Contents
Low Alloy Steel Overview: Properties, Uses, Grades
- John
Alloy steels are a diverse group of metals tailored to exhibit enhanced properties by adding specific alloying elements. Low alloy steel is especially recognized for its outstanding workability, suitable for precision components used in demanding industrial applications.
In this article, SteelPro Group will help you understand the material and its applications, providing insights into how low-alloy steel is used to efficiently and cost-effectively meet the demands of various industries.
What Is Low Alloy Steel?
Low alloy steel is characterized by its modest content of alloying elements, generally not exceeding 5% of its total composition. These elements commonly include chromium, nickel, molybdenum, and sometimes vanadium. Compared to ordinary carbon steel, low alloy steel offers enhanced mechanical properties and durability, while maintaining a lower cost and better weldability. The low percentage of alloying elements contributes to the steel’s high strength-to-weight ratio, making it highly effective in applications requiring durability without excessive bulk.
What is HSLA Steel?
High Strength Low Alloy (HSLA) steel is a subgroup of low alloy steel valued for its superior strength and durability. This type of steel retains the advantages of low alloy steel—such as good machinability and competitive cost—but with an even greater strength-to-weight ratio and better resistance to atmospheric corrosion. This makes HSLA steel ideal for structural and engineering applications
Low Alloy Steel Key Features
Increased Strength
Low alloy steel is engineered to achieve higher strength than plain carbon steel due to the strategic addition of alloying elements such as chromium, molybdenum, and nickel. These elements enhance the steel’s structure at a molecular level, allowing it to endure greater stresses and loads without a significant increase in cost.
Enhanced Toughness
This steel category is noted for its toughness, which enables it to absorb energy and withstand impacts that would otherwise cause more brittle materials to fail. This characteristic is essential for applications in environments that demand durability under dynamic loads, such as in construction and industrial machinery.
Improved Corrosion Resistance
Although low in alloy content, specific elements like chromium and nickel in low alloy steel improve its resistance to corrosion beyond that of ordinary carbon steel.
Good Weldability
Despite the enhancements in strength and toughness, low alloy steel maintains good weldability. This property is crucial for manufacturing and construction sectors, where welding is a common method of joining materials. The ability to weld without losing strength at the joints makes low alloy steel ideal for the fabrication of large structures.
Cost Efficiency
Low alloy steel provides a cost-effective alternative to both standard carbon steel and higher alloyed steel. It offers a balance between cost and performance by delivering improved mechanical properties without the expense of high alloy percentages. This balance makes it a preferred material for many industrial applications where both strength and budget are key considerations.
Low Alloy Steel Grades
Low alloy steels come in multiple grades, each designed for particular uses and conditions. Here we discuss some of the most widely used grades, including 4130, 4140, 4340, and 8620, highlighting their unique properties and common uses.
4130 Steel
AISI 4130 steel is a chromium-molybdenum alloy steel recognized for its durability, excellent weldability, and resilience, even in cold conditions. It is frequently employed in the aerospace and automotive industries for parts like aircraft engine mounts and racing car chassis. The steel offers a great combination of strength and flexibility, making it a favored option for professional-grade bicycles and firearms as well.
4140 Steel
AISI 4140 steel, also chromium-molybdenum steel, is known for its superior toughness, high tensile strength, and good abrasion resistance. 4140 is commonly used in gears, axles, shafts, and fasteners manufacturing. It delivers a superb balance of durability against fatigue and resistance to abrasion.
4340 Steel
AISI 4340 steel is a nickel-chromium-molybdenum alloy steel prized for its exceptional strength, durability, and ability to withstand wear and fatigue. It’s particularly used in the aerospace industry for components like landing gear due to its ability to withstand heavy stresses. Furthermore, it is utilized in components such as gears, crankshafts, and other heavily loaded parts within the automotive and heavy equipment industries.
8620 Steel
AISI 8620 is a low-carbon nickel-chromium-molybdenum alloy steel, known primarily for its core strength and toughness. It is often used in the case-hardening process where it provides a tough core with a hard outer shell. This steel is commonly utilized in gear manufacturing, particularly automotive gears and other high-strength applications where toughness and impact resistance are required.
SteelPro Group offers 4130, 4140, 4340, and 8620 steel in form of plate, bar, and tube among others. Discover the strength and versatility of our alloys, perfectly suited for your most demanding engineering needs.
Low Alloy Steel Chemical Composition
| Element | 4130 Steel | 4140 Steel | 4340 Steel | 8620 Steel |
| Carbon (C) | 0.28-0.33% | 0.38-0.43% | 0.38-0.43% | 0.18-0.23% |
| Manganese (Mn) | 0.40-0.60% | 0.75-1.00% | 0.60-0.80% | 0.70-0.90% |
| Silicon (Si) | 0.15-0.35% | 0.15-0.35% | 0.15-0.35% | 0.15-0.35% |
| Chromium (Cr) | 0.80-1.10% | 0.80-1.10% | 0.70-0.90% | 0.40-0.60% |
| Molybdenum (Mo) | 0.15-0.25% | 0.15-0.25% | 0.20-0.30% | 0.15-0.25% |
| Nickel (Ni) | ≤0.25% | ≤0.25% | 1.65-2.00% | 0.40-0.70% |
Low Alloy Steel Mechanical Properties
| Grades | Tensile Strength (MPa) | Yield Strength (MPa) | Elongation (%) | Hardness (BHN) |
| 4130 Steel | 670 – 900 | 435 – 635 | 20 – 25 | 217 – 235 |
| 4140 Steel | 655 – 880 | 415 – 655 | 15 – 25 | 197 – 220 |
| 4340 Steel | 745 – 925 | 470 – 720 | 20 – 22 | 217 – 235 |
| 8620 Steel | 530 – 720 | 385 – 535 | 20 – 30 | 149 – 167 |
Low Alloy Steel Applications
Here’s a detailed table showcasing the applications of low alloy steel across various industries.
| Industry | Application | Grades |
| Automotive | Gears, axles, shafts | 4130, 4140 |
| Aerospace | Aircraft parts such as landing gear, frames | 4340, 300M |
| Construction and Infrastructure | Bridges, buildings, pipelines | 8620, 4130 |
| Energy Sector | Power generation equipment like boilers and turbines | A514, 4140 |
| Heavy Machinery and Equipment | Cranes, bulldozers, excavators | 4140, 4340 |
| Military and Defense | Vehicles, defense equipment | 46100, 4140 |
| Sporting Goods | Bicycle frames, golf club shafts, gym equipment | 4130, 4140 |
Discover High-Performance Low Alloy Steel with SteelPro Group
SteelPro Group offers a robust selection of low alloy steel grades including 4130, 4140, 4340, and 8620, available in plate, bar, and tube formats to meet your project specifications. We specialize in providing customized services and products tailored to your unique needs, from precise cutting and fabrication to specialized chemical compositions.
Our technical expertise allows us to support your projects with detailed performance data and engineered solutions. Contact us at SteelPro Group to discuss your needs. Our team is ready to assist you and meet your exact requirements.