{"id":20025,"date":"2024-12-23T01:16:00","date_gmt":"2024-12-22T17:16:00","guid":{"rendered":"https:\/\/steelprogroup.com\/?p=20025"},"modified":"2024-12-23T15:54:53","modified_gmt":"2024-12-23T07:54:53","slug":"skd61-steel-equivalent","status":"publish","type":"post","link":"https:\/\/steelprogroup.com\/ru\/tool-steel\/grades\/h13\/skd61-steel-equivalent\/","title":{"rendered":"\u042d\u043a\u0432\u0438\u0432\u0430\u043b\u0435\u043d\u0442 \u0441\u0442\u0430\u043b\u0438 SKD61 | H13 | 1.2344"},"content":{"rendered":"<p class=\"wp-block-paragraph\">\u041f\u043e\u0441\u043a\u043e\u043b\u044c\u043a\u0443 \u043c\u044b \u043e\u0431\u0441\u043b\u0443\u0436\u0438\u0432\u0430\u0435\u043c \u043a\u043b\u0438\u0435\u043d\u0442\u043e\u0432 \u043f\u043e \u0432\u0441\u0435\u043c\u0443 \u043c\u0438\u0440\u0443, \u043c\u044b \u0447\u0430\u0441\u0442\u043e \u043f\u043e\u043b\u0443\u0447\u0430\u0435\u043c \u0437\u0430\u043f\u0440\u043e\u0441\u044b \u043d\u0430 \u0437\u0430\u043a\u0443\u043f\u043a\u0443 \u0438\u0437 \u0440\u0430\u0437\u043d\u044b\u0445 \u0440\u0435\u0433\u0438\u043e\u043d\u043e\u0432. \u0415\u0441\u043b\u0438 \u0432\u044b \u0438\u0449\u0435\u0442\u0435 \u044d\u043a\u0432\u0438\u0432\u0430\u043b\u0435\u043d\u0442\u043d\u044b\u0435 \u043c\u0430\u0442\u0435\u0440\u0438\u0430\u043b\u044b \u0434\u043b\u044f \u0441\u0442\u0430\u043b\u0438 SKD61, SteelPro Group \u043c\u043e\u0436\u0435\u0442 \u0432\u0430\u043c \u043f\u043e\u043c\u043e\u0447\u044c. \u041c\u044b \u043d\u0435 \u0442\u043e\u043b\u044c\u043a\u043e \u043f\u043e\u0441\u0442\u0430\u0432\u043b\u044f\u0435\u043c \u043f\u0440\u043e\u0434\u0443\u043a\u0446\u0438\u044e \u0438\u0437 \u0438\u043d\u0441\u0442\u0440\u0443\u043c\u0435\u043d\u0442\u0430\u043b\u044c\u043d\u043e\u0439 \u0441\u0442\u0430\u043b\u0438 SKD61, \u043d\u043e \u0438 \u043f\u0440\u0435\u0434\u043b\u0430\u0433\u0430\u0435\u043c \u0441\u0430\u043c\u043e\u0435 \u043f\u0440\u043e\u0444\u0435\u0441\u0441\u0438\u043e\u043d\u0430\u043b\u044c\u043d\u043e\u0435 \u0438 \u0442\u0435\u0440\u043f\u0435\u043b\u0438\u0432\u043e\u0435 \u043e\u0431\u0441\u043b\u0443\u0436\u0438\u0432\u0430\u043d\u0438\u0435.<\/p><h2 class=\"wp-block-heading\">\u0427\u0442\u043e \u0442\u0430\u043a\u043e\u0435 \u0441\u0442\u0430\u043b\u044c SKD61?