By Shape

By Grades

Comparisons

Finish

Maintenance

S320GD (1.0250) Galvanized Steel Sheet/Plate

S320GD (1.0250) Galvanized Steel Sheet/Plate

We offer S320GD galvanized steel in sheets, plates, coils, pipes, tubes, etc., according to relevant EN standards, and can also be customized according to standards such as AISI, ASTM, GB, DIN, and JIS to meet your specific requirements.
  • Alloy or Not: Non-alloy
  • Technique: Hot Rolled, Cold Rolled
  • Size: As requested; details see product parameters
  • Galvanization: Hot-Dip, Electro, Pre
  • Condition: +HR/+CR/+A/+AR/+EG/+HDG, or as requested
  • Processing Service: Cutting, Slitting, Bending, Stamping, Punching, etc.
  • Certification: ISO 9001, CE
  • Inspection: SGS, TUV, Factory Inspection
  • Origin: Hubei/Henan/Jiangsu, China
  • Port: Qingdao, Tianjin, Lianyungang
  • MOQ: 5 tons (or as per negotiation)
  • Delivery Time: 8-14 Days
  • Payment: T/T, L/C

Product Detail

S320GD is a high-strength hot-dip galvanized low-carbon steel. The zinc coating on its surface provides added corrosion resistance and extends its lifespan. It contains elements like iron, carbon, manganese, and silicon, which give it good strength and formability.

The steel is easy to work with — it can be cut, bent, and stamped into various shapes, making it adaptable for different design and manufacturing needs. This flexibility makes it useful across a range of industries.

S320GD galvanized steel sheet/plate is commonly used in construction, automotive, and appliance sectors, especially for components exposed to harsh environments, like exterior walls, roofs, and car bodies. The zinc coating protects against moisture, acid rain, and other corrosive elements, making it ideal for areas with high humidity or fluctuating temperatures. It’s also used in light industrial machinery and outdoor equipment.

Contact us if you are unfamiliar with this product or have unanswered questions.

Features

S320GD galvanized steel sheets/plates could bring the following benefits to your project:

  1. No Rust – Keeps your steel rust-free for longer.
  2. Super Strong – Handles heavy loads and tough environments.
  3. Affordable – Great value for the price—long-lasting and cost-effective.
  4. Tough as Nails – Resists impacts and stays strong over time.
  5. Easy to Shape – Cuts, bends, and welds without hassle.
  6. Versatile – Perfect for construction, automotive, appliances, and more.
  7. Looks Good – Smooth, clean finish that looks sharp.
  8. Eco-Friendly – Coating is recyclable, supporting sustainability.

Applications

Construction
Roofing, wall cladding, structural beams, interior partitions, etc.

Automotive
Car body panels, frames, underbody parts, reinforcements, etc.

Appliances
Refrigerator panels, washing machine bodies, oven housings, air conditioner casings, etc.

HVAC
Ductwork, ventilation systems, air conditioning units, heat exchangers, etc.

Furniture
Shelving, bed frames, cabinets, office desks, etc.

Electronics
Enclosures, cabinets, chassis, mounting frames, etc.

Construction
Automotive
Appliances
Heat exchangers
Furniture
server racks

Product Parameters

ParameterDetails
StandardEN 10346, EN 10142, EN 10147, ISO 3575, JIS G 3302, ASTM A653 / A653M, ASTM A924 / A924M, DIN 17162, BS 1449, GB/T 2518, etc.
GradeS320GD
Metal Coating TypeZ (Pure Zinc), ZF (Zinc-Iron Alloy), ZA (Zinc-Aluminum Alloy), ZM (Zinc-Magnesium Alloy), AZ (Aluminum-Zinc Alloy), AS (Aluminum-Silicon Alloy)
ThicknessSheet0.5-6.0 mm, or as requested
Plate6-300 mm, or as requested
WidthSheet600-2,000 mm, or as requested
Plate900-4800 mm, or as requested
LengthSheet1,000-6,000 mm, or as requested
Plate3000-32000 mm, or as requested
Tolerance±1%, or as requested
GalvanizationHot-Dip Galvanizing, Electro-Galvanizing, Pre-Galvanizing
Zinc CoatingZ30-600 g/m²
Surface StructureRegular Spangle, Minimized Spangle, Zero Spangle, Big Spangle
Surface Treatment1) Skin Pass, Sand Blasted
2) Pre-painted
3) Galvanized
4) Oiled
5) Passivated
6) PE, SMP, PVDF, or other anti-corrosive coatings
7) As requested
Condition of Delivery+HR/+CR/+A/+AR/+EG/+HDG, or as requested
Testing MethodCCA/MPT/CST/SST/MA/NDT, etc.
ApplicationRoofing, wall cladding, structural beams, car body panels, underbody parts, refrigerator panels, washing machine bodies, ductwork, ventilation systems, shelving, cabinets, enclosures, etc.
CertificationApproved by ISO 9001, CE
PackagingStandard seaworthy packing, or as requested

*Condition of Delivery: HR – Hot Rolled, CR – Cold Rolled, A – Annealed, AR – As Rolled, EG – Electro-Galvanized, HDG – Hot-Dip Galvanized

*Testing Method: CCA – Chemical Composition Analysis, MPT – Mechanical Properties Testing, CST – Coating Surface Testing, SST – Salt Spray Testing, MA – Metallographic Analysis, NDT – Non-Destructive Testing

Material Specifications

Chemical Composition

GradeCSiMnPS
S320GD≤0.2≤0.6≤1.7≤0.1≤0.045

*According to EN 10346-2015.

Mechanical Properties

GradeTensile Strength (σb, MPa)Yield Strength (σs, MPa)Elongation (δ, %)
S320GD+Z≥390≥320A80: ≥17
S320GD+ZF
S320GD+ZA
S320GD+ZM
S320GD+AZ
S320GD+AS

*According to EN 10346-2015.

*The following minimum elongation values apply for different thicknesses:

  • 0.5mm < t ≤ 0.7mm: minimum elongation is reduced by 2% from the values in the table.
  • 0.35mm < t ≤ 0.5mm: minimum elongation is reduced by 4% from the values in the table.
  • t ≤ 0.35mm: minimum elongation is reduced by 7% from the values in the table.

Why Choose Us

Consistent Quality

We address your primary quality concerns with S320GD galvanized steel sheets/plates — such as coating uniformity, potential missed spots, and coating adhesion — through continuous hot-dip galvanizing processes & strict control of temperature and timing, non-destructive thickness testing with magnetic gauges, and multi-step-pre-treatment, including acid cleaning and surface preparation, to ensure consistent performance, corrosion resistance, and long-lasting durability across various environments.

Consistent Quality

Precise Dimensions

We guarantee the dimensional accuracy of our S320GD galvanized steel sheets/plates, maintaining tight tolerances within ±0.01 mm through precision equipment and ISO 9001-certified processes. Every batch undergoes 100% inspection, with zero deviation complaints in the past 5 years. We ensure smooth project execution without installation delays.

Precise Dimensions

Stable Supply

We have 3 factories with a combined annual capacity of over 500,000 tons. In the event of any unforeseen circumstances, we can coordinate across factories to ensure stable production and on-time delivery.

Stable Supply

Stable & Competitive Pricing

We maintain upstream raw material suppliers with price-lock agreements in place to effectively manage material cost fluctuations. Also, considering that our clients may face pressure from market changes, we will try our best to offer reasonable discounts to both new and existing clients.

Stable & Competitive Pricing

Secure Packaging & Shipping

Packaging can be customized according to your requirements. We provide transparent, real-time photos of the packaging and loading process for your verification. You can also choose your trusted freight forwarder for transportation to ensure the entire logistics process is secure and reliable.

Secure Packaging & Shipping

About Us

Founded in 1999, SteelPRO Group operates three factories with a combined annual production capacity of over 500,000 tons. We specialize in manufacturing a wide range of steel products, including round steel, profiles, plates, and pipes. Our portfolio encompasses low-alloy structural steel, tool steel, special steel, and more.

With strict adherence to global standards such as GB, ASTM, DIN, EN, and JIS, we ensure high-quality products, including heat-treated, machined, and prestressed steel. Our solutions are trusted by customers in diverse industries, and we proudly export to different countries across Europe, North America, and Asia.

At SteelPRO, we are dedicated to delivering tailored steel solutions and growing alongside our dear clients.

Certification

FAQ

What are your prices?

Our prices are subject to change depending on supply and market conditions. For an accurate and up-to-date quote, please contact our sales team directly.

Can you provide relevant documentation?

Yes, we can provide a wide range of documentation, including Certificates of Analysis/Conformance, Insurance, Certificates of Origin, and any other required export documents. 

What is the average lead time?

As per mass production, the lead time is 5-20 days after:

1) we have received your deposit; 2) we have received your final confirmation on your orders.

If our lead time doesn’t meet your deadlines, please contact our sales directly in advance in case of any potential issues. We will try to accommodate your needs in all cases, and we are able to do so in most cases.

Can you provide free samples?

Yes, we can provide free samples for quality evaluation. However, shipping costs are generally covered by your company.

Can I visit your factory?

Of course! You are welcome to visit our factory. Please contact us in advance to arrange a convenient time for your visit, and we will gladly organize a tour and provide any necessary information to ensure a productive visit.

Our Service

SteelPRO Group – manufacturer and solution provider for special steel, offering multi-industry application solutions and customised services, 100% quality free, accompanying customers in their growth!

Our Quality Control

  • Roundness
  • Tolerance
  • Microstructure
  • Non-Destructive Testing
  • Destructive Testing
  • Process Control

Service Integration Processing

  • Welding
  • Metal Fabrication
  • CNC Machining
  • Lathe
  • Forming

CONTACT

Please enable JavaScript in your browser to complete this form.

Related Products

Quotation

Qingdao,China

Manufacturer

Scroll to Top

Send Message

Please enable JavaScript in your browser to complete this form.
Case study Page 1
Case study Page 2
Case study Page 3
Case study Page 4
Case study Page 5
Case study Page 6
Case study Page 7
Case study Page 8
Case study Page 9
Case study Page 10
Case study Page 11
Case study Page 12
Case study Page 13