SteelPRO Group is a leading manufacturer and supplier of 304 Stainless Steel Wires in China. We provide:
UNS S30400 wire, 1.4301 wire, 304 round/flat/square/rectangular/wedge wire, 304 annealed wire, 304 cold drawn wire, 304 hard drawn wire, 304 soft wire, 304 spring wire, 304 welded wire, 304 wire mesh, 304 wire rope, 304 bright wire, etc.
| Standard | ASTM A580, EN 10270-3, GB/T 4240 |
|---|---|
| Grade | 06Cr19Ni10, 1.4301, SUS 304, UNS S30400 |
| Length | 100 m – 1000 m (328' – 3280'), Customized |
| Diameter | 0.1 mm – 10 mm (0.004'' – 0.394''), Customized |
| Surface Finish | 2B, BA, Customized., Electropolished, Hairline, No.4, No.8, Passivated, Sand Blast |
| Shape | Customized, Flat, Hexagonal, Oval, Rectangular, Round, Square, Triangular, Wedge |
| Form | Annealed Wire, Braided Wire, Bright Wire, Cold Drawn Wire, Hard Drawn Wire, Plated Wire, Shaped Wire, Soft Wire, Spring Wire, Support Wire, Welding Wire, Wire Mesh, Wire Rope |
| Terms | Specification |
|---|---|
| Minimum Order Quantity: | 5 Tons |
| Price: | To be negotiated |
| Packaging Details: |
As Requested
|
| Delivery Time: | Within 7-10 Working Days |
| Payment Terms: | T/T, L/C, Credit Card |
| Supply Ability: | 100000 Tons per month |
| Certification: | RoHS, BIS, SABS, tisi, KS, JIS, ISO9001 |
| Export To: |
United States, Russian Federation, Canada, India, Brazil, Mexico, Australia, France, Indonesia, Italy, Korea, Malaysia, Netherlands, Philippines, Singapore, Spain, Ukraine, etc.
|
| Element | Chromium, Cr | Nickel, Ni | Carbon, C | Manganese, Mn | Silicon, Si | Phosphorus, P | Sulfur, S | Nitrogen, N | Iron, Fe |
|---|---|---|---|---|---|---|---|---|---|
| Content (%) | 18.0-20.0 | 8.0-10.5 | ≤0.08 | ≤2.0 | ≤1.0 | ≤0.045 | ≤0.03 | ≤0.10 | Balance |
| Property | Metric | Imperial |
|---|---|---|
| Tensile Strength | 505 MPa | 73.2 ksi |
| Yield Strength (at 0.2% offset) | 215 MPa | 31.2 ksi |
| Brinell Hardness | 123 | 123 |
| Rockwell Hardness | 70 | 70 |
| Vickers Hardness | 129 | 129 |
| Elongation at Break (in 50 mm) | 70% | 70% |
| Young’s Modulus | 193-200 GPa | 28-29 msi |
Common heat treatment processes of 304 wire:
1.Welding
2.Metal Fabrication
3.CNC Machining
4.Lathe
5.Forming
6.OEM/ODM
7.Quenching
8.Tempering
UT And Hardness Testing Info
At SteelPRO Group, we understand the importance of delivering your goods in pristine condition. That’s why we prioritize robust packing solutions to prevent any damage before your shipment arrives. We offer a range of packing methods and customization options to meet your specific needs. Trust us to handle your products with the utmost care and professionalism.
We provide the following packing options (but not limited to these) based on different conditions:
SteelPRO Group is a leading manufacturer and solutions provider of specialty steel. We are dedicated to delivering tailored, high-quality solutions across diverse industries. With a commitment to 100% quality assurance, we partner with our clients for mutual growth and success. Trust us to provide the expertise and reliability you need for your critical applications.
Choose us as your trusted partner, and you will get: