S280GD Galvanized Steel Coil | 1.0244
- John
Galvanized steel is an essential material in contemporary building and production, recognized for its excellent resistance to corrosion. S280GD galvanized steel, in particular, stands out as a versatile material, offering a balance of strength and durability.
At SteelPro Group, we provide high-quality S280GD galvanized steel coils and sheets to meet the demanding requirements of construction frameworks, automotive components, and household appliances. This article will introduce you to the characteristics, applications, and technical specifications of S280GD, so you can make informed decisions about your next project.
S280GD Hot-dip Galvanized Steel Description
S280GD is a strong, low-alloy structural steel that’s widely used in construction and manufacturing. With a minimum yield strength of 280 MPa, it’s tough enough for demanding structural tasks. The hot-dip zinc coating provides superior protection against corrosion, guaranteeing extended durability. Thanks to this blend of strength and protection, the S280GD is perfect for structural frames, roofing systems, and other heavy-duty applications.
The name S280GD is derived from European standard EN 10346 and stands for:
- S: Structural grade steel.
- 280: Minimum yield strength of 280 MPa.
- GD: Suitable for continuous hot-dip galvanization.
SteelPro Group offers S280GD galvanized steel in various forms, including coils, sheets, and strips. Each product supports a range of metal coatings such as Z275, Z100, and AZ150, meeting rigorous quality standards.
S280GD Steel Equivalent Grades
Under EN10346:2015, the equivalent grade for S280GD is 1.0244.
Additional Equivalent Materials (for reference only):
- EN 10346: 1.0244
- DIN 17162: StE280-3Z
- ASTM A653: Grade 40 (structural)
- JIS G3302: SGCC (structural use)
S280GD Steel Applications
- Construction: Structural frameworks, roofing systems, wall panels, steel decking, and facade elements.
- Automotive: Underbody components, reinforcements, brackets, door panels, and exhaust system parts.
- Appliances: Washing machine drums, dryer housings, refrigerator panels, HVAC enclosures, and water heater tanks.
- Agricultural Equipment: Silos, storage bins, farming machinery components, and greenhouse structures.
S280GD Steel Properties
High Corrosion Resistance:
The hot-dip galvanizing process creates a durable zinc coating that effectively prevents rust, ensuring the steel can withstand prolonged exposure to humidity and wet conditions.
Enhanced Structural Stability:
S280GD maintains its mechanical performance under both static and dynamic loads, making it reliable for load-bearing frameworks and dynamic structures like bridges and cranes.
Excellent Formability:
This steel grade can be easily shaped into complex components such as roofing profiles, wall cladding, and structural panels without cracking or losing surface quality.
Strong Coating Adhesion:
The zinc coating is tightly bonded to the steel surface, ensuring long-term corrosion protection even after cutting, bending, or forming.
Outstanding Weather Resistance:
S280GD resists environmental wear in harsh climates, including prolonged exposure to rain, snow, and temperature fluctuations, ensuring a consistent performance over time.
High Heat Reflectivity and Insulation Capability:
Its surface can reflect a significant amount of radiant heat, helping to maintain stable interior temperatures in structures and making it an effective material for energy-efficient roofing or insulation.
S280GD Galvanized Steel Coil Chemical Composition
| Element | Content (weight%) |
| Carbon (C) | ≤ 0.20 |
| Manganese (Mn) | ≤ 1.70 |
| Phosphorus (P) | ≤ 0.10 |
| Sulfur (S) | ≤ 0.045 |
| Silicon (Si) | ≤ 0.60 |
S280GD Galvanized Steel Coil Mecahmical Properties
| Property | Value | |
| Tensile Strength (Rm) | 360 MPa | |
| 0.2% Proof Strength (Rp0.2) | 280 MPa | |
| Min. Elongation (A, Lo = 80 mm) | – | 18% |
| 0.5mm < t ≤ 0.7mm | 16% | |
| 0.35mm < t ≤ 0.5mm | 14% | |
| t ≤ 0.35mm | 11% | |
| Bending Center Diameter (mm) | 1a | |
| S280GD tensile strength can range up to 140 MPa, depending on the specific material grade and processing conditions. | ||
S280GD Galvanized Steel Applications
- Building and Construction: Roofing sheets, wall cladding, structural panels, siding, and light framing components.
- Automotive Industry: Exterior body panels, inner reinforcements, undercarriage parts, and structural beams.
- HVAC Systems and Ductwork: Ventilation ducts, air conditioning units, exhaust systems, and heating panels.
- Consumer Appliances: Washing machine drums, refrigerator doors, oven liners, and microwave casings.
- Industrial Equipment: Storage tanks, light industrial frameworks, agricultural machinery parts, and container panels.
S280GD Galvanized Steel Products Specifications
S280GD galvanized steel is available in three primary forms at SteelPro Group: coils, sheets, and strips. Each product form is designed to meet specific industry needs, offering various sizes and thicknesses suitable for a wide range of applications.
| Product | Thickness Range | Width Range | Length Range |
| S280GD Steel Coil | 0.30 mm to 3.00 mm (0.012″ to 0.118″) | 600 mm to 1500 mm (23.62″ to 59.06″) | Custom lengths available |
| S280GD Steel Sheet | 0.30 mm to 3.00 mm (0.012″ to 0.118″) | 600 mm to 1500 mm (23.62″ to 59.06″) | |
| S280GD Steel Strip | 0.30 mm to 2.50 mm (0.012″ to 0.098″) | 30 mm to 500 mm (1.18″ to 19.69″) |
S280GD Steel Coating Types and Functions
At SteelPro Group, we offer a range of S280GD galvanized steel products with different coating types. The coating weight typically ranges from Z60 to Z275 g/m², and we can provide specific thicknesses based on your needs.
| Coating Type | Properties | Applications |
| S280GD+Z (Zinc Coating) | Provides basic corrosion protection. | General outdoor use, light industrial applications. |
| S280GD+ZF (Zinc-iron Alloy Coating) | Enhanced wear resistance and corrosion protection. | Automotive, industrial settings. |
| S280GD+ZA (Zinc-aluminum Alloy Coating) | Better high-temperature resistance and durability. | Roofing, machinery, high-heat environments. |
| S280GD+ZM (Zinc-magnesium Coating) | Superior corrosion resistance in aggressive environments. | Marine structures, coastal areas, chemicals. |
| S280GD+AZ (Zinc-aluminum-magnesium Coating) | Maximum protection in harsh environments. | Automotive, construction, extreme weather. |
| S280GD+AS (Zinc-silver Alloy Coating) | Improved aesthetics and corrosion resistance. | Consumer goods, appliances, decorative elements. |
In addition to our wide range of coatings, SteelPro Group also offers various surface treatments including passivation, oil coating, chromate coating, and phosphate coating.
S280GD Steel Coil | Strip | Sheet Manufacturer
SteelPro Group is your trusted partner for top-quality galvanized steel, including S280GD, S250GD, and S320GD. With our advanced coatings and surface treatments, we ensure that our products offer unmatched durability and performance. Let us help you achieve long-lasting, cost-effective solutions for your next project. Reach out to us today for the best in galvanized steel products.