409L Stainless Steel Sheet | Coil | Plate | Pipe
409L Stainless Steel Sheet | Coil | Plate | Pipe
We are SteelPRO Group, a professional supplier of 409L stainless steel sheets, coils, plates, and pipes:
We offer x2crti12 steel sheets, 409L seamless pipes, 409L cold rolled coils and plates, and 409L rectangular pipes and so on. Our services include cold rolling, annealing, pickling, surface finishing, hot rolling, perforation, embossing, cladding, slitting, and welding. We also support custom processing options.
| Standard | ASTM A240 / A240M, ASTM A268 / A268M |
|---|---|
| Grade | 022Cr11Ti, 1.4512, SUS409L |
| Thickness | Coil: 0.3 mm (0.012 in) to 6.0 mm (0.236 in), Customized, Plate: 6.0 mm (0.236 in) to 50.0 mm (1.968 in), Sheet: 0.3 mm (0.012 in) to 6.0 mm (0.236 in) |
| Full Width | Customized, Plate: 1500 mm (59.06 in) to 2000 mm (78.74 in), Sheet & Coil: 1000 mm (39.37 in) to 1500 mm (59.06 in) |
| Length | Customized, Pipe: 6000 mm (236.22 in), Plate: 6000 mm (236.22 in) to 12000 mm (472.44 in), Sheet: 2000 mm (78.74 in) to 6000 mm (236.22 in) |
| ID | Coil: 508 mm (20 in) to 610 mm (24 in), Customized |
| OD | 6 mm (0.236 in) to 610 mm (24.02 in), Customized |
| Surface Finish | 2B, BA, HL, Mirror, No. 1, No.4, Pickled, Polished |
| Form | Clad Plate, Flat Plate, Flat Sheets, Perforated Sheets, Round Pipe, Seamless Pipe, Slit Coil, Standard Coil, Welded Pipe |
409L Stainless Steel Sheet | Coil | Plate | Pipe
409L Stainless Steel Sheet | Coil | Plate | Pipe
- 409L Stainless Steel Sheet
- 409L stainless steel sheet is a flat, thin metal form. It has good corrosion resistance, weldability, and durability. It’s mainly used in automotive exhaust systems, heat exchangers, and kitchen appliances.
- 409L Stainless Steel Coil
- 409L stainless steel coil is a rolled, continuous strip of metal. It offers excellent corrosion resistance, flexibility, and easy formability. It is widely used in car parts, industrial machinery, and construction materials.
- 409L Stainless Steel Plate
- 409L stainless steel plate is a thicker, flat metal sheet. It is strong, resistant to high temperatures, and easy to weld. It is often used in structural components, pressure vessels, and large equipment.
- 409L Stainless Steel Pipe
- 409L stainless steel pipe is a hollow, cylindrical metal tube. It features high strength, corrosion resistance, and good weldability. It’s commonly used in automotive exhaust systems, chemical processing, and fluid transport.
Business Term
Business Term
| Terms | Specification |
|---|---|
| Minimum Order Quantity: | 5 Tons |
| Price: | To be negotiated |
| Packaging Details: |
As Requested
|
| Delivery Time: | Within 7-10 Working Days |
| Payment Terms: | T/T, L/C, Credit Card |
| Supply Ability: | 100000 Tons per month |
| Certification: | RoHS, BIS, SABS, tisi, KS, JIS, ISO9001 |
| Export To: |
United Kingdom, United States, Australia, Canada, India, Philippines, New Zealand, South Africa, Malaysia, Korea, Russian Federation, United Arab Emirates, Singapore, Brazil, Indonesia, Hong Kong, Thailand, Vietnam, Saudi Arabia, Ireland, Turkey, Taiwan, Germany, Pakistan, etc.
|
Chemical Compositions
Chemical Compositions
| Element | Carbon (C) | Manganese (Mn) | Phosphorus (P) | Sulfur (S) | Silicon (Si) | Chromium (Cr) | Nickel (Ni) | Titanium (Ti) | Nitrogen (N) |
|---|---|---|---|---|---|---|---|---|---|
| Sheet | ≤ 0.03% | ≤ 1.00% | ≤ 0.045% | ≤ 0.03% | ≤ 1.00% | 10.5-11.7% | ≤ 0.50% | 0.5-0.75% | ≤ 0.03% |
| Coil | ≤0.03% | ≤1.00% | ≤0.040% | ≤0.020% | ≤1.00% | 10.5-11.7% | ≤0.50% | 0.75x(C+N)-0.75% | ≤ 0.03% |
| Plate | ≤0.03% | ≤1.00% | ≤0.040% | ≤0.030% | ≤1.00% | 10.5-11.7% | ≤0.75% | 0.2-0.5% | ≤ 0.03% |
| Pipe | ≤0.03% | ≤1.00% | ≤0.040% | ≤0.020% | ≤1.00% | 10.5-11.7% | ≤0.50% | 6xC to 0.75 | ≤ 0.03% |
Mechanical Properties
Mechanical Properties
| Properties | Sheet Metric Units | Sheet Imperial Units | Coil Metric Units | Coil Imperial Units | Plate Metric Unit | Plate Imperial Unit | Pipe Metric Unit | Pipe Imperial Unit |
|---|---|---|---|---|---|---|---|---|
| Tensile Strength | 380-550 MPa | 55-80 ksi | 380-450 MPa | 55-65 ksi | 380-450 MPa | 55-65 ksi | 380-550 MPa | 55-80 ksi |
| Yield Strength | 170-310 MPa | 25-45 ksi | 170-260 MPa | 25-38 ksi | 175 MPa | 25 ksi | ≥ 170 MPa | ≥ 25 ksi |
| Vickers Hardness | 140-200 HV | 140-200 HV | 140-200 HV | 140-200 HV | 150 HV | 150 HV | 140-160 HV | 140-160 HV |
| Brinell Hardness | 130-190 HB | 130-190 HB | 130-190 HB | 130-190 HB | 146 HB | 146 HB | 130-180 HB | 130-180 HB |
| Rockwell Hardness | B75-B95 | B75-B95 | 70-90 HRB | 70-90 HRB | 75 HRB | 75 HRB | 70-85 HRB | 70-85 HRB |
| Elongation | 20-40% | 20-40% | 25-35% | 25-35% | 0.2 | 0.2 | ≥ 20% | ≥ 20% |
| Elastic Modulus | 190-210 GPa | 27.6-30.5 x10³ ksi | 200 GPa | 29,000 ksi | 200 GPa | 29 x 10³ ksi | 200 GPa | 29000 ksi |
Heat Treatment
Heat Treatment
- Annealing
- Temperature:
- Sheet: 790-900°C
- Coil: 750-850°C
- Plate: 790-900°C
- Pipe: 700-800°C
- Process:
- Sheet: Heat the sheet, then cool slowly to relieve stress and improve ductility.
