If you need steel that is strong, durable, and resistant to corrosion, DX52D Galvanized Steel is a great choice. At SteelPro Group, we offer high-quality DX52D galvanized coils, sheets, and pipes. Whether making car parts, roofing sheets, or machinery components, DX52D provides the strength and protection you are looking for.
DX52D Hot-dip Galvanized Steel Description
DX52D is a type of cold-rolled steel that is hot-dip galvanized for enhanced durability and protection. What distinguishes it is its unique blend of flexibility and durability. The steel is designed for applications that require deep drawing and shaping. It is ideal for complex parts like car body panels and roofing sheets. With a minimum yield strength of 220 MPa, it provides an ideal combination of bendability and durability.
- DX signifies that the steel is well-suited for deep drawing processes, allowing it to be easily molded into intricate shapes without compromising its strength.
- 52 refers to the minimum yield strength (in MPa) of the steel, which is approx. 220 MPa.
- D indicates it is produced by hot-dip galvanization.
SteelPro Group DX52D Galvanized Steel is available in various product forms, including coils, sheets, and pipes. It can be molded into different forms based on the specific requirements of your project.
DX52D Steel Equivalent Grades
- EN 10346-2015: 1.0918
- EN 10346-2009: 1.0350
- VDA 239-100: CR1 steel
DX52D Material Properties
Excellent formability
DX52D is perfect for processes like deep drawing and stamping. It can be molded into intricate shapes while maintaining its strength and stability.
Corrosion resistance
The zinc coating forms a strong shield against corrosion, prolonging the durability of the material, even in exposed or moisture-prone conditions.
Good surface quality
The smooth surface finish allows for easy coating application, ensuring paints and other finishes adhere well.
Moderate strength
With a minimum yield strength of 220 MPa, DX52D balances strength with flexibility, making it suitable for a wide range of uses.
Versatility
DX52D is available in coils, sheets, and pipes and is used in various industries, including automotive, construction, and home appliances.
DX52D Galvanized Coil Chemical Composition
| Element | Content (%) |
| Carbon (C) | ≤ 0.12 |
| Silicon (Si) | ≤ 0.5 |
| Manganese (Mn) | ≤ 0.6 |
| Phosphorus (P) | ≤ 0.1 |
| Sulfur (S) | ≤ 0.045 |
| Titanium (Ti) | ≤ 0.3 |
DX52D Galvanized Coil Mecahmical Properties
| Property | Value |
| Tensile Strength | 270 – 420 MPa |
| Yield Strength (0.2% Proof Strength) | 140 – 300 MPa |
| Minimum Elongation | 26% (Lo = 80 mm) |
Additional Information:
- For thickness 0.5mm < t ≤ 0.7mm, the minimum elongation is reduced by 2% compared to the value in the table.
- For thickness 0.35mm < t ≤ 0.5mm, the minimum elongation is reduced by 4%.
- For thickness t ≤ 0.35mm, the minimum elongation is reduced by 7%.
- For surface quality grade A, the upper yield strength is limited to 360 MPa.
DX52D Galvanized Steel Applications
| Industry | Application | Properties |
| Automotive | Car body panels, exterior components, structural parts | Strength, corrosion resistance |
| Construction | Roofing sheets, wall panels, building frames | Durability, weather resistance |
| Home Appliances | Washing machines, refrigerators, microwaves | Formability, rust resistance |
| Agricultural Equipment | Machinery parts, storage solutions | Strength, outdoor durability |
SteelPro Group offers high-quality DX52D Galvanized Steel for various industries. Whether for the automotive industry, construction projects, or household equipment, we deliver dependable solutions tailored to your unique requirements.
DX52D Galvanized Steel Products Specifications
At SteelPro Group, we offer a variety of DX52D Galvanized Steel products. Whether you’re dealing with coils, sheets, or pipes, we offer comprehensive product specifications to guarantee you receive the ideal material for your project.
| Dimensions | Coils | Width: 600 – 1,250 mm (23.62″ – 49.21″) | |
| Thickness: 0.30 – 2.00 mm (0.012″ – 0.079″) | |||
| Sheets | Width: 600 – 1,250 mm (23.62″ – 49.21″) | ||
| Thickness: 0.30 – 2.00 mm (0.012″ – 0.079″) | |||
| Pipes | Outer Diameter: 20 – 100 mm (0.79″ – 3.94″) | ||
| Thickness: 1.00 – 4.00 mm (0.039″ – 0.157″) | |||
| Coating Type | +Z,+ZF,+ZA,+ZM,+AZ | ||
| Coating Thickness | Z100 – Z250 g/m² | ||
| Surface | Big Spangle, Small Spangle, No Spangle | ||
Expert Advice on Choosing the Right Coating Type
Selecting the right coating type for DX52D Galvanized Steel depends on the environment and application. Here’s a quick guide:
- +Z (Standard Galvanized): Suitable for general applications with moderate corrosion exposure.
- +ZF (Zinc-Fe Alloy): Ideal for automotive and parts exposed to mechanical stress.
- +ZA (Zinc-Aluminum Alloy): Offers superior protection in harsh outdoor environments.
- +ZM (Zinc-Magnesium Alloy): Best for extreme weather conditions and heavy-duty applications.
- +AZ (Zinc-Aluminum-Magnesium Alloy): Provides maximum corrosion resistance for highly corrosive environments.
High-Quality DX52D Galvanized Steel for Your Projects
At SteelPro Group, we offer high-quality DX52D Galvanized Steel in different forms, including coils, sheets, and pipes, to suit your specific project requirements. We also provide PPGI DX51D as an alternative where suitable. With our industry expertise, competitive pricing, and reliable delivery, we’re here to help you select the right materials for your needs. Contact us today for expert advice and tailored solutions.