{"id":7858,"date":"2024-08-08T03:52:00","date_gmt":"2024-08-07T19:52:00","guid":{"rendered":"https:\/\/app11147.cloudwayssites.com\/?p=7858"},"modified":"2025-02-18T10:25:27","modified_gmt":"2025-02-18T02:25:27","slug":"austenitic","status":"publish","type":"post","link":"https:\/\/steelprogroup.com\/ru\/stainless-steel\/type\/austenitic\/","title":{"rendered":"\u0410\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0430\u044f \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c: \u043e\u043f\u0440\u0435\u0434\u0435\u043b\u0435\u043d\u0438\u0435, \u0441\u043e\u0441\u0442\u0430\u0432, \u0441\u0432\u043e\u0439\u0441\u0442\u0432\u0430, \u043c\u0430\u0440\u043a\u0438, \u043f\u0440\u0438\u043c\u0435\u043d\u0435\u043d\u0438\u0435 \u0438 \u043c\u043d\u043e\u0433\u043e\u0435 \u0434\u0440\u0443\u0433\u043e\u0435"},"content":{"rendered":"<h2 class=\"wp-block-heading\">\u0427\u0442\u043e \u0442\u0430\u043a\u043e\u0435 \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0430\u044f \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c?<\/h2><p class=\"wp-block-paragraph\">\u0410\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0430\u044f \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u2014 \u043e\u0434\u0438\u043d \u0438\u0437 \u043f\u044f\u0442\u0438 \u043e\u0441\u043d\u043e\u0432\u043d\u044b\u0445 \u043a\u043b\u0430\u0441\u0441\u043e\u0432 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0435\u0439 \u0441\u0442\u0430\u043b\u0438, \u043e\u043f\u0440\u0435\u0434\u0435\u043b\u044f\u0435\u043c\u044b\u0445 \u043a\u0440\u0438\u0441\u0442\u0430\u043b\u043b\u0438\u0447\u0435\u0441\u043a\u043e\u0439 \u0441\u0442\u0440\u0443\u043a\u0442\u0443\u0440\u043e\u0439 \u0441 \u0433\u0440\u0430\u043d\u0435\u0446\u0435\u043d\u0442\u0440\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u043e\u0439 \u043a\u0443\u0431\u0438\u0447\u0435\u0441\u043a\u043e\u0439 (\u0413\u0426\u041a) \u043a\u0440\u0438\u0441\u0442\u0430\u043b\u043b\u0438\u0447\u0435\u0441\u043a\u043e\u0439 \u0441\u0442\u0440\u0443\u043a\u0442\u0443\u0440\u043e\u0439, \u0432 \u043e\u0441\u043d\u043e\u0432\u043d\u043e\u043c \u0441\u043e\u0441\u0442\u043e\u044f\u0449\u0435\u0439 \u0438\u0437 \u0445\u0440\u043e\u043c\u0430 15-32% \u0438 \u043d\u0438\u043a\u0435\u043b\u044f 8-37%, \u0441 \u0431\u0430\u043b\u0430\u043d\u0441\u043e\u043c \u0434\u0440\u0443\u0433\u0438\u0445 \u044d\u043b\u0435\u043c\u0435\u043d\u0442\u043e\u0432, \u0442\u0430\u043a\u0438\u0445 \u043a\u0430\u043a \u043c\u0430\u0440\u0433\u0430\u043d\u0435\u0446 \u0438 \u0430\u0437\u043e\u0442. \u0410\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0430\u044f \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u043e\u0431\u043b\u0430\u0434\u0430\u0435\u0442 \u043f\u0440\u0435\u0432\u043e\u0441\u0445\u043e\u0434\u043d\u043e\u0439 \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u043e\u0439 \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c\u044e \u0438 \u0444\u043e\u0440\u043c\u0443\u0435\u043c\u043e\u0441\u0442\u044c\u044e, \u0432\u044b\u0441\u043e\u043a\u043e\u0439 \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c\u044e \u0438 \u043f\u043b\u0430\u0441\u0442\u0438\u0447\u043d\u043e\u0441\u0442\u044c\u044e, \u0430 \u0442\u0430\u043a\u0436\u0435 \u043d\u0435\u043c\u0430\u0433\u043d\u0438\u0442\u043d\u0430. \u0420\u0430\u0441\u043f\u0440\u043e\u0441\u0442\u0440\u0430\u043d\u0435\u043d\u043d\u044b\u0435 \u043c\u0430\u0440\u043a\u0438 \u0432\u043a\u043b\u044e\u0447\u0430\u044e\u0442 304, 316 \u0438 310. \u0410\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0430\u044f \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u0448\u0438\u0440\u043e\u043a\u043e \u0438\u0441\u043f\u043e\u043b\u044c\u0437\u0443\u0435\u0442\u0441\u044f \u0432 \u043f\u0438\u0449\u0435\u0432\u043e\u0439, \u0445\u0438\u043c\u0438\u0447\u0435\u0441\u043a\u043e\u0439 \u0438 \u043c\u0435\u0434\u0438\u0446\u0438\u043d\u0441\u043a\u043e\u0439 \u043f\u0440\u043e\u043c\u044b\u0448\u043b\u0435\u043d\u043d\u043e\u0441\u0442\u0438.&nbsp;<\/p><h3 class=\"wp-block-heading\">\u041a\u0440\u0438\u0441\u0442\u0430\u043b\u043b\u0438\u0447\u0435\u0441\u043a\u0430\u044f \u0441\u0442\u0440\u0443\u043a\u0442\u0443\u0440\u0430 \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u043e\u0439 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0435\u0439 \u0441\u0442\u0430\u043b\u0438<\/h3><p class=\"wp-block-paragraph\">\u0410\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0430\u044f \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u0438\u043c\u0435\u0435\u0442 \u0433\u0440\u0430\u043d\u0435\u0446\u0435\u043d\u0442\u0440\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u0443\u044e \u043a\u0443\u0431\u0438\u0447\u0435\u0441\u043a\u0443\u044e (\u0413\u0426\u041a) \u043a\u0440\u0438\u0441\u0442\u0430\u043b\u043b\u0438\u0447\u0435\u0441\u043a\u0443\u044e \u0441\u0442\u0440\u0443\u043a\u0442\u0443\u0440\u0443. \u042d\u0442\u043e \u0442\u0438\u043f \u043a\u0440\u0438\u0441\u0442\u0430\u043b\u043b\u0438\u0447\u0435\u0441\u043a\u043e\u0439 \u0441\u0442\u0440\u0443\u043a\u0442\u0443\u0440\u044b. \u041f\u0440\u0435\u0434\u0441\u0442\u0430\u0432\u044c\u0442\u0435 \u0441\u0435\u0431\u0435 \u043a\u0443\u0431 \u0441 \u0430\u0442\u043e\u043c\u043e\u043c \u0432 \u043a\u0430\u0436\u0434\u043e\u043c \u0438\u0437 \u0432\u043e\u0441\u044c\u043c\u0438 \u0443\u0433\u043b\u043e\u0432 \u0438 \u0434\u043e\u043f\u043e\u043b\u043d\u0438\u0442\u0435\u043b\u044c\u043d\u044b\u043c \u0430\u0442\u043e\u043c\u043e\u043c \u0432 \u0446\u0435\u043d\u0442\u0440\u0435 \u043a\u0430\u0436\u0434\u043e\u0439 \u0433\u0440\u0430\u043d\u0438. \u0422\u0430\u043a\u0430\u044f \u0441\u0442\u0440\u0443\u043a\u0442\u0443\u0440\u0430 \u043e\u0447\u0435\u043d\u044c \u043a\u043e\u043c\u043f\u0430\u043a\u0442\u043d\u0430, \u0430\u0442\u043e\u043c\u044b \u0440\u0430\u0441\u043f\u043e\u043b\u043e\u0436\u0435\u043d\u044b \u0431\u043b\u0438\u0437\u043a\u043e \u0434\u0440\u0443\u0433 \u043a \u0434\u0440\u0443\u0433\u0443, \u0447\u0442\u043e \u0434\u0435\u043b\u0430\u0435\u0442 \u043c\u0430\u0442\u0435\u0440\u0438\u0430\u043b \u0431\u043e\u043b\u0435\u0435 \u0441\u0442\u0430\u0431\u0438\u043b\u044c\u043d\u044b\u043c \u0438 \u043c\u0435\u043d\u0435\u0435 \u0441\u043a\u043b\u043e\u043d\u043d\u044b\u043c \u043a \u0440\u0430\u0437\u0440\u0443\u0448\u0435\u043d\u0438\u044e \u043f\u0440\u0438 \u0434\u0435\u0444\u043e\u0440\u043c\u0430\u0446\u0438\u0438.&nbsp;<\/p><p class=\"wp-block-paragraph\">\u0422\u0430\u043a\u0430\u044f \u0441\u0442\u0440\u0443\u043a\u0442\u0443\u0440\u0430 \u043e\u0431\u0435\u0441\u043f\u0435\u0447\u0438\u0432\u0430\u0435\u0442 \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u043e\u0439 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0435\u0439 \u0441\u0442\u0430\u043b\u0438:<\/p><ul class=\"wp-block-list\"><li>\u0412\u044b\u0441\u043e\u043a\u0430\u044f \u043f\u043b\u0430\u0441\u0442\u0438\u0447\u043d\u043e\u0441\u0442\u044c, \u0432\u044f\u0437\u043a\u043e\u0441\u0442\u044c \u0438 \u043a\u043e\u0432\u043a\u043e\u0441\u0442\u044c<\/li>\n\n<li>\u0425\u043e\u0440\u043e\u0448\u0438\u0435 \u043c\u0435\u0445\u0430\u043d\u0438\u0447\u0435\u0441\u043a\u0438\u0435 \u0441\u0432\u043e\u0439\u0441\u0442\u0432\u0430 \u043f\u0440\u0438 \u0432\u044b\u0441\u043e\u043a\u0438\u0445 \u0438 \u043d\u0438\u0437\u043a\u0438\u0445 \u0442\u0435\u043c\u043f\u0435\u0440\u0430\u0442\u0443\u0440\u0430\u0445<\/li>\n\n<li>\u0412\u044b\u0441\u043e\u043a\u0430\u044f \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u0430\u044f \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c \u0438 \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c \u043a \u043e\u043a\u0438\u0441\u043b\u0435\u043d\u0438\u044e<\/li>\n\n<li>\u041d\u0435\u043c\u0430\u0433\u043d\u0438\u0442\u043d\u044b\u0435 \u0441\u0432\u043e\u0439\u0441\u0442\u0432\u0430<\/li><\/ul><p class=\"wp-block-paragraph\"><\/p><h3 class=\"wp-block-heading\">\u041a\u0430\u043a \u0444\u043e\u0440\u043c\u0438\u0440\u0443\u0435\u0442\u0441\u044f \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0430\u044f \u0441\u0442\u0440\u0443\u043a\u0442\u0443\u0440\u0430 \u0432 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0435\u0439 \u0441\u0442\u0430\u043b\u0438?<\/h3><p class=\"wp-block-paragraph\">\u0410\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u044b\u0435 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0438\u0435 \u0441\u0442\u0430\u043b\u0438 \u0434\u043e\u0441\u0442\u0438\u0433\u0430\u044e\u0442 \u0441\u0432\u043e\u0435\u0439 \u0443\u043d\u0438\u043a\u0430\u043b\u044c\u043d\u043e\u0439 \u0441\u0442\u0440\u0443\u043a\u0442\u0443\u0440\u044b \u0437\u0430 \u0441\u0447\u0435\u0442 \u0434\u043e\u0431\u0430\u0432\u043b\u0435\u043d\u0438\u044f \u043b\u0435\u0433\u0438\u0440\u0443\u044e\u0449\u0438\u0445 \u044d\u043b\u0435\u043c\u0435\u043d\u0442\u043e\u0432, \u0442\u0430\u043a\u0438\u0445 \u043a\u0430\u043a <strong>\u043d\u0438\u043a\u0435\u043b\u044c<\/strong> \u0438 <strong>\u0445\u0440\u043e\u043c<\/strong>.&nbsp;<\/p><p class=\"wp-block-paragraph\">\u0412 <strong>\u0447\u0438\u0441\u0442\u043e\u0435 \u0436\u0435\u043b\u0435\u0437\u043e<\/strong> \u0438\u043b\u0438 <strong>\u0443\u0433\u043b\u0435\u0440\u043e\u0434\u0438\u0441\u0442\u0430\u044f \u0441\u0442\u0430\u043b\u044c<\/strong>, <strong>\u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0430\u044f (\u0433\u0440\u0430\u043d\u0435\u0446\u0435\u043d\u0442\u0440\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u0430\u044f \u043a\u0443\u0431\u0438\u0447\u0435\u0441\u043a\u0430\u044f) \u0441\u0442\u0440\u0443\u043a\u0442\u0443\u0440\u0430 \u0441\u0442\u0430\u0431\u0438\u043b\u044c\u043d\u0430 \u0442\u043e\u043b\u044c\u043a\u043e \u043f\u0440\u0438 \u0432\u044b\u0441\u043e\u043a\u0438\u0445 \u0442\u0435\u043c\u043f\u0435\u0440\u0430\u0442\u0443\u0440\u0430\u0445<\/strong>\u2014 \u043e\u043a\u043e\u043b\u043e 1340\u00b0F (727\u00b0C) \u0438\u043b\u0438 \u0432\u044b\u0448\u0435. \u041e\u0434\u043d\u0430\u043a\u043e, \u043a\u043e\u0433\u0434\u0430 \u043f\u0440\u0438\u0431\u043b\u0438\u0437\u0438\u0442\u0435\u043b\u044c\u043d\u043e <strong>18% \u0445\u0440\u043e\u043c<\/strong> \u0438<strong> 8% \u043d\u0438\u043a\u0435\u043b\u044c<\/strong> \u0434\u043e\u0431\u0430\u0432\u043b\u044f\u044e\u0442\u0441\u044f \u043a \u0441\u0442\u0430\u043b\u0438, \u044d\u0442\u0430 \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0430\u044f \u0441\u0442\u0440\u0443\u043a\u0442\u0443\u0440\u0430 \u0441\u0442\u0430\u043d\u043e\u0432\u0438\u0442\u0441\u044f <strong>\u0441\u0442\u0430\u0431\u0438\u043b\u044c\u043d\u044b\u0439<\/strong> \u0447\u0435\u0440\u0435\u0437 <strong>\u0432\u0435\u0441\u044c \u0434\u0438\u0430\u043f\u0430\u0437\u043e\u043d \u0442\u0435\u043c\u043f\u0435\u0440\u0430\u0442\u0443\u0440<\/strong>, \u043e\u0442 \u043a\u043e\u043c\u043d\u0430\u0442\u043d\u043e\u0439 \u0442\u0435\u043c\u043f\u0435\u0440\u0430\u0442\u0443\u0440\u044b \u0434\u043e \u0442\u043e\u0447\u043a\u0438 \u043f\u043b\u0430\u0432\u043b\u0435\u043d\u0438\u044f.<\/p><p class=\"wp-block-paragraph\">\u041d\u0438\u043a\u0435\u043b\u044c \u0434\u0435\u0439\u0441\u0442\u0432\u0443\u0435\u0442 \u043a\u0430\u043a <strong>\u0441\u0442\u0430\u0431\u0438\u043b\u0438\u0437\u0430\u0442\u043e\u0440 \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u0430<\/strong>, \u0447\u0442\u043e \u043f\u043e\u0437\u0432\u043e\u043b\u044f\u0435\u0442 \u0441\u043e\u0445\u0440\u0430\u043d\u044f\u0442\u044c \u0433\u0440\u0430\u043d\u0435\u0446\u0435\u043d\u0442\u0440\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u0443\u044e \u043a\u0443\u0431\u0438\u0447\u0435\u0441\u043a\u0443\u044e \u0440\u0435\u0448\u0435\u0442\u043a\u0443 \u0434\u0430\u0436\u0435 \u043f\u0440\u0438 \u0431\u043e\u043b\u0435\u0435 \u043d\u0438\u0437\u043a\u0438\u0445 \u0442\u0435\u043c\u043f\u0435\u0440\u0430\u0442\u0443\u0440\u0430\u0445. \u0425\u0440\u043e\u043c \u043d\u0435 \u0442\u043e\u043b\u044c\u043a\u043e \u043f\u043e\u0432\u044b\u0448\u0430\u0435\u0442 \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u0443\u044e \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c, \u043d\u043e \u0438 \u0441\u043f\u043e\u0441\u043e\u0431\u0441\u0442\u0432\u0443\u0435\u0442 <strong>\u0441\u0442\u0430\u0431\u0438\u043b\u044c\u043d\u043e\u0441\u0442\u044c \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u043e\u0439 \u0444\u0430\u0437\u044b<\/strong>. \u0422\u0430\u043a\u043e\u0435 \u0441\u043e\u0447\u0435\u0442\u0430\u043d\u0438\u0435 \u044d\u043b\u0435\u043c\u0435\u043d\u0442\u043e\u0432 \u043f\u043e\u043c\u043e\u0433\u0430\u0435\u0442 \u043f\u043e\u0434\u0434\u0435\u0440\u0436\u0438\u0432\u0430\u0442\u044c \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0443\u044e \u0441\u0442\u0440\u0443\u043a\u0442\u0443\u0440\u0443, \u043e\u0431\u0435\u0441\u043f\u0435\u0447\u0438\u0432\u0430\u044f \u0442\u0430\u043a\u0438\u0435 \u043f\u0440\u0435\u0438\u043c\u0443\u0449\u0435\u0441\u0442\u0432\u0430, \u043a\u0430\u043a \u0443\u043b\u0443\u0447\u0448\u0435\u043d\u043d\u0430\u044f \u043f\u043b\u0430\u0441\u0442\u0438\u0447\u043d\u043e\u0441\u0442\u044c \u0438 \u043e\u0442\u043b\u0438\u0447\u043d\u0430\u044f \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u0430\u044f \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c.<\/p><h2 class=\"wp-block-heading\">\u0425\u0438\u043c\u0438\u0447\u0435\u0441\u043a\u0438\u0439 \u0441\u043e\u0441\u0442\u0430\u0432 \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u043e\u0439 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0435\u0439 \u0441\u0442\u0430\u043b\u0438<\/h2><p class=\"wp-block-paragraph\">\u0410\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0430\u044f \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u0432 \u043e\u0441\u043d\u043e\u0432\u043d\u043e\u043c \u0441\u043e\u0441\u0442\u043e\u0438\u0442 \u0438\u0437 \u0445\u0440\u043e\u043c\u0430, \u043d\u0438\u043a\u0435\u043b\u044f \u0438 \u0443\u0433\u043b\u0435\u0440\u043e\u0434\u0430, \u0430 \u0442\u0430\u043a\u0436\u0435 \u0434\u0440\u0443\u0433\u0438\u0445 \u044d\u043b\u0435\u043c\u0435\u043d\u0442\u043e\u0432, \u0443\u043b\u0443\u0447\u0448\u0430\u044e\u0449\u0438\u0445 \u043e\u043f\u0440\u0435\u0434\u0435\u043b\u0435\u043d\u043d\u044b\u0435 \u0441\u0432\u043e\u0439\u0441\u0442\u0432\u0430.