{"id":5220,"date":"2024-07-09T02:47:02","date_gmt":"2024-07-09T02:47:02","guid":{"rendered":"http:\/\/35.162.249.169\/?page_id=5220"},"modified":"2024-11-19T18:23:50","modified_gmt":"2024-11-19T10:23:50","slug":"alloy-steel","status":"publish","type":"page","link":"https:\/\/steelprogroup.com\/ru\/alloy-steel\/","title":{"rendered":"\u041b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u0430\u044f \u0441\u0442\u0430\u043b\u044c"},"content":{"rendered":"<div data-elementor-type=\"wp-page\" data-elementor-id=\"5220\" class=\"elementor elementor-5220\" data-elementor-post-type=\"page\">\n\t\t\t\t<div class=\"elementor-element elementor-element-623df3f7 e-flex e-con-boxed e-con e-parent\" data-id=\"623df3f7\" data-element_type=\"container\" data-settings=\"{&quot;background_background&quot;:&quot;classic&quot;}\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t<div class=\"elementor-element elementor-element-6b6ce14f e-con-full e-flex e-con e-child\" data-id=\"6b6ce14f\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-59604b93 elementor-widget elementor-widget-heading\" data-id=\"59604b93\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t<h1 class=\"elementor-heading-title elementor-size-default\">\u041b\u0415\u0413\u0418\u0420\u041e\u0412\u0410\u041d\u041d\u0410\u042f \u0421\u0422\u0410\u041b\u042c<\/h1>\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-3a979877 elementor-widget elementor-widget-heading\" data-id=\"3a979877\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t<h3 class=\"elementor-heading-title elementor-size-default\"><span>\u041f\u0440\u0435\u0432\u043e\u0441\u0445\u043e\u0434\u043d\u0430\u044f \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c. \u0423\u0441\u0442\u043e\u0439\u0447\u0438\u0432\u043e\u0441\u0442\u044c \u043a \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u0438. \u0423\u043b\u0443\u0447\u0448\u0438\u0442\u0435 \u0441\u0432\u043e\u0438 \u043f\u0440\u043e\u0435\u043a\u0442\u044b \u0441 \u043f\u043e\u043c\u043e\u0449\u044c\u044e \u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u043e\u0439 \u0441\u0442\u0430\u043b\u0438.<\/span>\n<\/h3>\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-5cf2823e elementor-align-center elementor-widget elementor-widget-button\" data-id=\"5cf2823e\" data-element_type=\"widget\" data-widget_type=\"button.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t<a class=\"elementor-button elementor-button-link elementor-size-sm\" href=\"#elementor-action:action=popup:open&settings=eyJpZCI6IjM5NTEiLCJ0b2dnbGUiOmZhbHNlfQ==\">\n\t\t\t\t\t\t<span class=\"elementor-button-content-wrapper\">\n\t\t\t\t\t\t<span class=\"elementor-button-icon\">\n\t\t\t\t<svg aria-hidden=\"true\" class=\"e-font-icon-svg e-fas-long-arrow-alt-right\" viewbox=\"0 0 448 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M313.941 216H12c-6.627 0-12 5.373-12 12v56c0 6.627 5.373 12 12 12h301.941v46.059c0 21.382 25.851 32.09 40.971 16.971l86.059-86.059c9.373-9.373 9.373-24.569 0-33.941l-86.059-86.059c-15.119-15.119-40.971-4.411-40.971 16.971V216z\"><\/path><\/svg>\t\t\t<\/span>\n\t\t\t\t\t\t\t\t\t<span class=\"elementor-button-text\">\u0421\u0412\u042f\u0416\u0418\u0422\u0415\u0421\u042c \u0421 \u041d\u0410\u041c\u0418<\/span>\n\t\t\t\t\t<\/span>\n\t\t\t\t\t<\/a>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-4e363d96 e-flex e-con-boxed e-con e-parent\" data-id=\"4e363d96\" data-element_type=\"container\" data-settings=\"{&quot;background_background&quot;:&quot;classic&quot;}\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t<div class=\"elementor-element elementor-element-aaf759f e-con-full e-flex e-con e-child\" data-id=\"aaf759f\" data-element_type=\"container\">\n\t\t<div class=\"elementor-element elementor-element-4a88f1a1 e-con-full e-flex e-con e-child\" data-id=\"4a88f1a1\" data-element_type=\"container\" data-settings=\"{&quot;background_background&quot;:&quot;classic&quot;}\">\n\t\t\t\t<div class=\"elementor-element elementor-element-e950e5c eael-infobox-content-align--center eael-infobox-icon-bg-shape-none eael-infobox-icon-hover-bg-shape-none elementor-widget elementor-widget-eael-info-box\" data-id=\"e950e5c\" data-element_type=\"widget\" data-widget_type=\"eael-info-box.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t        <div class=\"eael-infobox\">\n\t            <div class=\"infobox-icon eael-icon-only\">\n\n            \n                            <div class=\"infobox-icon-wrap\">\n                    <svg aria-hidden=\"true\" class=\"e-font-icon-svg e-fas-building\" viewbox=\"0 0 448 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M436 480h-20V24c0-13.255-10.745-24-24-24H56C42.745 0 32 10.745 32 24v456H12c-6.627 0-12 5.373-12 12v20h448v-20c0-6.627-5.373-12-12-12zM128 76c0-6.627 5.373-12 12-12h40c6.627 0 12 5.373 12 12v40c0 6.627-5.373 12-12 12h-40c-6.627 0-12-5.373-12-12V76zm0 96c0-6.627 5.373-12 12-12h40c6.627 0 12 5.373 12 12v40c0 6.627-5.373 12-12 12h-40c-6.627 0-12-5.373-12-12v-40zm52 148h-40c-6.627 0-12-5.373-12-12v-40c0-6.627 5.373-12 12-12h40c6.627 0 12 5.373 12 12v40c0 6.627-5.373 12-12 12zm76 160h-64v-84c0-6.627 5.373-12 12-12h40c6.627 0 12 5.373 12 12v84zm64-172c0 6.627-5.373 12-12 12h-40c-6.627 0-12-5.373-12-12v-40c0-6.627 5.373-12 12-12h40c6.627 0 12 5.373 12 12v40zm0-96c0 6.627-5.373 12-12 12h-40c-6.627 0-12-5.373-12-12v-40c0-6.627 5.373-12 12-12h40c6.627 0 12 5.373 12 12v40zm0-96c0 6.627-5.373 12-12 12h-40c-6.627 0-12-5.373-12-12V76c0-6.627 5.373-12 12-12h40c6.627 0 12 5.373 12 12v40z\"><\/path><\/svg>                <\/div>\n            \n            \n        <\/div>\n            <div class=\"infobox-content eael-icon-only\">\n            <h3 class=\"title\">\u041f\u0440\u0435\u0438\u043c\u0443\u0449\u0435\u0441\u0442\u0432\u0430 \u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u043e\u0439 \u0441\u0442\u0430\u043b\u0438<\/h3><div><div><span class=\"text-only\">\u0423\u0437\u043d\u0430\u0439\u0442\u0435 \u043e \u043f\u0440\u0435\u0438\u043c\u0443\u0449\u0435\u0441\u0442\u0432\u0430\u0445 \u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u043e\u0439 \u0441\u0442\u0430\u043b\u0438<\/span><\/div><\/div>        <div class=\"infobox-button\">\n            <a class=\"eael-infobox-button\" href=\"#1\">\n                                <span class=\"infobox-button-text\">\u0443\u0437\u043d\u0430\u0442\u044c \u0431\u043e\u043b\u044c\u0448\u0435<\/span>\n                                                            <svg aria-hidden=\"true\" class=\"eael_infobox_button_icon_right e-font-icon-svg e-fas-arrow-right\" viewbox=\"0 0 448 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M190.5 66.9l22.2-22.2c9.4-9.4 24.6-9.4 33.9 0L441 239c9.4 9.4 9.4 24.6 0 33.9L246.6 467.3c-9.4 9.4-24.6 9.4-33.9 0l-22.2-22.2c-9.5-9.5-9.3-25 .4-34.3L311.4 296H24c-13.3 0-24-10.7-24-24v-32c0-13.3 10.7-24 24-24h287.4L190.9 101.2c-9.8-9.3-10-24.8-.4-34.3z\"><\/path><\/svg>                                                <\/a>\n        <\/div>\n            <\/div>\n            <\/div>\n\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-3e0ee9ec e-con-full e-flex e-con e-child\" data-id=\"3e0ee9ec\" data-element_type=\"container\" data-settings=\"{&quot;background_background&quot;:&quot;classic&quot;}\">\n\t\t\t\t<div class=\"elementor-element elementor-element-3ed7a2ac eael-infobox-content-align--center eael-infobox-icon-bg-shape-none eael-infobox-icon-hover-bg-shape-none elementor-widget elementor-widget-eael-info-box\" data-id=\"3ed7a2ac\" data-element_type=\"widget\" data-widget_type=\"eael-info-box.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t        <div class=\"eael-infobox\">\n\t            <div class=\"infobox-icon eael-icon-only\">\n\n            \n                            <div class=\"infobox-icon-wrap\">\n                    <svg aria-hidden=\"true\" class=\"e-font-icon-svg e-fas-building\" viewbox=\"0 0 448 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M436 480h-20V24c0-13.255-10.745-24-24-24H56C42.745 0 32 10.745 32 24v456H12c-6.627 0-12 5.373-12 12v20h448v-20c0-6.627-5.373-12-12-12zM128 76c0-6.627 5.373-12 12-12h40c6.627 0 12 5.373 12 12v40c0 6.627-5.373 12-12 12h-40c-6.627 0-12-5.373-12-12V76zm0 96c0-6.627 5.373-12 12-12h40c6.627 0 12 5.373 12 12v40c0 6.627-5.373 12-12 12h-40c-6.627 0-12-5.373-12-12v-40zm52 148h-40c-6.627 0-12-5.373-12-12v-40c0-6.627 5.373-12 12-12h40c6.627 0 12 5.373 12 12v40c0 6.627-5.373 12-12 12zm76 160h-64v-84c0-6.627 5.373-12 12-12h40c6.627 0 12 5.373 12 12v84zm64-172c0 6.627-5.373 12-12 12h-40c-6.627 0-12-5.373-12-12v-40c0-6.627 5.373-12 12-12h40c6.627 0 12 5.373 12 12v40zm0-96c0 6.627-5.373 12-12 12h-40c-6.627 0-12-5.373-12-12v-40c0-6.627 5.373-12 12-12h40c6.627 0 12 5.373 12 12v40zm0-96c0 6.627-5.373 12-12 12h-40c-6.627 0-12-5.373-12-12V76c0-6.627 5.373-12 12-12h40c6.627 0 12 5.373 12 12v40z\"><\/path><\/svg>                <\/div>\n            \n            \n        <\/div>\n            <div class=\"infobox-content eael-icon-only\">\n            <h3 class=\"title\">\u0422\u0438\u043f\u044b \u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u043e\u0439 \u0441\u0442\u0430\u043b\u0438<\/h3><div><div><span class=\"text-only\">\u0423\u0437\u043d\u0430\u0439\u0442\u0435 \u043e \u0442\u0438\u043f\u0435 \u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u043e\u0439 \u0441\u0442\u0430\u043b\u0438<\/span><\/div><\/div>        <div class=\"infobox-button\">\n            <a class=\"eael-infobox-button\" href=\"#2\">\n                                <span class=\"infobox-button-text\">\u0443\u0437\u043d\u0430\u0442\u044c \u0431\u043e\u043b\u044c\u0448\u0435<\/span>\n                                                            <svg aria-hidden=\"true\" class=\"eael_infobox_button_icon_right e-font-icon-svg e-fas-arrow-right\" viewbox=\"0 0 448 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M190.5 66.9l22.2-22.2c9.4-9.4 24.6-9.4 33.9 0L441 239c9.4 9.4 9.4 24.6 0 33.9L246.6 467.3c-9.4 9.4-24.6 9.4-33.9 0l-22.2-22.2c-9.5-9.5-9.3-25 .4-34.3L311.4 296H24c-13.3 0-24-10.7-24-24v-32c0-13.3 10.7-24 24-24h287.4L190.9 101.2c-9.8-9.3-10-24.8-.4-34.3z\"><\/path><\/svg>                                                <\/a>\n        <\/div>\n            <\/div>\n            <\/div>\n\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-5aa3b0f4 e-con-full e-flex e-con e-child\" data-id=\"5aa3b0f4\" data-element_type=\"container\" data-settings=\"{&quot;background_background&quot;:&quot;classic&quot;}\">\n\t\t\t\t<div class=\"elementor-element elementor-element-6caf9d82 eael-infobox-content-align--center eael-infobox-icon-bg-shape-none eael-infobox-icon-hover-bg-shape-none elementor-widget elementor-widget-eael-info-box\" data-id=\"6caf9d82\" data-element_type=\"widget\" data-widget_type=\"eael-info-box.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t        <div class=\"eael-infobox\">\n\t            <div class=\"infobox-icon eael-icon-only\">\n\n            \n                            <div class=\"infobox-icon-wrap\">\n                    <svg aria-hidden=\"true\" class=\"e-font-icon-svg e-fas-building\" viewbox=\"0 0 448 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M436 480h-20V24c0-13.255-10.745-24-24-24H56C42.745 0 32 10.745 32 24v456H12c-6.627 0-12 5.373-12 12v20h448v-20c0-6.627-5.373-12-12-12zM128 76c0-6.627 5.373-12 12-12h40c6.627 0 12 5.373 12 12v40c0 6.627-5.373 12-12 12h-40c-6.627 0-12-5.373-12-12V76zm0 96c0-6.627 5.373-12 12-12h40c6.627 0 12 5.373 12 12v40c0 6.627-5.373 12-12 12h-40c-6.627 0-12-5.373-12-12v-40zm52 148h-40c-6.627 0-12-5.373-12-12v-40c0-6.627 5.373-12 12-12h40c6.627 0 12 5.373 12 12v40c0 6.627-5.373 12-12 12zm76 160h-64v-84c0-6.627 5.373-12 12-12h40c6.627 0 12 5.373 12 12v84zm64-172c0 6.627-5.373 12-12 12h-40c-6.627 0-12-5.373-12-12v-40c0-6.627 5.373-12 12-12h40c6.627 0 12 5.373 12 12v40zm0-96c0 6.627-5.373 12-12 12h-40c-6.627 0-12-5.373-12-12v-40c0-6.627 5.373-12 12-12h40c6.627 0 12 5.373 12 12v40zm0-96c0 6.627-5.373 12-12 12h-40c-6.627 0-12-5.373-12-12V76c0-6.627 5.373-12 12-12h40c6.627 0 12 5.373 12 12v40z\"><\/path><\/svg>                <\/div>\n            \n            \n        <\/div>\n            <div class=\"infobox-content eael-icon-only\">\n            <h3 class=\"title\">\u041e\u0442\u0440\u0430\u0441\u043b\u0438 \u0438 \u043f\u0440\u0438\u043b\u043e\u0436\u0435\u043d\u0438\u044f<\/h3><div><div><span class=\"text-only\">\u0418\u0437\u0443\u0447\u0438\u0442\u0435 \u043e\u0442\u0440\u0430\u0441\u043b\u0438, \u043f\u043e\u043b\u0443\u0447\u0430\u044e\u0449\u0438\u0435 \u0432\u044b\u0433\u043e\u0434\u0443 \u043e\u0442 \u0438\u0441\u043f\u043e\u043b\u044c\u0437\u043e\u0432\u0430\u043d\u0438\u044f \u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u043e\u0439 \u0441\u0442\u0430\u043b\u0438<\/span><\/div><\/div>        <div class=\"infobox-button\">\n            <a class=\"eael-infobox-button\" href=\"#3\">\n                                <span class=\"infobox-button-text\">\u0443\u0437\u043d\u0430\u0442\u044c \u0431\u043e\u043b\u044c\u0448\u0435<\/span>\n                                                            <svg aria-hidden=\"true\" class=\"eael_infobox_button_icon_right e-font-icon-svg e-fas-arrow-right\" viewbox=\"0 0 448 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M190.5 66.9l22.2-22.2c9.4-9.4 24.6-9.4 33.9 0L441 239c9.4 9.4 9.4 24.6 0 33.9L246.6 467.3c-9.4 9.4-24.6 9.4-33.9 0l-22.2-22.2c-9.5-9.5-9.3-25 .4-34.3L311.4 296H24c-13.3 0-24-10.7-24-24v-32c0-13.3 10.7-24 24-24h287.4L190.9 101.2c-9.8-9.3-10-24.8-.4-34.3z\"><\/path><\/svg>                                                <\/a>\n        <\/div>\n            <\/div>\n            <\/div>\n\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-4a492e12 e-con-full e-flex e-con e-child\" data-id=\"4a492e12\" data-element_type=\"container\" data-settings=\"{&quot;background_background&quot;:&quot;classic&quot;}\">\n\t\t\t\t<div class=\"elementor-element elementor-element-79e57cc9 eael-infobox-content-align--center eael-infobox-icon-bg-shape-none eael-infobox-icon-hover-bg-shape-none elementor-widget elementor-widget-eael-info-box\" data-id=\"79e57cc9\" data-element_type=\"widget\" data-widget_type=\"eael-info-box.