- Coil: Heat to temperature, hold, and cool slowly in air or furnace.
- Plate: Heat and hold, then air cool or water quench.
- Pipe: Heat to temperature, then cool in air.
- Temperature:
- Stress Relieving
- Temperature:
- Sheet: 200-300°C
- Coil: 200-300°C
- Plate: 200-400°C
- Pipe: 400-450°C
- Process:
- Sheet: Heat the sheet, hold for a short time, then air cool to reduce residual stresses.
- Coil: Heat to temperature, hold for 1-2 hours, then air cool.
- Plate: Heat and hold for 1-2 hours, then air cool.
- Pipe: Heat to temperature, hold for a short time, then air cool.
- Temperature:
- Solution Treatment
- Temperature:
- Sheet: Less common
- Coil: 950-1000°C
- Plate: Less common
- Pipe: 950-1050°C
- Process:
- Sheet: Less common
- Coil: Heat to temperature, hold, then quench in water.
- Plate: Less common
- Pipe: Heat to temperature, then water quench.
- Temperature:
Characteristic
Characteristic
- 409L Stainless Steel Sheet:
- Corrosion Resistance: Resists corrosion, especially in automotive environments.
- Weldability: Easily welded without the risk of intergranular corrosion.
- Formability: Good formability for various shapes and sizes.
- 409L Stainless Steel Coil:
- Flexibility: Easily rolled and cut to specific dimensions.
- Surface Finish: Available in multiple surface finishes like 2B, BA, and No.4.
- Strength: Maintains good mechanical strength at high temperatures.
- 409L Stainless Steel Plate:
- Durability: High strength and durability, even under heavy loads.
- Heat Resistance: Performs well at elevated temperatures.
- Thickness Variety: Available in a wide range of thicknesses for different applications.
- 409L Stainless Steel Pipe:
- Corrosion Resistance: Excellent resistance to oxidation and corrosive environments.
- High Strength: Strong and durable, suitable for high-pressure applications.
- Weldability: Easily weldable, maintaining structural integrity.
Our Service
Our Service
1.Welding
2.Metal Fabrication
3.CNC Machining
4.Lathe
5.Forming
6.OEM/ODM
7.Quenching
8.Tempering
UT And Hardness Testing
UT And Hardness Testing
UT And Hardness Testing Info
Surface Finish
Surface Finish
2B Surface
2D Surface
BA Surface
6K Surface
8K Surface
HL Surface
NO.1 Surface
NO.4 Surface
Embossed Surface
Packing
Packing
- 409L Stainless Steel Sheet:
We use waterproof paper and sturdy pallets to protect 409L sheets from moisture and damage. Careful handling prevents surface scratches, ensuring perfect delivery. - 409L Stainless Steel Coil:
Coils are wrapped in anti-rust paper and secured on pallets with straps. This prevents oxidation and rolling and ensures the coils arrive intact. - 409L Stainless Steel Plate:
Plastic film and wooden pallets are used for packing 409L plates. Larger plates are framed to prevent deformation, ensuring safe and undamaged delivery. - 409L Stainless Steel Pipe:
Pipe ends are capped and bundled on pallets or frames to prevent rolling and damage. This packing ensures pipes arrive in excellent condition.
Why Choose Us
Why Choose Us
-
Ample Stock: Large inventory with custom services. Includes special sizes, surface finishes, and processing services.
-
Global Coverage: A global supply chain and service network to meet the needs of international customers.
-
Quick Response: Fast response within 24 hours for quotations, and professional technical support and after-sales service. Lifetime warranty.
-
Compliance and Certification: Products meet ASTM standards, with SGS or TUV certificates. Each package is labeled for easy identification.
-
Diverse Shipping Options: Choose from FOB, CFR, and CIF shipping methods. Select the best terms to optimize costs and ensure safety.