SteelPRO Group is a leading manufacturer and supplier of 304 Stainless Steel Coils in China. We provide:
1.4301 stainless steel coil, UNS S30400 stainless steel coil, ASTM A240 304 stainless steel coil, 304 stainless steel hot rolled coil, 304 stainless steel cold rolled coil, 304 stainless steel annealed coil, 304 stainless steel pickled coil, 304 stainless steel slit coil, 304 stainless steel brushed coil, 304 stainless steel polished coil, 304 stainless steel mirror coil, 304 stainless steel matted coil, 304 stainless steel bead blasted coil, 304 stainless steel embossed coil, 304 stainless steel etched coil, 304 stainless steel mill coil, 304 stainless steel sheared coil, 304 stainless steel welded coil, 304 stainless steel plate/sheet/strip/foil, etc.
| Standard | ASTM A240 / A240M, EN 10088-2 |
|---|---|
| Grade | 06Cr19Ni10, 1.4301, SUS 304, UNS S30400 |
| Thickness | 0.3 mm – 6 mm (0.012'' – 0.236''), Customized |
| Full Width | 1000 mm – 2000 mm (39.37'' – 78.74''), Customized |
| Edge | Customized, Deburred Edge, Mill Edge, Sheared Edge, Slit Edge |
| Surface Finish | 2B, 2D, 8K, BA, Brush, Checkered, Customized, Embossed, Etching, Hair Line, Mirror, No.1, No.4, No.8, Sand Blast |
| Technique | Annealing, Cold Rolling, Cutting to Length, Pickling, Slitting |
| Form | Brushed Coil, Cold Rolled Coil, Customized, Foils, Hot Rolled Coil, HRAP Coil, Mill Coil, Mirror Coil, Patterned Coil, Perforated Coil, Plates, Polished Coil, PVC-Coated Coil, Sheets, Slit Coil, Strips, Tin-Plated Coil, Titanium-Coated Coil |
| Terms | Specification |
|---|---|
| Minimum Order Quantity: | 5 Tons |
| Price: | To be negotiated |
| Packaging Details: |
As Requested
|
| Delivery Time: | Within 7-10 Working Days |
| Payment Terms: | T/T, L/C, Credit Card |
| Supply Ability: | 100000 Tons per month |
| Certification: | RoHS, BIS, SABS, tisi, KS, JIS, ISO9001 |
| Export To: |
United States, United Kingdom, Australia, Canada, Malaysia, India, Japan, Mexico, Netherlands, Poland, Russian Federation, Singapore, South Africa, Sweden, Afghanistan, Albania, etc.
|
| Element | Chromium, Cr | Nickel, Ni | Carbon, C | Manganese, Mn | Silicon, Si | Phosphorus, P | Sulfur, S | Nitrogen, N | Iron, Fe |
|---|---|---|---|---|---|---|---|---|---|
| Content (%) | 18.0-20.0 | 8.0-10.5 | ≤0.08 | ≤2.0 | ≤1.0 | ≤0.045 | ≤0.03 | ≤0.10 | Balance |
| Property | Metric | Imperial |
|---|---|---|
| Tensile Strength | 505 MPa | 73.2 ksi |
| Yield Strength (at 0.2% offset) | 215 MPa | 31.2 ksi |
| Brinell Hardness | 123 | 123 |
| Rockwell Hardness | 70 | 70 |
| Vickers Hardness | 129 | 129 |
| Elongation at Break (in 50 mm) | 70% | 70% |
| Young’s Modulus | 193-200 GPa | 28-29 msi |
1.Welding
2.Metal Fabrication
3.CNC Machining
4.Lathe
5.Forming
6.OEM/ODM
7.Quenching
8.Tempering
UT And Hardness Testing Info
At SteelPRO Group, we understand the importance of delivering your goods in pristine condition. That’s why we prioritize robust packing solutions to prevent any damage before your shipment arrives. We offer a range of packing methods and customization options to meet your specific needs. Trust us to handle your products with the utmost care and professionalism.
SteelPRO Group is a leading manufacturer and solutions provider of specialty steel. We are dedicated to delivering tailored, high-quality solutions across diverse industries. With a commitment to 100% quality assurance, we partner with our clients for mutual growth and success. Trust us to provide the expertise and reliability you need for your critical applications.
Choose us as your trusted partner, and you will get: