Q195 Galvanized Wire
Q195 Galvanized Wire
SteelPRO Group provides high-quality Q195 galvanized steel wire that complies with international standards such as GB/T 700, ASTM A36, SS400, S235JR, etc. Our products have excellent corrosion resistance and durability, and are suitable for construction, agriculture, industrial manufacturing and other fields. SteelPRO Group is committed to providing customers with stable and reliable galvanized steel wire solutions, and provides customized specifications and packaging services according to needs to ensure efficient and safe delivery to all regions of the world.
- Standards: GB/T 700, ASTM A641, JIS G3547, etc.
- Grades: Q195, Q235, A36, S235JR, SS400, etc.
- Wire gauge: 8-24 gauge, 14 gauge, 16 gauge, 12 gauge, etc.
- Technology: Hot dip galvanizing, electro galvanizing
- Special Use: Marine engineering, agricultural greenhouses, electrical grounding wires, protective nets, cage, etc.
- Form: Coil, Spool, Rope, Mesh
- Certification: ISO 9001, CE
Q195 Galvanized Wire
Q195 Galvanized Wire
Product Specifications
Product Specifications
| Product Name | Q195 Galvanized Steel Wire | ||
| Wire Diameter | 0.15mm – 8.00mm, Customized | ||
| Wire Coil Weight | 20-1200kg | ||
| Wire Coil Length | Varies by coil weight, common lengths include 100 m, 200 m, 300 m, Customized | ||
| Coil Outer Diameter | 800 – 1200 mm | ||
| Coil Inner Diameter | 400 – 600 mm | ||
| Zinc Layer | 20-400g/m², g30, g40, g60, g90, Customized, etc. | ||
| Elongation | ≥15% | ||
| Tensile strength | 300 – 500 MPa | ||
| Load strength | (Depends on sight line) | ||
| Coating Material | Polyester (PE), Silicone Polyester (SMP), High Durable Polyester (HDP), Fluoropolymer (PVDF) | ||
| Surface Treatment | anti-finger print/skin pass/oiled/dry/chromated/Embossed/Lamination | ||
| Test | Zinc Coating Thickness Test, Adhesion Test, Peel, Bend, Salt Spray Test, Tensile Test, Elongation, etc. | ||
| Tolerance | ±1% | ||
| Processing Service | Bending, Welding, Decoiling, Cutting, Punching | ||
| Invoicing | By actual weight | ||
| Delivery Time | 7-15 days | ||
| Payment | T/T, L/C, Credit Card | ||
| Port | Shanghai, Qingdao or according to your requirement | ||
| Packaging Details | In bundles, in bulk, customized packing | ||
Chemical Compositions
Chemical Compositions
| Element | Carbon (C) | Silicon (Si) | Manganese (Mn) | Phosphorus (P) | Sulfur (S) |
|---|---|---|---|---|---|
| Content (%) | 0.06 – 0.12 | ≤ 0.30 | 0.25 – 0.50 | ≤ 0.035 | ≤ 0.040 |
Mechanical properties
Mechanical properties
| Property | Value |
|---|---|
| Tensile Strength (MPa) | 315 – 430 |
| Yield Strength (MPa) | ≥ 195 |
| Elongation (%) | ≥ 10 |
| Vickers Hardness (HV) | 70 – 120 |
| Brinell Hardness (HB) | 60 – 100 |
| Rockwell Hardness (HRB) | 55 – 75 |
| Elastic Modulus (GPa) | ~ 200 |
Industries & Applications
Industries & Applications
- Construction: Binding and reinforcement wire, tie wire for formwork. Reinforcement in masonry structures and wire lath in roofing installations.
- Agriculture: Vineyard trellis wire, plant support, fencing for livestock.
- Industrial Manufacturing: Production of wire mesh, nails, and fasteners.
- Household Applications: DIY crafts, picture hanging, light-duty home repairs.
- Packaging and Logistics: Bundling wire, cable reinforcement, and secure packaging.
- Automotive Industry: Used in seat springs and interior reinforcement.
- Electronics Industry: Used for grounding wires and components in electronic devices.
- Fishing Gear: Fabrication of durable fish traps, cages, and line leaders.
- Art Installations and Sculptures: Used by artists for wire-based sculptures and installations due to its pliability and surface finish.
- Aerospace and Defense: Light-duty support structures and wire mesh for insulation or shielding.
Other Infomation
Other Infomation
When Q195 galvanized steel wire reaches the end of its service life or the project is over, it is recommended that you recycle and dispose of it in the following environmentally friendly ways:
Recycling and reuse: Q195 galvanized steel wire is a highly recyclable metal material that can be sent to local recycling stations or scrap metal processing plants. Through recycling, the iron and zinc in the steel wire can be reprocessed and reused, avoiding waste of resources while reducing the burden on the environment.
Safe disposal of discarded steel wire: When discarding steel wire, it is recommended to avoid throwing it away at will, especially in outdoor environments. If it cannot be sent to the recycling point in time, the discarded steel wire can be stored in a moisture-proof and rust-proof place and wait for unified recycling and treatment to ensure that it will not pollute the soil or water source due to long-term exposure.
Environmental advantages of resource recycling: Through recycling, the metal components of Q195 galvanized steel wire can be recycled many times. This not only reduces the need for mining new resources, but also reduces the energy consumption of raw materials production, helping you to continue the value of the product in an environmentally friendly way after the project is completed.
What are the benefits of using our Q195 galvanized steel wire?
- Reduce replacement frequency:The high-quality zinc layer of Q195 galvanized steel wire effectively prevents oxidation and prolongs service life. Compared with ordinary steel wire, it can significantly reduce the need for replacement, thereby saving procurement and maintenance costs.
- Reduce maintenance costs:The excellent anti-corrosion performance makes Q195 galvanized steel wire unnecessary for frequent coating maintenance, reducing daily maintenance expenses in long-term outdoor exposure environments, saving time and labor.
- Optimize material and construction costs:The durability and stability of galvanized steel wire reduce the risk of material failure during construction, avoid repeated construction and rework, and help customers effectively control project costs.
Our Inventory
Our Inventory
SteelPRO Group has become a trusted partner for many customers with its strong production capacity and rich industry experience. Our production lines are equipped with advanced equipment and have efficient and stable production capacity to meet the needs of large and diverse orders. Through close cooperation with partners in various industries around the world, we not only increase production but also ensure strict quality control. Our production process is strictly carried out in accordance with international standards. From material selection and processing to galvanizing and packaging, every link is carefully tested to ensure that the products meet the highest standards in durability, corrosion resistance and strength. We are committed to providing customers with a stable and high-quality product experience through innovative technology and continuous optimization of production processes.
Main products: Q195 galvanized steel wire, steel pipes, steel plates, steel coils, steel bars, steel strips, stainless steel series, carbon steel series, high-strength steel series, nuclear grade steel, galvanized steel, steel for wind and solar energy, etc.
Packing
Packing
We use high-standard packaging solutions to ensure that Q195 galvanized steel wire always maintains its quality during long-distance transportation. Each roll of steel wire is first tightly wrapped with a moisture-proof plastic film to prevent rust or damage caused by changes in environmental humidity. The outer layer is wrapped in a durable woven bag, and some products are reinforced with wooden pallets or iron brackets to improve safety and stability during loading, unloading and transportation. The packaging size and method can be flexibly adjusted according to customer needs to better adapt to different storage and transportation conditions. In addition, our products have been successfully exported to the Middle East, South America, Africa, Southeast Asia and many other regions, ensuring that each batch of products reaches customers safely and efficiently, meeting the global market’s demand for high-quality galvanized steel wire.
Our Service
Our Service
1.Welding
2.Metal Fabrication
3.CNC Machining
4.Lathe
5.Forming
6.OEM/ODM
7.Quenching
8.Tempering
How to confirm the production progress of the order?
We provide real-time order tracking services, and customers can contact the account manager at any time to obtain the production progress and estimated delivery time, ensuring that the whole process is transparent and controllable.
What documents or certifications can SteelPRO Group provide?
We can provide material reports, quality certificates, export certifications, etc. to ensure that the products meet the quality and safety requirements of the customer’s country.
Will the price of Q195 galvanized steel wire be adjusted with market fluctuations?
Yes, since the market price of steel may be affected by raw materials and market demand, our product prices will be adjusted appropriately. To ensure that you get the best quotation, please contact the sales team in time.
Does SteelPRO Group provide customized services?
Yes, we provide customized services, including wire diameter, zinc layer thickness, packaging method, etc., to better meet your project needs.
Is there a minimum order quantity requirement for Q195 galvanized steel wire?
We can flexibly adjust the minimum order quantity according to the actual needs of customers to meet various needs from small batch purchases to large-scale projects.
Can the SteelPRO Group team assist customers in choosing the right products?
Yes. Our experienced team will provide professional advice based on your specific needs, application scenarios and budget to help you choose the most suitable product solution.