SteelPRO Group, as a stainless steel manufacturer and supplier, provides 316L and other stainless steel plates in multiple grades, sizes and thicknesses. We have a rich inventory to meet your customized needs.
Our products: 316L hot rolled plate, 316L cold rolled plate, 1.4404 polished plate, checkered/diamond plate, perforated plate, decorative plate, etched plate, corrugated plate, etc.
Standard | ASTM A240, ASTM A480, EN 10088-2, ISO 9445 |
---|---|
Grade | 00Cr17Ni14Mo2, 0Cr18Ni12Mo2Ti, 1.4404, SUS316L, X2CrNiMo17-12-2 |
Length | 1000 mm-6000 mm (39.37-236.22 in), Customized |
Thickness | 0.5 mm-100 mm (0.02-3.94 in), Customized |
Full Width | 1000 mm-2000 mm (39.37-78.74 in), Customized |
Surface Finish | 2B, 2D, 2K, 4K, 6K, 8K, BA, Customized, Embossed, HL, No.4, SB |
Technique | Cold Drawn, Cold Rolled, Hot Rolled |
Form | Coated Plate, Coil, Cold-Rolled Plate, Embossed Plate, etc., Etched Plate, Flat Plate & Sheet, Hot-Rolled Plate, Perforated Plate, Polished Plate, Sheet, Strip |
Terms | Specification |
---|---|
Minimum Order Quantity: | 5 Tons |
Price: | To be negotiated |
Packaging Details: |
As Requested
|
Delivery Time: | Within 7-10 Working Days |
Payment Terms: | T/T, L/C, Credit Card |
Supply Ability: | 100000 Tons per month |
Certification: | RoHS, BIS, SABS, tisi, KS, JIS, ISO9001 |
Export To: |
United States, Canada, Australia, Malaysia, Russian Federation, United Kingdom, France, India, Indonesia, Israel, Japan, Korea, Philippines, Puerto Rico, Singapore, South Africa, Switzerland, Thailand, Vietnam, etc.
|
Carbon (C) | Silicon (Si) | Manganese (Mn) | Phosphorus (P) | Sulfur (S) | Chromium (Cr) | Nickel (Ni) | Molybdenum (Mo) | Nitrogen (N) |
---|---|---|---|---|---|---|---|---|
≤ 0.03 | ≤ 0.75 | ≤ 2.00 | ≤ 0.045 | ≤ 0.030 | 16.0 – 18.0 | 10.0 – 14.0 | 2.0 – 3.0 | ≤ 0.10 |
Properties | Metric Unit | Imperial Unit |
---|---|---|
Tensile Strength | 485 – 620 MPa | 70 – 90 ksi |
Yield Strength | ≥ 170 MPa | ≥ 25 ksi |
Vickers Hardness | 152 HV | 152 HV |
Brinell Hardness | 146 HB | 146 HB |
Rockwell Hardness | 95 HRB | 95 HRB |
Elongation | ≥ 40% | ≥ 40% |
Elastic Modulus | 193 – 200 GPa | 28 – 29 x 10⁶ psi |
1.Welding
2.Metal Fabrication
3.CNC Machining
4.Lathe
5.Forming
6.OEM/ODM
7.Quenching
8.Tempering
UT And Hardness Testing Info