SteelPRO Group is a reliable supplier of 431 Stainless Steel Plate from China:
We offer 431 Stainless Steel plates, 431 hot rolled plates, 431 cold rolled plates, 431 annealed plates, 431 polished plates, 431 satin finish plates, 431 mill finish plates, 431 brushed plates, and 431 etched plates. We provide customizable processing methods, including cutting, bending, welding, grinding, polishing, drilling, punching, laser cutting, heat treatment, water jet cutting, and shearing.
| Standard | ASTM A240 |
|---|---|
| Grade | 1Cr17Ni2, SUS431, X29CrMo13-4 |
| Length | 6000 mm (236.22 in) to 12000 mm (472.44 in), Customized |
| Thickness | 10 mm (0.39 in), 12 mm (0.47 in), 15 mm (0.59 in), 20 mm (0.79 in), 3 mm (0.12 in), 6 mm (0.24 in), Customized |
| Width | 1000 mm (39.37 in), 1200 mm (47.24 in), 1500 mm (59.06 in), 2000 mm (78.74 in) |
| Surface Finish | 2B, BA, Brushed, Etched, HL, Mirror, No.1, No.4, Polished, Satin |
| Technique | Annealing, Bending, Cold Rolling, Grinding, Hot Rolling, Punching, Shearing, Welding |
| Form | Annealed plate, Brushed plate, Cold Rolled Plate and Sheet, Etched Plate, Hot Rolled Plate and Sheet, Pickled Plate, Polished Plate, Satin finish plate, Tempered plate |
| Terms | Specification |
|---|---|
| Minimum Order Quantity: | 5 Tons |
| Price: | To be negotiated |
| Packaging Details: |
As Requested
|
| Delivery Time: | Within 7-10 Working Days |
| Payment Terms: | T/T, L/C, Credit Card |
| Supply Ability: | 100000 Tons per month |
| Certification: | RoHS, BIS, SABS, tisi, KS, JIS, ISO9001 |
| Export To: |
United States, Korea, Russian Federation, United Kingdom, India, Vietnam, Brazil, France, Taiwan, Turkey, Romania, Lithuania, Netherlands, Philippines, Australia, Poland, Italy, Pakistan, Canada, Colombia, Argentina, Spain, Singapore, South Africa, Mexico, Germany, Bangladesh, Palestine, State of, Japan, Czech Republic, Indonesia, Hong Kong, Ukraine, Belgium, United Arab Emirates, Malaysia, etc.
|
| Element | Carbon (C) | Silicon (Si) | Manganese (Mn) | Phosphorus (P) | Sulfur (S) | Chromium (Cr) | Nickel (Ni) | Molybdenum (Mo) |
|---|---|---|---|---|---|---|---|---|
| Composition % | 0.12-0.20% | 0.50% max | 1.00% max | 0.040% max | 0.030% max | 15.00-17.00% | 1.25-2.50% | 0.20-0.50% |
| Properties | Metric Unit | Imperial Unit |
|---|---|---|
| Tensile Strength | 930-1080 MPa | 135-157 ksi |
| Yield Strength | 680-895 MPa | 98.6-130 ksi |
| Vickers Hardness | 270-320 HV | 270-320 HV |
| Brinell Hardness | 250-300 HB | 250-300 HB |
| Rockwell Hardness | 24-32 HRC | 24-32 HRC |
| Elongation | 15% | 15% |
| Elastic Modulus | 200 GPa | 29,000 ksi |
Here are the characteristics of 431 Stainless Steel Plate:
1.Welding
2.Metal Fabrication
3.CNC Machining
4.Lathe
5.Forming
6.OEM/ODM
7.Quenching
8.Tempering
UT And Hardness Testing Info
SteelPRO Group is a Manufacturer and solutions provider for specialty steel, offering custom services and 100% quality assurance!
Choose us and we can offer you: