SGHC Galvanized Steel Sheet & Plate

SGHC Galvanized Steel Sheet & Plate

SteelPRO Group offers SGHC galvanized steel sheets with excellent corrosion resistance and durability. Our products are available in a variety of forms, including flat sheets, coils and plates, suitable for a wide range of applications in the construction, automotive and manufacturing industries. At the same time, we also have other grades and types of galvanized steel, such as Q195, SGCC, DX51D, DC01, roofing sheets, pipes, etc. We provide excellent services, from custom manufacturing to expert consultation, ensuring that our customers receive tailor-made solutions.

  • Standard: ASTM A653/A653M, EN 10346, JIS G3302, GB/T 2518
  • Grades: SGHC, S220GD, Q195, Q235, SGCC, etc.
  • Technology: Hot dip galvanizing
  • Certification: ISO, TUV, SGS, BIS, CE

SGHC Galvanized Steel Sheet & Plate

SGHC Galvanized Steel Sheet & Plate

Our SGHC galvanized steel sheets are hot-dip galvanized to provide a uniform zinc layer on the surface, providing excellent corrosion protection, making them ideal for use in construction, automotive and infrastructure. Compared to other brands, the galvanizing thickness of SGHC steel sheets is more uniform, which can effectively prevent corrosion and extend service life. In addition, our steel sheet substrate is stronger and can withstand greater loads and pressures, making it particularly suitable for applications that require higher load-bearing capacity. In terms of processing, the surface of SGHC steel sheets is smoother, reducing losses during processing and ensuring product consistency and quality. Due to its excellent corrosion resistance and high strength, the long-term durability and cost-effectiveness of SGHC steel sheets are better than most similar products on the market, reducing the frequency of maintenance and replacement, and bringing better returns on investment.
Galvanized steel sheet

Product Specifications

Product Specifications

Product Name SGHC Galvanized Steel Sheet & Plate
Thickness 0.12mm – 10.0mm, Customized
Width Regular: 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, Customized
Length 1000mm – 6000mm, Customized
Coil ID 508mm/610mm
Zinc Coating 20-400g/m², g30, g40, g60, g90, Z20-Z29, Z81-Z120, etc.
Surface Treatment Anti-finger print / Skin pass / Oiled / Dry / Chromated / Embossed / Lamination
Spangle Zero Spangle / Mini Spangle / Regular Spangle / Large Spangle
Edge Mill edge, Cut edge
Hardness Soft Hard(<60)

Medium Hard(60-85)

Full Hard(85-95)

Test Zinc Coating Thickness Test, Salt Spray Test, Adhesion Test, Tensile Test, Bend Test, etc.
Tolerance ±1%
Processing Service Bending, Welding, Decoiling, Cutting, Punching
Invoicing By actual weight
Delivery Time 7-15 days
Payment T/T, L/C, Credit Card
Port Shanghai, Qingdao or according to your requirement
Packaging Details In bundles, in bulk, customized packing

Chemical Compositions

Chemical Compositions

ElementCarbon (C)Manganese (Mn)Phosphorus (P)Sulfur (S)Silicon (Si)
Composition Range (%)≤ 0.260.30 – 0.80≤ 0.04≤ 0.050.10 – 0.60

Mechanical properties

Mechanical properties

PropertyTypical Value
Tensile Strength (MPa)270 – 440
Yield Strength (MPa)210 – 350
Elongation (%)≥ 20
Vickers Hardness (HV)80 – 180
Brinell Hardness (HB)70 – 170
Rockwell Hardness (HRB)60 – 90
Elastic Modulus (GPa)200

Industries & Applications

Industries & Applications

  • Construction: Roofing panels and systems, wall cladding and facades, structural beams and columns, steel frames for buildings.
  • Automotive Industry: Car bodies and chassis components, structural parts for enhanced durability, exterior panels to resist corrosion.
  • Manufacturing: Appliances such as refrigerators and washing machines, industrial equipment and machinery components, furniture and shelving units.
  • Infrastructure: Bridges and highway barriers, fencing and security barriers, utility poles and communication towers.
  • Agricultural Applications: Silos and storage tanks, livestock shelters and barns.
  • HVAC Systems: Ductwork and ventilation components, air conditioning units.
Galvanized steel sheet

Other Infomation

Other Infomation

Galvanized steel sheet

We can produce SGHC galvanized steel sheets in different hardness levels depending on your needs. Here is a simple classification:

Soft Hardness (<60 HRB):
This is the most flexible option and is easy to bend and form. It is ideal for applications where the steel needs to be formed into specific shapes, such as automotive parts or appliances.