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t        <div class=\"eael-infobox\">\n\t            <div class=\"infobox-icon eael-icon-only\">\n\n            \n                            <div class=\"infobox-icon-wrap\">\n                    <svg aria-hidden=\"true\" class=\"e-font-icon-svg e-fas-building\" viewbox=\"0 0 448 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M436 480h-20V24c0-13.255-10.745-24-24-24H56C42.745 0 32 10.745 32 24v456H12c-6.627 0-12 5.373-12 12v20h448v-20c0-6.627-5.373-12-12-12zM128 76c0-6.627 5.373-12 12-12h40c6.627 0 12 5.373 12 12v40c0 6.627-5.373 12-12 12h-40c-6.627 0-12-5.373-12-12V76zm0 96c0-6.627 5.373-12 12-12h40c6.627 0 12 5.373 12 12v40c0 6.627-5.373 12-12 12h-40c-6.627 0-12-5.373-12-12v-40zm52 148h-40c-6.627 0-12-5.373-12-12v-40c0-6.627 5.373-12 12-12h40c6.627 0 12 5.373 12 12v40c0 6.627-5.373 12-12 12zm76 160h-64v-84c0-6.627 5.373-12 12-12h40c6.627 0 12 5.373 12 12v84zm64-172c0 6.627-5.373 12-12 12h-40c-6.627 0-12-5.373-12-12v-40c0-6.627 5.373-12 12-12h40c6.627 0 12 5.373 12 12v40zm0-96c0 6.627-5.373 12-12 12h-40c-6.627 0-12-5.373-12-12v-40c0-6.627 5.373-12 12-12h40c6.627 0 12 5.373 12 12v40zm0-96c0 6.627-5.373 12-12 12h-40c-6.627 0-12-5.373-12-12V76c0-6.627 5.373-12 12-12h40c6.627 0 12 5.373 12 12v40z\"><\/path><\/svg>                <\/div>\n            \n            \n        <\/div>\n            <div class=\"infobox-content eael-icon-only\">\n            <h3 class=\"title\">\u0420\u0430\u0437\u043c\u0435\u0440\u044b \u0438 \u0441\u0432\u043e\u0439\u0441\u0442\u0432\u0430<\/h3><div><div><span class=\"text-only\">\u0423\u0437\u043d\u0430\u0439\u0442\u0435 \u043e \u0440\u0430\u0437\u043c\u0435\u0440\u0430\u0445 \u0438 \u0441\u0432\u043e\u0439\u0441\u0442\u0432\u0430\u0445<\/span><\/div><\/div>        <div class=\"infobox-button\">\n            <a class=\"eael-infobox-button\" href=\"#4\">\n                                <span class=\"infobox-button-text\">\u0443\u0437\u043d\u0430\u0442\u044c \u0431\u043e\u043b\u044c\u0448\u0435<\/span>\n                                                            <svg aria-hidden=\"true\" class=\"eael_infobox_button_icon_right e-font-icon-svg e-fas-arrow-right\" viewbox=\"0 0 448 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M190.5 66.9l22.2-22.2c9.4-9.4 24.6-9.4 33.9 0L441 239c9.4 9.4 9.4 24.6 0 33.9L246.6 467.3c-9.4 9.4-24.6 9.4-33.9 0l-22.2-22.2c-9.5-9.5-9.3-25 .4-34.3L311.4 296H24c-13.3 0-24-10.7-24-24v-32c0-13.3 10.7-24 24-24h287.4L190.9 101.2c-9.8-9.3-10-24.8-.4-34.3z\"><\/path><\/svg>                                                <\/a>\n        <\/div>\n            <\/div>\n            <\/div>\n\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-101972d8 e-flex e-con-boxed e-con e-parent\" data-id=\"101972d8\" data-element_type=\"container\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t<div class=\"elementor-element elementor-element-25dcdd05 e-con-full e-flex e-con e-child\" data-id=\"25dcdd05\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-688bc1ea elementor-widget elementor-widget-heading\" data-id=\"688bc1ea\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">\u0412\u0432\u0435\u0434\u0435\u043d\u0438\u0435 \u0432 \u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u0443\u044e \u0441\u0442\u0430\u043b\u044c<\/h2>\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-58d68b2 elementor-widget elementor-widget-text-editor\" data-id=\"58d68b2\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<!-- x-tinymce\/html -->\n\n\u041b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u2014 \u044d\u0442\u043e \u0442\u0438\u043f \u0441\u0442\u0430\u043b\u0438, \u0432 \u0441\u043e\u0441\u0442\u0430\u0432 \u043a\u043e\u0442\u043e\u0440\u043e\u0439 \u0432\u0445\u043e\u0434\u044f\u0442 \u0440\u0430\u0437\u043b\u0438\u0447\u043d\u044b\u0435 \u043b\u0435\u0433\u0438\u0440\u0443\u044e\u0449\u0438\u0435 \u044d\u043b\u0435\u043c\u0435\u043d\u0442\u044b, \u0442\u0430\u043a\u0438\u0435 \u043a\u0430\u043a \u0445\u0440\u043e\u043c, \u043d\u0438\u043a\u0435\u043b\u044c, \u043c\u043e\u043b\u0438\u0431\u0434\u0435\u043d, \u0432\u0430\u043d\u0430\u0434\u0438\u0439, \u043c\u0430\u0440\u0433\u0430\u043d\u0435\u0446 \u0438 \u043a\u0440\u0435\u043c\u043d\u0438\u0439, \u0434\u043b\u044f \u0443\u043b\u0443\u0447\u0448\u0435\u043d\u0438\u044f \u0435\u0435 \u043c\u0435\u0445\u0430\u043d\u0438\u0447\u0435\u0441\u043a\u0438\u0445 \u0441\u0432\u043e\u0439\u0441\u0442\u0432 \u0438 \u044d\u043a\u0441\u043f\u043b\u0443\u0430\u0442\u0430\u0446\u0438\u043e\u043d\u043d\u044b\u0445 \u0445\u0430\u0440\u0430\u043a\u0442\u0435\u0440\u0438\u0441\u0442\u0438\u043a. \u0421\u043e\u0434\u0435\u0440\u0436\u0430\u043d\u0438\u0435 \u0443\u0433\u043b\u0435\u0440\u043e\u0434\u0430 \u0432 \u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u043e\u0439 \u0441\u0442\u0430\u043b\u0438 \u043c\u043e\u0436\u0435\u0442 \u0432\u0430\u0440\u044c\u0438\u0440\u043e\u0432\u0430\u0442\u044c\u0441\u044f, \u0447\u0442\u043e \u043f\u043e\u0437\u0432\u043e\u043b\u044f\u0435\u0442 \u0438\u0441\u043f\u043e\u043b\u044c\u0437\u043e\u0432\u0430\u0442\u044c \u0448\u0438\u0440\u043e\u043a\u0438\u0439 \u0441\u043f\u0435\u043a\u0442\u0440 \u0445\u0430\u0440\u0430\u043a\u0442\u0435\u0440\u0438\u0441\u0442\u0438\u043a, \u0430\u0434\u0430\u043f\u0442\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u044b\u0445 \u043a \u043a\u043e\u043d\u043a\u0440\u0435\u0442\u043d\u044b\u043c \u0441\u0444\u0435\u0440\u0430\u043c \u043f\u0440\u0438\u043c\u0435\u043d\u0435\u043d\u0438\u044f. \u041b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u043e\u0431\u044b\u0447\u043d\u043e \u0438\u043c\u0435\u0435\u0442 \u043f\u0440\u0435\u0434\u0435\u043b \u0442\u0435\u043a\u0443\u0447\u0435\u0441\u0442\u0438 \u043e\u0442 250 \u0434\u043e 550 \u041c\u041f\u0430 (\u043e\u0442 36,26 \u0434\u043e 79,77 ksi) \u0438 \u043f\u0440\u0435\u0434\u0435\u043b \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u0438 \u043d\u0430 \u0440\u0430\u0441\u0442\u044f\u0436\u0435\u043d\u0438\u0435 \u043e\u0442 600 \u0434\u043e 1500 \u041c\u041f\u0430 (\u043e\u0442 87,02 \u0434\u043e 217,56 ksi). \u041e\u043d\u0430 \u0438\u0437\u0432\u0435\u0441\u0442\u043d\u0430 \u0441\u0432\u043e\u0435\u0439 \u043f\u0440\u0435\u0432\u043e\u0441\u0445\u043e\u0434\u043d\u043e\u0439 \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c\u044e, \u0442\u0432\u0435\u0440\u0434\u043e\u0441\u0442\u044c\u044e, \u0432\u044f\u0437\u043a\u043e\u0441\u0442\u044c\u044e, \u043f\u043b\u0430\u0441\u0442\u0438\u0447\u043d\u043e\u0441\u0442\u044c\u044e \u0438 \u0432\u044b\u0441\u043e\u043a\u043e\u0442\u0435\u043c\u043f\u0435\u0440\u0430\u0442\u0443\u0440\u043d\u044b\u043c\u0438 \u0445\u0430\u0440\u0430\u043a\u0442\u0435\u0440\u0438\u0441\u0442\u0438\u043a\u0430\u043c\u0438. \u0421\u043e\u0441\u0442\u0430\u0432 \u0441\u0442\u0430\u043b\u0438 \u043c\u043e\u0436\u043d\u043e \u0440\u0435\u0433\u0443\u043b\u0438\u0440\u043e\u0432\u0430\u0442\u044c \u0441 \u043f\u043e\u043c\u043e\u0449\u044c\u044e \u043f\u0440\u043e\u0446\u0435\u0441\u0441\u043e\u0432 \u0442\u0435\u0440\u043c\u0438\u0447\u0435\u0441\u043a\u043e\u0439 \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0438, \u0447\u0442\u043e\u0431\u044b \u043f\u0440\u0435\u0432\u0440\u0430\u0442\u0438\u0442\u044c \u0435\u0435 \u0432 <a href=\"https:\/\/steelprogroup.com\/ru\/hot-rolled-steel\/\" style=\"color:#ec1c24;font-weight:500;\">\u0413\u043e\u0440\u044f\u0447\u0435\u043a\u0430\u0442\u0430\u043d\u0430\u044f \u0441\u0442\u0430\u043b\u044c<\/a>, \u043f\u043e\u0432\u044b\u0448\u0430\u044f \u0435\u0435 \u0437\u0430\u043a\u0430\u043b\u0438\u0432\u0430\u0435\u043c\u043e\u0441\u0442\u044c, \u0438\u0437\u043d\u043e\u0441\u043e\u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c \u0438 \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u0443\u044e \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c. \u041b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u0432\u044b\u0441\u043e\u043a\u043e \u0446\u0435\u043d\u0438\u0442\u0441\u044f \u043d\u0430 \u0440\u044b\u043d\u043a\u0435 \u0437\u0430 \u0435\u0435 \u0443\u043d\u0438\u0432\u0435\u0440\u0441\u0430\u043b\u044c\u043d\u043e\u0441\u0442\u044c \u0438 \u0443\u043b\u0443\u0447\u0448\u0435\u043d\u043d\u044b\u0435 \u0441\u0432\u043e\u0439\u0441\u0442\u0432\u0430, \u0447\u0442\u043e \u0434\u0435\u043b\u0430\u0435\u0442 \u0435\u0435 \u0438\u0434\u0435\u0430\u043b\u044c\u043d\u043e\u0439 \u0434\u043b\u044f \u0441\u043b\u043e\u0436\u043d\u044b\u0445 \u043f\u0440\u0438\u043c\u0435\u043d\u0435\u043d\u0438\u0439 \u0432 \u0442\u0430\u043a\u0438\u0445 \u043e\u0442\u0440\u0430\u0441\u043b\u044f\u0445, \u043a\u0430\u043a \u0430\u0432\u0442\u043e\u043c\u043e\u0431\u0438\u043b\u0435\u0441\u0442\u0440\u043e\u0435\u043d\u0438\u0435, \u0430\u044d\u0440\u043e\u043a\u043e\u0441\u043c\u0438\u0447\u0435\u0441\u043a\u0430\u044f \u043f\u0440\u043e\u043c\u044b\u0448\u043b\u0435\u043d\u043d\u043e\u0441\u0442\u044c, \u0441\u0442\u0440\u043e\u0438\u0442\u0435\u043b\u044c\u0441\u0442\u0432\u043e \u0438 \u043f\u0440\u043e\u0438\u0437\u0432\u043e\u0434\u0441\u0442\u0432\u043e.\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-7b7ddfef elementor-align-left elementor-widget elementor-widget-button\" data-id=\"7b7ddfef\" data-element_type=\"widget\" data-widget_type=\"button.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t<a class=\"elementor-button elementor-button-link elementor-size-sm\" href=\"#elementor-action:action=popup:open&settings=eyJpZCI6IjM5NTEiLCJ0b2dnbGUiOmZhbHNlfQ==\">\n\t\t\t\t\t\t<span class=\"elementor-button-content-wrapper\">\n\t\t\t\t\t\t<span class=\"elementor-button-icon\">\n\t\t\t\t<svg aria-hidden=\"true\" class=\"e-font-icon-svg e-fas-long-arrow-alt-right\" viewbox=\"0 0 448 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M313.941 216H12c-6.627 0-12 5.373-12 12v56c0 6.627 5.373 12 12 12h301.941v46.059c0 21.382 25.851 32.09 40.971 16.971l86.059-86.059c9.373-9.373 9.373-24.569 0-33.941l-86.059-86.059c-15.119-15.119-40.971-4.411-40.971 16.971V216z\"><\/path><\/svg>\t\t\t<\/span>\n\t\t\t\t\t\t\t\t\t<span class=\"elementor-button-text\">\u0417\u0410\u041f\u0420\u041e\u0421\u0418\u0422\u042c \u0426\u0415\u041d\u0423 <\/span>\n\t\t\t\t\t<\/span>\n\t\t\t\t\t<\/a>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-5438032c e-con-full e-flex e-con e-child\" data-id=\"5438032c\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-7b58dc05 elementor-widget elementor-widget-image\" data-id=\"7b58dc05\" data-element_type=\"widget\" data-widget_type=\"image.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t<img decoding=\"async\" src=\"https:\/\/steelprogroup.com\/wp-content\/uploads\/elementor\/thumbs\/alloy-steel-pipe-qx9ysqcq83lyfgd0e86k6u1g15hba4xd9gsmd5lglk.jpg\" title=\"\u0442\u0440\u0443\u0431\u0430 \u0438\u0437 \u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u043e\u0439 \u0441\u0442\u0430\u043b\u0438\" alt=\"\u0442\u0440\u0443\u0431\u0430 \u0438\u0437 \u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u043e\u0439 \u0441\u0442\u0430\u043b\u0438\" loading=\"lazy\" \/>\t\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-c2d1cc1 e-flex e-con-boxed e-con e-parent\" data-id=\"c2d1cc1\" data-element_type=\"container\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t\t\t<div class=\"elementor-element elementor-element-99e51d8 elementor-widget elementor-widget-menu-anchor\" data-id=\"99e51d8\" data-element_type=\"widget\" data-widget_type=\"menu-anchor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<div class=\"elementor-menu-anchor\" id=\"1\"><\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-143a325a e-con-full e-flex e-con e-parent\" data-id=\"143a325a\" data-element_type=\"container\">\n\t\t<div class=\"elementor-element elementor-element-6c787cbd e-flex e-con-boxed e-con e-child\" data-id=\"6c787cbd\" data-element_type=\"container\" data-settings=\"{&quot;background_background&quot;:&quot;classic&quot;}\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t<div class=\"elementor-element elementor-element-63f4357b e-con-full e-flex e-con e-child\" data-id=\"63f4357b\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-6c3c6279 elementor-widget elementor-widget-heading\" data-id=\"6c3c6279\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">\u041f\u0440\u0435\u0438\u043c\u0443\u0449\u0435\u0441\u0442\u0432\u0430 \u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u043e\u0439 \u0441\u0442\u0430\u043b\u0438<\/h2>\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-4b1ea040 elementor-widget elementor-widget-text-editor\" data-id=\"4b1ea040\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<div style=\"-webkit-font-smoothing: antialiased; text-rendering: optimizelegibility; font-size: 18px; font-weight: 400; letter-spacing: 0.2px; line-height: 30px; margin-bottom: 10px; list-style: none; position: relative;\"><p>\u041b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u0438\u043c\u0435\u0435\u0442 \u0440\u044f\u0434 \u0441\u0443\u0449\u0435\u0441\u0442\u0432\u0435\u043d\u043d\u044b\u0445 \u043f\u0440\u0435\u0438\u043c\u0443\u0449\u0435\u0441\u0442\u0432:<br \/><!-- x-tinymce\/html --><\/p><ul style=\"list-style: none; padding-left: 15px;\"><li><strong>\u041f\u0440\u0435\u0432\u043e\u0441\u0445\u043e\u0434\u043d\u0430\u044f \u0441\u0438\u043b\u0430:<\/strong> \u0423\u0441\u0438\u043b\u0435\u043d\u0430 \u043b\u0435\u0433\u0438\u0440\u0443\u044e\u0449\u0438\u043c\u0438 \u044d\u043b\u0435\u043c\u0435\u043d\u0442\u0430\u043c\u0438, \u043e\u0431\u0435\u0441\u043f\u0435\u0447\u0438\u0432\u0430\u044e\u0449\u0438\u043c\u0438 \u0431\u043e\u043b\u0435\u0435 \u0432\u044b\u0441\u043e\u043a\u0443\u044e \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c \u043f\u043e \u0441\u0440\u0430\u0432\u043d\u0435\u043d\u0438\u044e \u0441 \u0443\u0433\u043b\u0435\u0440\u043e\u0434\u0438\u0441\u0442\u043e\u0439 \u0441\u0442\u0430\u043b\u044c\u044e.