Contents
S220GD Galvanized Steel Coil | 1.0242
- John
S220GD galvanized steel coil is a high-quality steel product coated with zinc through a hot-dip galvanizing process. It not only resists corrosion and weathering but is also versatile. SteelPro Group’s hot-rolled and cold-rolled S220GD offers strong structural performance in environments where traditional steel might fail. It delivers dependability and enduring performance in applications ranging from roofing products to vehicle components.
S220GD Galvanized Steel Description
S220GD is a metal-coated structural steel designed to balance strength, formability, and corrosion resistance. It is a low-carbon steel substrate processed through continuous hot-dip galvanization. The “S220GD” designation indicates a minimum yield strength of 220 MPa. This steel offers excellent formability and superior surface quality, making it ideal for applications such as roofing sheets, wall cladding, and ventilation ducts.
SteelPro Group supplies S220GD primarily as coils and sheets, providing various coating options including S220GD+Z, S220GD+ZF, S220GD+ZA, and S220GD+AZ.
S220GD Galvanized Steel Equivalent Grades
Under EN10346:2015, the equivalent grade for S220GD is 1.0241.
Additional Equivalent Materials (for reference only):
- G3302: JIS SGCC
- ASTM A653: CS Type B
- BS EN 10327: DX51D
- ISO 3575: SGHC
S220GD Galvanized Steel Properties
- High Strength: With a minimum yield strength of 220 MPa, S220GD provides reliable structural integrity.
- Excellent Corrosion Resistance: The zinc layer offers a strong defense against oxidation and environmental deterioration, increasing the product’s lifespan.
- Superior Surface Quality: S220GD features an enhanced surface finish. It offers a consistent, smooth surface that supports efficient downstream processing and coating.
- Good Formability: The low-carbon composition and consistent coating allow for easy shaping, bending, welding, and profiling.
- Good Weldability: S220GD supports a variety of welding methods. Its galvanized coating is designed to maintain good adhesion and integrity even after welding.
S220GD Galvanized Steel Coil Chemical Composition
| Element | Composition (%) |
| Carbon (C) | ≤ 0.2 |
| Silicon (Si) | ≤ 0.6 |
| Manganese (Mn) | ≤ 1.7 |
| Phosphorus (P) | ≤ 0.1 |
| Sulfur (S) | ≤ 0.045 |
S220GD Galvanized Steel Coil Mecahmical Properties
| Property | Value |
| Tensile strength (Rm) | 300 MPa |
| Proof strength (Rp0.2, 0.2%) | 220 MPa |
| Minimum elongation (Lo = 80 mm) | 20% |
| ①Minimum elongation varies with thickness:0.5mm < t ≤ 0.7mm: reduce elongation by 2%0.35mm < t ≤ 0.5mm: reduce elongation by 4%t ≤ 0.35mm: reduce elongation by 7%②S220GD tensile strength can reach up to 140 MPa. | |
S220GD Galvanized Steel Applications
- Building and Construction: Roofing sheets, wall cladding, structural panels, siding, and light framing components.
- Automotive Industry: Exterior body panels, inner reinforcements, undercarriage parts, and structural beams.
- HVAC Systems and Ductwork: Ventilation ducts, air conditioning units, exhaust systems, and heating panels.
- Consumer Appliances: Washing machine drums, refrigerator doors, oven liners, and microwave casings.
- Industrial Equipment: Storage tanks, light industrial frameworks, agricultural machinery parts, and container panels.
S220GD Galvanized Steel Products Specifications
SteelPro Group offers a comprehensive range of S220GD galvanized steel products, including coils, sheets, tubes, pipes, and strips. Our advanced production lines are equipped with state-of-the-art processing machinery, enabling us to provide precision-cut dimensions, custom surface finishes, and tailored fabrication services to meet specific customer requirements.
| Specification | Description | ||
| Product Form | Coils, strips | ||
| Product Dimensions | Width | Coils: 600–1250 mm (23.6–49.2 in) Strips: 20–600 mm (0.8–23.6 in) | |
| Thickness | Coils: 0.35–2.0 mm (0.014–0.079 in) Strips: 0.35–2.0 mm (0.014–0.079 in) | ||
| Coating Type | Z、ZF、ZA 、AZ | ||
| Coating Thickness | Z60–Z275 | ||
| Surface Finish | NA, MA, MB, MC | ||
S220GD Steel Coil & Strip Surface Finish
S220GD galvanized steel is available in various surface qualities to meet diverse application needs. The classifications include:
NA (Normal Surface Finish)
This surface finish provides consistent zinc coverage. It is typically used for interior construction components and structural elements where surface appearance is not a priority.
MA (Medium Surface Finish)
This surface finish offers a smoother texture than NA. It is commonly used for exterior panels and cladding that require a balance of appearance and durability.
MB (High-Quality Surface Finish)
This surface finish delivers a more refined texture. It is ideal for automotive body panels and appliances that need a clean, uniform appearance before painting or coating.
MC (Critical Surface Finish)
This surface finish achieves exceptional smoothness and uniformity. It is often used for visible architectural elements where aesthetics are of paramount importance, particularly in coated steel applications.
Premium S220GD Galvanized Steel Supplier
SteelPro Group takes pride in delivering S220GD galvanized steel that meets the highest quality standards. Using state-of-the-art manufacturing processes, we deliver accurate construction and dependable quality in every item. Our ability to customize materials and provide timely deliveries means we can adapt to a wide range of project requirements.
With a strong emphasis on quality and flexibility, SteelPro Group’s S220GD steel is designed to help you achieve exceptional results in all your applications.