We are SteelPRO Group, a professional supplier of 409L stainless steel sheets, coils, plates, and pipes:
We offer x2crti12 steel sheets, 409L seamless pipes, 409L cold rolled coils and plates, and 409L rectangular pipes and so on. Our services include cold rolling, annealing, pickling, surface finishing, hot rolling, perforation, embossing, cladding, slitting, and welding. We also support custom processing options.
Standard | ASTM A240 / A240M, ASTM A268 / A268M |
---|---|
Grade | 022Cr11Ti, 1.4512, SUS409L |
Thickness | Coil: 0.3 mm (0.012 in) to 6.0 mm (0.236 in), Customized, Plate: 6.0 mm (0.236 in) to 50.0 mm (1.968 in), Sheet: 0.3 mm (0.012 in) to 6.0 mm (0.236 in) |
Full Width | Customized, Plate: 1500 mm (59.06 in) to 2000 mm (78.74 in), Sheet & Coil: 1000 mm (39.37 in) to 1500 mm (59.06 in) |
Length | Customized, Pipe: 6000 mm (236.22 in), Plate: 6000 mm (236.22 in) to 12000 mm (472.44 in), Sheet: 2000 mm (78.74 in) to 6000 mm (236.22 in) |
ID | Coil: 508 mm (20 in) to 610 mm (24 in), Customized |
OD | 6 mm (0.236 in) to 610 mm (24.02 in), Customized |
Surface Finish | 2B, BA, HL, Mirror, No. 1, No.4, Pickled, Polished |
Form | Clad Plate, Flat Plate, Flat Sheets, Perforated Sheets, Round Pipe, Seamless Pipe, Slit Coil, Standard Coil, Welded Pipe |
Terms | Specification |
---|---|
Minimum Order Quantity: | 5 Tons |
Price: | To be negotiated |
Packaging Details: |
As Requested
|
Delivery Time: | Within 7-10 Working Days |
Payment Terms: | T/T, L/C, Credit Card |
Supply Ability: | 100000 Tons per month |
Certification: | RoHS, BIS, SABS, tisi, KS, JIS, ISO9001 |
Export To: |
United Kingdom, United States, Australia, Canada, India, Philippines, New Zealand, South Africa, Malaysia, Korea, Russian Federation, United Arab Emirates, Singapore, Brazil, Indonesia, Hong Kong, Thailand, Vietnam, Saudi Arabia, Ireland, Turkey, Taiwan, Germany, Pakistan, etc.
|
Element | Carbon (C) | Manganese (Mn) | Phosphorus (P) | Sulfur (S) | Silicon (Si) | Chromium (Cr) | Nickel (Ni) | Titanium (Ti) | Nitrogen (N) |
---|---|---|---|---|---|---|---|---|---|
Sheet | ≤ 0.03% | ≤ 1.00% | ≤ 0.045% | ≤ 0.03% | ≤ 1.00% | 10.5-11.7% | ≤ 0.50% | 0.5-0.75% | ≤ 0.03% |
Coil | ≤0.03% | ≤1.00% | ≤0.040% | ≤0.020% | ≤1.00% | 10.5-11.7% | ≤0.50% | 0.75x(C+N)-0.75% | ≤ 0.03% |
Plate | ≤0.03% | ≤1.00% | ≤0.040% | ≤0.030% | ≤1.00% | 10.5-11.7% | ≤0.75% | 0.2-0.5% | ≤ 0.03% |
Pipe | ≤0.03% | ≤1.00% | ≤0.040% | ≤0.020% | ≤1.00% | 10.5-11.7% | ≤0.50% | 6xC to 0.75 | ≤ 0.03% |
Properties | Sheet Metric Units | Sheet Imperial Units | Coil Metric Units | Coil Imperial Units | Plate Metric Unit | Plate Imperial Unit | Pipe Metric Unit | Pipe Imperial Unit |
---|---|---|---|---|---|---|---|---|
Tensile Strength | 380-550 MPa | 55-80 ksi | 380-450 MPa | 55-65 ksi | 380-450 MPa | 55-65 ksi | 380-550 MPa | 55-80 ksi |
Yield Strength | 170-310 MPa | 25-45 ksi | 170-260 MPa | 25-38 ksi | 175 MPa | 25 ksi | ≥ 170 MPa | ≥ 25 ksi |
Vickers Hardness | 140-200 HV | 140-200 HV | 140-200 HV | 140-200 HV | 150 HV | 150 HV | 140-160 HV | 140-160 HV |
Brinell Hardness | 130-190 HB | 130-190 HB | 130-190 HB | 130-190 HB | 146 HB | 146 HB | 130-180 HB | 130-180 HB |
Rockwell Hardness | B75-B95 | B75-B95 | 70-90 HRB | 70-90 HRB | 75 HRB | 75 HRB | 70-85 HRB | 70-85 HRB |
Elongation | 20-40% | 20-40% | 25-35% | 25-35% | 0.2 | 0.2 | ≥ 20% | ≥ 20% |
Elastic Modulus | 190-210 GPa | 27.6-30.5 x10³ ksi | 200 GPa | 29,000 ksi | 200 GPa | 29 x 10³ ksi | 200 GPa | 29000 ksi |
1.Welding
2.Metal Fabrication
3.CNC Machining
4.Lathe
5.Forming
6.OEM/ODM
7.Quenching
8.Tempering
UT And Hardness Testing Info