<\/li><li><strong>\u041a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u0430\u044f \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c:<\/strong> \u041b\u0435\u0433\u0438\u0440\u0443\u044e\u0449\u0438\u0435 \u044d\u043b\u0435\u043c\u0435\u043d\u0442\u044b, \u0442\u0430\u043a\u0438\u0435 \u043a\u0430\u043a \u0445\u0440\u043e\u043c \u0438 \u043d\u0438\u043a\u0435\u043b\u044c, \u043f\u043e\u0432\u044b\u0448\u0430\u044e\u0442 \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u0443\u044e \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c, \u0447\u0442\u043e \u0434\u0435\u043b\u0430\u0435\u0442 \u0435\u0433\u043e \u043f\u0440\u0438\u0433\u043e\u0434\u043d\u044b\u043c \u0434\u043b\u044f \u044d\u043a\u0441\u043f\u043b\u0443\u0430\u0442\u0430\u0446\u0438\u0438 \u0432 \u0441\u0443\u0440\u043e\u0432\u044b\u0445 \u0443\u0441\u043b\u043e\u0432\u0438\u044f\u0445.<\/li><li><strong>\u0418\u0437\u043d\u043e\u0441\u043e\u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c:<\/strong> \u0422\u0430\u043a\u0438\u0435 \u044d\u043b\u0435\u043c\u0435\u043d\u0442\u044b, \u043a\u0430\u043a \u0432\u0430\u043d\u0430\u0434\u0438\u0439 \u0438 \u043c\u043e\u043b\u0438\u0431\u0434\u0435\u043d, \u043f\u043e\u0432\u044b\u0448\u0430\u044e\u0442 \u0438\u0437\u043d\u043e\u0441\u043e\u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c, \u043f\u0440\u043e\u0434\u043b\u0435\u0432\u0430\u044f \u0441\u0440\u043e\u043a \u0441\u043b\u0443\u0436\u0431\u044b \u0434\u0435\u0442\u0430\u043b\u0435\u0439.<\/li><li><strong>\u0422\u0435\u043f\u043b\u043e\u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c:<\/strong> \u0421\u043e\u0445\u0440\u0430\u043d\u044f\u0435\u0442 \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c \u0438 \u0442\u0432\u0435\u0440\u0434\u043e\u0441\u0442\u044c \u043f\u0440\u0438 \u0432\u044b\u0441\u043e\u043a\u0438\u0445 \u0442\u0435\u043c\u043f\u0435\u0440\u0430\u0442\u0443\u0440\u0430\u0445, \u0438\u0434\u0435\u0430\u043b\u044c\u043d\u043e \u043f\u043e\u0434\u0445\u043e\u0434\u0438\u0442 \u0434\u043b\u044f \u0432\u044b\u0441\u043e\u043a\u043e\u0442\u0435\u043c\u043f\u0435\u0440\u0430\u0442\u0443\u0440\u043d\u044b\u0445 \u043f\u0440\u0438\u043c\u0435\u043d\u0435\u043d\u0438\u0439.<\/li><li><strong>\u041f\u0440\u043e\u043a\u0430\u043b\u0438\u0432\u0430\u0435\u043c\u043e\u0441\u0442\u044c:<\/strong> \u041b\u0435\u0433\u0438\u0440\u0443\u044e\u0449\u0438\u0435 \u044d\u043b\u0435\u043c\u0435\u043d\u0442\u044b \u0443\u043b\u0443\u0447\u0448\u0430\u044e\u0442 \u043f\u0440\u043e\u043a\u0430\u043b\u0438\u0432\u0430\u0435\u043c\u043e\u0441\u0442\u044c, \u043e\u0431\u0435\u0441\u043f\u0435\u0447\u0438\u0432\u0430\u044f \u0431\u043e\u043b\u0435\u0435 \u0433\u043b\u0443\u0431\u043e\u043a\u0443\u044e \u0437\u0430\u043a\u0430\u043b\u043a\u0443 \u043f\u0440\u0438 \u0442\u0435\u0440\u043c\u0438\u0447\u0435\u0441\u043a\u043e\u0439 \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0435.<\/li><li><strong>\u0423\u043d\u0438\u0432\u0435\u0440\u0441\u0430\u043b\u044c\u043d\u043e\u0441\u0442\u044c:<\/strong> \u0414\u043e\u0441\u0442\u0443\u043f\u0435\u043d \u0432 \u0448\u0438\u0440\u043e\u043a\u043e\u043c \u0430\u0441\u0441\u043e\u0440\u0442\u0438\u043c\u0435\u043d\u0442\u0435 \u043c\u0430\u0440\u043e\u043a, \u0447\u0442\u043e \u0434\u0435\u043b\u0430\u0435\u0442 \u0435\u0433\u043e \u043f\u0440\u0438\u0433\u043e\u0434\u043d\u044b\u043c \u0434\u043b\u044f \u0440\u0430\u0437\u043d\u043e\u043e\u0431\u0440\u0430\u0437\u043d\u043e\u0433\u043e \u043f\u0440\u0438\u043c\u0435\u043d\u0435\u043d\u0438\u044f \u0432 \u0440\u0430\u0437\u043b\u0438\u0447\u043d\u044b\u0445 \u043e\u0442\u0440\u0430\u0441\u043b\u044f\u0445 \u043f\u0440\u043e\u043c\u044b\u0448\u043b\u0435\u043d\u043d\u043e\u0441\u0442\u0438.<\/li><li>\u00a0<\/li><\/ul><\/div>\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-46ad9d77 e-con-full e-flex e-con e-child\" data-id=\"46ad9d77\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-8788054 elementor-widget elementor-widget-image\" data-id=\"8788054\" data-element_type=\"widget\" data-widget_type=\"image.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t<img decoding=\"async\" src=\"https:\/\/steelprogroup.com\/wp-content\/uploads\/elementor\/thumbs\/alloy-steel-plate-scaled-qxa5zfhn6lpchg15n1j8jnkgo2qa6qek855jmfqus8.jpg\" title=\"\u043f\u043b\u0430\u0441\u0442\u0438\u043d\u0430 \u0438\u0437 \u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u043e\u0439 \u0441\u0442\u0430\u043b\u0438\" alt=\"\u043f\u043b\u0430\u0441\u0442\u0438\u043d\u0430 \u0438\u0437 \u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u043e\u0439 \u0441\u0442\u0430\u043b\u0438\" loading=\"lazy\" \/>\t\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-275507d e-flex e-con-boxed e-con e-parent\" data-id=\"275507d\" data-element_type=\"container\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t<div class=\"elementor-element elementor-element-efef143 e-con-full e-flex e-con e-child\" data-id=\"efef143\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-953c14c elementor-widget elementor-widget-menu-anchor\" data-id=\"953c14c\" data-element_type=\"widget\" data-widget_type=\"menu-anchor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<div class=\"elementor-menu-anchor\" id=\"2\"><\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-20128eb e-flex e-con-boxed e-con e-parent\" data-id=\"20128eb\" data-element_type=\"container\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t<div class=\"elementor-element elementor-element-6ee6693d e-con-full e-flex e-con e-child\" data-id=\"6ee6693d\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-6c52482e elementor-widget elementor-widget-heading\" data-id=\"6c52482e\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">\u0422\u0438\u043f\u044b \u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u043e\u0439 \u0441\u0442\u0430\u043b\u0438<\/h2>\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-68b4c7b4 elementor-align-left elementor-widget elementor-widget-button\" data-id=\"68b4c7b4\" data-element_type=\"widget\" data-widget_type=\"button.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t<a class=\"elementor-button elementor-button-link elementor-size-sm\" href=\"#elementor-action:action=popup:open&settings=eyJpZCI6IjM5NTEiLCJ0b2dnbGUiOmZhbHNlfQ==\">\n\t\t\t\t\t\t<span class=\"elementor-button-content-wrapper\">\n\t\t\t\t\t\t<span class=\"elementor-button-icon\">\n\t\t\t\t<svg aria-hidden=\"true\" class=\"e-font-icon-svg e-fas-long-arrow-alt-right\" viewbox=\"0 0 448 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M313.941 216H12c-6.627 0-12 5.373-12 12v56c0 6.627 5.373 12 12 12h301.941v46.059c0 21.382 25.851 32.09 40.971 16.971l86.059-86.059c9.373-9.373 9.373-24.569 0-33.941l-86.059-86.059c-15.119-15.119-40.971-4.411-40.971 16.971V216z\"><\/path><\/svg>\t\t\t<\/span>\n\t\t\t\t\t\t\t\t\t<span class=\"elementor-button-text\">\u0417\u0410\u041f\u0420\u041e\u0421\u0418\u0422\u042c \u0426\u0415\u041d\u0423 <\/span>\n\t\t\t\t\t<\/span>\n\t\t\t\t\t<\/a>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-793de363 elementor-widget elementor-widget-text-editor\" data-id=\"793de363\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<!-- x-tinymce\/html -->\n\n\u041b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u043f\u043e\u0434\u0440\u0430\u0437\u0434\u0435\u043b\u044f\u0435\u0442\u0441\u044f \u043d\u0430 \u0442\u0440\u0438 \u043e\u0441\u043d\u043e\u0432\u043d\u044b\u0435 \u043a\u0430\u0442\u0435\u0433\u043e\u0440\u0438\u0438 \u0432 \u0437\u0430\u0432\u0438\u0441\u0438\u043c\u043e\u0441\u0442\u0438 \u043e\u0442 \u043a\u043e\u043b\u0438\u0447\u0435\u0441\u0442\u0432\u0430 \u0441\u043e\u0434\u0435\u0440\u0436\u0430\u0449\u0438\u0445\u0441\u044f \u0432 \u043d\u0435\u0439 \u043b\u0435\u0433\u0438\u0440\u0443\u044e\u0449\u0438\u0445 \u044d\u043b\u0435\u043c\u0435\u043d\u0442\u043e\u0432: \u043d\u0438\u0437\u043a\u043e\u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u0430\u044f \u0441\u0442\u0430\u043b\u044c, \u0441\u0440\u0435\u0434\u043d\u0435\u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u0438 \u0432\u044b\u0441\u043e\u043a\u043e\u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u0430\u044f \u0441\u0442\u0430\u043b\u044c.\n<ul>\n \t<li><strong>\u041d\u0438\u0437\u043a\u043e\u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u0430\u044f \u0441\u0442\u0430\u043b\u044c (\u0441\u043e\u0434\u0435\u0440\u0436\u0430\u043d\u0438\u0435 \u043b\u0435\u0433\u0438\u0440\u0443\u044e\u0449\u0438\u0445 \u044d\u043b\u0435\u043c\u0435\u043d\u0442\u043e\u0432 &lt;5%)<\/strong>\n<ul>\n \t<li><strong>\u0411\u043e\u0440\u0441\u043e\u0434\u0435\u0440\u0436\u0430\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c:<\/strong> \u0422\u0432\u0435\u0440\u0434\u044b\u0439, \u0438\u0437\u043d\u043e\u0441\u043e\u0441\u0442\u043e\u0439\u043a\u0438\u0439, \u0438\u0441\u043f\u043e\u043b\u044c\u0437\u0443\u0435\u0442\u0441\u044f \u0432 \u0430\u0432\u0442\u043e\u043c\u043e\u0431\u0438\u043b\u044c\u043d\u044b\u0445 \u0438 \u0441\u0435\u043b\u044c\u0441\u043a\u043e\u0445\u043e\u0437\u044f\u0439\u0441\u0442\u0432\u0435\u043d\u043d\u044b\u0445 \u0434\u0435\u0442\u0430\u043b\u044f\u0445.<\/li>\n \t<li><strong>\u0410\u0418\u0421\u0418 4140<\/strong> \u0438 <strong>4340<\/strong>: \u0412\u044b\u0441\u043e\u043a\u0430\u044f \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c \u0438 \u0443\u0434\u0430\u0440\u043d\u0430\u044f \u0432\u044f\u0437\u043a\u043e\u0441\u0442\u044c \u0434\u043b\u044f \u0437\u0443\u0431\u0447\u0430\u0442\u044b\u0445 \u043f\u0435\u0440\u0435\u0434\u0430\u0447 \u0438 \u0430\u044d\u0440\u043e\u043a\u043e\u0441\u043c\u0438\u0447\u0435\u0441\u043a\u043e\u0439 \u043f\u0440\u043e\u043c\u044b\u0448\u043b\u0435\u043d\u043d\u043e\u0441\u0442\u0438.<\/li>\n \t<li><strong>\u0410\u0418\u0421\u0418 6150<\/strong>, <strong>8620<\/strong>, \u0438 <strong>4130<\/strong>: \u0418\u0441\u043f\u043e\u043b\u044c\u0437\u0443\u0435\u0442\u0441\u044f \u0434\u043b\u044f \u043f\u0440\u0443\u0436\u0438\u043d, \u043a\u043e\u043b\u0435\u043d\u0447\u0430\u0442\u044b\u0445 \u0432\u0430\u043b\u043e\u0432 \u0438 \u0430\u0432\u0442\u043e\u0441\u043f\u043e\u0440\u0442\u0430.<\/li>\n<\/ul>\n<\/li>\n \t<li><strong>\u0421\u0440\u0435\u0434\u043d\u0435\u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u0430\u044f \u0441\u0442\u0430\u043b\u044c (\u0441\u043e\u0434\u0435\u0440\u0436\u0430\u043d\u0438\u0435 \u043b\u0435\u0433\u0438\u0440\u0443\u044e\u0449\u0438\u0445 \u044d\u043b\u0435\u043c\u0435\u043d\u0442\u043e\u0432 5%-10%)<\/strong>\n<ul>\n \t<li><strong>300\u041c<\/strong>: \u0412\u044b\u0441\u043e\u043a\u043e\u043f\u0440\u043e\u0447\u043d\u0430\u044f \u043d\u0438\u0437\u043a\u043e\u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u0434\u043b\u044f \u0448\u0430\u0441\u0441\u0438 \u0441\u0430\u043c\u043e\u043b\u0435\u0442\u043e\u0432.<\/li>\n \t<li><strong>\u041a\u0440\u0435\u043c\u043d\u0438\u0435\u0432\u0430\u044f \u0441\u0442\u0430\u043b\u044c<\/strong>: \u0414\u043b\u044f \u0443\u043b\u0443\u0447\u0448\u0435\u043d\u0438\u044f \u044d\u043b\u0435\u043a\u0442\u0440\u0438\u0447\u0435\u0441\u043a\u0438\u0445 \u0445\u0430\u0440\u0430\u043a\u0442\u0435\u0440\u0438\u0441\u0442\u0438\u043a \u0442\u0440\u0430\u043d\u0441\u0444\u043e\u0440\u043c\u0430\u0442\u043e\u0440\u043e\u0432 \u0438 \u0434\u0432\u0438\u0433\u0430\u0442\u0435\u043b\u0435\u0439.<\/li>\n \t<li><a href=\"https:\/\/steelprogroup.com\/ru\/tool-steel\/\"style=\"color:#ec1c24;font-weight:500\"><strong>\u0418\u043d\u0441\u0442\u0440\u0443\u043c\u0435\u043d\u0442\u0430\u043b\u044c\u043d\u0430\u044f \u0441\u0442\u0430\u043b\u044c<\/strong><\/a>: \u0412\u044b\u0441\u043e\u043a\u0430\u044f \u0442\u0432\u0435\u0440\u0434\u043e\u0441\u0442\u044c \u0438 \u0438\u0437\u043d\u043e\u0441\u043e\u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c, \u0438\u0441\u043f\u043e\u043b\u044c\u0437\u0443\u0435\u0442\u0441\u044f \u0432 \u0440\u0435\u0436\u0443\u0449\u0438\u0445 \u0438 \u0441\u0432\u0435\u0440\u043b\u0438\u043b\u044c\u043d\u044b\u0445 \u0438\u043d\u0441\u0442\u0440\u0443\u043c\u0435\u043d\u0442\u0430\u0445.<\/li>\n<\/ul>\n<\/li>\n \t<li><strong>\u0412\u044b\u0441\u043e\u043a\u043e\u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u0430\u044f \u0441\u0442\u0430\u043b\u044c (\u0441\u043e\u0434\u0435\u0440\u0436\u0430\u043d\u0438\u0435 \u043b\u0435\u0433\u0438\u0440\u0443\u044e\u0449\u0438\u0445 \u044d\u043b\u0435\u043c\u0435\u043d\u0442\u043e\u0432 &gt;10%)<\/strong>\n<ul>\n \t<li><strong>\u0418\u043d\u0441\u0442\u0440\u0443\u043c\u0435\u043d\u0442\u0430\u043b\u044c\u043d\u0430\u044f \u0441\u0442\u0430\u043b\u044c H13<\/strong>: \u043f\u0440\u043e\u0447\u043d\u044b\u0439, \u0442\u0432\u0435\u0440\u0434\u044b\u0439, \u0442\u0435\u0440\u043c\u043e\u0441\u0442\u043e\u0439\u043a\u0438\u0439, \u0438\u0441\u043f\u043e\u043b\u044c\u0437\u0443\u0435\u0442\u0441\u044f \u0434\u043b\u044f \u0438\u0437\u0433\u043e\u0442\u043e\u0432\u043b\u0435\u043d\u0438\u044f \u0448\u0442\u0430\u043c\u043f\u043e\u0432, \u0444\u043e\u0440\u043c \u0438 \u0438\u043d\u0441\u0442\u0440\u0443\u043c\u0435\u043d\u0442\u043e\u0432.<\/li>\n \t<li><strong>\u041d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c AISI 316 <\/strong>: \u041a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u043e\u0441\u0442\u043e\u0439\u043a\u0438\u0439, \u0432\u044b\u0441\u043e\u043a\u043e\u0442\u0435\u043c\u043f\u0435\u0440\u0430\u0442\u0443\u0440\u043d\u044b\u0439, \u0434\u043b\u044f \u0438\u0441\u043f\u043e\u043b\u044c\u0437\u043e\u0432\u0430\u043d\u0438\u044f \u0432 \u043c\u043e\u0440\u0441\u043a\u043e\u0439 \u0438 \u0445\u0438\u043c\u0438\u0447\u0435\u0441\u043a\u043e\u0439 \u043f\u0440\u043e\u043c\u044b\u0448\u043b\u0435\u043d\u043d\u043e\u0441\u0442\u0438.<\/li>\n \t<li><strong>\u041c\u0430\u0440\u0442\u0435\u043d\u0441\u0438\u0442\u043d\u0430\u044f \u0441\u0442\u0430\u043b\u044c<\/strong>: \u0421\u0432\u0435\u0440\u0445\u043f\u0440\u043e\u0447\u043d\u044b\u0439 \u0438 \u043f\u0440\u043e\u0447\u043d\u044b\u0439, \u0434\u043b\u044f \u0430\u044d\u0440\u043e\u043a\u043e\u0441\u043c\u0438\u0447\u0435\u0441\u043a\u043e\u0439 \u043e\u0442\u0440\u0430\u0441\u043b\u0438 \u0438 \u0432\u044b\u0441\u043e\u043a\u0438\u0445 \u044d\u043a\u0441\u043f\u043b\u0443\u0430\u0442\u0430\u0446\u0438\u043e\u043d\u043d\u044b\u0445 \u0445\u0430\u0440\u0430\u043a\u0442\u0435\u0440\u0438\u0441\u0442\u0438\u043a.