Hot Dip Galvanized S320GD Steel Coil | 1.0250
- John
Hot-dip galvanized S320GD steel is a versatile and durable material. It is dependable for building structures and serves as a durable option for exterior use.
SteelPro Group, a leader in the steel industry, provides high-quality S320GD steel products tailored to meet the diverse needs of our clients. Our products offer exceptional value and performance.
S320GD Hot-dip Galvanized Steel Description
Hot dip galvanized S320GD steel is a high-strength steel. “320” indicates the minimum yield strength of 320 MPa. S320GD steel is widely recognized for its excellent formability, strength, and superior corrosion protection. It can be produced through hot rolling and cold rolling, with a hot dip galvanizing treatment applied. It is extensively utilized in fields such as the vehicle manufacturing and building industries.
SteelPro Group provides S320GD in the form of coils and strips, ensuring high-quality material for diverse projects.
S320GD Equivalent Grades
S320GD is equivalent to the European standard EN10346:2015 grade 1.0250.
SteelPro Group manufactures S320GD steel in compliance with EN10346:2015 and other international standards, ensuring consistent quality, durability, and corrosion resistance
S320GD Galvanized Steel Coil Chemical Composition
| Element | Maximum Content (%) |
| Carbon (C) | 0.2 |
| Silicon (Si) | 0.6 |
| Manganese (Mn) | 1.7 |
| Phosphorus (P) | 0.1 |
| Sulfur (S) | 0.045 |
S320GD Galvanized Steel Coil Mecahmical Properties
| Property | Value |
| Tensile Strength (Rm) | 290 – 390 MPa |
| 0.2% Proof Strength (Rp0.2) | ≥ 320 MPa |
| Minimum Elongation (Lo = 80 mm) (A) | ≥ 17% |
Note:
The minimum elongation requirement varies with thickness:
- 0.5 mm < t ≤ 0.7 mm: The minimum elongation is reduced by 2% compared to the listed value.
- 0.35 mm < t ≤ 0.5 mm: The minimum elongation is reduced by 4% compared to the listed value.
- t ≤ 0.35 mm: The minimum elongation is reduced by 7% compared to the listed value.
The tensile strength range for this grade can vary by up to 140 MPa, depending on processing conditions and coating specifications.
S320GD Galvanized Steel Applications
SteelPro Group supplies S320GD steel in coils and strips, ensuring reliable quality tailored to diverse industry needs. It combination of durability, strength, and cost efficiency.
- Construction and Infrastructure: Roofing panels, wall cladding, structural frameworks, bridges, guardrails, and support beams.
- Automotive Industry: Body panels, chassis components, reinforcements, crash-resistant structures.
- Manufacturing and Engineering: Metal enclosures, HVAC ducts, electrical cabinets, storage systems, and machinery parts.
- Agricultural Equipment: Silos, fencing, farm machinery, outdoor storage facilities.
- Energy and Utilities: Power transmission towers, solar panel supports, wind turbine components, industrial pipelines, and water tanks.
S320GD Galvanized Steel Coil Specifications
| Specification | Metric (mm) | Imperial (inch) |
| Thickness | 0.3 – 3.0 mm | 0.012 – 0.118 in |
| Width | 600 – 1500 mm | 23.62 – 59.06 in |
S320GD Galvanized Steel Strip Specifications
| Specification | Metric (mm) | Imperial (inch) |
| Thickness | 0.3 – 3.0 mm | 0.012 – 0.118 in |
| Width | 20 – 600 mm | 0.79 – 23.62 in |
SteelPro Group offers S320GD steel coils and strips in various widths and thicknesses. We also supply S320GD galvanized steel with custom specifications to meet diverse industry needs.
S320GD Steel Coil & Strip Coatings
| Coating Designation | Total Coating Mass (g/m², both sides) | Coating Thickness (µm per side) |
| Z100 | 100 | ~7 |
| Z140 | 140 | ~10 |
| Z200 | 200 | ~14 |
| Z275 | 275 | ~20 |
| Z350 | 350 | ~25 |
Key Considerations:
- A thicker coating improves protection against corrosion, making it perfect for demanding outdoor conditions.
- Lower coating weight is often chosen for indoor applications or painted surfaces, where additional protection is unnecessary.
- The coating is applied uniformly during the hot dip galvanization, ensuring consistent protection across the steel surface.
SteelPro Group offers customized coating options to meet specific industry needs, ensuring optimal performance in construction, automotive, and manufacturing applications.
S320GD Steel Coil & Strip Coatings
The table below summarizes the common surface treatment options:
| Surface Treatment | Purpose | Key Benefits | Common Applications |
| Passivation (Chromate Coating) | Reduces white rust formation and oxidation | Improves corrosion resistance and surface brightness | Roofing, construction, structural steel |
| Oiling | Prevents oxidation during transport and storage | Protects against fingerprints and scratches | Automotive, precision manufacturing |
| Phosphate Treatment | Enhances paint adhesion for post-coating processes | Improves coating durability and uniformity | Painted steel products, industrial coatings |
| Anti-Fingerprint Coating | Prevents smudging and oxidation | Enhances aesthetics and durability | Home appliances, decorative applications |
SteelPro Group provides customized surface treatment options to meet industry-specific needs, ensuring optimal protection, process efficiency, and long-term durability.
Premium S320GD Galvanized Steel Supplier
SteelPro Group is a trusted supplier of high-quality S320GD galvanized steel. Our products include coil, pipe, and sheet. We provide custom specifications, surface treatments, and industry-specific solutions to support your manufacturing, construction, and industrial needs. Contact us today to find the perfect S320GD galvanized steel for your application.