10CrMo9-10 | Alloy Pressure Vessel Steel

10CrMo9-10 | Alloy Pressure Vessel Steel

10CrMo9-10 is a chromium-molybdenum alloy steel for high-temperature pressure vessels under EN 10028-2. The name reflects 10% chromium (10), “Cr” for chromium, “Mo” for molybdenum, and “9-10” for 0.9-1.0% molybdenum. It has excellent high-temperature strength, weldability, and resistance to corrosion and creep. It’s used in power plants, petrochemical industries, and boilers. Similar grades are USA A387Gr.22, GB 12CrMo, JIS SCMV4.

Description

What is 10CrMo9-10?

10CrMo9-10 is a steel with around 10% chromium and 0.9-1.0% molybdenum, forming a solid alloy pressure vessel steel. It has high-temperature strength, weldability, and resistance to creep and corrosion. Typically hot-rolled, it’s used in power plants and petrochemical industries. It is available in different heat-treated forms, such as normalized, quenched, and tempered.

Why Choose 10CrMo9-10 Alloy Pressure Vessel Steel?

Selecting the right steel is critical in demanding environments like power plants and petrochemical industries. That’s why we recommend 10CrMo9-10—it’s designed to easily handle extreme conditions. 10CrMo9-10 provides excellent high-temperature strength, great weldability, and strong resistance to creep and corrosion. With this steel, you can reduce maintenance costs, extend equipment life, and ensure consistent reliability. What makes 10CrMo9-10 stand out is its higher molybdenum and chromium content, giving it better heat and corrosion resistance compared to 16Mo3 and 13CrMo4-5. It’s a great fit for tougher applications. For alternatives, we suggest looking at A387Gr.22, GB 12CrMo, or JIS SCMV4, which also offers strong performance in pressure vessel applications.

Product Specification

Category Details
Quality Standard EN 10028-2
Certifications ISO 9001, CE, EN 10216-2, HIC, IGC, IMPACT, EN 10204
Thickness 6-150mm
Width 900-4800mm
Length 3000-25000mm
Weight Depends on length and width
Outer diameter (OD) Pipes:10mm – 610mm, Bars: 20mm – 300mm
Inner diameter (ID) Pipes: 6mm – 600mm
Tolerances Thickness: ±0.3mm to ±0.6mm, Width: ±2mm to ±5mm, Length: ±10mm to ±20mm
Technology Hot Rolling
Processing Service Bending, Welding, Decoiling, Cutting, Punching
Shapes Pressure Vessel Steel Plate, Pressure Vessel Steel Sheet, Pipes, Profiles
MOQ (Minimum Order Quantity) 5 tons (according to the actual tonnage)
Lead Time Typically 7-20 days
Price Terms & Payment Based on customer requirements, T/T, L/C
Ports Qingdao, Lianyungang, Dalian
Export Countries Southeast Asia, Central Asia, Europe, Russia, South America, Middle East, etc.
Shipping Method Offers Sea, Air and Customized Shipping

Chemical Compositions

ElementContent (%)
Chromium, Cr2.00-2.50
Molybdenum, Mo0.90-1.10
Carbon, C0.08-0.14
Silicon, Si0.10-0.35
Manganese, Mn0.40-0.60
Phosphorus, P≤ 0.025
Sulfur, S≤ 0.010
Nitrogen, N≤ 0.012
Iron, FeBalance

Mechanical Properties

PropertyMetricImperial
Tensile Strength450-600 MPa65,000-87,000 psi
Yield Strength280-400 MPa40,000-58,000 psi
Brinell Hardness135-185 HB135-185 HB
Rockwell Hardness74-88 HRB74-88 HRB
Vickers Hardness140-190 HV140-190 HV
Elongation19-25%19-25%
Elastic Modulus190-210 GPa27.6-30.5 Mpsi

Data After Normalizing Processing

 

PropertyMetricImperial
Tensile Strength510-670 MPa74,000-97,000 psi
Yield Strength300-450 MPa44,000-65,000 psi
Brinell Hardness160-200 HB160-200 HB
Rockwell Hardness80-92 HRB80-92 HRB
Vickers Hardness160-210 HV160-210 HV
Elongation18-24%18-24%
Elastic Modulus190-210 GPa27.6-30.5 Mpsi

Industries & Applications

IndustriesProducts
Power GenerationBoilers, Heat Exchangers, Turbines, Piping Systems, Pressure Vessels
Oil and GasPipelines, Heat Exchangers, Valve Bodies, Refinery Components, Oilfield Equipment
Chemical ProcessingReactors, Distillation Towers, Pressure Vessels, Storage Tanks, Piping Systems
PetrochemicalRefinery Equipment, Heat Exchangers, Flare Systems, Columns, Pressure Vessels
ShipbuildingBoiler Components, Heat Exchangers, Marine Piping Systems, Pressure Vessels, Engine Parts
Nuclear PowerReactor Pressure Vessels, Steam Generators, Piping Systems, Heat Exchangers, Control Rods
AerospaceEngine Components, Exhaust Systems, Heat Exchangers, Pressure Vessels, High-Temperature Tubing
Industrial MachineryHydraulic Cylinders, Boiler Components, Pressure Vessels, Heat Exchangers, Industrial Furnaces
AutomotiveExhaust Systems, Turbocharger Housings, Heat Exchangers, Engine Components, Pressure Vessels

Packing

SteelPRO Group’s packing methods for 10CrMo9-10 alloy steel ensure top-level protection and efficiency. Here are four key advantages we offer:

  • Customized Packing Solutions: We adapt packaging to the specific dimensions and requirements of 10CrMo9-10, ensuring safe transport for pipes, bars, or sheets.
  • Corrosion Prevention: Materials are wrapped in moisture-resistant films and sealed with corrosion inhibitors to prevent rust during long-distance shipping.
  • Secure Bundling: Strong steel or plastic straps are used to bundle products tightly, minimizing movement during transportation and reducing the risk of damage.
  • Comprehensive Impact Protection: We use reinforced edge guards and protective layers to prevent any impact damage, ensuring the product arrives in perfect condition.