<\/li>\n<\/ul>\n<\/li>\n<\/ul>\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-8a86a87 e-con-full e-flex e-con e-child\" data-id=\"8a86a87\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-b0dfd64 elementor-arrows-position-inside elementor-pagination-position-outside elementor-widget elementor-widget-image-carousel\" data-id=\"b0dfd64\" data-element_type=\"widget\" data-settings=\"{&quot;slides_to_show&quot;:&quot;1&quot;,&quot;navigation&quot;:&quot;both&quot;,&quot;autoplay&quot;:&quot;yes&quot;,&quot;pause_on_hover&quot;:&quot;yes&quot;,&quot;pause_on_interaction&quot;:&quot;yes&quot;,&quot;autoplay_speed&quot;:5000,&quot;infinite&quot;:&quot;yes&quot;,&quot;effect&quot;:&quot;slide&quot;,&quot;speed&quot;:500}\" data-widget_type=\"image-carousel.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<div class=\"elementor-image-carousel-wrapper swiper-container\" dir=\"ltr\">\n\t\t\t<div class=\"elementor-image-carousel swiper-wrapper swiper-image-stretch\" aria-live=\"off\">\n\t\t\t\t\t\t\t\t<div class=\"swiper-slide\" role=\"group\" aria-roledescription=\"slide\" aria-label=\"1 \u0438\u0437 1\"><figure class=\"swiper-slide-inner\"><img decoding=\"async\" class=\"swiper-slide-image\" src=\"https:\/\/steelprogroup.com\/wp-content\/uploads\/elementor\/thumbs\/alloy-steel-stocking-qx9yxfjoea2916ce5jqcw6cff4gfapyh0wtf6igkc8.jpg\" alt=\"\u0447\u0443\u043b\u043e\u043a \u0438\u0437 \u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u043e\u0439 \u0441\u0442\u0430\u043b\u0438\" \/><\/figure><\/div>\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-7a5914f e-flex e-con-boxed e-con e-parent\" data-id=\"7a5914f\" data-element_type=\"container\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t\t\t<div class=\"elementor-element elementor-element-5ceb1f3e elementor-widget elementor-widget-menu-anchor\" data-id=\"5ceb1f3e\" data-element_type=\"widget\" data-widget_type=\"menu-anchor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<div class=\"elementor-menu-anchor\" id=\"3\"><\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-63993b92 e-con-full e-flex e-con e-parent\" data-id=\"63993b92\" data-element_type=\"container\">\n\t\t<div class=\"elementor-element elementor-element-7ceeefb3 e-flex e-con-boxed e-con e-child\" data-id=\"7ceeefb3\" data-element_type=\"container\" data-settings=\"{&quot;background_background&quot;:&quot;classic&quot;}\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t\t\t<div class=\"elementor-element elementor-element-23d5be86 elementor-widget elementor-widget-heading\" data-id=\"23d5be86\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">\u041e\u0442\u0440\u0430\u0441\u043b\u0438 \u0438 \u043f\u0440\u0438\u043b\u043e\u0436\u0435\u043d\u0438\u044f<\/h2>\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-676bdfb3 elementor-widget elementor-widget-text-editor\" data-id=\"676bdfb3\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<span style=\"color: #5e5e5e; font-family: Jost, sans-serif; font-size: 18px; margin: -; letter-spacing: 0.2px;\">\u041b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u2014 \u044d\u0442\u043e \u0441\u043f\u0435\u0446\u0438\u0430\u043b\u0438\u0437\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u044b\u0439 \u0442\u0438\u043f \u0441\u0442\u0430\u043b\u0438, \u043f\u0440\u0435\u0434\u043d\u0430\u0437\u043d\u0430\u0447\u0435\u043d\u043d\u044b\u0439 \u0434\u043b\u044f \u0438\u0441\u043f\u043e\u043b\u044c\u0437\u043e\u0432\u0430\u043d\u0438\u044f \u0432 \u0441\u043b\u043e\u0436\u043d\u044b\u0445 \u0443\u0441\u043b\u043e\u0432\u0438\u044f\u0445 \u0432 \u0440\u0430\u0437\u043b\u0438\u0447\u043d\u044b\u0445 \u043e\u0442\u0440\u0430\u0441\u043b\u044f\u0445 \u043f\u0440\u043e\u043c\u044b\u0448\u043b\u0435\u043d\u043d\u043e\u0441\u0442\u0438. \u0415\u0435 \u0432\u044b\u0431\u0438\u0440\u0430\u044e\u0442 \u0437\u0430 \u0435\u0435 \u043f\u0440\u0435\u0432\u043e\u0441\u0445\u043e\u0434\u043d\u0443\u044e \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c, \u0436\u0435\u0441\u0442\u043a\u043e\u0441\u0442\u044c \u0438 \u0443\u0441\u0442\u043e\u0439\u0447\u0438\u0432\u043e\u0441\u0442\u044c \u043a \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u0438 \u0438 \u0432\u044b\u0441\u043e\u043a\u0438\u043c \u0442\u0435\u043c\u043f\u0435\u0440\u0430\u0442\u0443\u0440\u0430\u043c, \u0447\u0442\u043e \u0434\u0435\u043b\u0430\u0435\u0442 \u0435\u0435 \u0438\u0434\u0435\u0430\u043b\u044c\u043d\u043e\u0439 \u0434\u043b\u044f \u0430\u0432\u0442\u043e\u043c\u043e\u0431\u0438\u043b\u044c\u043d\u043e\u0439, \u0430\u044d\u0440\u043e\u043a\u043e\u0441\u043c\u0438\u0447\u0435\u0441\u043a\u043e\u0439 \u0438 \u0441\u0442\u0440\u043e\u0438\u0442\u0435\u043b\u044c\u043d\u043e\u0439 \u043f\u0440\u043e\u043c\u044b\u0448\u043b\u0435\u043d\u043d\u043e\u0441\u0442\u0438.<\/span>\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-52605d93 elementor-widget elementor-widget-text-editor\" data-id=\"52605d93\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<p><span style=\"-webkit-font-smoothing: antialiased; text-rendering: optimizelegibility; font-weight: bold; margin: 0; color: #5e5e5e; font-family: Jost, sans-serif; font-size: 18px; letter-spacing: 0.2px;\">\u041d\u0435\u043a\u043e\u0442\u043e\u0440\u044b\u0435 \u0440\u0430\u0441\u043f\u0440\u043e\u0441\u0442\u0440\u0430\u043d\u0435\u043d\u043d\u044b\u0435 \u043e\u0442\u0440\u0430\u0441\u043b\u0438 \u0438 \u043e\u0431\u043b\u0430\u0441\u0442\u0438 \u043f\u0440\u0438\u043c\u0435\u043d\u0435\u043d\u0438\u044f \u0432\u043a\u043b\u044e\u0447\u0430\u044e\u0442 \u0432 \u0441\u0435\u0431\u044f:<\/span><\/p>\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-64ec9f5c e-con-full e-flex e-con e-child\" data-id=\"64ec9f5c\" data-element_type=\"container\">\n\t\t<div class=\"elementor-element elementor-element-74820c9c e-con-full e-flex e-con e-child\" data-id=\"74820c9c\" data-element_type=\"container\">\n\t\t<div class=\"elementor-element elementor-element-7772d937 e-con-full e-flex e-con e-child\" data-id=\"7772d937\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-354072d7 elementor-widget elementor-widget-image\" data-id=\"354072d7\" data-element_type=\"widget\" data-widget_type=\"image.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t<img fetchpriority=\"high\" decoding=\"async\" width=\"380\" height=\"280\" src=\"https:\/\/steelprogroup.com\/wp-content\/uploads\/2024\/07\/1-21.png\" class=\"attachment-2048x2048 size-2048x2048 wp-image-4740\" alt=\"\u0417\u043d\u0430\u0447\u043e\u043a \u043a\u043e\u043d\u0432\u0435\u0439\u0435\u0440\u043d\u043e\u0439 \u043b\u0435\u043d\u0442\u044b \u0441 \u044f\u0449\u0438\u043a\u0430\u043c\u0438 \u0438 \u0448\u0435\u0441\u0442\u0435\u0440\u043d\u0435\u0439 \u043d\u0430 \u0437\u0430\u0434\u043d\u0435\u043c \u043f\u043b\u0430\u043d\u0435 \u0432 \u043a\u0440\u0430\u0441\u043d\u043e\u043c \u043a\u043e\u043d\u0442\u0443\u0440\u0435.\" srcset=\"https:\/\/steelprogroup.com\/wp-content\/uploads\/2024\/07\/1-21.png 380w, https:\/\/steelprogroup.com\/wp-content\/uploads\/2024\/07\/1-21-300x221.png 300w\" sizes=\"(max-width: 380px) 100vw, 380px\" \/>\t\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-534d73d6 e-con-full e-flex e-con e-child\" data-id=\"534d73d6\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-4e613b37 elementor-widget elementor-widget-heading\" data-id=\"4e613b37\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t<h3 class=\"elementor-heading-title elementor-size-default\">\u0410\u0432\u0442\u043e\u043c\u043e\u0431\u0438\u043b\u044c\u043d\u0430\u044f \u043f\u0440\u043e\u043c\u044b\u0448\u043b\u0435\u043d\u043d\u043e\u0441\u0442\u044c<\/h3>\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-3fad37df elementor-widget elementor-widget-text-editor\" data-id=\"3fad37df\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<span style=\"color: #5e5e5e; font-family: Jost, sans-serif; font-size: 18px; letter-spacing: 0.2px;\">\u0418\u0441\u043f\u043e\u043b\u044c\u0437\u0443\u0435\u0442\u0441\u044f \u043f\u0440\u0438 \u0438\u0437\u0433\u043e\u0442\u043e\u0432\u043b\u0435\u043d\u0438\u0438 \u0432\u044b\u0441\u043e\u043a\u043e\u043f\u0440\u043e\u0447\u043d\u044b\u0445 \u0434\u0435\u0442\u0430\u043b\u0435\u0439, \u0442\u0430\u043a\u0438\u0445 \u043a\u0430\u043a \u0448\u0435\u0441\u0442\u0435\u0440\u043d\u0438, \u0432\u0430\u043b\u044b \u0438 \u0441\u0438\u0441\u0442\u0435\u043c\u044b \u043f\u043e\u0434\u0432\u0435\u0441\u043a\u0438.<\/span>\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-122490fa e-con-full e-flex e-con e-child\" data-id=\"122490fa\" data-element_type=\"container\">\n\t\t<div class=\"elementor-element elementor-element-1719af6e e-con-full e-flex e-con e-child\" data-id=\"1719af6e\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-67b1a424 elementor-widget elementor-widget-image\" data-id=\"67b1a424\" data-element_type=\"widget\" data-widget_type=\"image.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t<img decoding=\"async\" width=\"380\" height=\"280\" src=\"https:\/\/steelprogroup.com\/wp-content\/uploads\/2024\/07\/10a2b5bb-5e4e-4ebd-b3f5-37c1d9d251cb.png\" class=\"attachment-large size-large wp-image-4752\" alt=\"\u041a\u0440\u0430\u0441\u043d\u044b\u0439 \u0437\u043d\u0430\u0447\u043e\u043a \u0440\u0430\u043a\u0435\u0442\u044b.\" srcset=\"https:\/\/steelprogroup.com\/wp-content\/uploads\/2024\/07\/10a2b5bb-5e4e-4ebd-b3f5-37c1d9d251cb.png 380w, https:\/\/steelprogroup.com\/wp-content\/uploads\/2024\/07\/10a2b5bb-5e4e-4ebd-b3f5-37c1d9d251cb-300x221.png 300w\" sizes=\"(max-width: 380px) 100vw, 380px\" \/>\t\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-35a3fde5 e-con-full e-flex e-con e-child\" data-id=\"35a3fde5\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-1b6a14a7 elementor-widget elementor-widget-heading\" data-id=\"1b6a14a7\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t<h3 class=\"elementor-heading-title elementor-size-default\">\u0410\u044d\u0440\u043e\u043a\u043e\u0441\u043c\u0438\u0447\u0435\u0441\u043a\u0430\u044f \u043f\u0440\u043e\u043c\u044b\u0448\u043b\u0435\u043d\u043d\u043e\u0441\u0442\u044c<\/h3>\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-3a24e3d9 elementor-widget elementor-widget-text-editor\" data-id=\"3a24e3d9\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<span style=\"color: #5e5e5e; font-family: Jost, sans-serif; font-size: 18px; letter-spacing: 0.2px;\">\u0418\u0434\u0435\u0430\u043b\u044c\u043d\u043e \u043f\u043e\u0434\u0445\u043e\u0434\u0438\u0442 \u0434\u043b\u044f \u0442\u0430\u043a\u0438\u0445 \u043a\u0440\u0438\u0442\u0438\u0447\u0435\u0441\u043a\u0438 \u0432\u0430\u0436\u043d\u044b\u0445 \u043a\u043e\u043c\u043f\u043e\u043d\u0435\u043d\u0442\u043e\u0432, \u043a\u0430\u043a \u0448\u0430\u0441\u0441\u0438, \u0434\u0435\u0442\u0430\u043b\u0438 \u0434\u0432\u0438\u0433\u0430\u0442\u0435\u043b\u044f \u0438 \u044d\u043b\u0435\u043c\u0435\u043d\u0442\u044b \u043a\u043e\u043d\u0441\u0442\u0440\u0443\u043a\u0446\u0438\u0438, \u0442\u0440\u0435\u0431\u0443\u044e\u0449\u0438\u0435 \u0432\u044b\u0441\u043e\u043a\u043e\u0439 \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u0438 \u0438 \u0443\u0441\u0442\u0430\u043b\u043e\u0441\u0442\u043d\u043e\u0439 \u0443\u0441\u0442\u043e\u0439\u0447\u0438\u0432\u043e\u0441\u0442\u0438.<\/span>\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-486ea8a2 e-con-full e-flex e-con e-child\" data-id=\"486ea8a2\" data-element_type=\"container\">\n\t\t<div class=\"elementor-element elementor-element-2c41c43 e-con-full e-flex e-con e-child\" data-id=\"2c41c43\" data-element_type=\"container\">\n\t\t<div class=\"elementor-element elementor-element-672d168d e-con-full e-flex e-con e-child\" data-id=\"672d168d\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-ff8a52c elementor-widget elementor-widget-image\" data-id=\"ff8a52c\" data-element_type=\"widget\" data-widget_type=\"image.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t<img decoding=\"async\" width=\"380\" height=\"280\" src=\"https:\/\/steelprogroup.com\/wp-content\/uploads\/2024\/07\/20240705-175012-1.png\" class=\"attachment-large size-large wp-image-4951\" alt=\"\u041a\u0440\u0430\u0441\u043d\u044b\u0439 \u0437\u043d\u0430\u0447\u043e\u043a \u0433\u043e\u0440\u043e\u0434\u0441\u043a\u043e\u0433\u043e \u043f\u0435\u0439\u0437\u0430\u0436\u0430 \u0441\u043e \u0437\u0434\u0430\u043d\u0438\u044f\u043c\u0438.\" srcset=\"https:\/\/steelprogroup.com\/wp-content\/uploads\/2024\/07\/20240705-175012-1.png 380w, https:\/\/steelprogroup.com\/wp-content\/uploads\/2024\/07\/20240705-175012-1-300x221.png 300w\" sizes=\"(max-width: 380px) 100vw, 380px\" \/>\t\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-23d97ebb e-con-full e-flex e-con e-child\" data-id=\"23d97ebb\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-2d1ba698 elementor-widget elementor-widget-heading\" data-id=\"2d1ba698\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t<h3 class=\"elementor-heading-title elementor-size-default\">\u0421\u0442\u0440\u043e\u0438\u0442\u0435\u043b\u044c\u043d\u0430\u044f \u043f\u0440\u043e\u043c\u044b\u0448\u043b\u0435\u043d\u043d\u043e\u0441\u0442\u044c<\/h3>\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-6813cabf elementor-widget elementor-widget-text-editor\" data-id=\"6813cabf\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<span style=\"color: #5e5e5e; font-family: Jost, sans-serif; font-size: 18px; letter-spacing: 0.2px;\">\u0418\u0441\u043f\u043e\u043b\u044c\u0437\u0443\u0435\u0442\u0441\u044f \u0432 \u0441\u0442\u0440\u043e\u0438\u0442\u0435\u043b\u044c\u043d\u044b\u0445 \u043a\u043e\u043d\u0441\u0442\u0440\u0443\u043a\u0446\u0438\u044f\u0445, \u0442\u0430\u043a\u0438\u0445 \u043a\u0430\u043a \u0431\u0430\u043b\u043a\u0438 \u0438 \u043a\u043e\u043b\u043e\u043d\u043d\u044b, \u0433\u0434\u0435 \u0442\u0440\u0435\u0431\u0443\u0435\u0442\u0441\u044f \u0438\u0441\u043a\u043b\u044e\u0447\u0438\u0442\u0435\u043b\u044c\u043d\u0430\u044f \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c \u0438 \u0436\u0435\u0441\u0442\u043a\u043e\u0441\u0442\u044c.