&nbsp;<\/p><ul class=\"wp-block-list\"><li><strong>\u0425\u0440\u043e\u043c <\/strong>(\u041a\u0440)<strong> (15-32%)<\/strong> \u043e\u0431\u0435\u0441\u043f\u0435\u0447\u0438\u0432\u0430\u0435\u0442 \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u0443\u044e \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c \u0437\u0430 \u0441\u0447\u0435\u0442 \u043e\u0431\u0440\u0430\u0437\u043e\u0432\u0430\u043d\u0438\u044f \u043f\u0430\u0441\u0441\u0438\u0432\u043d\u043e\u0433\u043e \u0441\u043b\u043e\u044f \u043e\u043a\u0441\u0438\u0434\u0430 \u0445\u0440\u043e\u043c\u0430, \u043a\u043e\u0442\u043e\u0440\u044b\u0439 \u0441\u0430\u043c\u043e\u0432\u043e\u0441\u0441\u0442\u0430\u043d\u0430\u0432\u043b\u0438\u0432\u0430\u0435\u0442\u0441\u044f \u043f\u0440\u0438 \u0432\u043e\u0437\u0434\u0435\u0439\u0441\u0442\u0432\u0438\u0438 \u0432\u043e\u0437\u0434\u0443\u0445\u0430 \u0438\u043b\u0438 \u0432\u043b\u0430\u0433\u0438.&nbsp;<\/li>\n\n<li><strong>\u043d\u0438\u043a\u0435\u043b\u044c <\/strong>(\u041d\u0438)<strong> (8-37%)<\/strong> \u0441\u0442\u0430\u0431\u0438\u043b\u0438\u0437\u0438\u0440\u0443\u0435\u0442 \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0443\u044e \u0441\u0442\u0440\u0443\u043a\u0442\u0443\u0440\u0443, \u0443\u043b\u0443\u0447\u0448\u0430\u044f \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c, \u043f\u043b\u0430\u0441\u0442\u0438\u0447\u043d\u043e\u0441\u0442\u044c, \u0444\u043e\u0440\u043c\u0443\u0435\u043c\u043e\u0441\u0442\u044c \u0438 \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u0443\u044e \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c.&nbsp;<\/li>\n\n<li><strong>\u0423\u0433\u043b\u0435\u0440\u043e\u0434 <\/strong>(\u0421)<strong> <\/strong>\u043f\u043e\u0434\u0434\u0435\u0440\u0436\u0438\u0432\u0430\u0435\u0442\u0441\u044f \u043d\u0430 \u043e\u0447\u0435\u043d\u044c \u043d\u0438\u0437\u043a\u043e\u043c \u0443\u0440\u043e\u0432\u043d\u0435, \u043a\u0430\u043a \u043f\u0440\u0430\u0432\u0438\u043b\u043e<strong> \u043d\u0438\u0436\u0435 0,08%,<\/strong> \u043e\u0441\u043e\u0431\u0435\u043d\u043d\u043e \u0432 \u043d\u0438\u0437\u043a\u043e\u0443\u0433\u043b\u0435\u0440\u043e\u0434\u0438\u0441\u0442\u044b\u0445 \u043c\u0430\u0440\u043a\u0430\u0445, \u0442\u0430\u043a\u0438\u0445 \u043a\u0430\u043a 304L \u0438 316L (\u043d\u0438\u0436\u0435 0,03%), \u0447\u0442\u043e\u0431\u044b \u0441\u0432\u0435\u0441\u0442\u0438 \u043a \u043c\u0438\u043d\u0438\u043c\u0443\u043c\u0443 \u0432\u044b\u0434\u0435\u043b\u0435\u043d\u0438\u0435 \u043a\u0430\u0440\u0431\u0438\u0434\u043e\u0432 \u0432\u043e \u0432\u0440\u0435\u043c\u044f \u0441\u0432\u0430\u0440\u043a\u0438, \u0442\u0435\u043c \u0441\u0430\u043c\u044b\u043c \u0441\u043d\u0438\u0436\u0430\u044f \u0440\u0438\u0441\u043a \u043c\u0435\u0436\u043a\u0440\u0438\u0441\u0442\u0430\u043b\u043b\u0438\u0442\u043d\u043e\u0439 \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u0438.<\/li><\/ul><p class=\"wp-block-paragraph\"><\/p><p class=\"wp-block-paragraph\">\u041a\u0440\u043e\u043c\u0435 \u0442\u043e\u0433\u043e,<\/p><ul class=\"wp-block-list\"><li><strong>\u041c\u0430\u0440\u0433\u0430\u043d\u0435\u0446 <\/strong>(\u041c\u043d)<strong> \u043c\u043e\u0436\u0435\u0442 \u0447\u0430\u0441\u0442\u0438\u0447\u043d\u043e \u0437\u0430\u043c\u0435\u043d\u0438\u0442\u044c \u043d\u0438\u043a\u0435\u043b\u044c<\/strong> \u0432 \u043d\u0435\u043a\u043e\u0442\u043e\u0440\u044b\u0445 \u0441\u043f\u043b\u0430\u0432\u0430\u0445, \u043e\u0441\u043e\u0431\u0435\u043d\u043d\u043e \u0432 \u0441\u0435\u0440\u0438\u0438 200, \u0434\u0435\u0439\u0441\u0442\u0432\u0443\u0435\u0442 \u043a\u0430\u043a \u0441\u0442\u0430\u0431\u0438\u043b\u0438\u0437\u0430\u0442\u043e\u0440 \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u0430 \u0438 \u043f\u043e\u0432\u044b\u0448\u0430\u0435\u0442 \u0440\u0430\u0441\u0442\u0432\u043e\u0440\u0438\u043c\u043e\u0441\u0442\u044c \u0430\u0437\u043e\u0442\u0430 \u0438 \u043f\u0440\u0435\u0434\u0435\u043b \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u0438 \u043f\u0440\u0438 \u0440\u0430\u0441\u0442\u044f\u0436\u0435\u043d\u0438\u0438, \u0430 \u0442\u0430\u043a\u0436\u0435 \u0441\u043d\u0438\u0436\u0430\u0435\u0442 \u043f\u0440\u043e\u0438\u0437\u0432\u043e\u0434\u0441\u0442\u0432\u0435\u043d\u043d\u044b\u0435 \u0437\u0430\u0442\u0440\u0430\u0442\u044b.&nbsp;<\/li>\n\n<li><strong>\u041c\u043e\u043b\u0438\u0431\u0434\u0435\u043d<\/strong> (\u041c\u043e)<strong> (2%-3%)<\/strong> \u0434\u043e\u0431\u0430\u0432\u043b\u044f\u0435\u0442\u0441\u044f \u0434\u043b\u044f \u043f\u043e\u0432\u044b\u0448\u0435\u043d\u0438\u044f \u0443\u0441\u0442\u043e\u0439\u0447\u0438\u0432\u043e\u0441\u0442\u0438 \u043a \u0442\u043e\u0447\u0435\u0447\u043d\u043e\u0439 \u0438 \u0449\u0435\u043b\u0435\u0432\u043e\u0439 \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u0438, \u043e\u0441\u043e\u0431\u0435\u043d\u043d\u043e \u0432 \u0441\u0440\u0435\u0434\u0430\u0445 \u0441 \u0432\u044b\u0441\u043e\u043a\u0438\u043c \u0441\u043e\u0434\u0435\u0440\u0436\u0430\u043d\u0438\u0435\u043c \u0445\u043b\u043e\u0440\u0438\u0434\u043e\u0432, \u0442\u0430\u043a\u0438\u0445 \u043a\u0430\u043a \u043c\u043e\u0440\u0441\u043a\u0430\u044f \u0432\u043e\u0434\u0430.&nbsp;<\/li>\n\n<li><strong>\u0410\u0437\u043e\u0442<\/strong> (N) \u0443\u0432\u0435\u043b\u0438\u0447\u0438\u0432\u0430\u0435\u0442 \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c \u0438 \u043f\u043e\u0432\u044b\u0448\u0430\u0435\u0442 \u0443\u0441\u0442\u043e\u0439\u0447\u0438\u0432\u043e\u0441\u0442\u044c \u043a \u043b\u043e\u043a\u0430\u043b\u044c\u043d\u043e\u0439 \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u0438<strong>,<\/strong> \u043e\u0441\u043e\u0431\u0435\u043d\u043d\u043e \u0432 \u0441\u043f\u043b\u0430\u0432\u0430\u0445 \u0441 \u0432\u044b\u0441\u043e\u043a\u0438\u043c\u0438 \u044d\u043a\u0441\u043f\u043b\u0443\u0430\u0442\u0430\u0446\u0438\u043e\u043d\u043d\u044b\u043c\u0438 \u0445\u0430\u0440\u0430\u043a\u0442\u0435\u0440\u0438\u0441\u0442\u0438\u043a\u0430\u043c\u0438.&nbsp;<\/li>\n\n<li><strong>\u041c\u0435\u0434\u044c <\/strong>(\u041a\u0443) <strong>\u0438\u043d\u043e\u0433\u0434\u0430 \u0434\u043e\u0431\u0430\u0432\u043b\u044f\u0435\u0442\u0441\u044f,<\/strong> \u043e\u0441\u043e\u0431\u0435\u043d\u043d\u043e \u0432 \u0441\u043f\u0435\u0446\u0438\u0430\u043b\u0438\u0437\u0438\u0440\u043e\u0432\u0430\u043d\u043d\u044b\u0445 \u0441\u043f\u043b\u0430\u0432\u0430\u0445, \u0434\u043b\u044f \u043f\u043e\u0432\u044b\u0448\u0435\u043d\u0438\u044f \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u0438 \u043a \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u0438 \u0432 \u043e\u043f\u0440\u0435\u0434\u0435\u043b\u0435\u043d\u043d\u044b\u0445 \u043a\u0438\u0441\u043b\u044b\u0445 \u0441\u0440\u0435\u0434\u0430\u0445, \u0442\u0430\u043a\u0438\u0445 \u043a\u0430\u043a \u0441\u0435\u0440\u043d\u0430\u044f \u0438 \u0444\u043e\u0441\u0444\u043e\u0440\u043d\u0430\u044f \u043a\u0438\u0441\u043b\u043e\u0442\u0430.<\/li><\/ul><p class=\"wp-block-paragraph\"><\/p><p class=\"wp-block-paragraph\">*<em>\u0410\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0430\u044f \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u043c\u043e\u0436\u0435\u0442 \u0442\u0430\u043a\u0436\u0435 \u0441\u043e\u0434\u0435\u0440\u0436\u0430\u0442\u044c \u0441\u043b\u0435\u0434\u044b \u0442\u0430\u043a\u0438\u0445 \u044d\u043b\u0435\u043c\u0435\u043d\u0442\u043e\u0432, \u043a\u0430\u043a <\/em><strong><em>\u043a\u0440\u0435\u043c\u043d\u0438\u0439 <\/em><\/strong><em>(\u0421\u0438), <\/em><strong><em>\u0444\u043e\u0441\u0444\u043e\u0440 <\/em><\/strong><em>(\u041f), <\/em><strong><em>\u0441\u0435\u0440\u0430 <\/em><\/strong><em>(\u0421), <\/em><strong><em>\u0442\u0438\u0442\u0430\u043d <\/em><\/strong><em>(\u0422\u0438), <\/em><strong><em>\u043d\u0438\u043e\u0431\u0438\u0439 <\/em><\/strong><em>(\u041d\u0431), \u0438 <\/em><strong><em>\u043a\u043e\u0431\u0430\u043b\u044c\u0442 <\/em><\/strong><em>(Co), \u043d\u043e \u043c\u044b \u043d\u0435 \u0431\u0443\u0434\u0435\u043c \u043e\u0431\u0441\u0443\u0436\u0434\u0430\u0442\u044c \u0438\u0445 \u0437\u0434\u0435\u0441\u044c \u043f\u043e\u0434\u0440\u043e\u0431\u043d\u043e.<\/em><\/p><h2 class=\"wp-block-heading\">\u0421\u0432\u043e\u0439\u0441\u0442\u0432\u0430 \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u043e\u0439 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0435\u0439 \u0441\u0442\u0430\u043b\u0438<\/h2><p class=\"wp-block-paragraph\">\u0412\u043e\u0442 \u0442\u0440\u0438 \u043e\u0441\u043d\u043e\u0432\u043d\u044b\u0435 \u043f\u0440\u0438\u0447\u0438\u043d\u044b, \u043a\u043e\u0442\u043e\u0440\u044b\u0435 \u0434\u0435\u043b\u0430\u044e\u0442 \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0443\u044e \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0443\u044e \u0441\u0442\u0430\u043b\u044c \u0443\u043d\u0438\u043a\u0430\u043b\u044c\u043d\u043e\u0439:<\/p><ol class=\"wp-block-list\"><li>\u041e\u0442\u043b\u0438\u0447\u043d\u0430\u044f \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u0430\u044f \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c \u0432\u043e \u043c\u043d\u043e\u0433\u0438\u0445 \u0441\u0440\u0435\u0434\u0430\u0445.<\/li>\n\n<li>\u0412\u044b\u0441\u043e\u043a\u0430\u044f \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c \u0438 \u043f\u043b\u0430\u0441\u0442\u0438\u0447\u043d\u043e\u0441\u0442\u044c \u0434\u0430\u0436\u0435 \u043f\u0440\u0438 \u043d\u0438\u0437\u043a\u0438\u0445 \u0442\u0435\u043c\u043f\u0435\u0440\u0430\u0442\u0443\u0440\u0430\u0445.<\/li>\n\n<li>\u041d\u0435\u043c\u0430\u0433\u043d\u0438\u0442\u0435\u043d \u0438 \u043c\u043e\u0436\u0435\u0442 \u0431\u044b\u0442\u044c \u0437\u0430\u043a\u0430\u043b\u0435\u043d \u0442\u043e\u043b\u044c\u043a\u043e \u0445\u043e\u043b\u043e\u0434\u043d\u043e\u0439 \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u043e\u0439.<\/li><\/ol><p class=\"wp-block-paragraph\"><\/p><p class=\"wp-block-paragraph\">\u041e\u0437\u043d\u0430\u043a\u043e\u043c\u044c\u0442\u0435\u0441\u044c \u0441 \u0442\u0430\u0431\u043b\u0438\u0446\u0435\u0439 \u043d\u0438\u0436\u0435, \u0447\u0442\u043e\u0431\u044b \u043e\u0437\u043d\u0430\u043a\u043e\u043c\u0438\u0442\u044c\u0441\u044f \u0441 \u043e\u0441\u043d\u043e\u0432\u043d\u044b\u043c\u0438 \u0441\u0432\u043e\u0439\u0441\u0442\u0432\u0430\u043c\u0438 \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u043e\u0439 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0435\u0439 \u0441\u0442\u0430\u043b\u0438:<\/p><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u0421\u0432\u043e\u0439\u0441\u0442\u0432\u043e<\/strong><\/td><td><strong>\u041e\u043f\u0438\u0441\u0430\u043d\u0438\u0435<\/strong><\/td><td><strong>\u041f\u0440\u043e\u0438\u0437\u0432\u043e\u0434\u0438\u0442\u0435\u043b\u044c\u043d\u043e\u0441\u0442\u044c<\/strong><\/td><td><strong>\u0417\u0430\u043c\u0435\u0447\u0430\u043d\u0438\u044f<\/strong><\/td><\/tr><tr><td><a href=\"https:\/\/steelprogroup.com\/ru\/stainless-steel\/properties\/corrosion-resistant\/\">\u041a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u0430\u044f \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c<\/a><\/td><td>\u0421\u043f\u043e\u0441\u043e\u0431\u043d\u043e\u0441\u0442\u044c \u043f\u0440\u043e\u0442\u0438\u0432\u043e\u0441\u0442\u043e\u044f\u0442\u044c \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u0438 \u0438 \u043e\u043a\u0438\u0441\u043b\u0435\u043d\u0438\u044e.<\/td><td>\u041e\u0442\u043b\u0438\u0447\u043d\u043e \u043f\u043e\u0434\u0445\u043e\u0434\u0438\u0442 \u0434\u043b\u044f \u0440\u0430\u0431\u043e\u0442\u044b \u0432 \u043e\u043a\u0438\u0441\u043b\u0438\u0442\u0435\u043b\u044c\u043d\u044b\u0445 \u0441\u0440\u0435\u0434\u0430\u0445 \u0431\u043b\u0430\u0433\u043e\u0434\u0430\u0440\u044f \u0432\u044b\u0441\u043e\u043a\u043e\u043c\u0443 \u0441\u043e\u0434\u0435\u0440\u0436\u0430\u043d\u0438\u044e \u0445\u0440\u043e\u043c\u0430 \u0438 \u043d\u0438\u043a\u0435\u043b\u044f.<\/td><td>\u041c\u043e\u043b\u0438\u0431\u0434\u0435\u043d \u043f\u043e\u0432\u044b\u0448\u0430\u0435\u0442 \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u0443\u044e \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c \u0432 \u0441\u0440\u0435\u0434\u0430\u0445 \u0441 \u0432\u044b\u0441\u043e\u043a\u0438\u043c \u0441\u043e\u0434\u0435\u0440\u0436\u0430\u043d\u0438\u0435\u043c \u0445\u043b\u043e\u0440\u0438\u0434\u043e\u0432.<\/td><\/tr><tr><td>\u041c\u0435\u0445\u0430\u043d\u0438\u0447\u0435\u0441\u043a\u0438\u0435 \u0441\u0432\u043e\u0439\u0441\u0442\u0432\u0430<\/td><td>\u0412\u043a\u043b\u044e\u0447\u0430\u0435\u0442 \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c, \u0443\u0434\u0430\u0440\u043d\u0443\u044e \u0432\u044f\u0437\u043a\u043e\u0441\u0442\u044c, \u0442\u0432\u0435\u0440\u0434\u043e\u0441\u0442\u044c \u0438 \u043f\u043b\u0430\u0441\u0442\u0438\u0447\u043d\u043e\u0441\u0442\u044c.<\/td><td>\u041f\u0440\u043e\u0447\u043d\u044b\u0439, \u0432\u044f\u0437\u043a\u0438\u0439, \u0441 \u0445\u043e\u0440\u043e\u0448\u0435\u0439 \u043f\u043b\u0430\u0441\u0442\u0438\u0447\u043d\u043e\u0441\u0442\u044c\u044e \u0438 \u0443\u043c\u0435\u0440\u0435\u043d\u043d\u043e\u0439 \u0442\u0432\u0435\u0440\u0434\u043e\u0441\u0442\u044c\u044e.<\/td><td>\u0412\u044b\u0441\u043e\u043a\u0430\u044f \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c \u0438 \u0432\u044f\u0437\u043a\u043e\u0441\u0442\u044c \u043f\u043e\u043c\u043e\u0433\u0430\u044e\u0442 \u043f\u0440\u043e\u0442\u0438\u0432\u043e\u0441\u0442\u043e\u044f\u0442\u044c \u0434\u0435\u0444\u043e\u0440\u043c\u0430\u0446\u0438\u0438 \u043f\u043e\u0434 \u0434\u0435\u0439\u0441\u0442\u0432\u0438\u0435\u043c \u0432\u044b\u0441\u043e\u043a\u0438\u0445 \u043d\u0430\u043f\u0440\u044f\u0436\u0435\u043d\u0438\u0439, \u0430 \u0445\u043e\u0440\u043e\u0448\u0430\u044f \u043f\u043b\u0430\u0441\u0442\u0438\u0447\u043d\u043e\u0441\u0442\u044c \u043f\u0440\u0435\u0434\u043e\u0442\u0432\u0440\u0430\u0449\u0430\u0435\u0442 \u0440\u0430\u0441\u0442\u0440\u0435\u0441\u043a\u0438\u0432\u0430\u043d\u0438\u0435 \u043f\u043e\u0434 \u0434\u0435\u0439\u0441\u0442\u0432\u0438\u0435\u043c \u043d\u0430\u043f\u0440\u044f\u0436\u0435\u043d\u0438\u0439.