By Shape

By Grades

Comparisons

Finish

Maintenance

410 Stainless Steel Plate | Sheet

410 Stainless Steel Plate | Sheet

We are 410 stainless steel plate and sheet supplier. We offer various product types, including 410 stainless steel foil, cold-rolled sheets, hot-rolled plates, and cut-to-size options, in equivalent grades such as SS410, 1.4006, and X12Cr13. Our processing methods include annealing, hardening, tempering, normalizing, stress relieving, quenching, and more. We also provide custom product services.

Standard

ASTM A240, ASTM A276, ASTM A479

Grade

1.4006, 410S21, S41000, X12Cr13

Length

1,000 mm (39.37 in) to 6,000 mm (19.68 ft), Customized

Width

1,000 mm (39.37 in) to 1,524 mm (60 in), Customized

Surface Finish

2B, 2D, BA, No. 1, NO. 4

Technique

Bending, Cutting, Heat Treatment, Passivation, Pickling, Polishing, Welding

Form

Cold Rolled Sheets, Hot Rolled Plates, Perforated Sheets, Polished Sheets, Textured Sheets

410 Stainless Steel Plate | Sheet

410 Stainless Steel Plate | Sheet

410 Stainless Steel Plates and Sheets are products made from a family of martensitic stainless steel. This steel contains high chromium, which provides good corrosion resistance and strength. Known for its hardness and durability, 410 stainless steel is magnetic and can be hardened through heat treatment. It is commonly used in applications where high strength and wear resistance are essential, such as in automotive parts, structural components, and industrial equipment.
Sheet plate of stainless steel

Business Terms

Business Terms

Terms Specification
Minimum Order Quantity: 5 Tons
Price: To be negotiated
Packaging Details:
As Requested
Delivery Time: Within 7-10 Working Days
Payment Terms: T/T, L/C, Credit Card
Supply Ability: 100000 Tons per month
Certification: RoHS, BIS, SABS, tisi, KS, JIS, ISO9001
Export To:
United States, Korea, Russian Federation, United Kingdom, India, Brazil, etc.

Chemical Compositions

Chemical Compositions

ElementCMnSiCrNiPSFe
Composition Range (%)0.08 – 0.151.00 max1.00 max11.50 – 13.500.75 max0.04 max0.03 maxBalance

Mechanical Properties

Mechanical Properties

Mechanical PropertyValue (Metric)Value (Imperial)
Tensile Strength480 – 620 MPa70 – 90 ksi
Yield Strength275 – 450 MPa40 – 65 ksi
Brinell Hardness (HB)170 – 201 HB170 – 201 HB
Rockwell Hardness (HRC)20 – 30 HRC20 – 30 HRC
Vickers Hardness (HV)180 – 230 HV180 – 230 HV
Elongation20% – 25%20% – 25%
Elastic Modulus200 GPa29 x 10³ ksi

Heat Treatment

Heat Treatment

Stainless steel sheet plate heat-treatment
  1. Normalizing
    • Heat to 900°C to 955°C (1650°F to 1750°F) and hold at this temperature. Then, cool in the air.
    • Refines grain structure and improves mechanical properties.
  2. Annealing
    • Heat to 815°C to 900°C (1500°F to 1650°F) and hold at this temperature. Then, cool slowly in the furnace to room temperature.
    • Reduces hardness and improves machinability.
  3. Quenching
    • Heat to 925°C to 1010°C (1700°F to 1850°F) and hold at the temperature. Then, rapidly cool by air or oil quenching.
    • Increases hardness and forms a martensitic structure.
  4. Tempering
    • Heat to 200°C to 600°C (400°F to 1100°F) and hold to relieve stresses from quenching. Cool slowly in the air.
    • Adjusts hardness and improves toughness.
  5. Stress Relieving
    • If necessary, heat to 650°C to 760°C (1200°F to 1400°F) and hold to reduce residual stresses from welding or cold working. Cool slowly in the air.
    • Reduces residual stresses and improves stability.

Characteristic

Characteristic

  • Moderate Corrosion Resistance: Suitable for use in environments with low to moderate exposure to corrosive elements.
  • High Strength: Ideal for applications requiring the pipe to withstand high pressure and mechanical stress.
  • Enhanced Wear Resistance: Capable of being hardened through heat treatment to resist wear and abrasion.
  • Hardness: This pipe can be hardened through heat treatment, enhancing its wear resistance for longer service life.
  • Efficient Machinability: This can be easily processed using standard machining techniques.
  • Conditional Weldability: Requires careful welding practices, including preheating and post-weld treatments, to avoid potential issues.
  • Magnetic Properties: The pipe is magnetic in both annealed and hardened conditions.
  • Versatile Finish Options: 410 stainless steel plate and sheet can be finished in various ways, including polishing, to meet different aesthetic and functional requirements.
Automobile processing plant

Our Service

Our Service

1.Welding

2.Metal Fabrication

3.CNC Machining

4.Lathe

5.Forming

6.OEM/ODM

7.Quenching 

8.Tempering

UT And Hardness Testing

UT And Hardness Testing

UT And Hardness Testing Info

Surface Finish

Surface Finish

Stainless Steel Sheet Plate Surface Finish

2B Surface

Stainless Steel Sheet Plate Surface Finish

2D Surface

BA Surface

6K Surface

Stainless Steel Sheet Plate Surface Finish

8K Surface

Stainless Steel Sheet Plate Surface Finish

HL Surface

Stainless Steel Sheet Plate Surface Finish

NO.1 Surface

Stainless Steel Sheet Plate Surface Finish

NO.4 Surface

Embossed Surface

Packing

Packing

When you choose us for your 410 stainless steel plate and sheet needs, you can trust that your products will be delivered securely and ready for immediate use. We provide:

  • Tailored Protection: Each plate and sheet is inspected, wrapped in custom-fit protective materials, and separated by interleaving layers to prevent surface damage.
  • Heavy-Duty Crating: Plates and sheets are securely placed in reinforced wooden crates with steel banding to ensure stability during transit, preventing bending or warping.
  • Edge Protection: Apply protective edge guards or corner protectors to shield the edges of the plates and sheets from impact or bending during handling and shipping.
  • End-to-End Security: The packaging process includes careful stacking, securing, and sealing, with each package labeled for easy identification and handling.
  • Customized Packaging: Our packaging solutions are tailored to fit the specific dimensions and quantities of your order, ensuring maximum protection and ease of handling.
sheet_plate -packing
sheet plate packing
sheet plate packing
sheet plate packing
sheet plate packing
sheet plate packing

Why Choose Us

Why Choose Us

The workers are visiting factory

At SteelPRO Group, we are committed to delivering top-quality stainless steel products that meet industry standards. With years of experience in the stainless steel industry, we understand the specific needs of our clients and provide tailored solutions.

Quality Control: Our products undergo strict quality control processes to ensure they meet the highest standards of reliability and durability.

Competitive Pricing: We offer high-quality products at competitive prices, ensuring you get the best value for your investment.

Customer Support: Our knowledgeable team provides expert advice and assistance, helping you find the right product for your specific requirements.

Scroll to Top

Send Message

Please enable JavaScript in your browser to complete this form.
Case study Page 1
Case study Page 2
Case study Page 3
Case study Page 4
Case study Page 5
Case study Page 6
Case study Page 7
Case study Page 8
Case study Page 9
Case study Page 10
Case study Page 11
Case study Page 12
Case study Page 13