<\/span>\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-76c2f5e6 e-con-full e-flex e-con e-child\" data-id=\"76c2f5e6\" data-element_type=\"container\">\n\t\t<div class=\"elementor-element elementor-element-4214d46 e-con-full e-flex e-con e-child\" data-id=\"4214d46\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-417be238 elementor-widget elementor-widget-image\" data-id=\"417be238\" data-element_type=\"widget\" data-widget_type=\"image.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t<img loading=\"lazy\" decoding=\"async\" width=\"380\" height=\"280\" src=\"https:\/\/steelprogroup.com\/wp-content\/uploads\/2024\/07\/20240705-175017.png\" class=\"attachment-large size-large wp-image-4613\" alt=\"\u041a\u0440\u0430\u0441\u043d\u044b\u0439 \u0437\u043d\u0430\u0447\u043e\u043a \u0442\u0440\u0430\u043a\u0442\u043e\u0440\u0430.\" srcset=\"https:\/\/steelprogroup.com\/wp-content\/uploads\/2024\/07\/20240705-175017.png 380w, https:\/\/steelprogroup.com\/wp-content\/uploads\/2024\/07\/20240705-175017-300x221.png 300w\" sizes=\"(max-width: 380px) 100vw, 380px\" \/>\t\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-2cb1da49 e-con-full e-flex e-con e-child\" data-id=\"2cb1da49\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-5a0155b0 elementor-widget elementor-widget-heading\" data-id=\"5a0155b0\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t<h3 class=\"elementor-heading-title elementor-size-default\">\u041f\u0440\u043e\u0438\u0437\u0432\u043e\u0434\u0441\u0442\u0432\u043e<\/h3>\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-226550c9 elementor-widget elementor-widget-text-editor\" data-id=\"226550c9\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<span style=\"color: #5e5e5e; font-family: Jost, sans-serif; font-size: 18px; letter-spacing: 0.2px;\">\u0428\u0438\u0440\u043e\u043a\u043e \u0438\u0441\u043f\u043e\u043b\u044c\u0437\u0443\u0435\u0442\u0441\u044f \u0432 \u043f\u0440\u043e\u0438\u0437\u0432\u043e\u0434\u0441\u0442\u0432\u0435 \u043f\u0440\u043e\u043c\u044b\u0448\u043b\u0435\u043d\u043d\u044b\u0445 \u0438\u043d\u0441\u0442\u0440\u0443\u043c\u0435\u043d\u0442\u043e\u0432, \u0434\u0435\u0442\u0430\u043b\u0435\u0439 \u043c\u0430\u0448\u0438\u043d \u0438 \u0444\u043e\u0440\u043c \u0431\u043b\u0430\u0433\u043e\u0434\u0430\u0440\u044f \u0441\u0432\u043e\u0435\u0439 \u0438\u0437\u043d\u043e\u0441\u043e\u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u0438 \u0438 \u0442\u0432\u0435\u0440\u0434\u043e\u0441\u0442\u0438.<\/span>\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-378030e e-con-full e-flex e-con e-child\" data-id=\"378030e\" data-element_type=\"container\">\n\t\t<div class=\"elementor-element elementor-element-7a0c1eb5 e-con-full e-flex e-con e-child\" data-id=\"7a0c1eb5\" data-element_type=\"container\">\n\t\t<div class=\"elementor-element elementor-element-19220365 e-con-full e-flex e-con e-child\" data-id=\"19220365\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-1f8d9674 elementor-widget elementor-widget-image\" data-id=\"1f8d9674\" data-element_type=\"widget\" data-widget_type=\"image.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t<img loading=\"lazy\" decoding=\"async\" width=\"380\" height=\"280\" src=\"https:\/\/steelprogroup.com\/wp-content\/uploads\/2024\/07\/81ba3545-6056-4f47-bd49-b39759e8e1b0-1.png\" class=\"attachment-large size-large wp-image-5379\" alt=\"\u041a\u0440\u0430\u0441\u043d\u044b\u0439 \u0437\u043d\u0430\u0447\u043e\u043a \u043c\u043e\u0440\u0441\u043a\u043e\u0439 \u043d\u0435\u0444\u0442\u044f\u043d\u043e\u0439 \u0432\u044b\u0448\u043a\u0438 \u0441 \u043f\u0442\u0438\u0446\u0430\u043c\u0438 \u0438 \u0432\u0435\u0440\u0442\u043e\u043b\u0435\u0442\u043e\u043c.\" srcset=\"https:\/\/steelprogroup.com\/wp-content\/uploads\/2024\/07\/81ba3545-6056-4f47-bd49-b39759e8e1b0-1.png 380w, https:\/\/steelprogroup.com\/wp-content\/uploads\/2024\/07\/81ba3545-6056-4f47-bd49-b39759e8e1b0-1-300x221.png 300w\" sizes=\"(max-width: 380px) 100vw, 380px\" \/>\t\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-74b45ae0 e-con-full e-flex e-con e-child\" data-id=\"74b45ae0\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-48302717 elementor-widget elementor-widget-heading\" data-id=\"48302717\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t<h3 class=\"elementor-heading-title elementor-size-default\">\u042d\u043d\u0435\u0440\u0433\u0435\u0442\u0438\u0447\u0435\u0441\u043a\u0438\u0439 \u0441\u0435\u043a\u0442\u043e\u0440<\/h3>\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-7775811b elementor-widget elementor-widget-text-editor\" data-id=\"7775811b\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<span style=\"color: #5e5e5e; font-family: Jost, sans-serif; font-size: 18px; letter-spacing: 0.2px;\">\u0418\u0441\u043f\u043e\u043b\u044c\u0437\u0443\u0435\u0442\u0441\u044f \u0432 \u044d\u043d\u0435\u0440\u0433\u0435\u0442\u0438\u0447\u0435\u0441\u043a\u043e\u043c \u043e\u0431\u043e\u0440\u0443\u0434\u043e\u0432\u0430\u043d\u0438\u0438, \u0438\u043d\u0441\u0442\u0440\u0443\u043c\u0435\u043d\u0442\u0430\u0445 \u0434\u043b\u044f \u0431\u0443\u0440\u0435\u043d\u0438\u044f \u043d\u0435\u0444\u0442\u044f\u043d\u044b\u0445 \u0438 \u0433\u0430\u0437\u043e\u0432\u044b\u0445 \u0441\u043a\u0432\u0430\u0436\u0438\u043d, \u0430 \u0442\u0430\u043a\u0436\u0435 \u0442\u0440\u0443\u0431\u043e\u043f\u0440\u043e\u0432\u043e\u0434\u0430\u0445, \u043f\u043e\u0441\u043a\u043e\u043b\u044c\u043a\u0443 \u043e\u0431\u043b\u0430\u0434\u0430\u0435\u0442 \u0432\u044b\u0441\u043e\u043a\u043e\u0439 \u0442\u0435\u0440\u043c\u043e\u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c\u044e \u0438 \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u043e\u0439 \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c\u044e.<\/span>\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-58a1a21d e-con-full e-flex e-con e-child\" data-id=\"58a1a21d\" data-element_type=\"container\">\n\t\t<div class=\"elementor-element elementor-element-2eba6b47 e-con-full e-flex e-con e-child\" data-id=\"2eba6b47\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-1cef2699 elementor-widget elementor-widget-image\" data-id=\"1cef2699\" data-element_type=\"widget\" data-widget_type=\"image.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t<img loading=\"lazy\" decoding=\"async\" width=\"380\" height=\"280\" src=\"https:\/\/steelprogroup.com\/wp-content\/uploads\/2024\/07\/4ed8418e-1000-4416-82a6-fc4d015d4b73.png\" class=\"attachment-large size-large wp-image-5549\" alt=\"\u041a\u0440\u0430\u0441\u043d\u044b\u0439 \u043a\u043e\u043d\u0442\u0443\u0440\u043d\u044b\u0439 \u0437\u043d\u0430\u0447\u043e\u043a \u0441\u0435\u0442\u0438 \u043e\u0431\u043b\u0430\u0447\u043d\u044b\u0445 \u0432\u044b\u0447\u0438\u0441\u043b\u0435\u043d\u0438\u0439.\" srcset=\"https:\/\/steelprogroup.com\/wp-content\/uploads\/2024\/07\/4ed8418e-1000-4416-82a6-fc4d015d4b73.png 380w, https:\/\/steelprogroup.com\/wp-content\/uploads\/2024\/07\/4ed8418e-1000-4416-82a6-fc4d015d4b73-300x221.png 300w\" sizes=\"(max-width: 380px) 100vw, 380px\" \/>\t\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-d256e04 e-con-full e-flex e-con e-child\" data-id=\"d256e04\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-56c446a8 elementor-widget elementor-widget-heading\" data-id=\"56c446a8\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t<h3 class=\"elementor-heading-title elementor-size-default\">\u0418\u0437\u0433\u043e\u0442\u043e\u0432\u043b\u0435\u043d\u0438\u0435 \u0438\u043d\u0441\u0442\u0440\u0443\u043c\u0435\u043d\u0442\u043e\u0432 \u0438 \u0448\u0442\u0430\u043c\u043f\u043e\u0432<\/h3>\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-13502505 elementor-widget elementor-widget-text-editor\" data-id=\"13502505\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<span style=\"color: #5e5e5e; font-family: Jost, sans-serif; font-size: 18px; letter-spacing: 0.2px;\">\u041f\u0440\u0435\u0434\u043f\u043e\u0447\u0442\u0438\u0442\u0435\u043b\u044c\u043d\u043e \u0434\u043b\u044f \u0448\u0442\u0430\u043c\u043f\u043e\u0432, \u0444\u043e\u0440\u043c \u0438 \u0438\u043d\u0441\u0442\u0440\u0443\u043c\u0435\u043d\u0442\u043e\u0432, \u0442\u0440\u0435\u0431\u0443\u044e\u0449\u0438\u0445 \u0432\u044b\u0441\u043e\u043a\u043e\u0439 \u0442\u0432\u0435\u0440\u0434\u043e\u0441\u0442\u0438, \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u0438 \u0438 \u0442\u0435\u0440\u043c\u043e\u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u0438.<\/span>\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-32a1808 e-con-full e-flex e-con e-child\" data-id=\"32a1808\" data-element_type=\"container\">\n\t\t<div class=\"elementor-element elementor-element-41d3292d e-con-full e-flex e-con e-child\" data-id=\"41d3292d\" data-element_type=\"container\">\n\t\t<div class=\"elementor-element elementor-element-7ca0a82a e-con-full e-flex e-con e-child\" data-id=\"7ca0a82a\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-6e9c11d6 elementor-widget elementor-widget-image\" data-id=\"6e9c11d6\" data-element_type=\"widget\" data-widget_type=\"image.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t<img loading=\"lazy\" decoding=\"async\" width=\"380\" height=\"280\" src=\"https:\/\/steelprogroup.com\/wp-content\/uploads\/2024\/07\/20240705-175007-1.png\" class=\"attachment-large size-large wp-image-5374\" alt=\"\u041a\u0440\u0430\u0441\u043d\u044b\u0439 \u0437\u043d\u0430\u0447\u043e\u043a \u0433\u0440\u0443\u0437\u043e\u0432\u043e\u0433\u043e \u0441\u0443\u0434\u043d\u0430 \u0441 \u0433\u0430\u0435\u0447\u043d\u044b\u043c \u043a\u043b\u044e\u0447\u043e\u043c \u0438 \u0432\u0435\u0442\u0440\u044f\u043d\u043e\u0439 \u0442\u0443\u0440\u0431\u0438\u043d\u043e\u0439.\" srcset=\"https:\/\/steelprogroup.com\/wp-content\/uploads\/2024\/07\/20240705-175007-1.png 380w, https:\/\/steelprogroup.com\/wp-content\/uploads\/2024\/07\/20240705-175007-1-300x221.png 300w\" sizes=\"(max-width: 380px) 100vw, 380px\" \/>\t\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-186ce82c e-con-full e-flex e-con e-child\" data-id=\"186ce82c\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-3bdbffd2 elementor-widget elementor-widget-heading\" data-id=\"3bdbffd2\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t<h3 class=\"elementor-heading-title elementor-size-default\">\u0421\u0443\u0434\u043e\u0441\u0442\u0440\u043e\u0435\u043d\u0438\u0435<\/h3>\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-23fd52bc elementor-widget elementor-widget-text-editor\" data-id=\"23fd52bc\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<span style=\"color: #5e5e5e; font-family: Jost, sans-serif; font-size: 18px; letter-spacing: 0.2px;\">\u0418\u0441\u043f\u043e\u043b\u044c\u0437\u0443\u0435\u0442\u0441\u044f \u0432 \u0441\u0442\u0440\u043e\u0438\u0442\u0435\u043b\u044c\u0441\u0442\u0432\u0435 \u0441\u0443\u0434\u043e\u0432 \u0438 \u043c\u043e\u0440\u0441\u043a\u0438\u0445 \u0441\u043e\u043e\u0440\u0443\u0436\u0435\u043d\u0438\u0439 \u0431\u043b\u0430\u0433\u043e\u0434\u0430\u0440\u044f \u0441\u0432\u043e\u0435\u0439 \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u0438 \u043a \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u0438 \u0438 \u0432\u044b\u0441\u043e\u043a\u043e\u0439 \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u0438.<\/span>\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-1c4e2bdd e-con-full e-flex e-con e-child\" data-id=\"1c4e2bdd\" data-element_type=\"container\">\n\t\t<div class=\"elementor-element elementor-element-6b6881c7 e-con-full e-flex e-con e-child\" data-id=\"6b6881c7\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-71bd72d1 elementor-widget elementor-widget-image\" data-id=\"71bd72d1\" data-element_type=\"widget\" data-widget_type=\"image.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t<img loading=\"lazy\" decoding=\"async\" width=\"380\" height=\"280\" src=\"https:\/\/steelprogroup.com\/wp-content\/uploads\/2024\/07\/20240705-175021-1.png\" class=\"attachment-large size-large wp-image-4952\" alt=\"\u041a\u0440\u0430\u0441\u043d\u043e-\u0431\u0435\u043b\u044b\u0439 \u0437\u043d\u0430\u0447\u043e\u043a \u043f\u043e\u0435\u0437\u0434\u0430 \u0432\u043d\u0443\u0442\u0440\u0438 \u0442\u0443\u043d\u043d\u0435\u043b\u044f.\" srcset=\"https:\/\/steelprogroup.com\/wp-content\/uploads\/2024\/07\/20240705-175021-1.png 380w, https:\/\/steelprogroup.com\/wp-content\/uploads\/2024\/07\/20240705-175021-1-300x221.png 300w\" sizes=\"(max-width: 380px) 100vw, 380px\" \/>\t\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-6347655f e-con-full e-flex e-con e-child\" data-id=\"6347655f\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-794bcdd1 elementor-widget elementor-widget-heading\" data-id=\"794bcdd1\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t<h3 class=\"elementor-heading-title elementor-size-default\">\u0416\u0435\u043b\u0435\u0437\u043d\u043e\u0434\u043e\u0440\u043e\u0436\u043d\u0430\u044f \u043f\u0440\u043e\u043c\u044b\u0448\u043b\u0435\u043d\u043d\u043e\u0441\u0442\u044c<\/h3>\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-25409983 elementor-widget elementor-widget-text-editor\" data-id=\"25409983\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<span style=\"color: #5e5e5e; font-family: Jost, sans-serif; font-size: 18px; letter-spacing: 0.2px;\">\u041f\u0440\u0438\u043c\u0435\u043d\u044f\u0435\u0442\u0441\u044f \u0432 \u043f\u0440\u043e\u0438\u0437\u0432\u043e\u0434\u0441\u0442\u0432\u0435 \u0436\u0435\u043b\u0435\u0437\u043d\u043e\u0434\u043e\u0440\u043e\u0436\u043d\u044b\u0445 \u043f\u0443\u0442\u0435\u0439 \u0438 \u043a\u043e\u043c\u043f\u043e\u043d\u0435\u043d\u0442\u043e\u0432, \u043e\u0431\u0435\u0441\u043f\u0435\u0447\u0438\u0432\u0430\u044f \u0434\u043e\u043b\u0433\u043e\u0432\u0435\u0447\u043d\u043e\u0441\u0442\u044c \u0438 \u0438\u0437\u043d\u043e\u0441\u043e\u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c \u043f\u0440\u0438 \u0431\u043e\u043b\u044c\u0448\u0438\u0445 \u043d\u0430\u0433\u0440\u0443\u0437\u043a\u0430\u0445 \u0438 \u0447\u0430\u0441\u0442\u043e\u043c \u0438\u0441\u043f\u043e\u043b\u044c\u0437\u043e\u0432\u0430\u043d\u0438\u0438.