<\/td><\/tr><tr><td>\u0422\u0435\u043f\u043b\u043e\u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c<\/td><td>\u0421\u043f\u043e\u0441\u043e\u0431\u043d\u043e\u0441\u0442\u044c \u0432\u044b\u0434\u0435\u0440\u0436\u0438\u0432\u0430\u0442\u044c \u0432\u044b\u0441\u043e\u043a\u0438\u0435 \u0442\u0435\u043c\u043f\u0435\u0440\u0430\u0442\u0443\u0440\u044b \u0431\u0435\u0437 \u0443\u0445\u0443\u0434\u0448\u0435\u043d\u0438\u044f \u0441\u0432\u043e\u0439\u0441\u0442\u0432.<\/td><td>\u0425\u043e\u0440\u043e\u0448\u0430\u044f \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c \u043a \u043e\u043a\u0438\u0441\u043b\u0435\u043d\u0438\u044e \u043f\u0440\u0438 \u0432\u044b\u0441\u043e\u043a\u0438\u0445 \u0442\u0435\u043c\u043f\u0435\u0440\u0430\u0442\u0443\u0440\u0430\u0445.<\/td><td>\u0414\u043b\u0438\u0442\u0435\u043b\u044c\u043d\u043e\u0435 \u0432\u043e\u0437\u0434\u0435\u0439\u0441\u0442\u0432\u0438\u0435 \u0432\u044b\u0441\u043e\u043a\u0438\u0445 \u0442\u0435\u043c\u043f\u0435\u0440\u0430\u0442\u0443\u0440 \u043c\u043e\u0436\u0435\u0442 \u043f\u0440\u0438\u0432\u0435\u0441\u0442\u0438 \u043a \u043e\u0431\u0440\u0430\u0437\u043e\u0432\u0430\u043d\u0438\u044e \u0448\u0435\u043b\u0443\u0448\u0435\u043d\u0438\u044f.<\/td><\/tr><tr><td>\u042d\u0444\u0444\u0435\u043a\u0442\u0438\u0432\u043d\u043e\u0441\u0442\u044c \u043f\u0440\u0438 \u043d\u0438\u0437\u043a\u0438\u0445 \u0442\u0435\u043c\u043f\u0435\u0440\u0430\u0442\u0443\u0440\u0430\u0445<\/td><td>\u042d\u043a\u0441\u043f\u043b\u0443\u0430\u0442\u0430\u0446\u0438\u043e\u043d\u043d\u044b\u0435 \u0445\u0430\u0440\u0430\u043a\u0442\u0435\u0440\u0438\u0441\u0442\u0438\u043a\u0438 \u043c\u0430\u0442\u0435\u0440\u0438\u0430\u043b\u0430 \u0432 \u0445\u043e\u043b\u043e\u0434\u043d\u044b\u0445 \u0443\u0441\u043b\u043e\u0432\u0438\u044f\u0445.<\/td><td>\u0418\u0441\u043a\u043b\u044e\u0447\u0438\u0442\u0435\u043b\u044c\u043d\u0430\u044f \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c, \u0443\u0441\u0442\u043e\u0439\u0447\u0438\u0432\u043e\u0441\u0442\u044c \u043a \u0445\u0440\u0443\u043f\u043a\u0438\u043c \u0440\u0430\u0437\u0440\u0443\u0448\u0435\u043d\u0438\u044f\u043c.<\/td><td>\u041f\u043e\u0434\u0445\u043e\u0434\u0438\u0442 \u0434\u043b\u044f \u043a\u0440\u0438\u043e\u0433\u0435\u043d\u043d\u044b\u0445 \u043f\u0440\u0438\u043c\u0435\u043d\u0435\u043d\u0438\u0439, \u0433\u0434\u0435 \u043f\u0440\u0435\u0434\u043e\u0442\u0432\u0440\u0430\u0449\u0435\u043d\u0438\u0435 \u0445\u0440\u0443\u043f\u043a\u043e\u0441\u0442\u0438 \u0438\u043c\u0435\u0435\u0442 \u0440\u0435\u0448\u0430\u044e\u0449\u0435\u0435 \u0437\u043d\u0430\u0447\u0435\u043d\u0438\u0435.<\/td><\/tr><tr><td>\u0424\u043e\u0440\u043c\u0443\u0435\u043c\u043e\u0441\u0442\u044c<\/td><td>\u041b\u0435\u0433\u043a\u043e\u0441\u0442\u044c \u0444\u043e\u0440\u043c\u043e\u0432\u0430\u043d\u0438\u044f \u043f\u043e\u0441\u0440\u0435\u0434\u0441\u0442\u0432\u043e\u043c \u043c\u0435\u0445\u0430\u043d\u0438\u0447\u0435\u0441\u043a\u0438\u0445 \u043f\u0440\u043e\u0446\u0435\u0441\u0441\u043e\u0432.<\/td><td>\u041e\u0442\u043b\u0438\u0447\u043d\u0430\u044f \u0444\u043e\u0440\u043c\u0443\u0435\u043c\u043e\u0441\u0442\u044c, \u043f\u043e\u0434\u0445\u043e\u0434\u0438\u0442 \u043a\u0430\u043a \u0434\u043b\u044f \u0445\u043e\u043b\u043e\u0434\u043d\u043e\u0439, \u0442\u0430\u043a \u0438 \u0434\u043b\u044f \u0433\u043e\u0440\u044f\u0447\u0435\u0439 \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0438.<\/td><td>\u0412\u044b\u0441\u043e\u043a\u0430\u044f \u043f\u043b\u0430\u0441\u0442\u0438\u0447\u043d\u043e\u0441\u0442\u044c \u0434\u0435\u043b\u0430\u0435\u0442 \u0435\u0433\u043e \u0438\u0434\u0435\u0430\u043b\u044c\u043d\u044b\u043c \u0434\u043b\u044f \u0438\u0437\u0433\u043e\u0442\u043e\u0432\u043b\u0435\u043d\u0438\u044f \u0441\u043b\u043e\u0436\u043d\u044b\u0445 \u0444\u043e\u0440\u043c.<\/td><\/tr><tr><td><a href=\"https:\/\/steelprogroup.com\/ru\/stainless-steel\/welding\/\">\u0421\u0432\u0430\u0440\u0438\u0432\u0430\u0435\u043c\u043e\u0441\u0442\u044c<\/a><\/td><td>\u0412\u043e\u0437\u043c\u043e\u0436\u043d\u043e\u0441\u0442\u044c \u0441\u0432\u0430\u0440\u043a\u0438 \u0431\u0435\u0437 \u043f\u043e\u0442\u0435\u0440\u0438 \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u0438.<\/td><td>\u0412\u044b\u0441\u043e\u043a\u0430\u044f \u0441\u0432\u0430\u0440\u0438\u0432\u0430\u0435\u043c\u043e\u0441\u0442\u044c \u043f\u0440\u0438 \u0441\u043e\u0445\u0440\u0430\u043d\u0435\u043d\u0438\u0438 \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u043e\u0439 \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u0438.<\/td><td>\u041f\u043e\u0441\u043b\u0435\u0441\u0432\u0430\u0440\u043e\u0447\u043d\u0430\u044f \u0442\u0435\u0440\u043c\u0438\u0447\u0435\u0441\u043a\u0430\u044f \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0430 \u043e\u0431\u044b\u0447\u043d\u043e \u043d\u0435 \u0442\u0440\u0435\u0431\u0443\u0435\u0442\u0441\u044f, \u0447\u0442\u043e \u0434\u0435\u043b\u0430\u0435\u0442 \u044d\u0442\u043e\u0442 \u043c\u0430\u0442\u0435\u0440\u0438\u0430\u043b \u0438\u0434\u0435\u0430\u043b\u044c\u043d\u044b\u043c \u0434\u043b\u044f \u043f\u0440\u0438\u043c\u0435\u043d\u0435\u043d\u0438\u044f \u0432 \u0441\u0442\u0440\u043e\u0438\u0442\u0435\u043b\u044c\u0441\u0442\u0432\u0435 \u0438 \u0430\u0432\u0442\u043e\u043c\u043e\u0431\u0438\u043b\u044c\u043d\u043e\u0439 \u043f\u0440\u043e\u043c\u044b\u0448\u043b\u0435\u043d\u043d\u043e\u0441\u0442\u0438.<\/td><\/tr><tr><td>\u041e\u0431\u0440\u0430\u0431\u0430\u0442\u044b\u0432\u0430\u0435\u043c\u043e\u0441\u0442\u044c<\/td><td>\u041b\u0435\u0433\u043a\u043e\u0441\u0442\u044c \u0440\u0435\u0437\u043a\u0438, \u0444\u043e\u0440\u043c\u043e\u0432\u043a\u0438 \u0438 \u043e\u0442\u0434\u0435\u043b\u043a\u0438 \u043c\u0430\u0442\u0435\u0440\u0438\u0430\u043b\u0430.<\/td><td>\u0423\u043c\u0435\u0440\u0435\u043d\u043d\u0430\u044f; \u0443\u043f\u0440\u043e\u0447\u043d\u0435\u043d\u0438\u0435 \u0438 \u0438\u0437\u043d\u043e\u0441 \u0438\u043d\u0441\u0442\u0440\u0443\u043c\u0435\u043d\u0442\u0430 \u043c\u043e\u0436\u043d\u043e \u043a\u043e\u043d\u0442\u0440\u043e\u043b\u0438\u0440\u043e\u0432\u0430\u0442\u044c \u043f\u0443\u0442\u0435\u043c \u043e\u043f\u0442\u0438\u043c\u0438\u0437\u0430\u0446\u0438\u0438.<\/td><td>\u0418\u0441\u043f\u043e\u043b\u044c\u0437\u043e\u0432\u0430\u043d\u0438\u0435 \u043e\u0441\u0442\u0440\u044b\u0445 \u0438\u043d\u0441\u0442\u0440\u0443\u043c\u0435\u043d\u0442\u043e\u0432 \u0438 \u0431\u043e\u043b\u0435\u0435 \u043d\u0438\u0437\u043a\u0438\u0445 \u0441\u043a\u043e\u0440\u043e\u0441\u0442\u0435\u0439 \u0440\u0435\u0437\u0430\u043d\u0438\u044f \u043c\u043e\u0436\u0435\u0442 \u0443\u043b\u0443\u0447\u0448\u0438\u0442\u044c \u043e\u0431\u0440\u0430\u0431\u0430\u0442\u044b\u0432\u0430\u0435\u043c\u043e\u0441\u0442\u044c. \u0425\u043e\u043b\u043e\u0434\u043d\u0430\u044f \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0430 \u043c\u043e\u0436\u0435\u0442 \u043f\u043e\u0432\u044b\u0441\u0438\u0442\u044c \u0442\u0432\u0435\u0440\u0434\u043e\u0441\u0442\u044c.<\/td><\/tr><tr><td><a href=\"https:\/\/steelprogroup.com\/ru\/stainless-steel\/properties\/magnetic\/\">\u041c\u0430\u0433\u043d\u0438\u0442\u043d\u044b\u0435 \u0441\u0432\u043e\u0439\u0441\u0442\u0432\u0430<\/a><\/td><td>\u0421\u043a\u043b\u043e\u043d\u043d\u043e\u0441\u0442\u044c \u043f\u0440\u043e\u044f\u0432\u043b\u044f\u0442\u044c \u043c\u0430\u0433\u043d\u0438\u0442\u043d\u043e\u0435 \u043f\u043e\u0432\u0435\u0434\u0435\u043d\u0438\u0435.<\/td><td>\u041d\u0435\u043c\u0430\u0433\u043d\u0438\u0442\u0435\u043d, \u043d\u043e \u043f\u043e\u0441\u043b\u0435 \u0445\u043e\u043b\u043e\u0434\u043d\u043e\u0439 \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0438 \u043c\u043e\u0436\u0435\u0442 \u043f\u0440\u043e\u044f\u0432\u0438\u0442\u044c\u0441\u044f \u0441\u043b\u0430\u0431\u0430\u044f \u043c\u0430\u0433\u043d\u0438\u0442\u043d\u043e\u0441\u0442\u044c.<\/td><td>\u0425\u043e\u043b\u043e\u0434\u043d\u0430\u044f \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0430 \u043c\u043e\u0436\u0435\u0442 \u0432\u044b\u0437\u044b\u0432\u0430\u0442\u044c \u043d\u0435\u0431\u043e\u043b\u044c\u0448\u043e\u0439 \u043c\u0430\u0433\u043d\u0435\u0442\u0438\u0437\u043c, \u043a\u043e\u0442\u043e\u0440\u044b\u0439 \u043c\u043e\u0436\u0435\u0442 \u043f\u043e\u0432\u043b\u0438\u044f\u0442\u044c \u043d\u0430 \u043d\u0435\u043c\u0430\u0433\u043d\u0438\u0442\u043d\u044b\u0435 \u043f\u0440\u0438\u043c\u0435\u043d\u0435\u043d\u0438\u044f.<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u041f\u0440\u0435\u0438\u043c\u0443\u0449\u0435\u0441\u0442\u0432\u0430 \u0438 \u043d\u0435\u0434\u043e\u0441\u0442\u0430\u0442\u043a\u0438 \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u043e\u0439 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0435\u0439 \u0441\u0442\u0430\u043b\u0438<\/h2><p class=\"wp-block-paragraph\">\u0410\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0430\u044f \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u043e\u0431\u0435\u0441\u043f\u0435\u0447\u0438\u0432\u0430\u0435\u0442 \u0441\u043b\u0435\u0434\u0443\u044e\u0449\u0438\u0435 \u043f\u0440\u0435\u0438\u043c\u0443\u0449\u0435\u0441\u0442\u0432\u0430:<\/p><ol class=\"wp-block-list\"><li>\u041e\u0442\u043b\u0438\u0447\u043d\u0430\u044f \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u0430\u044f \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c \u0432 \u0448\u0438\u0440\u043e\u043a\u043e\u043c \u0434\u0438\u0430\u043f\u0430\u0437\u043e\u043d\u0435 \u0441\u0440\u0435\u0434.<\/li>\n\n<li>\u0412\u044b\u0441\u043e\u043a\u0430\u044f \u043f\u043b\u0430\u0441\u0442\u0438\u0447\u043d\u043e\u0441\u0442\u044c, \u0447\u0442\u043e \u043e\u0431\u043b\u0435\u0433\u0447\u0430\u0435\u0442 \u0444\u043e\u0440\u043c\u043e\u0432\u043a\u0443 \u0438 \u0441\u0432\u0430\u0440\u043a\u0443.<\/li>\n\n<li>\u0421\u043e\u0445\u0440\u0430\u043d\u044f\u0435\u0442 \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c \u043f\u0440\u0438 \u0432\u044b\u0441\u043e\u043a\u0438\u0445 \u0442\u0435\u043c\u043f\u0435\u0440\u0430\u0442\u0443\u0440\u0430\u0445.<\/li>\n\n<li>\u0423\u0441\u0442\u043e\u0439\u0447\u0438\u0432 \u043a \u043e\u043a\u0438\u0441\u043b\u0435\u043d\u0438\u044e \u0434\u0430\u0436\u0435 \u0432\u043e \u0432\u043b\u0430\u0436\u043d\u043e\u043c \u0432\u043e\u0437\u0434\u0443\u0445\u0435.<\/li>\n\n<li>\u0412 \u043e\u0442\u043e\u0436\u0436\u0435\u043d\u043d\u043e\u043c \u0441\u043e\u0441\u0442\u043e\u044f\u043d\u0438\u0438 \u043d\u0435\u043c\u0430\u0433\u043d\u0438\u0442\u0435\u043d.<\/li><\/ol><p class=\"wp-block-paragraph\"><\/p><p class=\"wp-block-paragraph\">\u041e\u043d \u0442\u0430\u043a\u0436\u0435 \u0441\u0442\u0430\u043b\u043a\u0438\u0432\u0430\u0435\u0442\u0441\u044f \u0441 \u043f\u0440\u043e\u0431\u043b\u0435\u043c\u0430\u043c\u0438 \u0438 \u043d\u0435\u0434\u043e\u0441\u0442\u0430\u0442\u043a\u0430\u043c\u0438, \u043f\u0435\u0440\u0435\u0447\u0438\u0441\u043b\u0435\u043d\u043d\u044b\u043c\u0438 \u043d\u0438\u0436\u0435:<\/p><ol class=\"wp-block-list\"><li>\u0411\u043e\u043b\u0435\u0435 \u0432\u044b\u0441\u043e\u043a\u0430\u044f \u0441\u0442\u043e\u0438\u043c\u043e\u0441\u0442\u044c \u0438\u0437-\u0437\u0430 \u0438\u0441\u043f\u043e\u043b\u044c\u0437\u043e\u0432\u0430\u043d\u0438\u044f \u043b\u0435\u0433\u0438\u0440\u0443\u044e\u0449\u0438\u0445 \u044d\u043b\u0435\u043c\u0435\u043d\u0442\u043e\u0432, \u0442\u0430\u043a\u0438\u0445 \u043a\u0430\u043a \u043d\u0438\u043a\u0435\u043b\u044c.<\/li>\n\n<li>\u0412 \u043e\u043f\u0440\u0435\u0434\u0435\u043b\u0435\u043d\u043d\u044b\u0445 \u0443\u0441\u043b\u043e\u0432\u0438\u044f\u0445 \u043f\u043e\u0434\u0432\u0435\u0440\u0436\u0435\u043d \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u043e\u043c\u0443 \u0440\u0430\u0441\u0442\u0440\u0435\u0441\u043a\u0438\u0432\u0430\u043d\u0438\u044e \u043f\u043e\u0434 \u043d\u0430\u043f\u0440\u044f\u0436\u0435\u043d\u0438\u0435\u043c.<\/li>\n\n<li>\u0422\u0440\u0443\u0434\u043d\u043e \u043f\u043e\u0434\u0434\u0430\u0435\u0442\u0441\u044f \u043c\u0435\u0445\u0430\u043d\u0438\u0447\u0435\u0441\u043a\u043e\u0439 \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0435 \u0438\u0437-\u0437\u0430 \u0441\u0432\u043e\u0439\u0441\u0442\u0432 \u0443\u043f\u0440\u043e\u0447\u043d\u0435\u043d\u0438\u044f.<\/li>\n\n<li>\u0411\u043e\u043b\u0435\u0435 \u043d\u0438\u0437\u043a\u0430\u044f \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c \u043f\u043e \u0441\u0440\u0430\u0432\u043d\u0435\u043d\u0438\u044e \u0441 \u0434\u0440\u0443\u0433\u0438\u043c\u0438 \u0442\u0438\u043f\u0430\u043c\u0438 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0435\u0439 \u0441\u0442\u0430\u043b\u0438.<\/li>\n\n<li>\u041f\u043b\u043e\u0445\u0430\u044f \u0443\u0441\u0442\u043e\u0439\u0447\u0438\u0432\u043e\u0441\u0442\u044c \u043a \u0438\u0437\u043d\u043e\u0441\u0443 \u0438 \u0438\u0441\u0442\u0438\u0440\u0430\u043d\u0438\u044e.