Medium Hardness (60-85 HRB):
This is a good middle ground – stronger than soft steel, but still flexible enough to be used in a variety of applications. It is often used in areas such as construction and roofing where strength and machinability need to be balanced.

Galvanized steel sheet

Full Hardness (85-95 HRB):
This is the toughest option and has the highest strength. It is ideal for applications that require the steel to withstand a lot of wear and tear, such as heavy machinery or structural components. Keep in mind that it is less flexible and therefore not as easily formed.

So depending on what you are using the steel for, we can adjust the hardness to suit your needs. Just tell us what you are looking for and we will make sure you get the right choice!

Our Inventory

Our Inventory

Stainless steel plate is displayed after packaging.

At SteelPRO Group, our commitment to quality and innovation is backed by world-class production facilities that enable us to consistently meet the needs of our customers around the world. With advanced production lines, high-tech equipment and an experienced workforce, we are able to produce large quantities of high-quality galvanized steel sheets and other steel products. Our strong relationships with trusted suppliers and strategic partnerships with key players in the industry ensure that we can maintain a reliable and efficient production cycle to deliver products on time without compromising on quality.

Main products: steel pipes, steel plates, steel coils, steel bars, steel strips, stainless steel series, carbon steel series, high-strength steel series, nuclear grade steel, galvanized steel, steel for wind and solar energy, etc.

Packing

Packing

At SteelPRO Group, we prioritize safe and secure packaging to ensure your products arrive in perfect condition. Our galvanized steel sheets and other steel products are carefully packaged with high-quality materials to prevent damage during transportation. We use protective layers such as plastic wrap, wooden boxes, and metal straps to secure the product and minimize the risk of scratches, rust, or dents. We offer custom packaging options to meet specific customer requirements, ensuring safe delivery anywhere in the world.

sheet_plate -packing
sheet plate packing
sheet plate packing
sheet plate packing
sheet plate packing
sheet plate packing

Our Service

Our Service

1.Welding

2.Metal Fabrication

3.CNC Machining

4.Lathe

5.Forming

6.OEM/ODM

7.Quenching 

8.Tempering

How corrosion resistant is SGHC galvanized steel?

SGHC galvanized steel sheets have excellent corrosion resistance due to their thick, uniform zinc coating. This makes them ideal for use in harsh environments such as construction, automotive, and outdoor applications.

Is SGHC galvanized steel easy to weld and form?

Yes, SGHC galvanized steel sheets are designed to be easily processed and fabricated. The material retains its strength and the zinc coating remains intact during the welding and forming process, ensuring high-quality results.

Can SteelPRO Group provide technical support for using SGHC galvanized steel?

Of course! Our team will provide you with expert guidance and technical support to help you get the most out of SGHC galvanized steel in your project.

Does SteelPRO Group offer custom services for galvanized steel products?

Yes, we offer custom solutions for galvanized steel products, including specific sizes, thicknesses, and coatings tailored to your project requirements. Our team can work with you to meet your exact specifications.

What is SteelPRO Group's quality assurance process?

At SteelPRO Group, we follow a strict quality control process throughout our production process. Every batch of galvanized steel products is tested for thickness, corrosion resistance and strength consistency to ensure our products meet the highest industry standards.

Can SteelPRO Group offer long-term supply agreements for large projects?

Yes, SteelPRO Group offers long-term supply agreements for large and ongoing projects. We work closely with our customers to establish a reliable supply chain, ensuring continuous delivery of SGHC galvanized steel sheets over an extended period of time, and offering flexible terms based on your project needs.

CONTACT

Please enable JavaScript in your browser to complete this form.

Certificates and Cooperation

Certificates and Cooperation

Related Products

Related Products

Scroll to Top

Send Message

Please enable JavaScript in your browser to complete this form.
Case study Page 1
Case study Page 2
Case study Page 3
Case study Page 4
Case study Page 5
Case study Page 6
Case study Page 7
Case study Page 8
Case study Page 9
Case study Page 10
Case study Page 11
Case study Page 12
Case study Page 13