<\/span>\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-50112ae5 e-flex e-con-boxed e-con e-parent\" data-id=\"50112ae5\" data-element_type=\"container\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t\t\t<div class=\"elementor-element elementor-element-6e14ebde elementor-widget elementor-widget-menu-anchor\" data-id=\"6e14ebde\" data-element_type=\"widget\" data-widget_type=\"menu-anchor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<div class=\"elementor-menu-anchor\" id=\"4\"><\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-79222e02 e-con-full e-flex e-con e-parent\" data-id=\"79222e02\" data-element_type=\"container\">\n\t\t<div class=\"elementor-element elementor-element-43590cda e-flex e-con-boxed e-con e-child\" data-id=\"43590cda\" data-element_type=\"container\" data-settings=\"{&quot;background_background&quot;:&quot;classic&quot;}\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t\t\t<div class=\"elementor-element elementor-element-ee824d1 elementor-widget elementor-widget-heading\" data-id=\"ee824d1\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">\u0420\u0430\u0437\u043c\u0435\u0440\u044b \u0438 \u0441\u0432\u043e\u0439\u0441\u0442\u0432\u0430<\/h2>\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-323cb172 elementor-widget elementor-widget-text-editor\" data-id=\"323cb172\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<span style=\"color: #5e5e5e; margin: 0; font-family: Jost, sans-serif; font-size: 18px; letter-spacing: 0.2px;\">\u0422\u043e, \u043a\u0432\u0430\u043b\u0438\u0444\u0438\u0446\u0438\u0440\u0443\u0435\u0442\u0441\u044f \u043b\u0438 \u0441\u0442\u0430\u043b\u044c \u043a\u0430\u043a \u043f\u043b\u0430\u0441\u0442\u0438\u043d\u0430 \u0438\u043b\u0438 \u043b\u0438\u0441\u0442, \u0437\u0430\u0432\u0438\u0441\u0438\u0442 \u043e\u0442 \u0441\u043f\u0435\u0446\u0438\u0444\u0438\u043a\u0430\u0446\u0438\u0438, \u0438\u0441\u043f\u043e\u043b\u044c\u0437\u0443\u0435\u043c\u043e\u0439 \u0434\u043b\u044f \u0441\u0435\u0440\u0442\u0438\u0444\u0438\u043a\u0430\u0446\u0438\u0438. \u0421\u0443\u0449\u0435\u0441\u0442\u0432\u0443\u0435\u0442 \u0431\u043e\u043b\u044c\u0448\u043e\u0435 \u0441\u043e\u0432\u043f\u0430\u0434\u0435\u043d\u0438\u0435 \u0432 \u043f\u043e\u043f\u0443\u043b\u044f\u0440\u043d\u044b\u0445 \u0442\u043e\u043b\u0449\u0438\u043d\u0430\u0445 \u043c\u0435\u0436\u0434\u0443 \u043f\u043b\u0430\u0441\u0442\u0438\u043d\u043e\u0439 \u0438 \u043b\u0438\u0441\u0442\u043e\u043c, \u043d\u043e \u0441\u0442\u0430\u043b\u044c\u043d\u044b\u0435 \u043f\u043b\u0430\u0441\u0442\u0438\u043d\u044b \u043f\u0440\u0435\u0434\u043b\u0430\u0433\u0430\u044e\u0442\u0441\u044f \u0432 \u0433\u043e\u0440\u0430\u0437\u0434\u043e \u0431\u043e\u043b\u0435\u0435 \u0448\u0438\u0440\u043e\u043a\u043e\u043c \u0434\u0438\u0430\u043f\u0430\u0437\u043e\u043d\u0435 \u0440\u0430\u0437\u043c\u0435\u0440\u043e\u0432.<\/span>\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-79620e9a elementor-widget elementor-widget-shortcode\" data-id=\"79620e9a\" data-element_type=\"widget\" data-widget_type=\"shortcode.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<div class=\"elementor-shortcode\">\n<table id=\"tablepress-55\" class=\"tablepress tablepress-id-55\">\n<thead>\n<tr class=\"row-1\">\n\t<th class=\"column-1\"><\/th><th class=\"column-2\">\u0410\u0418\u0421\u0418 4340<\/th><th class=\"column-3\">\u0410\u0418\u0421\u0418 8620<\/th><th class=\"column-4\">\u0410\u0418\u0421\u0418 6150<\/th>\n<\/tr>\n<\/thead>\n<tbody class=\"row-striping row-hover\">\n<tr class=\"row-2\">\n\t<td class=\"column-1\">\u041f\u0440\u0435\u0434\u0435\u043b \u0442\u0435\u043a\u0443\u0447\u0435\u0441\u0442\u0438<\/td><td class=\"column-2\">745 \u041c\u041f\u0430 (108 \u0442\u044b\u0441.\u0444\u0443\u043d\u0442\u043e\u0432\/\u043a\u0432.\u0434\u044e\u0439\u043c)<\/td><td class=\"column-3\">620 \u041c\u041f\u0430 (90 \u0442\u044b\u0441.\u0444\u0443\u043d\u0442\u043e\u0432\/\u043a\u0432.\u0434\u044e\u0439\u043c)<\/td><td class=\"column-4\">760 \u041c\u041f\u0430 (110 \u0442\u044b\u0441.\u0444\u0443\u043d\u0442\u043e\u0432\/\u043a\u0432.\u0434\u044e\u0439\u043c)<\/td>\n<\/tr>\n<tr class=\"row-3\">\n\t<td class=\"column-1\">\u041f\u0440\u0435\u0434\u0435\u043b \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u0438<\/td><td class=\"column-2\">1100 \u041c\u041f\u0430 (160 \u0442\u044b\u0441.\u0444\u0443\u043d\u0442\u043e\u0432\/\u043a\u0432.\u0434\u044e\u0439\u043c)<\/td><td class=\"column-3\">930 \u041c\u041f\u0430 (135 \u0442\u044b\u0441.\u0444\u0443\u043d\u0442\u043e\u0432\/\u043a\u0432.\u0434\u044e\u0439\u043c)<\/td><td class=\"column-4\">1080 \u041c\u041f\u0430 (157 \u0442\u044b\u0441.\u0444\u0443\u043d\u0442\u043e\u0432\/\u043a\u0432.\u0434\u044e\u0439\u043c)<\/td>\n<\/tr>\n<tr class=\"row-4\">\n\t<td class=\"column-1\">\u0421\u0442\u0430\u043d\u0434\u0430\u0440\u0442 \u043c\u0430\u0442\u0435\u0440\u0438\u0430\u043b\u0430<\/td><td class=\"column-2\">ASTM A29\/A29M<\/td><td class=\"column-3\">ASTM A29\/A29M<\/td><td class=\"column-4\">ASTM A29\/A29M<\/td>\n<\/tr>\n<tr class=\"row-5\">\n\t<td class=\"column-1\">\u0422\u0432\u0435\u0440\u0434\u043e\u0441\u0442\u044c \u043f\u043e \u0412\u0438\u043a\u043a\u0435\u0440\u0441\u0443<\/td><td class=\"column-2\">\u041f\u0440\u0438\u043c\u0435\u0440\u043d\u043e 248-302 HV<\/td><td class=\"column-3\">\u041f\u0440\u0438\u043c\u0435\u0440\u043d\u043e 156-207 HV<\/td><td class=\"column-4\">\u041f\u0440\u0438\u043c\u0435\u0440\u043d\u043e 248-302 HV<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-1074e3f0 e-con-full e-flex e-con e-parent\" data-id=\"1074e3f0\" data-element_type=\"container\">\n\t\t<div class=\"elementor-element elementor-element-3dac49fc e-con-full e-flex e-con e-child\" data-id=\"3dac49fc\" data-element_type=\"container\" data-settings=\"{&quot;background_background&quot;:&quot;classic&quot;}\">\n\t\t<div class=\"elementor-element elementor-element-d145dff e-flex e-con-boxed e-con e-child\" data-id=\"d145dff\" data-element_type=\"container\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t<div class=\"elementor-element elementor-element-3b905db4 e-con-full e-flex e-con e-child\" data-id=\"3b905db4\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-2ba72527 elementor-widget elementor-widget-heading\" data-id=\"2ba72527\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">\u041b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u0430\u044f \u0441\u0442\u0430\u043b\u044c, \u043a\u043e\u0433\u0434\u0430 \u0438 \u0433\u0434\u0435 \u043e\u043d\u0430 \u0432\u0430\u043c \u043d\u0443\u0436\u043d\u0430<\/h2>\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-5e7e4b06 elementor-widget elementor-widget-text-editor\" data-id=\"5e7e4b06\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<p style=\"-webkit-font-smoothing: antialiased; text-rendering: optimizelegibility; margin-bottom: 20px; font-size: 18px; font-weight: 400; letter-spacing: 0.2px; line-height: 30px; color: #5e5e5e; font-family: Jost, sans-serif; font-style: normal;\"><span style=\"color: #747474; font-size: 16px; letter-spacing: 0.2px;\">\u0417\u0434\u0435\u0441\u044c \u0432\u044b \u043f\u043e\u043b\u0443\u0447\u0430\u0435\u0442\u0435 \u0431\u043e\u043b\u044c\u0448\u0435, \u0447\u0435\u043c \u043f\u0440\u043e\u0441\u0442\u043e \u043a\u0430\u0447\u0435\u0441\u0442\u0432\u0435\u043d\u043d\u0443\u044e \u0441\u0442\u0430\u043b\u044c. \u0418\u043c\u0435\u044f \u043c\u043d\u043e\u0436\u0435\u0441\u0442\u0432\u043e \u043f\u0440\u0435\u0434\u043f\u0440\u0438\u044f\u0442\u0438\u0439 \u043f\u043e \u0432\u0441\u0435\u0439 \u0441\u0442\u0440\u0430\u043d\u0435, \u0441\u043f\u043e\u0441\u043e\u0431\u043d\u044b\u0445 \u043f\u043e\u0441\u0442\u0430\u0432\u043b\u044f\u0442\u044c \u0432\u044b\u0441\u043e\u043a\u043e\u043f\u0440\u043e\u0447\u043d\u0443\u044e \u0441\u0442\u0430\u043b\u044c, \u043c\u044b \u0442\u0430\u043a\u0436\u0435 \u043c\u043e\u0436\u0435\u043c \u0440\u0430\u0431\u043e\u0442\u0430\u0442\u044c \u0441 \u0432\u0430\u043c\u0438, \u0447\u0442\u043e\u0431\u044b \u0443\u043f\u0440\u0430\u0432\u043b\u044f\u0442\u044c \u0432\u0430\u0448\u0438\u043c\u0438 \u0437\u0430\u043f\u0430\u0441\u0430\u043c\u0438, \u0433\u0430\u0440\u0430\u043d\u0442\u0438\u0440\u0443\u044f, \u0447\u0442\u043e \u0432\u044b \u043f\u043e\u043b\u0443\u0447\u0438\u0442\u0435 \u043f\u0440\u043e\u0434\u0443\u043a\u0446\u0438\u044e \u0442\u043e\u0433\u0434\u0430 \u0438 \u0442\u0430\u043c, \u0433\u0434\u0435 \u043e\u043d\u0430 \u0432\u0430\u043c \u043d\u0443\u0436\u043d\u0430, \u0447\u0442\u043e\u0431\u044b \u043f\u043e\u0434\u0434\u0435\u0440\u0436\u0438\u0432\u0430\u0442\u044c \u0431\u0435\u0441\u043f\u0435\u0440\u0435\u0431\u043e\u0439\u043d\u043e\u0441\u0442\u044c \u0432\u0430\u0448\u0435\u0433\u043e \u043f\u0440\u043e\u0438\u0437\u0432\u043e\u0434\u0441\u0442\u0432\u0430.<\/span><\/p>\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-594a9289 e-con-full e-flex e-con e-child\" data-id=\"594a9289\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-608707b9 elementor-align-left elementor-widget elementor-widget-button\" data-id=\"608707b9\" data-element_type=\"widget\" data-widget_type=\"button.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t<a class=\"elementor-button elementor-button-link elementor-size-sm\" href=\"#elementor-action:action=popup:open&settings=eyJpZCI6IjM5NTEiLCJ0b2dnbGUiOmZhbHNlfQ==\">\n\t\t\t\t\t\t<span class=\"elementor-button-content-wrapper\">\n\t\t\t\t\t\t<span class=\"elementor-button-icon\">\n\t\t\t\t<svg aria-hidden=\"true\" class=\"e-font-icon-svg e-fas-long-arrow-alt-right\" viewbox=\"0 0 448 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M313.941 216H12c-6.627 0-12 5.373-12 12v56c0 6.627 5.373 12 12 12h301.941v46.059c0 21.382 25.851 32.09 40.971 16.971l86.059-86.059c9.373-9.373 9.373-24.569 0-33.941l-86.059-86.059c-15.119-15.119-40.971-4.411-40.971 16.971V216z\"><\/path><\/svg>\t\t\t<\/span>\n\t\t\t\t\t\t\t\t\t<span class=\"elementor-button-text\">\u0417\u0410\u041f\u0420\u041e\u0421\u0418\u0422\u042c \u0426\u0415\u041d\u0423 <\/span>\n\t\t\t\t\t<\/span>\n\t\t\t\t\t<\/a>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-30a3ed06 e-flex e-con-boxed e-con e-child\" data-id=\"30a3ed06\" data-element_type=\"container\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t<div class=\"elementor-element elementor-element-6171c75 e-con-full e-flex e-con e-child\" data-id=\"6171c75\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-443034e elementor-widget elementor-widget-heading\" data-id=\"443034e\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\">\u0418\u0437\u0443\u0447\u0438\u0442\u0435 \u043d\u0430\u0448\u0438 \u0434\u043e\u0441\u0442\u0443\u043f\u043d\u044b\u0435 \u0441\u0442\u0430\u043b\u044c\u043d\u044b\u0435 \u0438\u0437\u0434\u0435\u043b\u0438\u044f \u0438 \u043c\u0430\u0440\u043a\u0438<\/h2>\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-50f3895a elementor-widget elementor-widget-text-editor\" data-id=\"50f3895a\" data-element_type=\"widget\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t<p style=\"-webkit-font-smoothing: antialiased; text-rendering: optimizelegibility; margin-bottom: 20px; font-size: 18px; font-weight: 400; letter-spacing: 0.2px; line-height: 30px; color: #5e5e5e; font-family: Jost, sans-serif; font-style: normal;\"><span style=\"color: #747474; font-size: 16px; letter-spacing: 0.2px;\">\u041d\u0430\u0448\u0438 \u0437\u043d\u0430\u043d\u0438\u044f \u0438 \u043e\u043f\u044b\u0442 \u043e\u0431\u0435\u0441\u043f\u0435\u0447\u0438\u0432\u0430\u044e\u0442 \u043f\u043e\u0447\u0442\u0438 100% \u0442\u043e\u0447\u043d\u0443\u044e \u043f\u043e\u0441\u0442\u0430\u0432\u043a\u0443 \u0438\u0437\u0434\u0435\u043b\u0438\u0439 \u0438\u0437 \u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u043e\u0439 \u0441\u0442\u0430\u043b\u0438, \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u0430\u043d\u043d\u044b\u0445 \u0438 \u0443\u043f\u0430\u043a\u043e\u0432\u0430\u043d\u043d\u044b\u0445 \u0432 \u0442\u043e\u0447\u043d\u043e\u043c \u0441\u043e\u043e\u0442\u0432\u0435\u0442\u0441\u0442\u0432\u0438\u0438 \u0441 \u0432\u0430\u0448\u0438\u043c\u0438 \u0441\u043f\u0435\u0446\u0438\u0444\u0438\u043a\u0430\u0446\u0438\u044f\u043c\u0438.<\/span><\/p>\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-7f789e06 e-con-full e-flex e-con e-child\" data-id=\"7f789e06\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-696109f2 elementor-align-left elementor-widget elementor-widget-button\" data-id=\"696109f2\" data-element_type=\"widget\" data-widget_type=\"button.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t<a class=\"elementor-button elementor-size-sm\" role=\"button\">\n\t\t\t\t\t\t<span class=\"elementor-button-content-wrapper\">\n\t\t\t\t\t\t<span class=\"elementor-button-icon\">\n\t\t\t\t<svg aria-hidden=\"true\" class=\"e-font-icon-svg e-fas-long-arrow-alt-right\" viewbox=\"0 0 448 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M313.941 216H12c-6.627 0-12 5.373-12 12v56c0 6.627 5.373 12 12 12h301.941v46.059c0 21.382 25.851 32.09 40.971 16.971l86.059-86.059c9.373-9.373 9.373-24.569 0-33.941l-86.059-86.059c-15.119-15.119-40.971-4.411-40.971 16.971V216z\"><\/path><\/svg>\t\t\t<\/span>\n\t\t\t\t\t\t\t\t\t<span class=\"elementor-button-text\">\u0421\u041c\u041e\u0422\u0420\u0415\u0422\u042c \u0412\u0421\u0415 \u0420\u0415\u0421\u0423\u0420\u0421\u042b<\/span>\n\t\t\t\t\t<\/span>\n\t\t\t\t\t<\/a>\n\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-35480a42 e-flex e-con-boxed e-con e-parent\" data-id=\"35480a42\" data-element_type=\"container\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t\t\t<div class=\"elementor-element elementor-element-1be4e684 elementor-widget elementor-widget-menu-anchor\" data-id=\"1be4e684\" data-element_type=\"widget\" data-widget_type=\"menu-anchor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<div class=\"elementor-menu-anchor\" id=\"CONTANTUS\"><\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-e7007b2 e-flex e-con-boxed e-con e-parent\" data-id=\"e7007b2\" data-element_type=\"container\" data-settings=\"{&quot;background_background&quot;:&quot;classic&quot;}\">\n\t\t\t\t\t<div class=\"e-con-inner\">\n\t\t<div class=\"elementor-element elementor-element-7e675e9 e-con-full e-flex e-con e-child\" data-id=\"7e675e9\" data-element_type=\"container\">\n\t\t\t\t<div class=\"elementor-element elementor-element-202d4eae elementor-widget elementor-widget-eael-adv-accordion\" data-id=\"202d4eae\" data-element_type=\"widget\" data-widget_type=\"eael-adv-accordion.