SteelPRO Group ensures that every detail of 10CrMo9-10 packing is carefully handled to protect your investment!

Machining

10CrMo9-10 Heat Treatment Product Options

At SteelPRO Group, we supply 10CrMo9-10 pressure vessel steel in the following heat-treated and processed forms:

  • Normalized 10CrMo9-10 (at 910-950°C): Enhanced strength and toughness, ideal for high-temperature and pressure applications.
  • Normalized and Tempered 10CrMo9-10 (tempered at 650-700°C): Optimized for improved ductility and resistance to brittle fracture, widely used in pressure vessels and boilers.
  • Annealed 10CrMo9-10 (at 650-700°C): For improved machinability and stress relief, suitable for moderate-pressure environments.
  • Quenched and Tempered 10CrMo9-10: Excellent mechanical strength and hardness, typically used for high-stress critical components.
  • Hot Rolled 10CrMo9-10: Non-heat-treated form with good weldability and flexibility for further processing.

We provide tailored heat treatments based on your specific project requirements.

10CrMo9-10 Surface Finish

At SteelPRO Group, we offer the following surface treatments for 10CrMo9-10 steel:

  • Shot Blasting: Removes rust, scale, and contaminants, providing a clean surface ready for coating.
  • Painting/Priming: Adds corrosion protection and improves aesthetics with a durable coating layer.
  • Galvanizing (Hot-Dip): Provides long-lasting corrosion resistance by coating the steel with a protective zinc layer.
  • Pickling: Cleans the surface from oxides and scales, improving the surface finish for further processing or coating.
  • Passivation: Enhances corrosion resistance by treating the steel surface with a protective oxide layer.

Custom surface treatment requirements can be accommodated upon request.

Disclaimer 
The above information on heat treatment options and surface finish processes for 10CrMo9-10 steel reflects the services provided by SteelPRO Group. The suitability of these services for your specific applications may vary depending on project requirements and conditions. We recommend consulting with our technical team or a metallurgical expert to ensure the right treatment and finishing are selected for optimal performance. SteelPRO Group assumes no liability for the application of this information without proper consultation.

10CrMo9-10 Pressure Vessel Steel Manufacturer

The workers are visiting factory

As a trusted supplier of 10CrMo9-10 Alloy Pressure Vessel Steel, we provide comprehensive solutions to meet your project’s needs:

1. Competitive Pricing and On-Time Delivery: We offer competitive rates while ensuring timely delivery to keep your project on schedule.

2. Full Range of Products: From pipes to plates, we supply a wide range of 10CrMo9-10 products, with advanced processing services like cutting, welding, and bending to meet precise specifications.

3. Strict Quality Assurance and Certification: Our 10CrMo9-10 steel undergoes rigorous testing, certified according to industry standards such as EN 10204 3.1/3.2, guaranteeing high quality and reliability.

4. Custom Solutions, Safe Packaging, and Efficient Logistics: We provide tailored steel solutions, secure packaging to protect materials in transit, and efficient logistics to ensure smooth and timely delivery.

SteelPRO Group stands as your authoritative partner for 10CrMo9-10 pressure vessel steel.

Our Service

SteelPRO Group – manufacturer and solution provider for special steel, offering multi-industry application solutions and customised services, 100% quality free, accompanying customers in their growth!

Our Quality Control

  • Roundness
  • Tolerance
  • Microstructure
  • Non-Destructive Testing
  • Destructive Testing
  • Process Control

Service Integration Processing

  • Welding
  • Metal Fabrication
  • CNC Machining
  • Lathe
  • Forming

What Is The Maximum Operating Temperature For 10CrMo9-10 Steel?

The maximum operating temperature for 10CrMo9-10 steel is typically around 580°C, making it suitable for high-temperature environments like boilers and pressure vessels.

Can You Supply Both Seamless And Welded 10CrMo9-10 Pipes?

Yes, we supply both seamless and welded 10CrMo9-10 pipes, depending on your project requirements and specifications.

Is 10CrMo9-10 Suitable For High-Pressure Applications?

Yes, 10CrMo9-10 is designed specifically for high-pressure applications due to its excellent strength and temperature resistance.

What Is Your Average Production Capacity Per Month?

Our production capacity varies depending on the product, but we can typically handle large-scale orders efficiently, ensuring stable and consistent supply.

Can You Provide Technical Support For Complex Project Requirements?

Yes, we offer comprehensive technical support to ensure that our products meet your project’s specific needs, including consultation on material selection and specifications.

Are There Discounts For Bulk Orders?

Yes, we offer competitive pricing and volume-based discounts for bulk orders to help optimize your procurement costs.

CONTACT

Please enable JavaScript in your browser to complete this form.

CONTACT

Please enable JavaScript in your browser to complete this form.

Certifications

Other Products

Scroll to Top

Send Message

Please enable JavaScript in your browser to complete this form.
Case study Page 1
Case study Page 2
Case study Page 3
Case study Page 4
Case study Page 5
Case study Page 6
Case study Page 7
Case study Page 8
Case study Page 9
Case study Page 10
Case study Page 11
Case study Page 12
Case study Page 13