<\/li><\/ol><p class=\"wp-block-paragraph\"><\/p><h2 class=\"wp-block-heading\">\u041f\u043e\u0434\u0433\u0440\u0443\u043f\u043f\u044b \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u043e\u0439 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0435\u0439 \u0441\u0442\u0430\u043b\u0438<\/h2><p class=\"wp-block-paragraph\">\u0410\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0430\u044f \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u0434\u0435\u043b\u0438\u0442\u0441\u044f \u043d\u0430 \u0434\u0432\u0435 \u043f\u043e\u0434\u0433\u0440\u0443\u043f\u043f\u044b AISI <strong>\u0421\u0435\u0440\u0438\u044f 200<\/strong> \u0438 \u0410\u0418\u0421\u0418 <strong>\u0421\u0435\u0440\u0438\u044f 300<\/strong>. \u041e\u0431\u0435 \u0441\u0435\u0440\u0438\u0438 \u043f\u0440\u0438\u0437\u043d\u0430\u043d\u044b \u0410\u043c\u0435\u0440\u0438\u043a\u0430\u043d\u0441\u043a\u0438\u043c \u0438\u043d\u0441\u0442\u0438\u0442\u0443\u0442\u043e\u043c \u0447\u0443\u0433\u0443\u043d\u0430 \u0438 \u0441\u0442\u0430\u043b\u0438 (AISI), \u0410\u043c\u0435\u0440\u0438\u043a\u0430\u043d\u0441\u043a\u0438\u043c \u043e\u0431\u0449\u0435\u0441\u0442\u0432\u043e\u043c \u043f\u043e \u0438\u0441\u043f\u044b\u0442\u0430\u043d\u0438\u044f\u043c \u0438 \u043c\u0430\u0442\u0435\u0440\u0438\u0430\u043b\u0430\u043c (ASTM) \u0438 \u0434\u0440\u0443\u0433\u0438\u043c\u0438 \u043e\u0440\u0433\u0430\u043d\u0438\u0437\u0430\u0446\u0438\u044f\u043c\u0438 \u043f\u043e \u0432\u0441\u0435\u043c\u0443 \u043c\u0438\u0440\u0443. <strong>\u0413\u043b\u0430\u0432\u043d\u043e\u0435 \u043e\u0442\u043b\u0438\u0447\u0438\u0435<\/strong> \u0437\u0430\u043a\u043b\u044e\u0447\u0430\u0435\u0442\u0441\u044f \u0432 \u0442\u043e\u043c, \u0447\u0442\u043e \u0432 \u0441\u0435\u0440\u0438\u0438 200 \u0438\u0441\u043f\u043e\u043b\u044c\u0437\u0443\u044e\u0442\u0441\u044f \u043c\u0430\u0440\u0433\u0430\u043d\u0435\u0446 \u0438 \u0430\u0437\u043e\u0442 \u0441 \u043c\u0435\u043d\u044c\u0448\u0438\u043c \u0441\u043e\u0434\u0435\u0440\u0436\u0430\u043d\u0438\u0435\u043c \u043d\u0438\u043a\u0435\u043b\u044f, \u0442\u043e\u0433\u0434\u0430 \u043a\u0430\u043a \u0432 \u0441\u0435\u0440\u0438\u0438 300 \u0438\u0441\u043f\u043e\u043b\u044c\u0437\u0443\u044e\u0442\u0441\u044f \u0431\u043e\u043b\u0435\u0435 \u0432\u044b\u0441\u043e\u043a\u0438\u0435 \u0443\u0440\u043e\u0432\u043d\u0438 \u0445\u0440\u043e\u043c\u0430 \u0438 \u043d\u0438\u043a\u0435\u043b\u044f.<\/p><h3 class=\"wp-block-heading\">\u0421\u0435\u0440\u0438\u044f AISI 200<\/h3><p class=\"wp-block-paragraph\">\u041d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u0441\u0435\u0440\u0438\u0438 AISI 200 \u0444\u043e\u0440\u043c\u0438\u0440\u0443\u0435\u0442 \u0441\u0432\u043e\u044e \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0443\u044e \u0441\u0442\u0440\u0443\u043a\u0442\u0443\u0440\u0443 \u043f\u0443\u0442\u0435\u043c \u0434\u043e\u0431\u0430\u0432\u043b\u0435\u043d\u0438\u044f \u043c\u0430\u0440\u0433\u0430\u043d\u0446\u0430 \u0438 \u0430\u0437\u043e\u0442\u0430 \u0441 \u0443\u043c\u0435\u043d\u044c\u0448\u0435\u043d\u043d\u044b\u043c \u043a\u043e\u043b\u0438\u0447\u0435\u0441\u0442\u0432\u043e\u043c \u043d\u0438\u043a\u0435\u043b\u044f. \u041c\u0430\u0440\u0433\u0430\u043d\u0435\u0446 \u0438 \u0430\u0437\u043e\u0442 \u043f\u043e\u0434\u0434\u0435\u0440\u0436\u0438\u0432\u0430\u044e\u0442 \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0443\u044e \u0441\u0442\u0440\u0443\u043a\u0442\u0443\u0440\u0443 \u0438 \u043f\u043e\u0432\u044b\u0448\u0430\u044e\u0442 \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c. \u0420\u0430\u0441\u043f\u0440\u043e\u0441\u0442\u0440\u0430\u043d\u0435\u043d\u043d\u044b\u0435 \u043c\u0430\u0440\u043a\u0438 \u0432\u043a\u043b\u044e\u0447\u0430\u044e\u0442 201 \u0438 202. \u041e\u043d\u0430 \u043e\u0431\u044b\u0447\u043d\u043e \u0438\u0441\u043f\u043e\u043b\u044c\u0437\u0443\u0435\u0442\u0441\u044f \u0432 \u043a\u0443\u0445\u043e\u043d\u043d\u043e\u0439 \u0443\u0442\u0432\u0430\u0440\u0438, \u0430\u0432\u0442\u043e\u043c\u043e\u0431\u0438\u043b\u044c\u043d\u043e\u0439 \u043e\u0442\u0434\u0435\u043b\u043a\u0435 \u0438 \u043e\u0431\u043e\u0440\u0443\u0434\u043e\u0432\u0430\u043d\u0438\u0438 \u0434\u043b\u044f \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0438 \u043f\u0438\u0449\u0435\u0432\u044b\u0445 \u043f\u0440\u043e\u0434\u0443\u043a\u0442\u043e\u0432 \u0438\u0437-\u0437\u0430 \u0441\u0432\u043e\u0435\u0439 \u044d\u043a\u043e\u043d\u043e\u043c\u0438\u0447\u0435\u0441\u043a\u043e\u0439 \u044d\u0444\u0444\u0435\u043a\u0442\u0438\u0432\u043d\u043e\u0441\u0442\u0438.<\/p><h3 class=\"wp-block-heading\">\u0421\u0435\u0440\u0438\u044f AISI 300<\/h3><p class=\"wp-block-paragraph\"><a href=\"https:\/\/steelprogroup.com\/ru\/stainless-steel\/grades\/300-series\/\">\u041d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u0441\u0435\u0440\u0438\u0438 AISI 300<\/a> \u0444\u043e\u0440\u043c\u0438\u0440\u0443\u0435\u0442 \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0443\u044e \u0441\u0442\u0440\u0443\u043a\u0442\u0443\u0440\u0443 \u043f\u0443\u0442\u0435\u043c \u0434\u043e\u0431\u0430\u0432\u043b\u0435\u043d\u0438\u044f \u0431\u043e\u043b\u044c\u0448\u0435\u0433\u043e \u043a\u043e\u043b\u0438\u0447\u0435\u0441\u0442\u0432\u0430 \u0445\u0440\u043e\u043c\u0430 \u0438 \u043d\u0438\u043a\u0435\u043b\u044f. \u0425\u0440\u043e\u043c \u043f\u0440\u043e\u0442\u0438\u0432\u043e\u0441\u0442\u043e\u0438\u0442 \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u0438, \u0430 \u043d\u0438\u043a\u0435\u043b\u044c \u0434\u043e\u0431\u0430\u0432\u043b\u044f\u0435\u0442 \u043f\u043b\u0430\u0441\u0442\u0438\u0447\u043d\u043e\u0441\u0442\u0438 \u0438 \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u0438. \u0428\u0438\u0440\u043e\u043a\u043e \u0438\u0441\u043f\u043e\u043b\u044c\u0437\u0443\u044e\u0442\u0441\u044f \u0442\u0430\u043a\u0438\u0435 \u0440\u0430\u0441\u043f\u0440\u043e\u0441\u0442\u0440\u0430\u043d\u0435\u043d\u043d\u044b\u0435 \u043c\u0430\u0440\u043a\u0438, \u043a\u0430\u043a 304 (18\/8 \u0438\u043b\u0438 A2) \u0438 316 (A4). \u0421\u0435\u0440\u0438\u044f 300 \u043e\u0431\u044b\u0447\u043d\u043e \u0438\u0441\u043f\u043e\u043b\u044c\u0437\u0443\u0435\u0442\u0441\u044f \u0432 \u0441\u0442\u0440\u043e\u0438\u0442\u0435\u043b\u044c\u0441\u0442\u0432\u0435, \u0445\u0438\u043c\u0438\u0447\u0435\u0441\u043a\u043e\u0439 \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0435 \u0438 \u043c\u0435\u0434\u0438\u0446\u0438\u043d\u0441\u043a\u043e\u043c \u043e\u0431\u043e\u0440\u0443\u0434\u043e\u0432\u0430\u043d\u0438\u0438 \u0438\u0437-\u0437\u0430 \u0441\u0432\u043e\u0435\u0439 \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u0438 \u0438 \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u043e\u0439 \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u0438.<\/p><h2 class=\"wp-block-heading\">\u041c\u0430\u0440\u043a\u0438 \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u043e\u0439 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0435\u0439 \u0441\u0442\u0430\u043b\u0438&nbsp;<\/h2><p class=\"wp-block-paragraph\">\u0412\u0437\u0433\u043b\u044f\u043d\u0438\u0442\u0435 \u043d\u0430 \u0440\u0430\u0441\u043f\u0440\u043e\u0441\u0442\u0440\u0430\u043d\u0435\u043d\u043d\u044b\u0435 \u043c\u0430\u0440\u043a\u0438 \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u043e\u0439 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0435\u0439 \u0441\u0442\u0430\u043b\u0438:<\/p><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u041e\u0446\u0435\u043d\u043a\u0430<\/strong><\/td><td><strong>\u042d\u043a\u0432\u0438\u0432\u0430\u043b\u0435\u043d\u0442\u043d\u044b\u0439 \u043a\u043b\u0430\u0441\u0441 (UNS\/EN)<\/strong><\/td><td><strong>\u041e\u043f\u0438\u0441\u0430\u043d\u0438\u0435<\/strong><\/td><td><strong>\u0420\u0430\u0441\u043f\u0440\u043e\u0441\u0442\u0440\u0430\u043d\u0435\u043d\u043d\u044b\u0435 \u043f\u0440\u0438\u043b\u043e\u0436\u0435\u043d\u0438\u044f<\/strong><\/td><\/tr><tr><td><a href=\"https:\/\/steelprogroup.com\/ru\/stainless-steel\/grades\/grade-302\/\" target=\"_blank\" data-type=\"post\" data-id=\"10950\" rel=\"noreferrer noopener\">302<\/a><\/td><td>S30200 \/ 1.4300<\/td><td>\u041e\u0431\u0449\u0435\u0433\u043e \u043d\u0430\u0437\u043d\u0430\u0447\u0435\u043d\u0438\u044f 18-8<\/td><td>\u041f\u0440\u0443\u0436\u0438\u043d\u044b, \u0448\u0430\u0439\u0431\u044b, \u0433\u0430\u0439\u043a\u0438, \u0431\u043e\u043b\u0442\u044b, \u0430\u0432\u0442\u043e\u043c\u043e\u0431\u0438\u043b\u044c\u043d\u0430\u044f \u043e\u0442\u0434\u0435\u043b\u043a\u0430<\/td><\/tr><tr><td><a href=\"https:\/\/steelprogroup.com\/ru\/stainless-steel\/grades\/grade-202\/\" target=\"_blank\" data-type=\"post\" data-id=\"10958\" rel=\"noreferrer noopener\">202<\/a><\/td><td>\u042120200 \/ 1.4373<\/td><td>N \u0438 Mn \u0447\u0430\u0441\u0442\u0438\u0447\u043d\u043e \u0437\u0430\u043c\u0435\u043d\u044f\u044e\u0442 Ni<\/td><td>\u041a\u0443\u0445\u043e\u043d\u043d\u0430\u044f \u0443\u0442\u0432\u0430\u0440\u044c, \u0430\u0432\u0442\u043e\u043c\u043e\u0431\u0438\u043b\u044c\u043d\u044b\u0435 \u0434\u0435\u0442\u0430\u043b\u0438, \u0436\u0435\u043b\u0435\u0437\u043d\u043e\u0434\u043e\u0440\u043e\u0436\u043d\u044b\u0435 \u0432\u0430\u0433\u043e\u043d\u044b, \u043c\u043e\u0439\u043a\u0438<\/td><\/tr><tr><td><a href=\"https:\/\/steelprogroup.com\/ru\/stainless-steel\/grades\/grade-201\/\">201<\/a><\/td><td>\u042120100 \/ 1.4372<\/td><td>N \u0438 Mn \u0447\u0430\u0441\u0442\u0438\u0447\u043d\u043e \u0437\u0430\u043c\u0435\u043d\u044f\u044e\u0442 Ni<\/td><td>\u041a\u0443\u0445\u043e\u043d\u043d\u0430\u044f \u0443\u0442\u0432\u0430\u0440\u044c, \u043a\u043e\u043d\u0441\u0442\u0440\u0443\u043a\u0446\u0438\u0438 \u043f\u0440\u0438\u0431\u043e\u0440\u043e\u0432, \u0436\u0435\u043b\u0435\u0437\u043d\u043e\u0434\u043e\u0440\u043e\u0436\u043d\u044b\u0435 \u0432\u0430\u0433\u043e\u043d\u044b, \u0448\u043b\u0430\u043d\u0433\u0438<\/td><\/tr><tr><td><a href=\"https:\/\/steelprogroup.com\/ru\/stainless-steel\/grades\/grade-305\/\" target=\"_blank\" data-type=\"post\" data-id=\"8501\" rel=\"noreferrer noopener\">305<\/a><\/td><td>S30500 \/ 1.4303<\/td><td>\u0423\u0432\u0435\u043b\u0438\u0447\u0435\u043d\u043e \u0441\u043e\u0434\u0435\u0440\u0436\u0430\u043d\u0438\u0435 Ni \u0434\u043b\u044f \u0441\u043d\u0438\u0436\u0435\u043d\u0438\u044f \u0443\u043f\u0440\u043e\u0447\u043d\u0435\u043d\u0438\u044f<\/td><td>\u0414\u0435\u0442\u0430\u043b\u0438 \u0433\u043b\u0443\u0431\u043e\u043a\u043e\u0439 \u0432\u044b\u0442\u044f\u0436\u043a\u0438, \u044d\u043b\u0435\u043a\u0442\u0440\u043e\u043d\u043d\u044b\u0435 \u043a\u043e\u043c\u043f\u043e\u043d\u0435\u043d\u0442\u044b, \u043a\u0443\u0445\u043e\u043d\u043d\u044b\u0435 \u043c\u043e\u0439\u043a\u0438, \u043f\u0440\u0443\u0436\u0438\u043d\u044b<\/td><\/tr><tr><td><a href=\"https:\/\/steelprogroup.com\/ru\/stainless-steel\/grades\/grade-304\/\" target=\"_blank\" data-type=\"post\" data-id=\"8332\" rel=\"noreferrer noopener\">304<\/a><\/td><td>S30400 \/ 1.4301<\/td><td>\u0411\u043e\u043b\u0435\u0435 \u043d\u0438\u0437\u043a\u0438\u0439 C \u0434\u043b\u044f \u043b\u0443\u0447\u0448\u0435\u0439 \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u043e\u0439 \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u0438 \u0441\u0432\u0430\u0440\u043d\u044b\u0445 \u043a\u043e\u043d\u0441\u0442\u0440\u0443\u043a\u0446\u0438\u0439<\/td><td>\u0425\u0438\u043c\u0438\u0447\u0435\u0441\u043a\u0438\u0435 \u043a\u043e\u043d\u0442\u0435\u0439\u043d\u0435\u0440\u044b, \u043a\u0443\u0445\u043e\u043d\u043d\u043e\u0435 \u043e\u0431\u043e\u0440\u0443\u0434\u043e\u0432\u0430\u043d\u0438\u0435, \u0430\u0440\u0445\u0438\u0442\u0435\u043a\u0442\u0443\u0440\u043d\u044b\u0435 \u043f\u0430\u043d\u0435\u043b\u0438, \u0440\u0435\u0437\u0435\u0440\u0432\u0443\u0430\u0440\u044b<\/td><\/tr><tr><td>304L<\/td><td>S30403 \/ 1.4306, 1.4307<\/td><td>\u0421\u043d\u0438\u0436\u0435\u043d\u0438\u0435 \u0441\u043e\u0434\u0435\u0440\u0436\u0430\u043d\u0438\u044f \u0421 \u0434\u043b\u044f \u043e\u0431\u0435\u0441\u043f\u0435\u0447\u0435\u043d\u0438\u044f \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u043e\u0439 \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u0438 \u043f\u043e\u0441\u043b\u0435 \u0441\u0432\u0430\u0440\u043a\u0438<\/td><td>\u041a\u043e\u043d\u0441\u0442\u0440\u0443\u043a\u0446\u0438\u043e\u043d\u043d\u044b\u0435 \u044d\u043b\u0435\u043c\u0435\u043d\u0442\u044b \u0432 \u0443\u0441\u043b\u043e\u0432\u0438\u044f\u0445 \u0432\u044b\u0441\u043e\u043a\u0438\u0445 \u0442\u0435\u043c\u043f\u0435\u0440\u0430\u0442\u0443\u0440, \u0442\u0435\u043f\u043b\u043e\u043e\u0431\u043c\u0435\u043d\u043d\u0438\u043a\u0438, \u0434\u0435\u0442\u0430\u043b\u0438 \u043d\u0435\u0444\u0442\u0435\u043f\u0435\u0440\u0435\u0440\u0430\u0431\u0430\u0442\u044b\u0432\u0430\u044e\u0449\u0438\u0445 \u0437\u0430\u0432\u043e\u0434\u043e\u0432, \u043e\u0431\u043e\u0440\u0443\u0434\u043e\u0432\u0430\u043d\u0438\u0435 \u0434\u043b\u044f \u0445\u0438\u043c\u0438\u0447\u0435\u0441\u043a\u043e\u0439 \u043f\u0435\u0440\u0435\u0440\u0430\u0431\u043e\u0442\u043a\u0438<\/td><\/tr><tr><td>304\u041d<\/td><td>S30451 \/ 1.4315<\/td><td>\u0414\u043e\u0431\u0430\u0432\u043b\u0435\u043d \u0430\u0437\u043e\u0442 \u0434\u043b\u044f \u0443\u0432\u0435\u043b\u0438\u0447\u0435\u043d\u0438\u044f \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u0438<\/td><td>\u041a\u043e\u043d\u0441\u0442\u0440\u0443\u043a\u0446\u0438\u043e\u043d\u043d\u044b\u0435 \u044d\u043b\u0435\u043c\u0435\u043d\u0442\u044b, \u0430\u0432\u0442\u043e\u043c\u043e\u0431\u0438\u043b\u044c\u043d\u044b\u0435 \u0432\u044b\u0445\u043b\u043e\u043f\u043d\u044b\u0435 \u0441\u0438\u0441\u0442\u0435\u043c\u044b, \u0445\u0438\u043c\u0438\u0447\u0435\u0441\u043a\u0438\u0435 \u0440\u0435\u0437\u0435\u0440\u0432\u0443\u0430\u0440\u044b, \u0441\u0443\u0434\u043e\u0432\u043e\u0435 \u043e\u0431\u043e\u0440\u0443\u0434\u043e\u0432\u0430\u043d\u0438\u0435<\/td><\/tr><tr><td>304NL<\/td><td>S30453 \/ 1.4311<\/td><td>\u0414\u043e\u0431\u0430\u0432\u043b\u0435\u043d \u0430\u0437\u043e\u0442 \u0434\u043b\u044f \u0443\u0432\u0435\u043b\u0438\u0447\u0435\u043d\u0438\u044f \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u0438<\/td><td>\u041a\u043e\u043d\u0441\u0442\u0440\u0443\u043a\u0446\u0438\u043e\u043d\u043d\u044b\u0435 \u044d\u043b\u0435\u043c\u0435\u043d\u0442\u044b \u0432 \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u044b\u0445 \u0441\u0440\u0435\u0434\u0430\u0445, \u0441\u0432\u0430\u0440\u043d\u044b\u0435 \u044d\u043b\u0435\u043c\u0435\u043d\u0442\u044b, \u0434\u0435\u0442\u0430\u043b\u0438 \u043c\u043e\u0440\u0441\u043a\u043e\u0433\u043e \u043d\u0430\u0437\u043d\u0430\u0447\u0435\u043d\u0438\u044f, \u0441\u043e\u0441\u0443\u0434\u044b \u043f\u043e\u0434 \u0434\u0430\u0432\u043b\u0435\u043d\u0438\u0435\u043c<\/td><\/tr><tr><td><a href=\"https:\/\/steelprogroup.com\/ru\/stainless-steel\/grades\/grade-303\/\" target=\"_blank\" data-type=\"post\" data-id=\"8822\" rel=\"noreferrer noopener\">303<\/a><\/td><td>S30300 \/ 1.4305<\/td><td>S \u0434\u043e\u0431\u0430\u0432\u043b\u0435\u043d\u043e \u0434\u043b\u044f \u043e\u0431\u0440\u0430\u0431\u0430\u0442\u044b\u0432\u0430\u0435\u043c\u043e\u0441\u0442\u0438<\/td><td>\u0412\u0438\u043d\u0442\u044b, \u0433\u0430\u0439\u043a\u0438, \u0431\u043e\u043b\u0442\u044b, \u0432\u0430\u043b\u044b, \u043a\u043b\u0430\u043f\u0430\u043d\u044b<\/td><\/tr><tr><td>303Se<\/td><td>S30323 \/ 1.4300<\/td><td>Se \u0434\u043e\u0431\u0430\u0432\u043b\u0435\u043d \u0434\u043b\u044f \u043b\u0443\u0447\u0448\u0435\u0439 \u043e\u0431\u0440\u0430\u0431\u0430\u0442\u044b\u0432\u0430\u0435\u043c\u043e\u0441\u0442\u0438<\/td><td>\u0412\u044b\u0441\u043e\u043a\u043e\u0442\u043e\u0447\u043d\u0430\u044f \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0430 \u0434\u0435\u0442\u0430\u043b\u0435\u0439, \u044d\u043b\u0435\u043a\u0442\u0440\u043e\u0440\u0430\u0441\u043f\u0440\u0435\u0434\u0435\u043b\u0438\u0442\u0435\u043b\u044c\u043d\u0430\u044f \u0430\u043f\u043f\u0430\u0440\u0430\u0442\u0443\u0440\u0430, \u043a\u043b\u0430\u043f\u0430\u043d\u044b, \u0440\u0430\u0437\u044a\u0435\u043c\u044b<\/td><\/tr><tr><td>S30430<\/td><td>S30430 \/ 1.4567<\/td><td>\u0414\u043e\u0431\u0430\u0432\u043b\u0435\u043d\u0430 \u043c\u0435\u0434\u044c \u0434\u043b\u044f \u0443\u043b\u0443\u0447\u0448\u0435\u043d\u0438\u044f \u0445\u043e\u043b\u043e\u0434\u043d\u043e\u0439 \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0438<\/td><td>\u0410\u0432\u0442\u043e\u043c\u043e\u0431\u0438\u043b\u044c\u043d\u044b\u0435 \u0442\u0435\u043f\u043b\u043e\u043e\u0431\u043c\u0435\u043d\u043d\u0438\u043a\u0438, \u0441\u043e\u0441\u0443\u0434\u044b \u0432\u044b\u0441\u043e\u043a\u043e\u0433\u043e \u0434\u0430\u0432\u043b\u0435\u043d\u0438\u044f, \u0442\u0440\u0443\u0431\u044b, \u0430\u0440\u0445\u0438\u0442\u0435\u043a\u0442\u0443\u0440\u043d\u044b\u0435 \u043f\u0440\u0438\u043b\u043e\u0436\u0435\u043d\u0438\u044f<\/td><\/tr><tr><td><a href=\"https:\/\/steelprogroup.com\/ru\/stainless-steel\/grades\/grade-316\/\" target=\"_blank\" data-type=\"post\" data-id=\"10280\" rel=\"noreferrer noopener\">316<\/a><\/td><td>S31600 \/ 1.4401<\/td><td>\u0414\u043e\u0431\u0430\u0432\u043b\u0435\u043d Mo \u0434\u043b\u044f \u043f\u043e\u0432\u044b\u0448\u0435\u043d\u0438\u044f \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u043e\u0439 \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u0438<\/td><td>\u041c\u0435\u0434\u0438\u0446\u0438\u043d\u0441\u043a\u0438\u0435 \u0438\u043d\u0441\u0442\u0440\u0443\u043c\u0435\u043d\u0442\u044b, \u0441\u0443\u0434\u043e\u0432\u043e\u0435 \u043e\u0431\u043e\u0440\u0443\u0434\u043e\u0432\u0430\u043d\u0438\u0435, \u0445\u0438\u043c\u0438\u0447\u0435\u0441\u043a\u0438\u0435 \u043a\u043e\u043d\u0442\u0435\u0439\u043d\u0435\u0440\u044b, \u043e\u0431\u043e\u0440\u0443\u0434\u043e\u0432\u0430\u043d\u0438\u0435 \u0434\u043b\u044f \u043f\u0435\u0440\u0435\u0440\u0430\u0431\u043e\u0442\u043a\u0438 \u043f\u0438\u0449\u0435\u0432\u044b\u0445 \u043f\u0440\u043e\u0434\u0443\u043a\u0442\u043e\u0432<\/td><\/tr><tr><td>316L<\/td><td>S31603 \/ 1.4404, 1.4435<\/td><td>\u0421\u043d\u0438\u0436\u0435\u043d\u0438\u0435 \u0441\u043e\u0434\u0435\u0440\u0436\u0430\u043d\u0438\u044f \u0421 \u0434\u043b\u044f \u043e\u0431\u0435\u0441\u043f\u0435\u0447\u0435\u043d\u0438\u044f \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u043e\u0439 \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u0438 \u043f\u043e\u0441\u043b\u0435 \u0441\u0432\u0430\u0440\u043a\u0438<\/td><td>\u0424\u0430\u0440\u043c\u0430\u0446\u0435\u0432\u0442\u0438\u0447\u0435\u0441\u043a\u043e\u0435 \u043e\u0431\u043e\u0440\u0443\u0434\u043e\u0432\u0430\u043d\u0438\u0435, \u043c\u043e\u0440\u0441\u043a\u043e\u0435 \u043f\u0440\u0438\u043c\u0435\u043d\u0435\u043d\u0438\u0435, \u0440\u0435\u0437\u0435\u0440\u0432\u0443\u0430\u0440\u044b \u0434\u043b\u044f \u0445\u0438\u043c\u0438\u0447\u0435\u0441\u043a\u043e\u0439 \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0438, \u043f\u043e\u0432\u0435\u0440\u0445\u043d\u043e\u0441\u0442\u0438 \u0434\u043b\u044f \u043f\u0440\u0438\u0433\u043e\u0442\u043e\u0432\u043b\u0435\u043d\u0438\u044f \u043f\u0438\u0449\u0438<\/td><\/tr><tr><td><a href=\"https:\/\/steelprogroup.com\/ru\/stainless-steel\/grades\/grade-316n\/\" target=\"_blank\" data-type=\"post\" data-id=\"11040\" rel=\"noreferrer noopener\">316\u041d<\/a><\/td><td>S31651 \/ 1.4429<\/td><td>\u0414\u043e\u0431\u0430\u0432\u043b\u0435\u043d \u0430\u0437\u043e\u0442 \u0434\u043b\u044f \u0443\u0432\u0435\u043b\u0438\u0447\u0435\u043d\u0438\u044f \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u0438<\/td><td>\u0412\u044b\u0441\u043e\u043a\u043e\u043f\u0440\u043e\u0447\u043d\u044b\u0435 \u0434\u0435\u0442\u0430\u043b\u0438 \u0432 \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u044b\u0445 \u0441\u0440\u0435\u0434\u0430\u0445, \u0441\u043e\u0441\u0443\u0434\u044b \u043f\u043e\u0434 \u0434\u0430\u0432\u043b\u0435\u043d\u0438\u0435\u043c, \u043c\u043e\u0440\u0441\u043a\u0438\u0435 \u043a\u043e\u043c\u043f\u043e\u043d\u0435\u043d\u0442\u044b, \u043c\u0435\u0434\u0438\u0446\u0438\u043d\u0441\u043a\u0438\u0435 \u043f\u0440\u0438\u0431\u043e\u0440\u044b<\/td><\/tr><tr><td>316\u041b\u041d<\/td><td>S31653 \/ 1.4429<\/td><td>\u0421\u043e\u0434\u0435\u0440\u0436\u0430\u043d\u0438\u0435 \u0443\u0433\u043b\u0435\u0440\u043e\u0434\u0430 \u0443\u043c\u0435\u043d\u044c\u0448\u0435\u043d\u043e, \u0434\u043b\u044f \u043f\u043e\u0432\u044b\u0448\u0435\u043d\u0438\u044f \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u0438 \u0434\u043e\u0431\u0430\u0432\u043b\u0435\u043d \u0430\u0437\u043e\u0442<\/td><td>\u041a\u043e\u043c\u043f\u043e\u043d\u0435\u043d\u0442\u044b \u044f\u0434\u0435\u0440\u043d\u043e\u0433\u043e \u0440\u0435\u0430\u043a\u0442\u043e\u0440\u0430, \u043a\u0440\u0438\u043e\u0433\u0435\u043d\u043d\u044b\u0435 \u0441\u043e\u0441\u0443\u0434\u044b, \u0445\u0438\u043c\u0438\u0447\u0435\u0441\u043a\u043e\u0435 \u0442\u0435\u0445\u043d\u043e\u043b\u043e\u0433\u0438\u0447\u0435\u0441\u043a\u043e\u0435 \u043e\u0431\u043e\u0440\u0443\u0434\u043e\u0432\u0430\u043d\u0438\u0435, \u0442\u0440\u0443\u0431\u043e\u043f\u0440\u043e\u0432\u043e\u0434\u044b \u0432\u044b\u0441\u043e\u043a\u043e\u0433\u043e \u0434\u0430\u0432\u043b\u0435\u043d\u0438\u044f<\/td><\/tr><tr><td>316\u0424<\/td><td>S31620 \/ 1.4436<\/td><td>\u0414\u043e\u0431\u0430\u0432\u043b\u0435\u043d\u044b S \u0438 P \u0434\u043b\u044f \u0443\u043b\u0443\u0447\u0448\u0435\u043d\u0438\u044f \u043e\u0431\u0440\u0430\u0431\u0430\u0442\u044b\u0432\u0430\u0435\u043c\u043e\u0441\u0442\u0438<\/td><td>\u0414\u0435\u0442\u0430\u043b\u0438 \u043d\u0430\u0441\u043e\u0441\u043e\u0432, \u043a\u043e\u043c\u043f\u043e\u043d\u0435\u043d\u0442\u044b \u043a\u043b\u0430\u043f\u0430\u043d\u043e\u0432, \u0432\u0430\u043b\u044b, \u043f\u0440\u0435\u0446\u0438\u0437\u0438\u043e\u043d\u043d\u044b\u0435 \u0444\u0438\u0442\u0438\u043d\u0433\u0438<\/td><\/tr><tr><td><a href=\"https:\/\/steelprogroup.com\/ru\/stainless-steel\/grades\/317-317l\/\" target=\"_blank\" data-type=\"post\" data-id=\"10948\" rel=\"noreferrer noopener\">317<\/a><\/td><td>S31700 \/ 1.4449<\/td><td>\u0414\u043e\u0431\u0430\u0432\u043b\u0435\u043d\u043e \u0431\u043e\u043b\u044c\u0448\u0435 Mo \u0438 Cr \u0434\u043b\u044f \u043b\u0443\u0447\u0448\u0435\u0439 \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u043e\u0439 \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u0438<\/td><td>\u0425\u0438\u043c\u0438\u0447\u0435\u0441\u043a\u043e\u0435 \u0442\u0435\u0445\u043d\u043e\u043b\u043e\u0433\u0438\u0447\u0435\u0441\u043a\u043e\u0435 \u043e\u0431\u043e\u0440\u0443\u0434\u043e\u0432\u0430\u043d\u0438\u0435, \u043c\u043e\u0440\u0441\u043a\u043e\u0435 \u043f\u0440\u0438\u043c\u0435\u043d\u0435\u043d\u0438\u0435, \u0444\u0430\u0440\u043c\u0430\u0446\u0435\u0432\u0442\u0438\u0447\u0435\u0441\u043a\u043e\u0435 \u043e\u0431\u043e\u0440\u0443\u0434\u043e\u0432\u0430\u043d\u0438\u0435, \u043d\u0435\u0444\u0442\u0435\u0445\u0438\u043c\u0438\u0447\u0435\u0441\u043a\u0438\u0435 \u0437\u0430\u0432\u043e\u0434\u044b<\/td><\/tr><tr><td><a href=\"https:\/\/steelprogroup.com\/ru\/stainless-steel\/grades\/317-317l\/\" target=\"_blank\" data-type=\"post\" data-id=\"10948\" rel=\"noreferrer noopener\">317L<\/a><\/td><td>S31703 \/ 1.4438<\/td><td>\u0421\u043d\u0438\u0436\u0435\u043d\u0438\u0435 \u0441\u043e\u0434\u0435\u0440\u0436\u0430\u043d\u0438\u044f \u0421 \u0434\u043b\u044f \u0443\u043b\u0443\u0447\u0448\u0435\u043d\u0438\u044f \u0441\u0432\u0430\u0440\u043e\u0447\u043d\u044b\u0445 \u0445\u0430\u0440\u0430\u043a\u0442\u0435\u0440\u0438\u0441\u0442\u0438\u043a<\/td><td>\u041e\u0431\u043e\u0440\u0443\u0434\u043e\u0432\u0430\u043d\u0438\u0435 \u0434\u043b\u044f \u0446\u0435\u043b\u043b\u044e\u043b\u043e\u0437\u043d\u043e-\u0431\u0443\u043c\u0430\u0436\u043d\u043e\u0439 \u043f\u0440\u043e\u043c\u044b\u0448\u043b\u0435\u043d\u043d\u043e\u0441\u0442\u0438, \u0445\u0438\u043c\u0438\u0447\u0435\u0441\u043a\u0438\u0435 \u0440\u0435\u0437\u0435\u0440\u0432\u0443\u0430\u0440\u044b, \u043c\u043e\u0440\u0441\u043a\u0438\u0435 \u0441\u043e\u043e\u0440\u0443\u0436\u0435\u043d\u0438\u044f, \u0441\u0438\u0441\u0442\u0435\u043c\u044b \u0434\u0435\u0441\u0443\u043b\u044c\u0444\u0443\u0440\u0430\u0446\u0438\u0438 \u0434\u044b\u043c\u043e\u0432\u044b\u0445 \u0433\u0430\u0437\u043e\u0432<\/td><\/tr><tr><td>310, 310\u0421<\/td><td>S31000, S31008 \/ 1.4840, 1.4845<\/td><td>\u0411\u043e\u043b\u044c\u0448\u0435 Cr \u0438 Ni \u0434\u043b\u044f \u0435\u0449\u0435 \u043b\u0443\u0447\u0448\u0435\u0439 \u0442\u0435\u0440\u043c\u043e\u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u0438<\/td><td>\u0424\u0443\u0442\u0435\u0440\u043e\u0432\u043a\u0430 \u043f\u0435\u0447\u0435\u0439, \u043a\u043e\u043c\u043f\u043e\u043d\u0435\u043d\u0442\u044b \u043f\u0435\u0447\u0435\u0439, \u043a\u0430\u043c\u0435\u0440\u044b \u0441\u0433\u043e\u0440\u0430\u043d\u0438\u044f, \u0442\u0435\u043f\u043b\u043e\u043e\u0431\u043c\u0435\u043d\u043d\u0438\u043a\u0438<\/td><\/tr><tr><td><a href=\"https:\/\/steelprogroup.com\/ru\/stainless-steel\/grades\/grade-309\/\" target=\"_blank\" data-type=\"post\" data-id=\"11610\" rel=\"noreferrer noopener\">309<\/a>, 309\u0421<\/td><td>\u042130900, \u042130908\/1.4828, 1.4833<\/td><td>\u0423\u0432\u0435\u043b\u0438\u0447\u0435\u043d\u043e \u0441\u043e\u0434\u0435\u0440\u0436\u0430\u043d\u0438\u0435 Cr \u0438 Ni \u0434\u043b\u044f \u043f\u043e\u0432\u044b\u0448\u0435\u043d\u0438\u044f \u0442\u0435\u0440\u043c\u043e\u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u0438<\/td><td>\u0414\u0435\u0442\u0430\u043b\u0438 \u043f\u0435\u0447\u0435\u0439, \u0442\u0435\u043f\u043b\u043e\u043e\u0431\u043c\u0435\u043d\u043d\u0438\u043a\u0438, \u0444\u0443\u0442\u0435\u0440\u043e\u0432\u043a\u0430 \u043f\u0435\u0447\u0435\u0439, \u043e\u0431\u043e\u0440\u0443\u0434\u043e\u0432\u0430\u043d\u0438\u0435 \u0434\u043b\u044f \u043d\u0435\u0444\u0442\u0435\u043f\u0435\u0440\u0435\u0440\u0430\u0431\u0430\u0442\u044b\u0432\u0430\u044e\u0449\u0438\u0445 \u0437\u0430\u0432\u043e\u0434\u043e\u0432<\/td><\/tr><tr><td><a href=\"https:\/\/steelprogroup.com\/ru\/stainless-steel\/grades\/grade-314\/\">314<\/a><\/td><td>S31400 \/ 1.4841<\/td><td>\u0423\u0432\u0435\u043b\u0438\u0447\u0435\u043d\u043e \u0441\u043e\u0434\u0435\u0440\u0436\u0430\u043d\u0438\u0435 Si \u0434\u043b\u044f \u043c\u0430\u043a\u0441\u0438\u043c\u0430\u043b\u044c\u043d\u043e\u0439 \u0442\u0435\u0440\u043c\u043e\u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u0438<\/td><td>\u0414\u0435\u0442\u0430\u043b\u0438 \u043f\u0435\u0447\u0435\u0439, \u0433\u0430\u0437\u043e\u0432\u044b\u0435 \u0433\u043e\u0440\u0435\u043b\u043a\u0438, \u043a\u0430\u043c\u0435\u0440\u044b \u0441\u0433\u043e\u0440\u0430\u043d\u0438\u044f, \u0442\u0435\u043f\u043b\u043e\u043e\u0431\u043c\u0435\u043d\u043d\u0438\u043a\u0438<\/td><\/tr><tr><td>330<\/td><td>N08330 \/ 1.4886<\/td><td>\u0414\u043e\u0431\u0430\u0432\u043b\u0435\u043d Ni \u0434\u043b\u044f \u0443\u0441\u0442\u043e\u0439\u0447\u0438\u0432\u043e\u0441\u0442\u0438 \u043a \u043d\u0430\u0443\u0433\u043b\u0435\u0440\u043e\u0436\u0438\u0432\u0430\u043d\u0438\u044e \u0438 \u0442\u0435\u0440\u043c\u0438\u0447\u0435\u0441\u043a\u043e\u043c\u0443 \u0443\u0434\u0430\u0440\u0443<\/td><td>\u0414\u0435\u0442\u0430\u043b\u0438 \u043f\u0435\u0447\u0435\u0439, \u043a\u043e\u043c\u043f\u043e\u043d\u0435\u043d\u0442\u044b \u0433\u0430\u0437\u043e\u0432\u044b\u0445 \u0442\u0443\u0440\u0431\u0438\u043d, \u0442\u0435\u043f\u043b\u043e\u043e\u0431\u043c\u0435\u043d\u043d\u0438\u043a\u0438, \u043e\u0431\u043e\u0440\u0443\u0434\u043e\u0432\u0430\u043d\u0438\u0435 \u0434\u043b\u044f \u0445\u0438\u043c\u0438\u0447\u0435\u0441\u043a\u0438\u0445 \u043f\u0440\u043e\u0446\u0435\u0441\u0441\u043e\u0432<\/td><\/tr><tr><td>302\u0411<\/td><td>\u042130215 \/ \u2013<\/td><td>\u0414\u043e\u0431\u0430\u0432\u043b\u0435\u043d \u043a\u0440\u0435\u043c\u043d\u0438\u0439 \u0434\u043b\u044f \u043f\u043e\u0432\u044b\u0448\u0435\u043d\u0438\u044f \u0443\u0441\u0442\u043e\u0439\u0447\u0438\u0432\u043e\u0441\u0442\u0438 \u043a \u043e\u0431\u0440\u0430\u0437\u043e\u0432\u0430\u043d\u0438\u044e \u043d\u0430\u043a\u0438\u043f\u0438<\/td><td>\u041a\u043e\u043c\u043f\u043e\u043d\u0435\u043d\u0442\u044b \u043f\u0435\u0447\u0435\u0439, \u0442\u0435\u043f\u043b\u043e\u043e\u0431\u043c\u0435\u043d\u043d\u0438\u043a\u0438, \u0430\u0432\u0442\u043e\u043c\u043e\u0431\u0438\u043b\u044c\u043d\u044b\u0435 \u043a\u043e\u043b\u043b\u0435\u043a\u0442\u043e\u0440\u044b<\/td><\/tr><tr><td><a href=\"https:\/\/steelprogroup.com\/ru\/stainless-steel\/308\/\" target=\"_blank\" data-type=\"post\" data-id=\"7937\" rel=\"noreferrer noopener\">308<\/a><\/td><td>S30800 \/ 1.4332<\/td><td>\u0411\u043e\u043b\u0435\u0435 \u0432\u044b\u0441\u043e\u043a\u043e\u0435 \u0441\u043e\u0434\u0435\u0440\u0436\u0430\u043d\u0438\u0435 Cr \u0438 Ni, \u0438\u0441\u043f\u043e\u043b\u044c\u0437\u0443\u0435\u0442\u0441\u044f \u0432 \u043e\u0441\u043d\u043e\u0432\u043d\u043e\u043c \u0434\u043b\u044f \u0441\u0432\u0430\u0440\u043a\u0438<\/td><td>\u0421\u0432\u0430\u0440\u043e\u0447\u043d\u044b\u0435 \u043f\u0440\u0443\u0442\u043a\u0438, \u043f\u0440\u0438\u0441\u0430\u0434\u043e\u0447\u043d\u044b\u0435 \u043c\u0430\u0442\u0435\u0440\u0438\u0430\u043b\u044b, \u0432\u044b\u0441\u043e\u043a\u043e\u0442\u0435\u043c\u043f\u0435\u0440\u0430\u0442\u0443\u0440\u043d\u044b\u0435 \u0432\u044b\u0445\u043b\u043e\u043f\u043d\u044b\u0435 \u0441\u0438\u0441\u0442\u0435\u043c\u044b, \u0444\u0443\u0442\u0435\u0440\u043e\u0432\u043a\u0430 \u043f\u0435\u0447\u0435\u0439<\/td><\/tr><tr><td><a href=\"https:\/\/steelprogroup.com\/ru\/stainless-steel\/grades\/grade-321\/\" target=\"_blank\" data-type=\"post\" data-id=\"10964\" rel=\"noreferrer noopener\">321<\/a><\/td><td>S32100 \/ 1.4541<\/td><td>\u0414\u043e\u0431\u0430\u0432\u043b\u0435\u043d Ti \u0434\u043b\u044f \u043f\u0440\u0435\u0434\u043e\u0442\u0432\u0440\u0430\u0449\u0435\u043d\u0438\u044f \u043e\u0441\u0430\u0436\u0434\u0435\u043d\u0438\u044f \u043a\u0430\u0440\u0431\u0438\u0434\u043e\u0432<\/td><td>\u0412\u044b\u0445\u043b\u043e\u043f\u043d\u044b\u0435 \u0441\u0438\u0441\u0442\u0435\u043c\u044b \u0441\u0430\u043c\u043e\u043b\u0435\u0442\u043e\u0432, \u0442\u0435\u0440\u043c\u043e\u043e\u043a\u0438\u0441\u043b\u0438\u0442\u0435\u043b\u0438, \u0434\u0435\u0442\u0430\u043b\u0438 \u043f\u0435\u0447\u0435\u0439, \u0442\u0435\u043f\u043b\u043e\u043e\u0431\u043c\u0435\u043d\u043d\u0438\u043a\u0438<\/td><\/tr><tr><td><a href=\"https:\/\/steelprogroup.com\/ru\/stainless-steel\/grades\/grade-347\/\">347<\/a><\/td><td>S34700 \/ 1.4550<\/td><td>\u0414\u043e\u0431\u0430\u0432\u043b\u0435\u043d\u044b Nb \u0438 Ta \u0434\u043b\u044f \u043f\u0440\u0435\u0434\u043e\u0442\u0432\u0440\u0430\u0449\u0435\u043d\u0438\u044f \u043e\u0441\u0430\u0436\u0434\u0435\u043d\u0438\u044f \u043a\u0430\u0440\u0431\u0438\u0434\u043e\u0432<\/td><td>\u0410\u044d\u0440\u043e\u043a\u043e\u0441\u043c\u0438\u0447\u0435\u0441\u043a\u0438\u0435 \u043a\u043e\u043c\u043f\u043e\u043d\u0435\u043d\u0442\u044b, \u0432\u044b\u0441\u043e\u043a\u043e\u0442\u0435\u043c\u043f\u0435\u0440\u0430\u0442\u0443\u0440\u043d\u043e\u0435 \u043e\u0431\u043e\u0440\u0443\u0434\u043e\u0432\u0430\u043d\u0438\u0435, \u0441\u0432\u0430\u0440\u043d\u044b\u0435 \u0434\u0435\u0442\u0430\u043b\u0438 \u043a\u043e\u0442\u043b\u043e\u0432, \u0433\u0430\u0437\u043e\u0442\u0443\u0440\u0431\u0438\u043d\u043d\u044b\u0435 \u0434\u0432\u0438\u0433\u0430\u0442\u0435\u043b\u0438<\/td><\/tr><tr><td>348<\/td><td>S34800 \/ 1.4551<\/td><td>Ta \u0438 Co \u043e\u0433\u0440\u0430\u043d\u0438\u0447\u0435\u043d\u044b \u0434\u043b\u044f \u0438\u0441\u043f\u043e\u043b\u044c\u0437\u043e\u0432\u0430\u043d\u0438\u044f \u0432 \u044f\u0434\u0435\u0440\u043d\u043e\u0439 \u043e\u0431\u043b\u0430\u0441\u0442\u0438<\/td><td>\u0414\u0435\u0442\u0430\u043b\u0438 \u044f\u0434\u0435\u0440\u043d\u044b\u0445 \u0440\u0435\u0430\u043a\u0442\u043e\u0440\u043e\u0432, \u0432\u044b\u0441\u043e\u043a\u043e\u0442\u0435\u043c\u043f\u0435\u0440\u0430\u0442\u0443\u0440\u043d\u044b\u0435 \u043a\u043e\u043c\u043f\u043e\u043d\u0435\u043d\u0442\u044b \u0441\u0430\u043c\u043e\u043b\u0435\u0442\u043e\u0432, \u043a\u043e\u043c\u043f\u043e\u043d\u0435\u043d\u0442\u044b \u0434\u043b\u044f \u0433\u0435\u043d\u0435\u0440\u0430\u0446\u0438\u0438 \u044d\u043b\u0435\u043a\u0442\u0440\u043e\u044d\u043d\u0435\u0440\u0433\u0438\u0438, \u0442\u0435\u043f\u043b\u043e\u043e\u0431\u043c\u0435\u043d\u043d\u0438\u043a\u0438<\/td><\/tr><tr><td>205<\/td><td>\u042120500 \/ \u2013<\/td><td>N \u0438 Mn \u0447\u0430\u0441\u0442\u0438\u0447\u043d\u043e \u0437\u0430\u043c\u0435\u043d\u044f\u044e\u0442 Ni<\/td><td>\u041a\u043e\u043c\u043c\u0435\u0440\u0447\u0435\u0441\u043a\u043e\u0435 \u043f\u0438\u0449\u0435\u0432\u043e\u0435 \u043e\u0431\u043e\u0440\u0443\u0434\u043e\u0432\u0430\u043d\u0438\u0435, \u043a\u0443\u0445\u043e\u043d\u043d\u0430\u044f \u0442\u0435\u0445\u043d\u0438\u043a\u0430, \u0440\u0435\u0437\u0435\u0440\u0432\u0443\u0430\u0440\u044b \u0434\u043b\u044f \u0445\u0440\u0430\u043d\u0435\u043d\u0438\u044f, \u0441\u0432\u0430\u0440\u043d\u044b\u0435 \u043a\u043e\u043d\u0441\u0442\u0440\u0443\u043a\u0446\u0438\u0438<\/td><\/tr><tr><td>384<\/td><td>\u042138400 \/ \u2013<\/td><td>\u0411\u043e\u043b\u044c\u0448\u0435 Ni \u0434\u043b\u044f \u0441\u043d\u0438\u0436\u0435\u043d\u0438\u044f \u0443\u043f\u0440\u043e\u0447\u043d\u0435\u043d\u0438\u044f<\/td><td>\u0414\u0435\u0442\u0430\u043b\u0438 \u0433\u043b\u0443\u0431\u043e\u043a\u043e\u0439 \u0432\u044b\u0442\u044f\u0436\u043a\u0438, \u0432\u0438\u043d\u0442\u044b, \u0431\u043e\u043b\u0442\u044b, \u043f\u0440\u0443\u0436\u0438\u043d\u044b, \u043a\u0440\u0435\u043f\u0435\u0436\u0438<\/td><\/tr><tr><td>329<\/td><td>S32900 \/ 1.4460<\/td><td><strong><em>(\u0414\u0443\u043f\u043b\u0435\u043a\u0441: \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442 + \u0444\u0435\u0440\u0440\u0438\u0442)<\/em><\/strong> \u0423\u0432\u0435\u043b\u0438\u0447\u0435\u043d\u043e \u0441\u043e\u0434\u0435\u0440\u0436\u0430\u043d\u0438\u0435 Cr \u0438 \u0443\u043c\u0435\u043d\u044c\u0448\u0435\u043d\u043e \u0441\u043e\u0434\u0435\u0440\u0436\u0430\u043d\u0438\u0435 Ni \u0434\u043b\u044f \u043f\u043e\u0432\u044b\u0448\u0435\u043d\u0438\u044f \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u0438 \u043a \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u043e\u043c\u0443 \u0440\u0430\u0441\u0442\u0440\u0435\u0441\u043a\u0438\u0432\u0430\u043d\u0438\u044e \u043f\u043e\u0434 \u043d\u0430\u043f\u0440\u044f\u0436\u0435\u043d\u0438\u0435\u043c<\/td><td>\u041d\u0435\u0444\u0442\u0435\u0433\u0430\u0437\u043e\u043f\u0440\u043e\u0432\u043e\u0434\u044b, \u0441\u0443\u0434\u043e\u0432\u043e\u0435 \u043e\u0431\u043e\u0440\u0443\u0434\u043e\u0432\u0430\u043d\u0438\u0435, \u0445\u0438\u043c\u0438\u0447\u0435\u0441\u043a\u0438\u0435 \u0440\u0435\u0437\u0435\u0440\u0432\u0443\u0430\u0440\u044b, \u0441\u043e\u0441\u0443\u0434\u044b \u043f\u043e\u0434 \u0434\u0430\u0432\u043b\u0435\u043d\u0438\u0435\u043c<\/td><\/tr><\/tbody><\/table><\/figure><h3 class=\"wp-block-heading\">\u041a\u0430\u043a\u0430\u044f \u043c\u0430\u0440\u043a\u0430 \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u043e\u0439 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0435\u0439 \u0441\u0442\u0430\u043b\u0438 \u044f\u0432\u043b\u044f\u0435\u0442\u0441\u044f \u043b\u0443\u0447\u0448\u0435\u0439?<\/h3><p class=\"wp-block-paragraph\">\u041d\u0435 \u0441\u0443\u0449\u0435\u0441\u0442\u0432\u0443\u0435\u0442 \u0443\u043d\u0438\u0432\u0435\u0440\u0441\u0430\u043b\u044c\u043d\u043e\u0439 \u00ab\u043b\u0443\u0447\u0448\u0435\u0439\u00bb \u043c\u0430\u0440\u043a\u0438 \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u043e\u0439 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0435\u0439 \u0441\u0442\u0430\u043b\u0438. \u042d\u0442\u043e \u0437\u0430\u0432\u0438\u0441\u0438\u0442 \u043e\u0442 \u0440\u0430\u0437\u043b\u0438\u0447\u043d\u044b\u0445 \u0444\u0430\u043a\u0442\u043e\u0440\u043e\u0432. \u0414\u043b\u044f \u043e\u0431\u0449\u0438\u0445 \u0446\u0435\u043b\u0435\u0439 \u0440\u0430\u0441\u043f\u0440\u043e\u0441\u0442\u0440\u0430\u043d\u0435\u043d\u0430 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c 304 \u0438\u0437-\u0437\u0430 \u0435\u0435 \u0445\u043e\u0440\u043e\u0448\u0435\u0439 \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u043e\u0439 \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u0438 \u0438 \u043f\u0440\u043e\u0441\u0442\u043e\u0442\u044b \u0438\u0437\u0433\u043e\u0442\u043e\u0432\u043b\u0435\u043d\u0438\u044f. \u0414\u043b\u044f \u0431\u043e\u043b\u0435\u0435 \u0432\u044b\u0441\u043e\u043a\u043e\u0439 \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u043e\u0439 \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u0438, \u043d\u0430\u043f\u0440\u0438\u043c\u0435\u0440, \u0432 \u043c\u043e\u0440\u0441\u043a\u043e\u0439 \u0441\u0440\u0435\u0434\u0435, \u043b\u0443\u0447\u0448\u0435 \u043f\u043e\u0434\u043e\u0439\u0434\u0435\u0442 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c 316, \u043f\u043e\u0441\u043a\u043e\u043b\u044c\u043a\u0443 \u043e\u043d\u0430 \u0441\u043e\u0434\u0435\u0440\u0436\u0438\u0442 \u043c\u043e\u043b\u0438\u0431\u0434\u0435\u043d. \u0414\u043b\u044f \u0432\u044b\u0441\u043e\u043a\u043e\u0442\u0435\u043c\u043f\u0435\u0440\u0430\u0442\u0443\u0440\u043d\u044b\u0445 \u043f\u0440\u0438\u043c\u0435\u043d\u0435\u043d\u0438\u0439 \u043f\u043e\u0434\u0445\u043e\u0434\u0438\u0442 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c 310 \u0438\u0437-\u0437\u0430 \u0435\u0435 \u043f\u0440\u0435\u0432\u043e\u0441\u0445\u043e\u0434\u043d\u043e\u0439 \u0442\u0435\u0440\u043c\u043e\u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u0438. \u041a\u0430\u0436\u0434\u0430\u044f \u043c\u0430\u0440\u043a\u0430 \u0438\u043c\u0435\u0435\u0442 \u0441\u0432\u043e\u0438 \u0441\u043e\u0431\u0441\u0442\u0432\u0435\u043d\u043d\u044b\u0435 \u0441\u0438\u043b\u044c\u043d\u044b\u0435 \u0441\u0442\u043e\u0440\u043e\u043d\u044b, \u043f\u043e\u044d\u0442\u043e\u043c\u0443 \u043b\u0443\u0447\u0448\u0438\u0439 \u0432\u044b\u0431\u043e\u0440 \u0437\u0430\u0432\u0438\u0441\u0438\u0442 \u043e\u0442 \u043a\u043e\u043d\u043a\u0440\u0435\u0442\u043d\u044b\u0445 \u043f\u043e\u0442\u0440\u0435\u0431\u043d\u043e\u0441\u0442\u0435\u0439.<\/p><h2 class=\"wp-block-heading\">\u041f\u0440\u0438\u043c\u0435\u043d\u0435\u043d\u0438\u0435 \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u043e\u0439 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0435\u0439 \u0441\u0442\u0430\u043b\u0438<\/h2><p class=\"wp-block-paragraph\">\u041e\u0437\u043d\u0430\u043a\u043e\u043c\u044c\u0442\u0435\u0441\u044c \u0441 \u0442\u0430\u0431\u043b\u0438\u0446\u0435\u0439 \u043d\u0438\u0436\u0435, \u0447\u0442\u043e\u0431\u044b \u0443\u0437\u043d\u0430\u0442\u044c \u043e\u0431 \u043e\u0441\u043d\u043e\u0432\u043d\u044b\u0445 \u043e\u0442\u0440\u0430\u0441\u043b\u044f\u0445 \u0438 \u043e\u0431\u043b\u0430\u0441\u0442\u044f\u0445 \u043f\u0440\u0438\u043c\u0435\u043d\u0435\u043d\u0438\u044f, \u0433\u0434\u0435 \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0430\u044f \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u0438\u0441\u043f\u043e\u043b\u044c\u0437\u0443\u0435\u0442\u0441\u044f \u0447\u0430\u0449\u0435 \u0432\u0441\u0435\u0433\u043e:&nbsp;<\/p><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u041f\u0440\u043e\u043c\u044b\u0448\u043b\u0435\u043d\u043d\u043e\u0441\u0442\u044c<\/strong><\/td><td><strong>\u041f\u0440\u0438\u043b\u043e\u0436\u0435\u043d\u0438\u0435<\/strong><\/td><\/tr><tr><td>\u0415\u0434\u0430 \u0438 \u043d\u0430\u043f\u0438\u0442\u043a\u0438<\/td><td>\u0420\u0435\u0437\u0435\u0440\u0432\u0443\u0430\u0440\u044b, \u0442\u0440\u0443\u0431\u043e\u043f\u0440\u043e\u0432\u043e\u0434\u044b, \u0435\u043c\u043a\u043e\u0441\u0442\u0438 \u0434\u043b\u044f \u0445\u0440\u0430\u043d\u0435\u043d\u0438\u044f, \u0442\u0435\u0445\u043d\u043e\u043b\u043e\u0433\u0438\u0447\u0435\u0441\u043a\u043e\u0435 \u043e\u0431\u043e\u0440\u0443\u0434\u043e\u0432\u0430\u043d\u0438\u0435<\/td><\/tr><tr><td>\u041c\u0435\u0434\u0438\u0446\u0438\u043d\u0430 \u0438 \u0444\u0430\u0440\u043c\u0430\u0446\u0435\u0432\u0442\u0438\u043a\u0430<\/td><td>\u0425\u0438\u0440\u0443\u0440\u0433\u0438\u0447\u0435\u0441\u043a\u0438\u0435 \u0438\u043d\u0441\u0442\u0440\u0443\u043c\u0435\u043d\u0442\u044b, \u0438\u043c\u043f\u043b\u0430\u043d\u0442\u0438\u0440\u0443\u0435\u043c\u044b\u0435 \u0443\u0441\u0442\u0440\u043e\u0439\u0441\u0442\u0432\u0430, \u0441\u0442\u0435\u0440\u0438\u043b\u0438\u0437\u0430\u0446\u0438\u043e\u043d\u043d\u044b\u0435 \u043b\u043e\u0442\u043a\u0438, \u0434\u0438\u0430\u0433\u043d\u043e\u0441\u0442\u0438\u0447\u0435\u0441\u043a\u043e\u0435 \u043e\u0431\u043e\u0440\u0443\u0434\u043e\u0432\u0430\u043d\u0438\u0435<\/td><\/tr><tr><td>\u0425\u0438\u043c\u0438\u0447\u0435\u0441\u043a\u0430\u044f \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0430<\/td><td>\u0422\u0435\u043f\u043b\u043e\u043e\u0431\u043c\u0435\u043d\u043d\u0438\u043a\u0438, \u0420\u0435\u0430\u043a\u0442\u043e\u0440\u044b, \u041d\u0430\u0441\u043e\u0441\u044b, \u041a\u043b\u0430\u043f\u0430\u043d\u044b<\/td><\/tr><tr><td>\u041d\u0435\u0444\u0442\u044c \u0438 \u0433\u0430\u0437<\/td><td>\u0422\u0440\u0443\u0431\u043e\u043f\u0440\u043e\u0432\u043e\u0434\u044b, \u043c\u043e\u0440\u0441\u043a\u0438\u0435 \u043f\u043b\u0430\u0442\u0444\u043e\u0440\u043c\u044b, \u0441\u043e\u0441\u0443\u0434\u044b \u043f\u043e\u0434 \u0434\u0430\u0432\u043b\u0435\u043d\u0438\u0435\u043c, \u0442\u0435\u043f\u043b\u043e\u043e\u0431\u043c\u0435\u043d\u043d\u0438\u043a\u0438<\/td><\/tr><tr><td>\u0410\u0432\u0442\u043e\u043c\u043e\u0431\u0438\u043b\u044c\u043d\u044b\u0439<\/td><td>\u0412\u044b\u0445\u043b\u043e\u043f\u043d\u044b\u0435 \u0441\u0438\u0441\u0442\u0435\u043c\u044b, \u0442\u043e\u043f\u043b\u0438\u0432\u043d\u044b\u0435 \u0431\u0430\u043a\u0438, \u044d\u043b\u0435\u043c\u0435\u043d\u0442\u044b \u043e\u0442\u0434\u0435\u043b\u043a\u0438, \u0434\u0430\u0442\u0447\u0438\u043a\u0438<\/td><\/tr><tr><td>\u0410\u044d\u0440\u043e\u043a\u043e\u0441\u043c\u0438\u0447\u0435\u0441\u043a\u0430\u044f \u043f\u0440\u043e\u043c\u044b\u0448\u043b\u0435\u043d\u043d\u043e\u0441\u0442\u044c<\/td><td>\u041a\u043e\u043c\u043f\u043e\u043d\u0435\u043d\u0442\u044b \u0434\u0432\u0438\u0433\u0430\u0442\u0435\u043b\u044f, \u043a\u0440\u0435\u043f\u0435\u0436, \u043a\u043e\u043d\u0441\u0442\u0440\u0443\u043a\u0442\u0438\u0432\u043d\u044b\u0435 \u044d\u043b\u0435\u043c\u0435\u043d\u0442\u044b, \u0432\u044b\u0445\u043b\u043e\u043f\u043d\u044b\u0435 \u0441\u0438\u0441\u0442\u0435\u043c\u044b<\/td><\/tr><tr><td>\u0421\u0442\u0440\u043e\u0438\u0442\u0435\u043b\u044c\u0441\u0442\u0432\u043e<\/td><td>\u041a\u0440\u043e\u0432\u043b\u044f, \u0424\u0430\u0441\u0430\u0434\u043d\u044b\u0435 \u043f\u0430\u043d\u0435\u043b\u0438, \u041f\u0435\u0440\u0438\u043b\u0430, \u041a\u043e\u043d\u0441\u0442\u0440\u0443\u043a\u0446\u0438\u043e\u043d\u043d\u044b\u0435 \u043e\u043f\u043e\u0440\u044b<\/td><\/tr><tr><td>\u0413\u0435\u043d\u0435\u0440\u0430\u0446\u0438\u044f \u044d\u043b\u0435\u043a\u0442\u0440\u043e\u044d\u043d\u0435\u0440\u0433\u0438\u0438<\/td><td>\u041a\u043e\u0442\u043b\u044b, \u0442\u0443\u0440\u0431\u0438\u043d\u044b, \u0443\u0441\u0442\u0430\u043d\u043e\u0432\u043a\u0438 \u0434\u0435\u0441\u0443\u043b\u044c\u0444\u0443\u0440\u0430\u0446\u0438\u0438 \u0434\u044b\u043c\u043e\u0432\u044b\u0445 \u0433\u0430\u0437\u043e\u0432, \u043a\u043e\u043c\u043f\u043e\u043d\u0435\u043d\u0442\u044b \u044f\u0434\u0435\u0440\u043d\u044b\u0445 \u0440\u0435\u0430\u043a\u0442\u043e\u0440\u043e\u0432<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u0410\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0430\u044f, \u043c\u0430\u0440\u0442\u0435\u043d\u0441\u0438\u0442\u043d\u0430\u044f, \u0444\u0435\u0440\u0440\u0438\u0442\u043d\u0430\u044f, \u0434\u0443\u043f\u043b\u0435\u043a\u0441\u043d\u0430\u044f \u0438 \u0443\u043f\u0440\u043e\u0447\u043d\u0435\u043d\u043d\u0430\u044f \u0434\u0438\u0441\u043f\u0435\u0440\u0441\u0438\u043e\u043d\u043d\u044b\u043c \u0442\u0432\u0435\u0440\u0434\u0435\u043d\u0438\u0435\u043c \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c<\/h2><p class=\"wp-block-paragraph\">\u0421\u0440\u0430\u0432\u043d\u0438\u0442\u0435 \u043f\u044f\u0442\u044c \u043a\u043b\u0430\u0441\u0441\u043e\u0432 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0435\u0439 \u0441\u0442\u0430\u043b\u0438 \u0432 \u0442\u0430\u0431\u043b\u0438\u0446\u0435 \u043d\u0438\u0436\u0435:<\/p><figure class=\"wp-block-table\"><table><tbody><tr><td><strong>\u0421\u0432\u043e\u0439\u0441\u0442\u0432\u043e<\/strong><\/td><td><strong>\u0410\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0430\u044f \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c<\/strong><\/td><td><a href=\"http:\/\/steelprogroup.com\/ru\/stainless-steel\/types\/martensite\/\" target=\"_blank\" rel=\"noreferrer noopener\"><strong>\u041c\u0430\u0440\u0442\u0435\u043d\u0441\u0438\u0442\u043d\u0430\u044f \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c<\/strong><\/a><\/td><td><a href=\"https:\/\/steelprogroup.com\/ru\/stainless-steel\/type\/ferritic\/\" target=\"_blank\" rel=\"noreferrer noopener\"><strong>\u0424\u0435\u0440\u0440\u0438\u0442\u043d\u0430\u044f \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c<\/strong><\/a><\/td><td><a href=\"https:\/\/steelprogroup.com\/ru\/stainless-steel\/type\/duplex\/\" target=\"_blank\" rel=\"noreferrer noopener\"><strong>\u0414\u0443\u043f\u043b\u0435\u043a\u0441\u043d\u0430\u044f \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c<\/strong><\/a><\/td><td><strong><a href=\"https:\/\/steelprogroup.com\/ru\/stainless-steel\/type\/precipitation-hardening\/\">\u0414\u0438\u0441\u043f\u0435\u0440\u0441\u0438\u043e\u043d\u043d\u043e-\u0442\u0432\u0435\u0440\u0434\u0435\u044e\u0449\u0438\u0439<\/a><\/strong><\/td><\/tr><tr><td>\u041a\u0440\u0438\u0441\u0442\u0430\u043b\u043b\u0438\u0447\u0435\u0441\u043a\u0430\u044f \u0441\u0442\u0440\u0443\u043a\u0442\u0443\u0440\u0430<\/td><td>\u0410\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u044b\u0439 (\u0413\u0426\u041a)<\/td><td>\u041c\u0430\u0440\u0442\u0435\u043d\u0441\u0438\u0442\u043d\u044b\u0439 (BCT)<\/td><td>\u0424\u0435\u0440\u0440\u0438\u0442\u043d\u044b\u0439 (\u041e\u0426\u041a)<\/td><td>\u0410\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u044b\u0439 + \u0444\u0435\u0440\u0440\u0438\u0442\u043d\u044b\u0439, \u043e\u0431\u044b\u0447\u043d\u043e 50% + 50%<\/td><td>\u041c\u0430\u0440\u0442\u0435\u043d\u0441\u0438\u0442\u043d\u044b\u0439 \u0438\u043b\u0438 \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u044b\u0439 + \u0434\u0438\u0441\u043f\u0435\u0440\u0441\u0438\u043e\u043d\u043d\u043e-\u0442\u0432\u0435\u0440\u0434\u0435\u044e\u0449\u0438\u0439<\/td><\/tr><tr><td>\u041c\u0435\u0445\u0430\u043d\u0438\u0447\u0435\u0441\u043a\u0430\u044f \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c<\/td><td>\u0412\u044b\u0441\u043e\u043a\u0430\u044f \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c, \u0445\u043e\u0440\u043e\u0448\u0430\u044f \u043f\u043b\u0430\u0441\u0442\u0438\u0447\u043d\u043e\u0441\u0442\u044c<\/td><td>\u0412\u044b\u0441\u043e\u043a\u0430\u044f \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c, \u0432\u044b\u0441\u043e\u043a\u0430\u044f \u0442\u0432\u0435\u0440\u0434\u043e\u0441\u0442\u044c<\/td><td>\u0423\u043c\u0435\u0440\u0435\u043d\u043d\u0430\u044f \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c, \u0445\u043e\u0440\u043e\u0448\u0430\u044f \u0432\u044f\u0437\u043a\u043e\u0441\u0442\u044c<\/td><td>\u0412\u044b\u0441\u043e\u043a\u0430\u044f \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c, \u043f\u0440\u0435\u0432\u043e\u0441\u0445\u043e\u0434\u043d\u043e\u0435 \u0441\u043e\u043f\u0440\u043e\u0442\u0438\u0432\u043b\u0435\u043d\u0438\u0435 \u0440\u0430\u0437\u0440\u0443\u0448\u0435\u043d\u0438\u044e<\/td><td>\u041e\u0447\u0435\u043d\u044c \u0432\u044b\u0441\u043e\u043a\u0430\u044f \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c \u043f\u043e\u0441\u043b\u0435 \u0442\u0435\u0440\u043c\u043e\u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0438<\/td><\/tr><tr><td>\u041a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u0430\u044f \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c<\/td><td>\u041f\u0440\u0435\u0432\u043e\u0441\u0445\u043e\u0434\u043d\u043e, \u043e\u0441\u043e\u0431\u0435\u043d\u043d\u043e \u0432 \u043a\u0438\u0441\u043b\u044b\u0445 \u0438 \u0445\u043b\u043e\u0440\u0438\u0434\u043d\u044b\u0445 \u0441\u0440\u0435\u0434\u0430\u0445<\/td><td>\u0423\u043c\u0435\u0440\u0435\u043d\u043d\u0430\u044f, \u043f\u043e\u0434\u0432\u0435\u0440\u0436\u0435\u043d\u0430 \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u0438 \u0432 \u0441\u0443\u0440\u043e\u0432\u044b\u0445 \u0443\u0441\u043b\u043e\u0432\u0438\u044f\u0445<\/td><td>\u0425\u043e\u0440\u043e\u0448\u043e, \u043e\u0441\u043e\u0431\u0435\u043d\u043d\u043e \u0432 \u043e\u043a\u0438\u0441\u043b\u0438\u0442\u0435\u043b\u044c\u043d\u044b\u0445 \u0441\u0440\u0435\u0434\u0430\u0445<\/td><td>\u041f\u0440\u0435\u0432\u043e\u0441\u0445\u043e\u0434\u043d\u043e, \u043e\u0441\u043e\u0431\u0435\u043d\u043d\u043e \u0432 \u0445\u043b\u043e\u0440\u0438\u0434\u043d\u043e\u0439 \u0438 \u043c\u043e\u0440\u0441\u043a\u043e\u0439 \u0441\u0440\u0435\u0434\u0435<\/td><td>\u0425\u043e\u0440\u043e\u0448\u043e, \u043d\u043e \u0445\u0443\u0436\u0435, \u0447\u0435\u043c \u0443 \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u044b\u0445 \u0438\u043b\u0438 \u0434\u0443\u043f\u043b\u0435\u043a\u0441\u043d\u044b\u0445 \u0442\u0438\u043f\u043e\u0432<\/td><\/tr><tr><td>\u0421\u0432\u0430\u0440\u0438\u0432\u0430\u0435\u043c\u043e\u0441\u0442\u044c<\/td><td>\u041e\u0442\u043b\u0438\u0447\u043d\u043e, \u043c\u0438\u043d\u0438\u043c\u0430\u043b\u044c\u043d\u043e\u0435 \u0432\u043e\u0437\u0434\u0435\u0439\u0441\u0442\u0432\u0438\u0435 \u0441\u0432\u0430\u0440\u043a\u0438<\/td><td>\u041f\u043b\u043e\u0445\u043e, \u0442\u0440\u0435\u0431\u0443\u0435\u0442\u0441\u044f \u043f\u0440\u0435\u0434\u0432\u0430\u0440\u0438\u0442\u0435\u043b\u044c\u043d\u0430\u044f \u0438 \u043f\u043e\u0441\u043b\u0435\u0434\u0443\u044e\u0449\u0430\u044f \u0442\u0435\u0440\u043c\u0438\u0447\u0435\u0441\u043a\u0430\u044f \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0430<\/td><td>\u0422\u0440\u0435\u0431\u0443\u0435\u0442\u0441\u044f \u0443\u043c\u0435\u0440\u0435\u043d\u043d\u0430\u044f \u043f\u043e\u0441\u043b\u0435\u0441\u0432\u0430\u0440\u043e\u0447\u043d\u0430\u044f \u0442\u0435\u0440\u043c\u043e\u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0430<\/td><td>\u0425\u043e\u0440\u043e\u0448\u043e, \u043d\u043e \u0441\u043a\u043e\u0440\u043e\u0441\u0442\u044c \u043e\u0445\u043b\u0430\u0436\u0434\u0435\u043d\u0438\u044f \u043d\u0435\u043e\u0431\u0445\u043e\u0434\u0438\u043c\u043e \u043a\u043e\u043d\u0442\u0440\u043e\u043b\u0438\u0440\u043e\u0432\u0430\u0442\u044c<\/td><td>\u0425\u043e\u0440\u043e\u0448\u043e, \u043d\u043e \u043f\u043e\u0441\u043b\u0435 \u0441\u0432\u0430\u0440\u043a\u0438 \u0442\u0440\u0435\u0431\u0443\u0435\u0442\u0441\u044f \u0442\u0435\u0440\u043c\u043e\u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0430<\/td><\/tr><tr><td>\u0422\u0435\u0440\u043c\u0438\u0447\u0435\u0441\u043a\u0430\u044f \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0430<\/td><td>\u041d\u0435\u0432\u043e\u0437\u043c\u043e\u0436\u043d\u043e \u0437\u0430\u043a\u0430\u043b\u0438\u0442\u044c \u0442\u0435\u0440\u043c\u0438\u0447\u0435\u0441\u043a\u043e\u0439 \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u043e\u0439, \u043c\u043e\u0436\u043d\u043e \u0443\u043f\u0440\u043e\u0447\u043d\u0438\u0442\u044c \u0445\u043e\u043b\u043e\u0434\u043d\u043e\u0439 \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u043e\u0439<\/td><td>\u0417\u0430\u043a\u0430\u043b\u043a\u0430 \u0438 \u043e\u0442\u043f\u0443\u0441\u043a \u0434\u043b\u044f \u0440\u0435\u0433\u0443\u043b\u0438\u0440\u043e\u0432\u0430\u043d\u0438\u044f \u0442\u0432\u0435\u0440\u0434\u043e\u0441\u0442\u0438<\/td><td>\u041d\u0435 \u043f\u043e\u0434\u043b\u0435\u0436\u0438\u0442 \u0442\u0435\u0440\u043c\u0438\u0447\u0435\u0441\u043a\u043e\u0439 \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0435, \u043c\u043e\u0436\u0435\u0442 \u0431\u044b\u0442\u044c \u0443\u043f\u0440\u043e\u0447\u043d\u0435\u043d \u0445\u043e\u043b\u043e\u0434\u043d\u043e\u0439 \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u043e\u0439<\/td><td>\u0421\u043e\u0445\u0440\u0430\u043d\u044f\u0435\u0442 \u0445\u043e\u0440\u043e\u0448\u0438\u0435 \u0441\u0432\u043e\u0439\u0441\u0442\u0432\u0430 \u043f\u043e\u0441\u043b\u0435 \u0442\u0435\u0440\u043c\u0438\u0447\u0435\u0441\u043a\u043e\u0439 \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0438<\/td><td>\u0423\u043f\u0440\u043e\u0447\u043d\u0435\u043d\u0438\u0435 \u043c\u0435\u0442\u043e\u0434\u043e\u043c \u0434\u0438\u0441\u043f\u0435\u0440\u0441\u0438\u043e\u043d\u043d\u043e\u0433\u043e \u0442\u0432\u0435\u0440\u0434\u0435\u043d\u0438\u044f<\/td><\/tr><tr><td>\u0422\u0438\u043f\u0438\u0447\u043d\u044b\u0435 \u043f\u0440\u0438\u043c\u0435\u043d\u0435\u043d\u0438\u044f<\/td><td>\u041f\u0438\u0449\u0435\u0432\u0430\u044f \u043f\u0440\u043e\u043c\u044b\u0448\u043b\u0435\u043d\u043d\u043e\u0441\u0442\u044c, \u0445\u0438\u043c\u0438\u0447\u0435\u0441\u043a\u043e\u0435 \u043e\u0431\u043e\u0440\u0443\u0434\u043e\u0432\u0430\u043d\u0438\u0435, \u043c\u0435\u0434\u0438\u0446\u0438\u043d\u0441\u043a\u0438\u0435 \u043f\u0440\u0438\u0431\u043e\u0440\u044b<\/td><td>\u041b\u043e\u043f\u0430\u0441\u0442\u0438, \u0432\u0430\u043b\u044b, \u043c\u0435\u0445\u0430\u043d\u0438\u0447\u0435\u0441\u043a\u0438\u0435 \u043a\u043e\u043c\u043f\u043e\u043d\u0435\u043d\u0442\u044b<\/td><td>\u0410\u0432\u0442\u043e\u043c\u043e\u0431\u0438\u043b\u044c\u043d\u044b\u0435 \u0432\u044b\u0445\u043b\u043e\u043f\u043d\u044b\u0435 \u0441\u0438\u0441\u0442\u0435\u043c\u044b, \u0442\u0435\u043f\u043b\u043e\u043e\u0431\u043c\u0435\u043d\u043d\u0438\u043a\u0438<\/td><td>\u041c\u043e\u0440\u0441\u043a\u043e\u0435 \u043c\u0430\u0448\u0438\u043d\u043e\u0441\u0442\u0440\u043e\u0435\u043d\u0438\u0435, \u043d\u0435\u0444\u0442\u0435- \u0438 \u0433\u0430\u0437\u043e\u043f\u0440\u043e\u0432\u043e\u0434\u044b<\/td><td>\u0410\u044d\u0440\u043e\u043a\u043e\u0441\u043c\u0438\u0447\u0435\u0441\u043a\u0430\u044f, \u044f\u0434\u0435\u0440\u043d\u0430\u044f, \u0432\u044b\u0441\u043e\u043a\u043e\u043f\u0440\u043e\u0447\u043d\u0430\u044f \u043f\u0440\u043e\u043c\u044b\u0448\u043b\u0435\u043d\u043d\u043e\u0441\u0442\u044c<\/td><\/tr><\/tbody><\/table><\/figure><h2 class=\"wp-block-heading\">\u0427\u0442\u043e \u0432\u0430\u0441 \u0442\u0430\u043a\u0436\u0435 \u043c\u043e\u0436\u0435\u0442 \u0431\u0435\u0441\u043f\u043e\u043a\u043e\u0438\u0442\u044c<\/h2><p class=\"wp-block-paragraph\">\u0422\u0435\u043f\u0435\u0440\u044c, \u043a\u043e\u0433\u0434\u0430 \u0432\u044b \u0438\u043c\u0435\u0435\u0442\u0435 \u0431\u043e\u043b\u0435\u0435 \u0433\u043b\u0443\u0431\u043e\u043a\u043e\u0435 \u043f\u0440\u0435\u0434\u0441\u0442\u0430\u0432\u043b\u0435\u043d\u0438\u0435 \u043e\u0431 \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u043e\u0439 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0435\u0439 \u0441\u0442\u0430\u043b\u0438, \u0435\u0441\u0442\u044c \u0435\u0449\u0435 \u043d\u0435\u0441\u043a\u043e\u043b\u044c\u043a\u043e \u043e\u0431\u0449\u0438\u0445 \u0432\u043e\u043f\u0440\u043e\u0441\u043e\u0432, \u043a\u043e\u0442\u043e\u0440\u044b\u0435 \u0437\u0430\u0441\u043b\u0443\u0436\u0438\u0432\u0430\u044e\u0442 \u0432\u0430\u0448\u0435\u0433\u043e \u0432\u043d\u0438\u043c\u0430\u043d\u0438\u044f\uff1a&nbsp;<\/p><h3 class=\"wp-block-heading\">\u0412 \u0447\u0435\u043c \u0440\u0430\u0437\u043d\u0438\u0446\u0430 \u043c\u0435\u0436\u0434\u0443 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0435\u0439 \u0441\u0442\u0430\u043b\u044c\u044e \u0438 \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u043e\u0439 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0435\u0439 \u0441\u0442\u0430\u043b\u044c\u044e?