H13 Steel Tolerance: Precision and Quality from SteelPro Group
- John
SteelPro Group provides H13 tool steel products, including H13 steel plates, rods, and rounds. With decades of experience in the industry, we ensure that all of our products are made with strict tolerance control to meet the diverse needs of our clients.
H13 Steel Products And Tolerance Ranges
At SteelPro Group, we offer a wide range of H13 tool steel products, each with specific dimensions and tolerance control to ensure compatibility with your manufacturing processes. Here is an overview of the H13 steel product forms we offer and their corresponding tolerance ranges:
H13 Steel Tolerance According to Standards
Here is a summary of common tolerance ranges based on ASTM A681, DIN 17350, and JIS G4404:
| Standard | Product Form | Tolerance Range (Metric) | Tolerance Range (Imperial) |
| ASTM A681 | Steel Plates | ±1.0 mm to ±2.0 mm | ±0.039 in to ±0.079 in |
| Round Bars | ±0.25 mm to ±0.50 mm | ±0.010 in to ±0.020 in | |
| Flat Bars | ±0.5 mm to ±1.0 mm | ±0.020 in to ±0.039 in | |
| JIS G4404 | Round Bars | ±0.3 mm to ±0.6 mm | ±0.012 in to ±0.024 in |
| Flat Bars | ±0.5 mm to ±1.5 mm | ±0.020 in to ±0.059 in | |
| DIN 17350 | Steel Rounds | ±0.3 mm to ±0.5 mm | ±0.012 in to ±0.020 in |
| Square Bars | ±0.5 mm to ±1.0 mm | ±0.020 in to ±0.039 in |
We ensure that all our H13 tool steel products not only meet these standards but are also manufactured with tight tolerances for added precision.
H13 Tool Steel Product Forms and Sizes
We offer H13 tool steel in various forms, with strict tolerances and high precision. Below are the common sizes for H13 tool steel products. If you need sizes outside these ranges or custom tooling components, we are happy to provide tailored solutions to meet your exact needs.
| Product Form | Dimension | Metric Range | Imperial Range |
| Bars | Diameter | 25 mm – 300 mm | 1″ – 12″ |
| Length | 3000 mm – 6000 mm | 10′ – 20′ | |
| Plates | Thickness | 10 mm – 150 mm | 0.4″ – 6″ |
| Width | 200 mm – 1250 mm | 8″ – 50″ | |
| Length | 500 mm – 3000 mm | 20″ – 118″ | |
| Rounds | Diameter | 50 mm – 300 mm | 2″ – 12″ |
| Length | 1000 mm – 4000 mm | 3′ – 13′ | |
| Forged Blocks | Thickness | 100 mm – 250 mm | 4″ – 10″ |
| Width | 200 mm – 1000 mm | 8″ – 40″ | |
| Length | 500 mm – 3000 mm | 20″ – 118″ |
H13 Steel: Get the Precision You Need with SteelPro Group
We do not just supply H13 tool steel. we offer custom cutting, machining, heat treatment, and surface finishing services to meet your exact needs. Whether you need precise dimensions, special shapes, or custom sizes, we have the tools and expertise to deliver.
Contact us today to discuss your project. Let us work together to provide the right H13 steel products and services for your needs.