S250GD (1.0242) Galvanized Steel Coil

We offer S250GD galvanized steel coils, sheets, plates, pipes, tubes, etc., according to relevant EN standards, and can also be customized according to standards such as AISI, ASTM, GB, DIN, and JIS to meet your specific requirements.
  • Alloy or Not: Non-alloy
  • Technique: Hot Rolled, Cold Rolled
  • Thickness: 0.12-6.0 mm, or as requested
  • Width: 600-1500 mm, or as requested
  • Weight: 3-20 tons
  • Galvanization: Hot-dip Galvanizing, Electro-Galvanizing, Pre-Galvanizing
  • Processing Service: Shearing, Flattening, Cut-to-Length, Coiling, Bending, etc.
  • Certification: ISO 9001, CE
  • Inspection: SGS, TUV, Factory Inspection
  • Origin: Hubei/Henan/Jiangsu, China
  • Port: Qingdao, Tianjin, Lianyungang
  • MOQ: 5 tons (or as per negotiation)
  • Delivery Time: 8-14 Days
  • Payment: T/T, L/C

Product Detail

S250GD galvanized steel coil is a low-carbon, hot-dip galvanized steel composed of iron, carbon, manganese, silicon, and trace amounts of phosphorus and sulfur. The steel coil is coated with zinc to provide better corrosion resistance, with various coating thicknesses available and different coatings, such as standard hot-dip galvanized and aluminum-zinc alloy coatings for enhanced protection.

With a yield strength of 250 MPa, S250GD offers good strength and formability, suitable for processes such as cold rolling, hot rolling, welding, and forming. The steel undergoes rolling and annealing treatments to improve its mechanical properties and surface smoothness.

Additionally, the zinc coating is highly durable and fully recyclable, which reduces maintenance needs and resource consumption, making it an eco-friendly and sustainable choice.

S250GD is widely used in construction, automotive, and home appliance industries, particularly in environments where corrosion resistance is essential, such as roofing, exterior walls, car bodies, and appliance casings. In the automotive industry, it is used for components like body structures, chassis, and doors, offering durability and versatility in industrial manufacturing.

Contact us if you are unfamiliar with this product or have unanswered questions.

Features

S250GD galvanized steel coils could bring the following benefits to your project:

  1. Corrosion-Resistant – Stays rust-free in tough conditions.
  2. High Strength – Reliable for structural and heavy-duty uses.
  3. Cost-Effective – Durable, low-maintenance, and long-lasting.
  4. Versatile – Perfect for construction, automotive, and appliances.
  5. Easy to Form – Flexible for various designs without losing strength.
  6. Clean Finish – Looks good in both functional and decorative applications.
  7. Eco-Friendly – Fully recyclable, supporting sustainable practices.

Applications

Construction
Roofing panels, wall cladding, structural frames, steel framing systems, etc.

Automotive
Car body panels, chassis parts, seat frames, exhaust systems, etc.

Electrical
Electrical enclosures, distribution boxes, cable trays, transformer housings, etc.

Furniture
Shelving units, metal bed frames, office furniture, filing cabinets, etc.

Household Appliances
Washing machine bodies, refrigerator panels, microwave oven enclosures, air conditioner casings, etc.

Packaging
Metal cans, storage drums, protective steel packaging, shipping containers, etc.

Construction
Automotive
Electrical
Furniture
Appliances
Metal cans

Product Parameters

ParameterDetails
StandardEN 10346:2015, ISO 3575:2016, ASTM A653/A653M-22, JIS G3302:2010, GB/T 2518-2008, GB/T 14977-2002, etc.
GradeS250GD
Metal Coating TypeZ (Pure Zinc), ZF (Zinc-Iron Alloy), ZA (Zinc-Aluminum Alloy), ZM (Zinc-Magnesium Alloy), AZ (Aluminum-Zinc Alloy), AS (Aluminum-Silicon Alloy)
Thickness0.12-6.0 mm, or as requested
Width600-1500 mm, or as requested; Standard 1000 mm, 1250 mm, 1500mm
Coil ID508-610 mm
Coil Weight3-20 metric tons per coil
Tolerance±1%, or as requested
GalvanizationHot-Dip Galvanizing, Electro-Galvanizing, Pre-Galvanizing
Zinc CoatingZ30-600 g/m²
Surface StructureRegular spangle, Minimized spangle, Zero spangle, Big spangle
Surface Treatment1) Skin Pass, Sand Blasted
2) Pre-painted
3) Galvanized
4) Oiled
5) Passivated
6) PE, PVDF, or other anti-corrosive coatings
7) As requested
Condition of Delivery+HR/+CR/+A/+O/+UPK, or as requested
Testing MethodCCA/MPT/CST/SST/MA/NDT, etc.
ApplicationRoofing panels, wall cladding, structural frames, car body panels, chassis parts, electrical enclosures, shelving units, refrigerator panels, storage drums, shipping containers, etc.
CertificationApproved by ISO 9001, CE
PackagingStandard seaworthy packing, or as requested

*Condition of Delivery: HR – Hot Rolled, CR – Cold Rolled, A – Annealed, O – Oiled, UPK – Unpickled

*Testing Method: CCA – Chemical Composition Analysis, MPT – Mechanical Properties Testing, CST – Coating Surface Testing, SST – Salt Spray Testing, MA – Metallographic Analysis, NDT – Non-Destructive Testing

Material Specifications

Chemical Composition

GradeCSiMnPS
S250GD≤0.2≤0.6≤1.7≤0.1≤0.045

*According to EN 10346-2015.

Mechanical Properties

GradeTensile Strength (σb, MPa)Yield Strength (σs, MPa)Elongation (δ, %)
S250GD+Z≥330≥250A80: ≥19
S250GD+ZF
S250GD+ZA
S250GD+ZM
S250GD+AZ
S250GD+AS

*According to EN 10346-2015.

*The following minimum elongation values apply for different thicknesses:

  • 0.5mm < t ≤ 0.7mm: minimum elongation is reduced by 2% from the values in the table.
  • 0.35mm < t ≤ 0.5mm: minimum elongation is reduced by 4% from the values in the table.
  • t ≤ 0.35mm: minimum elongation is reduced by 7% from the values in the table.

 

Why Choose Us

Consistent Quality

We address your primary quality concerns with S250GD galvanized steel coils — such as coating uniformity, potential missed spots, and coating adhesion — through continuous hot-dip galvanizing processes & strict control of temperature and timing, non-destructive thickness testing with magnetic gauges, and multi-step-pre-treatment, including acid cleaning and surface preparation, to ensure consistent performance, corrosion resistance, and long-lasting durability across various environments.

Consistent Quality

Precise Dimensions

We guarantee the dimensional accuracy of our S250GD galvanized steel coils, maintaining tight tolerances within ±0.01 mm through precision equipment and ISO 9001-certified processes. Every batch undergoes 100% inspection, with zero deviation complaints in the past 5 years. We ensure smooth project execution without installation delays.

Precise Dimensions

Stable Supply

We have 3 factories with a combined annual capacity of over 500,000 tons. In the event of any unforeseen circumstances, we can coordinate across factories to ensure stable production and on-time delivery.

Stable Supply

Stable & Competitive Pricing

We maintain upstream raw material suppliers with price-lock agreements in place to effectively manage material cost fluctuations. Also, considering that our clients may face pressure from market changes, we will try our best to offer reasonable discounts to both new and existing clients.

Stable & Competitive Pricing

Secure Packaging & Shipping

Packaging can be customized according to your requirements. We provide transparent, real-time photos of the packaging and loading process for your verification. You can also choose your trusted freight forwarder for transportation to ensure the entire logistics process is secure and reliable.

Secure Packaging & Shipping

About Us

Founded in 1999, SteelPRO Group operates three factories with a combined annual production capacity of over 500,000 tons. We specialize in manufacturing a wide range of steel products, including round steel, profiles, plates, and pipes. Our portfolio encompasses low-alloy structural steel, tool steel, special steel, and more.

With strict adherence to global standards such as GB, ASTM, DIN, EN, and JIS, we ensure high-quality products, including heat-treated, machined, and prestressed steel. Our solutions are trusted by customers in diverse industries, and we proudly export to different countries across Europe, North America, and Asia.

At SteelPRO, we are dedicated to delivering tailored steel solutions and growing alongside our dear clients.

Certification

FAQ

What are your prices?

Our prices are subject to change depending on supply and market conditions. For an accurate and up-to-date quote, please contact our sales team directly.

Can you provide relevant documentation?

Yes, we can provide a wide range of documentation, including Certificates of Analysis/Conformance, Insurance, Certificates of Origin, and any other required export documents. 

What is the average lead time?

As per mass production, the lead time is 5-20 days after:

1) we have received your deposit; 2) we have received your final confirmation on your orders.

If our lead time doesn’t meet your deadlines, please contact our sales directly in advance in case of any potential issues. We will try to accommodate your needs in all cases, and we are able to do so in most cases.

Can you provide free samples?

Yes, we can provide free samples for quality evaluation. However, shipping costs are generally covered by your company.

Can I visit your factory?

Of course! You are welcome to visit our factory. Please contact us in advance to arrange a convenient time for your visit, and we will gladly organize a tour and provide any necessary information to ensure a productive visit.

Our Service

SteelPRO Group – manufacturer and solution provider for special steel, offering multi-industry application solutions and customised services, 100% quality free, accompanying customers in their growth!

Our Quality Control

  • Roundness
  • Tolerance
  • Microstructure
  • Non-Destructive Testing
  • Destructive Testing
  • Process Control

Service Integration Processing

  • Welding
  • Metal Fabrication
  • CNC Machining
  • Lathe
  • Forming

CONTACT

Please enable JavaScript in your browser to complete this form.

Related Products

Quotation

Qingdao,China

Manufacturer

Scroll to Top

Send Message

Please enable JavaScript in your browser to complete this form.
Case study Page 1
Case study Page 2
Case study Page 3
Case study Page 4
Case study Page 5
Case study Page 6
Case study Page 7
Case study Page 8
Case study Page 9
Case study Page 10
Case study Page 11
Case study Page 12
Case study Page 13