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t        <div class=\"eael-adv-accordion\" id=\"eael-adv-accordion-202d4eae\" data-scroll-on-click=\"no\" data-scroll-speed=\"300\" data-accordion-id=\"202d4eae\" data-accordion-type=\"toggle\" data-toogle-speed=\"300\">\n    <div class=\"eael-accordion-list\">\n                <div id=\"is-alloy-steel-rust-proof\" class=\"elementor-tab-title eael-accordion-header\" tabindex=\"0\" data-tab=\"1\" aria-controls=\"elementor-tab-content-5391\"><svg aria-hidden=\"true\" class=\"fa-toggle e-font-icon-svg e-fas-angle-right\" viewbox=\"0 0 256 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M224.3 273l-136 136c-9.4 9.4-24.6 9.4-33.9 0l-22.6-22.6c-9.4-9.4-9.4-24.6 0-33.9l96.4-96.4-96.4-96.4c-9.4-9.4-9.4-24.6 0-33.9L54.3 103c9.4-9.4 24.6-9.4 33.9 0l136 136c9.5 9.4 9.5 24.6.1 34z\"><\/path><\/svg><h3 class=\"eael-accordion-tab-title\">\u0423\u0441\u0442\u043e\u0439\u0447\u0438\u0432\u0430 \u043b\u0438 \u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u043a \u0440\u0436\u0430\u0432\u0447\u0438\u043d\u0435?<\/h3><\/div><div id=\"elementor-tab-content-5391\" class=\"eael-accordion-content clearfix\" data-tab=\"1\" aria-labelledby=\"is-alloy-steel-rust-proof\"><p>\u041d\u0435\u0442, \u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u043d\u0435 \u044f\u0432\u043b\u044f\u0435\u0442\u0441\u044f \u043f\u043e\u043b\u043d\u043e\u0441\u0442\u044c\u044e \u0443\u0441\u0442\u043e\u0439\u0447\u0438\u0432\u043e\u0439 \u043a \u0440\u0436\u0430\u0432\u0447\u0438\u043d\u0435, \u043d\u043e \u043e\u043d\u0430 \u043c\u043e\u0436\u0435\u0442 \u0431\u044b\u0442\u044c \u0431\u043e\u043b\u0435\u0435 \u0443\u0441\u0442\u043e\u0439\u0447\u0438\u0432\u043e\u0439 \u043a \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u0438, \u0447\u0435\u043c \u043e\u0431\u044b\u0447\u043d\u0430\u044f \u0443\u0433\u043b\u0435\u0440\u043e\u0434\u0438\u0441\u0442\u0430\u044f \u0441\u0442\u0430\u043b\u044c, \u0432 \u0437\u0430\u0432\u0438\u0441\u0438\u043c\u043e\u0441\u0442\u0438 \u043e\u0442 \u0438\u0441\u043f\u043e\u043b\u044c\u0437\u0443\u0435\u043c\u044b\u0445 \u043b\u0435\u0433\u0438\u0440\u0443\u044e\u0449\u0438\u0445 \u044d\u043b\u0435\u043c\u0435\u043d\u0442\u043e\u0432, \u0442\u0430\u043a\u0438\u0445 \u043a\u0430\u043a \u0445\u0440\u043e\u043c \u0438 \u043d\u0438\u043a\u0435\u043b\u044c.<\/p><\/div>\n                <\/div><div class=\"eael-accordion-list\">\n                <div id=\"what-are-the-benefits-of-alloy-steel\" class=\"elementor-tab-title eael-accordion-header\" tabindex=\"0\" data-tab=\"2\" aria-controls=\"elementor-tab-content-5392\"><svg aria-hidden=\"true\" class=\"fa-toggle e-font-icon-svg e-fas-angle-right\" viewbox=\"0 0 256 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M224.3 273l-136 136c-9.4 9.4-24.6 9.4-33.9 0l-22.6-22.6c-9.4-9.4-9.4-24.6 0-33.9l96.4-96.4-96.4-96.4c-9.4-9.4-9.4-24.6 0-33.9L54.3 103c9.4-9.4 24.6-9.4 33.9 0l136 136c9.5 9.4 9.5 24.6.1 34z\"><\/path><\/svg><h3 class=\"eael-accordion-tab-title\">\u041a\u0430\u043a\u043e\u0432\u044b \u043f\u0440\u0435\u0438\u043c\u0443\u0449\u0435\u0441\u0442\u0432\u0430 \u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u043e\u0439 \u0441\u0442\u0430\u043b\u0438?<\/h3><\/div><div id=\"elementor-tab-content-5392\" class=\"eael-accordion-content clearfix\" data-tab=\"2\" aria-labelledby=\"what-are-the-benefits-of-alloy-steel\"><p>\u041b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u043e\u0431\u0435\u0441\u043f\u0435\u0447\u0438\u0432\u0430\u0435\u0442 \u043f\u043e\u0432\u044b\u0448\u0435\u043d\u043d\u0443\u044e \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c, \u0443\u0434\u0430\u0440\u043d\u0443\u044e \u0432\u044f\u0437\u043a\u043e\u0441\u0442\u044c, \u0442\u0432\u0435\u0440\u0434\u043e\u0441\u0442\u044c \u0438 \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u0443\u044e \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c \u043f\u043e \u0441\u0440\u0430\u0432\u043d\u0435\u043d\u0438\u044e \u0441 \u043e\u0431\u044b\u0447\u043d\u043e\u0439 \u0443\u0433\u043b\u0435\u0440\u043e\u0434\u0438\u0441\u0442\u043e\u0439 \u0441\u0442\u0430\u043b\u044c\u044e. \u041e\u043d\u0430 \u0442\u0430\u043a\u0436\u0435 \u043c\u043e\u0436\u0435\u0442 \u0431\u044b\u0442\u044c \u0430\u0434\u0430\u043f\u0442\u0438\u0440\u043e\u0432\u0430\u043d\u0430 \u0434\u043b\u044f \u043e\u043f\u0440\u0435\u0434\u0435\u043b\u0435\u043d\u043d\u044b\u0445 \u0441\u0432\u043e\u0439\u0441\u0442\u0432 \u0441 \u043f\u043e\u043c\u043e\u0449\u044c\u044e \u0440\u0430\u0437\u043b\u0438\u0447\u043d\u044b\u0445 \u043b\u0435\u0433\u0438\u0440\u0443\u044e\u0449\u0438\u0445 \u044d\u043b\u0435\u043c\u0435\u043d\u0442\u043e\u0432.<\/p><\/div>\n                <\/div><div class=\"eael-accordion-list\">\n                <div id=\"does-alloy-tarnish-easily\" class=\"elementor-tab-title eael-accordion-header\" tabindex=\"0\" data-tab=\"3\" aria-controls=\"elementor-tab-content-5393\"><svg aria-hidden=\"true\" class=\"fa-toggle e-font-icon-svg e-fas-angle-right\" viewbox=\"0 0 256 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M224.3 273l-136 136c-9.4 9.4-24.6 9.4-33.9 0l-22.6-22.6c-9.4-9.4-9.4-24.6 0-33.9l96.4-96.4-96.4-96.4c-9.4-9.4-9.4-24.6 0-33.9L54.3 103c9.4-9.4 24.6-9.4 33.9 0l136 136c9.5 9.4 9.5 24.6.1 34z\"><\/path><\/svg><h3 class=\"eael-accordion-tab-title\">\u041b\u0435\u0433\u043a\u043e \u043b\u0438 \u0441\u043f\u043b\u0430\u0432 \u0442\u0443\u0441\u043a\u043d\u0435\u0435\u0442?<\/h3><\/div><div id=\"elementor-tab-content-5393\" class=\"eael-accordion-content clearfix\" data-tab=\"3\" aria-labelledby=\"does-alloy-tarnish-easily\"><p>\u0421\u043a\u043b\u043e\u043d\u043d\u043e\u0441\u0442\u044c \u0441\u043f\u043b\u0430\u0432\u0430 \u043a \u043f\u043e\u0442\u0443\u0441\u043a\u043d\u0435\u043d\u0438\u044e \u0437\u0430\u0432\u0438\u0441\u0438\u0442 \u043e\u0442 \u0435\u0433\u043e \u0441\u043e\u0441\u0442\u0430\u0432\u0430. \u041d\u0435\u043a\u043e\u0442\u043e\u0440\u044b\u0435 \u0441\u043f\u043b\u0430\u0432\u044b, \u0442\u0430\u043a\u0438\u0435 \u043a\u0430\u043a \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c, \u0443\u0441\u0442\u043e\u0439\u0447\u0438\u0432\u044b \u043a \u043f\u043e\u0442\u0443\u0441\u043a\u043d\u0435\u043d\u0438\u044e, \u0432 \u0442\u043e \u0432\u0440\u0435\u043c\u044f \u043a\u0430\u043a \u0434\u0440\u0443\u0433\u0438\u0435 \u043c\u043e\u0433\u0443\u0442 \u043f\u043e\u0442\u0443\u0441\u043a\u043d\u0435\u0442\u044c \u0431\u043e\u043b\u0435\u0435 \u043b\u0435\u0433\u043a\u043e.<\/p><\/div>\n                <\/div><div class=\"eael-accordion-list\">\n                <div id=\"is-alloy-steel-safe-for-food\" class=\"elementor-tab-title eael-accordion-header\" tabindex=\"0\" data-tab=\"4\" aria-controls=\"elementor-tab-content-5394\"><svg aria-hidden=\"true\" class=\"fa-toggle e-font-icon-svg e-fas-angle-right\" viewbox=\"0 0 256 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M224.3 273l-136 136c-9.4 9.4-24.6 9.4-33.9 0l-22.6-22.6c-9.4-9.4-9.4-24.6 0-33.9l96.4-96.4-96.4-96.4c-9.4-9.4-9.4-24.6 0-33.9L54.3 103c9.4-9.4 24.6-9.4 33.9 0l136 136c9.5 9.4 9.5 24.6.1 34z\"><\/path><\/svg><h3 class=\"eael-accordion-tab-title\">\u0411\u0435\u0437\u043e\u043f\u0430\u0441\u043d\u0430 \u043b\u0438 \u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u0434\u043b\u044f \u043f\u0438\u0449\u0435\u0432\u044b\u0445 \u043f\u0440\u043e\u0434\u0443\u043a\u0442\u043e\u0432?<\/h3><\/div><div id=\"elementor-tab-content-5394\" class=\"eael-accordion-content clearfix\" data-tab=\"4\" aria-labelledby=\"is-alloy-steel-safe-for-food\"><p>\u0414\u0430, \u043d\u0435\u043a\u043e\u0442\u043e\u0440\u044b\u0435 \u0432\u0438\u0434\u044b \u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u043e\u0439 \u0441\u0442\u0430\u043b\u0438, \u043e\u0441\u043e\u0431\u0435\u043d\u043d\u043e \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c, \u0431\u0435\u0437\u043e\u043f\u0430\u0441\u043d\u044b \u0434\u043b\u044f \u043a\u043e\u043d\u0442\u0430\u043a\u0442\u0430 \u0441 \u043f\u0438\u0449\u0435\u0432\u044b\u043c\u0438 \u043f\u0440\u043e\u0434\u0443\u043a\u0442\u0430\u043c\u0438, \u043f\u043e\u0441\u043a\u043e\u043b\u044c\u043a\u0443 \u043e\u043d\u0438 \u0443\u0441\u0442\u043e\u0439\u0447\u0438\u0432\u044b \u043a \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u0438 \u0438 \u043d\u0435 \u0432\u044b\u0434\u0435\u043b\u044f\u044e\u0442 \u0432\u0440\u0435\u0434\u043d\u044b\u0445 \u0432\u0435\u0449\u0435\u0441\u0442\u0432.<\/p><\/div>\n                <\/div><div class=\"eael-accordion-list\">\n                <div id=\"whats-better-metal-or-alloy-steel\" class=\"elementor-tab-title eael-accordion-header\" tabindex=\"0\" data-tab=\"5\" aria-controls=\"elementor-tab-content-5395\"><svg aria-hidden=\"true\" class=\"fa-toggle e-font-icon-svg e-fas-angle-right\" viewbox=\"0 0 256 512\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\"><path d=\"M224.3 273l-136 136c-9.4 9.4-24.6 9.4-33.9 0l-22.6-22.6c-9.4-9.4-9.4-24.6 0-33.9l96.4-96.4-96.4-96.4c-9.4-9.4-9.4-24.6 0-33.9L54.3 103c9.4-9.4 24.6-9.4 33.9 0l136 136c9.5 9.4 9.5 24.6.1 34z\"><\/path><\/svg><h3 class=\"eael-accordion-tab-title\">\u0427\u0442\u043e \u043b\u0443\u0447\u0448\u0435: \u043c\u0435\u0442\u0430\u043b\u043b \u0438\u043b\u0438 \u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u0430\u044f \u0441\u0442\u0430\u043b\u044c?<\/h3><\/div><div id=\"elementor-tab-content-5395\" class=\"eael-accordion-content clearfix\" data-tab=\"5\" aria-labelledby=\"whats-better-metal-or-alloy-steel\"><p>\u00ab\u041b\u0443\u0447\u0448\u0435\u00bb \u0437\u0430\u0432\u0438\u0441\u0438\u0442 \u043e\u0442 \u043e\u0431\u043b\u0430\u0441\u0442\u0438 \u043f\u0440\u0438\u043c\u0435\u043d\u0435\u043d\u0438\u044f. \u041b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u043e\u0431\u044b\u0447\u043d\u043e \u043e\u0431\u043b\u0430\u0434\u0430\u0435\u0442 \u043f\u0440\u0435\u0432\u043e\u0441\u0445\u043e\u0434\u043d\u044b\u043c\u0438 \u043c\u0435\u0445\u0430\u043d\u0438\u0447\u0435\u0441\u043a\u0438\u043c\u0438 \u0441\u0432\u043e\u0439\u0441\u0442\u0432\u0430\u043c\u0438 \u0438 \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u043e\u0439 \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c\u044e \u043f\u043e \u0441\u0440\u0430\u0432\u043d\u0435\u043d\u0438\u044e \u0441 \u043e\u0431\u044b\u0447\u043d\u044b\u043c\u0438 \u043c\u0435\u0442\u0430\u043b\u043b\u0430\u043c\u0438, \u0447\u0442\u043e \u0434\u0435\u043b\u0430\u0435\u0442 \u0435\u0435 \u0431\u043e\u043b\u0435\u0435 \u043f\u043e\u0434\u0445\u043e\u0434\u044f\u0449\u0435\u0439 \u0434\u043b\u044f \u0441\u043b\u043e\u0436\u043d\u044b\u0445 \u043e\u0431\u043b\u0430\u0441\u0442\u0435\u0439 \u043f\u0440\u0438\u043c\u0435\u043d\u0435\u043d\u0438\u044f.<\/p><\/div>\n                <\/div><\/div>\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t<div class=\"elementor-element elementor-element-456dddac e-con-full e-flex e-con e-child\" data-id=\"456dddac\" data-element_type=\"container\" data-settings=\"{&quot;background_background&quot;:&quot;classic&quot;}\">\n\t\t<div class=\"elementor-element elementor-element-5731078d e-con-full e-flex e-con e-child\" data-id=\"5731078d\" data-element_type=\"container\" data-settings=\"{&quot;background_background&quot;:&quot;classic&quot;}\">\n\t\t\t\t<div class=\"elementor-element elementor-element-250baec4 elementor-widget elementor-widget-heading\" data-id=\"250baec4\" data-element_type=\"widget\" data-widget_type=\"heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t<h2 class=\"elementor-heading-title elementor-size-default\"><h3>\u041a\u041e\u041d\u0422\u0410\u041a\u0422<\/h3><\/h2>\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-49aade92 elementor-widget elementor-widget-shortcode\" data-id=\"49aade92\" data-element_type=\"widget\" data-widget_type=\"shortcode.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<div class=\"elementor-shortcode\"><div class=\"wpforms-container wpforms-container-full wpforms-form-abandonment wpforms-render-modern\" id=\"wpforms-3253\"><form id=\"wpforms-form-3253\" class=\"wpforms-validate wpforms-form wpforms-ajax-form\" data-formid=\"3253\" method=\"post\" enctype=\"multipart\/form-data\" action=\"\/wp-json\/wp\/v2\/pages\/5220\" data-token=\"637365b0e915045bfe0e99984885b0a2\" data-token-time=\"1793480098\" data-trp-original-action=\"\/ru\/wp-json\/wp\/v2\/pages\/5220\"><noscript class=\"wpforms-error-noscript\">\u0414\u043b\u044f \u0437\u0430\u043f\u043e\u043b\u043d\u0435\u043d\u0438\u044f \u0434\u0430\u043d\u043d\u043e\u0439 \u0444\u043e\u0440\u043c\u044b JavaScript \u0432 \u0431\u0440\u0430\u0443\u0437\u0435\u0440\u0435.<\/noscript><div class=\"wpforms-hidden\" id=\"wpforms-error-noscript\">\u0414\u043b\u044f \u0437\u0430\u043f\u043e\u043b\u043d\u0435\u043d\u0438\u044f \u0434\u0430\u043d\u043d\u043e\u0439 \u0444\u043e\u0440\u043c\u044b JavaScript \u0432 \u0431\u0440\u0430\u0443\u0437\u0435\u0440\u0435.