b0\u5883\u3092\u907f\u3051\u308b<\/span><\/h3><p class=\"c1 wp-block-paragraph\"><span class=\"c0\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306f\u3001\u4fdd\u8b77\u7528\u306e\u4e9c\u925b\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u304c\u640d\u306a\u308f\u308c\u308b\u7279\u5b9a\u306e\u74b0\u5883\u306b\u3055\u3089\u3055\u308c\u308b\u3068\u9306\u3073\u308b\u3053\u3068\u304c\u3042\u308a\u307e\u3059\u3002 <\/span><\/p><ul class=\"wp-block-list c4 lst-kix_rjxtihivtxr6-0 start\"><li><span class=\"c0\">\u6e7f\u5ea6\u3068\u5869\u5206\u6fc3\u5ea6\u304c\u9ad8\u3044\u6cbf\u5cb8\u5730\u57df\u3067\u306f\u3001\u4e9c\u925b\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u306e\u52a3\u5316\u304c\u65e9\u307e\u308a\u3001\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u304c\u9306\u3073\u3084\u3059\u304f\u306a\u308a\u307e\u3059\u3002<\/span><\/li>\n\n<li><span class=\"c0\">\u6c5a\u67d3\u7269\u8cea\u3084\u9178\u6027\u96e8\u306e\u3042\u308b\u5de5\u696d\u5730\u5e2f\u3067\u306f\u3001\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u304c\u8150\u98df\u6027\u5316\u5b66\u7269\u8cea\u306b\u3055\u3089\u3055\u308c\u3001\u4fdd\u8b77\u5c64\u304c\u5f90\u3005\u306b\u6469\u8017\u3057\u3066\u3044\u304d\u307e\u3059\u3002<\/span><\/li>\n\n<li><span class=\"c0\">\u6975\u7aef\u306a pH \u30ec\u30d9\u30eb\u306e\u74b0\u5883\uff08\u9178\u6027\u307e\u305f\u306f\u30a2\u30eb\u30ab\u30ea\u6027\uff09\u3067\u306f\u3001\u4e9c\u925b\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u304c\u640d\u50b7\u3057\u3001\u305d\u306e\u4e0b\u306e\u92fc\u9244\u306b\u9306\u304c\u65e9\u304f\u767a\u751f\u3059\u308b\u53ef\u80fd\u6027\u304c\u3042\u308a\u307e\u3059\u3002<\/span><\/li><\/ul><p class=\"c1 wp-block-paragraph\"><span class=\"c0\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u677f\u3092\u8150\u98df\u3057\u3084\u3059\u3044\u74b0\u5883\u306b\u3055\u3089\u3055\u306a\u3044\u3067\u304f\u3060\u3055\u3044\u3002\u3053\u306e\u3088\u3046\u306a\u74b0\u5883\u3067\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u677f\u3092\u4f7f\u7528\u3059\u308b\u5834\u5408\u306f\u3001\u65e9\u671f\u306e\u9306\u306e\u767a\u751f\u3092\u9632\u3050\u305f\u3081\u3001\u8ffd\u52a0\u306e\u4fdd\u8b77\u5bfe\u7b56\u3092\u8b1b\u3058\u308b\u3053\u3068\u3092\u304a\u52e7\u3081\u3057\u307e\u3059\u3002<\/span><\/p><p class=\"c1 wp-block-paragraph\"><span class=\"c0\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306f\u8010\u8150\u98df\u6027\u304c\u3042\u308a\u307e\u3059\u304c\u3001\u9069\u5207\u306a\u6392\u6c34\u3068\u63db\u6c17\u3092\u78ba\u4fdd\u3059\u308b\u3053\u3068\u304c\u4f9d\u7136\u3068\u3057\u3066\u91cd\u8981\u3067\u3059\u3002<\/span><\/p><h3 class=\"wp-block-heading c1 c5\" id=\"h.w8gorjzapw4w\"><span class=\"c3\">\u30ac\u30eb\u30d0\u30cb\u30c3\u30af\u8150\u98df\u3092\u907f\u3051\u308b<\/span><\/h3><p class=\"c1 wp-block-paragraph\"><span class=\"c0\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306f\u3001\u9285\u3084\u771f\u936e\u306a\u3069\u306e\u7570\u7a2e\u91d1\u5c5e\u3068\u76f4\u63a5\u63a5\u89e6\u3055\u305b\u306a\u3044\u3067\u304f\u3060\u3055\u3044\u3002\u3053\u308c\u3089\u306e\u91d1\u5c5e\u306f\u3001\u7279\u306b\u6e7f\u6c17\u306e\u591a\u3044\u74b0\u5883\u3067\u306f\u4e9c\u925b\u30e1\u30c3\u30ad\u3068\u53cd\u5fdc\u3057\u3001\u8150\u98df\u3092\u65e9\u3081\u308b\u53ef\u80fd\u6027\u304c\u3042\u308a\u307e\u3059\u3002<\/span><\/p><h3 class=\"wp-block-heading c1 c5\" id=\"h.7ttdnai7mrtg\"><span class=\"c3\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u677f\u3078\u306e\u5806\u7a4d\u3092\u907f\u3051\u308b<\/span><\/h3><p class=\"c1 wp-block-paragraph\"><span class=\"c0\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u677f\u306e\u8868\u9762\u3092\u5b9a\u671f\u7684\u306b\u6e05\u6383\u3057\u3066\u304f\u3060\u3055\u3044\u3002\u6c5a\u308c\u3001\u6e7f\u6c17\u3001\u6c5a\u67d3\u7269\u8cea\u304c\u84c4\u7a4d\u3059\u308b\u3068\u3001\u8868\u9762\u306b\u6c34\u5206\u304c\u9589\u3058\u8fbc\u3081\u3089\u308c\u3001\u6642\u9593\u306e\u7d4c\u904e\u3068\u3068\u3082\u306b\u4e9c\u925b\u30e1\u30c3\u30ad\u304c\u5f31\u307e\u308a\u307e\u3059\u3002\u9589\u3058\u8fbc\u3081\u3089\u308c\u305f\u6c34\u5206\u3084\u30b4\u30df\u306f\u3001\u7279\u306b\u6e7f\u6c17\u3084\u6c5a\u67d3\u3055\u308c\u305f\u74b0\u5883\u3067\u306f\u3001\u9306\u306e\u767a\u751f\u30ea\u30b9\u30af\u3092\u9ad8\u3081\u307e\u3059\u3002<\/span><\/p><p class=\"c1 wp-block-paragraph\"><span class=\"c0\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u3092\u9069\u5207\u306b\u6d17\u6d44\u3059\u308b\u306b\u306f\u3001\u67d4\u3089\u304b\u3044\u5e03\u304b\u30d6\u30e9\u30b7\u3092\u4f7f\u3044\u3001\u4e2d\u6027\u6d17\u5264\u3068\u6c34\u3067\u512a\u3057\u304f\u6d17\u3063\u3066\u304f\u3060\u3055\u3044\u3002\u5f37\u529b\u306a\u5316\u5b66\u85ac\u54c1\u3084\u7814\u78e8\u5264\u5165\u308a\u306e\u305f\u308f\u3057\u306f\u4e9c\u925b\u30e1\u30c3\u30ad\u3092\u50b7\u3081\u308b\u53ef\u80fd\u6027\u304c\u3042\u308b\u305f\u3081\u3001\u4f7f\u7528\u3057\u306a\u3044\u3067\u304f\u3060\u3055\u3044\u3002\u3088\u304f\u3059\u3059\u304e\u3001\u8868\u9762\u306b\u6b8b\u7559\u7269\u304c\u6b8b\u3089\u306a\u3044\u3088\u3046\u306b\u4e7e\u71e5\u3055\u305b\u3066\u304f\u3060\u3055\u3044\u3002<\/span><\/p><h2 class=\"wp-block-heading c12 c5\" id=\"h.gj0v45s60lv\"><span class=\"c2\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u677f\u3092\u9306\u304b\u3089\u5b88\u308b\u306b\u306f\u3069\u3046\u3059\u308c\u3070\u3044\u3044\u3067\u3059\u304b?<\/span><\/h2><h3 class=\"wp-block-heading c1 c5\" id=\"h.9dsc7dryaawe\"><span class=\"c3\">\u4fdd\u8b77\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0<\/span><\/h3><p class=\"c1 wp-block-paragraph\"><span class=\"c0\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u306b\u4fdd\u8b77\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u3084\u5857\u6599\u3092\u5857\u5e03\u3059\u308b\u3053\u3068\u3067\u3001\u8150\u98df\u306b\u5bfe\u3059\u308b\u9632\u5fa1\u5c64\u304c\u3055\u3089\u306b\u5f37\u5316\u3055\u308c\u307e\u3059\u3002\u4e00\u822c\u7684\u306a\u4fdd\u8b77\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u306b\u306f\u4ee5\u4e0b\u306e\u3082\u306e\u304c\u3042\u308a\u307e\u3059\u3002<\/span><\/p><ul class=\"wp-block-list c4 lst-kix_yn09gu6asuyj-0 start\"><li><span class=\"c13\">\u30b8\u30f3\u30af\u30ea\u30c3\u30c1\u30da\u30a4\u30f3\u30c8<\/span><\/li><\/ul><p class=\"c1 wp-block-paragraph\"><span class=\"c0\">\u3053\u308c\u3089\u306e\u5857\u6599\u306f\u4e9c\u925b\u7c92\u5b50\u3092\u9ad8\u6fc3\u5ea6\u306b\u542b\u307f\u3001\u5143\u306e\u4e9c\u925b\u30e1\u30c3\u30ad\u5c64\u3068\u540c\u69d8\u306e\u4fdd\u8b77\u6027\u80fd\u3092\u767a\u63ee\u3057\u307e\u3059\u3002\u4e9c\u925b\u3092\u591a\u304f\u542b\u3080\u5857\u6599\u306f\u3001\u640d\u50b7\u7b87\u6240\u306e\u88dc\u4fee\u306b\u6700\u9069\u3067\u3001\u65e2\u5b58\u306e\u4e9c\u925b\u30e1\u30c3\u30ad\u5c64\u3092\u88dc\u5f37\u3057\u3001\u9306\u3092\u9632\u304e\u307e\u3059\u3002<\/span><\/p><ul class=\"wp-block-list c4 lst-kix_yn09gu6asuyj-0\"><li><span class=\"c13\">\u30a8\u30dd\u30ad\u30b7\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0<\/span><\/li><\/ul><p class=\"c1 wp-block-paragraph\"><span class=\"c0\">\u3053\u308c\u3089\u306e\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u306f\u3001\u6e7f\u6c17\u3084\u5316\u5b66\u7269\u8cea\u306b\u5bfe\u3059\u308b\u512a\u308c\u305f\u4fdd\u8b77\u6027\u80fd\u3092\u5099\u3048\u3001\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u677f\u306e\u4e0a\u306b\u8010\u4e45\u6027\u306e\u3042\u308b\u30b7\u30fc\u30eb\u30c9\u3092\u5f62\u6210\u3057\u307e\u3059\u3002\u305d\u306e\u305f\u3081\u3001\u92fc\u677f\u304c\u904e\u9177\u306a\u6761\u4ef6\u306b\u3055\u3089\u3055\u308c\u308b\u53ef\u80fd\u6027\u306e\u3042\u308b\u7523\u696d\u74b0\u5883\u306b\u6700\u9069\u3067\u3059\u3002<\/span><\/p><ul class=\"wp-block-list c4 lst-kix_yn09gu6asuyj-0\"><li><span class=\"c13\">\u30dd\u30ea\u30a6\u30ec\u30bf\u30f3\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0<\/span><\/li><\/ul><p class=\"c1 wp-block-paragraph\"><span class=\"c0\">\u30dd\u30ea\u30a6\u30ec\u30bf\u30f3\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u306f\u3001\u591a\u304f\u306e\u5834\u5408\u3001\u6700\u4e0a\u5c64\u3068\u3057\u3066\u4f7f\u7528\u3055\u308c\u3001\u512a\u308c\u305f\u7d2b\u5916\u7dda\u8010\u6027\u3092\u5099\u3048\u3001\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u677f\u3092\u592a\u967d\u5149\u306b\u3088\u308b\u6469\u8017\u304b\u3089\u4fdd\u8b77\u3057\u307e\u3059\u3002\u4e9c\u925b\u5c64\u3092\u4fdd\u8b77\u3057\u3001\u7f8e\u3057\u3044\u5916\u89b3\u3092\u7dad\u6301\u3059\u308b\u305f\u3081\u306b\u3001\u5c4b\u5916\u3067\u5857\u5e03\u3055\u308c\u308b\u3053\u3068\u304c\u4e00\u822c\u7684\u3067\u3059\u3002<\/span><\/p><ul class=\"wp-block-list c4 lst-kix_yn09gu6asuyj-0\"><li><span class=\"c13\">\u30a2\u30af\u30ea\u30eb\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0<\/span><\/li><\/ul><p class=\"c1 wp-block-paragraph\"><span class=\"c0\">\u30a2\u30af\u30ea\u30eb\u30d9\u30fc\u30b9\u306e\u30af\u30ea\u30a2\u30b3\u30fc\u30c8\u3068\u30b7\u30fc\u30e9\u30f3\u30c8\u306f\u5857\u5e03\u304c\u5bb9\u6613\u3067\u3001\u8150\u98df\u6027\u306e\u4f4e\u3044\u74b0\u5883\u306b\u304a\u3044\u3066\u57fa\u672c\u7684\u306a\u4fdd\u8b77\u3092\u63d0\u4f9b\u3057\u307e\u3059\u3002\u6c4e\u7528\u6027\u304c\u9ad8\u304f\u3001\u9069\u5ea6\u306a\u8010\u4e45\u6027\u3092\u5099\u3048\u3066\u3044\u307e\u3059\u3002<\/span><\/p><ul class=\"wp-block-list c4 lst-kix_yn09gu6asuyj-0\"><li><span class=\"c13\">\u7c89\u4f53\u5857\u6599<\/span><\/li><\/ul><p class=\"c1 wp-block-paragraph\"><span class=\"c0\">\u7c89\u4f53\u5857\u6599\u306f\u3001\u8010\u4e45\u6027\u3068\u5747\u4e00\u6027\u306b\u512a\u308c\u305f\u4ed5\u4e0a\u304c\u308a\u3092\u5b9f\u73fe\u3057\u3001\u74b0\u5883\u30b9\u30c8\u30ec\u30b9\u306b\u5bfe\u3059\u308b\u9ad8\u3044\u8010\u6027\u3092\u5099\u3048\u3066\u3044\u307e\u3059\u3002\u4e7e\u71e5\u7c89\u672b\u3068\u3057\u3066\u5857\u5e03\u3057\u3001\u52a0\u71b1\u786c\u5316\u3055\u305b\u308b\u3053\u3068\u3067\u3001\u539a\u304f\u5bc6\u7740\u3057\u305f\u5c64\u3092\u5f62\u6210\u3057\u3001\u8010\u4e45\u6027\u3092\u5411\u4e0a\u3055\u305b\u307e\u3059\u3002<\/span><\/p><h3 class=\"wp-block-heading c5 c10\" id=\"h.4nq2qobhmsra\"><span class=\"c3\">\u5b9a\u671f\u7684\u306a\u70b9\u691c\u3068\u30e1\u30f3\u30c6\u30ca\u30f3\u30b9<\/span><\/h3><p class=\"c1 wp-block-paragraph\"><span class=\"c0\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u677f\u306f\u3001\u50b7\u3084\u4e9c\u925b\u304c\u6469\u8017\u3057\u3066\u3044\u308b\u53ef\u80fd\u6027\u306e\u3042\u308b\u7b87\u6240\u304c\u306a\u3044\u304b\u3001\u5b9a\u671f\u7684\u306b\u70b9\u691c\u3057\u3066\u304f\u3060\u3055\u3044\u3002\u50b7\u3084\u9732\u51fa\u7b87\u6240\u3092\u898b\u3064\u3051\u305f\u5834\u5408\u306f\u3001\u3059\u3050\u306b\u30b8\u30f3\u30af\u30ea\u30c3\u30c1\u30da\u30a4\u30f3\u30c8\u307e\u305f\u306f\u9069\u5207\u306a\u4fdd\u8b77\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u3067\u88dc\u4fee\u3057\u3066\u304f\u3060\u3055\u3044\u3002\u3053\u306e\u3088\u3046\u306a\u9069\u5207\u306a\u30e1\u30f3\u30c6\u30ca\u30f3\u30b9\u306f\u3001\u8150\u98df\u306e\u62e1\u5927\u3092\u9632\u304e\u3001\u92fc\u677f\u3092\u9577\u6301\u3061\u3055\u305b\u308b\u306e\u306b\u5f79\u7acb\u3061\u307e\u3059\u3002<\/span><\/p><h2 class=\"wp-block-heading c1 c5\" id=\"h.p0azx7fg2ckm\"><span class=\"c2\">\u5747\u4e00\u306a\u4e9c\u925b\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u306f\u5927\u304d\u306a\u52b9\u679c\u3092\u767a\u63ee\u3057\u307e\u3059<\/span><\/h2><p class=\"c1 wp-block-paragraph\"><span class=\"c0\">\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u677f\u306e\u9306\u3092\u9632\u3050\u306b\u306f\u3001\u5747\u4e00\u306a\u4e9c\u925b\u30e1\u30c3\u30ad\u3082\u91cd\u8981\u3067\u3059\u3002\u30e1\u30c3\u30ad\u304c\u4e0d\u5747\u4e00\u3060\u3068\u3001\u5f31\u70b9\u304c\u9732\u51fa\u3057\u3001\u9306\u306e\u30ea\u30b9\u30af\u304c\u9ad8\u307e\u308a\u3001\u8010\u4e45\u6027\u3082\u4f4e\u4e0b\u3057\u307e\u3059\u3002<\/span><\/p><p class=\"c1 wp-block-paragraph\">Steel Pro Group\u306f\u53b3\u683c\u306a\u88fd\u9020\u57fa\u6e96\u3092\u9075\u5b88\u3057\u3001\u3059\u3079\u3066\u306e\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u88fd\u54c1\u306b\u5747\u4e00\u306a\u4e9c\u925b\u30b3\u30fc\u30c6\u30a3\u30f3\u30b0\u3092\u65bd\u3057\u3001\u512a\u308c\u305f\u8010\u8150\u98df\u6027\u3092\u5b9f\u73fe\u3057\u3066\u3044\u307e\u3059\u3002\u307e\u305f\u3001\u4ee5\u4e0b\u306e\u3088\u3046\u306a\u8ffd\u52a0\u51e6\u7406\u3082\u63d0\u4f9b\u3057\u3066\u3044\u307e\u3059\u3002 <span class=\"c15\"><a class=\"c11\" href=\"https:\/\/www.google.com\/url?q=https:\/\/steelprogroup.com\/product-category\/galvanized-steel\/ppgi\/%23StainlessSteel&amp;sa=D&amp;source=editors&amp;ust=1741666753445055&amp;usg=AOvVaw33wfSttm7oV0V5ro8XArAG\">PPGI<\/a><\/span><span class=\"c0\">\u3001\u3055\u3089\u306b\u9632\u9306\u6027\u3092\u9ad8\u3081\u307e\u3059\u3002 <\/span><\/p><p class=\"wp-block-paragraph\">&nbsp;<\/p>","protected":false},"excerpt":{"rendered":"<p>\u4e9c\u925b\u30e1\u30c3\u30ad\u92fc\u677f\u306e\u5bff\u547d\u3092\u6700\u5927\u9650\u306b\u5ef6\u3070\u3059\u305f\u3081\u306e\u9632\u9306\u5bfe\u7b56\u3092\u3054\u7d39\u4ecb\u3057\u307e\u3059\u3002Steel Pro Group\u306e\u30ac\u30a4\u30c9\u306b\u306f\u3001\u9577\u6301\u3061\u3055\u305b\u308b\u305f\u3081\u306b\u5fc5\u8981\u306a\u60c5\u5831\u304c\u3059\u3079\u3066\u63c3\u3063\u3066\u3044\u307e\u3059\u3002<\/p>","protected":false},"author":1,"featured_media":21580,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"_eb_attr":"","rank_math_lock_modified_date":false,"site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"categories":[4314],"tags":[],"class_list":["post-21579","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-maintenance-galvanized-steel"],"acf":[],"_links":{"self":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts\/21579","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/comments?post=21579"}],"version-history":[{"count":0,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts\/21579\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/media\/21580"}],"wp:attachment":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/media?parent=21579"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/categories?post=21579"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/tags?post=21579"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}