<\/h2><p class=\"wp-block-paragraph\">SKD61 \u2014 \u0438\u043d\u0441\u0442\u0440\u0443\u043c\u0435\u043d\u0442\u0430\u043b\u044c\u043d\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u043f\u0440\u0435\u043c\u0438\u0443\u043c-\u043a\u043b\u0430\u0441\u0441\u0430, \u0438\u0437\u0432\u0435\u0441\u0442\u043d\u0430\u044f \u0441\u0432\u043e\u0435\u0439 \u0432\u044b\u0441\u043e\u043a\u043e\u0439 \u0442\u0432\u0435\u0440\u0434\u043e\u0441\u0442\u044c\u044e, \u0438\u0437\u043d\u043e\u0441\u043e\u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c\u044e \u0438 \u0442\u0435\u0440\u043c\u0438\u0447\u0435\u0441\u043a\u043e\u0439 \u0441\u0442\u0430\u0431\u0438\u043b\u044c\u043d\u043e\u0441\u0442\u044c\u044e. \u041e\u043d\u0430 \u0448\u0438\u0440\u043e\u043a\u043e \u0438\u0441\u043f\u043e\u043b\u044c\u0437\u0443\u0435\u0442\u0441\u044f \u0432 \u043f\u0440\u043e\u0438\u0437\u0432\u043e\u0434\u0441\u0442\u0432\u0435 \u0444\u043e\u0440\u043c, \u043b\u0438\u0442\u044c\u0435 \u043f\u043e\u0434 \u0434\u0430\u0432\u043b\u0435\u043d\u0438\u0435\u043c \u0438 \u0442\u044f\u0436\u0435\u043b\u043e\u043c \u043f\u0440\u043e\u0438\u0437\u0432\u043e\u0434\u0441\u0442\u0432\u0435, \u043e\u0431\u0435\u0441\u043f\u0435\u0447\u0438\u0432\u0430\u044f \u0434\u043e\u043b\u0433\u043e\u0432\u0435\u0447\u043d\u043e\u0441\u0442\u044c \u0434\u0430\u0436\u0435 \u0432 \u044d\u043a\u0441\u0442\u0440\u0435\u043c\u0430\u043b\u044c\u043d\u044b\u0445 \u0443\u0441\u043b\u043e\u0432\u0438\u044f\u0445.<\/p><h2 class=\"wp-block-heading\">\u041e\u0431\u0437\u043e\u0440 \u044d\u043a\u0432\u0438\u0432\u0430\u043b\u0435\u043d\u0442\u043e\u0432 \u0441\u0442\u0430\u043b\u0438 SKD61<\/h2><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u041e\u0431\u043b\u0430\u0441\u0442\u044c<\/strong><\/td><td><strong>\u042d\u043a\u0432\u0438\u0432\u0430\u043b\u0435\u043d\u0442\u043d\u0430\u044f \u043c\u0430\u0440\u043a\u0430 \u0441\u0442\u0430\u043b\u0438<\/strong><\/td><\/tr><tr><td>\u042f\u043f\u043e\u043d\u0438\u044f (JIS)<\/td><td>\u0421\u041a\u041461<\/td><\/tr><tr><td>\u0413\u0411 (\u041a\u0438\u0442\u0430\u0439)<\/td><td>4Cr5MoSiV<\/td><\/tr><tr><td>\u0413\u0435\u0440\u043c\u0430\u043d\u0438\u044f (\u0414\u0418\u041d)<\/td><td>1.2344<\/td><\/tr><tr><td>\u0421\u0428\u0410 (AISI)<\/td><td>\u041d13<\/td><\/tr><tr><td>\u041c\u0435\u0436\u0434\u0443\u043d\u0430\u0440\u043e\u0434\u043d\u044b\u0439 (\u0418\u0421\u041e)<\/td><td>X40CrMoV5-1<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u0421\u0440\u0430\u0432\u043d\u0435\u043d\u0438\u0435 \u0441\u0442\u0430\u043b\u0438 SKD61 | H13 | 1.2344<\/h2><h3 class=\"wp-block-heading\">\u0421\u0440\u0430\u0432\u043d\u0435\u043d\u0438\u0435 \u0445\u0438\u043c\u0438\u0447\u0435\u0441\u043a\u043e\u0433\u043e \u0441\u043e\u0441\u0442\u0430\u0432\u0430<\/h3><figure class=\"wp-block-table\"><table><tbody><tr><td>\u0422\u0438\u043f<\/td><td>\u0421<\/td><td>\u041c\u043d<\/td><td>\u041f<\/td><td>\u0421<\/td><td>\u0421\u0438<\/td><td>\u041a\u0440<\/td><td>\u0412<\/td><td>\u041c\u043e<\/td><\/tr><tr><td>\u041d13<\/td><td>0.32 &#8211; 0.45<\/td><td>0.2 &#8211; 0.6<\/td><td>\u2264 0,03<\/td><td>\u2264 0,03<\/td><td>0.8 &#8211; 1.25<\/td><td>4.75 &#8211; 5.5<\/td><td>0.8 &#8211; 1.2<\/td><td>1.1 &#8211; 1.75<\/td><\/tr><tr><td>1.2344\/X40CrMoV5-1<\/td><td>0.33 -0.41<\/td><td>0.25 &#8211; 0.5<\/td><td>\u2264 0,03<\/td><td>\u2264 0,02<\/td><td>0.8 &#8211; 1.2<\/td><td>4.8 &#8211; 5.5<\/td><td>&#8211;<\/td><td>0.3 &#8211; 0.5<\/td><\/tr><tr><td>\u0421\u041a\u041461<\/td><td>0.35 &#8211; 0.42<\/td><td>0.25 &#8211; 0.3<\/td><td>\u2264 0,02<\/td><td>\u2264 0,02<\/td><td>0.8 -1.2<\/td><td>4.8 &#8211; 5.5<\/td><td>0.8 &#8211; 1.15<\/td><td>1.5<\/td><\/tr><\/tbody><\/table><\/figure><h3 class=\"wp-block-heading\">\u0421\u0440\u0430\u0432\u043d\u0435\u043d\u0438\u0435 \u043c\u0435\u0445\u0430\u043d\u0438\u0447\u0435\u0441\u043a\u0438\u0445 \u0441\u0432\u043e\u0439\u0441\u0442\u0432<\/h3><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u041c\u0430\u0440\u043a\u0430 \u0441\u0442\u0430\u043b\u0438<\/strong><\/td><td><strong>BHN (\u043e\u0442\u043e\u0436\u0436\u0435\u043d\u043d\u044b\u0439)<\/strong><\/td><td><strong>BHN (\u0445\u043e\u043b\u043e\u0434\u043d\u043e\u0442\u044f\u043d\u0443\u0442\u044b\u0439)<\/strong><\/td><\/tr><tr><td>\u041d13<\/td><td>235 \u043c\u0430\u043a\u0441.<\/td><td>262 \u043c\u0430\u043a\u0441.<\/td><\/tr><tr><td>1.2344 \/ X40CrMoV5-1<\/td><td>229 \u043c\u0430\u043a\u0441.<\/td><td>250 \u043c\u0430\u043a\u0441.<\/td><\/tr><tr><td>\u0421\u041a\u041461<\/td><td>229 \u043c\u0430\u043a\u0441.<\/td><td>250 \u043c\u0430\u043a\u0441.<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u0421\u043e\u043e\u0431\u0440\u0430\u0436\u0435\u043d\u0438\u044f \u043f\u0440\u0438 \u0432\u044b\u0431\u043e\u0440\u0435 \u0441\u0442\u0430\u043b\u0438, \u044d\u043a\u0432\u0438\u0432\u0430\u043b\u0435\u043d\u0442\u043d\u043e\u0439 SKD61<\/h2><h3 class=\"wp-block-heading\">\u0420\u0430\u0441\u0445\u043e\u0434\u044b<\/h3><p class=\"wp-block-paragraph\">\u0415\u0441\u043b\u0438 \u0432\u044b \u0437\u0430\u043a\u0443\u043f\u0430\u0435\u0442\u0435 \u0437\u0430 \u0440\u0443\u0431\u0435\u0436\u043e\u043c, \u0432\u0441\u0435\u0433\u0434\u0430 \u0443\u0447\u0438\u0442\u044b\u0432\u0430\u0439\u0442\u0435 \u0441\u0442\u043e\u0438\u043c\u043e\u0441\u0442\u044c \u0434\u043e\u0441\u0442\u0430\u0432\u043a\u0438 \u0438 \u0438\u043c\u043f\u043e\u0440\u0442\u043d\u044b\u0435 \u043f\u043e\u0448\u043b\u0438\u043d\u044b. \u041d\u0430\u043f\u0440\u0438\u043c\u0435\u0440, \u043f\u043e\u043a\u0443\u043f\u043a\u0430 SKD61 \u0438\u0437 \u041a\u0438\u0442\u0430\u044f \u043c\u043e\u0436\u0435\u0442 \u043f\u0440\u0435\u0434\u043b\u043e\u0436\u0438\u0442\u044c \u0431\u043e\u043b\u0435\u0435 \u043d\u0438\u0437\u043a\u0443\u044e \u0446\u0435\u043d\u0443 \u043d\u0430 \u043c\u0430\u0442\u0435\u0440\u0438\u0430\u043b, \u043d\u043e \u0441\u0442\u043e\u0438\u043c\u043e\u0441\u0442\u044c \u0434\u043e\u0441\u0442\u0430\u0432\u043a\u0438 \u043c\u043e\u0436\u0435\u0442 \u043f\u043e\u0432\u043b\u0438\u044f\u0442\u044c \u043d\u0430 \u043e\u0431\u0449\u0443\u044e \u0441\u0442\u043e\u0438\u043c\u043e\u0441\u0442\u044c. \u041a\u0440\u0430\u0439\u043d\u0435 \u0432\u0430\u0436\u043d\u043e \u0443\u0447\u0438\u0442\u044b\u0432\u0430\u0442\u044c \u043e\u0431\u0449\u0438\u0435 \u0440\u0430\u0441\u0445\u043e\u0434\u044b, \u0430 \u043d\u0435 \u0442\u043e\u043b\u044c\u043a\u043e \u0441\u0442\u043e\u0438\u043c\u043e\u0441\u0442\u044c \u0441\u0430\u043c\u043e\u0439 \u0441\u0442\u0430\u043b\u0438.<\/p><h3 class=\"wp-block-heading\">\u0414\u043e\u0441\u0442\u0443\u043f\u043d\u043e\u0441\u0442\u044c<\/h3><p class=\"wp-block-paragraph\">\u0427\u0442\u043e \u043a\u0430\u0441\u0430\u0435\u0442\u0441\u044f \u0434\u043e\u0441\u0442\u0443\u043f\u043d\u043e\u0441\u0442\u0438, \u0442\u043e \u0441\u0442\u0430\u043b\u0438 H13 \u0438 SKD61 \u043b\u0435\u0433\u0447\u0435 \u043d\u0430\u0439\u0442\u0438 \u043f\u043e \u0432\u0441\u0435\u043c\u0443 \u043c\u0438\u0440\u0443. \u0421 \u0434\u0440\u0443\u0433\u043e\u0439 \u0441\u0442\u043e\u0440\u043e\u043d\u044b, \u0441\u0442\u0430\u043b\u044c 1.2344 \u043c\u043e\u0436\u0435\u0442 \u0431\u044b\u0442\u044c \u0441\u043b\u043e\u0436\u043d\u0435\u0435 \u0431\u044b\u0441\u0442\u0440\u043e \u043d\u0430\u0439\u0442\u0438, \u043e\u0441\u043e\u0431\u0435\u043d\u043d\u043e \u0437\u0430 \u043f\u0440\u0435\u0434\u0435\u043b\u0430\u043c\u0438 \u0415\u0432\u0440\u043e\u043f\u044b.<\/p><p class=\"wp-block-paragraph\">\u0412 SteelPro Group \u043c\u044b \u0433\u0430\u0440\u0430\u043d\u0442\u0438\u0440\u0443\u0435\u043c, \u0447\u0442\u043e \u0441\u0442\u0430\u043b\u044c SKD61 \u0438 \u0435\u0435 \u044d\u043a\u0432\u0438\u0432\u0430\u043b\u0435\u043d\u0442\u044b \u0431\u0443\u0434\u0443\u0442 \u0448\u0438\u0440\u043e\u043a\u043e \u0434\u043e\u0441\u0442\u0443\u043f\u043d\u044b \u0438 \u043c\u043e\u0433\u0443\u0442 \u0431\u044b\u0442\u044c \u0431\u044b\u0441\u0442\u0440\u043e \u043f\u043e\u043b\u0443\u0447\u0435\u043d\u044b, \u0433\u0434\u0435 \u0431\u044b \u0432\u044b \u043d\u0438 \u043d\u0430\u0445\u043e\u0434\u0438\u043b\u0438\u0441\u044c.&nbsp;<\/p><h3 class=\"wp-block-heading\">\u041a\u043e\u043d\u0442\u0440\u043e\u043b\u044c \u043a\u0430\u0447\u0435\u0441\u0442\u0432\u0430<\/h3><p class=\"wp-block-paragraph\">\u0425\u043e\u0442\u044f SKD61, H13 \u0438 1.2344 \u044f\u0432\u043b\u044f\u044e\u0442\u0441\u044f \u0432\u044b\u0441\u043e\u043a\u043e\u043a\u0430\u0447\u0435\u0441\u0442\u0432\u0435\u043d\u043d\u044b\u043c\u0438 \u0441\u0442\u0430\u043b\u044f\u043c\u0438, \u0432\u0430\u0436\u043d\u043e \u0443\u0431\u0435\u0434\u0438\u0442\u044c\u0441\u044f, \u0447\u0442\u043e \u0432\u044b \u0432\u044b\u0431\u0440\u0430\u043b\u0438 \u043f\u0440\u0430\u0432\u0438\u043b\u044c\u043d\u044b\u0439 \u043c\u0430\u0442\u0435\u0440\u0438\u0430\u043b \u0434\u043b\u044f \u0432\u0430\u0448\u0438\u0445 \u043a\u043e\u043d\u043a\u0440\u0435\u0442\u043d\u044b\u0445 \u0442\u0440\u0435\u0431\u043e\u0432\u0430\u043d\u0438\u0439. \u0423\u0431\u0435\u0434\u0438\u0442\u0435\u0441\u044c, \u0447\u0442\u043e \u043f\u043e\u0441\u0442\u0430\u0432\u0449\u0438\u043a \u043f\u0440\u0435\u0434\u043e\u0441\u0442\u0430\u0432\u043b\u044f\u0435\u0442 \u0441\u0435\u0440\u0442\u0438\u0444\u0438\u043a\u0430\u0442\u044b \u0438 \u0433\u0430\u0440\u0430\u043d\u0442\u0438\u0440\u0443\u0435\u0442, \u0447\u0442\u043e \u0441\u0442\u0430\u043b\u044c \u0441\u043e\u043e\u0442\u0432\u0435\u0442\u0441\u0442\u0432\u0443\u0435\u0442 \u0432\u0430\u0448\u0438\u043c \u0442\u0440\u0435\u0431\u0443\u0435\u043c\u044b\u043c \u0441\u0442\u0430\u043d\u0434\u0430\u0440\u0442\u0430\u043c.<\/p><h2 class=\"wp-block-heading\">\u0410\u043b\u044c\u0442\u0435\u0440\u043d\u0430\u0442\u0438\u0432\u043d\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u0434\u043b\u044f SKD61 | H13 | 1.2344 \u041f\u0440\u0438\u043c\u0435\u043d\u0435\u043d\u0438\u0435 \u0441\u0442\u0430\u043b\u0438<\/h2><p class=\"wp-block-paragraph\">\u0412 SteelPro Group \u043c\u044b \u043f\u043e\u043d\u0438\u043c\u0430\u0435\u043c, \u0447\u0442\u043e \u0438\u043d\u043e\u0433\u0434\u0430 \u0434\u0440\u0443\u0433\u0430\u044f \u043c\u0430\u0440\u043a\u0430 \u0441\u0442\u0430\u043b\u0438 \u043c\u043e\u0436\u0435\u0442 \u043b\u0443\u0447\u0448\u0435 \u043f\u043e\u0434\u0445\u043e\u0434\u0438\u0442\u044c \u0434\u043b\u044f \u0432\u0430\u0448\u0438\u0445 \u043a\u043e\u043d\u043a\u0440\u0435\u0442\u043d\u044b\u0445 \u043d\u0443\u0436\u0434. \u0412\u043e\u0442 \u043d\u0435\u0441\u043a\u043e\u043b\u044c\u043a\u043e \u0430\u043b\u044c\u0442\u0435\u0440\u043d\u0430\u0442\u0438\u0432 SKD61 \u043d\u0430 \u043e\u0441\u043d\u043e\u0432\u0435 \u0440\u0430\u0437\u043b\u0438\u0447\u043d\u044b\u0445 \u043f\u0440\u0438\u043c\u0435\u043d\u0435\u043d\u0438\u0439:<\/p><h3 class=\"wp-block-heading\">\u0414\u043b\u044f \u0432\u044b\u0441\u043e\u043a\u043e\u0442\u0435\u043c\u043f\u0435\u0440\u0430\u0442\u0443\u0440\u043d\u044b\u0445 \u043f\u0440\u0438\u043c\u0435\u043d\u0435\u043d\u0438\u0439<\/h3><p class=\"wp-block-paragraph\">\u0414\u043b\u044f \u0433\u043e\u0440\u044f\u0447\u0438\u0445 \u0440\u0430\u0431\u043e\u0442, \u0441\u0432\u044f\u0437\u0430\u043d\u043d\u044b\u0445 \u0441 \u0432\u044b\u0441\u043e\u043a\u0438\u043c\u0438 \u0442\u0435\u043c\u043f\u0435\u0440\u0430\u0442\u0443\u0440\u0430\u043c\u0438, <strong>\u041d11<\/strong> \u044f\u0432\u043b\u044f\u0435\u0442\u0441\u044f \u043d\u0430\u0434\u0435\u0436\u043d\u043e\u0439 \u0430\u043b\u044c\u0442\u0435\u0440\u043d\u0430\u0442\u0438\u0432\u043e\u0439. \u041e\u043d \u043e\u0431\u0435\u0441\u043f\u0435\u0447\u0438\u0432\u0430\u0435\u0442 \u0431\u043e\u043b\u044c\u0448\u043e\u0439 <strong>\u0442\u0435\u0440\u043c\u0438\u0447\u0435\u0441\u043a\u0430\u044f \u0441\u0442\u0430\u0431\u0438\u043b\u044c\u043d\u043e\u0441\u0442\u044c<\/strong> \u0438 \u0443\u0441\u0442\u043e\u0439\u0447\u0438\u0432\u043e\u0441\u0442\u044c \u043a \u0440\u0430\u0441\u0442\u0440\u0435\u0441\u043a\u0438\u0432\u0430\u043d\u0438\u044e \u043f\u0440\u0438 \u0432\u044b\u0441\u043e\u043a\u0438\u0445 \u0442\u0435\u043c\u043f\u0435\u0440\u0430\u0442\u0443\u0440\u0430\u0445, \u0447\u0442\u043e \u0434\u0435\u043b\u0430\u0435\u0442 \u0435\u0433\u043e \u0438\u0434\u0435\u0430\u043b\u044c\u043d\u044b\u043c \u0434\u043b\u044f \u0432\u044b\u0441\u043e\u043a\u043e\u0442\u0435\u043c\u043f\u0435\u0440\u0430\u0442\u0443\u0440\u043d\u043e\u0433\u043e \u0444\u043e\u0440\u043c\u043e\u0432\u0430\u043d\u0438\u044f \u0438 \u043a\u043e\u0432\u043a\u0438.<\/p><h3 class=\"wp-block-heading\">\u0414\u043b\u044f \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u0438 \u0438 \u0434\u043e\u043b\u0433\u043e\u0432\u0435\u0447\u043d\u043e\u0441\u0442\u0438<\/h3><p class=\"wp-block-paragraph\">\u0415\u0441\u043b\u0438 \u0432\u0430\u043c \u043d\u0443\u0436\u043d\u043e \u0431\u043e\u043b\u044c\u0448\u0435 <strong>\u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c<\/strong> \u043d\u0435 \u0436\u0435\u0440\u0442\u0432\u0443\u044f \u043f\u0440\u043e\u0438\u0437\u0432\u043e\u0434\u0438\u0442\u0435\u043b\u044c\u043d\u043e\u0441\u0442\u044c\u044e, \u0440\u0430\u0441\u0441\u043c\u043e\u0442\u0440\u0438\u0442\u0435 <strong>\u0418\u043d\u0441\u0442\u0440\u0443\u043c\u0435\u043d\u0442\u0430\u043b\u044c\u043d\u0430\u044f \u0441\u0442\u0430\u043b\u044c D2<\/strong>. \u041e\u043d \u043e\u0442\u043b\u0438\u0447\u043d\u043e \u043f\u043e\u0434\u0445\u043e\u0434\u0438\u0442 \u0434\u043b\u044f <strong>\u0445\u043e\u043b\u043e\u0434\u043d\u0430\u044f \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0430<\/strong> \u0438\u043d\u0441\u0442\u0440\u0443\u043c\u0435\u043d\u0442\u043e\u0432 \u0438 \u0438\u043c\u0435\u0435\u0442 \u0445\u043e\u0440\u043e\u0448\u0438\u0439 \u0431\u0430\u043b\u0430\u043d\u0441 \u0438\u0437\u043d\u043e\u0441\u043e\u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u0438 \u0438 \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u0438.<\/p><h2 class=\"wp-block-heading\">\u041f\u0440\u0438\u043e\u0431\u0440\u0435\u0442\u0438\u0442\u0435 \u0441\u0442\u0430\u043b\u044c SKD61 \u0443 SteelPro Group<\/h2><p class=\"wp-block-paragraph\">\u041b\u0438 <a href=\"https:\/\/steelprogroup.com\/ru\/tool-steel\/h13\/\">SKD61, H13, 1.2344<\/a>, \u0438\u043b\u0438 \u043b\u044e\u0431\u043e\u0439 \u0434\u0440\u0443\u0433\u043e\u0439 \u044d\u043a\u0432\u0438\u0432\u0430\u043b\u0435\u043d\u0442, \u043c\u044b \u043f\u043e\u0441\u0442\u0430\u0432\u043b\u044f\u0435\u043c \u0432\u044b\u0441\u043e\u043a\u043e\u043a\u0430\u0447\u0435\u0441\u0442\u0432\u0435\u043d\u043d\u044b\u0435 \u043c\u0430\u0442\u0435\u0440\u0438\u0430\u043b\u044b, \u043f\u043e\u0434\u043a\u0440\u0435\u043f\u043b\u0435\u043d\u043d\u044b\u0435 \u043e\u0442\u0440\u0430\u0441\u043b\u0435\u0432\u044b\u043c \u043e\u043f\u044b\u0442\u043e\u043c. \u0411\u043b\u0430\u0433\u043e\u0434\u0430\u0440\u044f \u043d\u0430\u0448\u0435\u0439 \u043e\u0431\u0448\u0438\u0440\u043d\u043e\u0439 \u0433\u043b\u043e\u0431\u0430\u043b\u044c\u043d\u043e\u0439 \u0441\u0435\u0442\u0438 \u0432\u044b \u043c\u043e\u0436\u0435\u0442\u0435 \u0440\u0430\u0441\u0441\u0447\u0438\u0442\u044b\u0432\u0430\u0442\u044c \u043d\u0430 \u0441\u0432\u043e\u0435\u0432\u0440\u0435\u043c\u0435\u043d\u043d\u044b\u0435 \u043f\u043e\u0441\u0442\u0430\u0432\u043a\u0438 \u0438 \u043d\u0438\u043a\u043e\u0433\u0434\u0430 \u0431\u043e\u043b\u044c\u0448\u0435 \u043d\u0435 \u0431\u0435\u0441\u043f\u043e\u043a\u043e\u0438\u0442\u044c\u0441\u044f \u043e \u043d\u0435\u0445\u0432\u0430\u0442\u043a\u0435 \u043c\u0430\u0442\u0435\u0440\u0438\u0430\u043b\u043e\u0432. \u0421\u0432\u044f\u0436\u0438\u0442\u0435\u0441\u044c \u0441 \u043d\u0430\u043c\u0438 \u0441\u0435\u0433\u043e\u0434\u043d\u044f, \u0447\u0442\u043e\u0431\u044b \u0443\u0437\u043d\u0430\u0442\u044c, \u043a\u0430\u043a \u043d\u0430\u0448\u0438 \u0432\u044b\u0441\u043e\u043a\u043e\u043a\u0430\u0447\u0435\u0441\u0442\u0432\u0435\u043d\u043d\u044b\u0435 \u0441\u0442\u0430\u043b\u044c\u043d\u044b\u0435 \u0438\u0437\u0434\u0435\u043b\u0438\u044f \u0438 \u044d\u043a\u0441\u043f\u0435\u0440\u0442\u043d\u043e\u0435 \u043e\u0431\u0441\u043b\u0443\u0436\u0438\u0432\u0430\u043d\u0438\u0435 \u043c\u043e\u0433\u0443\u0442 \u043f\u0440\u043e\u0434\u0432\u0438\u043d\u0443\u0442\u044c \u0432\u0430\u0448 \u0431\u0438\u0437\u043d\u0435\u0441 \u0432\u043f\u0435\u0440\u0435\u0434!<\/p>","protected":false},"excerpt":{"rendered":"<p>\u041f\u043e\u0441\u043a\u043e\u043b\u044c\u043a\u0443 \u043c\u044b \u043e\u0431\u0441\u043b\u0443\u0436\u0438\u0432\u0430\u0435\u043c \u043a\u043b\u0438\u0435\u043d\u0442\u043e\u0432 \u043f\u043e \u0432\u0441\u0435\u043c\u0443 \u043c\u0438\u0440\u0443, \u043c\u044b \u0447\u0430\u0441\u0442\u043e \u043f\u043e\u043b\u0443\u0447\u0430\u0435\u043c \u0437\u0430\u043f\u0440\u043e\u0441\u044b \u043d\u0430 \u0437\u0430\u043a\u0443\u043f\u043a\u0438 \u0438\u0437 \u0440\u0430\u0437\u043d\u044b\u0445 \u0440\u0435\u0433\u0438\u043e\u043d\u043e\u0432. \u0415\u0441\u043b\u0438 \u0432\u044b \u0438\u0449\u0435\u0442\u0435 [\u2026]<\/p>","protected":false},"author":1,"featured_media":19991,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"_eb_attr":"","rank_math_lock_modified_date":false,"site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"categories":[4296,4294,4293],"tags":[],"class_list":["post-20025","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-h13","category-grades-tool-steel","category-tool-steel"],"acf":[],"_links":{"self":[{"href":"https:\/\/steelprogroup.com\/ru\/wp-json\/wp\/v2\/posts\/20025","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/steelprogroup.com\/ru\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/steelprogroup.com\/ru\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ru\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ru\/wp-json\/wp\/v2\/comments?post=20025"}],"version-history":[{"count":0,"href":"https:\/\/steelprogroup.com\/ru\/wp-json\/wp\/v2\/posts\/20025\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ru\/wp-json\/wp\/v2\/media\/19991"}],"wp:attachment":[{"href":"https:\/\/steelprogroup.com\/ru\/wp-json\/wp\/v2\/media?parent=20025"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/steelprogroup.com\/ru\/wp-json\/wp\/v2\/categories?post=20025"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/steelprogroup.com\/ru\/wp-json\/wp\/v2\/tags?post=20025"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}