Galvanized Steel S350GD Coil | 1.0529 EN10346-2015
- John
Metal-coated structural steel, such as Galvanized Steel S350GD, combines high strength with corrosion resistance through the protective layer of zinc. This material is perfect for uses that demand robust strength and enduring defense.
SteelPro Group’s S350GD galvanized steel is specifically designed for construction and outdoor structures, offering customized solutions to meet the unique needs of your projects.
S350GD Galvanized Steel Description
Galvanized Steel S350GD is a high-strength structural steel designed to withstand demanding applications. The “S350” designation indicates a minimum yield strength of 350 megapascals (MPa), ensuring its reliability and durability in structural settings. The “GD” refers to hot-dip galvanizing, a method in which the steel is submerged in molten zinc. This coating forms a protective layer that significantly enhances the steel’s resistance to corrosion, ensuring long-term performance even in harsh environments.
S350GD is particularly valued for its ability to bear heavy loads, resist rust and corrosion, and maintain durability over time, even when exposed to moisture, chemicals, or extreme weather conditions. These attributes make it an ideal choice for building construction, outdoor structures, roofing, and automotive components.
SteelPro Group offers S350GD in multiple forms—coil, strip, and flat—allowing for tailored solutions that meet the unique needs of your projects.
S350GD Galvanized Steel Properties
- High Strength: Minimum yield strength of 350 MPa, ensuring robust load-bearing capacity for structural applications.
- Corrosion Resistance: Hot-dip galvanization provides a durable zinc coating, offering excellent protection against rust and environmental degradation.
- Durability: Engineered to endure harsh weather conditions, chemicals, and humidity, making it perfect for exterior and industrial uses.
- Formability: Good workability for various manufacturing processes, including welding, cutting, and bending.
S350GD Coil Chemical Composition
| Element | Content |
| Carbon (C) | max 0.2% |
| Silicon (Si) | max 0.6% |
| Manganese (Mn) | max 1.7% |
| Phosphorus (P) | max 0.1% |
| Sulfur (S) | max 0.045% |
- If additional elements are included in the material by mutual agreement during the inquiry or ordering process, any necessary adjustments to the classification will be indicated in our inspection report.
S350GD Coil Mechanical Properties
| Property | Value | |
| Tensile Strength (Rm) | 420 MPa | |
| 0.2% Proof Strength (Rp0.2) | 35 MPa | |
| Min. Elongation (A, Lo = 80 mm) | – | 16 % |
| 0.5 < t ≤ 0.7mm | 14% | |
| 0.35 < t ≤ 0.5mm | 12% | |
| t ≤ 0.35mm | 9% | |
- “t” refers to thickness.
- The tensile strength of this grade can range up to 140 MPa.
S350GD Galvanized Steel Applications
S350GD coated steel is extensively utilized in different sectors due to its excellent strength, long-lasting performance, and corrosion resistance. Below are key industries and applications:
- Construction: Building structures, Bridges, Structural components
- Roofing and Cladding: Roofing panels, Wall cladding, Exterior facades
- Automotive Industry: Chassis components, Body panels, Structural reinforcements
- Outdoor Structures: Fences, Gates, Poles, Outdoor furniture
- Industrial Equipment: Machinery frames, Equipment housings, Storage tanks
S350GD Products Standards
Here are the standards related to different types of coated steel products and their technical delivery conditions. All S350GD products provided by SteelPro Group comply with the following standards.
| Standard | Product |
| EN 10346: 2009 | Continuously hot-dip coated steel flat products |
| EN 10326: 2004 | Continuously hot-dip coated strip and sheet of structural steel |
| EN 10147: 2000 | Continuously hot-dip zinc-coated structural steel strip and sheet |
| EN 10154: 2002 | Continuously hot-dip aluminium-silicon (AS) coated steel strip and sheet |
| EN 10162: 2003 | Cold rolled steel sections, dimensional and cross-sectional tolerances |
S350GD Coil Specifications
| Specification | Metric (mm) | Imperial (inches) |
| Thickness Range | 0.3 – 3.0 | 0.012 – 0.118 |
| Width Range | 600 – 1500 | 23.62 – 59.06 |
S350GD Strip Specifications
| Specification | Metric (mm) | Imperial (inches) |
| Thickness Range | 0.3 – 3.0 | 0.012 – 0.118 |
| Width Range | 30 – 1000 | 1.18 – 39.37 |
S350GD Flat Specifications
| Specification | Metric (mm) | Imperial (inches) |
| Thickness Range | 1.0 – 12.0 | 0.039 – 0.472 |
| Width Range | 100 – 2000 | 3.94 – 78.74 |
SteelPro Group offers S350GD galvanized steel in a variety of specifications, including coils, strips, flats, sheets, and pipes. We also provide tailor-made sizes to meet your specific requirements.
S350GD Galvanized Steel Metal Coating
| Coating Type | Coating Thickness (μm) | Coating Weight (g/m²) | Application |
| Zinc Coating (Z) | 30 – 275 | 50 – 500 | General industrial use, construction, automotive |
| Aluminum Coating (Al) | 30 – 80 | 50 – 200 | High-temperature resistance, roofing |
| Zinc-Aluminum Alloy Coating (ZA) | 50 – 150 | 100 – 300 | Enhanced corrosion resistance, marine environments |
| Galvalume Coating (Zn-Al) | 20 – 150 | 50 – 180 | Roofing, cladding, and high-durability applications |
S350GD Galvanized Steel Custom Solutions
SteelPro Group offers S350GD galvanized steel with a range of surface treatments, including chromate conversion, passivation, and oiling, to enhance durability and performance. We also offer personalized packaging and accurate length cutting to suit your unique project requirements. For customized solutions and professional advice, contact us today, and allow our team to assist you in choosing the perfect S350GD steel for your needs.