SteelPRO Group is a trusted supplier of 409 stainless steel rods, bars, and strips.
We offer 409 annealed rods, 409 cold-finished rods, 409 pickled bars, 1.4512 straightened bars, S40900 hot-rolled strips, and 409 slit strips. Our services include cutting, grinding, heat treatment, surface finishing, drilling, bending, laser cutting, forming and welding.
| Standard | ASTM A240, ASTM A276, ASTM A313 | 
|---|---|
| Grade | 09Cr19Ni10, 1.4509, SUS409 | 
| Length | Customized, Strip, bar, rod: 1000 mm to 6000 mm (39.37 inch to 236.22 inch) | 
| Diameter | Bar: 10 mm to 200 mm (0.39 in to 7.87 in), Customized, Rod: 5 mm to 100 mm (0.20 in to 3.94 in) | 
| Surface Finish | 2B, Brushed, Electropolishing, Hairline, No. 1, NO. 4, No. 8, Pickling | 
| Technique | Cold Rolling, Grinding, Heat Treatment, Hot Rolling, Passivation, Pickling | 
| Form | Annealed Strip, Cold-Finished Rod/Bar, Cold-Rolled Strip, Ground Rod/Bar, Hot-Rolled Rod/Bar, Hot-Rolled Strip, Pickled Strip, Polished Rod/Bar, Polished Strip, Threaded Rod | 
 
													| Terms | Specification | 
|---|---|
| Minimum Order Quantity: | 5 Tons | 
| Price: | To be negotiated | 
| Packaging Details: | As Requested | 
| Delivery Time: | Within 7-10 Working Days | 
| Payment Terms: | T/T, L/C, Credit Card | 
| Supply Ability: | 100000 Tons per month | 
| Certification: | RoHS, BIS, SABS, tisi, KS, JIS, ISO9001 | 
| Export To: | United States, Australia, India, Canada, Pakistan, Portugal, United Kingdom, Afghanistan, Albania, Algeria, American Samoal, Andorra, Angola, Anguilla, Antigua And Barbuda, Argentina, Armenia, Austria, Azerbaijan, Bahamas, Bahrain, Bangladesh, Belarus, Belgium, Belize, Benin, Bhutan, Bolivia, etc. | 
| Element | Carbon (C) | Manganese (Mn) | Phosphorus (P) | Sulfur (S) | Silicon (Si) | Chromium (Cr) | Nickel (Ni) | Titanium (Ti) | Nitrogen (N) | Iron (Fe) | 
|---|---|---|---|---|---|---|---|---|---|---|
| rods/bars/strip | 0.08 max | 1.00 max | 0.045 max | 0.030 max | 1.00 max | 10.5-11.75% | 0.50 max | 6 x C min | ≤ 0.030% | Balance | 
| Properties | Metric Units of 409 stainless steel | Imperial Units of 409 stainless steel | 
|---|---|---|
| Tensile Strength | 450-550 MPa | 65-80 ksi | 
| Yield Strength | 275-350 MPa | 40-50 ksi | 
| Vickers Hardness | 140-160 HV | 140-160 HV | 
| Brinell Hardness | 150-180 HB | 150-180 HB | 
| Rockwell Hardness | 70-80 HRB | 70-80 HRB | 
| Elongation | 20-30% | 20-30% | 
| Elastic Modulus | 200 GPa | 29 x 10^6 psi | 
 
													 
													1.Welding
2.Metal Fabrication
3.CNC Machining
4.Lathe
5.Forming
6.OEM/ODM
7.Quenching
8.Tempering
UT And Hardness Testing Info
 
													 
													 
													 
													 
													 
													 
													SteelPRO Group is a Manufacturer and solutions provider for specialty steel, offering custom services and 100% quality assurance!