SteelPRO Group is a reliable supplier of 316 Stainless Steel Plate from China:
We offer 316 hot-rolled plate, 316 cold-rolled plate, 316 seamless plate, 316 welded plate, 316 annealed plate, 316 polished plate, 316 perforated plate, 316 patterned plate. We provide custom processing options including cutting, bending, welding, drilling, polishing, heat treatment, surface finishing, waterjet cutting, laser cutting, and shearing.
| Standard | ASTM A240 |
|---|---|
| Grade | 0Cr17Ni12Mo2, SUS316, X5CrNiMo17-12-2 |
| Length | 6000 mm (236.22 in) to 12000 mm (472.44 in), Customized |
| Thickness | 1.5 mm (0.059 in) to 100 mm (3.937 in), Customized |
| Width | 1000 mm (39.37 in) to 2500 mm (98.43 in), Customized |
| Surface Finish | 2B, 2D, BA, Brushed, HL, Mirror, No.1, No.4, No.8, Satin |
| Technique | Annealed, Brushed, Cold Rolled, Embossed, Hot Rolled, Perforated, Pickled, Polished, Welded |
| Form | Cold Rolled Plate, Cold Rolled Sheet, Embossed Plate, Flat Plate, Heat Treated Plate, Hot Rolled Plate, Hot Rolled Sheet, Perforated Plate, Rolled Plate, Welded Plate |
| Terms | Specification |
|---|---|
| Minimum Order Quantity: | 5 Tons |
| Price: | To be negotiated |
| Packaging Details: |
As Requested
|
| Delivery Time: | Within 7-10 Working Days |
| Payment Terms: | T/T, L/C, Credit Card |
| Supply Ability: | 100000 Tons per month |
| Certification: | RoHS, BIS, SABS, tisi, KS, JIS, ISO9001 |
| Export To: |
United States, United Kingdom, Australia, India, Korea, Hong Kong, Russian Federation, Brazil, Malaysia, Canada, PhilippinesUnited States, Indonesia, Israel, Afghanistan, Albania, Algeria, American Samoa, Andorra, Angola, AnguillaAntigua And Barbuda, Argentina, Armenia, Austria, Azerbaijan, Bahamas, Bahrain, Bangladesh, Belarus, Belgium, Belize, Benin, Bhutan, Bolivia, etc.
|
| Element | Carbon (C) | Chromium (Cr) | Nickel (Ni) | Manganese (Mn) | Silicon (Si) | Phosphorus (P) | Sulfur (S) | Molybdenum (Mo) | Nitrogen (N) | Iron (Fe) |
|---|---|---|---|---|---|---|---|---|---|---|
| Range | 0.08 max | 16.0 – 18.0 | 10.0 – 14.0 | 2.0 max | 1.0 max | 0.045 max | 0.03 max | 2.0 – 3.0 | 0.10 max | Balance |
| Properties | Metric Unit | Imperial Unit |
|---|---|---|
| Tensile Strength | 515 – 690 MPa | 74,700 – 100,000 psi |
| Yield Strength | 205 MPa | 30,000 psi |
| Vickers Hardness | 150 – 220 HV | 150 – 220 HV |
| Brinell Hardness | 146 – 217 HB | 146 – 217 HB |
| Rockwell Hardness | B80 – B95 | B80 – B95 |
| Elongation | 40% | 40% |
| Elastic Modulus | 193 – 200 GPa | 28,000 – 29,000 ksi |
Here are the characteristics of 316 Stainless Steel Plate:
1.Welding
2.Metal Fabrication
3.CNC Machining
4.Lathe
5.Forming
6.OEM/ODM
7.Quenching
8.Tempering
UT And Hardness Testing Info