SteelPRO Group is a leading manufacturer and supplier of 430 Stainless Steel Wires in China. We provide:
ASTM A580 430 wire, UNS S43000 wire, 1.4016 wire, 430 stainless steel round/flat/square/rectangular/wedge wire, 430 stainless steel annealed wire, 430 stainless steel cold drawn wire, 430 stainless steel hard drawn wire, 430 stainless steel soft wire, 430 stainless steel spring wire, 430 stainless steel welded wire, 430 stainless steel wire mesh, 430 stainless steel wire rope, 430 stainless steel bright wire, etc.
| Standard | AISI 430, ASTM A580, EN 10088-3 |
|---|---|
| Grade | 1.4016, 1Cr15, SUS 430, UNS S43000 |
| Length | 500 mm – 3,000 mm (19.69" – 118.11"), Customized |
| Diameter | 0.10 mm – 5.00 mm (0.0039" – 0.197"), Customized |
| Surface Finish | BA, Bright, Brushed, Customized., Electropolished, Matte, Mill |
| Shape | Customized, Flat, Hexagonal, Oval, Rectangular, Round, Square, Triangular, Wedge |
| Form | Annealed Wire, Braided Wire, Bright Wire, Cold Drawn Wire, etc., Hard Drawn Wire, Plated Wire, Shaped Wire, Soft Wire, Spring Wire, Support Wire, Welding Wire, Wire Mesh, Wire Rope |
| Terms | Specification |
|---|---|
| Minimum Order Quantity: | 5 Tons |
| Price: | To be negotiated |
| Packaging Details: |
As Requested
|
| Delivery Time: | Within 7-10 Working Days |
| Payment Terms: | T/T, L/C, Credit Card |
| Supply Ability: | 100000 Tons per month |
| Certification: | RoHS, BIS, SABS, tisi, KS, JIS, ISO9001 |
| Export To: |
United States, Canada, India, Australia, New Zealand, Singapore, South Africa, etc.
|
| Element | Carbon, C | Chromium, Cr | Iron, Fe | Manganese, Mn | Phosphorus, P | Sulfur, S | Silicon, Si |
|---|---|---|---|---|---|---|---|
| Wt. % | ≤ 0.12 | 14 – 18 | 79 – 87 | ≤ 1 | ≤ 0.04 | ≤ 0.03 | ≤ 1 |
| Property | Metric | Imperial |
|---|---|---|
| Tensile Strength, Ultimate | 517 MPa | 75 ksi |
| Yield Strength (at 0.2% offset) | 345 MPa | 50 ksi |
| Rockwell Hardness (B) | 85 | 85 |
| Elongation at Break | 25% (in 50 mm) | 25% (in 2”) |
| Young’s Modulus | 200 GPa | 29 msi |
Common heat treatment processes of ss 430 wires:
Note: 430 stainless steel cannot be hardened by heat treatment due to its ferritic structure.
1.Welding
2.Metal Fabrication
3.CNC Machining
4.Lathe
5.Forming
6.OEM/ODM
7.Quenching
8.Tempering
UT And Hardness Testing Info
At SteelPRO Group, we understand the importance of delivering your goods in pristine condition. That’s why we prioritize robust packing solutions to prevent any damage before your shipment arrives. We offer a range of packing methods and customization options to meet your specific needs. Trust us to handle your products with the utmost care and professionalism.
We provide the following packing options (but not limited to these) based on different conditions:
SteelPRO Group is a leading manufacturer and solutions provider of specialty steel. We are dedicated to delivering tailored, high-quality solutions across diverse industries. With a commitment to 100% quality assurance, we partner with our clients for mutual growth and success. Trust us to provide the expertise and reliability you need for your critical applications.
Choose us as your trusted partner, and you will get: