{"id":9889,"date":"2024-09-04T18:51:50","date_gmt":"2024-09-04T10:51:50","guid":{"rendered":"https:\/\/app11147.cloudwayssites.com\/?p=9889"},"modified":"2025-02-17T17:55:50","modified_gmt":"2025-02-17T09:55:50","slug":"magnetic","status":"publish","type":"post","link":"https:\/\/steelprogroup.com\/ja\/stainless-steel\/properties\/magnetic\/","title":{"rendered":"\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u78c1\u6027\u3092\u6301\u3064\u304b\uff1f"},"content":{"rendered":"<p class=\"wp-block-paragraph\">\u30b9\u30c6\u30f3\u30ec\u30b9\u30fb\u30b9\u30c1\u30fc\u30eb\u306f\u4eca\u306b\u59cb\u307e\u3063\u305f\u3053\u3068\u3067\u306f\u306a\u3044\u3002\u6628\u591c\u3001\u30b9\u30c6\u30f3\u30ec\u30b9\u88fd\u306e\u53f0\u6240\u7528\u54c1\u3092\u4f7f\u3063\u3066\u5915\u98df\u3092\u4f5c\u3063\u305f\u3070\u304b\u308a\u304b\u3082\u3057\u308c\u306a\u3044\u3002 <strong>\u3057\u304b\u3057\u3001\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u304c\u78c1\u6c17\u3092\u5e2f\u3073\u3066\u3044\u308b\u304b\u3069\u3046\u304b\u3001\u3054\u5b58\u3058\u3060\u308d\u3046\u304b\uff1f<\/strong> \u7b54\u3048\u306f\u30a4\u30a8\u30b9\u3067\u3082\u3042\u308a\u30ce\u30fc\u3067\u3082\u3042\u308b\u3002\u307b\u3068\u3093\u3069\u306e\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u975e\u78c1\u6027\u3067\u3059\u304c\u3001\u78c1\u6027\u3092\u6301\u3064\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u3082\u3042\u308a\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u306a\u305c\u78c1\u6027\u3092\u6301\u3064\u306e\u304b\uff1f<\/h2><p class=\"wp-block-paragraph\">\u7c21\u5358\u306b\u8a00\u3048\u3070\u3001\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u304c\u78c1\u6027\u3092\u6301\u3064\u305f\u3081\u306b\u306f\u3001\u4ee5\u4e0b\u306e\u6761\u4ef6\u3092\u6e80\u305f\u3059\u5fc5\u8981\u304c\u3042\u308b\uff1a<\/p><ol class=\"wp-block-list\"><li>\u9244\u5206\u304c\u542b\u307e\u308c\u3066\u3044\u306a\u3051\u308c\u3070\u306a\u3089\u306a\u3044\u3002<\/li>\n\n<li>\u30de\u30eb\u30c6\u30f3\u30b5\u30a4\u30c8\u7d44\u7e54\uff08BCT\uff09\u307e\u305f\u306f\u30d5\u30a7\u30e9\u30a4\u30c8\u7d44\u7e54\uff08BCC\uff09\u304c\u5fc5\u8981\u3067\u3042\u308b\u3002<\/li><\/ol><p class=\"wp-block-paragraph\"><em>* BCT\uff1a\u4f53\u5fc3\u6b63\u65b9\u6676\u3001BCC\uff1a\u4f53\u5fc3\u7acb\u65b9\u6676\u3002\u3069\u3061\u3089\u3082\u7d50\u6676\u69cb\u9020\u3067\u3042\u308b\u3002<\/em><\/p><p class=\"wp-block-paragraph\">\u3059\u3079\u3066\u306e\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u9244\u3092\u542b\u307f\u3001\u9244\u306f\u672c\u8cea\u7684\u306b\u78c1\u6027\u3092\u6301\u3064\u3002\u3057\u304b\u3057\u3001\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u304c\u78c1\u6027\u3092\u6301\u3064\u304b\u3069 \u3046\u304b\u306f\u3001\u305d\u306e\u7d50\u6676\u69cb\u9020\u306b\u3088\u308b\u3002\u5408\u91d1\u304c <a href=\"https:\/\/steelprogroup.com\/ja\/stainless-steel\/type\/austenitic\/\">\u30aa\u30fc\u30b9\u30c6\u30ca\u30a4\u30c8\u7cfb<\/a>\u306e\u5834\u5408\u3001\u4e00\u822c\u306b\u975e\u78c1\u6027\u3067\u3042\u308b\u3002\u9244\u3092\u542b\u3093\u3067\u3044\u308b\u306b\u3082\u304b\u304b\u308f\u3089\u305a\u3001\u7d50\u6676\u69cb\u9020\u304c\u78c1\u6027\u3092\u793a\u3055\u306a\u3044\u304b\u3089\u3067\u3042\u308b\u3002&nbsp;<\/p><h3 class=\"wp-block-heading\">\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u6c38\u4e45\u78c1\u77f3\u304b\uff1f<\/h3><p class=\"wp-block-paragraph\">\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u4e00\u822c\u7684\u306b\u6c38\u4e45\u78c1\u77f3\u3067\u306f\u306a\u3044\u3002\u78c1\u6027\u3092\u6301\u3064\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u3082\u3042\u308b\u304c\u3001\u5916 \u90e8\u78c1\u754c\u3092\u53d6\u308a\u9664\u304f\u3068\u78c1\u6027\u3092\u5931\u3046\u3002\u9244\u3084\u30b3\u30d0\u30eb\u30c8\u304b\u3089\u4f5c\u3089\u308c\u308b\u3088\u3046\u306a\u6c38\u4e45\u78c1\u77f3\u306f\u3001\u6642\u9593\u304c\u7d4c\u3063\u3066\u3082\u78c1\u6027\u3092\u4fdd\u3061\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u78c1\u6027\u306f\u4f55\u306b\u5f71\u97ff\u3055\u308c\u308b\u306e\u304b\uff1f<\/h2><p class=\"wp-block-paragraph\">\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u304c\u78c1\u6027\u3092\u6301\u3064\u304b\u3069\u3046\u304b\u3092\u6c7a\u5b9a\u3059\u308b\u3082\u306e\u306f\u308f\u304b\u3063\u3066\u3044\u308b\u3002\u30b9\u30c6\u30f3\u30ec\u30b9\u306e\u78c1\u6027\u306b\u5f71\u97ff\u3092\u4e0e\u3048\u308b\u8981\u56e0\u3092\u4ee5\u4e0b\u306b\u793a\u3059\uff1a<\/p><ol class=\"wp-block-list\"><li><strong>\u5408\u91d1\u7d44\u6210\uff1a<\/strong> \u30af\u30ed\u30e0\u3084\u30cb\u30c3\u30b1\u30eb\u306a\u3069\u306e\u5408\u91d1\u5143\u7d20\u306e\u7a2e\u985e\u3068\u91cf\u306f\u3001\u30b9\u30c6\u30f3\u30ec \u30b9\u92fc\u306e\u78c1\u6c17\u7279\u6027\u306b\u5f71\u97ff\u3092\u4e0e\u3048\u308b\u3002<\/li>\n\n<li><strong>\u71b1\u51e6\u7406\uff1a<\/strong> \u7570\u306a\u308b\u71b1\u51e6\u7406\u5de5\u7a0b\u306f\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u7d50\u6676\u69cb\u9020\u3092\u5909\u5316\u3055\u305b\u3001\u305d\u306e\u7d50\u679c\u3001\u78c1\u6c17\u7279\u6027\u306b\u5f71\u97ff\u3092\u4e0e\u3048\u308b\u3002<\/li>\n\n<li><strong>\u51b7\u9593\u52a0\u5de5\uff1a<\/strong> \u51b7\u9593\u5727\u5ef6\u306e\u3088\u3046\u306a\u5de5\u7a0b\u306f\u3001\u7d50\u6676\u69cb\u9020\u3092\u5909\u5316\u3055\u305b\u308b\u3053\u3068\u3067\u3001\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306b\u78c1\u6027\u3092\u5c0e\u5165\u3059\u308b\u3053\u3068\u304c\u3067\u304d\u308b\u3002<\/li>\n\n<li><strong>\u6e29\u5ea6\u3060\uff1a<\/strong> \u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u78c1\u6c17\u7279\u6027\u306f\u6e29\u5ea6\u306b\u3088\u3063\u3066\u5909\u5316\u3059\u308b\u3053\u3068\u304c\u3042\u308a\u307e\u3059\u3002<\/li>\n\n<li><strong>\u4e0d\u7d14\u7269\u306e\u5b58\u5728<\/strong>:\u4e0d\u7d14\u7269\u306f\u7d50\u6676\u69cb\u9020\u306e\u5747\u4e00\u6027\u3092\u4e71\u3057\u3001\u78c1\u6c17\u7279\u6027\u3092\u4f4e\u4e0b\u3055\u305b\u305f\u308a\u5909\u5316\u3055\u305b\u305f\u308a\u3059\u308b\u53ef\u80fd\u6027\u304c\u3042\u308b\u3002<\/li><\/ol><h2 class=\"wp-block-heading\">\u78c1\u6027\u3092\u6301\u3064\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\uff1f\u305d\u3046\u3067\u306a\u3044\u3082\u306e\u306f\uff1f&nbsp;<\/h2><p class=\"wp-block-paragraph\">\u4e00\u822c\u7684\u306b\u3001\u307b\u3068\u3093\u3069\u306e\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u975e\u78c1\u6027 \u3067\u3042\u308b\u3002\u30d5\u30a7\u30e9\u30a4\u30c8\u7cfb\u304a\u3088\u3073\u30de\u30eb\u30c6\u30f3\u30b5\u30a4\u30c8\u7cfb\u30b9\u30c6\u30f3\u30ec \u30b9\u92fc\u306e\u3088\u3046\u306a\u7279\u6b8a\u306a\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u78c1\u6027\u3092\u6709\u3057\u3001\u30aa\u30fc\u30b9 \u30c6\u30ca\u30a4\u30c8\u7cfb\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u4e00\u822c\u7684\u306b\u975e\u78c1\u6027\u3067\u3042\u308b\u3002&nbsp;<\/p><p class=\"wp-block-paragraph\">\u4e00\u822c\u7684\u306a\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u7a2e\u3067\u3001\u78c1\u6027\u307e\u305f\u306f\u975e\u78c1\u6027 \u306e\u3082\u306e\u3092\u3044\u304f\u3064\u304b\u7d39\u4ecb\u3059\u308b\uff1a<\/p><h3 class=\"wp-block-heading\"><strong>\u78c1\u6027\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc<\/strong><\/h3><ul class=\"wp-block-list\"><li>\u30d5\u30a7\u30e9\u30a4\u30c8\u7cfb\uff1a430\u3001409<\/li>\n\n<li>\u30de\u30eb\u30c6\u30f3\u30b5\u30a4\u30c8\u7cfb\uff1a410\u3001420\u3001440C<\/li>\n\n<li>\u30c7\u30e5\u30d7\u30ec\u30c3\u30af\u30b9<strong>:<\/strong> 2205, 2507<\/li><\/ul><h3 class=\"wp-block-heading\"><strong>\u975e\u78c1\u6027\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc<\/strong><\/h3><ul class=\"wp-block-list\"><li>\u30aa\u30fc\u30b9\u30c6\u30ca\u30a4\u30c8\u7cfb\uff1a304\u3001316\u3001310<\/li><\/ul><h3 class=\"wp-block-heading\"><strong>\u7279\u5225\u306a\u30b1\u30fc\u30b9<\/strong><\/h3><p class=\"wp-block-paragraph\">\u4ee5\u4e0b\u306e\u3088\u3046\u306a\u30aa\u30fc\u30b9\u30c6\u30ca\u30a4\u30c8\u7cfb\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u3002 <a href=\"https:\/\/steelprogroup.com\/ja\/stainless-steel\/grades\/grade-304\/\">304<\/a> \u305d\u3057\u3066 <a href=\"https:\/\/steelprogroup.com\/ja\/stainless-steel\/grades\/grade-316\/\" data-type=\"post\" data-id=\"10280\" target=\"_blank\" rel=\"noreferrer noopener\">316<\/a>\u306f\u901a\u5e38\u975e\u78c1\u6027\u3067\u3042\u308b\u3002\u3057\u304b\u3057\u3001\u5927\u898f\u6a21\u306a\u51b7\u9593\u52a0\u5de5\u3084\u6eb6\u63a5\u306e\u5f8c\u306b\u306f\u3001\u30de\u30eb\u30c6\u30f3\u30b5\u30a4\u30c8\u306e\u5f62\u6210\u306b\u3088\u308a\u308f\u305a\u304b\u306b\u78c1\u6027\u3092\u5e2f\u3073\u308b\u3053\u3068\u304c\u3042\u308b\u3002<\/p><p class=\"wp-block-paragraph\">\u9006\u306b\u3001\u78c1\u6027\u3092\u6301\u3064\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u304c\u975e\u78c1 \u6027\u306b\u306a\u308b\u3053\u3068\u306f\u3042\u307e\u308a\u306a\u3044\u3002\u3042\u308b\u7a2e\u306e\u71b1\u51e6\u7406\u306f\u3001\u30d5\u30a7\u30e9\u30a4\u30c8\u92fc\u3084\u30de\u30eb \u30c6\u30f3\u30b5\u30a4\u30c8\u92fc\u306e\u78c1\u6027\u3092\u4f4e\u4e0b\u3055\u305b\u308b\u304c\u3001\u78c1\u6027\u3092\u5b8c \u5168\u306b\u9664\u53bb\u3059\u308b\u3053\u3068\u306f\u901a\u5e38\u306a\u3044\u3002<\/p><h3 class=\"wp-block-heading\">\u4e8c\u76f8\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u78c1\u6027\u306b\u304a\u3044\u3066\u7279\u5225\u3067\u3042\u308b<\/h3><p class=\"wp-block-paragraph\"><a href=\"https:\/\/steelprogroup.com\/ja\/stainless-steel\/type\/duplex\/\">\u4e8c\u76f8\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc<\/a> \u306f\u30aa\u30fc\u30b9\u30c6\u30ca\u30a4\u30c8\u3068\u30d5\u30a7\u30e9\u30a4\u30c8\u306e\u6df7\u5408\u7d44\u7e54\u3092\u6301\u3061\u3001\u3053\u308c\u304c\u90e8\u5206\u7684\u306a\u78c1\u6c17\u7279\u6027\u3092\u4e0e\u3048\u3066\u3044\u308b\u3002\u7d14\u7c8b\u306a\u30d5\u30a7\u30e9\u30a4\u30c8\u92fc\u3084\u30de\u30eb\u30c6\u30f3\u30b5\u30a4\u30c8\u92fc\u307b\u3069\u78c1\u6027\u306f\u5f37\u304f\u306a\u3044\u304c\u3001\u7d14\u7c8b\u306a\u30aa\u30fc\u30b9\u30c6\u30ca\u30a4\u30c8\u92fc\u3088\u308a\u306f\u78c1\u6027\u304c\u5f37\u3044\u3002\u3053\u306e\u4e8c\u76f8\u69cb\u9020\u306f\u3001\u3042\u308b\u7a0b\u5ea6\u306e\u78c1\u6027\u3092\u542b\u3080\u4e21\u76f8\u306e\u6709\u76ca\u306a\u7279\u6027\u3092\u517c\u306d\u5099\u3048\u3066\u3044\u308b\u3002<\/p><h2 class=\"wp-block-heading\">\u306a\u305c\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306b\u3068\u3063\u3066\u78c1\u6027\u304c\u91cd\u8981\u306a\u8981\u7d20\u306a\u306e\u304b\uff1f<\/h2><p class=\"wp-block-paragraph\">\u78c1\u6027\u306f\u3001\u69d8\u3005\u306a\u7528\u9014\u3001\u7279\u306b\u78c1\u6c17\u5e72\u6e09\u306b\u654f\u611f\u306a\u74b0 \u5883\u306b\u304a\u3051\u308b\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u9069\u5408\u6027\u3068\u6027\u80fd\u306b\u5f71\u97ff\u3059 \u308b\u305f\u3081\u3001\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306b\u3068\u3063\u3066\u8003\u616e\u3059\u3079\u304d\u91cd\u8981\u306a \u8981\u7d20\u3067\u3042\u308b\u3002&nbsp;<\/p><p class=\"wp-block-paragraph\">\u3055\u3089\u306b\u78c1\u6027\u306f\u3001\u6a5f\u68b0\u52a0\u5de5\u3001\u6210\u5f62\u3001\u6eb6\u63a5\u306a\u3069\u306e\u52a0\u5de5\u5de5\u7a0b\u306e\u8907\u96d1\u3055\u3084\u96e3\u6613\u5ea6\u306b\u3082\u5f71\u97ff\u3059\u308b\u3002\u4f8b\u3048\u3070\u3001\u78c1\u6027\u306f\u91d1\u5c5e\u7247\u304c\u78c1\u6027\u8868\u9762\u306b\u4ed8\u7740\u3059\u308b\u305f\u3081\u3001\u6a5f\u68b0\u52a0\u5de5\u3092\u8907\u96d1\u306b\u3059\u308b\u3002\u307e\u305f\u3001\u78c1\u6027\u6750\u6599\u306f\u6eb6\u63a5\u6642\u306b\u30a2\u30fc\u30af\u30d6\u30ed\u30fc\u3092\u5f15\u304d\u8d77\u3053\u3057\u3001\u6eb6\u63a5\u54c1\u8cea\u306e\u4f4e\u4e0b\u306b\u3064\u306a\u304c\u308a\u307e\u3059\u3002\u3057\u305f\u304c\u3063\u3066\u3001\u52a0\u5de5\u5de5\u7a0b\u306e\u7cbe\u5ea6\u3068\u54c1\u8cea\u3092\u78ba\u4fdd\u3059\u308b\u305f\u3081\u306b\u306f\u3001\u78c1\u6c17\u7279\u6027\u3092\u8003\u616e\u3059\u308b\u5fc5\u8981\u304c\u3042\u308a\u307e\u3059\u3002<\/p><h2 class=\"wp-block-heading\">\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u4ee5\u5916\u306e\u78c1\u6027\u92fc\u7a2e<\/h2><p class=\"wp-block-paragraph\">\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u4ed6\u306b\u3001\u78c1\u6027\u92fc\u306b\u306f\u3044\u304f\u3064\u304b\u306e\u7a2e\u985e\u304c\u3042\u308a\u307e\u3059\u3002\u4e0b\u306e\u8868\u3067\u7c21\u5358\u306b\u6bd4\u8f03\u3057\u3066\u307f\u307e\u3057\u3087\u3046\uff1a<\/p><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u30b9\u30c1\u30fc\u30eb\u30bf\u30a4\u30d7<\/strong><\/td><td><strong>\u96fb\u6c17\u92fc\uff08\u30b1\u30a4\u7d20\u92fc\uff09<\/strong><\/td><td><strong>\u30de\u30ec\u30fc\u30b8\u30f3\u30b0\u92fc<\/strong><\/td><td><strong><a href=\"https:\/\/steelprogroup.com\/ja\/alloy-steel\/\">\u5408\u91d1\u92fc<\/a><\/strong><\/td><td><strong><a href=\"https:\/\/steelprogroup.com\/ja\/plain-carbon-steel\/\">\u70ad\u7d20\u92fc<\/a><\/strong><\/td><td><strong><a href=\"https:\/\/steelprogroup.com\/ja\/tool-steel\/\">\u5de5\u5177\u92fc<\/a><\/strong><\/td><td><strong><a href=\"https:\/\/steelprogroup.com\/ja\/stainless-steel\/\">\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc<\/a><\/strong><\/td><\/tr><tr><td><strong>\u78c1\u6c17<\/strong><\/td><td>\u9ad8\u3044<\/td><td>\u9ad8\u3044<\/td><td>\u4e2d\uff5e\u9ad8<\/td><td>\u4e2d\u7a0b\u5ea6<\/td><td>\u4e2d\u7a0b\u5ea6<\/td><td>\u5168\u822c\u7684\u306b\u4f4e\u3044<\/td><\/tr><tr><td><strong>\u900f\u78c1\u7387<\/strong><\/td><td>\u975e\u5e38\u306b\u9ad8\u3044<\/td><td>\u9ad8\u3044<\/td><td>\u4e2d\uff5e\u9ad8<\/td><td>\u4e2d\u7a0b\u5ea6<\/td><td>\u4e2d\u7a0b\u5ea6<\/td><td>\u4f4e\u3044<\/td><\/tr><tr><td><strong>\u4fdd\u78c1\u529b<\/strong><\/td><td>\u4f4e\u3044<\/td><td>\u4f4e\u3044<\/td><td>\u4e2d\u7a0b\u5ea6<\/td><td>\u9ad8\u3044<\/td><td>\u9ad8\u3044<\/td><td>\u9ad8\u3044<\/td><\/tr><tr><td><strong>\u7533\u3057\u8fbc\u307f<\/strong><\/td><td>\u5909\u5727\u5668\u3001\u96fb\u6c17\u30e2\u30fc\u30bf\u30fc\u3001\u767a\u96fb\u6a5f<\/td><td>\u822a\u7a7a\u5b87\u5b99\u3001\u5de5\u5177\u7528\u9014<\/td><td>\u69d8\u3005\u306a\u7523\u696d\u7528\u9014<\/td><td>\u7dcf\u5408\u30a8\u30f3\u30b8\u30cb\u30a2\u30ea\u30f3\u30b0\u3001\u5efa\u8a2d<\/td><td>\u9ad8\u786c\u5ea6\u3092\u5fc5\u8981\u3068\u3059\u308b\u5de5\u5177<\/td><td>\u8010\u98df\u7528\u9014\u3001\u8abf\u7406\u5668\u5177\u3001\u533b\u7642\u5668\u5177<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u6c17\u306b\u306a\u308b\u60c5\u5831<\/h2><h3 class=\"wp-block-heading\">\u78c1\u77f3\u306f\u30b9\u30c6\u30f3\u30ec\u30b9\u3092\u50b7\u3064\u3051\u308b\u304b\uff1f<\/h3><p class=\"wp-block-paragraph\">\u78c1\u77f3\u306f\u3001\u3042\u308b\u7a2e\u306e\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\uff08\u30d5\u30a7\u30e9\u30a4\u30c8\u7cfb\u30b9\u30c6 \u30f3\u30ec\u30b9\u92fc\u306a\u3069\uff09\u3092\u5f15\u304d\u4ed8\u3051\u308b\u3053\u3068\u304c\u3042\u308b\u304c\u3001\u305d\u306e\u69cb\u9020 \u3084\u6027\u80fd\u3092\u640d\u306a\u3046\u3053\u3068\u306f\u306a\u3044\u3002<\/p><h3 class=\"wp-block-heading\">\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u3092\u78c1\u5316\u3059\u308b\u65b9\u6cd5<\/h3><p class=\"wp-block-paragraph\">\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u3092\u78c1\u5316\u3059\u308b\u306b\u306f\u3001\u5f37\u3044\u78c1\u5834\u306b\u3055\u3089 \u3057\u305f\u308a\u3001\u5f37\u529b\u306a\u78c1\u77f3\u3067\u3053\u3059\u3063\u305f\u308a\u3059\u308b\u3002\u30de\u30eb\u30c6\u30f3\u30b5\u30a4\u30c8\u7cfb\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306a\u3069\u3001\u30b9\u30c6\u30f3\u30ec \u30b9\u92fc\u306e\u7a2e\u985e\u306b\u3088\u3063\u3066\u306f\u3001\u78c1\u5316\u3057\u3084\u3059\u3044\u3082\u306e\u3082\u3042\u308b\u3002<\/p><h3 class=\"wp-block-heading\">\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u304b\u3089\u78c1\u6c17\u3092\u9664\u53bb\u3059\u308b\u306b\u306f\uff1f<\/h3><p class=\"wp-block-paragraph\">\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u304b\u3089\u78c1\u6027\u3092\u53d6\u308a\u9664\u304f\u306b\u306f\u3001\u30ad\u30e5\u30ea\u30fc\u70b9\u3092\u8d85 \u3048\u308b\u6e29\u5ea6\u307e\u3067\u52a0\u71b1\u3057\u3001\u305d\u306e\u5f8c\u51b7\u5374\u3059\u308c\u3070\u3088\u3044\u3002\u30ad\u30e5\u30ea\u30fc\u70b9\u3068\u306f\u3001\u6750\u6599\u304c\u78c1\u6027\u3092\u5931\u3046\u6e29\u5ea6\u3067\u3042\u308b\u3002\u3082\u30461\u3064\u306e\u65b9\u6cd5\u306f\u3001\u5f90\u3005\u306b\u5f37\u5ea6\u304c\u4f4e\u4e0b\u3059\u308b\u4ea4\u756a\u78c1\u5834\u3092\u767a\u751f\u3055\u305b\u3001\u92fc\u3092\u6d88\u78c1\u3059\u308b\u30c7\u30ac\u30a6\u30b5\u30fc\u3092\u4f7f\u7528\u3059\u308b\u3053\u3068\u3067\u3042\u308b\u3002<\/p><h3 class=\"wp-block-heading\">\u98df\u54c1\u7528\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u78c1\u6027\u3092\u6301\u3064\u304b\uff1f<\/h3><p class=\"wp-block-paragraph\">304\u3084316\u306e\u3088\u3046\u306a\u98df\u54c1\u7528\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u3001\u51b7\u9593\u52a0\u5de5\u306b\u3088\u308a\u308f\u305a\u304b\u306a\u78c1\u6027\u304c\u751f\u3058\u308b\u3053\u3068\u306f\u3042\u308b\u304c\u3001\u4e00\u822c\u306b\u78c1\u6027\u3092\u6301\u305f\u306a\u3044\u3002<\/p><h3 class=\"wp-block-heading\">\u3059\u3079\u3066\u306e400\u30b7\u30ea\u30fc\u30ba\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u78c1\u6027\u3067\u3059\u304b\uff1f<\/h3><p class=\"wp-block-paragraph\">\u306f\u3044\u3001400\u30b7\u30ea\u30fc\u30ba\u306e\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u3059\u3079\u3066\u78c1\u6027\u304c\u3042\u308a\u307e\u3059\u3002\u4e00\u822c\u7684\u306a\u30b0\u30ec\u30fc\u30c9\u306f\u6b21\u306e\u3068\u304a\u308a\u3067\u3059\u3002 <a href=\"https:\/\/steelprogroup.com\/ja\/stainless-steel\/grades\/grade-410\/\">410<\/a>, <a href=\"https:\/\/steelprogroup.com\/ja\/stainless-steel\/grades\/grade-420\/\">420<\/a>\u305d\u3057\u3066 <a href=\"https:\/\/steelprogroup.com\/ja\/stainless-steel\/grades\/grade-430\/\">430<\/a>.<\/p><h2 class=\"wp-block-heading\">\u307e\u3068\u3081\u3068\u3055\u3089\u306b<\/h2><p class=\"wp-block-paragraph\">\u3053\u306e\u8a18\u4e8b\u3067\u306f\u3001\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u304c\u78c1\u6027\u3092\u6301\u3064\u7406\u7531\u3001\u78c1\u6027\u306b\u5f71\u97ff\u3092\u4e0e\u3048\u308b\u3082\u306e\u3001\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u7a2e\u985e\u3084\u7b49\u7d1a\u304c\u78c1\u6027\u3092\u6301\u3064\u304b\u3069\u3046\u304b\u306a\u3069\u3001\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306e\u78c1\u6c17\u7279\u6027\u306b\u3064\u3044\u3066\u7c21\u5358\u306b\u8aac\u660e\u3057\u307e\u3059\u3002\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u3084\u305d\u306e\u4ed6\u306e\u92fc\u7a2e\u306b\u3064\u3044\u3066\u8a73\u3057\u304f\u77e5\u308a\u305f\u3044\u65b9\u306f\u3001\u4ee5\u4e0b\u3092\u3054\u89a7\u304f\u3060\u3055\u3044\u3002 <a href=\"https:\/\/steelprogroup.com\/ja\/blog\/\">\u30d6\u30ed\u30b0<\/a> \u307e\u305f\u306f <a href=\"https:\/\/steelprogroup.com\/ja\/contact-us\/\">\u91d1\u5c5e\u5c02\u9580\u5bb6\u3078\u306e\u304a\u554f\u3044\u5408\u308f\u305b<\/a>.<\/p><p class=\"wp-block-paragraph\">\u7279\u6b8a\u92fc\u306e\u30c8\u30c3\u30d7\u30e1\u30fc\u30ab\u30fc\u304a\u3088\u3073\u30bd\u30ea\u30e5\u30fc\u30b7\u30e7\u30f3\u30d7\u30ed\u30d0\u30a4\u30c0\u30fc\u3068\u3057\u3066\u3001100%\u306e\u54c1\u8cea\u4fdd\u8a3c\u3068\u3068\u3082\u306b\u3001\u591a\u696d\u7a2e\u306b\u308f\u305f\u308b\u30a2\u30d7\u30ea\u30b1\u30fc\u30b7\u30e7\u30f3\u30bd\u30ea\u30e5\u30fc\u30b7\u30e7\u30f3\u3068\u30ab\u30b9\u30bf\u30de\u30a4\u30ba\u3055\u308c\u305f\u30b5\u30fc\u30d3\u30b9\u3092\u63d0\u4f9b\u3057\u3001\u304a\u5ba2\u69d8\u3068\u3068\u3082\u306b\u6210\u9577\u3059\u308b\u3053\u3068\u3092\u304a\u7d04\u675f\u3057\u307e\u3059\u3002\u8a2a\u554f <a href=\"https:\/\/steelprogroup.com\/ja\">\u30a6\u30a7\u30d6\u30b5\u30a4\u30c8<\/a> \u307e\u305f\u306f <a href=\"https:\/\/steelprogroup.com\/ja\/contact-us\/\">\u898b\u7a4d\u3082\u308a\u3092\u9001\u308b<\/a>\u6298\u308a\u8fd4\u3057\u3054\u9023\u7d61\u3044\u305f\u3057\u307e\u3059\uff01<br><\/p>","protected":false},"excerpt":{"rendered":"<p>\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u306f\u4eca\u65e5\u3067\u306f\u76ee\u65b0\u3057\u3044\u3082\u306e\u3067\u306f\u3042\u308a\u307e\u305b\u3093\u3002\u6628\u6669\u3001\u30b9\u30c6\u30f3\u30ec\u30b9\u92fc\u88fd\u306e\u8abf\u7406\u5668\u5177\u3092\u4f7f\u3063\u3066\u5915\u98df\u3092\u4f5c\u3063\u305f\u3070\u304b\u308a\u304b\u3082\u3057\u308c\u307e\u305b\u3093\u3002 [\u2026]<\/p>","protected":false},"author":1,"featured_media":9892,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"_eb_attr":"","rank_math_lock_modified_date":false,"site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"categories":[4202,112],"tags":[],"class_list":["post-9889","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-properties","category-stainless-steel"],"acf":[],"_links":{"self":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts\/9889","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/comments?post=9889"}],"version-history":[{"count":0,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/posts\/9889\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/media\/9892"}],"wp:attachment":[{"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/media?parent=9889"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/categories?post=9889"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/steelprogroup.com\/ja\/wp-json\/wp\/v2\/tags?post=9889"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}