<\/div><div class=\"wpforms-field-container\"><div id=\"wpforms-3253-field_0-container\" class=\"wpforms-field wpforms-field-name\" data-field-id=\"0\"><label class=\"wpforms-field-label wpforms-label-hide\" for=\"wpforms-3253-field_0\" aria-hidden=\"false\">\u0418\u043c\u044f <span class=\"wpforms-required-label\" aria-hidden=\"true\">*<\/span><\/label><input type=\"text\" id=\"wpforms-3253-field_0\" class=\"wpforms-field-large wpforms-field-required\" name=\"wpforms[fields][0]\" placeholder=\"\u0418\u043c\u044f*\" aria-errormessage=\"wpforms-3253-field_0-error\" required><\/div><div id=\"wpforms-3253-field_5-container\" class=\"wpforms-field wpforms-field-text\" data-field-id=\"5\"><label class=\"wpforms-field-label wpforms-label-hide\" for=\"wpforms-3253-field_5\" aria-hidden=\"false\">\u041e\u0434\u043d\u043e\u0441\u0442\u0440\u043e\u0447\u043d\u044b\u0439 \u0442\u0435\u043a\u0441\u0442<\/label><input type=\"text\" id=\"wpforms-3253-field_5\" class=\"wpforms-field-large\" name=\"wpforms[fields][5]\" placeholder=\"\u041f\u0440\u0435\u0434\u043c\u0435\u0442\" aria-errormessage=\"wpforms-3253-field_5-error\" ><\/div><div id=\"wpforms-3253-field_4-container\" class=\"wpforms-field wpforms-field-email\" data-field-id=\"4\"><label class=\"wpforms-field-label wpforms-label-hide\" for=\"wpforms-3253-field_4\" aria-hidden=\"false\">\u042d\u043b\u0435\u043a\u0442\u0440\u043e\u043d\u043d\u0430\u044f \u043f\u043e\u0447\u0442\u0430 <span class=\"wpforms-required-label\" aria-hidden=\"true\">*<\/span><\/label><input type=\"email\" id=\"wpforms-3253-field_4\" class=\"wpforms-field-large wpforms-field-required\" name=\"wpforms[fields][4]\" placeholder=\"\u042d\u043b\u0435\u043a\u0442\u0440\u043e\u043d\u043d\u0430\u044f \u043f\u043e\u0447\u0442\u0430*\" spellcheck=\"false\" aria-errormessage=\"wpforms-3253-field_4-error\" required><\/div><div id=\"wpforms-3253-field_2-container\" class=\"wpforms-field wpforms-field-textarea\" data-field-id=\"2\"><label class=\"wpforms-field-label wpforms-label-hide\" for=\"wpforms-3253-field_2\" aria-hidden=\"false\">\u041a\u043e\u043c\u043c\u0435\u043d\u0442\u0430\u0440\u0438\u0439 \u0438\u043b\u0438 \u0441\u043e\u043e\u0431\u0449\u0435\u043d\u0438\u0435 <span class=\"wpforms-required-label\" aria-hidden=\"true\">*<\/span><\/label><textarea id=\"wpforms-3253-field_2\" class=\"wpforms-field-large wpforms-field-required\" name=\"wpforms[fields][2]\" placeholder=\"\u0412\u0430\u0448\u0435 \u0441\u043e\u043e\u0431\u0449\u0435\u043d\u0438\u0435*\u0414\u043b\u0438\u043d\u0430*\u0428\u0438\u0440\u0438\u043d\u0430*\u0422\u043e\u043b\u0449\u0438\u043d\u0430*\u041a\u043e\u043b\u0438\u0447\u0435\u0441\u0442\u0432\u043e*\" aria-errormessage=\"wpforms-3253-field_2-error\" required><\/textarea><\/div><div id=\"wpforms-3253-field_6-container\" class=\"wpforms-field wpforms-field-hidden\" data-field-id=\"6\"><input type=\"hidden\" id=\"wpforms-3253-field_6\" name=\"wpforms[fields][6]\" value=\"https:\/\/steelprogroup.com\/ru\/wp-json\/wp\/v2\/pages\/5220\"><\/div><div id=\"wpforms-3253-field_8-container\" class=\"wpforms-field wpforms-field-hidden\" data-field-id=\"8\"><input type=\"hidden\" id=\"wpforms-3253-field_8\" name=\"wpforms[fields][8]\" value=\"{entry_geolocation}\"><\/div><\/div><!-- .wpforms-field-container --><div class=\"wpforms-submit-container\" ><input type=\"hidden\" name=\"wpforms[id]\" value=\"3253\"><input type=\"hidden\" name=\"page_title\" value=\"\"><input type=\"hidden\" name=\"page_url\" value=\"https:\/\/steelprogroup.com\/ru\/wp-json\/wp\/v2\/pages\/5220\"><button type=\"submit\" name=\"wpforms[submit]\" id=\"wpforms-submit-3253\" class=\"wpforms-submit\" data-alt-text=\"SENDING...\" data-submit-text=\"SEND MESSAGE\" aria-live=\"assertive\" value=\"wpforms-submit\">\u041e\u0422\u041f\u0420\u0410\u0412\u0418\u0422\u042c \u0421\u041e\u041e\u0411\u0429\u0415\u041d\u0418\u0415<\/button><img loading=\"lazy\" decoding=\"async\" src=\"https:\/\/steelprogroup.com\/wp-content\/plugins\/wpforms\/assets\/images\/submit-spin.svg\" class=\"wpforms-submit-spinner\" style=\"display: none;\" width=\"26\" height=\"26\" alt=\"\u0417\u0430\u0433\u0440\u0443\u0437\u043a\u0430\"><\/div><input type=\"hidden\" name=\"trp-form-language\" value=\"ru\"\/><\/form><\/div>  <!-- .wpforms-container --><\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<\/div>","protected":false},"excerpt":{"rendered":"<p>\u041b\u0415\u0413\u0418\u0420\u041e\u0412\u0410\u041d\u041d\u0410\u042f \u0421\u0422\u0410\u041b\u042c \u041f\u0440\u0435\u0432\u043e\u0441\u0445\u043e\u0434\u043d\u0430\u044f \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c. \u0423\u0441\u0442\u043e\u0439\u0447\u0438\u0432\u0430 \u043a \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u0438. \u0423\u043b\u0443\u0447\u0448\u0438\u0442\u0435 \u0441\u0432\u043e\u0438 \u043f\u0440\u043e\u0435\u043a\u0442\u044b \u0441 \u043f\u043e\u043c\u043e\u0449\u044c\u044e \u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u043e\u0439 \u0441\u0442\u0430\u043b\u0438. \u041a\u041e\u041d\u0422\u0410\u041a\u0422\u042b \u041f\u0440\u0435\u0438\u043c\u0443\u0449\u0435\u0441\u0442\u0432\u0430 \u043b\u0435\u0433\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u043e\u0439 \u0441\u0442\u0430\u043b\u0438 \u041d\u0430\u0439\u0434\u0438\u0442\u0435 [\u2026]<\/p>","protected":false},"author":1,"featured_media":0,"parent":0,"menu_order":34,"comment_status":"closed","ping_status":"closed","template":"","meta":{"_acf_changed":false,"_eb_attr":"","rank_math_lock_modified_date":false,"site-sidebar-layout":"no-sidebar","site-content-layout":"","ast-site-content-layout":"full-width-container","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"disabled","ast-breadcrumbs-content":"","ast-featured-img":"disabled","footer-sml-layout":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"class_list":["post-5220","page","type-page","status-publish","hentry"],"acf":[],"rankMath":{"parentDomain":"steelprogroup.com","noFollowDomains":[],"noFollowExcludeDomains":[],"noFollowExternalLinks":false,"featuredImageNotice":"\u041f\u043e\u043a\u0430\u0437\u0430\u043d\u043d\u043e\u0435 \u0438\u0437\u043e\u0431\u0440\u0430\u0436\u0435\u043d\u0438\u0435 \u0434\u043e\u043b\u0436\u043d\u043e \u0431\u044b\u0442\u044c \u0440\u0430\u0437\u043c\u0435\u0440\u043e\u043c \u043d\u0435 \u043c\u0435\u043d\u0435\u0435 200 \u043d\u0430 200 \u043f\u0438\u043a\u0441\u0435\u043b\u0435\u0439, \u0447\u0442\u043e\u0431\u044b \u0435\u0433\u043e \u043c\u043e\u0433\u043b\u0438 \u0443\u0432\u0438\u0434\u0435\u0442\u044c Facebook \u0438 \u0434\u0440\u0443\u0433\u0438\u0435 \u0441\u0430\u0439\u0442\u044b \u0441\u043e\u0446\u0438\u0430\u043b\u044c\u043d\u044b\u0445 \u0441\u0435\u0442\u0435\u0439.","pluginReviewed":false,"postSettings":{"linkSuggestions":true,"useFocusKeyword":false},"frontEndScore":false,"postName":"alloy-steel","permalinkFormat":"https:\/\/steelprogroup.com\/ru\/%pagename%\/","showLockModifiedDate":true,"assessor":{"focusKeywordLink":"https:\/\/steelprogroup.com\/wp-admin\/edit.php?focus_keyword=%focus_keyword%&post_type=%post_type%","hasTOCPlugin":true,"primaryTaxonomy":false,"serpData":{"title":"%title% | High-Performance Steel%page% %sep% %sitename%","description":"Alloy steel, enhanced with chromium and nickel, offers superior strength and corrosion resistance. Essential in automotive, aerospace, and construction.","focusKeywords":"Alloy Steel","pillarContent":false,"canonicalUrl":"","breadcrumbTitle":"","advancedRobots":{"max-snippet":"-1","max-video-preview":"-1","max-image-preview":"large"},"facebookTitle":"","facebookDescription":"","facebookImage":"","facebookImageID":"","facebookHasOverlay":false,"facebookImageOverlay":"","facebookAuthor":"","twitterCardType":"","twitterUseFacebook":true,"twitterTitle":"","twitterDescription":"","twitterImage":"","twitterImageID":"","twitterHasOverlay":false,"twitterImageOverlay":"","twitterPlayerUrl":"","twitterPlayerSize":"","twitterPlayerStream":"","twitterPlayerStreamCtype":"","twitterAppDescription":"","twitterAppIphoneName":"","twitterAppIphoneID":"","twitterAppIphoneUrl":"","twitterAppIpadName":"","twitterAppIpadID":"","twitterAppIpadUrl":"","twitterAppGoogleplayName":"","twitterAppGoogleplayID":"","twitterAppGoogleplayUrl":"","twitterAppCountry":"","robots":{"index":true},"twitterAuthor":"\u0438\u043c\u044f \u043f\u043e\u043b\u044c\u0437\u043e\u0432\u0430\u0442\u0435\u043b\u044f","primaryTerm":0,"authorName":"John","titleTemplate":"%title% %page% %sep% %sitename%","descriptionTemplate":"%excerpt%","showScoreFrontend":true,"lockModifiedDate":false},"powerWords":[],"diacritics":{"A":"[\\u0410\\u0430]","B":"[\\u0411\\u0431]","V":"[\\u0412\\u0432]","G":"[\\u0413\\u0433]","D":"[\\u0414\\u0434]","YE":"[\\u0415\\u0435]","YO":"[\\u0401\\u0451]","ZH":"[\\u0416\\u0436]","Z":"[\\u0417\\u0437]","EE":"[\\u0418\\u0438]","YI":"[\\u0419\\u0439]","K":"[\\u041A\\u043A]","L":"[\\u041B\\u043B]","M":"[\\u041C\\u043c]","P":"[\\u041F\\u043F]","T":"[\\u0422\\u0442]","U":"[\\u0423\\u0443]","F":"[\\u0424\\u0444]","H":"[\\u0425\\u0445]","TS":"[\\u0426\\u0446]","CH":"[\\u0427\\u0447]","SH":"[\\u0428\\u0448\\u0429\\u0449]","I":"[\\u042B\\u044B]","E":"[\\u042D\\u044D]","YU":"[\\u042E\\u044E]","YA":"[\\u042F\\u044F]","N":"[\\u041D\\u043D]"},"researchesTests":["contentHasTOC","contentHasShortParagraphs","contentHasAssets","keywordInTitle","keywordInMetaDescription","keywordInPermalink","keywordIn10Percent","keywordInContent","keywordInSubheadings","keywordInImageAlt","keywordDensity","keywordNotUsed","lengthContent","lengthPermalink","linksHasInternal","linksHasExternals","linksNotAllExternals","titleStartWithKeyword","titleSentiment","titleHasPowerWords","titleHasNumber","hasContentAI"],"hasRedirection":true,"hasBreadcrumb":true},"homeUrl":"https:\/\/steelprogroup.com\/ru","objectID":5220,"objectType":"post","locale":"ru","localeFull":"ru_RU","overlayImages":{"play":{"name":"Play \u0438\u043a\u043e\u043d\u043a\u0430","url":"https:\/\/steelprogroup.com\/wp-content\/plugins\/seo-by-rank-math\/assets\/admin\/img\/icon-play.png","path":"\/home\/steelprogroup\/htdocs\/steelprogroup.com\/wp-content\/plugins\/seo-by-rank-math\/assets\/admin\/img\/icon-play.png","position":"middle_center"},"gif":{"name":"GIF \u0438\u043a\u043e\u043d\u043a\u0430","url":"https:\/\/steelprogroup.com\/wp-content\/plugins\/seo-by-rank-math\/assets\/admin\/img\/icon-gif.png","path":"\/home\/steelprogroup\/htdocs\/steelprogroup.com\/wp-content\/plugins\/seo-by-rank-math\/assets\/admin\/img\/icon-gif.png","position":"middle_center"}},"defautOgImage":"https:\/\/steelprogroup.com\/wp-content\/plugins\/seo-by-rank-math\/assets\/admin\/img\/social-placeholder.jpg","customPermalinks":true,"isUserRegistered":false,"autoSuggestKeywords":false,"connectSiteUrl":"https:\/\/rankmath.com\/auth?site=https%3A%2F%2Fsteelprogroup.com%2Fru&r=https%3A%2F%2Fsteelprogroup.com%2Fru%2Fwp-json%2Fwp%2Fv2%2Fpages%2F5220%3Fnonce%3Da98a031a49&pro=1","maxTags":100,"trendsIcon":"<svg width=\"100%\" height=\"100%\" viewBox=\"0 0 36 36\" version=\"1.1\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\" xmlns:xlink=\"http:\/\/www.w3.org\/1999\/xlink\" fit=\"\" preserveAspectRatio=\"xMidYMid meet\" focusable=\"false\">\n\t\t<g id=\"Page-1\" stroke=\"none\" stroke-width=\"1\" fill=\"none\" fill-rule=\"evenodd\">\n\t\t\t<g id=\"Trends-Arrow\">\n\t\t\t\t<g id=\"TrendsArrow\">\n\t\t\t\t\t<path d=\"M1.11227159,26.3181534 L10.2875029,17.1429221 L13.7152617,20.5706809 L4.5400304,29.7459122 C4.20518633,30.0807563 3.66229681,30.0807562 3.32745277,29.7459122 L1.11136262,27.529822 C0.776518575,27.194978 0.776518548,26.6520885 1.11136262,26.3172444 L1.11227159,26.3181534 Z\" id=\"Shape\" fill=\"#4285F4\" fill-rule=\"nonzero\"><\/path>\n\t\t\t\t\t<path d=\"M14.3201543,14.3211528 L22.283717,22.2847155 L19.4658829,25.1025495 C19.1310388,25.4373936 18.5881494,25.4373937 18.2533053,25.1025495 L10.2906516,17.1398959 L13.1084857,14.3220618 C13.4429747,13.987572 13.9851638,13.9871653 14.3201543,14.3211528 Z\" id=\"Shape\" fill=\"#EA4335\" fill-rule=\"nonzero\"><\/path>\n\t\t\t\t\t<polygon id=\"Rectangle-path\" fill=\"#FABB05\" fill-rule=\"nonzero\" points=\"18.8573051 18.8577571 28.2843236 9.43073862 31.7120824 12.8584974 22.2850639 22.2855159\"><\/polygon>\n\t\t\t\t\t<path d=\"M35.0711567,15.5054713 L35.0711567,7 L35.0711567,7 C35.0711567,6.44771525 34.6234415,6 34.0711567,6 L25.5656854,6 L25.5656854,6 C25.0134007,6 24.5656854,6.44771525 24.5656854,7 C24.5656854,7.26521649 24.6710423,7.5195704 24.8585786,7.70710678 L33.3640499,16.2125781 L33.3640499,16.2125781 C33.7545742,16.6031024 34.3877392,16.6031024 34.7782635,16.2125781 C34.9657999,16.0250417 35.0711567,15.7706878 35.0711567,15.5054713 Z\" id=\"Shape\" fill=\"#34A853\" fill-rule=\"nonzero\"><\/path>\n\t\t\t\t\t<rect id=\"Rectangle-path\" x=\"0\" y=\"0\" width=\"36\" height=\"36\"><\/rect>\n\t\t\t\t<\/g>\n\t\t\t<\/g>\n\t\t<\/g>\n\t<\/svg>","showScore":true,"siteFavIcon":"https:\/\/steelprogroup.com\/wp-content\/uploads\/2024\/07\/cropped-Steel-pro-logo-\u8bbe\u8ba1-7-\u6062\u590d\u7684-32x32.png","canUser":{"general":false,"advanced":false,"snippet":false,"social":false,"analysis":false,"analytics":false,"content_ai":false},"isPro":true,"is_front_page":false,"trendsUpgradeLink":"https:\/\/steelprogroup.com\/wp-admin\/admin.php?page=rank-math&view=help","trendsUpgradeLabel":"\u0410\u043a\u0442\u0438\u0432\u0438\u0440\u043e\u0432\u0430\u0442\u044c \u0441\u0435\u0439\u0447\u0430\u0441","trendsPreviewImage":"https:\/\/steelprogroup.com\/wp-content\/plugins\/seo-by-rank-math\/assets\/admin\/img\/trends-preview.jpg","currentEditor":false,"homepageData":{"assessor":{"powerWords":[],"diacritics":true,"researchesTests":["contentHasTOC","contentHasShortParagraphs","contentHasAssets","keywordInTitle","keywordInMetaDescription","keywordInPermalink","keywordIn10Percent","keywordInContent","keywordInSubheadings","keywordInImageAlt","keywordDensity","keywordNotUsed","lengthContent","lengthPermalink","linksHasInternal","linksHasExternals","linksNotAllExternals","titleStartWithKeyword","titleSentiment","titleHasPowerWords","titleHasNumber","hasContentAI"],"hasBreadcrumb":true,"serpData":{"title":"%sitename% %page% %sep% %sitedesc%","description":"","titleTemplate":"%sitename% %page% %sep% %sitedesc%","descriptionTemplate":"","focusKeywords":"","breadcrumbTitle":"Home","robots":{"index":true},"advancedRobots":{"max-snippet":"-1","max-video-preview":"-1","max-image-preview":"large"},"facebookTitle":"","facebookDescription":"","facebookImage":"","facebookImageID":""}}},"tocTitle":"Table of Contents","tocExcludeHeadings":[],"listStyle":"ul"},"_links":{"self":[{"href":"https:\/\/steelprogroup.com\/ru\/wp-json\/wp\/v2\/pages\/5220","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/steelprogroup.com\/ru\/wp-json\/wp\/v2\/pages"}],"about":[{"href":"https:\/\/steelprogroup.com\/ru\/wp-json\/wp\/v2\/types\/page"}],"author":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ru\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ru\/wp-json\/wp\/v2\/comments?post=5220"}],"version-history":[{"count":0,"href":"https:\/\/steelprogroup.com\/ru\/wp-json\/wp\/v2\/pages\/5220\/revisions"}],"wp:attachment":[{"href":"https:\/\/steelprogroup.com\/ru\/wp-json\/wp\/v2\/media?parent=5220"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}