We are a supplier of prime quality 317L stainless steel pipes, offering various types including seamless, welded, straight, and coiled pipes. Our manufacturing processes include seamless, ERW, SSAW, and LSAW. We also provide customized services. If you require specialized processing and high-quality steel, please get in touch with us.
| Standard | ASTM A213, ASTM A269, ASTM A312 |
|---|---|
| Grade | 1.4438, SUS317L |
| Length | 6000 mm(20 feet) or custom lengths |
| OD | 6 mm(0.25 in) to 406.4 mm(16 inches) |
| WT | 0.5 mm(0.020 in) to 50 mm(2 in) |
| Surface Finish | Annealed, Bright, Mill, Pickled, Polished |
| Form | Bend Pipe, Corrugated Pipe, Seamless Pipe, Spiral Pipe, Tubing, Welded Pipe |
| Terms | Specifications |
|---|---|
| Minimum Order Quantity: | 5 Tons |
| Price: | To be negotiated |
| Packaging Details: |
As Requested
|
| Delivery Time: | Within 7-10 Working Days |
| Payment Terms: | T/T, L/C, Credit Card |
| Supply Ability: | 100000 Tons per month |
| Certification: | RoHS, BIS, SABS, tisi, KS, JIS, ISO9001 |
| Export To: |
United States, India, Korea
|
| Element | Cr | Ni | Mo | C | Mn | Si | P | S | N | Fe |
|---|---|---|---|---|---|---|---|---|---|---|
| Composition (%) | 18.0 – 20.0 | 11.0 – 15.0 | 3.0 – 4.0 | 0.030 max | 2.0 max | 1.0 max | 0.045 max | 0.030 max | 0.10 max | Balance |
| Mechanical Property | Value(Metric) | Value(Imperial) |
|---|---|---|
| Tensile Strength | 515 MPa | 75 ksi |
| Yield Strength | 205 MPa | 30 ksi |
| Vickers Hardness (HV) | 140 – 190 | 140 – 190 |
| Brinell Hardness (HB) | 146 – 200 | 146 – 200 |
| Rockwell Hardness (HRC) | 70 – 95 | 40 |
| Elongation | 40% | 35% |
| Elastic Modulus | 193 GPa | 28,000 ksi |
1.Welding
2.Metal Fabrication
3.CNC Machining
4.Lathe
5.Forming
6.OEM/ODM
7.Quenching
8.Tempering
UT And Hardness Testing Info
To deliver your 317L stainless steel tubes in perfect condition, our packaging solutions adhere to international shipping and safety standards. We regularly perform quality checks on our packaging process to ensure that your order meets all regulatory requirements.
When you choose us for your 317L stainless steel pipe needs, you can trust that your products will be delivered securely and ready for immediate use.
At SteelPRO Group, we are committed to delivering top-quality stainless steel products that meet industry standards. With years of experience in the stainless steel industry, we understand the specific needs of our clients and provide tailored solutions.
Quality Control: Our products undergo strict quality control processes to ensure they meet the highest standards of reliability and durability.
Competitive Pricing: We offer high-quality products at competitive prices, ensuring you get the best value for your investment.
Customer Support: Our knowledgeable team provides expert advice and assistance, helping you find the right product for your specific requirements.