Contents
DX53D Galvanized Steel Sheet | 1.0951 | 1.0355
- John
If you need strong, rust-resistant, and easy-to-shape steel, DX53D galvanized steel is a great choice. It is designed for deep drawing and complex forming, making it ideal for car parts, home appliances, and construction materials.
At SteelPro Group, we supply DX53D galvanized steel sheets and coils with customizable solutions. Whether you’re making automotive panels, building materials, or precision parts, our high-quality steel ensures durability, reliability, and cost efficiency.
What Is DX53D Hot-dip Galvanized Steel?
DX53D galvanized steel is low-carbon steel coated with a layer of zinc through a hot-dip galvanizing process. This coating enhances its corrosion resistance, making it ideal for applications that require high formability and durability. Unlike standard galvanized steel, DX53D is specially designed for deep drawing, meaning it can be stretched and shaped into complex forms without cracking or losing strength.
What Does the DX53D Name Mean?
- D – Indicates it is designed for deep-drawing applications
- X – Indicates the steel is not specified for a particular strength level, allowing for high ductility.
- 53 – Represents the deep drawing grade, which is more formable than DX51D and DX52D.
- D – Means the steel is hot-dip galvanized.
DX53D Steel Equivalent Grades
Under the EN 10346:2009 standard, DX53D corresponds to steel grade 1.0355. In the EN 10346:2015 standard, its equivalent designation is 1.0952.
DX53D Galvanized Steel Applications
- Automotive Industry: Car body panels, inner structural parts, reinforcement components, fuel tanks, chassis components, battery casings, and decorative trims.
- Household Appliances: Washing machine drums, refrigerator panels, oven enclosures, air conditioner casings, dishwasher interiors, and microwave oven structures.
- Construction and Roofing: Metal cladding, roofing sheets, wall panels, structural profiles, rainwater drainage systems, garage doors, and insulation-backed panels.
- Electrical and Industrial Equipment: Electrical enclosures, control cabinets, transformer casings, air ventilation ducts, industrial storage units, and safety barriers.
- Furniture and Decorative Applications: Storage cabinets, office furniture frames, shelving systems, modular partitions, architectural facades, and decorative panels.
DX53D Material Properties
- Exceptional Formability – DX53D is specifically engineered for deep drawing without cracking or material failure, making it suitable for intricate shapes and stamped components.
- Superior Corrosion Resistance – The hot-dip galvanized zinc coating protects against rust, oxidation, and environmental exposure, significantly extending the material’s lifespan.
- Smooth Surface Quality – Available in NA, MA, MB, and MC surface finishes, DX53D ensures aesthetic appeal and consistent coating adhesion, making it ideal for painted or coated applications.
- Good Weldability – Compatible with various resistance welding, arc welding, and laser welding techniques, ensuring easy integration into assembly lines.
- High Ductility – The low-carbon steel base provides excellent flexibility and bendability, allowing it to be shaped into complex geometries without losing mechanical integrity.
DX53D Galvanized Steel Coil Chemical Composition
| Element | Maximum Content (%) |
| Carbon (C) | 0.12 |
| Silicon (Si) | 0.5 |
| Manganese (Mn) | 0.6 |
| Phosphorus (P) | 0.1 |
| Sulfur (S) | 0.045 |
| Titanium (Ti) | 0.3 |
DX53D Galvanized Steel Coil Mecahmical Properties
| Property | Value |
| Tensile Strength (Rm) | 270 – 380 MPa |
| Yield Strength (Re) / (Rp0.2) | 140 – 260 MPa |
| Minimum Elongation (A80) | ≥ 30% |
For thinner DX53D galvanized steel sheets, the minimum elongation values decrease as the thickness reduces. The adjustments are as follows:
- 0.5mm < t ≤ 0.7mm → Min elongation is 2% lower than the table value.
- 0.35mm < t ≤ 0.5mm → Min elongation is 4% lower than the table value.
- t ≤ 0.35mm → Min elongation is 7% lower than the table value.
DX53D Galvanized Steel Products Specifications
At SteelPro Group, we offer DX53D galvanized steel in multiple formats to suit various manufacturing needs:
- DX53D Galvanized Steel Coils – For large-scale industrial applications and further processing.
- DX53D Galvanized Steel Sheets – Cut to standard or custom dimensions.
- DX53D Galvanized Steel Strips – For precision applications requiring narrow widths.
Below are the product specifications for each form:
DX53D Galvanized Steel Coils
| Specification | Metric (mm) | Imperial (inch) |
| Thickness | 0.3 – 3.0 mm | 0.012 – 0.118 in |
| Width | 600 – 1500 mm | 23.62 – 59.06 in |
DX53D Galvanized Steel Sheets
| Specification | Metric (mm) | Imperial (inch) |
| Thickness | 0.3 – 3.0 mm | 0.012 – 0.118 in |
| Width | 600 – 1500 mm | 23.62 – 59.06 in |
| Length | 1000 – 6000 mm | 39.37 – 236.22 in |
DX53D Galvanized Steel Strips
| Specification | Metric (mm) | Imperial (inch) |
| Thickness | 0.3 – 3.0 mm | 0.012 – 0.118 in |
| Width | 20 – 600 mm | 0.79 – 23.62 in |
Coating Types
DX53D galvanized steel supports various coating types to enhance corrosion resistance:
- Z (Galvanized Coating) – Pure zinc coating for excellent corrosion protection.
- ZF (Galvannealed Coating) – Zinc-iron alloy coating for improved paint adhesion.
- ZA (Zinc-Aluminum Coating) – Aluminum addition enhances durability and heat resistance.
Available coating weights range from Z100 to Z275, depending on the application’s environmental exposure requirements.
Surface Treatment
To meet different processing and end-use requirements, we provide various surface treatments:
- Chromate Treatment (Cr3+ or Cr6+) – Enhances corrosion resistance.
- Oiled – Prevents white rust during storage and transportation.
- Dry (Unoiled & Unpassivated) – Suitable for further processing such as painting or welding.
Surface Quality
Our DX53D galvanized steel is available in different surface quality grades to meet aesthetic and performance needs:
- NA – Standard surface with minimal imperfections.
- MA – Improved surface quality for visible applications.
- MB – High surface finish, suitable for coating and painting.
- MC – Premium surface for the most demanding applications requiring top-tier uniformity.
With a variety of coatings, surface treatments, and quality grades, SteelPro Group ensures that DX53D galvanized steel meets the highest industry standards for durability, formability, and corrosion resistance.
DX53D Steel Sheet, Coil & Strip Customizable Supply
At SteelPro Group, we supply DX53D galvanized steel in coils, sheets, and strips, tailored to meet diverse industrial needs. With precise manufacturing, strict quality control, and advanced coatings, our products ensure exceptional formability, corrosion resistance, and durability across multiple industries.
We also offer DX54D galvanized steel pipe, which provides even higher formability for more demanding deep-drawing applications. Contact us today to discuss your DX53D or DX54D galvanized steel requirements and receive a customized quote.