304L Stainless Steel Coil

304L Stainless Steel Coil

SteelPRO Group is a leading manufacturer and supplier of 304L Stainless Steel Coils in China. We provide:

ASTM A240 304L stainless steel coil, UNS S30403 stainless steel coil, 1.4307 stainless steel coil, 304L stainless steel hot rolled coil, 304L stainless steel cold rolled coil, 304L stainless steel annealed coil, 304L stainless steel pickled coil, 304L stainless steel welded coil, 304L stainless steel slit coil, 304L stainless steel mill coil, 304L stainless steel polished coil,  304L stainless steel perforated coil, 304L stainless steel PVC coated coil, 304L stainless steel galvanized coil, 304 stainless steel plate/sheet/strip/foil, etc.

Standard

ASTM A240 / A240M, EN 10088-2

Grade

1.4307, SUS304L, UNS S30403

Thickness

0.3 mm – 6 mm (0.012'' – 0.236''), Customized

Full Width

1000 mm – 2000 mm (39.37'' – 78.74''), Customized

Edge

Mill Edge, Slit Edge, Trimmed Edge

Surface Finish

2B, 2D, 8K, BA, Brush, Checkered, Customized, Embossed, Etching, Hair Line, Mirror, No.1, No.4, No.8, Sand Blast

Technique

Annealing, Cold Rolling, Cutting to Length, Pickling, Slitting

Form

Brushed Coil, Cold Rolled Coil, Customized, Foils, Hot Rolled Coil, HRAP Coil, Mill Coil, Mirror Coil, Patterned Coil, Perforated Coil, Plates, Polished Coil, PVC-Coated Coil, Sheets, Slit Coil, Strips, Tin-Plated Coil, Titanium-Coated Coil

304L Stainless Steel Coil

304L Stainless Steel Coil

304L stainless steel coil is a low-carbon variant of 304, offering excellent corrosion resistance and weldability. It is ideal for applications requiring formability, such as chemical processing, food industry equipment, and architectural projects. The low carbon content reduces carbide precipitation during welding, making it suitable for heavy-duty environments. Choose 304L stainless steel coil for reliable performance and versatility in demanding applications.
304l stainless steel coil product

Business Terms

Business Terms

Terms Specification
Minimum Order Quantity: 5 Tons
Price: To be negotiated
Packaging Details:
As Requested
Delivery Time: Within 7-10 Working Days
Payment Terms: T/T, L/C, Credit Card
Supply Ability: 100000 Tons per month
Certification: RoHS, BIS, SABS, tisi, KS, JIS, ISO9001
Export To:
United States, Canada, Philippines, Australia, Korea, Mexico, Russian Federation, United Kingdom , etc.

Chemical Composition

Chemical Composition

ElementChromium, CrNickel, NiManganese, MnSilicon, SiCarbon, CPhosphorus, PSulfur, SNitrogen, NIron, Fe
Content (%)18.0-20.08.0-12.0≤ 2.00≤ 0.75≤ 0.030≤ 0.045≤ 0.030≤ 0.10Balance

Mechanical Properties

Mechanical Properties

PropertyMetricImperial
Tensile Strength (0% cold-worked)564 MPa81.8 ksi
Yield Strength (0% cold-worked)210 MPa30.5 ksi
Brinell Hardness (HB)––
Rockwell Hardness (HRB)8282
Vickers Hardness (HV)159159
Elongation at Break (In 50mm/2”)58 %58 %
Young’s Modulus193 – 200 GPa28.0 – 29.0 Msi

Heat Treatment

Heat Treatment

Heat treatment for stainless steel coil

Common heat treatment processes of SS 304 coils:

  1. Normalizing
    • Not applicable
    • Reason: 304L stainless steel is not typically normalized due to its stable austenitic structure.
  2. Annealing
    • Temperature: 1,040°C – 1,120°C (1,904°F – 2,048°F)
    • Process: Heat to the specified temperature, then cool rapidly in the air or water to ensure full annealing.
  3. Quenching
    • Not recommended
    • Reason: Quenching can lead to unnecessary stress and potential cracking in 304L stainless steel.
  4. Tempering
    • Not applicable
    • Reason: Tempering is generally unnecessary for 304L stainless steel, as heat treatment does not harden it.

Characteristics

Characteristics

  • Low carbon content reduces the risk of carbide precipitation during welding.
  • Excellent resistance to intergranular corrosion after welding.
  • Maintains good mechanical properties at both high and low temperatures.
  • Compatible with various forming and drawing processes.
  • Versatile for use in a wide range of industrial applications.
Application is made from 304l stainless steel coil.

Our Service

Our Service

1.Welding

2.Metal Fabrication

3.CNC Machining

4.Lathe

5.Forming

6.OEM/ODM

7.Quenching 

8.Tempering

UT & Hardness Testing

UT & Hardness Testing

UT And Hardness Testing Info

Surface Finish

Surface Finish

Packing

Packing

At SteelPRO Group, we understand the importance of delivering your goods in pristine condition. That’s why we prioritize robust packing solutions to prevent any damage before your shipment arrives. We offer a range of packing methods and customization options to meet your specific needs. Trust us to handle your products with the utmost care and professionalism.

  • Wooden Pallet
  • Plastic Film Wrapping
  • Steel Strapping
  • Paper Wrapping
  • Edge Protection
  • Horizontal Packing
  • Vertical Packing
  • Plastic or Metal Skids
  • Wooden Crates
  • Customized Packaging
Packing image for coil
Packing image for coil
Packing image for coil
Packing image for coil
Packing image for coil
Packing image for coil

Why Choose Us

Why Choose Us

The factory for steel coil

SteelPRO Group is a leading manufacturer and solutions provider of specialty steel. We are dedicated to delivering tailored, high-quality solutions across diverse industries. With a commitment to 100% quality assurance, we partner with our clients for mutual growth and success. Trust us to provide the expertise and reliability you need for your critical applications.

Choose us as your trusted partner, and you will get:

  • 17+ Years of Manufacturing Experience
  • 1M+ Tons Annual Capacity
  • 100% Quality Promise
  • Factory Direct Sales Price
  • Complete Specifications & Ample Storage
  • Prompt Delivery
  • Customized Solutions
Scroll to Top

Send Message

Please enable JavaScript in your browser to complete this form.
Case study Page 1
Case study Page 2
Case study Page 3
Case study Page 4
Case study Page 5
Case study Page 6
Case study Page 7
Case study Page 8
Case study Page 9
Case study Page 10
Case study Page 11
Case study Page 12
Case study Page 13