<\/h3><p class=\"wp-block-paragraph\">\u041d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u043e\u0442\u043d\u043e\u0441\u0438\u0442\u0441\u044f \u043a \u0441\u0435\u043c\u0435\u0439\u0441\u0442\u0432\u0443 \u0441\u043f\u043b\u0430\u0432\u043e\u0432 \u043d\u0430 \u043e\u0441\u043d\u043e\u0432\u0435 \u0436\u0435\u043b\u0435\u0437\u0430, \u0438\u0437\u0432\u0435\u0441\u0442\u043d\u044b\u0445 \u0441\u0432\u043e\u0435\u0439 \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u043e\u0439 \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c\u044e. \u0410\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0430\u044f \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u2014 \u044d\u0442\u043e \u043e\u0441\u043e\u0431\u044b\u0439 \u0442\u0438\u043f \u0432 \u044d\u0442\u043e\u0439 \u0433\u0440\u0443\u043f\u043f\u0435, \u0438\u0437\u0432\u0435\u0441\u0442\u043d\u044b\u0439 \u0441\u0432\u043e\u0438\u043c \u0432\u044b\u0441\u043e\u043a\u0438\u043c \u0441\u043e\u0434\u0435\u0440\u0436\u0430\u043d\u0438\u0435\u043c \u0445\u0440\u043e\u043c\u0430 \u0438 \u043d\u0438\u043a\u0435\u043b\u044f, \u0447\u0442\u043e \u043f\u043e\u0432\u044b\u0448\u0430\u0435\u0442 \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u0443\u044e \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c \u0438 \u043f\u0440\u043e\u0447\u043d\u043e\u0441\u0442\u044c. \u042d\u0442\u043e \u0442\u0430\u043a\u0436\u0435 \u043d\u0430\u0438\u0431\u043e\u043b\u0435\u0435 \u0447\u0430\u0441\u0442\u043e \u0438\u0441\u043f\u043e\u043b\u044c\u0437\u0443\u0435\u043c\u044b\u0439 \u0442\u0438\u043f \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0435\u0439 \u0441\u0442\u0430\u043b\u0438, \u0441\u043e\u0441\u0442\u0430\u0432\u043b\u044f\u044e\u0449\u0438\u0439 \u043e\u043a\u043e\u043b\u043e 70% \u0432\u0441\u0435\u0433\u043e \u043f\u0440\u043e\u0438\u0437\u0432\u043e\u0434\u0441\u0442\u0432\u0430 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0435\u0439 \u0441\u0442\u0430\u043b\u0438.<\/p><h3 class=\"wp-block-heading\">\u041a\u0430\u043a\u0438\u0435 \u0435\u0449\u0435 \u0432\u0438\u0434\u044b \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0435\u0439 \u0441\u0442\u0430\u043b\u0438 \u0441\u0443\u0449\u0435\u0441\u0442\u0432\u0443\u044e\u0442 \u043f\u043e\u043c\u0438\u043c\u043e \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u043e\u0439 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0435\u0439 \u0441\u0442\u0430\u043b\u0438?<\/h3><p class=\"wp-block-paragraph\">\u0414\u0440\u0443\u0433\u0438\u0435 \u0442\u0438\u043f\u044b \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0435\u0439 \u0441\u0442\u0430\u043b\u0438 \u0432\u043a\u043b\u044e\u0447\u0430\u044e\u0442 \u0444\u0435\u0440\u0440\u0438\u0442\u043d\u0443\u044e \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0443\u044e \u0441\u0442\u0430\u043b\u044c, \u043c\u0430\u0440\u0442\u0435\u043d\u0441\u0438\u0442\u043d\u0443\u044e \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0443\u044e \u0441\u0442\u0430\u043b\u044c, \u0434\u0443\u043f\u043b\u0435\u043a\u0441\u043d\u0443\u044e \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0443\u044e \u0441\u0442\u0430\u043b\u044c \u0438 \u0434\u0438\u0441\u043f\u0435\u0440\u0441\u0438\u043e\u043d\u043d\u043e-\u0442\u0432\u0435\u0440\u0434\u0435\u044e\u0449\u0443\u044e \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0443\u044e \u0441\u0442\u0430\u043b\u044c.<\/p><h3 class=\"wp-block-heading\">\u0411\u0443\u0434\u0435\u0442 \u043b\u0438 \u0440\u0436\u0430\u0432\u0435\u0442\u044c \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0430\u044f \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c?<\/h3><p class=\"wp-block-paragraph\">\u0410\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0430\u044f \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u043e\u0431\u043b\u0430\u0434\u0430\u0435\u0442 \u0432\u044b\u0441\u043e\u043a\u043e\u0439 \u0443\u0441\u0442\u043e\u0439\u0447\u0438\u0432\u043e\u0441\u0442\u044c\u044e \u043a \u0440\u0436\u0430\u0432\u0447\u0438\u043d\u0435. \u041e\u0434\u043d\u0430\u043a\u043e \u043e\u043d\u0430 \u0432\u0441\u0435 \u0440\u0430\u0432\u043d\u043e \u043c\u043e\u0436\u0435\u0442 \u0440\u0436\u0430\u0432\u0435\u0442\u044c \u0432 \u044d\u043a\u0441\u0442\u0440\u0435\u043c\u0430\u043b\u044c\u043d\u044b\u0445 \u0443\u0441\u043b\u043e\u0432\u0438\u044f\u0445, \u043d\u0430\u043f\u0440\u0438\u043c\u0435\u0440, \u043f\u0440\u0438 \u0434\u043b\u0438\u0442\u0435\u043b\u044c\u043d\u043e\u043c \u0432\u043e\u0437\u0434\u0435\u0439\u0441\u0442\u0432\u0438\u0438 \u0441\u043e\u043b\u0435\u043d\u043e\u0439 \u0432\u043e\u0434\u044b \u0438\u043b\u0438 \u0435\u0434\u043a\u0438\u0445 \u0445\u0438\u043c\u0438\u043a\u0430\u0442\u043e\u0432, \u0438\u043b\u0438 \u0435\u0441\u043b\u0438 \u0437\u0430\u0449\u0438\u0442\u043d\u044b\u0439 \u0441\u043b\u043e\u0439 \u043f\u043e\u0432\u0440\u0435\u0436\u0434\u0435\u043d \u0438\u043b\u0438 \u0438\u0437\u043d\u043e\u0448\u0435\u043d.<\/p><p class=\"wp-block-paragraph\"><strong>\u0421\u0432\u044f\u0437\u0430\u043d\u043d\u043e\u0435 \u0447\u0442\u0435\u043d\u0438\u0435<\/strong><br><a href=\"https:\/\/steelprogroup.com\/ru\/stainless-steel\/rust\/\" target=\"_blank\" rel=\"noreferrer noopener\">\u0411\u0443\u0434\u0435\u0442 \u043b\u0438 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u0440\u0436\u0430\u0432\u0435\u0442\u044c \u0438 \u043a\u0430\u043a \u0441 \u044d\u0442\u0438\u043c \u0441\u043f\u0440\u0430\u0432\u0438\u0442\u044c\u0441\u044f?<\/a><\/p><h3 class=\"wp-block-heading\">\u041c\u0430\u0433\u043d\u0438\u0442\u043d\u0430 \u043b\u0438 \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0430\u044f \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c?<\/h3><p class=\"wp-block-paragraph\">\u0410\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0430\u044f \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c, \u043a\u0430\u043a \u043f\u0440\u0430\u0432\u0438\u043b\u043e, \u043d\u0435\u043c\u0430\u0433\u043d\u0438\u0442\u043d\u0430. \u041e\u0434\u043d\u0430\u043a\u043e \u043e\u043d\u0430 \u043c\u043e\u0436\u0435\u0442 \u0441\u0442\u0430\u0442\u044c \u0441\u043b\u0435\u0433\u043a\u0430 \u043c\u0430\u0433\u043d\u0438\u0442\u043d\u043e\u0439 \u043f\u043e\u0441\u043b\u0435 \u0445\u043e\u043b\u043e\u0434\u043d\u043e\u0439 \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0438, \u0442\u0430\u043a\u043e\u0439 \u043a\u0430\u043a \u0433\u0438\u0431\u043a\u0430 \u0438\u043b\u0438 \u0444\u043e\u0440\u043c\u043e\u0432\u043a\u0430, \u0438\u0437-\u0437\u0430 \u043f\u0440\u0435\u0432\u0440\u0430\u0449\u0435\u043d\u0438\u044f \u0447\u0430\u0441\u0442\u0438 \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u0430 \u0432 \u043c\u0430\u0440\u0442\u0435\u043d\u0441\u0438\u0442.<\/p><p class=\"wp-block-paragraph\"><strong>\u0421\u0432\u044f\u0437\u0430\u043d\u043d\u043e\u0435 \u0447\u0442\u0435\u043d\u0438\u0435<\/strong><br><a href=\"https:\/\/steelprogroup.com\/ru\/stainless-steel\/properties\/magnetic\/\" target=\"_blank\" rel=\"noreferrer noopener\">\u041c\u0430\u0433\u043d\u0438\u0442\u0438\u0442\u0441\u044f \u043b\u0438 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c?<\/a><\/p><h3 class=\"wp-block-heading\">\u0411\u0435\u0437\u043e\u043f\u0430\u0441\u043d\u0430 \u043b\u0438 \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0430\u044f \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u0434\u043b\u044f \u043f\u0440\u0438\u0433\u043e\u0442\u043e\u0432\u043b\u0435\u043d\u0438\u044f \u043f\u0438\u0449\u0438?<\/h3><p class=\"wp-block-paragraph\">\u0414\u0430, \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0430\u044f \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u0431\u0435\u0437\u043e\u043f\u0430\u0441\u043d\u0430 \u0434\u043b\u044f \u043f\u0440\u0438\u0433\u043e\u0442\u043e\u0432\u043b\u0435\u043d\u0438\u044f \u043f\u0438\u0449\u0438 \u0438 \u0448\u0438\u0440\u043e\u043a\u043e \u0438\u0441\u043f\u043e\u043b\u044c\u0437\u0443\u0435\u0442\u0441\u044f \u0432 \u043a\u0443\u0445\u043e\u043d\u043d\u044b\u0445 \u043f\u0440\u0438\u043d\u0430\u0434\u043b\u0435\u0436\u043d\u043e\u0441\u0442\u044f\u0445 \u0438 \u043e\u0431\u043e\u0440\u0443\u0434\u043e\u0432\u0430\u043d\u0438\u0438 \u0434\u043b\u044f \u043e\u0431\u0440\u0430\u0431\u043e\u0442\u043a\u0438 \u043f\u0438\u0449\u0435\u0432\u044b\u0445 \u043f\u0440\u043e\u0434\u0443\u043a\u0442\u043e\u0432. \u0415\u0435 \u043a\u043e\u0440\u0440\u043e\u0437\u0438\u043e\u043d\u043d\u0430\u044f \u0441\u0442\u043e\u0439\u043a\u043e\u0441\u0442\u044c \u0438 \u043d\u0435\u0440\u0435\u0430\u043a\u0442\u0438\u0432\u043d\u043e\u0441\u0442\u044c \u0434\u0435\u043b\u0430\u044e\u0442 \u0435\u0435 \u0438\u0434\u0435\u0430\u043b\u044c\u043d\u043e\u0439 \u0434\u043b\u044f \u0438\u0441\u043f\u043e\u043b\u044c\u0437\u043e\u0432\u0430\u043d\u0438\u044f \u0441 \u043f\u0440\u043e\u0434\u0443\u043a\u0442\u0430\u043c\u0438 \u043f\u0438\u0442\u0430\u043d\u0438\u044f \u0438 \u043d\u0430\u043f\u0438\u0442\u043a\u0430\u043c\u0438, \u043f\u0440\u0435\u0434\u043e\u0442\u0432\u0440\u0430\u0449\u0430\u044f \u0437\u0430\u0433\u0440\u044f\u0437\u043d\u0435\u043d\u0438\u0435 \u0438 \u0441\u043e\u0445\u0440\u0430\u043d\u044f\u044f \u0432\u043a\u0443\u0441.<\/p><h2 class=\"wp-block-heading\">\u0420\u0435\u0437\u044e\u043c\u0435 \u0438 \u0434\u0430\u043b\u0435\u0435<\/h2><p class=\"wp-block-paragraph\">\u0412 \u044d\u0442\u043e\u0439 \u0441\u0442\u0430\u0442\u044c\u0435 \u043a\u0440\u0430\u0442\u043a\u043e \u043e\u0431\u044a\u044f\u0441\u043d\u044f\u0435\u0442\u0441\u044f \u043e\u043f\u0440\u0435\u0434\u0435\u043b\u0435\u043d\u0438\u0435, \u0441\u043e\u0441\u0442\u0430\u0432, \u0441\u0432\u043e\u0439\u0441\u0442\u0432\u0430, \u043c\u0430\u0440\u043a\u0438, \u043e\u0431\u043b\u0430\u0441\u0442\u0438 \u043f\u0440\u0438\u043c\u0435\u043d\u0435\u043d\u0438\u044f \u0438 \u0434\u0440\u0443\u0433\u0438\u0435 \u0432\u0430\u0436\u043d\u044b\u0435 \u0430\u0441\u043f\u0435\u043a\u0442\u044b \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u043e\u0439 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0435\u0439 \u0441\u0442\u0430\u043b\u0438. \u0427\u0442\u043e\u0431\u044b \u0443\u0437\u043d\u0430\u0442\u044c \u0431\u043e\u043b\u044c\u0448\u0435 \u043e \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0435\u0439 \u0441\u0442\u0430\u043b\u0438 \u0438\u043b\u0438 \u0434\u0440\u0443\u0433\u0438\u0445 \u0442\u0438\u043f\u0430\u0445 \u0441\u0442\u0430\u043b\u0438, \u043f\u043e\u0441\u0435\u0442\u0438\u0442\u0435 <a href=\"https:\/\/steelprogroup.com\/ru\/blog\/\">\u043d\u0430\u0448 \u0431\u043b\u043e\u0433<\/a> \u0438\u043b\u0438 <a href=\"https:\/\/steelprogroup.com\/ru\/contact-us\/\">\u0441\u0432\u044f\u0436\u0438\u0442\u0435\u0441\u044c \u0441 \u043d\u0430\u0448\u0438\u043c\u0438 \u044d\u043a\u0441\u043f\u0435\u0440\u0442\u0430\u043c\u0438 \u043f\u043e \u043c\u0435\u0442\u0430\u043b\u043b\u0443<\/a>.<\/p><p class=\"wp-block-paragraph\">\u041a\u0430\u043a \u0432\u0435\u0434\u0443\u0449\u0438\u0439 \u043f\u0440\u043e\u0438\u0437\u0432\u043e\u0434\u0438\u0442\u0435\u043b\u044c \u0438 \u043f\u043e\u0441\u0442\u0430\u0432\u0449\u0438\u043a \u0440\u0435\u0448\u0435\u043d\u0438\u0439 \u0434\u043b\u044f \u0441\u043f\u0435\u0446\u0438\u0430\u043b\u044c\u043d\u043e\u0439 \u0441\u0442\u0430\u043b\u0438, SteelPRO \u043f\u0440\u0435\u0434\u043e\u0441\u0442\u0430\u0432\u043b\u044f\u0435\u0442 \u043c\u043d\u043e\u0433\u043e\u043e\u0442\u0440\u0430\u0441\u043b\u0435\u0432\u044b\u0435 \u043f\u0440\u0438\u043a\u043b\u0430\u0434\u043d\u044b\u0435 \u0440\u0435\u0448\u0435\u043d\u0438\u044f \u0438 \u0438\u043d\u0434\u0438\u0432\u0438\u0434\u0443\u0430\u043b\u044c\u043d\u044b\u0435 \u0443\u0441\u043b\u0443\u0433\u0438. \u041c\u044b \u0433\u0430\u0440\u0430\u043d\u0442\u0438\u0440\u0443\u0435\u043c \u043a\u0430\u0447\u0435\u0441\u0442\u0432\u043e \u043f\u0440\u043e\u0434\u0443\u043a\u0446\u0438\u0438 100% \u0438 \u0441\u0442\u0440\u0435\u043c\u0438\u043c\u0441\u044f \u0440\u0430\u0441\u0442\u0438 \u0432\u043c\u0435\u0441\u0442\u0435 \u0441 \u043d\u0430\u0448\u0438\u043c\u0438 \u043a\u043b\u0438\u0435\u043d\u0442\u0430\u043c\u0438. \u041f\u043e\u0441\u0435\u0442\u0438\u0442\u044c <a href=\"https:\/\/steelprogroup.com\/ru\">\u043d\u0430\u0448 \u0441\u0430\u0439\u0442<\/a> \u0447\u0442\u043e\u0431\u044b \u0443\u0437\u043d\u0430\u0442\u044c \u0431\u043e\u043b\u044c\u0448\u0435, \u0438\u043b\u0438 <a href=\"https:\/\/steelprogroup.com\/ru\/contact-us\/\">\u043e\u0442\u043f\u0440\u0430\u0432\u044c\u0442\u0435 \u043d\u0430\u043c \u0437\u0430\u043f\u0440\u043e\u0441<\/a>. \u041c\u044b \u0441\u0432\u044f\u0436\u0435\u043c\u0441\u044f \u0441 \u0432\u0430\u043c\u0438 \u0432 \u0431\u043b\u0438\u0436\u0430\u0439\u0448\u0435\u0435 \u0432\u0440\u0435\u043c\u044f!<\/p>","protected":false},"excerpt":{"rendered":"<p>\u0427\u0442\u043e \u0442\u0430\u043a\u043e\u0435 \u0430\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0430\u044f \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c? \u0410\u0443\u0441\u0442\u0435\u043d\u0438\u0442\u043d\u0430\u044f \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0430\u044f \u0441\u0442\u0430\u043b\u044c \u2014 \u043e\u0434\u0438\u043d \u0438\u0437 \u043f\u044f\u0442\u0438 \u043e\u0441\u043d\u043e\u0432\u043d\u044b\u0445 \u043a\u043b\u0430\u0441\u0441\u043e\u0432 \u043d\u0435\u0440\u0436\u0430\u0432\u0435\u044e\u0449\u0435\u0439 \u0441\u0442\u0430\u043b\u0438, \u043e\u043f\u0440\u0435\u0434\u0435\u043b\u044f\u0435\u043c\u044b\u0445 [\u2026]<\/p>","protected":false},"author":1,"featured_media":7839,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"_eb_attr":"","rank_math_lock_modified_date":false,"site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","theme-transparent-header-meta":"","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"default","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"categories":[4216,112],"tags":[4275],"class_list":["post-7858","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-type","category-stainless-steel","tag-featured"],"acf":[],"_links":{"self":[{"href":"https:\/\/steelprogroup.com\/ru\/wp-json\/wp\/v2\/posts\/7858","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/steelprogroup.com\/ru\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/steelprogroup.com\/ru\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ru\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ru\/wp-json\/wp\/v2\/comments?post=7858"}],"version-history":[{"count":0,"href":"https:\/\/steelprogroup.com\/ru\/wp-json\/wp\/v2\/posts\/7858\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/steelprogroup.com\/ru\/wp-json\/wp\/v2\/media\/7839"}],"wp:attachment":[{"href":"https:\/\/steelprogroup.com\/ru\/wp-json\/wp\/v2\/media?parent=7858"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/steelprogroup.com\/ru\/wp-json\/wp\/v2\/categories?post=7858"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/steelprogroup.com\/ru\/wp-json\/wp\/v2\/tags?post=7858"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}